[0001] The invention belongs to the field of environmental protection recycling, and specifically relates to a method for recycling rare metals in waste vanadium-titanium denitration catalysts. Background Art
[0002] In recent years, with the rapid development of industrialization, large-scale emission of nitrogen oxides has caused many air pollution problems such as acid rain, photochemical smog, and haze. Selective oxidation-reduction technology (SCR) has been widely used in the field of denitrification. At present, about 140,000 tons of SCR denitrification catalysts are discarded every year, which can be converted into a volume of up to 250,000 cubic meters. The rational use of discarded denitrification catalysts is a technical problem faced by technicians in the field. Since vanadium-titanium denitrification catalysts contain many rare metal elements such as vanadium, titanium, and tungsten, how to efficiently recycle the rare metal elements in discarded denitrification catalysts has become a hot technical topic; Patent application number 201610156000X discloses a method for comprehensive recovery of valuable metals tungsten, vanadium and titanium in waste vanadium-tungsten-titanium denitration catalysts. This method can effectively recover valuable metals tungsten, titanium and the like in waste catalysts through sodium roasting, water leaching reaction, de-impurity treatment, calcium salt precipitation and acid leaching reaction. It is not only beneficial to reduce environmental pollution and realize the recycling of resources, but also to obtain considerable economic benefits by recovering valuable metals. However, the recovery efficiency of this method still needs to be improved. In view of the above shortcomings, a method for recovering rare metals from waste vanadium-titanium denitration catalysts is now needed, which can efficiently recover and utilize the rare metals in waste vanadium-titanium denitration catalysts. Summary of the invention
[0003] The purpose of the present invention is to provide a method for recovering rare metals from waste vanadium-titanium denitrification catalysts. The present invention solves the problems of low sodium sintering recovery efficiency and raw material adhesion during roasting by reasonably controlling the raw material ratio and various temperature process parameters; and the process is reasonably designed to achieve efficient separation of compounds containing rare metals, reduce the cost of recovery, and have good market application prospects.
[0004] The present invention provides the following technical solutions: A method for recovering rare metals from waste vanadium-titanium denitration catalysts, comprising the following steps: S1, mixing 10 to 20 parts by mass of waste vanadium titanium denitration catalyst, 10 to 20 parts by mass of sodium carbonate, and 5 to 10 parts by mass of sodium chloride to obtain a mixture; S2, crushing the mixture into 800-1000 meshes by a ball mill, and calcining at 700-800° C. for 3-4 hours to obtain a sintered product; S3, adding 100 to 200 parts by weight of water at a temperature of 75 to 80° C. to the sintered product, stirring for 1 to 2 hours, and filtering to obtain a titanium-containing solid and a filtrate 1; S4, adding 3-4 mol / L sulfuric acid to the titanium-containing solid, controlling the temperature at 60-90°C, reacting for 2-3 hours, adjusting the pH to 8-9, adding ammonium sulfate, stirring for 1-2 hours, filtering and drying to obtain titanium dioxide; S5, adjusting the pH value of filtrate 1 to 8.0-9.0, adding ammonium chloride to react for 1-2 hours to generate a precipitate, and filtering to obtain filtrate 2 and precipitate respectively; S6, calcining the precipitate at 500-600° C. for 20-40 min to obtain vanadium pentoxide; S7. Add hydrochloric acid to the filtrate 2 to adjust the pH value to 4.5-5.0, add calcium chloride to form a precipitate, wash the precipitate with hydrochloric acid for 20-40 minutes, and calcine at 300-400°C for 30-50 minutes to obtain tungsten trioxide and molybdenum trioxide.
[0005] Preferably, 14 parts by mass of waste vanadium titanium denitration catalyst, 14 parts by mass of sodium carbonate and 7 parts by mass of sodium chloride are mixed to obtain a mixture; Preferably, the mixture is crushed into 900 meshes by a ball mill, and calcined at 750° C. for 3.5 h to obtain a sintered product; Preferably, 150 parts by weight of water at a temperature of 78° C. is added to the sintered product, and then stirred for 1.5 hours, and filtered to obtain a titanium-containing solid and a filtrate 1; Preferably, the titanium-containing solid is added with 3.5 mol / L sulfuric acid, the temperature is controlled at 75° C., the reaction is carried out for 2.5 hours, the pH is adjusted to 8.5, ammonium sulfate is added, the mixture is stirred for 1.5 hours, and titanium dioxide is obtained after filtration and drying; Preferably, the pH value of filtrate 1 is adjusted to 8.5, and ammonium chloride is added to react for 1.5 hours to generate a precipitate, which is filtered to obtain filtrate 2 and the precipitate respectively; Preferably, the precipitate is calcined at 550° C. for 30 min to obtain vanadium pentoxide; Preferably, hydrochloric acid is added to the filtrate 2 to adjust the pH value to 4.8, calcium chloride is added to generate a precipitate, the precipitate is washed with hydrochloric acid for 30 minutes, and calcined at 350° C. for 40 minutes to obtain tungsten trioxide and molybdenum trioxide.
[0006] Beneficial effects of the present invention: The present invention solves the problems of low recovery efficiency of sodium sintering and raw material adhesion during calcination by reasonably controlling the raw material ratio and various temperature process parameters. The process of the present invention is reasonable, and can achieve efficient separation of compounds containing rare metals, reduce the cost of recovery, and has good market application prospects. DETAILED DESCRIPTION Example 1
[0007] A method for recovering rare metals from waste vanadium-titanium denitration catalysts, comprising the following steps: mixing 100 g of waste vanadium-titanium denitration catalysts with 100 g of sodium carbonate and 50 g of sodium chloride to obtain a mixture; crushing the mixture into 800 meshes using a ball mill, and calcining at 700° C. for 3 h to obtain a sintered product; adding 1000 g of water at a temperature of 75° C. to the sintered product, stirring for 1 h, and filtering to obtain a titanium-containing solid and a filtrate 1; adding 3 mol / L sulfuric acid to the titanium-containing solid, controlling the temperature at 60° C., reacting for 2 h, adjusting the pH to 8, adding ammonium sulfate, and stirring for 3 h. 1h, filtered and dried to obtain 7.8g of titanium dioxide (HPLC: 96%); the pH value of filtrate 1 was adjusted to 8.0, ammonium chloride was added to react for 1h to generate a precipitate, and the filtrate 2 and the precipitate were obtained by filtration; the precipitate was calcined at 500°C for 20min to obtain 23.6g of vanadium pentoxide (HPLC: 96%); hydrochloric acid was added to filtrate 2 to adjust the pH value to 4.5, calcium chloride was added to generate a precipitate, the precipitate was washed with hydrochloric acid for 20min, and calcined at 300°C for 30min to obtain tungsten trioxide and molybdenum trioxide 19.3g (HPLC: 94%). Example 2
[0008] A method for recovering rare metals from waste vanadium-titanium denitration catalysts, comprising the following steps: mixing 120 g of waste vanadium-titanium denitration catalysts, 120 g of sodium carbonate and 60 g of sodium chloride to obtain a mixture; crushing the mixture into 850 meshes using a ball mill, and calcining at 720° C. for 3.2 h to obtain a sintered product; adding 1200 g of water at a temperature of 77° C. to the sintered product, stirring for 1.2 h, and filtering to obtain a titanium-containing solid and a filtrate 1; adding 3.2 mol / L sulfuric acid to the titanium-containing solid, controlling the temperature at 70° C., reacting for 2.2 h, adjusting the pH to 8.2, adding ammonium sulfate, After stirring for 1.2 hours, filtration and drying, 10.3 g of titanium dioxide (HPLC: 96%) was obtained; the pH value of filtrate 1 was adjusted to 8.3, and ammonium chloride was added to react for 1.3 hours to generate a precipitate, which was filtered to obtain filtrate 2 and the precipitate respectively; the precipitate was calcined at 530°C for 25 minutes to obtain 33.6 g of vanadium pentoxide (HPLC: 95%); hydrochloric acid was added to filtrate 2 to adjust the pH value to 4.6, calcium chloride was added to generate a precipitate, the precipitate was rinsed with hydrochloric acid for 25 minutes, and calcined at 330°C for 35 minutes to obtain 22.6 g of tungsten trioxide and molybdenum trioxide (HPLC: 94%). Example 3
[0009] A method for recovering rare metals from waste vanadium-titanium denitration catalysts, comprising the following steps: mixing 140 g of waste vanadium-titanium denitration catalysts, 140 g of sodium carbonate and 70 g of sodium chloride to obtain a mixture; crushing the mixture into 900 meshes using a ball mill, and calcining at 750° C. for 3.5 h to obtain a sintered product; adding 1500 g of water at a temperature of 78° C. to the sintered product, stirring for 1.5 h, and filtering to obtain a titanium-containing solid and a filtrate 1; adding 3.5 mol / L sulfuric acid to the titanium-containing solid, controlling the temperature at 75° C., reacting for 2.5 h, adjusting the pH to 8.5, adding ammonium sulfate, After stirring for 1.5 hours, filtration and drying, 15.1 g of titanium dioxide (HPLC: 97%) was obtained; the pH value of filtrate 1 was adjusted to 8.5, and ammonium chloride was added to react for 1.5 hours to generate a precipitate, which was filtered to obtain filtrate 2 and the precipitate respectively; the precipitate was calcined at 550°C for 30 minutes to obtain 45.3 g of vanadium pentoxide (HPLC: 96%); hydrochloric acid was added to filtrate 2 to adjust the pH value to 4.8, calcium chloride was added to generate a precipitate, the precipitate was washed with hydrochloric acid for 30 minutes, and calcined at 350°C for 40 minutes to obtain 29.7 g of tungsten trioxide and molybdenum trioxide (HPLC: 95%). Example 4
[0010] A method for recovering rare metals from waste vanadium-titanium denitration catalysts comprises the following steps: mixing 180 g of waste vanadium-titanium denitration catalysts, 180 g of sodium carbonate and 80 g of sodium chloride to obtain a mixture; crushing the mixture into 950 meshes using a ball mill, and calcining at 780° C. for 3.7 h to obtain a sintered product; adding 1800 g of water at a temperature of 78° C. to the sintered product, stirring for 1.8 h, and filtering to obtain a titanium-containing solid and a filtrate 1; adding 3.7 mol / L sulfuric acid to the titanium-containing solid, controlling the temperature at 80° C., reacting for 2.8 h, adjusting the pH to 8.7, and adding ammonium sulfate; After stirring for 1.8 hours, filtration and drying, 15.1 g of titanium dioxide (HPLC: 94%) was obtained; the pH value of filtrate 1 was adjusted to 8.7, and ammonium chloride was added to react for 1.8 hours to generate a precipitate, which was filtered to obtain filtrate 2 and the precipitate respectively; the precipitate was calcined at 580°C for 35 minutes to obtain 41.3 g of vanadium pentoxide (HPLC: 95%); hydrochloric acid was added to filtrate 2 to adjust the pH value to 4.8, calcium chloride was added to generate a precipitate, the precipitate was washed with hydrochloric acid for 37 minutes, and calcined at 380°C for 46 minutes to obtain 29.6 g of tungsten trioxide and molybdenum trioxide (HPLC: 94%). Example 5
[0011] A method for recovering rare metals from waste vanadium-titanium denitration catalysts, comprising the following steps: mixing 200 g of waste vanadium-titanium denitration catalysts, 200 g of sodium carbonate and 100 g of sodium chloride to obtain a mixture; crushing the mixture into 1000 meshes using a ball mill, and calcining at 800° C. for 4 h to obtain a sintered product; adding 2000 g of water at 80° C. to the sintered product, stirring for 2 h, and filtering to obtain a titanium-containing solid and a filtrate 1; adding 4 mol / L sulfuric acid to the titanium-containing solid, controlling the temperature at 90° C., reacting for 3 h, adjusting the pH to 9, adding ammonium sulfate, and stirring for 2 h. 2h, filtered and dried to obtain 19.3g of titanium dioxide (HPLC: 96%); the pH value of filtrate 1 was adjusted to 9.0, ammonium chloride was added to react for 2h to generate a precipitate, and the filtrate 2 and the precipitate were obtained by filtration; the precipitate was calcined at 600℃ for 40min to obtain 57.1g of vanadium pentoxide (HPLC: 96%); hydrochloric acid was added to filtrate 2 to adjust the pH value to 5.0, calcium chloride was added to generate a precipitate, the precipitate was washed with hydrochloric acid for 40min, and calcined at 400℃ for 50min to obtain 40.1g of tungsten trioxide and molybdenum trioxide (HPLC: 95%).
[0012] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for recovering rare metals from waste vanadium-titanium denitration catalysts, characterized in that: Here are the steps: S1, mixing 10 to 20 parts by mass of waste vanadium titanium denitration catalyst, 10 to 20 parts by mass of sodium carbonate, and 5 to 10 parts by mass of sodium chloride to obtain a mixture; S2, crushing the mixture into 800-1000 meshes by a ball mill, and calcining at 700-800° C. for 3-4 hours to obtain a sintered product; S3, adding 100 to 200 parts by weight of water at a temperature of 75 to 80° C. to the sintered product, stirring for 1 to 2 hours, and filtering to obtain a titanium-containing solid and a filtrate 1; S4, adding 3-4 mol / L sulfuric acid to the titanium-containing solid, controlling the temperature at 60-90°C, reacting for 2-3 hours, adjusting the pH to 8-9, adding ammonium sulfate, stirring for 1-2 hours, filtering and drying to obtain titanium dioxide; S5, adjusting the pH value of filtrate 1 to 8.0-9.0, adding ammonium chloride to react for 1-2 hours to generate a precipitate, and filtering to obtain filtrate 2 and precipitate respectively; S6, calcining the precipitate at 500-600° C. for 20-40 min to obtain vanadium pentoxide; S7. Add hydrochloric acid to the filtrate 2 to adjust the pH value to 4.5-5.0, add calcium chloride to form a precipitate, wash the precipitate with hydrochloric acid for 20-40 minutes, and calcine at 300-400°C for 30-50 minutes to obtain tungsten trioxide and molybdenum trioxide.
2. The method for recovering rare metals from waste vanadium-titanium denitration catalyst according to claim 1, characterized in that: In step S1, 14 parts by mass of the waste vanadium titanium denitration catalyst, 14 parts by mass of sodium carbonate and 7 parts by mass of sodium chloride are mixed to obtain a mixture.
3. The method for recovering rare metals from waste vanadium-titanium denitration catalyst according to claim 1, characterized in that: In step S2, the mixture is crushed into 900 meshes by a ball mill and calcined at 750° C. for 3.5 h to obtain a sintered product.
4. The method for recovering rare metals from waste vanadium-titanium denitration catalyst according to claim 1, characterized in that: In step S3, 150 parts by mass of water at a temperature of 78° C. is added to the sintered product, which is then stirred for 1.5 hours and filtered to obtain a titanium-containing solid and a filtrate 1.
5. The method for recovering rare metals from waste vanadium-titanium denitration catalyst according to claim 1, characterized in that: In step S4, 3.5 mol / L sulfuric acid is added to the titanium-containing solid, the temperature is controlled at 75° C., the reaction is carried out for 2.5 hours, the pH is adjusted to 8.5, ammonium sulfate is added, stirred for 1.5 hours, and titanium dioxide is obtained after filtration and drying.
6. The method for recovering rare metals from waste vanadium-titanium denitration catalyst according to claim 1, characterized in that: In step S5, the pH value of the filtrate 1 is adjusted to 8.5, and ammonium chloride is added to react for 1.5 hours to generate a precipitate, which is filtered to obtain the filtrate 2 and the precipitate, respectively.
7. The method for recovering rare metals from waste vanadium-titanium denitration catalyst according to claim 1, characterized in that: In step S6, the precipitate is calcined at 550° C. for 30 min to obtain vanadium pentoxide.
8. The method for recovering rare metals from waste vanadium-titanium denitration catalyst according to claim 1, characterized in that: In step S7, hydrochloric acid is added to the filtrate 2 to adjust the pH value to 4.8, calcium chloride is added to generate a precipitate, the precipitate is washed with hydrochloric acid for 30 minutes, and calcined at 350° C. for 40 minutes to obtain tungsten trioxide and molybdenum trioxide.