Semiconductor device and power conversion device
By designing a structure in which the connection portion between the insulating film and the electrode is above the second upper surface of the electrode in the SiC semiconductor device, the stress problem caused by the increase in current density is solved, and the reliability and pass rate of the device are improved.
Patent Information
- Application Number
- CN202380029068.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-30
- Filing Date
- 2023-03-02
- Publication Date
- 2024-11-05
AI Technical Summary
When SiC semiconductor devices are used in high-pressure resistance, low-loss, and high-temperature environments, the increase in current density leads to increased stress, resulting in electrode damage and reduced reliability.
A semiconductor device structure is designed in which the first upper surface of the insulating film is connected to the protruding portion of the electrode, and the connection portion is formed at a distance of more than the second upper surface of the electrode, thereby reducing stress concentration and improving reliability.
By increasing the connection portion distance of the insulating film, stress concentration during assembly is effectively reduced, and the reliability and pass rate of the SiC semiconductor device are improved.
Smart Images

Figure CN118901141A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a semiconductor device and a power conversion device. Background Art
[0002] Silicon carbide (SiC) has better voltage resistance, lower resistance and heat resistance than silicon (Si). In order to use semiconductor devices in high voltage resistance, low loss and high temperature environments, power semiconductor devices such as MOSFET (Metal Oxide Semiconductor Field Effect Transistor) and IGBT (Insulated Gate Bipolar Transistor) made of SiC have been proposed.
[0003] Regarding these SiC semiconductor devices, for example, technologies have been proposed to miniaturize semiconductor devices by increasing the current density of semiconductor devices, or to reduce the number of semiconductor devices by using parasitic diodes (for example, Patent Document 1 and Patent Document 2). The above technologies reduce the manufacturing cost of SiC semiconductor devices, and therefore it is believed that they will be used in various components such as inverter components in the future.
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application Publication No. 2019-75411
[0007] Patent Document 2: Japanese Patent Application Publication No. 2020-13916 Summary of the invention
[0008] Problems to be solved by the invention
[0009] In SiC semiconductor devices, the high dielectric breakdown electric field of SiC is effectively utilized to develop smaller and more efficient semiconductor devices. However, due to the increase in the number of wirings for ensuring current capacity, the number of parts subjected to stress during assembly increases, and the stress increases due to the increase in temperature during operation accompanied by the increase in current density during power-on. As a result, electrodes such as the gate electrode of the semiconductor device are damaged, and there is a problem of reduced reliability of the semiconductor device.
[0010] Therefore, the present disclosure has been made in view of the above-mentioned problems, and an object of the present disclosure is to provide a technology capable of improving the reliability of a semiconductor device.
[0011] Means for solving problems
[0012] The semiconductor device disclosed in the present invention comprises: a semiconductor substrate; an electrode, at least a portion of which protrudes upward from a reference plane of the semiconductor substrate; and an insulating film, which covers the reference plane of the semiconductor substrate and the electrode, the insulating film having: a first upper surface, which corresponds to the reference plane of the semiconductor substrate and the at least a portion of the electrode protruding from the reference plane, respectively; and a protruding portion, which protrudes from the first upper surface, the distance between the reference plane of the semiconductor substrate and the connecting portion is greater than the distance between the reference plane of the semiconductor substrate and the second upper surface of the electrode, wherein the connecting portion is a connecting portion that connects the first upper surface of the insulating film and the surface of the protruding portion.
[0013] Effects of the Invention
[0014] According to the present disclosure, the distance between the reference surface of the semiconductor substrate and the connection portion is equal to or greater than the distance between the reference surface of the semiconductor substrate and the second upper surface of the electrode. With such a structure, the reliability of the semiconductor device can be improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 1 is a plan view showing the overall structure of the SiC semiconductor device according to the first embodiment.
[0016] Figure 2 : is a cross-sectional view showing the structure of the SiC semiconductor device according to the first embodiment.
[0017] Figure 3 1 is a flowchart showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0018] Figure 4 1 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0019] Figure 5 1 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0020] Figure 6 1 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0021] Figure 7 1 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0022] Figure 8 1 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0023] Fig. 9 1 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0024] Fig.10 1 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0025] Fig.11 1 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the first embodiment.
[0026] Fig.12 : is a cross-sectional view showing the structure of the SiC semiconductor device according to the first embodiment.
[0027] Fig.13 This is a cross-sectional view of a SEM image showing the structure of the SiC semiconductor device according to the first embodiment.
[0028] Fig.14 This is a cross-sectional view showing a packaging example of the SiC semiconductor device according to the first embodiment.
[0029] Fig.15 It is a graph showing the results of the test.
[0030] Fig.16 It is a cross-sectional view showing the structure of a SiC semiconductor device according to the second embodiment.
[0031] Fig.17 This is a flowchart showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0032] Fig.18 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0033] Fig.19 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0034] Fig. 20 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0035] Fig.21 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0036] Fig. 22 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0037] Fig.23 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0038] Fig.24 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0039] Fig.254 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0040] Fig.26 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0041] Fig. 27 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0042] Fig.28 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0043] Fig.29 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0044] Fig.30 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0045] Fig.31 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0046] Fig.32 4 is a cross-sectional view showing the manufacturing process of the SiC semiconductor device according to the second embodiment.
[0047] Fig.33 It is a cross-sectional view showing the structure of a SiC semiconductor device according to the second embodiment.
[0048] Fig.34 It is a graph showing the results of the test.
[0049] Fig.35 It is a cross-sectional view showing the structure of a SiC semiconductor device according to a third embodiment.
[0050] Fig.36 It is a cross-sectional view showing the structure of a SiC semiconductor device according to a third embodiment.
[0051] Fig.37 It is a cross-sectional view showing the structure of a SiC semiconductor device according to a third embodiment.
[0052] Fig.38 This is a block diagram showing the configuration of a power conversion system to which the power conversion device according to the fourth embodiment is applied. DETAILED DESCRIPTION
[0053] Hereinafter, the embodiments will be described with reference to the accompanying drawings. The features described in the following embodiments are illustrative, and all features are not essential. In addition, in the description shown below, the same or similar reference numerals are given to the same components in a plurality of embodiments, and mainly different components are described. In addition, in the description recorded below, specific positions and directions such as "up", "down", "left", "right", "front" or "back" may not necessarily be consistent with the positions and directions during actual implementation.
[0054] <Implementation Method 1>
[0055] Hereinafter, the semiconductor device of the first embodiment is described assuming that it is a SiC semiconductor device including silicon carbide (SiC) as a wide bandgap semiconductor. However, the material of the semiconductor device of the first embodiment may be ordinary silicon (Si) or a wide bandgap semiconductor other than silicon carbide (SiC). Examples of wide bandgap semiconductors other than silicon carbide (SiC) include gallium nitride (GaN) and diamond.
[0056] When the material of the semiconductor device is a wide bandgap semiconductor, it can achieve high withstand voltage, low loss, and use in high temperature environments. In particular, SiC has a higher dielectric breakdown electric field than Si, so the withstand voltage layer (such as the drift layer) used to achieve the same withstand voltage can be made thinner, or the impurity doping amount of the withstand voltage layer can be increased, thereby reducing the on-resistance, etc.
[0057] Figure 1 is a plan view showing the overall structure of the SiC semiconductor device according to the first embodiment. Figure 2 It means along Figure 1 A cross-sectional view of the structure of the SiC semiconductor device according to the first embodiment taken along line AA′.
[0058] The SiC semiconductor device comprises: an insulating protection film provided on Figure 1 The peripheral insulating region 10; the gate connecting portion 11; and Figure 2 The structure is surrounded by a peripheral insulating region 10 and is electrically connected to a gate connecting portion 11 .
[0059] Figure 2 The structure includes a SiC substrate 1 as an n-type semiconductor substrate, an n-type drift layer 2, a p-type base region 3, an n-type source region 4, a gate insulating film 5, a gate electrode 6 as an electrode, an interlayer insulating film 7 as an insulating film, a source electrode 8, and a drain electrode 9.
[0060] Figure 1 The gate connection portion 11 and Figure 2 The gate electrode 6 is electrically connected. In addition, the above n-type and p-type can also be replaced by p-type and n-type, respectively.
[0061] The SiC semiconductor device of the first embodiment is a MOSFET with a planar gate structure. Figure 2 The main unit structure of the SiC semiconductor device is shown in FIG. In the overall structure of an actual SiC semiconductor device, there are repeatedly arranged in the plane direction of the SiC substrate 1. Figure 1 The unit structure shown. In addition, the SiC semiconductor device of the present invention may also be a MOSFET with a trench gate structure, an IGBT, an RC-IGBT (Reverse Conducting-IGBT: reverse conducting insulated gate bipolar transistor), an SBD (Schottky Barrier Diode: Schottky barrier diode), or a PND (PN junction diode: PN junction diode). In Embodiment 2, an example in which the SiC semiconductor device of the present invention is a MOSFET with a trench gate structure is described.
[0062] Figure 3 1 is a flowchart showing the manufacturing process of the SiC semiconductor device according to the first embodiment. The SiC semiconductor device is manufactured according to this procedure.
[0063] In the semiconductor substrate preparation process of step S1, Figure 4 As shown, a drift layer 2 composed of SiC is formed as an epitaxial film on a first main surface (hereinafter referred to as a front surface) of a SiC substrate 1 .
[0064] Next, in the base region forming process of step S2, as shown in FIG. Figure 5 As shown, after a mask (not shown) made of resist or the like is formed on the n-type drift layer 2, p-type impurities are selectively ion-implanted to selectively form a base region 3 on the drift layer 2. Examples of p-type impurities include boron (B) and aluminum (Al).
[0065] Then, in the process of forming the source region in step S3, as shown in FIG. Figure 5 As shown, after a mask (not shown) made of a resist or the like is formed on the p-type base region 3, n-type impurities are selectively ion-implanted to selectively form the source region 4 on the upper portion of the base region 3. Examples of n-type impurities are phosphorus (P) and nitrogen (N).
[0066] Then, after the ion implantation, SiC substrate 1 is heat treated at high temperature by a heat treatment apparatus (not shown) to activate base region 3 and source region 4. Thus, p-type and n-type ions implanted into base region 3 and source region 4 are electrically activated.
[0067] Next, in the process of forming the gate insulating film in step S4, as shown in FIG. Figure 6As shown, a gate insulating film 5 is formed on the drift layer 2 , the base region 3 , and the source region 4 by a deposition method such as a thermal oxidation method or a chemical vapor growth method.
[0068] Then, in the gate electrode forming step of step S5, a gate electrode 6 is formed on the gate insulating film 5. The gate electrode 6 can be formed by depositing polycrystalline Si or poly-Si using chemical vapor growth or the like, or by depositing a tungsten film or tungsten silicide (WSi) when further high-speed operation of the SiC semiconductor device is desired. x ) film is formed.
[0069] Then, if Figure 7 As shown, the gate insulating film 5 and the gate electrode 6 are patterned using photolithography and dry etching or wet etching. The gate electrode 6 is patterned in such a manner that a pair of base regions 3 and a pair of source regions 4 are located below both ends of the gate electrode 6, and a portion of the drift layer 2 located between the pair of base regions 3 is located below the center portion of the gate electrode 6.
[0070] Next, in the interlayer insulating film forming process of step S6, as shown in FIG. Figure 8 As shown in FIG. 1 , a film made of TEOS (Tetra EthOxy Silane) or the like is formed as the interlayer insulating film 7 by, for example, using a vapor phase deposition (CVD) method. Fig. 9 As shown, the interlayer insulating film 7 is patterned using photolithography and dry etching or wet etching to expose a portion of the source region 4 .
[0071] Next, in the process of forming the source electrode in step S7, Fig.10 As shown, a source electrode 8 is formed on the source region 4 and the interlayer insulating film 7. The source electrode 8 is formed by, for example, appropriately forming a barrier metal composed of titanium or a titanium compound such as titanium nitride (TiN) on a film of aluminum, an aluminum alloy composed of aluminum and silicon, or nickel. Although not shown in the figure, the source electrode 8 is patterned using photolithography technology and dry etching or wet etching technology.
[0072] Then, in Figure 1 The insulating protective film is formed on the peripheral insulating region 10. The material of the insulating protective film is, for example, polyimide resin or silicone resin. In order to make the shape of the insulating protective film high-precision, it is preferred to use photolithography technology in the formation of the insulating protective film, and etching technology may also be used in combination. However, the method for forming the insulating protective film is not limited thereto, and for example, screen printing technology or drawing coating technology may also be used.
[0073] Next, in the SiC substrate thinning step of step S8, the second main surface (hereinafter referred to as the back surface) of the SiC substrate 1 is machined using a grinding tool to thin the SiC substrate 1. Fig.11 As shown, the SiC substrate 1 is thinned.
[0074] Then, in the drain electrode forming step of step S9, the drain electrode 9 is formed on the back side of the SiC substrate 1. Thus, the Figure 2 SiC semiconductor device. In addition, the drain electrode 9 is formed by forming a nickel film of about 600 nm by appropriately using a sputtering method or the like. If the surface of nickel is oxidized, the wettability of the solder alloy and nickel deteriorates, and the bonding state during chip bonding deteriorates. Therefore, a protective film can be formed on the surface of nickel using a metal with low reactivity such as gold or silver to form a drain electrode 9 composed of a laminated film of a nickel film and a protective film.
[0075] Fig.12 Yes means Figure 2 A cross-sectional view of the gate electrode 6 and its surrounding components in the structure of Fig.13 It means that the image was taken using a scanning electron microscope (SEM). Fig.12 A cross-sectional view of the image obtained by using the structure of Fig.12 , the upper surface of the SiC substrate 1 is indicated as a reference plane 1 a .
[0076] The gate electrode 6 is entirely disposed above the reference plane 1a of the SiC substrate 1, and the interlayer insulating film 7 covers the reference plane 1a of the SiC substrate 1 and the gate electrode 6. The interlayer insulating film 7 has a first upper surface 7a and a protruding portion 7b protruding from the first upper surface 7a, and the first upper surface 7a and the protruding portion 7b correspond to the reference plane 1a of the SiC substrate 1 and the gate electrode 6 protruding from the reference plane 1a, respectively.
[0077] exist Fig.12 7a shows the connection portion 7c connecting the first upper surface 7a of the interlayer insulating film 7 and the surface of the protruding portion 7b, and shows the distance h1 between the reference plane 1a of the SiC substrate 1 and the connection portion 7c. Fig.12 , a distance h2 between the reference plane 1a of the SiC substrate 1 and the second upper surface 6a of the gate electrode 6 is shown. In the first embodiment, the distance h1 is greater than or equal to the distance h2. That is, the ratio of the distance h1 to the distance h2 (h1 / h2) is greater than or equal to 1.
[0078] Fig.14 1 is a cross-sectional view showing an example of a package of a SiC semiconductor device according to the first embodiment. Fig.14 middle, Figure 2 The SiC semiconductor device is represented as SiC semiconductor device 12. Fig.14As shown, the back surface of SiC semiconductor device 12 is connected to lead frame 14a via solder 13, and the front surface of SiC semiconductor device 12 is connected to lead frame 14b via leads 15. SiC semiconductor device 12 and its surroundings are covered with mold resin 16.
[0079] For such Fig.14 In order to evaluate the accelerated degradation caused by repeated stress, the load of the tool during wire bonding of the lead 15 was set to 1.5 times the standard load.
[0080] Fig.15 : is a graph showing the results of the assembly test. The horizontal axis represents the ratio of the distance h1 to the distance h2 (h1 / h2), and the vertical axis represents the pass rate of SiC semiconductor devices judged as qualified products in the assembly test. Fig.15 As shown, when the ratio (h1 / h2) is greater than 1, the qualified rate of the assembled SiC semiconductor device can be improved. As described above, in the SiC semiconductor device of the first embodiment, the distance h1 is greater than the distance h2, and the ratio (h1 / h2) is greater than 1, so the qualified rate of the SiC semiconductor device can be improved, and the reliability can be improved.
[0081] In addition, in the above description, the case where the electrode covered by the interlayer insulating film 7 is the gate electrode 6 is described, but it is not limited to this. For example, the electrode covered by the interlayer insulating film 7 may also be a dummy electrode used as a dummy body of the gate electrode 6. This is also the same in the second embodiment described below.
[0082] <Implementation Method 2>
[0083] The SiC semiconductor device of the first embodiment is a semiconductor device with a planar gate structure, but the SiC semiconductor device of the second embodiment is a semiconductor device with a trench gate structure. The top view showing the overall structure of the SiC semiconductor device of the second embodiment is similar to the top view showing the overall structure of the SiC semiconductor device of the first embodiment ( Figure 1 )same.
[0084] Fig.16 It means along Figure 1 A cross-sectional view of the structure of the SiC semiconductor device according to the second embodiment taken along line AA′. Fig.16 The structure includes a SiC substrate 1 as an n-type semiconductor substrate, an n-type drift layer 2, a p-type base region 3, an n-type source region 4, a gate insulating film 5, a gate electrode 6 as an electrode, an interlayer insulating film 7 as an insulating film, a source electrode 8, a drain electrode 9, and a p-type bottom base region 17.
[0085] Figure 1The gate connection portion 11 and Fig.16 The gate electrode 6 is electrically connected. In addition, the above n-type and p-type can also be replaced by p-type and n-type. Fig.16 3 trench gate structures are shown in FIG. 1 , but the number of trench gate structures is not limited thereto. In the overall structure of an actual SiC semiconductor device, there are repeatedly arranged in the plane direction of the SiC substrate 1. Fig.16 Any number of trench gate configurations as shown.
[0086] Fig.17 1 is a flowchart showing the manufacturing process of the SiC semiconductor device according to the second embodiment. The SiC semiconductor device is manufactured according to this procedure.
[0087] In the semiconductor substrate preparation process of step S11, as Fig.18 As shown, a drift layer 2 containing SiC is formed as an epitaxial film on the front surface of a SiC substrate 1 .
[0088] Next, in the base region forming process of step S12, as shown in FIG. Fig.19 As shown, after a mask (not shown) made of resist or the like is formed on the n-type drift layer 2, p-type impurities are selectively ion-implanted to selectively form a base region 3 on the drift layer 2. The p-type impurities are, for example, boron (B) or aluminum (Al).
[0089] Then, in the process of forming the source region in step S13, Fig. 20 As shown, after a mask (not shown) made of a resist or the like is formed on the p-type base region 3, n-type impurities are selectively ion-implanted to selectively form the source region 4 on the upper portion of the base region 3. Examples of n-type impurities are phosphorus (P) and nitrogen (N).
[0090] Then, after the ion implantation, SiC substrate 1 is heat treated at high temperature by a heat treatment apparatus (not shown) to activate base region 3 and source region 4. Thus, p-type and n-type ions implanted into base region 3 and source region 4 are electrically activated.
[0091] Next, in the trench forming process of step S14, after forming a mask (not shown) made of a resist or the like that opens a portion of the source region 4, a trench is formed by dry etching using plasma or the like. Fig.21 The groove shown is a trench. In this case, if a resist mask that can fully withstand dry etching cannot be formed, Fig. 20 On the surface of the base region 3 and the source region 4, for example, an oxide film made of TEOS is formed, and dry etching is performed using the oxide film as a mask. In this case, a deeper trench can be formed.
[0092] Afterwards, if Fig. 22 As shown, in order to relax the electric field at the bottom of the trench gate structure, p-type impurities such as boron (B) and aluminum (Al) are ion-implanted into the bottom of the trench to form a bottom base region 17. In addition, when the electric field does not need to be relaxed, the bottom base region 17 may not be formed.
[0093] Then, in the gate insulating film formation process of step S15, the drift layer 2 is oxidized using a thermal oxidation method in order to remove plasma damage from the drift layer 2 when the trench is formed. In order to remove the plasma damage, it is preferable that the oxidation amount is large, but in the case of a large oxidation amount, the impurity layer formed in the drift layer 2 is reduced. In addition, from the measurement of the leakage current between the gate electrode 6 and the source electrode 8 of the finished product, it can be confirmed that if the thermal oxide film is 20 to 80 nm, more preferably 30 to 70 nm, the impurity layer is not substantially reduced, and the plasma damage is sufficiently removed from the drift layer 2.
[0094] Afterwards, if Fig.23 As shown, a gate insulating film 5 is formed in the trench by a deposition method such as thermal oxidation or chemical vapor growth. The thickness of the gate insulating film 5 on the side of the trench is preferably greater than the thickness of the gate insulating film 5 on the bottom side of the trench, and more preferably greater than 10% of the thickness of the gate insulating film 5 on the bottom side of the trench.
[0095] Then, in the gate electrode forming process of step S16, as shown in FIG. Fig.24 As shown, a gate electrode 6 is formed which is partially disposed in the trench. The gate electrode 6 can be formed by depositing polycrystalline Si or poly-Si using chemical vapor growth or the like, or by depositing a tungsten film or tungsten silicide (WSi) when further high-speed operation of the SiC semiconductor device is desired. x ) film is formed.
[0096] Then, if Fig.25 As shown, the gate electrode 6 is patterned using photolithography and dry etching or wet etching. In the patterning of the gate electrode 6, isotropic etching is preferably used, for example, if dry etching, etching using plasma containing SF6 is preferred, and if wet etching, etching using a mixed acid containing hydrofluoric acid and nitric acid is preferred.
[0097] In this embodiment 2, if Fig.25As shown, the gate electrode 6 includes a first electrode portion 6b protruding from a reference plane which is the upper surface of the SiC substrate and a second electrode portion 6c provided in a groove provided in the reference plane of the SiC substrate 1. In the plane direction of the SiC substrate 1, the width of the first electrode portion 6b is larger than the width of the second electrode portion 6c, and the gate electrode 6 as a whole has a T-shape. According to such a structure, the contact area between the gate electrode 6 and the drift layer 2, the base region 3, and the source region 4 can be increased. Therefore, when stress is generated during wiring or electrode bonding during assembly, the gate electrode 6 can be suppressed from being deformed in its length direction ( Fig.25 The inventors have confirmed through wiring-based assembly experiments that the sliding phenomenon is suppressed by the T-shaped gate electrode 6 as described above.
[0098] Thereafter, an oxide layer (not shown) is formed on the surface of the gate electrode 6 by thermal oxidation. The oxidation temperature at this time is, for example, preferably 850 to 1050°C, and more preferably about 900 to 1000°C.
[0099] Next, in the interlayer insulating film forming process of step S17, as shown in FIG. Fig.26 As shown in FIG. 1 , a film made of TEOS or the like is formed as the interlayer insulating film 7 by, for example, a vapor phase deposition (CVD) method. Fig. 27 As shown, the interlayer insulating film 7 is patterned using photolithography and dry etching or wet etching to expose a portion of the base region 3 and the source region 4 .
[0100] Next, in the process of forming the source electrode in step S18, as shown in FIG. Fig.28 As shown, a source electrode 8 is formed on the base region 3, the source region 4, and the interlayer insulating film 7. The source electrode 8 is formed by, for example, appropriately forming a barrier metal composed of titanium or a titanium compound such as titanium nitride (TiN) on a film of aluminum, an aluminum alloy composed of aluminum and silicon, or nickel. Although not shown in the figure, the source electrode 8 is patterned using photolithography technology and dry etching or wet etching technology.
[0101] Then, in Figure 1 The insulating protective film is formed on the peripheral insulating region 10. The material of the insulating protective film is, for example, polyimide resin or silicone resin. In order to make the shape of the insulating protective film high-precision, it is preferred to use photolithography technology in the formation of the insulating protective film, and etching technology may also be used in combination. However, the method for forming the insulating protective film is not limited thereto, and for example, screen printing technology or drawing coating technology may also be used.
[0102] Next, in the SiC substrate thinning step of step S19, the back side of the SiC substrate 1 is machined using a grinding tool to thin the SiC substrate 1. Fig.29 As shown, the SiC substrate 1 is thinned.
[0103] Then, in the drain electrode forming step of step S20, the drain electrode 9 is formed on the back side of the SiC substrate 1. Thus, the Fig.16 SiC semiconductor device. In addition, the drain electrode 9 is formed by forming a nickel film of about 600 nm by appropriately using a sputtering method or the like. If the surface of nickel is oxidized, the wettability of the solder alloy and nickel deteriorates, and the bonding state during chip bonding deteriorates. Therefore, a protective film can be formed on the surface of nickel using a metal with low reactivity such as gold or silver to form a drain electrode 9 composed of a laminated film of a nickel film and a protective film.
[0104] Next, another example is described in which the steps after the interlayer insulating film forming step of step S17 are different from the above example. In this example, the interlayer insulating film 7 is a TEOS film or SOG (Spin-On-Glass) film into which impurities such as B (boron) and P (phosphorus) are introduced. When the interlayer insulating film 7 is a TEOS film, a heat treatment at 700 to 900°C is performed after the TEOS film is formed. When the interlayer insulating film 7 is a SOG film, a heat treatment at 400 to 500°C is performed after the SOG film is formed. In this way, by performing a heat treatment corresponding to the material of the interlayer insulating film 7, such as Fig.30 As shown in FIG. 1 , the corner of the protrusion 7b protruding from the first upper surface 7a of the interlayer insulating film 7 marked with a dotted circle can be made larger than the corner of the protrusion 7b protruding from the first upper surface 7a. Fig.26 The corners are more rounded.
[0105] Then, the interlayer insulating film 7 is patterned. Then, in the process of forming the source electrode in step S18, as shown in FIG. Fig.31 As shown in FIG. 1 , a source electrode 8 is formed on the base region 3, the source region 4 and the interlayer insulating film 7. Then, after the thinning process of the SiC substrate in step S19 and the formation process of the drain electrode in step S20, the Fig.32 The SiC semiconductor device shown.
[0106] exist Fig.32 In the structure, by rounding the corners of the protrusion 7b, Fig.32 The concave portion marked with a dotted circle on the upper surface of the source electrode 8 is Fig.16 The concave portion is shallower, and the upper surface of the source electrode 8 is flattened. Fig.32 The inventors have confirmed that the bonding strength between the wiring lead and the source electrode 8 is Fig.16The bonding strength of the structure is higher, which can improve the reliability of the SiC semiconductor device. Fig.14 This is effective in a structure where the SiC semiconductor device 12 receives stress from various components such as the lead 15, the mold resin 16, and the lead frames 14a and 14b. In addition, the corners of the protrusion 7b are rounded and the upper surface of the source electrode 8 is flattened. Fig.32 In the structure, the reliability of the SiC semiconductor device is improved, which will be explained again later.
[0107] Fig.33 Yes means Fig.32 A cross-sectional view of the gate electrode 6 and its surrounding components in the structure of FIG. Fig.32 , the upper surface of the SiC substrate 1 is indicated as a reference plane 1 a .
[0108] The first electrode portion 6b of the gate electrode 6 protrudes from the reference plane 1a of the SiC substrate 1, and the interlayer insulating film 7 covers the reference plane 1a of the SiC substrate 1 and the gate electrode 6. The interlayer insulating film 7 has a first upper surface 7a and a protruding portion 7b protruding from the first upper surface 7a, and the first upper surface 7a and the protruding portion 7b correspond to the reference plane 1a of the SiC substrate 1 and the gate electrode 6 protruding from the reference plane 1a, respectively.
[0109] exist Fig.33 7a shows the connection portion 7c connecting the first upper surface 7a of the interlayer insulating film 7 and the surface of the protruding portion 7b, and shows the distance h1 between the reference plane 1a of the SiC substrate 1 and the connection portion 7c. Fig.33 , the distance h2 between the reference plane 1a of the SiC substrate 1 and the second upper surface 6a of the first electrode portion 6b is shown. In the second embodiment, as in the first embodiment, the distance h1 is greater than the distance h2, and the ratio of the distance h1 to the distance h2 (h1 / h2) is greater than 1. Thus, in the second embodiment, as in the first embodiment, the pass rate of the assembled SiC semiconductor device can be improved, and the reliability of the SiC semiconductor device can be improved. This is not only in Fig.16 In the structure or Fig.32 are the same in structure.
[0110] exist Fig.33 Graph 2 shows an angle θ1 formed between the reference plane 1 a of the SiC substrate 1 and the second side surface 7 e of the lower portion 7 d of the interlayer insulating film 7 below the first upper surface 7 a . Fig.33 The angle θ1 in the example is an angle formed between the reference plane 1 a of the SiC substrate 1 and the second side surface 7 e at a position halfway along the thickness of the lower portion 7 d .
[0111] In addition, Fig.332 shows an angle θ2 formed between the reference plane 1a of the SiC substrate 1 and the first side surface 7f of the protruding portion 7b of the interlayer insulating film 7. The first side surface 7f of the protruding portion 7b is, for example, a surface other than the upper surface of the protruding portion 7b. Fig.33 The angle θ2 in the example of θ is the angle between the reference plane 1a of the SiC substrate 1 and the first side surface 7f at a position halfway along the thickness of the protrusion 7b. Fig.32 and Fig.33 In the structure, the angle θ1 is greater than the angle θ2, and the ratio of the angle θ1 to the angle θ2 (θ1 / θ2) is greater than 1.
[0112] Fig.34 This is a graph showing the pass rate of SiC semiconductor devices after a switch test of 10,000 cycles to evaluate accelerated degradation in a structure where the ratio of the distance h1 to the distance h2 (h1 / h2) is 1. In this test, the current is set to 2 times the rated current. The horizontal axis represents the ratio of the angle θ1 to the angle θ2 (θ1 / θ2), and the vertical axis represents the pass rate of SiC semiconductor devices that were judged to be qualified in the switch test. Fig.34 As shown in FIG. 1 , it was confirmed that when the ratio (θ1 / θ2) is 1 or more, the reliability of the SiC semiconductor device can be improved.
[0113] The fact that the ratio (θ1 / θ2) is greater than or equal to 1 is substantially the same as the fact that the corners of the protrusion 7b are rounded. Therefore, when the ratio (θ1 / θ2) of the angle θ1 to the angle θ2 is greater than or equal to 1, the upper surface of the source electrode 8 can be flattened, and the bonding strength between the lead 15 and the source electrode 8 after wiring can be improved. In addition, the structure in which the ratio (θ1 / θ2) is greater than or equal to 1 can be applied not only to the trench gate structure of the second embodiment, but also to the planar gate structure of the first embodiment.
[0114] <Implementation Method 3>
[0115] In the present embodiment 3, the same reference numerals are given to the same components as those in the embodiment 1 or the embodiment 2, and their detailed description is omitted. The top view showing the overall structure of the SiC semiconductor device of the present embodiment 3 is similar to the top view showing the overall structure of the SiC semiconductor device of the present embodiment 1 or the embodiment 2 ( Figure 1 )same.
[0116] Fig.35 It means along Figure 1 A cross-sectional view of the structure of the SiC semiconductor device according to the third embodiment taken along line AA′. Fig.35 The structure includes a SiC substrate 1 as an n-type semiconductor substrate, an n-type drift layer 2, a p-type base region 3, an n-type source region 4, a gate insulating film 5, a gate electrode 6 as an electrode, an interlayer insulating film 7 as an insulating film, a source electrode 8, and a drain electrode 9.
[0117] Figure 1 The gate connection portion 11 and Fig.35 The gate electrode 6 is electrically connected. In addition, the above n-type and p-type can also be replaced by p-type and n-type, respectively.
[0118] Fig.36 Yes means Fig.35 An enlarged view of the positional relationship among the gate insulating film 5, the gate electrode 6 and the interlayer insulating film 7 in FIG. Fig.37 Yes means Fig.36 An enlarged view of the positional relationship between the end portion of the gate electrode 6 and the interlayer insulating film 7 in FIG.
[0119] In the third embodiment, the outer edge of the protrusion 7b of the interlayer insulating film 7 has a curved portion 7g in cross-sectional view. Furthermore, the connection portion 7i where the straight portion 7h and the curved portion 7g are connected in cross-sectional view of the upper surface of the protrusion 7b is located directly above the end of the gate electrode 6 or directly above the outer side of the end. In other words, the outer edge of the protrusion 7b has a curvature radius R. Fig.37 When the distance between the center point of the arc of the curvature radius R in the horizontal direction of the paper and the end of the gate electrode 6 is d, d is greater than or equal to 0.
[0120] In addition, the SiC semiconductor device of the third embodiment is a planar gate structure MOSFET, but it can also be a trench gate structure MOSFET, an IGBT, an RC-IGBT (Reverse Conducting-IGBT), an SBD (Schottky Barrier Diode), or a PND (PN junction diode).
[0121] The manufacturing process of the SiC semiconductor device of the third embodiment is Figure 3 The manufacturing process is the same as that shown in the flowchart of FIG. 1 , and the SiC semiconductor device is manufactured in this order. From step S1 to step S5, as shown in FIG. Figures 4 to 7 As shown, the same manufacturing process as in embodiment 1 is performed.
[0122] In the interlayer insulating film forming process of step S6, as Figure 8As shown, for example, a film composed of a TEOS (Tetra EthOxy Silane) film or an SOG (Spin-On-Glass) film is formed as the interlayer insulating film 7 by using a vapor phase deposition (CVD) method. At this time, the boron concentration contained in the interlayer insulating film 7 is set to 3 wt% or less. Therefore, when the interlayer insulating film 7 is a TEOS film, by performing a heat treatment at 700 to 900° C. after forming the TEOS film, the connecting portion 7i where the straight portion 7h and the curved portion 7g of the interlayer insulating film 7 are connected can be located just above the outer side of the end portion of the gate electrode 6. Similarly, when the interlayer insulating film 7 is an SOG film, by performing a heat treatment at 400 to 500° C. after forming the SOG film, the connecting portion 7i where the straight portion 7h and the curved portion 7g of the interlayer insulating film 7 are connected can be located just above the outer side of the end portion of the gate electrode 6.
[0123] Then, if Fig. 9 As shown, the interlayer insulating film 7 is patterned using photolithography and dry etching or wet etching to expose a portion of the source region 4 .
[0124] Afterwards, from step S7 to step S9, as shown in FIG. Figure 10 to Figure 11 As shown, the same manufacturing process as in Embodiment 1 is performed to complete Fig.35 The semiconductor device shown.
[0125] According to the above structure, Fig.15 As shown, the SiC semiconductor device is Fig.14 In the assembly test of the structure, the ratio (h1 / h2) is greater than 1, that is, the interlayer insulating film 7 covers the side of the gate electrode 6. As a result, the force in the left and right directions on the gate electrode 6 during wiring can be alleviated, so the pass rate of the assembled SiC semiconductor device can be improved. In addition, in the present embodiment 3, the connection part 7i where the straight part 7h and the curved part 7g are connected in the cross-section of the upper surface of the protrusion 7b of the interlayer insulating film 7 is located directly above the end of the gate electrode 6 or directly above the outside of the end. As a result, the force in the up and down directions on the gate electrode 6 during wiring can be alleviated, so the pass rate of the assembled SiC semiconductor device can be improved, and the reliability can be improved.
[0126] <Implementation Method 4>
[0127] The fourth embodiment applies the SiC semiconductor device of any one of the first to third embodiments to a power converter. The power converter of the fourth embodiment is not limited to a specific power converter, and the following describes a case where the power converter of the fourth embodiment is applied to a three-phase inverter.
[0128] Fig.38This is a block diagram schematically showing the configuration of a power conversion system to which the power conversion device 200 according to Embodiment 4 is applied. The power conversion system includes a power source 100 , the power conversion device 200 , and a load 300 .
[0129] The power supply 100 is a DC power supply, and supplies DC power to the power conversion device 200. The power supply 100 may be composed of various power supplies, such as a DC system, a solar cell, a storage battery, or a rectifier circuit or an AC / DC converter connected to an AC system. In addition, the power supply 100 may be composed of a DC / DC converter that converts the DC power output from the DC system into a predetermined power.
[0130] The power conversion device 200 is a three-phase inverter connected between the power supply 100 and the load 300. The power conversion device 200 converts the direct current supplied from the power supply 100 into alternating current, and supplies it to the load 300. The power conversion device 200 includes a main conversion circuit 201 and a control circuit 203. The main conversion circuit 201 converts the input direct current into alternating current, and outputs the alternating current. The control circuit 203 outputs a control signal for controlling the main conversion circuit 201 to the main conversion circuit 201.
[0131] Load 300 is a three-phase motor driven by AC power supplied from power converter 200. Load 300 is not limited to a specific use, and is a motor mounted on various electrical devices, such as a hybrid car, electric car, railway vehicle, elevator, or air conditioning device.
[0132] The following describes the details of the power conversion device 200. The main conversion circuit 201 includes a switching element and a freewheeling diode (not shown). The switching element switches, so that the main conversion circuit 201 converts the direct current supplied from the power supply 100 into alternating current, and supplies it to the load 300. The specific circuit structure of the main conversion circuit 201 has various structures, but the main conversion circuit 201 of the present embodiment 4 is a 2-level three-phase full-bridge circuit, which can be composed of 6 switching elements and 6 freewheeling diodes connected in reverse parallel to each switching element. At least one of the switching elements and freewheeling diodes of the main conversion circuit 201 applies the SiC semiconductor device 12 of any one of the above-mentioned embodiments 1 to 3 and their modified examples. The 6 switching elements are connected in series to form upper and lower arms for every 2 switching elements, and each upper and lower arm constitutes each phase (U phase, V phase, W phase) of the full-bridge circuit. Moreover, the output terminals of each upper and lower arm, that is, the three output terminals of the main conversion circuit 201, are connected to the load 300.
[0133] The main conversion circuit 201 includes a drive circuit (not shown) for driving each switching element. The drive circuit generates a drive signal for driving the switching element of the main conversion circuit 201 and supplies it to the control electrode of the switching element of the main conversion circuit 201. Specifically, the drive circuit outputs a drive signal for turning on the switching element and a drive signal for turning off the switching element to the control electrode of each switching element according to a control signal from a control circuit 203 described later. When the switching element is maintained in the on state, the drive signal is a voltage signal (on signal) above the threshold voltage of the switching element, and when the switching element is maintained in the off state, the drive signal is a voltage signal (off signal) below the threshold voltage of the switching element.
[0134] The control circuit 203 controls the switch elements of the main conversion circuit 201 to supply the desired power to the load 300. Specifically, the control circuit 203 calculates the time (on time) when each switch element of the main conversion circuit 201 should be in the on state based on the power to be supplied to the load 300. For example, the control circuit 203 can control the main conversion circuit 201 by pulse width modulation (PWM) control that modulates the on time of the switch element according to the voltage to be output. In addition, the control circuit 203 outputs a control instruction (control signal) to the drive circuit of the main conversion circuit 201 at each time point so that the on signal is output to the switch element that should be in the on state and the off signal is output to the switch element that should be in the off state. The drive circuit outputs the on signal or the off signal as a drive signal to the control electrode of each switch element according to the control signal.
[0135] The manufacturing method of the power conversion device 200 has the following steps. The SiC semiconductor device 12 is manufactured by the manufacturing method described in the above-mentioned embodiments 1 to 3 or their modified examples. The main conversion circuit 201 having the SiC semiconductor device 12 is formed. In addition, the control circuit 203 is formed. The power conversion device 200 is thus formed. When the main conversion circuit 201 is formed, for example, Fig.14 As shown, the drain electrode 9 of the SiC semiconductor device 12 is bonded to the lead frame 14 a via the solder 13 , and the source electrode 8 is bonded to the lead frame 14 b via the wire 15 .
[0136] According to the present embodiment 4, as at least one of the semiconductor devices constituting the main conversion circuit 201, the SiC semiconductor device 12 of any one of the embodiments 1 to 3 is used. As a result, unexpected adverse effects caused by stress during assembly of the SiC semiconductor device 12 can be suppressed, and adverse conditions caused by stress from peripheral components during switching operations can be suppressed. As a result, the reliability of the main conversion circuit 201 is improved. Therefore, the reliability of the power conversion device 200 can be improved.
[0137] In addition, in the present embodiment 4, an example of applying the SiC semiconductor device 12 to a 2-level three-phase inverter is described, but the present embodiment 4 is not limited to this and can be applied to various power conversion devices. In the present embodiment 4, the power conversion device is a 2-level power conversion device, but it can also be a multi-level power conversion device such as a 3-level power conversion device. In addition, in the case of supplying power to a single-phase load, the above-mentioned power conversion device can also be applied to a single-phase inverter. In addition, in the case of supplying power to a DC load, etc., the above-mentioned power conversion device can also be applied to a DC / DC converter or an AC / DC converter.
[0138] In addition, the power conversion device of this embodiment 4 is not limited to the case where the above-mentioned load is an electric motor. For example, it can also be used as a power supply device for any one of an electric discharge machine, a laser processing machine, an induction heating cooker, and a contactless power supply system. It can also be used as a power conditioner for a solar power generation system or a power storage system.
[0139] In addition, each embodiment and each modification example can be freely combined, or each embodiment and each modification example can be appropriately modified or omitted.
[0140] Description of symbols
[0141] 1: SiC substrate, 1a: reference plane, 6: gate electrode, 6a: second upper surface, 6b: first electrode portion, 6c: second electrode portion, 7: interlayer insulating film, 7a: first upper surface, 7b: protrusion, 7c: connection portion, 7d: lower portion, 7e: second side surface, 7f: first side surface, 7g: curved portion, 7h: straight portion, 7i: connection portion, 12: SiC semiconductor device, 201: main conversion circuit, 203: control circuit.
Claims
1. A semiconductor device comprising: Semiconductor substrates; an electrode, at least a portion of which protrudes upward from a reference surface of the semiconductor substrate; as well as an insulating film covering the reference surface of the semiconductor substrate and the electrode, The insulating film has: a first upper surface corresponding to the reference surface of the semiconductor substrate and the at least a portion of the electrode protruding from the reference surface, respectively; and a protrusion protruding from the first upper surface, A distance between the reference plane of the semiconductor substrate and a connection portion connecting the first upper surface of the insulating film and a surface of the protrusion is greater than a distance between the reference plane of the semiconductor substrate and a second upper surface of the electrode.
2. The semiconductor device according to claim 1, wherein All of the electrodes are disposed above the reference surface of the semiconductor substrate.
3. The semiconductor device according to claim 1, wherein The electrode comprises: a first electrode portion protruding from the reference surface of the semiconductor substrate; and The second electrode portion is provided in a groove provided on the reference surface of the semiconductor substrate.
4. The semiconductor device according to any one of claims 1 to 3, wherein: A ratio of an angle between the reference plane of the semiconductor substrate and a second side surface of the insulating film below the first upper surface to an angle between the reference plane of the semiconductor substrate and a first side surface of the protruding portion of the insulating film is greater than 1.
5. The semiconductor device according to any one of claims 1 to 4, wherein: The outer edge of the protrusion has a curved portion when viewed in cross section, A connection portion where the straight portion and the curved portion are connected in a cross-sectional view of the upper surface of the protrusion is located directly above the end of the electrode or directly above the outer side of the end.
6. The semiconductor device according to any one of claims 1 to 5, wherein: The material of the semiconductor device includes a wide bandgap semiconductor.
7. A power conversion device comprising: A main conversion circuit comprising the semiconductor device according to any one of claims 1 to 6, which converts input power and outputs the converted power; and A control circuit outputs a control signal for controlling the main conversion circuit to the main conversion circuit.