Method for machining sprue bush water ring of die-casting die through thermal expansion method

Through the combination of thermal expansion method and hydraulic equipment, the problems of water leakage and cooling and shrinkage at the connection during gate sleeve water ring processing are solved, and stable sealing and efficient production of gate sleeve are achieved, which extends product life and reduces costs. .

CN118926841AInactive Publication Date: 2024-11-12巢湖宜安云海科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411147786.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The processing method of existing gate sleeve water rings is likely to cause water leakage in the outer ring, affecting product quality and life, or due to unreasonable material selection, it causes cooling, shrinkage and cracking at the connection, destroying the accuracy of the inner hole, and increasing costs.

Method used

The outer ring is heated and expanded by thermal expansion, and hydraulic equipment is used to stably install it on the gate sleeve, and it is clamped and transported by robotic arms to ensure sealing and stability, avoid scalding by manual operations, and improve processing efficiency and quality.

Benefits of technology

It realizes a stable seal between the outer ring and the gate sleeve, avoids water leakage, extends product life, improves production efficiency and quality stability, and reduces subsequent welding and maintenance costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926841A_ABST
    Figure CN118926841A_ABST
Patent Text Reader

Abstract

The invention discloses a die-casting die thermal expansion method sprue bush water ring machining method, which relates to the technical field of sprue bushings, and comprises the following steps of outer ring material preparation, outer ring machining, sprue bush material preparation, sprue bush machining and outer ring and sprue bush installation. The inner diameter of the outer ring is designed to be 0.30-0.50 mm larger than the outer diameter of the sprue bush, it is guaranteed that the outer ring can be stably installed on the surface of the sprue bush after being heated, meanwhile, after the outer ring is cooled, welding does not need to be conducted on the outer ring and the sprue bush, the sealing performance between the outer ring and the sprue bush is improved, in the production process, no water leakage exists inside and outside, and the production efficiency is improved. The service life of the sprue bush is prolonged, in the whole outer ring and sprue bush mounting process, a mechanical arm is adopted for clamping and transferring the outer ring, operators are prevented from being scalded due to manual operation, and meanwhile the production and machining efficiency and the machining quality stability are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of sprue sleeves, in particular to a method for processing a sprue sleeve water ring of a die-casting mold by thermal expansion method. Background Art

[0002] The sprue sleeve of the die-casting mold cooperates with the punch at the front end of the injection to inject aluminum and magnesium alloy liquid into the mold cavity at high speed and high pressure for molding. The sprue sleeve water ring is a positioning structure for the sprue sleeve. Its design purpose is to ensure the precise alignment of the sprue sleeve and the mold nozzle, thereby improving the efficiency of the injection molding process and product quality. This structure usually adopts the Class B structure, and the positioning ring is used to achieve the precise alignment of the spherical surface of the sprue sleeve and the spherical surface of the nozzle. When designing the sprue sleeve water ring, it is necessary to consider the distance from the bottom of the spherical surface of the sprue sleeve to the panel to ensure that it does not exceed the maximum length that the injection molding machine nozzle can extend, so as to avoid affecting the smooth progress of the injection molding process.

[0003] For example, announcement number: CN213002496U discloses "a double-circulation cooling water jacket sprue sleeve", which includes a sprue sleeve body, a first cooling water jacket is installed at one end of the sprue sleeve body, the inner wall of the first cooling water jacket is connected to the second cooling water jacket, a barrel fixing stop is provided in the middle of one side of the sprue sleeve body away from the first cooling water jacket, and an anti-rotation flat mouth is provided on the outer wall of the sprue sleeve body.

[0004] However, in the prior art, there are two production methods for processing the water ring of the gate sleeve. One is to enlarge the outer ring and put it on the upper part of the gate sleeve, and then use welding to fix and seal it. However, this production method has high temperature, high pressure and strong impact during production, which can easily cause the outer ring to leak. Leakage will have a serious impact on the product, including sand holes and cold materials in the product, resulting in a high scrap rate of the product. The other method is to make the outer ring smaller and expand it by heating, and the sleeve is cooled and contracted to achieve a sealing effect. However, this production method is unreasonable in material selection, which leads to cooling and shrinkage cracking at the connection, destroying the accuracy of the inner hole of the gate sleeve, and causing the punch and inner hole to leak, the outer ring to leak, resulting in cold grids, sand holes, and scrap of the product. The sleeve is unstable, and the outer ring needs to be repaired and sealed. The gate sleeve is scrapped prematurely, increasing costs. Summary of the invention

[0005] The object of the present invention is to provide a method for processing a water ring of a gate sleeve by the thermal expansion method of a die-casting mold, so as to solve the problems raised in the above-mentioned background technology that the outer ring is enlarged, resulting in water leakage of the outer ring, which will have serious impact on the product, including sand holes and cold materials in the product, resulting in a high scrap rate of the product, and the outer ring is made small and expanded by heating, resulting in cooling, shrinkage and cracking at the connection, destroying the accuracy of the inner hole of the gate sleeve, and at the same time causing the punch to get stuck and the inner hole to leak, the outer ring to leak, resulting in cold grids, sand holes, and scrap of the product, the assembly is unstable, the outer ring needs to be repaired and sealed, the gate sleeve is scrapped prematurely, and the cost is increased.

[0006] To achieve the above object, the present invention provides the following technical solution: a method for processing a gate sleeve water ring of a die casting mold by thermal expansion method, comprising the following steps: S1. Outer ring material preparation: Select seamless steel pipe, cut and grind it; S2. Outer ring processing: cutting and polishing the outer ring; S3. Preparation of sprue sleeve materials: Select seamless steel pipes, cut and grind them; S4, sprue bushing processing: cutting and polishing the sprue bushing; S5. Installation of outer ring and sprue sleeve: Use heating equipment to heat the outer ring, then put the heated outer ring on the upper part of the sprue sleeve, and finally use pressurizing equipment to put the outer ring on the surface of the sprue sleeve.

[0007] Preferably, in step S1, the cutting and grinding of the seamless steel pipe in the preparation of the outer ring material includes the following steps: S11, the cutting equipment used for cutting the seamless steel pipe is one of a band saw machine, a plasma cutting machine, a pipe cutting machine or a water jet cutting machine, and when one of the band saw machine, the plasma cutting machine or the pipe cutting machine is used for cutting, a coolant is used for cooling during the cutting process; S12. The seamless steel pipe is ground using a CNC grinding machine.

[0008] Preferably, in step S2, the outer ring processing includes cutting the outer ring and polishing the outer ring, which includes the following steps: S21, the device for cutting the outer ring is a lathe or a milling machine, and the device for polishing the outer ring is a CNC polishing machine; S22. The cutting precision of the outer ring is IT6.

[0009] Preferably, in step S3, a seamless steel pipe is selected in the preparation of the sprue sleeve material, and cutting and grinding the seamless steel pipe include the following steps: S31, the cutting equipment used for cutting the seamless steel pipe is one of a band saw machine, a plasma cutting machine, a pipe cutting machine or a water jet cutting machine, and when one of the band saw machine, the plasma cutting machine or the pipe cutting machine is used for cutting, a coolant is used for cooling during the cutting process; S32. The seamless steel pipe is ground using a CNC grinding machine.

[0010] Preferably, in step S4, the sprue bushing is cut and polished in the sprue bushing processing, which includes the following steps: S41, the device for cutting the outer ring is a lathe or a milling machine, and the device for polishing the outer ring is a CNC polishing machine; S42, the cutting precision of the outer ring is IT6.

[0011] Preferably, in step S5, the outer ring is heated by using a heating device during the installation of the outer ring and the sprue bushing, and then the heated outer ring is sleeved on the upper part of the sprue bushing, and finally the outer ring is sleeved on the surface of the sprue bushing by using a pressurizing device, which includes the following steps: S51, the heating device used by the heating device to heat the outer ring is one of a high-frequency heater, a flame heating device, a high-temperature furnace or an induction heating machine; S52, using a clamping device to sleeve the heated outer ring onto the upper part of the gate sleeve; S53, the pressurizing device used to sleeve the outer ring onto the surface of the gate sleeve is a hydraulic device; The method heats the outer ring to a set temperature to generate appropriate thermal expansion, and then sleeves it on the upper part of the sprue sleeve. The outer ring is stably pressed down to a set position on the upper part of the sprue sleeve using hydraulic equipment. During the entire installation process of the outer ring and the sprue sleeve, a mechanical arm is used to clamp and transport the outer ring to avoid burns to operators during manual operation, while improving the efficiency of production and processing and the stability of processing quality.

[0012] Preferably, the heating temperature of the heating device is 680°C-800°C.

[0013] Preferably, the inner diameter of the outer ring is larger than the outer diameter of the sprue bushing.

[0014] Preferably, the inner diameter of the outer ring is 0.30-0.50 mm larger than the outer diameter of the sprue bushing.

[0015] Compared with the prior art, the present invention has the following beneficial effects: In this method, the inner diameter of the outer ring is designed to be 0.30-0.50 mm larger than the outer diameter of the sprue bushing, so that the outer ring can be stably installed on the surface of the sprue bushing after heating. At the same time, after the outer ring is cooled, there is no need to weld the outer ring and the sprue bushing, thereby improving the sealing between the outer ring and the sprue bushing, so that no water can be leaked inside or outside during the production process, and the service life of the sprue bushing is prolonged. At the same time, the outer ring is heated to reach the set temperature to produce appropriate thermal expansion, and then it is sleeved on the upper part of the gate sleeve. The outer ring is stably pressed down to the set position on the upper part of the gate sleeve using hydraulic equipment. During the entire installation process of the outer ring and the gate sleeve, a robotic arm is used to clamp and transport the outer ring to avoid burns to operators during manual operation, while improving the efficiency of production and processing as well as the stability of processing quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 The present invention is a flow chart of the method for processing the gate sleeve water ring of a die-casting mold by thermal expansion method. DETAILED DESCRIPTION

[0017] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the implementation regulations described are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0018] See also Figure 1 The present invention provides a technical solution: a method for processing a gate sleeve water ring of a die casting mold by thermal expansion method, comprising the following steps: Step 1: Prepare the outer ring material: Select a seamless steel pipe, cut and grind it; In step 1, the cutting and grinding of the seamless steel pipe in the preparation of the outer ring material includes the following steps: the cutting equipment used for cutting the seamless steel pipe is one of a band saw machine, a plasma cutting machine, a pipe cutting machine or a water jet cutting machine, and when the band saw machine, the plasma cutting machine or the pipe cutting machine is used for cutting, a coolant is used for cooling during the cutting process; the grinding equipment used for grinding the seamless steel pipe is a CNC grinder; Step 2, outer ring processing: cutting and polishing the outer ring; in step 2, the outer ring processing includes the following steps: the outer ring is cut by a lathe or a milling machine, and the outer ring is polished by a CNC polishing machine; the outer ring is cut with an accuracy of IT6; Step 3: Preparation of sprue sleeve materials: Select seamless steel pipes, cut and grind them; In step three, a seamless steel pipe is selected in the preparation of the gate sleeve material, and the cutting and grinding of the seamless steel pipe include the following steps: the cutting equipment used for cutting the seamless steel pipe is a band saw machine, a plasma cutting machine, a pipe cutting machine or a water jet cutting machine, and when the band saw machine, the plasma cutting machine or the pipe cutting machine is used for cutting, a coolant is used for cooling during the cutting process; the grinding equipment used for grinding the seamless steel pipe is a CNC grinder; Step 4, sprue bushing processing: cutting the sprue bushing and polishing the sprue bushing; in step 4, cutting the sprue bushing and polishing the sprue bushing in the sprue bushing processing includes the following steps: the equipment for cutting the outer ring is a lathe or a milling machine, and the equipment for polishing the outer ring is a CNC polishing machine; the precision of cutting the outer ring is IT6; Step 5, installation of outer ring and sprue sleeve: use heating equipment to heat the outer ring, then sleeve the heated outer ring on the upper part of the sprue sleeve, and finally use pressurizing equipment to sleeve the outer ring on the surface of the sprue sleeve; in step 5, the installation of the outer ring and sprue sleeve uses heating equipment to heat the outer ring, then sleeve the heated outer ring on the upper part of the sprue sleeve, and finally use pressurizing equipment to sleeve the outer ring on the surface of the sprue sleeve, including the following steps: the heating equipment used to heat the outer ring is a high-frequency heater, a flame heating equipment, a high-temperature furnace or an induction heating machine; the clamping equipment is used to sleeve the heated outer ring on the upper part of the sprue sleeve; the pressurizing equipment used to sleeve the outer ring on the surface of the sprue sleeve is a hydraulic equipment; the heating temperature of the heating equipment is 680℃-800℃, the inner diameter of the outer ring is larger than the outer diameter of the sprue sleeve, and the inner diameter of the outer ring is 0.30-0.50mm larger than the outer diameter of the sprue sleeve.

[0019] In the process of processing the water ring of the sprue sleeve in this method, the outer ring is heated to a set temperature to generate appropriate thermal expansion, and then it is sleeved on the upper part of the sprue sleeve. The outer ring is stably pressed down to the set position on the upper part of the sprue sleeve using hydraulic equipment. During the entire installation process of the outer ring and the sprue sleeve, a mechanical arm is used to clamp and transport the outer ring, thereby improving the efficiency of production and processing and the stability of processing quality. The inner diameter of the outer ring is designed to be 0.30-0.50mm larger than the outer diameter of the sprue bushing to ensure that the outer ring can be stably installed on the surface of the sprue bushing. At the same time, after the outer ring is cooled, there is no need to weld the outer ring and the sprue bushing.

[0020] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for processing a gate sleeve water ring of a die casting mold by thermal expansion method, characterized in that: The following steps are involved: S1. Outer ring material preparation: Select seamless steel pipe, cut and grind it; S2, outer ring processing: cutting and polishing the outer ring; S3. Preparation of sprue sleeve materials: Select seamless steel pipes, cut and grind them; S4, sprue bushing processing: cutting and polishing the sprue bushing; S5. Installation of outer ring and sprue sleeve: Use heating equipment to heat the outer ring, then put the heated outer ring on the upper part of the sprue sleeve, and finally use pressurizing equipment to put the outer ring on the surface of the sprue sleeve.

2. The method for processing a gate sleeve water ring of a die casting mold by thermal expansion method according to claim 1, characterized in that: In step S1, the cutting and grinding of the seamless steel pipe in the outer ring material preparation includes the following steps: S11, the cutting equipment used for cutting the seamless steel pipe is one of a band saw machine, a plasma cutting machine, a pipe cutting machine or a water jet cutting machine, and when one of the band saw machine, the plasma cutting machine or the pipe cutting machine is used for cutting, a coolant is used for cooling during the cutting process; S12. The seamless steel pipe is ground using a CNC grinding machine.

3. The method for processing a gate sleeve water ring of a die casting mold by thermal expansion method according to claim 1, characterized in that: In step S2, the outer ring processing includes cutting the outer ring and polishing the outer ring, which includes the following steps: S21, the device for cutting the outer ring is a lathe or a milling machine, and the device for polishing the outer ring is a CNC polishing machine; S22. The cutting precision of the outer ring is IT6.

4. The method for processing a gate sleeve water ring of a die casting mold by thermal expansion method according to claim 3, characterized in that: In step S3, a seamless steel pipe is selected from the sprue sleeve material preparation, and cutting and grinding the seamless steel pipe include the following steps: S31, the cutting equipment used for cutting the seamless steel pipe is one of a band saw machine, a plasma cutting machine, a pipe cutting machine or a water jet cutting machine, and when one of the band saw machine, the plasma cutting machine or the pipe cutting machine is used for cutting, a coolant is used for cooling during the cutting process; S32. The seamless steel pipe is ground using a CNC grinding machine.

5. The method for processing a gate sleeve water ring of a die casting mold by thermal expansion method according to claim 4, characterized in that: In step S4, the sprue bushing is cut and polished during the sprue bushing processing, including the following steps: S41, the device for cutting the outer ring is a lathe or a milling machine, and the device for polishing the outer ring is a CNC polishing machine; S42. The cutting precision of the outer ring is IT6.

6. The method for processing a gate sleeve water ring of a die casting mold by thermal expansion method according to claim 5, characterized in that: In step S5, the outer ring is heated by using a heating device during the installation of the outer ring and the sprue bushing, and then the heated outer ring is sleeved on the upper part of the sprue bushing, and finally the outer ring is sleeved on the surface of the sprue bushing by using a pressurizing device, including the following steps: S51, the heating device used by the heating device to heat the outer ring is one of a high-frequency heater, a flame heating device, a high-temperature furnace or an induction heating machine; S52, using a clamping device to sleeve the heated outer ring onto the upper part of the gate sleeve; S53, the pressurizing equipment used to connect the outer ring to the surface of the gate sleeve is a hydraulic equipment.

7. The method for processing a gate sleeve water ring of a die casting mold by thermal expansion method according to claim 6, characterized in that: The heating temperature of the heating device is 680°C-800°C.

8. The method for processing a gate sleeve water ring of a die casting mold by thermal expansion method according to claim 1, characterized in that: The inner diameter of the outer ring is greater than the outer diameter of the sprue bushing.

9. The method for processing a gate sleeve water ring of a die casting mold by thermal expansion method according to claim 1, characterized in that: The inner diameter of the outer ring is 0.30-0.50 mm larger than the outer diameter of the sprue bushing.