Preparation method of cementing material with ultralow water-binder ratio

By using agitating instruments and automated control systems during the preparation of ultra-high performance concrete, the problem of the need for multiple operators to prepare ultra-low slurry is solved, the consistency and reliability of material preparation are achieved, and the quality and safety of engineering are improved. .

CN118927405AInactive Publication Date: 2024-11-12CHINA CONSTR EIGHT ENG DIV CORP LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411092015.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-09
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the preparation of ultra-high performance concrete, the preparation of ultra-low slurry requires multiple operators to work together, resulting in high labor intensity and inconsistent material preparation, affecting project quality and safety.

Method used

A stirring instrument is used for slurry stirring, and the premixed dry powder and water is mixed by 1:1 ratio, combined with the distance measuring sensor and feeding controller, to ensure the consistency of stirring rate and material uniformity, calculate the delivery rate and quantity of premixed dry powder, and use CNC The display screen and chip enable automated control.

Benefits of technology

It reduces labor intensity, ensures the consistency and reliability of material preparation, improves the preparation efficiency and quality of ultra-high performance concrete, simplifies the operating process, and reduces operating risks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118927405A_ABST
    Figure CN118927405A_ABST
Patent Text Reader

Abstract

The invention relates to a preparation method of a cementing material with an ultralow water-binder ratio, which comprises the following steps: providing a stirring instrument and premixed dry powder, and adding water and part of the premixed dry powder into a stirring pot of the stirring instrument; starting the stirring instrument, and stirring and mixing water and the premixed dry powder to form slurry; continuously adding the residual premixed dry powder into the slurry and continuously stirring the slurry until the premixed dry powder is completely added; the stirring speed of the stirring instrument is increased to continuously stir the slurry until no powder block exists in the slurry, the operation is simple, and the use is convenient.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of slurry preparation, in particular to a method for preparing a cementitious material with an ultra-low water-to-binder ratio. Background Art

[0002] In the current field of building materials, ultra-high performance concrete (UHPC) has attracted widespread attention for its excellent mechanical properties and durability. UHPC is usually designed with an ultra-low water-binder ratio (W / B). This strategy effectively improves the strength and durability of concrete by reducing the amount of water, while reducing the risk of cracks and leakage, thereby improving the overall quality and safety of the project.

[0003] Ultra-high performance concrete often uses ultra-low water-binder ratio to design the mix ratio, which reduces the amount of water used, improves the strength and durability of concrete, reduces cracks and leakage problems, and improves the overall quality and safety of the project. However, when preparing ultra-low slurry, it is often necessary to add mixed dry powder when stirring the slurry so that water and mixed dry powder can be fully mixed to form ultra-low slurry. One person controls the stirring rate, and the others control the addition of mixed dry powder. This often requires multiple operators to operate when making ultra-low slurry. Summary of the invention

[0004] The purpose of the present invention is to overcome the defects of the prior art and provide a method for preparing ultra-low water-cement ratio cementitious material. The labor intensity is reduced by using a stirring instrument. At the same time, the stirring instrument is used to ensure that the speed is the same when the slurry is stirred, thereby ensuring the consistency and reliability of material preparation, and providing strong technical support for the wide application of UHPC.

[0005] The technical solution to achieve the above object is a method for preparing an ultra-low water-to-cement ratio cementitious material, comprising the following steps:

[0006] Providing a stirring apparatus and premixed dry powder, and adding water and a portion of the premixed dry powder into a stirring pot of the stirring apparatus;

[0007] Starting the stirring device to stir and mix the water and the premixed dry powder to form a slurry;

[0008] Continue adding the remaining premixed dry powder into the slurry and continue stirring the slurry until all the premixed dry powder has been added;

[0009] The stirring speed of the stirring device is increased to continue stirring the slurry until there is no powder lump inside the slurry.

[0010] Furthermore, when the premixed dry powder is continuously added to the slurry, the addition rate Fmax of the premixed dry powder is:

[0011] Fmax=K*ω*V

[0012] Wherein, K is a characteristic parameter for mixing the slurry, ω is the rotation rate of the stirring instrument, and V is the volume of the slurry.

[0013] Furthermore, the safe input amount X of the premixed dry powder is:

[0014] X=Fmax*G

[0015] Where G is the predetermined safety factor.

[0016] Furthermore, the calculation formula of the volume V of the slurry is:

[0017] V=C*h

[0018] Wherein C is the cross-sectional area of ​​the stirring pot of the stirring apparatus, and h is the height of the slurry in the stirring pot.

[0019] Furthermore, water and a portion of the premixed dry powder are added to the stirring pot of the stirring instrument, and the ratio of the water to the premixed dry powder is 1:1.

[0020] Furthermore, the stirring instrument is provided with a distance sensor, and the distance sensor measures the height of the slurry in the stirring pot.

[0021] Furthermore, a feeding controller is provided on the stirring instrument, and the remaining premixed dry powder is filled into the feeding controller;

[0022] When the stirring device continuously stirs the slurry, the premixed dry powder is continuously filled into the slurry through the feeding controller.

[0023] Furthermore, the stirring instrument is provided with a numerical control display screen.

[0024] Furthermore, a chip is provided in the stirring instrument, and the rate of continuous addition of the premixed dry powder is calculated by the chip.

[0025] Furthermore, the total amount of the premixed dry powder added and the ratio of the water added to the stirring pot are determined according to actual use requirements.

[0026] Compared with the prior art, the present invention has the following beneficial effects:

[0027] 1. By using a stirring instrument to ensure the same rate when stirring the slurry, the consistency and reliability of material preparation are ensured, providing strong technical support for the widespread application of UHPC.

[0028] 2. When adding premixed dry powder, determine the amount of premixed dry powder to be added based on the volume of the slurry in the stirring pot to ensure the yield of the mixed slurry. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 This is a structural diagram of an apparatus for preparing a method for ultra-low water-to-cementitious ratio cementitious material according to the present invention.

[0030] Figure 2 The present invention is a schematic diagram of an oval gear flowmeter in a flow controller of a method for preparing a cementitious material with an ultra-low water-to-cement ratio.

[0031] Figure 3 The present invention is a schematic diagram of a screw inserted into a flow controller in a method for preparing a cementitious material with an ultra-low water-to-cement ratio.

[0032] Figure 4 This is a schematic diagram of a wave wheel structure in a flow controller of a method for preparing an ultra-low water-to-cement ratio cementitious material according to the present invention.

[0033] Figure 5 This is a measurement effect diagram of a distance measuring sensor in a method for preparing a cementitious material with an ultra-low water-to-cement ratio according to the present invention.

[0034] Legend: 1. Base; 2. Column; 3. Motor; 4. CNC display screen; 5. Distance sensor; 6. Dry powder filling port; 7. Controlled discharge port; 71. Flow controller; 8. Stirring pot; 9. Stirring blade. DETAILED DESCRIPTION

[0035] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.

[0036] See also Figure 1 A method for preparing an ultra-low water-to-cement ratio cementitious material comprises the following steps: providing a stirring instrument and a premixed dry powder, adding water and a portion of the premixed dry powder into a stirring pot 8 of the stirring instrument; starting the stirring instrument, maintaining the rotation speed of the stirring instrument at a constant 60 r / min, stirring and mixing water and the premixed dry powder to form a slurry; continuously adding the remaining premixed dry powder into the slurry and continuously stirring the slurry until all the premixed dry powder has been added; increasing the stirring speed of the stirring instrument, raising the rotation speed of the stirring instrument to 120 r / min, and continuing to stir the slurry until there is no powder lump inside the slurry. Preferably, after the rotation speed of the stirring instrument is raised to 120 r / min, the stirring is accelerated for 10 s, the stirring is stopped, and the slurry is removed from the pot.

[0037] Furthermore, the stirring instrument includes: a base 1, a column 2 arranged on the base 1, a motor 3 is arranged on the top of the column 2, and a stirring blade 9 is connected to the output end of the motor 3. The stirring blade 9 is placed in the stirring pot 8 to stir the material in the stirring pot 8. Preferably, a support for placing the stirring pot 8 is provided on the side of the column 2 and below the stirring blade 9.

[0038] Furthermore, when the premixed dry powder is continuously added to the slurry, the addition rate Fmax of the premixed dry powder is:

[0039] Fmax=K*ω*V

[0040] Wherein, K is a characteristic parameter for mixing the slurry, ω is the rotation rate of the stirring instrument, and V is the volume of the slurry.

[0041] In the present invention, a preferred embodiment is: when the premixed dry powder is continuously added to the slurry, the slurry volume at a certain moment is 100ml (1*10 -4 m3), the speed is 60r / min (6.284rad / s), the K in the formula Fmax=K*ω*V is 0.016rad according to the material characteristic value table. -1 , then Fmax=K*ω*V=0.016*6.284*1*10 -4 =10ml / s, that is, at this time, add the premixed dry powder into the container at a rate of 10ml / s, and keep dynamic calculation and feeding until all the powder is added.

[0042] Furthermore, K=A1*A2*A3; wherein A1 is the structural parameter of the mixer, representing the influence of the mechanical structure and surface friction of the container on the stirring efficiency; A2 is the structural parameter of the stirring blade 9, representing the influence of the mechanical structure and surface friction of the blade on the stirring efficiency; A3 is the characteristic parameter of the premixed dry powder, and the characteristic parameter of A3 is determined by the material ratio and content in the premixed dry powder. When the solid powder is premixed evenly, A3 is a fixed constant, wherein A1 and A2 are fixed parameters of the stirring instrument, which are determined by the stirring instrument before leaving the factory.

[0043] Furthermore, the safe input amount X of the premixed dry powder is:

[0044] X=Fmax*G

[0045] Where G is a predetermined safety factor. Preferably, the safety factor G is determined according to the construction requirements on site, and the safety factor G is less than 1 to avoid adding too much premixed dry powder, and the stirring instrument cannot mix the premixed dry powder with the slurry in time, which leads to the phenomenon of powder lumps in the slurry formed by the final stirring, so that the overall quality of the slurry is reduced. In this embodiment, the safety factor is 90%. When Fmax=10ml / s, X=10*0.9=9ml / s, that is, the premixed dry powder is added to the slurry at a rate of 9ml / s.

[0046] Furthermore, the calculation formula of the volume V of the slurry is:

[0047] V=C*h

[0048] Wherein C is the cross-sectional area of ​​the stirring pot 8 of the stirring apparatus, and H is the height of the slurry in the stirring pot 8. Preferably, when the slurry is placed in the stirring pot 8, after ignoring the fillet of the container and the volume of the fan blades, the material in the cylindrical stirring pot 8 can be regarded as a cylinder, and its cross-sectional area is the cross-sectional area of ​​the stirring pot 8.

[0049] Furthermore, water and part of the premixed dry powder are added into the stirring pot 8 of the stirring instrument, and the ratio of the water to the premixed dry powder is 1:1.

[0050] Furthermore, the stirring apparatus is provided with a distance sensor 5, and the distance sensor 5 measures the height of the slurry in the stirring pot 8. Preferably, the distance sensor 5 measures the distance D between the distance sensor 5 and the slurry in the stirring bucket, and calculates h=h0-D to obtain the height of the slurry, wherein h0 is the setting height of the distance sensor 5.

[0051] Furthermore, a feeding controller is provided on the stirring instrument, and the remaining premixed dry powder is filled in the feeding controller; when the stirring instrument continuously stirs the slurry, the premixed dry powder is continuously filled into the slurry through the feeding controller.

[0052] Furthermore, the feeding controller includes: a flow controller 71 arranged on the side of the motor 3, a dry powder filling port 6 arranged on the top of the flow controller 71, and a controlled discharge port 7 arranged at the bottom of the flow controller 71. The flow controller 71 can be an elliptical gear flow meter, a screw or a pulsator feeding structure, so as to control the volume of the discharge per unit time.

[0053] Furthermore, the stirring instrument is provided with a numerical control display screen 4. Preferably, the numerical control display screen 4 is provided on the column 2, and the numerical control display screen 4 controls and connects the motor 3 and the flow controller. An operation interface is also provided on the numerical control display screen 4, so that even non-professionals can easily master the use of the equipment. This design not only improves the utilization rate and production efficiency of the equipment, but also reduces the operation risk and ensures the safety of production.

[0054] Furthermore, a chip is provided in the stirring instrument, and the rate of continuous addition of the premixed dry powder is calculated by the chip.

[0055] Furthermore, the total amount of the premixed dry powder added and the ratio of the water added to the stirring pot 8 are determined according to actual use requirements.

[0056] In the present invention, a preferred embodiment is: the proportion of the premixed dry powder is 75 parts by weight of PO525 cement, 10 parts by weight of silica fume, and 1 part by weight of water reducing powder, and the proportion of water added is 14 parts by weight of water, and 3 kg of slurry contains 420g of water, 2250g of cement, 300g of silica fume, and 30g of water reducing powder.

[0057] The following is an explanation of the use process of a method for preparing a ultra-low water-to-cementitious ratio cementitious material according to the present invention.

[0058] Step 1: Add all the premixed dry powder (cement, silica fume, water reducing powder) into a mixing container, premix evenly at a speed of 60r / min, and take out all 2580g of premixed dry powder for standby use.

[0059] Step 2: Weigh 420g of water and 420g of premixed dry powder, add them into the stirring pot 8, and stir them at a speed of 60r / min to form a slurry into a uniform slurry.

[0060] Step 3: Stir the slurry at a speed of 60r / min, and let the instrument enter the automatic feeding mode. The instrument measures and calculates the slurry volume through sensor data. For example, at a certain moment, the slurry volume is 100ml (1*10 -4 m3), the speed is 60r / min (6.284rad / s), the K in the formula Fmax=K*ω*V is 0.016rad according to the material characteristic value table. -1 , then Fmax=K*ω*

[0061] V=0.016*6.284*1*10 -4 =10ml / s, the machine adds premixed dry materials into the container at a rate of 10ml / s. If a safety factor of 90% is set, the feed rate is 9ml / s. Keep dynamic calculation and feeding until all the powder materials are added.

[0062] The present invention is described in detail above in conjunction with the embodiments of the accompanying drawings. A person skilled in the art can make various variations of the present invention according to the above description. Therefore, certain details in the embodiments should not constitute a limitation of the present invention, and the scope of protection of the present invention shall be defined by the scope of the attached claims.

Claims

1. A method for preparing an ultra-low water-to-cement ratio cementitious material, characterized in that: The steps include: Providing a stirring apparatus and premixed dry powder, and adding water and a portion of the premixed dry powder into a stirring pot of the stirring apparatus; Starting the stirring device to stir and mix the water and the premixed dry powder to form a slurry; Continue adding the remaining premixed dry powder into the slurry and continue stirring the slurry until all the premixed dry powder has been added; The stirring speed of the stirring device is increased to continue stirring the slurry until there is no powder lump inside the slurry.

2. The method for preparing a super-low water-to-binder ratio cementitious material according to claim 1, characterized in that: When the premixed dry powder is continuously added to the slurry, the addition rate Fmax of the premixed dry powder is: Fmax=K*ω*V Wherein, K is a characteristic parameter for mixing the slurry, ω is the rotation rate of the stirring instrument, and V is the volume of the slurry.

3. The method for preparing a super-low water-to-binder ratio cementitious material according to claim 2, characterized in that: The safe input amount X of the premixed dry powder is: X=Fmax*G Where G is the predetermined safety factor.

4. The method for preparing a super-low water-to-binder ratio cementitious material according to claim 2, characterized in that: The calculation formula of the volume V of the slurry is: V=C*h Wherein C is the cross-sectional area of ​​the stirring pot of the stirring apparatus, and h is the height of the slurry in the stirring pot.

5. The method for preparing a super low water-to-binder ratio cementitious material according to claim 1, characterized in that: Add water and a portion of the premixed dry powder into the stirring pot of the stirring instrument, wherein the ratio of the water to the premixed dry powder is 1:

1.

6. The method for preparing a super-low water-to-binder ratio cementitious material according to claim 1, characterized in that: The stirring instrument is provided with a distance sensor, and the distance sensor measures the height of the slurry in the stirring pot.

7. The method for preparing a super-low water-to-binder ratio cementitious material according to claim 1, characterized in that: A feeding controller is provided on the stirring instrument, and the remaining premixed dry powder is filled into the feeding controller; When the stirring device continuously stirs the slurry, the premixed dry powder is continuously filled into the slurry through the feeding controller.

8. The method for preparing a super-low water-to-binder ratio cementitious material according to claim 1, characterized in that: The stirring instrument is provided with a numerical control display screen.

9. The method for preparing a super-low water-to-binder ratio cementitious material according to claim 1, characterized in that: The stirring instrument is provided with a chip, through which the rate of continuous addition of the premixed dry powder is calculated.

10. The method for preparing a super-low water-to-binder ratio cementitious material according to claim 1, characterized in that: The total amount of the premixed dry powder added and the ratio of the water added to the stirring pot are determined according to actual use requirements.

Citation Information

Patent Citations

  • High speed stirring water, gelled material method for making high-performance concrete

    CN101264643A

  • Agitation method for UHPC and UHPC mixture

    CN108481550A

  • Ultra-high performance concrete mixing device and mixing method thereof

    CN118205104A

  • Concrete feeding and discharging device

    CN220146326U

  • Auto control system for pumping lightweight concrete

    KR1020100138195A