Ultra-white PVC background cloth and preparation method thereof
By applying a waterproof and whitening flame retardant layer on the PVC background cloth, the problems of insufficient color and poor wear resistance in the prior art are solved, higher brightness feedback and better wear resistance are achieved, and photography quality is improved and service life.
Patent Information
- Application Number
- CN202411144173.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-08
AI Technical Summary
The existing PVC background cloth is not white enough, resulting in insufficient brightness and affecting the quality of photography. At the same time, its waterproof, flame retardant and wear resistance are poor, which cannot meet the requirements of long-term use.
Use waterproof whitening flame retardant layer, including polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent and fluorescent whitening agent, and use spraying and drying steps to the background cloth main body. The layer is coated sideways to enhance its waterproof, flame retardant and wear resistance, and to enhance color with a fluorescent whitening agent.
It significantly improves the brightness feedback of the background cloth, improves the quality of the photography works, and enhances waterproof, flame retardant and wear resistance to meet the requirements of long-term use.
Smart Images

Figure CN118910899A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a PVC background cloth, in particular to an ultra-white PVC background cloth and a preparation method thereof, belonging to the technical field of background cloth preparation. Background Art
[0002] Background cloth is an essential material for indoor photography. There are monochrome background cloths and subject-based background cloths. Different venues require different background cloths. The material of the background cloth should match the size, environment, light and other factors of the venue, so that the shooting effect can be better.
[0003] Currently, background cloths are often made of PVC materials, which make them stronger and more durable, and can inhibit bacteria and prevent damage. However, the color of commonly used PVC background cloths is not white enough, resulting in insufficient brightness of the background cloth during shooting, which will directly affect the quality of photography, causing the photographic works to be insufficiently bright and clear. In addition, the waterproof, flame retardant and wear resistance of PVC background cloths are also poor, and cannot meet the requirements of long-term photography use. Summary of the invention
[0004] In view of the shortcomings of the prior art, the present invention provides an ultra-white PVC background cloth, and also provides a preparation method of the ultra-white PVC background cloth.
[0005] The technical solution adopted by the present invention to solve the above technical problems is: An ultra-white PVC background cloth, comprising a background cloth body, the surface of which is coated with a waterproof, whitening and flame-retardant layer, wherein the waterproof, whitening and flame-retardant layer comprises the following components by weight: 40-70 parts of polyvinyl chloride resin, 4-6 parts of ultraviolet absorber, 5-8 parts of coupling agent, 5-7 parts of plasticizer, 20-40 parts of phytic acid, 5-10 parts of wear-resistant agent, 4-7 parts of fluorescent brightener and 60-80 parts of water; The coupling agent is one of a silane coupling agent, a titanate coupling agent, and an aluminate coupling agent; the plasticizer is one of a phthalate plasticizer, a phosphate plasticizer, and a polyethylene oxide plasticizer.
[0006] Furthermore, the weight proportions of the components are as follows: 50-60 parts of polyvinyl chloride resin, 5-6 parts of ultraviolet absorber, 6-7 parts of coupling agent, 5-6 parts of plasticizer, 25-35 parts of phytic acid, 6-9 parts of anti-wear agent, 5-6 parts of fluorescent brightener and 70-80 parts of water.
[0007] Furthermore, the mass ratio of the fluorescent whitening agent to the polyvinyl chloride resin is 0.01-0.05:1, that is, 0.01-0.05 parts by mass of the fluorescent whitening agent is mixed with 1 part by mass of the polyvinyl chloride resin.
[0008] Furthermore, the mass ratio of the coupling agent to the plasticizer is 5-1.5.
[0009] A method for preparing an ultra-white PVC background cloth comprises the following steps: S1. Weigh polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent brightener and water by weight, put them into a mixing device and stir and mix them to obtain a waterproof, whitening and flame-retardant layer; S2, loading the obtained waterproof whitening flame retardant layer into a spraying device, and then using the spraying device to spray the waterproof whitening flame retardant layer onto both sides of the background cloth body; S3, placing the background cloth body after spraying in a drying device for drying; S4, hanging the dried background cloth body on an ironing device, ironing it to remove wrinkles and soften it, and then drying and rolling it up after ironing.
[0010] Furthermore, in the step S1, the mixing temperature is 50-150° C., and the mixing time is 30-60 min.
[0011] Furthermore, in the step S2, the spraying thickness of the waterproof, whitening and flame-retardant layer is 0.3-0.5 mm.
[0012] Furthermore, in the step S3, the temperature of the drying equipment is 60-80° C., and the drying time is controlled within 2 hours.
[0013] Furthermore, in the step S4, the temperature of the ironing device is 50-70° C. and the time is 5-10 minutes.
[0014] Furthermore, the spraying device is also equipped with an electric heater.
[0015] Compared with the prior art, the present invention has the following beneficial effects: The present application sets a waterproof, whitening and flame-retardant layer, and coats the waterproof, whitening and flame-retardant layer on both sides of the background cloth body. Since the waterproof, whitening and flame-retardant layer is made of a mixture of polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent brightener and water, the waterproof, whitening and flame-retardant layer has the characteristics of waterproof, flame retardant and wear resistance. At the same time, the addition of fluorescent brightener can also enhance the white color of the background cloth body, so that it can provide high brightness feedback during shooting, thereby improving the quality of photographic works.
[0016] The fluorescent whitening agent and polyvinyl chloride resin are mixed in a ratio of 0.01-0.05:1 as the optimal usage amount, so that the fluorescent whitening agent has the best whitening degree and avoids darkening and yellowing; and the ratio of coupling agent and plasticizer can make the two better mixed and avoid mutual influence. After the mixing temperature and time in S1 are specified, it is at the optimal use temperature and time of the fluorescent whitening agent to avoid affecting its whitening effect. The drying temperature in S3 is controlled at 60~80℃, and the set temperature is in line with the temperature range of PVC material to avoid thermal degradation caused by excessive temperature. The ironing temperature in S4 is also set to avoid damage to the background cloth body 1, and an electric heater is equipped on the spraying device to continuously heat the mixed solution in S1, so that the solution can always maintain a constant temperature during the spraying process to avoid its cooling and solidification affecting the coating. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic diagram of the preparation steps of the present invention; Figure 2 It is a schematic diagram of the structure of the background cloth main body and the waterproof, whitening and flame-retardant layer of the present invention.
[0018] In the figure, 1. Background cloth body; 2. Waterproof, whitening and flame retardant layer. DETAILED DESCRIPTION
[0019] The technical solution of the present invention will be clearly and completely described below in conjunction with the accompanying drawings and specific embodiments.
[0020] like Figure 2 An ultra-white PVC background cloth is shown, which includes a background cloth body 1, the surface of the background cloth body 1 is coated with a waterproof whitening flame retardant layer 2, and the waterproof whitening flame retardant layer 2 includes the following components by weight: 40-70 parts of polyvinyl chloride resin, 4-6 parts of ultraviolet absorber, 5-8 parts of coupling agent, 5-7 parts of plasticizer, 20-40 parts of phytic acid, 5-10 parts of wear resistance agent, 4-7 parts of fluorescent whitening agent and 60-80 parts of water; The coupling agent is one of silane coupling agent, titanate coupling agent, and aluminate coupling agent; the plasticizer is one of phthalate plasticizer, phosphate plasticizer, and polyethylene oxide plasticizer. Through the provision of the waterproof whitening flame retardant layer 2, the waterproof whitening flame retardant layer 2 is coated on both sides of the background cloth body 1. Since the waterproof whitening flame retardant layer 2 is made of polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent whitening agent and water, the waterproof whitening flame retardant layer 2 has the characteristics of waterproof, flame retardant and wear resistance; at the same time, the addition of fluorescent whitening agent can also improve the white color of the background cloth body 1, so that it can provide high brightness during shooting, improving the quality of the shooting works.
[0021] In this embodiment, the weight proportions of the components are as follows: 50 parts of polyvinyl chloride resin, 5 parts of ultraviolet absorber, 6 parts of coupling agent, 5 parts of plasticizer, 25 parts of phytic acid, 6 parts of wear resistance agent, 5 parts of fluorescent brightener and 70 parts of water, the mass ratio of fluorescent brightener to polyvinyl chloride resin is 0.02:1, and the mass ratio of coupling agent to plasticizer is 5-1.5; Figure 1 As shown, the preparation method thereof comprises the following steps: S1, weighing polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent brightener and water in parts by weight, putting them into a mixing device and stirring and mixing, so as to obtain a waterproof, whitening and flame-retardant layer 2; S2, loading the obtained waterproof whitening flame retardant layer 2 into a spraying device, and then using the spraying device to spray the waterproof whitening flame retardant layer 2 onto both sides of the background cloth body 1; S3, placing the background cloth body 1 after spraying in a drying device for drying; S4, hanging the dried background cloth body 1 on an ironing device, ironing it to remove wrinkles and soften it, and then drying and rolling it up after ironing.
[0022] In this embodiment, the weight proportions of the components are as follows: 60 parts of polyvinyl chloride resin, 6 parts of ultraviolet absorber, 7 parts of coupling agent, 6 parts of plasticizer, 30 parts of phytic acid, 7 parts of wear-resistant agent, 6 parts of fluorescent brightener and 80 parts of water, the mass ratio of fluorescent brightener to polyvinyl chloride resin is 0.03:1, and the mass ratio of coupling agent to plasticizer is 5-1.5; the preparation method comprises the following steps: S1, weighing polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent brightener and water in parts by weight, putting them into a mixing device and stirring and mixing, so as to obtain a waterproof, whitening and flame-retardant layer 2; S2, loading the obtained waterproof whitening flame retardant layer 2 into a spraying device, and then using the spraying device to spray the waterproof whitening flame retardant layer 2 onto both sides of the background cloth body 1; S3, placing the background cloth body 1 after spraying in a drying device for drying; S4, hanging the dried background cloth body 1 on an ironing device, ironing it to remove wrinkles and soften it, and then drying and rolling it up after ironing.
[0023] In this embodiment, the fluorescent whitening agent and the polyvinyl chloride resin are mixed in a ratio of 0.01-0.05:1 as the optimal usage amount, so that the whitening degree of the fluorescent whitening agent is the best and darkening and yellowing are avoided. The ratio of the coupling agent and the plasticizer can make the two better mixed and avoid mutual influence.
[0024] In this embodiment, in step S1, the mixing temperature is 50-150°C, and the mixing time is 30-60 minutes. In step S2, the spraying thickness of the waterproof whitening flame retardant layer 2 is 0.3-0.5 mm. In step S3, the temperature of the drying equipment is 60-80°C, and the drying time is controlled within 2 hours. In step S4, the temperature of the ironing equipment is 50-70°C, and the time is 5-10 minutes. The spraying device is also equipped with an electric heater. After the mixing temperature and time in S1 are specified, it is at the optimal use temperature and time of the fluorescent whitening agent to avoid affecting its whitening effect. The drying temperature in S3 is controlled at 60-80°C, and the set temperature is in line with the temperature range of the PVC material to avoid thermal degradation caused by excessive temperature. The setting of the ironing temperature in S4 is also to avoid damage to the background cloth body 1, and the electric heater is equipped on the spraying device, which can continuously heat the mixed solution in S1, so that the solution can always maintain a constant temperature during the spraying process to avoid its cooling and solidification affecting the coating.
[0025] In this embodiment, if Figure 1-Figure 2 As shown, the working process of an ultra-white PVC background cloth and a preparation method thereof provided in this embodiment is as follows: Step 1: Weigh polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent brightener and water by weight, put them into a mixing device, stir and mix, heat the temperature of the mixing device to 150° C., set the mixing time to 60 minutes, and completely mix the polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent brightener and water to obtain a waterproof, whitening and flame-retardant layer 2; Step 2: Fill the mixed solution into a spraying device, start the electric heater on the spraying device, use the electric heater to heat the solution in the spraying device to keep it at a constant temperature, and then use the spraying device to evenly spray the waterproof whitening and flame retardant layer 2 onto both sides of the background cloth body 1; Step 3: Place the background cloth body 1 after spraying in a drying device, set the temperature of the drying device to 80° C., control the drying time to within 2 hours, and start the drying device to dry the waterproof whitening and flame retardant layer 2 on the background cloth body 1 to solidify it; Step 4: After drying, take out the background cloth body 1 from the device, and then hang the background cloth body 1 on the ironing device, set the temperature of the ironing device to 70°C, and iron the background cloth body 1 for 10 minutes to remove wrinkles and soften the background cloth body 1. After ironing, let the background cloth body 1 dry naturally, and finally roll it up and store it with a winding roller.
[0026] In summary, in this embodiment, according to an ultra-white PVC background cloth and a preparation method thereof of this embodiment, the waterproof whitening flame retardant layer 2 is provided, and the waterproof whitening flame retardant layer 2 is coated on both sides of the background cloth body 1. Since the waterproof whitening flame retardant layer 2 is made by mixing polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent whitening agent and water, the waterproof whitening flame retardant layer 2 has the characteristics of waterproof, flame retardant and wear resistance. At the same time, the addition of fluorescent whitening agent can also improve the white color of the background cloth body 1, so that it can provide high brightness feedback during shooting, thereby improving the quality of the photos taken; the fluorescent whitening agent and polyvinyl chloride resin are mixed in a ratio of 0.01-0.05:1 as the best usage amount, The whitening degree of the fluorescent whitening agent is optimized to avoid darkening and yellowing, while the ratio of the coupling agent and the plasticizer can make the two better mixed to avoid mutual influence; after the mixing temperature and time in S1 are specified, the fluorescent whitening agent is at the best use temperature and time to avoid affecting its whitening effect, the drying temperature in S3 is controlled at 60~80℃, and the set temperature is in line with the temperature range of the PVC material to avoid thermal degradation caused by excessive temperature, and the ironing temperature in S4 is also set to avoid damage to the background cloth body 1, and an electric heater is equipped on the spraying device to continuously heat the mixed solution in S1, so that the solution can always maintain a constant temperature during the spraying process to avoid its cooling and solidification affecting the coating.
[0027] The above description shows and describes the preferred embodiments of the present invention. It should be understood that the present invention is not limited to the forms disclosed herein, and that changes and modifications made by those skilled in the art without departing from the spirit and scope of the present invention should be within the scope of protection of the claims attached to the present invention.
Claims
1. An ultra-white PVC background cloth, comprising a background cloth body (1), characterized in that: The surface of the background cloth body (1) is coated with a waterproof, whitening and flame-retardant layer (2), and the waterproof, whitening and flame-retardant layer (2) comprises the following components by weight: 40-70 parts of polyvinyl chloride resin, 4-6 parts of ultraviolet absorber, 5-8 parts of coupling agent, 5-7 parts of plasticizer, 20-40 parts of phytic acid, 5-10 parts of wear-resistant agent, 4-7 parts of fluorescent brightener and 60-80 parts of water; The coupling agent is one of a silane coupling agent, a titanate coupling agent, and an aluminate coupling agent; the plasticizer is one of a phthalate plasticizer, a phosphate plasticizer, and a polyethylene oxide plasticizer.
2. The ultra-white PVC background cloth according to claim 1, characterized in that: The weight proportions of the components are as follows: 50-60 parts of polyvinyl chloride resin, 5-6 parts of ultraviolet absorber, 6-7 parts of coupling agent, 5-6 parts of plasticizer, 25-35 parts of phytic acid, 6-9 parts of anti-wear agent, 5-6 parts of fluorescent brightener and 70-80 parts of water.
3. The ultra-white PVC background cloth according to claim 1, characterized in that: The mass ratio of the fluorescent brightener to the polyvinyl chloride resin is 0.01-0.05:
1.
4. The ultra-white PVC background cloth according to claim 1, characterized in that: The mass ratio of the coupling agent to the plasticizer is 5-1.
5.
5. The method for preparing the ultra-white PVC background cloth according to any one of claims 1 to 4, characterized in that: The following steps are involved: S1, weighing polyvinyl chloride resin, ultraviolet absorber, coupling agent, plasticizer, phytic acid, wear-resistant agent, fluorescent brightener and water according to weight, putting them into a mixing device and stirring and mixing, so as to obtain a waterproof, whitening and flame-retardant layer (2); S2, loading the obtained waterproof whitening flame retardant layer (2) into a spraying device, and then using the spraying device to spray the waterproof whitening flame retardant layer (2) onto both sides of the background cloth body (1); S3, placing the background cloth body (1) after spraying in a drying device for drying; S4, hanging the dried background cloth body (1) on an ironing device, ironing it to remove wrinkles and soften it, and then drying and rolling it up after ironing.
6. The method for preparing the ultra-white PVC background cloth according to claim 5, characterized in that: In the step S1, the mixing temperature is 50-150° C., and the mixing time is 30-60 min.
7. The method for preparing the ultra-white PVC background cloth according to claim 5, characterized in that: In the step S2, the spraying thickness of the waterproof, whitening and flame-retardant layer (2) is 0.3-0.5 mm.
8. The method for preparing the ultra-white PVC background cloth according to claim 5, characterized in that: In the step S3, the temperature of the drying equipment is 60-80° C., and the drying time is controlled within 2 hours.
9. The method for preparing the ultra-white PVC background cloth according to claim 5, characterized in that: In the step S4, the temperature of the ironing device is 50-70° C. and the time is 5-10 minutes.
10. The method for preparing the ultra-white PVC background cloth according to claim 5, characterized in that: The spraying device is also equipped with an electric heater.