Plastic film and processing technology thereof
By designing the coating structure and processing technology, sliding and rotating mechanical parts are used to form a serrated glue tape, uniform coating of plastic film is achieved, glue waste problem is solved, and processing efficiency and stability are improved.
Patent Information
- Application Number
- CN202411054713.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the existing plastic composite film processing technology, glue coating operations are prone to waste, affecting efficiency and cost.
A coating structure is designed, including a processing table, slide rod, moving part, scraper and air pump. By sliding and rotating mechanical parts, the formation and uniform coating of serrated glue tape is achieved, combining air holes and air pump to prevent Glue overflows, ensuring evenly distributed glue and reducing waste.
It realizes efficient and even coating of glue, reduces glue waste, simplifies subsequent compounding operations, and improves processing efficiency and equipment stability.
Smart Images

Figure CN118926028A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of plastic film processing, and in particular relates to a plastic film and a processing technology thereof. Background Art
[0002] Plastic film processing products are widely used in packaging, agriculture, construction, medical and other fields. There are many types of plastic films in the existing technology, including plastic composite films. Composite films refer to the combination of two or more plastic films of different materials and different properties through a specific process to form a film with comprehensive properties. It can have good barrier properties, oil resistance, water resistance, chemical resistance, mechanical strength and heat sealing properties, so it is widely used;
[0003] The preparation of plastic composite films can be completed in a variety of ways, for example, coating glue on a film body, and then using a hot pressing roller to squeeze another film body onto the film body to complete the composite work. However, when performing the glue coating operation, the relevant equipment in the prior art will drip a large amount of glue on the film body to ensure that the glue can fully cover the surface of the film body, but this method is very likely to cause a waste of glue. Summary of the invention
[0004] In view of this, the technical problem to be solved by the present invention is to provide a plastic film and a processing technology thereof, which can achieve a comprehensive coating effect on the plastic film while avoiding glue waste, thereby facilitating subsequent composite operations.
[0005] A coating structure includes a processing table and a connecting plate, a sliding rod is slidably connected to the processing table, a first tension spring is fixed between the processing table and the sliding rod, a moving part is slidably connected to the sliding rod, an adding groove is provided in the moving part, a hose capable of injecting glue into the adding groove is detachably connected to the moving part through bolts, a scraper is slidably connected to the connecting plate, a displacement sensor A is fixedly connected to the processing table, a moving end of the displacement sensor A is fixedly connected to the sliding rod, and a width of an upper opening of the adding groove is greater than a width of a lower opening of the adding groove.
[0006] The utility model also comprises a sliding block connected to the scraper, and the sliding block is connected to a testing part.
[0007] It also includes a rotating sleeve rotatably connected to the moving part, a contact head is slidably connected to the rotating sleeve, a second tension spring is fixedly connected between the rotating sleeve and the contact head, a displacement sensor B is fixedly connected to the rotating sleeve, the moving end of the displacement sensor B is fixedly connected to the contact head, and an electromagnetic block capable of adsorbing the sliding rod is fixedly connected to the processing table.
[0008] The processing table is provided with a plurality of air holes, and the lower side of the processing table is provided with two air pumps.
[0009] A plastic film processing technology, using the coating structure described above:
[0010] Step 1: Make the plastic film gradually pass over the upper side of the processing table from left to right;
[0011] Step 2: Use the electromagnetic block to adsorb and fix the slide bar, operate the rotating sleeve to rotate on the moving part, and rotate the rotating sleeve to a position where the contact head is perpendicular to the surface of the processing table;
[0012] Step 3, operating the moving part to slide on the slide rod until the contact head is out of the area where the plastic film is located;
[0013] Step 4, operating the two blocking rollers to slide towards each other until the two blocking rollers abut against both sides of the plastic film;
[0014] Step 5: Slide the scraper down to a suitable height and operate the plastic film to move from left to right;
[0015] Step 6: The hose is used to continuously inject glue into the adding tank, and the moving part is made to slide along the processing table;
[0016] Step seven, press another base film onto the plastic film with glue through a hot pressing roller to complete the laminating operation. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The present invention is further described in detail below with reference to the accompanying drawings and specific implementation methods.
[0018] Figure 1 It is a structural schematic diagram of the processing table;
[0019] Figure 2 It is a structural schematic diagram of the mobile part;
[0020] Figure 3 This is a schematic diagram of the structure for adding a slot;
[0021] Figure 4 It is a schematic diagram of the structure of the scraper;
[0022] Figure 5 It is a structural diagram of the test unit;
[0023] Figure 6 It is a structural schematic diagram of the slider;
[0024] Figure 7 It is a structural schematic diagram of the sliding bar;
[0025] Figure 8 and Fig. 9 It is a schematic diagram of the overall structure of a smear structure. DETAILED DESCRIPTION
[0026] like Figure 1-4 and Figure 7-9 As shown:
[0027] A coating structure includes a processing table 101 and a connecting plate 301, wherein a slide bar 103 is slidably connected to the processing table 101, a first tension spring is fixedly connected between the processing table 101 and the slide bar 103, a moving part 201 is slidably connected to the slide bar 103, an adding groove 202 is provided in the moving part 201, a hose capable of injecting glue into the adding groove 202 is detachably connected to the moving part 201 by bolts, a scraper 302 is slidably connected to the connecting plate 301, a first motor is fixedly connected to the slide bar 103, a lead screw is fixedly connected to the output shaft of the first motor, the lead screw is threadedly connected to the moving part 201, a displacement sensor A is fixedly connected to the processing table 101, a moving end of the displacement sensor A is fixedly connected to the slide bar 103, a first electric push rod capable of pushing the scraper 302 to slide is fixedly connected to the connecting plate 301, and the width of the upper opening of the adding groove 202 is greater than the width of the lower opening of the adding groove 202.
[0028] When applying glue on the surface of the plastic film, the plastic film is gradually passed over the upper side of the processing table 101 from left to right. During this process, the plastic film will first pass under the position of the slide bar 103. At this time, glue can be gradually added to the adding groove 202, and the moving part 201 can be reciprocated along the slide bar 103. At this time, the glue in the adding groove 202 will naturally fall along the opening on the lower side of the adding groove 202, and then fall onto the plastic film below. Since the plastic film is in a moving state from left to right, as the moving part 201 continues to slide and the glue continues to drip, a serrated glue strip can be applied on the plastic film. Before moving the plastic film, first operate the scraper 302 on the connecting plate 301 to move toward the plastic film. When the scraper 302 moves to a suitable position, the plastic film is moved and the plastic film is moved. The moving part 201 slides to achieve the coating effect of the serrated glue tape. After the serrated glue tape is formed, when the plastic film moves to the position of the serrated glue tape and contacts the scraper 302, the scraper 302 can scrape the serrated glue tape to change it from the original serrated rotating plate to a state of being completely and evenly coated on a certain area of the plastic film. As the plastic film and the moving part 201 continue to move, the plastic film passing through the scraper 302 will be fully distributed with glue. That is, the device does not need to spray glue on the plastic film in its entirety. Only by leaving a plurality of serrated glue tapes on the plastic film, the plastic film can be fully covered with glue. Therefore, the plastic film can be fully coated without wasting glue, which is convenient for the subsequent operation of compounding other film layers with the plastic film.
[0029] If the glue content needs to be increased or decreased according to actual production needs, the glue content in the serrated glue belt can be adjusted by adjusting the moving speed of the plastic film, thereby achieving the effect of increasing or decreasing the glue content;
[0030] At the same time, since the width of the upper opening of the adding groove 202 is greater than the width of the lower opening of the adding groove 202, when glue is injected into the adding groove 202, part of the glue will remain in the adding groove 202. At this time, the overall weight of the moving part 201 can be changed, so that the sliding rod 103 can slide on the processing table 101 to overcome the elastic force of the first tension spring, so that the displacement sensor A obtains the signal. If the sliding rod 103 is always maintained at this height, or only slides up and down slightly, it proves that the amount of glue added and the amount of glue discharged from the adding groove 202 are in a basically balanced state at this time. If the sliding rod 103 slides down more significantly, it proves that the amount of glue injected is much greater than the amount discharged, and glue overflow is likely to occur. At this time, the glue injection flow rate can be reduced to maintain balance. Then, the setting of the adding groove 202 can always make the glue drip at a reasonable flow rate, further avoiding glue waste.
[0031] At the same time, if the slide bar 103 slides up significantly, it proves that the injection amount of glue is far less than the discharge amount. At this time, the glue injection flow rate can be increased to maintain a balanced posture. If the slide bar 103 cannot slide down to the appropriate position smoothly no matter how it is adjusted, it proves that the hose may not be able to discharge the glue normally. At this time, staff are required to arrive at the site for manual observation and maintenance operations. That is, the equipment can also monitor the dripping of glue, and promptly discover the situation where the glue cannot drip normally, thereby ensuring processing stability.
[0032] like Figure 5 , Figure 6 and Figure 8 As shown:
[0033] It also includes a slider 401 connected to the scraper 302 , and a testing part 402 is connected to the slider 401 .
[0034] When the signal obtained by the displacement sensor A remains unchanged, or when the slide bar 103 slides up or down a long distance, the staff can operate the scraper 302 to slide on the connecting plate 301, and then use the test part 402 to actively move the slide bar 103 to slide, so as to test whether the displacement sensor A can obtain the signal, and then determine whether the working state of the displacement sensor A is normal. In this way, before the staff arrives at the site, a preliminary judgment can be made on the cause of the special signal, which brings convenience to the subsequent operation and maintenance operations at the site.
[0035] like Figure 1 , Figure 2 and Figure 8 As shown:
[0036] It also includes a rotating sleeve 204 rotatably connected to the moving part 201, a contact head 203 is slidably connected to the rotating sleeve 204, a second tension spring is fixed between the rotating sleeve 204 and the contact head 203, a displacement sensor B is fixed to the rotating sleeve 204, the moving end of the displacement sensor B is fixed to the contact head 203, and an electromagnetic block capable of adsorbing the sliding rod 103 is fixed to the processing table 101.
[0037] Before applying the serrated glue, the slide bar 103 is first adsorbed and fixed by the electromagnetic block, and then the rotating sleeve 204 is operated to rotate on the moving part 201, so that the rotating sleeve 204 rotates to a position where the contact head 203 is perpendicular to the surface of the processing table 101. During this process, the processing table 101 gradually presses the contact head 203 on the rotating sleeve 204 to overcome the elastic force of the second tension spring and slide, so that the displacement sensor B receives the signal. When the rotating sleeve 204 rotates to a position where the contact head 203 is perpendicular to the surface of the processing table 101, the moving part 201 is operated again. 01 slides on the slide bar 103, and the contact head 203 will always be in contact with the surface of the processing table 101. If the contact head 203 enters the area where the plastic film is located, the contact head 203 will slide slightly upward on the rotating sleeve 204. When the contact head 203 leaves the area where the plastic film is located, the contact head 203 will slide slightly downward. The signal received by the displacement sensor B can accurately determine the width of the plastic, thereby facilitating the setting of the range for the subsequent glue application operation and ensuring the stable progress of the subsequent processing.
[0038] like Figure 1 As shown:
[0039] The processing table 101 is provided with a plurality of air holes 102 , and two air extractors are provided at the lower side of the processing table 101 . The plurality of air holes 102 are symmetrically distributed at the front and rear sides of the processing table 101 , and the two air extractors are respectively installed at the lower sides of the plurality of air holes 102 in the front and rear areas of the processing table 101 .
[0040] When performing the plastic film width detection operation, two vacuum pumps are started, and then the two vacuum pumps are used to apply a downward adsorption effect to the left and right sides of the plastic film to be detected, to ensure that the plastic film will not warp when the contact head 203 is used for subsequent detection, thereby ensuring the accuracy of the detection result.
[0041] like Figure 8 As shown:
[0042] It also includes two blocking rollers 501 slidably connected to the processing table 101 . Two second electric push rods are fixedly connected to the processing table 101 . The telescopic rods of the two second electric push rods are fixedly connected to the two blocking rollers 501 , respectively.
[0043] After detecting the width of the plastic film, the two blocking rollers 501 can be operated to slide close to each other on the processing table 101 until the two blocking rollers 501 are against the two sides of the plastic film. Then, when glue is dripped subsequently, the two blocking rollers 501 can block the two sides of the plastic film to avoid glue overflow during the subsequent normal glue application operation, thereby ensuring stable operation of the equipment.
[0044] like Figure 8 As shown:
[0045] A baffle 502 is fixedly connected to each of the blocking rollers 501 .
[0046] The provision of the two baffles 502 can further increase the blocking effect of the blocking roller 501 on the glue, thereby further preventing the glue from overflowing.
[0047] like Figure 5 , Figure 6 and Figure 8 As shown:
[0048] The slider 401 is slidably connected to the scraper 302, and the testing part 402 is rotatably connected to the slider 401. A third tension spring is fixedly connected between the slider 401 and the scraper 302, and the elastic force of the third tension spring is greater than that of the first tension spring. A second motor capable of driving the testing part 402 to rotate is fixedly connected to the slider 401, and a displacement sensor C is fixedly connected to the scraper 302, and the moving end of the displacement sensor C is fixedly connected to the scraper 302.
[0049] If the displacement sensor A still cannot obtain a signal by operating the upward sliding scraper 302, the test part 402 can be operated to rotate on the slider 401 until the test part 402 is rotated to the position where the test part 402 overlaps with the lowermost end of the moving part 201 in the vertical direction, and then the moving part 201 is operated to slide on the slide bar 103 until the moving part 201 moves to the contact position with the test part 402. At this time, the moving part 201 is continuously slid so that the moving part 201 is moved by the test part 402. At the same time, since the elastic force of the third tension spring is greater than that of the first tension spring, the slide bar 103 can overcome the first tension spring and slide upward on the processing table 101, and further actively slide the slide bar 103 to test whether the displacement sensor A can obtain the signal, thereby further determining the working state of the displacement sensor A, avoiding the reason why the displacement sensor A cannot obtain a signal due to a failure of the power source driving the scraper 302 to slide upward, and ensuring the accuracy of the self-test result;
[0050] If the reason why the displacement sensor A cannot obtain a signal is that the electromagnetic block is always energized and the fixed posture of the slide bar 103 is not released, then when the moving part 201 contacts the test part 402, the test part 402 will be moved by the moving part 201, so that the slider 401 will slide on the scraper 302 to overcome the elastic force of the third tension spring. At this time, the signal can be obtained by the displacement sensor C, so as to further detect the fault condition.
[0051] like Figure 8-9 As shown:
[0052] An open container is detachably connected to the lower side of the processing table 101 via bolts.
[0053] The open container can further receive the glue that may overflow, thereby preventing the glue from overflowing and affecting the surrounding environment.
[0054] A plastic film processing technology, using the coating structure described above:
[0055] Step 1, allowing the plastic film to gradually pass over the upper side of the processing table 101 from left to right;
[0056] Step 2: Use the electromagnetic block to adsorb and fix the slide bar 103, operate the rotating sleeve 204 to rotate on the moving part 201, and rotate the rotating sleeve 204 to a position where the contact head 203 is perpendicular to the surface of the processing table 101;
[0057] Step 3, operate the moving part 201 to slide on the slide bar 103 until the contact head 203 is out of the area where the plastic film is located;
[0058] Step 4: operate the two blocking rollers 501 to slide towards each other until the two blocking rollers 501 abut against both sides of the plastic film;
[0059] Step 5, slide the scraper 302 down to a suitable height, and operate the plastic film to move from left to right;
[0060] Step 6: The hose continuously injects glue into the adding tank 202, and the moving part 201 slides along the processing table 101;
[0061] Step seven, press another base film onto the plastic film with glue through a hot pressing roller to complete the laminating operation.
[0062] A plastic film, the concrete is made by the plastic film processing technology.
Claims
1. A coating structure, characterized in that: The invention comprises a processing table (101) and a connecting plate (301), wherein a slide bar (103) is slidably connected to the processing table (101), a first tension spring is fixedly connected between the processing table (101) and the slide bar (103), a moving part (201) is slidably connected to the slide bar (103), an adding groove (202) is provided in the moving part (201), a hose capable of injecting glue into the adding groove (202) is detachably connected to the moving part (201) via bolts, a scraper (302) is slidably connected to the connecting plate (301), a displacement sensor A is fixedly connected to the processing table (101), a moving end of the displacement sensor A is fixedly connected to the slide bar (103), and a width of an upper opening of the adding groove (202) is greater than a width of a lower opening of the adding groove (202).
2. A coating structure according to claim 1, characterized in that: It also includes a sliding block (401) connected to the scraper (302), and a testing portion (402) is connected to the sliding block (401).
3. A coating structure according to claim 2, characterized in that: The device also includes a rotating sleeve (204) rotatably connected to the moving part (201), a contact head (203) being slidably connected to the rotating sleeve (204), a second tension spring being fixedly connected between the rotating sleeve (204) and the contact head (203), a displacement sensor B being fixedly connected to the rotating sleeve (204), a moving end of the displacement sensor B being fixedly connected to the contact head (203), and an electromagnetic block capable of adsorbing the sliding rod (103) being fixedly connected to the processing table (101).
4. A coating structure according to claim 3, characterized in that: The processing table (101) is provided with a plurality of air holes (102), and two air extractors are provided on the lower side of the processing table (101).
5. A coating structure according to claim 4, characterized in that: It also includes two blocking rollers (501) slidably connected to the processing table (101).
6. A coating structure according to claim 5, characterized in that: A baffle plate (502) is fixedly connected to each of the blocking rollers (501).
7. A coating structure according to claim 6, characterized in that: The slider (401) is slidably connected to the scraper (302), the testing part (402) is rotatably connected to the slider (401), a third tension spring is fixedly connected between the slider (401) and the scraper (302), and the elastic force of the third tension spring is greater than that of the first tension spring.
8. A coating structure according to claim 7, characterized in that: An open container is detachably connected to the lower side of the processing table (101) via bolts.
9. A plastic film processing process, characterized in that: Using a coating structure as claimed in claim 6: Step 1, allowing the plastic film to gradually pass over the upper side of the processing table (101) from left to right; Step 2, using an electromagnetic block to adsorb and fix the slide bar (103), and operating the rotating sleeve (204) to rotate on the moving part (201), so that the rotating sleeve (204) rotates to a position where the contact head (203) and the surface of the processing table (101) are perpendicular to each other; Step 3, operating the moving part (201) to slide on the sliding rod (103) until the contact head (203) is separated from the area where the plastic film is located; Step 4, operating the two blocking rollers (501) to slide towards each other until the two blocking rollers (501) abut against two sides of the plastic film; Step 5, slide the scraper (302) down to a suitable height, and operate the plastic film to move from left to right; Step 6, the hose is used to continuously inject glue into the adding tank (202), and the moving part (201) is made to slide along the processing table (101); Step seven, press another base film onto the plastic film with glue through a hot pressing roller to complete the laminating operation.
10. A plastic film, characterized in that: The concrete is obtained by the plastic film processing process described in claim 9.