Chip packaging body underfill anti-overflow control method and chip packaging method

By using laser height measurement and UV-cured adhesive to form a barrier wall in 2.5D chip packaging, the problem of passive component contamination caused by underfill overflow is solved, achieving efficient overflow control, improving chip packaging reliability and saving costs.

CN118919434APending Publication Date: 2024-11-08TONGFU CHAOWEI (SUZHOU) MICROELECTRONICS CO LTD
View PDF 0 Cites 4 Cited by

Patent Information

Application Number
CN202410989822.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In 2.5D chip packaging, the bottom filler is prone to overflow, causing contamination of passive components. Existing methods are inefficient, prone to secondary contamination, and require a lot of manpower and resources, and cannot effectively solve the problems of poor appearance and short circuits.

Method used

Laser height measurement is used to determine the dispensing height, forming a UV-curable adhesive barrier wall between the chip and the passive component. UV irradiation allows the adhesive to cure quickly, forming a barrier wall to prevent underfill from overflowing. The dispensing height and position are adjusted according to the degree of warpage.

Benefits of technology

It effectively prevents bottom filler from overflowing and contaminating passive components, improves reliability, saves manpower and resources, avoids customer complaints caused by incomplete wiping, and has a wide range of applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919434A_ABST
    Figure CN118919434A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides a chip packaging body underfill anti-overflow control method and a chip packaging method, and the control method comprises the steps: providing a chip packaging body which comprises a substrate, a chip which is inversely disposed on the substrate, and a passive element which is disposed on the substrate and is located at the outer side of the chip; determining the dispensing height at a preset position on the surface of the substrate between the chip and the passive element by adopting a laser height measurement mode; dispensing at a preset position according to the dispensing height to form an ultraviolet curing adhesive surrounding the outer side of the chip; performing ultraviolet irradiation on the ultraviolet curing adhesive to quickly cure the ultraviolet curing adhesive to form a blocking adhesive wall; when the underfill is filled between the chip and the substrate, the blocking glue wall can prevent the underfill from overflowing to the passive element. The problem that passive components are dirty due to overflow of underfill can be solved, reliability of the passive components is guaranteed, time and labor are saved, and cost is saved. And the blocking glue wall can control overflow of the underfill glue for the passive element in a targeted manner, and the application range is wide.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The disclosed embodiments belong to the field of semiconductor packaging technology, and specifically relate to a chip package bottom fill glue overflow prevention control method and a chip packaging method. Background Art

[0002] The design layout of 2.5D chip packaging products is becoming more and more compact, and the distance between the chip and passive components is becoming narrower and narrower. As a result, the flow of the bottom fill glue during the bottom filling process of 2.5D products can easily cause the glue of the passive components to become dirty, resulting in poor product appearance and short circuits of the passive components.

[0003] In order to solve the above problem, there is currently no effective method in the industry to solve this problem. The only way is to visually check the dirtiness of passive components before the bottom filling glue is cured and wipe it with a pointed cotton swab and a dust-free cloth to remove the glue. The problems currently encountered by this traditional method are:

[0004] 1) The traditional method of wiping with dust-free cloth is inefficient and ineffective;

[0005] 2) The traditional method of wiping the underfill glue with a dust-free cloth before it cures will cause the risk of secondary glue contamination;

[0006] 3) It requires a lot of manpower and material resources to solve;

[0007] 4) There is a risk of customer complaints due to improper wiping and abnormal escape.

[0008] In view of the above problems, it is necessary to propose a chip package bottom filler overflow prevention control method and a chip packaging method that are reasonably designed and effectively solve the above problems. Summary of the invention

[0009] The embodiments of the present disclosure aim to solve at least one of the technical problems existing in the prior art and provide a chip package bottom fill glue overflow prevention control method and a chip packaging method.

[0010] An aspect of an embodiment of the present disclosure provides a method for preventing overflow of underfill glue of a chip package, the control method comprising:

[0011] A chip package is provided; wherein the chip package comprises a substrate, a chip flipped on the substrate, and a passive component disposed on the substrate and located outside the chip;

[0012] At a preset position on the surface of the substrate between the chip and the passive component, a laser height measurement method is used to determine the glue dispensing height;

[0013] Dispensing glue at the preset position according to the dispensing height to form ultraviolet curing glue surrounding the outer side of the chip;

[0014] The UV curing glue is irradiated with UV rays to make it cure quickly to form a blocking glue wall; wherein, when the underfill glue is filled between the chip and the substrate, the blocking glue wall can prevent the underfill glue from overflowing to the passive component.

[0015] Optionally, the height of the blocking glue wall is greater than the thickness of the bottom filling glue.

[0016] Optionally, dispensing glue at the preset position according to the dispensing height includes:

[0017] Glue is dispensed at a distance of 0.5 mm to 1.5 mm from the edge of the chip according to preset glue dispensing parameters.

[0018] Optionally, performing dispensing according to preset dispensing parameters includes:

[0019] A nozzle with a dispensing size range of 15um to 25um is used for dispensing, and the dispensing weight range during the dispensing process is controlled to be 0.3mg to 0.8mg of curing glue per 10mm length.

[0020] Optionally, the step of irradiating the UV curing adhesive with UV rays to rapidly cure the UV curing adhesive comprises:

[0021] The intensity of the UV light used is in the range of 50mW / cm 2 ~100mW / cm 2 , the curing time is 5s to 8s.

[0022] Optionally, the step of determining the dispensing height by laser height measurement includes:

[0023] According to the warping degree of the substrate surface and the preset height of the blocking glue wall, the laser height is automatically measured on the surface of the substrate to determine the actual dispensing height of the ultraviolet curing glue.

[0024] Optionally, the automatic laser height measurement on the surface of the substrate to determine the actual dispensing height of the UV curing glue includes:

[0025] The actual dispensing height of the ultraviolet curing glue is automatically adjusted according to the warping degree at different positions of the substrate.

[0026] Optionally, after forming the ultraviolet curing glue surrounding the outer side of the chip, the method further includes:

[0027] The formed ultraviolet curing adhesive is inspected for appearance, and adhesive repair is performed if adhesive breakage is found.

[0028] Another aspect of the present disclosure provides a chip packaging method.

[0029] Packaging methods include:

[0030] Flipping the chip onto the substrate and mounting passive components on the outside of the chip;

[0031] A blocking glue wall is formed between the chip and the passive component;

[0032] An underfill is filled between the chip and the substrate to form an underfill layer, and the height of the blocking glue wall is greater than the height of the underfill layer; wherein,

[0033] The chip package underfill glue overflow prevention control method described above is used in the chip packaging process to prevent the underfill glue from overflowing to the passive component.

[0034] Optionally, filling an underfill between the chip and the substrate to form an underfill layer includes:

[0035] Filling the gap between the chip and the barrier glue wall with underfill glue, wherein the underfill glue flows to the gap between the chip and the substrate;

[0036] Performing an appearance inspection on the underfill, if the underfill does not overflow the blocking glue wall, curing the underfill to form the underfill layer.

[0037] The chip package bottom fill glue overflow prevention control method and chip packaging method of the disclosed embodiments can solve the problem of passive component dirtiness caused by the overflow of the bottom fill glue when the space between the chip and the passive component in the chip package is small. In addition, a blocking glue wall is formed between the chip and the passive component to block the overflow of the bottom fill glue. The height of the blocking glue wall can be set according to the height of the passive component, and the position and thickness of the blocking glue wall can also be set according to actual needs. The overflow of the bottom fill glue can be controlled in a targeted manner and has a wide range of applications. The control method can prevent the overflow of the bottom fill glue from contaminating the passive component, thereby ensuring the reliability of the passive component. There is no need to wipe the passive component, which saves time and effort and saves cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 This is a flow chart of a chip package bottom fill glue overflow prevention control method according to one embodiment of the present disclosure;

[0039] Figure 2 A schematic diagram of determining the actual dispensing height at the midpoint of a chip package according to another embodiment of the present disclosure;

[0040] Figure 3This is a schematic structural diagram of forming a blocking glue wall according to another embodiment of the present disclosure;

[0041] Figure 4 It is a schematic diagram of the anti-overflow effect of the underfill glue when there is or is not a blocking glue wall in the chip package of another embodiment of the disclosed embodiment;

[0042] Figure 5 A schematic diagram of a chip packaging method according to another embodiment of the present disclosure;

[0043] Figure 6 It is a structural schematic diagram of a chip packaging structure of another embodiment of the present disclosure. DETAILED DESCRIPTION

[0044] In order to enable those skilled in the art to better understand the technical solutions of the embodiments of the present disclosure, the embodiments of the present disclosure are further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0045] like Figure 1 As shown, the embodiment of the present disclosure provides a chip package underfill overflow prevention control method S100, the control method S100 comprising:

[0046] S110, providing a chip package; wherein the chip package includes a substrate, a chip flipped on the substrate, and a passive component disposed on the substrate and located outside the chip.

[0047] like Figure 2 As shown, a chip package is provided, wherein the chip package includes a substrate 110, a chip 120 and a passive component 130. The chip 120 is flip-chip mounted on the substrate 110 through solder balls 140, and the passive component 130 is disposed on the substrate 110 and is located outside the chip 120. The number and position of the passive components 130 are not specifically limited, and the passive components 130 can be distributed only on one side of the chip 120 or around the chip 120, which can be selected according to actual needs, and are not specifically limited in this embodiment.

[0048] S120, determining the dispensing height at a preset position on the surface of the substrate between the chip and the passive component by using a laser height measurement method.

[0049] Wherein, the method of determining the dispensing height by laser height measurement specifically includes:

[0050] According to the warping degree of the substrate 110 surface and the preset height of the blocking glue wall 150, the laser height is automatically measured on the surface of the substrate 110 to determine the actual dispensing height of the UV curing glue. According to the warping degree at different positions of the substrate 110, the actual dispensing height of the UV curing glue is automatically adjusted.

[0051] Specifically, Figure 2 As shown, considering the warpage of the substrate 110 surface and the small dispensing distance, in order to prevent dispensing abnormalities caused by the warpage of the substrate 110 surface during the dispensing process, it is necessary to perform automatic laser height measurement on the surface of the substrate 110 during dispensing ( Figure 2 The dots on the outside of the middle chip 120 on the substrate 110 are the initial positions A) of the curing glue measured by laser height. When dispensing glue, the dispensing program will automatically adjust the dispensing height according to the preset height of the blocking glue wall and the warping of different positions of the substrate 110 to obtain the actual dispensing height of the UV curing glue.

[0052] In the present embodiment, before the UV curing glue is formed at the preset position between the chip and the passive component, the actual dispensing height of the UV curing glue is obtained according to the warping degree of different positions of the substrate and the preset height of the blocking glue wall, and the influence of the warping of the substrate on the dispensing height is fully considered, so that the height of the blocking glue wall formed after dispensing reaches the preset height more accurately, and will not cause unevenness in the cured glue.

[0053] S130, dispensing glue at the preset position according to the dispensing height to form ultraviolet curing glue surrounding the outer side of the chip.

[0054] After determining the actual dispensing height of the blocking glue wall 150, step S130 is performed, that is, dispensing is performed at a preset position between the chip 120 and the passive component 130 according to the dispensing height to form an ultraviolet curing glue surrounding the outside of the chip 120. The specific implementation process of step S130 is as follows:

[0055] UV curing glue is dispensed at 0.5 mm to 1.5 mm from the edge of the chip 120 according to preset dispensing parameters to form UV curing glue surrounding the outside of the chip 120. The UV curing glue can prevent the underfill from overflowing to the passive component 130 and causing contamination of the passive component 130.

[0056] The dispensing is performed according to the dispensing parameters to form the ultraviolet curing glue surrounding the outer side of the chip 120, which may specifically include:

[0057] A nozzle with a dispensing size range of 15um to 25um is used for dispensing, and the dispensing weight range during the dispensing process is controlled to be 0.3mg to 0.8mg of curing glue per 10mm length, forming an ultraviolet curing glue surrounding the outside of the chip 120.

[0058] Specifically, Figure 3As shown, in this embodiment, a nozzle with a size of 20um is used for dispensing, and the dispensing weight during the dispensing process is controlled to be 0.5mg of UV curing glue per 10mm length. Dispensing is performed at a distance of 1mm from the edge of the chip 120, and the actual dispensing height range is 15um to 20um from the substrate, forming UV curing glue surrounding the outside of the chip 120.

[0059] It should be noted that in this embodiment, UV curing glue is used for dispensing. The UV curing glue has a short curing time, a simple curing process, and is relatively viscous, and will not contaminate passive components due to rapid flow. The curing glue may also be other types of glue as long as it can meet the requirements of this embodiment. The height of the curing glue can be selected according to the spacing between the chip and the substrate and the height of the passive components, and this embodiment does not make specific limitations.

[0060] In this embodiment, glue can be dispensed at a distance of 0.5 mm to 1.5 mm from the edge of the chip to form UV-curable glue surrounding the outside of the chip. When the interval between the chip and the passive component is small, the UV-curable glue formed by glue dispensing can prevent the bottom fill glue from overflowing into the passive component, thereby improving the reliability of the passive component.

[0061] Exemplarily, after forming the ultraviolet curing glue surrounding the outer side of the chip, the control method further includes:

[0062] The formed UV curing glue is inspected for appearance, and if there is any glue breakage, glue repair is performed. Specifically, after the glue is dispensed on the outer side of the chip 120, the UV curing glue is inspected for appearance to check whether there is any undesirable condition such as glue breakage. If there is, glue is re-dispensed at the corresponding position to repair the glue, so that the formed UV curing glue is connected end to end and surrounds the outer side of the chip 120, so as to prevent the bottom fill glue from overflowing.

[0063] S140, subjecting the UV curing glue to UV irradiation to make it cure quickly to form a blocking glue wall; wherein, when filling the underfill glue between the chip and the substrate, the blocking glue wall can prevent the underfill glue from overflowing to the passive component.

[0064] In this embodiment, the specific process of irradiating the UV curing adhesive with UV rays to rapidly cure the UV curing adhesive to form the blocking adhesive wall 150 is as follows:

[0065] The intensity range is 50mW / cm 2 ~100mW / cm 2 The UV curing glue is irradiated with ultraviolet rays for 5s to 8s, so that the UV curing glue after dispensing can be quickly cured.

[0066] After the UV curing glue is cured, a blocking glue wall 150 is formed around the outside of the chip 120. In this way, when the underfill glue is filled between the chip 120 and the substrate 110, the blocking glue wall 150 can effectively prevent the underfill glue from overflowing to the passive component 130, thereby preventing the passive component 130 from being contaminated by the underfill glue and improving the reliability of the passive component 130.

[0067] The height of the blocking glue wall 150 is greater than the thickness of the bottom filler filled between the chip 120 and the substrate 110. In other words, the height of the blocking glue wall 150 is higher than the height of the bottom filler layer 160, so that the blocking glue wall 150 can block the overflow of the bottom filler. The specific height of the blocking glue wall 150 can be specifically set according to the spacing between the substrate and the chip and the height of the passive component, and this embodiment does not make any specific restrictions.

[0068] In this embodiment, when curing the dispensed UV curing adhesive, the curing adhesive can be quickly cured only by UV irradiation, and the curing process is simple and the curing time is short, thus saving the time of the entire process.

[0069] like Figure 4 As shown in the figure, it is a schematic diagram of the anti-overflow effect of the underfill glue when there is or is not a blocking glue wall in the chip package in this embodiment. Among them, Leg1 is the glue overflow distance data without a blocking glue wall (in mm); Leg2 is the glue overflow distance data with a blocking glue wall (in mm); S1 / S2 / S3 / S4 represent the four edges of glue overflow. It can be seen from the figure that when the chip package is provided with a blocking glue wall, the problem of underfill glue overflow can be well controlled, thereby improving the reliability of passive components.

[0070] The chip package underfill glue overflow prevention control method of the disclosed embodiment can solve the problem of passive component dirtiness caused by underfill glue overflow when the space between the chip and the passive component in the chip package is small. In addition, a blocking glue wall is formed between the chip and the passive component to block the overflow of the underfill glue. The height of the blocking glue wall can be set according to the height of the passive component, and the position and thickness of the blocking glue wall can also be set according to actual needs. The overflow of the underfill glue can be controlled in a targeted manner and has a wide range of applications. The control method can prevent the overflow of the underfill glue from contaminating the passive component, thereby ensuring the reliability of the passive component. There is no need to wipe the passive component, which saves time, effort and cost.

[0071] like Figure 5 As shown, another aspect of the embodiment of the present disclosure provides a chip packaging method S200, the chip packaging method S200 comprising:

[0072] S210, flip the chip onto the substrate, and mount passive components on the outside of the chip.

[0073] like Figure 6 As shown, the chip 120 is flip-mounted on the substrate 110 via solder balls 140 , and the passive component 130 is mounted on the outer side of the chip 120 .

[0074] S220, forming a blocking glue wall between the chip and the passive component.

[0075] like Figure 6 As shown, by dispensing glue at a preset position between the chip 120 and the passive component 130, a blocking glue wall 150 is formed around the outside of the chip 120, so that when the underfill glue is filled between the chip 120 and the substrate 110, the blocking glue wall 150 can prevent the underfill glue from overflowing to the passive component 130. The formation process of the blocking glue wall 150 has been described in detail above and will not be repeated here.

[0076] S230, filling an underfill between the chip and the substrate to form an underfill layer, wherein the height of the blocking glue wall is greater than the height of the underfill layer; wherein, during the chip packaging process, the chip package underfill overflow prevention method described in the foregoing claims is adopted to prevent the underfill from overflowing to the passive component.

[0077] Specifically, the specific process of filling the underfill between the chip 120 and the substrate 110 to form the underfill layer 160 is as follows:

[0078] like Figure 3 and Figure 6 As shown, the underfill is filled between the chip 120 and the barrier glue wall 150 , and the underfill flows to between the chip 120 and the substrate 110 .

[0079] The underfill is inspected for appearance, and if the underfill does not overflow the blocking glue wall 150, the underfill is cured to form an underfill glue layer 160. The height of the blocking glue wall 150 is greater than the height of the underfill glue layer 160, so that the blocking glue wall 150 can prevent the underfill glue from overflowing.

[0080] The chip packaging method of the disclosed embodiment adopts the chip package bottom filler overflow prevention control method described above to prevent the bottom filler from overflowing to the passive components, thereby preventing the passive components from being contaminated, improving the reliability of the passive components, and improving the reliability of the entire chip structure.

[0081] It is to be understood that the above embodiments are merely exemplary embodiments used to illustrate the principles of the embodiments of the present disclosure, but the embodiments of the present disclosure are not limited thereto. For those of ordinary skill in the art, various modifications and improvements can be made without departing from the spirit and essence of the embodiments of the present disclosure, and these modifications and improvements are also considered to be within the protection scope of the embodiments of the present disclosure.

Claims

1. A chip package bottom fill glue overflow prevention control method, characterized in that: The control method comprises: A chip package is provided; wherein the chip package comprises a substrate, a chip flipped on the substrate, and a passive component disposed on the substrate and located outside the chip; At a preset position on the surface of the substrate between the chip and the passive component, a laser height measurement method is used to determine the glue dispensing height; Dispensing glue at the preset position according to the dispensing height to form ultraviolet curing glue surrounding the outer side of the chip; The UV curing glue is irradiated with UV rays to make it cure quickly to form a blocking glue wall; wherein, when the underfill glue is filled between the chip and the substrate, the blocking glue wall can prevent the underfill glue from overflowing to the passive component.

2. The control method according to claim 1, characterized in that: The height of the blocking glue wall is greater than the thickness of the bottom filling glue.

3. The control method according to claim 1, characterized in that: The step of dispensing glue at the preset position according to the dispensing glue height includes: Glue is dispensed at a distance of 0.5 mm to 1.5 mm from the edge of the chip according to preset glue dispensing parameters.

4. The control method according to claim 3, characterized in that: The dispensing according to the preset dispensing parameters includes: A nozzle with a dispensing size range of 15um to 25um is used for dispensing, and the dispensing weight range during the dispensing process is controlled to be 0.3mg to 0.8mg of curing glue per 10mm length.

5. The control method according to any one of claims 1 to 4, characterized in that: The step of irradiating the UV curing adhesive with UV rays to rapidly cure the UV curing adhesive comprises: The intensity of the UV light used is in the range of 50mW / cm 2 ~100mW / cm 2 , the curing time is 5s to 8s.

6. The control method according to any one of claims 1 to 4, characterized in that: The method of using laser height measurement to determine the dispensing height includes: According to the warping degree of the substrate surface and the preset height of the blocking glue wall, the laser height is automatically measured on the surface of the substrate to determine the actual dispensing height of the ultraviolet curing glue.

7. The control method according to claim 6, characterized in that: The automatic laser height measurement on the surface of the substrate to determine the actual dispensing height of the UV curing glue includes: The actual dispensing height of the ultraviolet curing glue is automatically adjusted according to the warping degree at different positions of the substrate.

8. The control method according to any one of claims 1 to 4, characterized in that: After forming the ultraviolet curing glue surrounding the outer side of the chip, the method further includes: The formed ultraviolet curing adhesive is inspected for appearance, and adhesive repair is performed if adhesive breakage is found.

9. A chip packaging method, characterized in that: The chip packaging method comprises: Flipping the chip onto the substrate and mounting passive components on the outside of the chip; A blocking glue wall is formed between the chip and the passive component; An underfill is filled between the chip and the substrate to form an underfill layer, and the height of the blocking glue wall is greater than the height of the underfill layer; wherein, The chip package underfill overflow prevention control method according to any one of claims 1 to 8 is used in the chip packaging process to prevent the underfill from overflowing onto the passive component.

10. The chip packaging method according to claim 9, characterized in that: The step of filling an underfill between the chip and the substrate to form an underfill layer comprises: Filling the gap between the chip and the barrier glue wall with underfill glue, wherein the underfill glue flows to the gap between the chip and the substrate; Performing an appearance inspection on the underfill, if the underfill does not overflow the blocking glue wall, curing the underfill to form the underfill layer.

Citation Information

Cited By

  • BNB dispensing process

    CN119140392A

  • A BNB dispensing process

    CN119140392B

  • Semiconductor device measurement method and system thereof

    TWI903871B

  • Packaging structure and electronic device

    WO2026113649A1