Automatic blow molding processing equipment and process for anti-deformation plastic container
By using automatic blow molding processing equipment in plastic container blow molding technology, the tube blank is cut from the inside by centrifugal force of rotating tubes and arc blades and is subject to targeted cleaning, the impact problem during the cutting process of the tube blank is solved and the molding is ensured. Quality and productivity.
Patent Information
- Application Number
- CN202411234395.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-11-12
AI Technical Summary
In the existing plastic container blow molding technology, the pipe blank is prone to depression and deformation and closing due to impact of external blades during the cutting process, affecting the molding quality.
Using an automatic blow molding processing equipment, the driving gear is driven to rotate through the first motor, and the rotating tube and arc blade are driven to cut the tube blank from the inside under the action of centrifugal force to avoid external impact, and to drive the bidirectional screw to rotate through the second motor. Drive the cover to close and clean the arc blades in a targeted manner to ensure the cleanliness of the cutting components.
Effectively prevent the recesses and deformation and closure of the pipe opening, ensure the smooth progress of blow molding, reduce the adhesion of arc blade residues, and improve production efficiency and molding quality.
Smart Images

Figure CN118927588A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of plastic container processing, in particular to automatic blow molding processing equipment and a process for anti-deformation plastic containers. Background Art
[0002] With the rapid development of modern industry, plastic containers have been widely used in many industries such as food, beverage, medicine, and chemical industry due to their advantages of lightness, durability, and low cost. At present, plastic container blow molding mainly adopts extrusion blow molding, injection blow molding and other methods. In extrusion blow molding, the plastic raw material is first heated and melted and then extruded into a tubular parison, and then the parison is placed in a blow mold, and air is blown into the parison to expand it and fit the mold cavity, thereby forming a plastic container.
[0003] At present, after the semi-molten tubular blank is squeezed into the mold, it is often necessary to use a cutter to cut the tube blank. However, the existing technology often uses a blade to cut horizontally from the outside of the tube blank when cutting the tube blank. However, during the cutting process, the blade first contacts the part of the tube blank, which will impact the tube blank, easily causing the tube blank to sink inward and the tube mouth to deform and close, thereby causing the tube mouth to be unable to dock with the air nozzle, affecting blow molding.
[0004] To this end, the present invention provides an automatic blow molding processing equipment and process for an anti-deformation plastic container. Summary of the invention
[0005] In view of the deficiencies in the prior art, the present invention provides an automatic blow molding processing equipment and process for anti-deformation plastic containers, which solves the problem that the blade cuts off from the outside of the tube blank, which will impact the tube blank and easily cause the tube blank to sink inward and the tube mouth to deform and close.
[0006] To achieve the above objectives, the present invention is implemented through the following technical solutions: an automatic blow molding processing equipment for anti-deformation plastic containers, comprising a base plate, a frame is installed on the top of the base plate, a bracket is installed on the top of the bracket, a moving component is also provided on the top of the base plate, a blowing component and a cleaning component are provided on the inner side of the frame, and a heating component and a cutting component are provided on the bracket; the heating component comprises an extrusion head, a heating rod and an electric push rod, the electric push rod is installed on the top of the bracket, and the output end of the electric push rod movably passes through the top of the bracket and extends downward, and the telescopic end of the electric push rod is installed with a heating rod; the cutting component comprises a first motor and a rotating tube, a support block is installed at the bottom end of the rotating tube, a rotating shaft is symmetrically rotated at the top end of the support block, and an arc-shaped blade is fixedly provided on the outer wall of the rotating shaft; the cleaning component comprises a second motor, a cover body and a water inlet hose, the outer wall of the water inlet hose is fixedly connected with two connecting pipes, and the outer walls of the two connecting pipes are fixedly connected with nozzles.
[0007] Preferably, the moving component includes a longitudinal moving unit installed on the top of the base plate, a moving plate is provided on the top of the longitudinal moving unit, a bidirectional moving unit is provided on the top of the moving plate, a mounting plate is symmetrically provided on the top of the bidirectional moving unit, and molds are installed on the tops of both mounting plates.
[0008] Preferably, the blowing assembly comprises a cylinder, which is fixedly mounted on the top of the frame, and a telescopic end of the cylinder movably passes through the top of the frame and extends downward, and an air nozzle is installed on the telescopic end of the cylinder.
[0009] Preferably, the extrusion head is arranged on the left side of the cylinder, and the extrusion head passes through and is installed on the top of the frame, the outer wall of the extrusion head is provided with a docking port, the top of the extrusion head is provided with a mounting hole, the heating rod is installed on the inner wall of the mounting hole, the heating rod passes through the inner cavity of the extrusion head and extends downward, and the outer wall of the heating rod does not fit the inner wall of the extrusion head, the interior of the heating rod is hollow, and is movably sleeved on the outer wall of the rotating tube.
[0010] Preferably, an extruder is provided on the left side of the bottom plate, and the output end of the extruder is connected to the inner cavity of the extrusion head through a docking port.
[0011] Preferably, the first motor is mounted on a bracket, a driving gear is mounted on the output shaft of the first motor, the rotating tube is mounted on one side surface of the bracket through a bearing seat, a driven gear is mounted on the end of the rotating tube, the driven gear is meshed and connected with the driving gear, a torsion spring is sleeved on the outside of the rotating shaft, the two ends of the torsion spring are respectively fixedly connected to the opposite side surfaces of the arc-shaped blade and the support block, an arc-shaped groove is symmetrically provided on the top of the support block, a limiting rod matched with the arc-shaped groove is fixedly connected to the bottom of the arc-shaped blade, the driven gear, the rotating tube and the support block are arranged to be through-connected from top to bottom, and a movable sleeve is arranged on the outer wall of the heating rod.
[0012] Preferably, the second motor is mounted on an outer wall of one side of the frame, and the output end of the second motor movably passes through the outer wall of the frame and extends inwardly, a bidirectional screw is installed at the output end of the second motor, one end of the bidirectional screw is rotatably installed on the inner wall of the frame, a movable plate is symmetrically threadedly installed on the surface of the bidirectional screw, two guide rods are slidably arranged on the movable plate, and both ends of the guide rods are respectively installed on the inner walls on opposite sides of the frame.
[0013] Preferably, the number of the cover bodies is set to two, and they are fixedly connected to two movable plates respectively, the nozzle penetrates the outer wall of one of the cover bodies and extends inward, a conical bucket is installed at the bottom of one of the cover bodies, and the bottom of the conical bucket is fixedly connected to a drainage hose.
[0014] The present invention also discloses an automatic blow molding process for an anti-deformation plastic container, which specifically comprises the following steps:
[0015] S1. Extrusion: First, plastic particles are added to the extruder. Under the action of high temperature, the plastic particles are melted, and the semi-molten tubular body is extruded downward through the extruder head until the tubular body enters between the two molds;
[0016] S2, mold closing: by operating the bidirectional moving unit, the two molds are brought close to each other for mold closing;
[0017] S3, tube cutting: when the tube is completely put into the mold and the mold is closed, the first motor is started to drive the driving gear to rotate, and the rotating tube is driven to rotate through the driven gear, so that the support block rotates. When the support block rotates, the two arc-shaped blades will be thrown outward under the action of centrifugal force, showing an expanded posture, so that the tube can be cut from the inside;
[0018] S4, Blow molding: The cut tube blank is transported to the bottom of the blowing assembly through the longitudinal moving unit, and the air nozzle is pushed downward by starting the cylinder to make it correspond with the interface on the mold. Then the external air source is injected into the mold through the air nozzle to expand the tube blank to fit the mold cavity, thereby forming the desired shape;
[0019] S5. Mold opening: After blow molding is completed, the two molds are opened by operating the bidirectional moving unit to move the two molds away from each other.
[0020] Preferably, in said S, when the tube is extruded, the electric push rod is started to push the heating rod downward, and the heating rod is inserted into the mold, so that the tube that is continuously extruded and exposed to the external environment can be heated and kept warm, and the heat loss of the tube can be slowed down;
[0021] In S5, when the curved blade is maintained, the second motor is started to drive the bidirectional screw to rotate, driving the two covers to approach each other, and cooperating with the conical bucket to form an inner cavity to cover the curved blade and the support block. The cleaning liquid is pumped out through the nozzle by a high-pressure water pump and flushed towards the curved blade to reduce the adhesion of residues.
[0022] Beneficial Effects
[0023] The present invention provides an automatic blow molding processing equipment and process for anti-deformation plastic containers. Compared with the prior art, it has the following beneficial effects:
[0024] (1) The automatic blow molding processing equipment and process for the anti-deformation plastic container drives the driving gear to rotate through the first motor, and drives the rotating tube to rotate through the driven gear, so that the support block rotates. When the support block rotates, the two arc-shaped blades will be thrown outward under the action of centrifugal force, showing an expanded posture, so that the tube blank can be cut from the inside. This method effectively avoids the impact of the traditional external horizontal cutter on the tube blank, prevents the tube blank from sinking inward and the tube mouth from deforming and closing, ensures that the tube mouth can be smoothly connected with the air nozzle, and ensures the smooth progress of blow molding.
[0025] (2) The automatic blow molding processing equipment and process for the anti-deformation plastic container starts the second motor to drive the two-way screw to rotate and drive the two cover bodies to close together, and cooperate with the conical bucket to form an inner cavity, which completely covers the arc blade and the support block in the cutting component, and can carry out targeted cleaning of the arc blade, effectively reducing the adhesion of residues, which not only ensures the cleanliness of the arc blade, but also reduces the problem of reduced sharpness of the arc blade due to residues.
[0026] (3) The automatic blow molding processing equipment and process of the anti-deformation plastic container, when the tube billet is extruded, the electric push rod is started to push the heating rod into the mold, which can heat and keep the tube billet that is continuously extruded and exposed to the outside. This can keep the tube billet at a suitable temperature, ensure the molding quality, reduce the time for additional adjustment of process parameters due to temperature drop, improve production efficiency, and reduce scrap rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a three-dimensional diagram of the external structure of the present invention;
[0028] Figure 2 It is a three-dimensional structural diagram of the mobile assembly of the present invention;
[0029] Figure 3 It is a three-dimensional structural diagram of the blowing assembly of the present invention;
[0030] Figure 4 is a partial cross-sectional view of the extrusion head of the present invention;
[0031] Figure 5 It is a partial structural exploded view of the present invention;
[0032] Figure 6 It is a partial structural exploded view of the present invention;
[0033] Figure 7 Schematic diagram of the unfolded posture of the arc-shaped blade of the present invention;
[0034] Figure 8 For the present invention Figure 7 A in the enlarged view;
[0035] Fig. 9 It is a three-dimensional structural diagram of the cleaning component of the present invention;
[0036] Fig.10 It is a three-dimensional structural diagram of the nozzle of the present invention.
[0037] In the figure: 1, bottom plate; 11, frame; 12, bracket; 2, moving assembly; 21, longitudinal moving unit; 22, moving plate; 23, bidirectional moving unit; 24, mounting plate; 25, mold; 3, blowing assembly; 31, cylinder; 32, air nozzle; 4, heating assembly; 41, extruder; 42, heating rod; 43, electric push rod; 44, heating rod; 45, docking port; 46, mounting hole; 5, cutting assembly; 51, first motor; 52, main Moving gear; 53, rotating tube; 54, bearing seat; 55, driven gear; 56, supporting block; 57, rotating shaft; 58, arc blade; 59, torsion spring; 510, arc groove; 511, limit rod; 6, cleaning component; 61, second motor; 62, bidirectional screw rod; 63, movable plate; 64, guide rod; 65, cover body; 66, conical bucket; 67, drainage hose; 68, water inlet hose; 69, connecting pipe; 610, nozzle; 7, extruder. DETAILED DESCRIPTION
[0038] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0039] See also Figure 1-10 , the present invention provides two technical solutions:
[0040] Embodiment 1: An automatic blow molding processing equipment for anti-deformation plastic containers, comprising a bottom plate 1, a frame 11 is installed on the top of the bottom plate 1, a bracket 12 is installed on the top of the bracket 11, a moving component 2 is also provided on the top of the bottom plate 1, a blowing component 3 and a cleaning component 6 are provided on the inner side of the frame 11, and a heating component 4 and a cutting component 5 are provided on the bracket 12; the heating component 4 comprises an extrusion head 41, a heating rod 42 and an electric push rod 43, the electric push rod 43 is installed on the top of the bracket 12, and the output end of the electric push rod 43 movably penetrates the bracket 1 2 and extends downward, a heating rod 44 is installed at the telescopic end of the electric push rod 43; the cutting assembly 5 includes a first motor 51 and a rotating tube 53, a support block 56 is installed at the bottom end of the rotating tube 53, a rotating shaft 57 is symmetrically rotated at the top of the supporting block 56, and an arc-shaped blade 58 is fixedly sleeved on the outer wall of the rotating shaft 57; the cleaning assembly 6 includes a second motor 61, a cover body 65 and a water inlet hose 68, the outer wall of the water inlet hose 68 is fixedly connected to two connecting pipes 69, and the outer walls of the two connecting pipes 69 are fixedly connected to nozzles 610.
[0041] In the embodiment of the present invention, the moving component 2 includes a longitudinal moving unit 21 installed on the top of the base plate 1, a moving plate 22 is provided on the top of the longitudinal moving unit 21, a bidirectional moving unit 23 is provided on the top of the moving plate 22, a mounting plate 24 is symmetrically provided on the top of the bidirectional moving unit 23, and molds 25 are installed on the top of the two mounting plates 24. The longitudinal moving unit 21 is mainly composed of linear rails, slides, lead screws and servo motors, which are existing technologies and are used to control the movement of the moving plate 22. The bidirectional moving unit 23 is mainly composed of linear rails, slides, bidirectional lead screws and servo motors, which are existing technologies and are used to control the closing and opening of the two molds 25.
[0042] In the embodiment of the present invention, the blowing assembly 3 includes a cylinder 31, which is fixedly mounted on the top of the frame 11, and the telescopic end of the cylinder 31 movably passes through the top of the frame 11 and extends downward, and the telescopic end of the cylinder 31 is installed with an air nozzle 32, and the cylinder 31 can accurately control the up and down movement of the air nozzle 32.
[0043] In the embodiment of the present invention, the extrusion head 41 is arranged on the left side of the cylinder 31, and the extrusion head 41 passes through and is installed on the top of the frame 11. The outer wall of the extrusion head 41 is provided with a docking port 45, and the top of the extrusion head 41 is provided with a mounting hole 46. The heating rod 42 is installed on the inner wall of the mounting hole 46. The heating rod 42 passes through the inner cavity of the extrusion head 41 and extends downward, and the outer wall of the heating rod 42 does not fit the inner wall of the extrusion head 41. The interior of the heating rod 42 is in a hollow state and is movably sleeved on the outer wall of the rotating tube 53. An extruder 7 is provided on the left side of the bottom plate 1, and the output end of the extruder 7 is connected with the inner cavity of the extrusion head 41 through the docking port 45. When the tube blank is extruded, the electric push rod 43 is started to push the heating rod 44 into the mold 25, so that the tube blank that is continuously extruded and exposed to the outside can be heated and kept warm, which can keep the tube blank at a suitable temperature, ensure the molding quality, reduce the time for additional adjustment of process parameters due to temperature drop, improve production efficiency, and reduce scrap rate.
[0044] In the embodiment of the present invention, the first motor 51 is mounted on the bracket 12, the output shaft of the first motor 51 is mounted with a driving gear 52, the rotating tube 53 is mounted on a side surface of the bracket 12 through a bearing seat 54, a driven gear 55 is mounted on the end of the rotating tube 53, the driven gear 55 is meshed and connected with the driving gear 52, a torsion spring 59 is sleeved on the outside of the rotating shaft 57, and the two ends of the torsion spring 59 are respectively fixedly connected to the arc blade 58 and the opposite side surfaces of the support block 56, the top of the support block 56 is symmetrically provided with an arc groove 510, and the bottom of the arc blade 58 is fixed. A limiting rod 511 is connected to cooperate with the arc groove 510, and the driven gear 55, the rotating tube 53 and the supporting block 56 are arranged to be through-connected from top to bottom, and are movably sleeved on the outer wall of the heating rod 44. When the tube blank completely enters the mold 25 and is closed, the first motor 51 is started to drive the driving gear 52 to rotate, and the rotating tube 53 is driven to rotate through the driven gear 55, so that the supporting block 56 rotates. When the supporting block 56 rotates, the two arc blades 58 will be thrown outward under the action of centrifugal force, showing an expanded posture, so that the tube blank can be cut from the inside. This method effectively avoids the impact of the traditional external horizontal cutter on the tube blank, prevents the tube blank from sinking inward and the tube mouth from deforming and closing, ensures that the tube mouth can be smoothly docked with the air nozzle 32, and ensures the smooth progress of blow molding. When the support block 56 no longer rotates, the centrifugal force will not act on the arc blade 58. Under the action of the torsion spring 59, the arc blade 58 retracts inward and returns to its original position. Through the cooperation of the arc groove 510 and the limit rod 511, the arc blade 58 is limited to avoid over-travel of rotation.
[0045] In the embodiment of the present invention, the second motor 61 is mounted on an outer wall of one side of the frame 11, and the output end of the second motor 61 movably penetrates the outer wall of the frame 11 and extends inwardly. A bidirectional screw rod 62 is mounted on the output end of the second motor 61, and one end of the bidirectional screw rod 62 is rotatably mounted on the inner wall of the frame 11. A movable plate 63 is symmetrically threadedly mounted on the surface of the bidirectional screw rod 62, and two guide rods 64 are slidably arranged on the movable plate 63. The two ends of the guide rod 64 are respectively mounted on the inner walls of the opposite sides of the frame 11. The number of cover bodies 65 is set to two, and they are respectively fixedly connected to the two movable plates 63. The nozzle 610 penetrates the outer wall of one of the cover bodies 65 and extends inwardly. A conical bucket 66 is installed at the bottom of one of the covers 65, and a drainage hose 67 is fixedly connected to the bottom of the conical bucket 66. The conical bucket 66 cooperates with the drainage hose 67 to facilitate the discharge of waste water after cleaning. By starting the second motor 61 to drive the two-way screw 62 to rotate and drive the two covers 65 to close to each other, and cooperate with the conical bucket 66 to form an inner cavity, which completely covers the arc blade 58 and the support block 56 in the cutting assembly 5, and can carry out targeted cleaning of the arc blade 58, effectively reducing the adhesion of residues. This not only ensures the cleanliness of the arc blade 58, but also reduces the problem of reduced sharpness of the arc blade 58 due to residues.
[0046] Example 2: Please refer to Figure 1-10 , compared with the first embodiment, the difference is:
[0047] The present invention also discloses a method for using an automatic blow molding processing device for an anti-deformation plastic container, which specifically comprises the following steps:
[0048] S1, extrusion: First, plastic particles are added to the extruder 7. Under the action of high temperature, the plastic particles are melted, and the semi-molten tubular mold is extruded downward through the extrusion head 41 until the tubular mold enters between the two molds 25;
[0049] S2, mold closing: by operating the bidirectional moving unit 23, the two molds 25 are brought closer to each other for mold closing;
[0050] S3, tube blank cutting: when the tube blank is completely entered into the mold 25 and the mold is closed, the first motor 51 is started to drive the driving gear 52 to rotate, and the rotating tube 53 is driven to rotate through the driven gear 55, so that the support block 56 rotates. When the support block 56 rotates, the two arc-shaped blades 58 are thrown outward under the action of centrifugal force, showing an expanded posture, so that the tube blank can be cut from the inside;
[0051] S4, blow molding: the cut tube blank is transported to the bottom of the blowing assembly 3 by the longitudinal moving unit 21, and the air nozzle 32 is pushed downward by starting the cylinder 31 to make it correspond with the interface on the mold 25, and then the external air source is injected into the mold 25 through the air nozzle 32, so that the tube blank expands and fits the mold cavity of the mold 25, thereby forming the desired shape;
[0052] S5, mold opening: After the blow molding is completed, the two molds 25 are moved away from each other by operating the bidirectional moving unit 23 to open the mold.
[0053] In the embodiment of the present invention, when the tube blank is extruded in S1, the electric push rod 43 is started to push the heating rod 44 downward, and the heating rod 44 is inserted into the mold 25, so that the tube blank that is continuously extruded and exposed to the external environment can be heated and kept warm, and the heat loss of the tube blank can be slowed down;
[0054] After the mold is opened in S5, when the curved blade 58 needs to be maintained, the water inlet hose 68 is connected to the external cleaning liquid source, the drainage hose 67 is connected to the wastewater recovery device, and the mold 25 is moved to a safe position without interfering with the movement of the cover body 65. At the same time, the equipment no longer extrude the tube blank outward, and then, by starting the second motor 61 to drive the bidirectional screw 62 to rotate, the two cover bodies 65 are driven to approach each other, and after the two cover bodies 65 are closed, they are combined with the conical bucket 66 to form an inner cavity. At this time, the curved blade 58 and the support block 56 in the cutting assembly 5 are completely covered, and the cleaning liquid is pumped out through the nozzle 610 by a high-pressure water pump, and the curved blade 58 is rinsed to reduce the adhesion of residues.
[0055] Meanwhile, the contents not described in detail in this specification belong to the prior art known to those skilled in the art.
[0056] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0057] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. An automatic blow molding processing equipment for anti-deformation plastic containers, comprising a bottom plate (1), a frame (11) is installed on the top of the bottom plate (1), a bracket (12) is installed on the top of the bracket (11), a moving component (2) is also provided on the top of the bottom plate (1), a blowing component (3) and a cleaning component (6) are provided on the inner side of the frame (11), and a heating component (4) and a cutting component (5) are provided on the bracket (12); The heating assembly (4) comprises an extrusion head (41), a heating rod (42) and an electric push rod (43), wherein the electric push rod (43) is mounted on the top of the bracket (12), and the output end of the electric push rod (43) movably passes through the top of the bracket (12) and extends downward, and the telescopic end of the electric push rod (43) is mounted with a heating rod (44); The cutting assembly (5) comprises a first motor (51) and a rotating tube (53), a supporting block (56) is installed at the bottom end of the rotating tube (53), a rotating shaft (57) is symmetrically rotated at the top end of the supporting block (56), and an arc-shaped blade (58) is fixedly sleeved on the outer wall of the rotating shaft (57); The cleaning assembly (6) comprises a second motor (61), a cover body (65) and a water inlet hose (68); the outer wall of the water inlet hose (68) is fixedly connected to two connecting pipes (69); and the outer walls of the two connecting pipes (69) are fixedly connected to a nozzle (610).
2. The automatic blow molding equipment for anti-deformation plastic containers according to claim 1, Features: The moving assembly (2) comprises a longitudinal moving unit (21) mounted on the top of the base plate (1); a moving plate (22) is provided on the top of the longitudinal moving unit (21); a bidirectional moving unit (23) is provided on the top of the moving plate (22); mounting plates (24) are symmetrically provided on the top of the bidirectional moving unit (23); and molds (25) are installed on the tops of the two mounting plates (24).
3. The automatic blow molding equipment for anti-deformation plastic containers according to claim 1, Features: The blowing assembly (3) comprises a cylinder (31), wherein the cylinder (31) is fixedly mounted on the top of the frame (11), and the telescopic end of the cylinder (31) movably penetrates the top of the frame (11) and extends downward, and an air nozzle (32) is mounted on the telescopic end of the cylinder (31).
4. The automatic blow molding equipment for anti-deformation plastic containers according to claim 1, Features: The extrusion head (41) is arranged on the left side of the cylinder (31), and the extrusion head (41) passes through and is installed on the top of the frame (11). The outer wall of the extrusion head (41) is provided with a docking port (45), and the top of the extrusion head (41) is provided with a mounting hole (46). The heating rod (42) is installed on the inner wall of the mounting hole (46). The heating rod (42) passes through the inner cavity of the extrusion head (41) and extends downward, and the outer wall of the heating rod (42) does not fit the inner wall of the extrusion head (41). The interior of the heating rod (42) is hollow and is movably sleeved on the outer wall of the rotating tube (53).
5. The automatic blow molding equipment for anti-deformation plastic containers according to claim 4, Features: An extruder (7) is provided on the left side of the bottom plate (1), and the output end of the extruder (7) is connected to the inner cavity of the extrusion head (41) through a docking port (45).
6. The automatic blow molding equipment for anti-deformation plastic containers according to claim 1, Features: The first motor (51) is mounted on the bracket (12); the output shaft of the first motor (51) is mounted with a driving gear (52); the rotating tube (53) is mounted on a side surface of the bracket (12) through a bearing seat (54); a driven gear (55) is mounted on the end of the rotating tube (53); the driven gear (55) is meshedly connected with the driving gear (52); a torsion spring (59) is sleeved on the outside of the rotating shaft (57); the two ends of the torsion spring (59) are respectively fixedly connected to the opposite side surfaces of the arc-shaped blade (58) and the supporting block (56); the top of the supporting block (56) is symmetrically provided with an arc-shaped groove (510); the bottom of the arc-shaped blade (58) is fixedly connected with a limiting rod (511) matched with the arc-shaped groove (510); the driven gear (55), the rotating tube (53) and the supporting block (56) are arranged to be through-connected from top to bottom, and are movably sleeved on the outer wall of the heating rod (44).
7. The automatic blow molding equipment for anti-deformation plastic containers according to claim 1, Features: The second motor (61) is mounted on an outer wall of one side of the frame (11); an output end of the second motor (61) movably penetrates the outer wall of the frame (11) and extends inward; a bidirectional screw rod (62) is mounted on the output end of the second motor (61); one end of the bidirectional screw rod (62) is rotatably mounted on the inner wall of the frame (11); a movable plate (63) is symmetrically threadedly mounted on the surface of the bidirectional screw rod (62); two guide rods (64) are slidably arranged on the movable plate (63); and two ends of the guide rods (64) are respectively mounted on the inner walls of opposite sides of the frame (11).
8. The automatic blow molding equipment for anti-deformation plastic containers according to claim 7, Features: The number of the cover bodies (65) is set to two, and they are fixedly connected to the two movable plates (63) respectively. The nozzle (610) penetrates the outer wall of one of the cover bodies (65) and extends inward. A conical bucket (66) is installed at the bottom of one of the cover bodies (65), and a drainage hose (67) is fixedly connected to the bottom of the conical bucket (66).
9. An automatic blow molding process for anti-deformation plastic containers. Features: The automatic blow molding processing equipment for the anti-deformation plastic container according to any one of claims 1 to 8 specifically comprises the following steps: S1, extrusion: first, plastic particles are added to the extruder (7), and under the action of high temperature, the plastic particles are melted, and the semi-molten tubular body is extruded downward through the extrusion head (41) until the tubular body enters between the two molds (25); S2, mold closing: by operating the bidirectional moving unit (23), the two molds (25) are brought close to each other for mold closing; S3, tube blank cutting: when the tube blank is completely inserted into the mold (25) and the mold is closed, the first motor (51) is started to drive the driving gear (52) to rotate, and the rotating tube (53) is driven to rotate through the driven gear (55), so that the support block (56) rotates. When the support block (56) rotates, the two arc-shaped blades (58) are thrown outward under the action of centrifugal force, showing an expanded posture, so that the tube blank can be cut from the inside; S4, blow molding: the cut tube blank is transported to the bottom of the blowing assembly (3) by the longitudinal moving unit (21), and the air nozzle (32) is pushed downward by starting the cylinder (31) so that it can correspond to the interface on the mold (25), and then the external air source is injected into the mold (25) through the air nozzle (32), so that the tube blank expands and fits the mold cavity (25), thereby forming a desired shape; S5, mold opening: After the blow molding is completed, the two molds (25) are moved away from each other by operating the bidirectional moving unit (23) to open the mold.
10. The automatic blow molding process for an anti-deformation plastic container according to claim 9, Features: In S1, when the tube is extruded, the electric push rod (43) is started to push the heating rod (44) downward, and the heating rod (44) is inserted into the mold (25), so that the tube that is continuously extruded and exposed to the external environment can be heated and kept warm, thereby slowing down the heat loss of the tube; In S5, when the arc-shaped blade (58) is maintained, the second motor (61) is started to drive the bidirectional screw (62) to rotate, thereby driving the two covers (65) to approach each other and cooperate with the conical bucket (66) to form an inner cavity to cover the arc-shaped blade (58) and the support block (56). A high-pressure water pump is used to pump out the cleaning liquid through the nozzle (610) and rinse the arc-shaped blade (58) to reduce the adhesion of residues.
Citation Information
Cited By
Automatic blow molding processing equipment and method for anti-deformation plastic container
CN122058524A