Inkjet ink composition, inkjet recording method, and inkjet recording apparatus

By using more than 4 OH groups of sugar alcohols, diols with 2 or 3 carbon atoms and low content of glycerol in inkjet ink, and sublimation transfer and drying treatment at specific temperatures, the current situation is solved There are problems of ink smoke and dryness in the technology, and efficient image transfer effect is achieved.

CN118931261APending Publication Date: 2024-11-12SEIKO EPSON CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410576814.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-11
Filing Date
2024-05-10
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing sublimation transfer ink containing glycerol is prone to smoke when heated, and the high boiling point of the sugar alcohol-based ink causes insufficient dryness of the transfer medium, and the image is easily transferred to the back surface.

Method used

The inkjet ink composition containing 4 or more OH groups, a diol having 2 or 3 carbon atoms, a permeable moisturizer and a low content of glycerol are used, and the inkjet ink composition is 150°C or more and 220°C or less. Sublimation transfer is performed at temperature, combining drying and winding processes above 50°C.

Benefits of technology

It effectively suppresses smoke generation, improves the dryness of paper and the color rendering of image, and ensures that the image is transferred in the correct position and is not easy to produce printing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure HDA0004832682170000011
    Figure HDA0004832682170000011
  • Figure HDA0004832682170000021
    Figure HDA0004832682170000021
  • Figure HDA0004832682170000031
    Figure HDA0004832682170000031
Patent Text Reader

Abstract

The invention provides an ink jet ink composition, an ink jet recording method and an ink jet recording apparatus which have low smoke generation and good dryness on paper. An inkjet ink composition includes: a sublimable dye; a sugar alcohol having four or more OH groups; dihydric alcohol, the number of carbon atoms being 2 or 3; a permeable humectant selected from one or more of glycol monoethers, dihydric alcohols having 4 or more carbon atoms, amides, and (poly) glyceryl ethers; and glycerol in an amount of 1 mass% or less relative to the total mass.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an inkjet ink composition, an inkjet recording method and an inkjet recording device. Background Art

[0002] The inkjet recording method is a method of recording by ejecting small droplets of ink from a fine nozzle and attaching them to a recording medium. This method has the characteristic that it can record high-resolution and high-quality images at high speed using a relatively inexpensive device. In addition, the inkjet recording method can also be used to dye (print and dye) cloth, etc.

[0003] As a recording method, there is a transfer type recording method using a sublimation dye. In this recording method, after the inkjet ink composition is attached to a transfer medium (paper, etc.) as a transfer source, the dye is transferred from the transfer medium to a transfer destination medium for dyeing without directly attaching the inkjet ink composition to the recording medium of the transfer object.

[0004] In the recording method by transfer, a sublimation dye is mixed with an inkjet ink composition, the composition is temporarily attached to a medium of a transfer source, and then the sublimation dye is sublimated by, for example, steam or heat to dye the recording medium of the recording object. As such a composition for sublimation transfer, for example, Patent Documents 1 to 3 disclose a composition containing a sublimation dye, wherein the sublimation dye contains glycerol or sugar alcohol.

[0005] Prior art literature

[0006] Patent Literature

[0007] Patent Document 1: International Publication No. 2005 / 121263

[0008] Patent Document 2: Japanese Patent Application Publication No. 2004-107647

[0009] Patent Document 3: Japanese Patent Application Publication No. 2004-107648 Summary of the invention

[0010] Technical problem to be solved by the invention

[0011] However, in sublimation transfer inks containing glycerol, glycerol may evaporate due to heating during sublimation transfer, cool in the air and reach a condensation point, thereby generating smoke from minute droplets. In addition, in sublimation transfer inks containing sugar alcohol instead of glycerol, since sugar alcohol has a high boiling point, the drying of the transfer medium surface may be insufficient, and the image may be transferred to the back side when the medium is rolled up.

[0012] Technical solutions to solve problems

[0013] In one embodiment of the inkjet ink composition according to the present invention, the composition comprises:

[0014] Sublimation dyes;

[0015] Sugar alcohols, with more than 4 OH groups;

[0016] Diols (diols), with 2 or 3 carbon atoms;

[0017] A penetrating moisturizer selected from the group consisting of glycol monoethers, diols having 4 or more carbon atoms, amides, and (poly)glycerol ethers; and

[0018] The content of glycerol is 1% by mass or less based on the total mass of the composition.

[0019] In one embodiment of the inkjet recording method according to the present invention, the method comprises:

[0020] A recording step of attaching the inkjet ink composition to a sheet-like recording medium;

[0021] a transfer step of placing the recording surface of the recording medium on an object to be dyed, heating the recording medium at a temperature of 150° C. to 220° C. to transfer the sublimation dye to the object to be dyed by sublimation; and

[0022] The peeling step is to peel the recording medium from the dyeing object after the image transfer.

[0023] In one embodiment of the inkjet recording method according to the present invention, the method comprises:

[0024] A recording step of attaching any of the above-mentioned inkjet ink compositions to a sheet-like recording medium;

[0025] a drying step of heating the recording medium to which the inkjet ink composition is attached at a temperature of 50° C. or higher; and

[0026] In the recovery step, the dried recording medium is wound into a roll.

[0027] In one embodiment of the inkjet recording device according to the present invention, the device comprises:

[0028] An inkjet head that allows the inkjet ink composition to adhere to a sheet-like recording medium;

[0029] a heater for heating the sheet-like recording medium at a temperature of 50° C. or higher; and

[0030] The recording medium is wound into a roll. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1is a table (Table 1) illustrating osmotic moisturizers.

[0032] Figure 2 This is a schematic diagram of an example of an inkjet recording device.

[0033] Figure 3 Table 2 describes the components of the inkjet ink compositions of Examples.

[0034] Figure 4 Table 3 describes the components of the inkjet ink compositions of Examples.

[0035] Figure 5 Table 4 shows the components of the inkjet ink compositions of Examples.

[0036] Figure 6 Table 5 describes the components of the inkjet ink composition of the comparative example.

[0037] Figure 7 Table 6 shows the evaluation results of Examples and Comparative Examples.

[0038] Description of Reference Numerals

[0039] 1: recording device; 2: recording head; 3: IR heater; 4: paper pressing heater; 5: post heater; 6: cooling fan; 7: preheater; 8: ventilation fan; 9: supply roller; 10: winding roller; M: recording medium (intermediate transfer medium). DETAILED DESCRIPTION

[0040] The following describes the embodiments of the present invention. The embodiments described below are used to illustrate examples of the present invention. The present invention is not limited to any of the following embodiments, and various variations of the embodiments are also included within the scope of not changing the gist of the present invention. In addition, all structures described below are not necessarily necessary structures of the present invention.

[0041] 1. Inkjet ink composition

[0042] The inkjet ink composition involved in this embodiment includes: a sublimating dye; a sugar alcohol having more than 4 OH groups; a diol having 2 or 3 carbon atoms; a penetrating moisturizer selected from one or more of glycol monoethers, diols having more than 4 carbon atoms, amides and (poly)glycerol ethers; and glycerol, which is 1% by mass or less relative to the total mass of the composition.

[0043] 1.1. Sublimation dyes

[0044] The inkjet ink composition of the present embodiment contains a sublimation dye (hereinafter also referred to as "sublimation dye" or "sublimation-type dye"). Sublimation dyes are dyes suitable for dyeing hydrophobic synthetic fibers such as polyester, nylon, and acetate, and are compounds that are insoluble or poorly soluble in water. In addition, sublimation dyes are dyes that have the property of sublimating by heating. There are no particular restrictions on the sublimation dyes used in the inkjet ink composition of the present embodiment, and specifically, the following dyes can be cited.

[0045] As sublimation dyes, disperse dyes and solvent dyes having the above-mentioned properties can be used. Specific examples of such dyes include CI Disperse Yellow 3, 7, 8, 23, 39, 51, 54, 60, 71, 86; CI Disperse Orange 1, 1:1, 5, 20, 25, 25:1, 33, 56, 76; CI Disperse Brown 2; CI Disperse Red 11, 50, 53, 55, 55:1, 59, 60, 65, 70, 75, 93, 146, 158, 190, 190:1, 207, 239, 240; CI Vat Red 41; CI Disperse Violet 8, 17, 23, 27, 28, 29, 36, 57; CI Disperse Blue 19, 26, 26:1, 35, 55, 56, 58, 64, 64:1, 72, 72:1, 81, 81:1, 91, 95, 108, 131, 141, 145, 359; CI Solvent Blue 36, 63, 105, 111, etc. These may be used alone or in combination of two or more.

[0046] Among the dyes exemplified above, from the viewpoint of storage stability of the inkjet ink composition, the inkjet ink composition of this embodiment is more preferably CI Disperse Yellow 3, 7, 8, 23, 51, 54, 60, 71, 86; CI Disperse Orange 20, 25, 25:1, 56, 76; CI Disperse Brown 2; CI Disperse Red 11, 53, 55, 55:1, 59, 60, 65, 70, 75, 146, 190 , 190:1, 207, 239, 240; CI Vat Red 41; CI Disperse Violet 8, 17, 23, 27, 28, 29, 36, 57; CI Disperse Blue 26, 26:1, 55, 56, 58, 64, 64:1, 72, 72:1, 81, 81:1, 91, 95, 108, 131, 141, 145, 359; CI Solvent Blue 36, 63, 105, 111, etc.

[0047] The sublimation dyes exemplified above are all compounds that are insoluble or poorly soluble in water, but can be well dispersed in water as long as they are within a specific concentration range, for example, by a dispersant described later. In addition, the sublimation dyes exemplified above have some differences in dispersibility or solubility, respectively. That is, depending on the type of the sublimation dye, the appropriate concentration range of the dispersant is different, and the solubility achieved by the dispersant is also different.

[0048] The sublimation dyes exemplified above may be used alone or in combination of two or more.

[0049] The total content of the sublimation dye is 10% by mass or less, preferably 0.1% by mass or more and 10% by mass or less, more preferably 0.2% by mass or more and 9.0% by mass or less, and further preferably 0.3% by mass or more and 8.0% by mass or less, relative to 100% by mass of the inkjet ink composition.

[0050] When the content of the sublimation dye is 0.1% by mass or more, the color development (OD value) of the obtained dyed product (transfer destination) tends to be more excellent. In addition, when the content of the sublimation dye is 10% by mass or less, the ejection stability tends to be good.

[0051] The sublimation dye can be dispersed by a dispersant. The dispersant has the function of dispersing the sublimation dye in the inkjet ink composition. The dispersant is not particularly limited, and examples thereof include anionic dispersants, nonionic dispersants, and polymer dispersants (resin dispersants).

[0052] As the anionic dispersant, preferably, there can be mentioned a formaldehyde condensate of an aromatic sulfonic acid. Examples of the "aromatic sulfonic acid" in the formaldehyde condensate of an aromatic sulfonic acid include creosote sulfonic acid, cresol sulfonic acid, phenol sulfonic acid, alkylnaphthalenesulfonic acids such as β-naphthalenesulfonic acid, methylnaphthalenesulfonic acid, and butylnaphthalenesulfonic acid, a mixture of β-naphthalenesulfonic acid and β-naphthalenesulfonic acid, a mixture of cresolsulfonic acid and 2-naphthol-6-sulfonic acid, lignin sulfonic acid and its salts, and the like.

[0053] As the anionic dispersant, formaldehyde condensates of β-naphthalenesulfonic acid, formaldehyde condensates of alkylnaphthalenesulfonic acid, formaldehyde condensates of creosote sulfonic acid, and salts thereof are preferred, and sodium salts are more preferred.

[0054] Examples of the nonionic dispersant include ethylene oxide adducts of phytosterol and ethylene oxide adducts of cholesterol.

[0055] Among them, commercially available products of naphthalenesulfonic acid-based dispersants include DemolNL: naphthalenesulfonic acid, manufactured by Kao Corporation, DemolMS, DemolN, DemolRN, DemolRN-L, DemolSC-30, DemolSN-B, DemolSS-L, DemolT, and DemolT-45.

[0056] Examples of polymer dispersants (also referred to as "resin dispersants") include acrylic resins and salts thereof such as polyacrylic acid, acrylic acid-acrylonitrile copolymers, acrylic acid-acrylate copolymers, vinyl acetate-acrylate copolymers, vinyl acetate-acrylic acid copolymers, styrene-acrylic acid copolymers, styrene-methacrylic acid copolymers, styrene-methacrylic acid-acrylate copolymers, styrene-α-methylstyrene-acrylic acid copolymers, styrene-α-methylstyrene-acrylic acid-acrylate copolymers, and vinylnaphthalene-acrylic acid copolymers; styrene-acrylic acid copolymers, styrene-methacrylic acid copolymers, and styrene-methacrylic acid-acrylate copolymers. Styrene resins and their salts such as acrylate copolymers, styrene-α-methylstyrene-acrylic acid copolymers, styrene-α-methylstyrene-acrylic acid-acrylate copolymers, styrene-maleic acid copolymers, and styrene-maleic anhydride copolymers; polymer compounds (resins) containing carbamate bonds formed by the reaction of isocyanate groups and hydroxyl groups, which may be linear and / or branched, and are irrelevant to the presence or absence of cross-linked structures, and their salts; polyvinyl alcohols and their salts; polyvinyl pyrrolidones and their salts; vinylnaphthalene-maleic acid copolymers and their salts; vinyl acetate-maleic acid ester copolymers and their salts; and vinyl acetate-crotonic acid copolymers and their salts, etc.

[0057] Commercially available products of styrene-based resin dispersants include, for example, X-200, X-1, X-205, and X-220 (manufactured by Starlight PMC Co., Ltd.). Commercially available products of acrylic resin dispersants include BYK-190, BYK-187, BYK-191, BYK-194N, and BYK-199 (manufactured by BYK-Chemie Co., Ltd.). Commercially available products of urethane-based resin dispersants include BYK-184, BYK-182, BYK-183, and BYK-185 (manufactured by BYK-Chemie Co., Ltd.).

[0058] Dispersants can be used alone or in combination. The total content of the dispersants is 0.1% by mass and 30% by mass relative to 100% by mass of the inkjet ink composition, preferably 0.5% by mass and 25% by mass, more preferably 1% by mass and 20% by mass, and further preferably 1.5% by mass and 15% by mass. The dispersion stability of the sublimation dye can be obtained by having a content of more than 0.1% by mass. In addition, if the content of the dispersant is less than 30% by mass, the sublimation dye will not be dissolved too much, and the viscosity can be suppressed to be small.

[0059] Among the dispersants exemplified above, it is further preferred to be selected from resin dispersants, particularly at least one of acrylic resins, styrene resins and urethane resins. In addition, in this case, the weight average molecular weight of the dispersant is further preferably above 500. By using such a resin dispersant as a dispersant, the dispersion stability of the sublimation dye can be further improved.

[0060] 1.2. Sugar alcohols

[0061] The inkjet ink composition of the present embodiment contains sugar alcohols having 4 or more OH groups (hereinafter also referred to as "hydroxyl groups" or "hydroxyl groups"). Examples of such sugar alcohols include sugars generated by reducing the carbonyl group of an aldose or ketose. Examples of such sugar alcohols include maltitol, lactitol, tetitol, pentitol, hexitol, erythritol, sorbitol, xylitol, mannitol, and inositol. Among these, more preferably, one or more selected from D-sorbitol, erythritol, and D-mannitol.

[0062] The molecular weights of some of the sugar alcohols exemplified above are described.

[0063] · Erythritol 122

[0064] ·Xylitol 152

[0065] ·D-Sorbitol 182

[0066] ·Lactitol 344

[0067] The viscosity (unit: mPa·s) of a 60 mass % aqueous solution of several sugar alcohols among the sugar alcohols exemplified above is described.

[0068] ·Xylitol 24.3

[0069] ·D-Sorbitol 32.8

[0070] In addition, the "60 mass % aqueous solution viscosity" means that a 60 mass % aqueous solution of each sugar alcohol was prepared and measured using a rheometer MCR302e (manufactured by Anton Paar) at a shear rate of 200 s.-1 The viscosity at 20° C. was measured. In addition, erythritol has a high viscosity and cannot be made into an aqueous solution, so it cannot be measured.

[0071] The surface tensions (unit: mN / m) of 10% by mass aqueous solutions of some of the sugar alcohols exemplified above are described.

[0072] ·Xylitol 74.1

[0073] ·D-Sorbitol 73.5

[0074] In addition, "surface tension of 10 mass % aqueous solution" shows the value of the surface tension at 20°C measured by preparing a 10 mass % aqueous solution of each sugar alcohol and using a surface tensiometer DY-300 (manufactured by Kyowa Interface Science Co., Ltd.).

[0075] The sugar alcohols exemplified above may be used alone or in combination of two or more. When the inkjet ink composition contains sugar alcohols, smoke generation can be reduced, and clogging recovery and image color development properties can be improved.

[0076] In addition, among sugar alcohols, it is more preferable to use a sugar alcohol having a viscosity of 35 mPa·s or less in a 60% by mass aqueous solution, more preferably 33 mPa·s or less, and even more preferably 30 mPa·s or less. When the viscosity of a 60% by mass aqueous solution of sugar alcohols is 35 mPa·s or less, the influence of the evaporation thickening property of the sugar alcohol can be further reduced, and the intermittent ejection stability can be further improved.

[0077] The content of the sugar alcohol is preferably 3% by mass or more and 15% by mass or less, more preferably 3% by mass or more and 13% by mass or less, further preferably 3% by mass or more and 11% by mass or less, and further preferably 4% by mass or more and 7% by mass or less, relative to the total mass of the inkjet ink composition. When the content of the sugar alcohol is within this range, clogging recovery, color development, and intermittent ejection stability can be better balanced.

[0078] 1.3. Diols with 2 or 3 carbon atoms

[0079] The inkjet ink composition involved in this embodiment contains a diol having 2 or 3 carbon atoms. Examples of the diol having 2 or 3 carbon atoms include ethylene glycol, 1,2-propanediol (propylene glycol), 1,3-propylene glycol, etc. Among these, propylene glycol is more preferably used. In addition, the inkjet ink composition may contain multiple types of these.

[0080] The inkjet ink composition contains a diol having 2 or 3 carbon atoms, thereby improving the drying property on the paper surface and reducing the influence of evaporation thickening property, thereby further improving the intermittent ejection stability.

[0081] The content of the diol having 2 or 3 carbon atoms in the inkjet ink composition is preferably 5% by mass or more and 15% by mass or less, more preferably 6% by mass or more and 14% by mass or less, and even more preferably 7% by mass or more and 13% by mass or less, relative to the total mass of the inkjet ink composition. When the content of the diol having 2 or 3 carbon atoms in the inkjet ink composition is within such a range, smoke generation can be further suppressed, and paper surface drying and intermittent ejection can be further improved.

[0082] 1.4. Penetrating moisturizers

[0083] The inkjet ink composition according to the present embodiment contains one or more penetrating moisturizing agents selected from glycol monoethers, diols having 4 or more carbon atoms, amides, and (poly)glycerol ethers.

[0084] The inkjet ink composition contains a penetrating moisturizer, which can improve the drying property of an image formed by the inkjet ink composition and improve the intermittent ejection stability. In addition, in this specification, a penetrating moisturizer is distinguished from a moisturizer, but the permeability of a penetrating moisturizer is not an essential characteristic, and moisturizers with low or no permeability are referred to as penetrating moisturizers.

[0085] In Table 1, penetrating moisturizers are exemplified.

[0086] In Table 1, the surface tension of a 10 mass % aqueous solution of each osmotic moisturizing agent is shown by preparing a 10 mass % aqueous solution and measuring the result using a surface tensiometer DY-300 (manufactured by Kyowa Interface Science Co., Ltd.).

[0087] The inkjet ink composition may contain an osmotic moisturizing agent other than those listed in Table 1. In addition, a plurality of osmotic moisturizing agents may be used. The surface tension of a 10 mass % aqueous solution of the osmotic moisturizing agent is preferably 45 mN / m or more and 67 mN / m or less, more preferably 46 mN / m or more and 65 mN / m or less, and further preferably 50 mN / m or more and 64 mN / m or less.

[0088] When the surface tension of the 10 mass % aqueous solution is within such a range, the color development, intermittent ejection stability, paper surface drying and clogging recovery of the inkjet ink composition are further improved. In addition, when it is within such a range, since the surface tension is more appropriate, the permeability is more appropriate and the color development of the obtained image is better. Moreover, since the viscosity and / or evaporation thickening property are also improved, the clogging recovery and / or intermittent ejection stability are also improved.

[0089] The content of the penetrating moisturizing agent is preferably 10% by mass or less, more preferably 7% by mass or less, and further preferably 5% by mass or less relative to the total mass of the inkjet ink composition. In addition, the lower limit of the content of the penetrating moisturizing agent is preferably 0.3% by mass or more, more preferably 0.5% by mass or more, and more preferably 1% by mass or more. By containing such a degree of penetrating moisturizing agent, the clogging recovery property and the color development property of the image of the inkjet ink composition can be made more excellent. In addition, the storage stability of the inkjet ink composition can also be made excellent.

[0090] More preferably, the penetrating moisturizer includes (poly)glycerol ethers. Examples of (poly)glycerol ethers include propylene glycol or polyglycerol alkylene oxide adducts. (Poly)glycerol ethers, i.e., polyglycerol ethers or glycerol ethers, have less fuming properties and are more likely to suppress fuming during transfer. For example, Uniox G-450, Uniox G-750, SC-E750, SC-E350, and SC-P750 shown in Table 1 can obtain the following results.

[0091] The fuming property of a 30% by weight aqueous solution was evaluated as follows. A 30% by weight aqueous solution of each (poly)glycerol ether was prepared, 10 drops of which were dropped onto a polyester 100% cloth Carl Dry (manufactured by Toray Industries, Ltd.) using a polyethylene pipette, and then the mixture was heated at 200°C for 40 seconds and 465 g / cm2 using a table-top automatic sublimation transfer press AF-54TEN (manufactured by Itsumi Co., Ltd.). 2 The pressure was increased to visually evaluate whether smoke was generated. As a result, Uniox G-450, Uniox G-750, SC-E750, SC-E350, and SC-P750 did not generate smoke.

[0092] One reason for this effect is believed to be the molecular weight of the (poly)glycerol ethers. From this viewpoint, when (poly)glycerol ethers are used, the weight average molecular weight is preferably 280 to 900, more preferably 300 to 800, and more preferably 350 to 750. In addition, from the viewpoints of the viscosity of the solution or the rate of increase in the viscosity of the solution when it is dried, the upper limit of the weight average molecular weight is preferably within the above range.

[0093] 1.5. Glycerol

[0094] The inkjet ink composition of the present embodiment contains glycerol in an amount of 1% by mass or less relative to the total mass. The inkjet ink composition does not contain glycerol in an amount exceeding 1% by mass relative to the total mass.

[0095] In the inkjet ink composition, glycerol is preferably not contained in an amount exceeding 0.5% by mass, and more preferably not contained in an amount exceeding 0.1% by mass. In addition, glycerol may or may not be contained in the inkjet ink composition, and when contained, the content is below the above content.

[0096] When the content of glycerol is within the above range, the inkjet ink composition is less likely to generate smoke and can exhibit excellent paper surface drying properties.

[0097] 1.6. Other ingredients

[0098] The inkjet ink composition may contain the following components in addition to the above components.

[0099] 1.6.1. Surfactants

[0100] The inkjet ink composition may contain a surfactant. The surfactant is not particularly limited, and examples thereof include acetylene glycol surfactants, fluorine surfactants, and silicone surfactants.

[0101] The acetylene glycol surfactant is not particularly limited, and examples thereof include Surfynol 104, 104E, 104H, 104A, 104BC, 104DPM, 104PA, 104PG-50, 104S, 420, 440, 465, 485, SE, SE-F, 504, 61, DF37, CT111, CT121, CT131, CT136, TG, GA, and DF110D (all trade names, Air Products Japan Co., Ltd.), Olfine B, Y, P, A, STG, SPC, E1004, E1010, PD-001, PD-002W, PD-003, PD-004, EXP.4001, EXP.4036, EXP.4051, AF-103, AF-104, AK-02, SK-14, AE-3 (all of the above are trade names, manufactured by Nissin Chemical Industry Co., Ltd.), Acetylenol E00, E00P, E40, E100 (all of the above are trade names, manufactured by Kawaken Fine Chemicals Co., Ltd.).

[0102] As the fluorine surfactant, a fluorine-modified polymer is preferably used, and a specific example thereof includes BYK-340 (trade name, manufactured by BYK-Chemie Japan Ltd.).

[0103] The silicone surfactant is not particularly limited, but preferably a polysiloxane compound can be cited. The polysiloxane compound is not particularly limited, but for example, a polyether-modified organosiloxane can be cited. Commercially available products of the polyether-modified organosiloxane include, for example, BYK-306, BYK-307, BYK-333, BYK-341, BYK-345, BYK-346, BYK-348 (the above are trade names, manufactured by BYK Chemical Japan Co., Ltd.), KF-351A, KF-352A, KF-353, KF-354L, KF-355A, KF-615A, KF-616A, KF-617A, KF-618A, KF-619A, KF-620A, KF-621B, KF-622C, KF-623D, KF-624E, KF-625F, KF-626A, KF-627A, KF-628A, KF-629A, KF-630A, KF-631B, KF-632A, KF-633 F-945, KF-640, KF-642, KF-643, KF-6020, X-22-4515, KF-6011, KF-6012, KF-6015, KF-6017 (the above are trade names, manufactured by Shin-Etsu Chemical Co., Ltd.), Silface SAG503A, Silface SAG014 (the above are trade names, manufactured by Nissin Chemical Co., Ltd.), etc.

[0104] The above-mentioned surfactants may be used alone or in combination of two or more.

[0105] When a surfactant is contained, the content thereof is preferably 0.1% by mass or more and 1.5% by mass or less relative to the total mass of the inkjet ink composition.

[0106] 1.6.2. Polyglycerols and betaines

[0107] The inkjet ink composition may further include at least one selected from polyglycerols and betaines. Polyglycerols and betaines have the property of being moisturizers, but in this specification, polyglycerols and betaines are distinguished as substances different from the above-mentioned penetrating moisturizers.

[0108] Examples of glycerols include dipropylene glycol S (manufactured by Sakamoto Yakuin Kogyo Co., Ltd.) (weight average molecular weight: 166, 60% aqueous solution viscosity: 20.8, 10% aqueous solution surface tension: 72.5), R-PG (manufactured by Sakamoto Yakuin Kogyo Co., Ltd.) (weight average molecular weight: 240, 60% aqueous solution viscosity: 29), polyglycerol #310 (manufactured by Sakamoto Yakuin Kogyo Co., Ltd.) (weight average molecular weight: 310, 60% aqueous solution viscosity: 22.8), etc.

[0109] Betaines are compounds that have positive and negative charges at non-adjacent positions in the same molecule, are not bonded to dissociable hydrogen atoms with positive charges, can form intramolecular salts, and have no charge as a whole molecule. In this embodiment, the positively charged site of betaines is preferably a quaternary ammonium cation.

[0110] There are no particular restrictions on betaines, and examples thereof include trialkylglycines such as trimethylglycine and triethylglycine, γ-butyrylbetaine, hominisine, trigonelline, carnitine, homoserine betaine, valine betaine, lysine betaine, ornithine betaine, alanine betaine, stachydrine, and glutamic acid betaine. Among them, the glycines contained in the inkjet ink composition are preferably selected from trialkylglycines, and more preferably trimethylglycine. Trialkylglycine is a compound formed by replacing three nitrogen atoms of glycine with an alkyl group. As a result, there is a tendency for the clogging recovery to be further improved. In addition, betaines can be used alone or in combination of two or more.

[0111] When polyglycerols and betaines are used, their total content is preferably 2.5% by mass to 9.5% by mass, more preferably 3% by mass to 8% by mass, and even more preferably 4% by mass to 8% by mass, relative to the total mass of the inkjet ink composition.

[0112] In addition, polyglycerols sometimes contain glycerol as an impurity, and when added in large quantities, smokiness sometimes occurs. In addition, when betaines are solid, when the amount added is large, clogging recovery is sometimes poor. From these viewpoints, it is preferred to make the content within the above range.

[0113] Polyglycerols and betaines have low evaporation thickening properties. Since the inkjet ink composition contains at least one of polyglycerols and betaines, the intermittent ejection stability can be improved by adding a small amount of them. In addition, the flight deflection or non-ejection of the inkjet ink composition caused by drying of the inkjet ink composition on the nozzle of the inkjet head can be suppressed, and the clogging recovery property can be excellent.

[0114] 1.6.3. Water

[0115] The inkjet ink composition of this embodiment may be an aqueous composition containing water. An "aqueous" composition refers to a composition in which water is one of the main solvents. Examples of water include pure water such as ion exchange water, ultrafiltration water, reverse osmosis water, and distilled water, and water with reduced ionic impurities such as ultrapure water. In addition, when water is sterilized by ultraviolet irradiation or addition of hydrogen peroxide, the generation of bacteria or fungi can be suppressed when the inkjet ink composition is stored for a long time.

[0116] The content of water is 30% by mass or more, preferably 40% by mass or more, more preferably 45% by mass or more, and further preferably 50% by mass or more, relative to the total amount (100% by mass) of the inkjet ink composition. The upper limit of the content of water is preferably 97% by mass or less, further preferably 90% by mass or less, further preferably 85% by mass or less, and further preferably 80% by mass or less, relative to the total amount (100% by mass) of the ink composition.

[0117] 1.6.4. Other ingredients

[0118] The inkjet ink composition of the present embodiment may contain various additives such as an organic solvent, a chelating agent, a rust inhibitor, a mildew inhibitor, an antioxidant, a reduction inhibitor, and an evaporation accelerator, as necessary.

[0119] 1.7. Manufacturing and physical properties

[0120] From the viewpoint of further improving the quality of images achieved by inkjet, the surface tension (static surface tension) of the inkjet ink composition of the present embodiment at 20° C. is preferably 18 mN / m or more and 40 mN / m or less, more preferably 20 mN / m or more and 35 mN / m or less, and even more preferably 22 mN / m or more and 33 mN / m or less. The surface tension can be measured, for example, by using an automatic surface tensiometer CBVP-Z (trade name, manufactured by Kyowa Interface Science Co., Ltd.) to confirm the surface tension when a platinum plate is wetted by the inkjet ink composition under an environment of 20° C.

[0121] From the same viewpoint, the viscosity of the inkjet ink composition at 20° C. is preferably 3 mPa·s or more and 10 mPa·s or less, and more preferably 3 mPa·s or more and 8 mPa·s or less. In addition, the viscosity can be measured, for example, using a viscoelasticity tester MCR-300 (trade name, manufactured by Pysica) to measure the viscosity at 20° C.

[0122] The inkjet ink composition is obtained by mixing the above-mentioned components in an arbitrary order and removing impurities by filtering or the like as needed. As a method for mixing the components, it is preferable to use a method in which the materials are added sequentially in a container having a stirring device such as a mechanical stirrer or a magnetic stirrer and stirred and mixed. As a filtering method, centrifugal filtration, filter filtration, etc. can be performed as needed.

[0123] 1.8. Effects

[0124] According to the inkjet ink composition of this embodiment, the sugar alcohol containing 4 or more OH groups is not easy to volatilize at a temperature of 220°C or less, and is not easy to generate smoke when heated. In addition, according to the inkjet ink composition, by combining a diol having 2 or 3 carbon atoms with high drying properties and low viscosity and a penetrating moisturizer, low smoke generation and paper surface drying properties can be achieved. In addition, according to the inkjet ink composition, since the content of glycerol is 1% by mass or less, smoke generation is suppressed.

[0125] 2. Inkjet recording method

[0126] 2.1. First embodiment

[0127] The inkjet recording method involved in this embodiment includes: a recording step, making the above-mentioned inkjet ink composition adhere to a sheet-like recording medium (intermediate transfer medium); a transfer step, making the recording surface of the recording medium (intermediate transfer medium) overlap with the dyed object (recorded medium), heating at a temperature of not less than 150°C and not more than 220°C, and sublimatingly transferring the sublimation dye to the dyed object (recorded medium); and a peeling step, peeling the recording medium (intermediate transfer medium) from the dyed object (recorded medium) after the image transfer.

[0128] The above-mentioned inkjet ink composition can be applied to a dyeing method (sublimation transfer inkjet recording method) for fabrics etc. by sublimation transfer. The inkjet recording method of the present embodiment can also be referred to as a method for producing a dyed article.

[0129] The inkjet recording method (method for producing a dyed article) of the present embodiment comprises: a step of attaching an inkjet ink composition to a recording surface of a recording medium; a step of arranging a recording medium on the recording surface of the recording medium; a step of heating the recording medium and the recording medium; and a step of peeling off the recording medium (intermediate transfer medium) from the dyed object (recorded medium). In other words, the inkjet recording method (method for producing a dyed article) of the present embodiment comprises: a recording step of applying the inkjet ink composition to the intermediate transfer medium using an inkjet method; a transfer step of heating the intermediate transfer medium applied with the ink composition in a state where the surface applied with the ink composition faces the dyed surface of the dyed article, so that the sublimation dye is transferred to the dyed article; and a peeling step of peeling off the recording medium (intermediate transfer medium) from the dyed object (recorded medium) after the image is transferred. Each step is described below.

[0130] <Recording process>

[0131] In this step, the inkjet ink composition is applied to the recording surface of the intermediate transfer medium (first recording medium) using the inkjet method. The inkjet ink composition can be ejected using a droplet ejection device (eg, an inkjet recording device described below).

[0132] As a method of ejecting droplets (inkjet method), a pressure method or a method of ejecting ink by heating the ink to generate bubbles (air bubbles) can be used, but from the viewpoint of the ease of deterioration of the ink composition, the pressure method is preferred. In addition, according to the inventor's research, it is known that in a recording head of a thin film pressure method, the shear rate applied to the inkjet ink composition is 100s -1 This is a more preferred shear rate in the inkjet ink composition of this embodiment.

[0133] As the intermediate transfer medium, sheet-shaped recording media can be cited, for example, paper such as ordinary paper, recording media provided with an ink receiving layer (referred to as special paper for inkjet, coated paper, etc.), etc., and more preferably paper provided with an ink receiving layer made of inorganic particles such as silicon dioxide. Thus, an intermediate record can be obtained that suppresses penetration of the recording surface during the drying process of the inkjet ink composition given to the intermediate transfer medium. In addition, if such a medium is used, it is further easy to leave a sublimation dye on the surface of the recording surface, and in the subsequent transfer process, the sublimation of the sublimation dye can be carried out more efficiently.

[0134] In this step, a variety of inkjet ink compositions can be used, thereby, for example, making it possible to expand the expressible color gamut.

[0135] <Transfer process>

[0136] Then, the recording surface of the intermediate transfer medium to which the ink composition is applied is heated in a state facing the object to be dyed (a state in which the second recording medium is arranged on the recording surface of the first recording medium), so that the sublimation dye constituting the inkjet ink composition is transferred to the object to be dyed. Thus, a dyed object using a cloth or the like as the object to be dyed is obtained.

[0137] The heating temperature in this step is 150° C. to 220° C., preferably 160° C. to 210° C. This can provide sufficient energy for transferring the sublimation dye to the dyed object, and can improve the productivity of the dyed object.

[0138] The heating time in this operation also depends on the heating temperature, but is more than 30 seconds and less than 90 seconds, preferably more than 45 seconds and less than 60 seconds.Thus, it is possible to obtain sufficient energy for making the sublimation dye transfer to the dyed article, and it is possible to make the productivity of the dyed article especially excellent.

[0139] In addition, this step can be performed by heating the intermediate transfer medium provided with the ink composition in a state opposite to the object to be dyed, and more preferably by heating the intermediate transfer medium in a state where the intermediate transfer medium and the object to be dyed are in close contact with each other, thereby, for example, a more vivid image can be recorded (dyed) on the second recording medium.

[0140] As the object to be dyed, for example, a sheet-like object such as cloth (hydrophobic fiber cloth, etc.) or a resin (plastic) film is suitably used. However, an object having a three-dimensional shape such as a sphere or a rectangular parallelepiped may be used in addition to the sheet-like shape.

[0141] In addition, as the dyed object, for example, glass, metal, and ceramic may be used in addition to resins and plastics. As the fibers constituting the cloth as the dyed object, for example, polyester fibers, nylon fibers, triacetate fibers, diacetate fibers, polyamide fibers, and blends of two or more of these fibers may be cited. In addition, blends of these with regenerated fibers such as rayon or natural fibers such as cotton, silk, and wool may also be used.

[0142] In addition, as the resin (plastic) film, the dyed object may include, for example, polyester film, polyurethane film, polycarbonate film, polyphenylene sulfide film, polyimide film, polyamide-imide film, etc. The resin (plastic) film may be a laminated body formed by laminating a plurality of layers, or may be composed of a gradient material in which the composition of the material changes obliquely.

[0143] <Peeling process>

[0144] In this step, after the image is transferred in the above-mentioned transfer step, the recording medium (intermediate transfer medium) is peeled off from the dyed object (recording medium). The peeling method is not particularly limited, and it can be performed using an appropriate device.

[0145] According to the inkjet recording method of the present embodiment, since the sublimation transfer temperature is 150° C. or higher and 220° C. or lower, volatilization of sugar alcohol is suppressed, and generation of smoke is suppressed.

[0146] 2.2. Second embodiment

[0147] The inkjet recording method according to the present embodiment includes: a recording step of attaching the inkjet ink composition to a sheet-like recording medium; a drying step of heating the recording medium to which the inkjet ink composition is attached at a temperature of 50° C. or higher; and a recovery step of winding the dried recording medium into a roll.

[0148] Since the recording process in the inkjet recording method of this embodiment is the same as the recording process of the first embodiment described above, the description thereof will be omitted.

[0149] <Drying process>

[0150] In the drying step, the recording medium (intermediate transfer medium) to which the inkjet ink composition has been attached in the recording step is heated at a temperature of 50° C. or higher. The heating method is not particularly limited, and for example, the heating can be performed using a post heater of the inkjet recording apparatus described below.

[0151] <Recycling Process>

[0152] In the recovery step, the recording medium (intermediate transfer medium) that has been dried in the drying step is wound into a roll. The recovery step can be performed using an appropriate winding device.

[0153] <Other Processes>

[0154] The inkjet recording method of this embodiment can further include a transfer process, a stripping process, etc. As the transfer process and the stripping process are the same as those of the first embodiment described above, description thereof is omitted. In this embodiment, the intermediate transfer medium is wound into a roll shape and then used in the transfer process. Thus, the degree of freedom of the process for obtaining printed and dyed articles can be increased.

[0155] According to the inkjet recording method of this embodiment, the drying process is performed by heating at a temperature of 50° C. or higher, and the diol evaporates, so that the paper surface is dry and the smoke generation during transfer can be suppressed. In addition, since the above-mentioned inkjet ink composition is used, the paper surface is dry in the drying process performed by heating at a temperature of 50° C. or higher, and it is difficult to produce print-through even if it is wound into a roll.

[0156] 3. Inkjet recording device

[0157] The above-mentioned inkjet ink composition can be applied to an inkjet recording device. The inkjet recording device at least has an ink storage container (ink cartridge, storage tank, etc.) for storing the above-mentioned inkjet ink composition and a recording head connected thereto, and is not particularly limited as long as the above-mentioned inkjet ink composition can be ejected from the recording head and an image can be formed on an intermediate transfer medium (transfer paper, etc.).

[0158] As the inkjet recording device of this embodiment, either a serial type or a line type can be used. In these types of inkjet recording devices, a recording head is mounted, and while changing the relative positional relationship between the recording medium (intermediate transfer medium) and the recording head, droplets of the inkjet ink composition can be ejected from the nozzle holes of the recording head at a predetermined timing (intermittently) and a predetermined volume (mass), so that the inkjet ink composition adheres to the recording medium (intermediate transfer medium) to form a predetermined image.

[0159] Here, in a serial type inkjet recording device, the conveying direction of the recording medium intersects with the direction of the reciprocating motion of the recording head, and the relative positional relationship between the recording medium and the recording head is changed by combining the reciprocating motion of the recording head and the conveying motion of the recording medium (including the reciprocating motion). In addition, in this case, a plurality of nozzle holes (holes for ejecting the ink composition) are usually arranged on the recording head, and a row of nozzle holes (nozzle row) is formed along the conveying direction of the recording medium. In addition, a plurality of nozzle rows may be formed on the recording head depending on the type or quantity of the ink composition.

[0160] In addition, in a line-type inkjet recording device, the recording head does not reciprocate, and the relative positional relationship between the recording medium and the recording head is changed by conveying the recording medium. In this case, a plurality of nozzle holes are usually arranged on the recording head, and a row of the nozzle holes (nozzle row) is formed in a direction intersecting the conveying direction of the recording medium.

[0161] The inkjet recording method uses a serial or line type inkjet recording device, but as long as the ink composition can be ejected as droplets through fine nozzle holes and the droplets can be attached to the recording medium, there is no particular limitation. For example, as a droplet ejection method (inkjet method), a pressure method or a method of ejecting the ink by heating the ink to generate bubbles (bubbles) can be used, but from the viewpoint of the ease of deterioration of the ink composition, the pressure method is preferred.

[0162] In the inkjet recording apparatus used in the present embodiment, for example, a heating unit, a drying unit, a roller unit, a winding device, and other well-known structures can be adopted without limitation.

[0163] An example of a recording device applicable to the inkjet recording method of this embodiment is described below. Figure 2 , a schematic cross-sectional view of an inkjet recording device according to one embodiment is shown. Figure 2 As shown, the recording device 1 includes a supply roller 9 , a recording head 2 , an IR heater 3 , a platen heater 4 , a post heater 5 , a cooling fan 6 , a preheater 7 , a ventilation fan 8 , and a winding roller 10 .

[0164] The inkjet ink composition is ejected from the recording head 2 onto the recording medium M (intermediate transfer medium) fed by the supply roller 9. As the recording head 2, a conventionally known method can be used. As an example of a known method, for example, a method of ejecting droplets by vibration of a piezoelectric element, that is, a recording head that forms ink droplets by mechanical deformation of an electrostrictive element can be cited. The recording head 2 can eject ink dots of the inkjet ink composition in multiple sizes from one nozzle, for example.

[0165] In the above-mentioned drying process, the recording medium (intermediate transfer medium) is heated after the recording process, and the process can be performed by the post-heater 5 in the recording device 1. In addition, although not shown in the figure, units such as a hot air mechanism (not shown) and a constant temperature bath (not shown) can be used. The post-heater 5 heats and dries the recording medium (intermediate transfer medium) to which the inkjet ink composition is attached. The post-heater 5 heats the recording medium (intermediate transfer medium) on which the image is recorded, so that the water contained in the inkjet ink composition evaporates and disperses more quickly, thereby suppressing penetration, etc. The heating of the recording medium (intermediate transfer medium) by the post-heater 5 is preferably above 50°C, and more preferably above 60°C and below 110°C.

[0166] The recording device 1 also includes an IR heater 3 that directly heats the recording head 2 or a platen heater 4 that heats the recording head 2 via a recording medium (intermediate transfer medium).

[0167] When the IR heater 3 is used, the recording medium (intermediate transfer medium) can also be heated from the recording head 2 side. Thus, the recording head 2 is also easily heated at the same time, but compared with the case where the pressure heater 4 or the like heats from the back side of the recording medium (intermediate transfer medium), the temperature can be increased without being affected by the thickness of the recording medium (intermediate transfer medium). In addition, when the pressure heater 4 is used, the recording medium (intermediate transfer medium) can be heated from the side opposite to the recording head 2 side. Thus, the recording head 2 is less likely to be heated.

[0168] In addition, the above-mentioned "heating the recording medium (intermediate transfer medium)" means raising the temperature of the recording medium (intermediate transfer medium) to a desired temperature, and is not limited to directly heating the recording medium (intermediate transfer medium). The recording device 1 may have a cooling fan 6. After drying, by cooling the ink composition on the recording medium (intermediate transfer medium) by the cooling fan 6, there is a tendency that a coating can be formed on the recording medium (intermediate transfer medium) with good adhesion.

[0169] In addition, the recording device 1 may include a preheater 7 for preheating (preheating) the recording medium (intermediate transfer medium) before ejecting the ink composition onto the recording medium (intermediate transfer medium). Furthermore, the recording device 1 may include a ventilation fan 8 in order to more efficiently dry the ink composition attached to the recording medium (intermediate transfer medium).

[0170] Recording is performed, and the recording medium M (intermediate transfer medium) that has undergone the drying process is wound up by the winding roller 10. In addition, the recording device 1 may not have the winding roller 10, for example, the recording medium M (intermediate transfer medium) that has undergone the drying process may be conveyed to a transfer device (not shown) to enter a transfer process and a peeling process.

[0171] 4. Examples and Comparative Examples

[0172] The present invention will be specifically described below with reference to the examples, but the present invention is not limited to these examples. In the following, unless otherwise specified, "part" and "%" are by mass. In addition, unless otherwise specified, the evaluation is performed under an environment of a temperature of 25.0°C and a relative humidity of 40.0%.

[0173] 4.1. Preparation of inkjet ink composition

[0174] The components were placed in a container to form the compositions shown in Tables 2 to 5, mixed and stirred for 2 hours using a magnetic stirrer, and then filtered using a membrane filter having a pore size of 5 μm to obtain inkjet ink compositions of Examples 1 to 24 and Comparative Examples 1 to 5. The numerical values ​​in the tables represent mass %.

[0175] In Tables 2 to 5, the details of the components described by trade names, abbreviations, etc. are as follows.

[0176] Uniox G-450: Glyceryl ethers: manufactured by NOF Corporation

[0177] ·SannixGP-250: Glyceryl ether: Made by Sanyo Chemical Industries, Ltd.

[0178] SC-E350: Polyglycerol ether: manufactured by Sakamoto Pharmaceutical Industry Co., Ltd.

[0179] SC-P750: Polyglycerol ether: manufactured by Sakamoto Pharmaceutical Industry Co., Ltd.

[0180] · Wilbride S-753: Glyceryl ether: Made by NOF Corporation

[0181] · Polyglycerol #310: Polyglycerols: manufactured by Sakamoto Pharmaceutical Industry Co., Ltd.

[0182] BYK-348: Silicone surfactant: manufactured by BYK Chemical Japan Ltd.

[0183] The dye dispersion 1 described in the table was prepared as follows.

[0184] <Dye Dispersion 1 (Surfactant Dispersion)>

[0185] A mixture of Kayaset Red B (CI Disperse Red 60, manufactured by Nippon Kayaku Co., Ltd.) (30 parts) as a sublimation dye, Lavelin RTMW-40 (40% aqueous solution of formaldehyde condensate of creosote sulfonate, manufactured by Daiichi Kogyo Seiyaku Co., Ltd.) (45 parts) as an anionic dispersant, NIKKOL RTMBPS-30 (EO (ethylene oxide) 30 mol adduct of phytosterol, manufactured by Nikko Chemical Co., Ltd.) (2 parts) as a nonionic dispersant, and ion-exchanged water (23 parts) was subjected to a dispersion treatment for about 15 hours by a sand mill using glass beads of 0.2 mm diameter under cooling. After adding ion-exchanged water (100 parts) to the liquid after the dispersion treatment to adjust the dye content to 15%, the mixture was filtered using glass fiber filter paper GC-50 (manufactured by Toyo Roshi Co., Ltd., filter pore size: 0.5 μm), thereby obtaining a dye dispersion liquid 1.

[0186] The dye dispersion 2 described in the table was prepared as follows.

[0187] <Dye Dispersion Liquid 2 (Resin Dispersion)>

[0188] 20 parts of JoncrylRTM678 (manufactured by BASF) were added to a mixture of 48% lithium hydroxide (3.2 parts), ion exchanged water (56.8 parts) and propylene glycol (20 parts), and the mixture was heated to 90 to 120°C and stirred for 5 hours to obtain an emulsion of JoncrylRTM678. A mixture of Kayaset Red B (manufactured by Nippon Kayaku Co., Ltd., CI Disperse Red 60) (30 parts) as a sublimation dye, the emulsion of JoncrylRTM678 (60 parts), ProxelRTMGXL (0.2 parts), Surfynol104PG50 (0.4 parts) and ion exchanged water (24 parts) was dispersed for about 15 hours by a sand mill using glass beads with a diameter of 0.2 mm under cooling. Ion exchange water (60 parts) and the emulsion of JoncrylRTM678 (30 parts) were added to the liquid after the dispersion treatment, and the dye content was adjusted to 15%. The liquid was filtered using glass fiber filter paper GC-50 (manufactured by Toyo Roshi Co., Ltd., filter pore size: 0.5 μm) to obtain dye dispersion 2.

[0189] The properties of the materials used in Examples and Comparative Examples are described below.

[0190] ·Xylitol: 60% aqueous solution viscosity = 24.3 mPa·s

[0191] ·D-Sorbitol: 60% aqueous solution viscosity = 32.8 mPa·s

[0192] ·Erythritol: 60% aqueous solution viscosity = insoluble

[0193] Propylene glycol: 60% aqueous solution viscosity = 9.8 mPa·s; 10% aqueous solution surface tension = 62.7 mN / m

[0194] 1,3-Propanediol: 60% aqueous solution viscosity = 8.7 mPa·s; 10% aqueous solution surface tension = 67.8 mN / m

[0195] Uniox G-450: Weight average molecular weight = 450; Surface tension of 10% aqueous solution = 63.7 mN / m

[0196] SannixGP-250: Weight average molecular weight = 250; Surface tension of 10% aqueous solution = 49.6 mN / m

[0197] SC-E350: weight average molecular weight = 350; surface tension of 10% aqueous solution = 58.6 mN / m SC-P750: weight average molecular weight = 750; surface tension of 10% aqueous solution = 46.1 mN / m Wilbride S-753: weight average molecular weight = 950; surface tension of 10% aqueous solution = 43.3 mN / m

[0198] · Triethylene glycol monomethyl ether: 10% aqueous solution surface tension = 60.6 mN / m

[0199] ·Diethylene glycol monobutyl ether: 10% aqueous solution surface tension = 35.0 mN / m ·Triethylene glycol: 10% aqueous solution surface tension = 66.0 mN / m

[0200] 1,2-Butanediol: Surface tension of 10% aqueous solution = 53.7 mN / m

[0201] ·ε-caprolactam: Surface tension of 10% aqueous solution = 54.1 mN / m

[0202] Glycerol: 60% aqueous solution viscosity = 11.4 mPa·s

[0203] Polypropylene glycol #310: 60% aqueous solution viscosity = 22.8 mPa·s

[0204] ·Trimethylglycine: 60% aqueous solution viscosity = 15.1 mPa·s

[0205] Evaluation methods

[0206] 4.2.1. Paper surface dryness

[0207] The inkjet ink compositions of Examples and Comparative Examples were used to transfer the sublimation transfer paper EPSON DS Transfer Multi-Purpose (manufactured by Seiko Epson Corporation) using PX-G930 (manufactured by Seiko Epson Corporation) at an ink adhesion amount of 8±0.5 mg / inch. 2 A full-screen pattern was printed in a manner. After a predetermined time, the printed surface was gently wiped with a Bemcot, and the presence or absence of transfer was visually evaluated. The evaluation was performed according to the following criteria, and the results are recorded in Table 6.

[0208] A: No transfer occurs 120 seconds after printing

[0209] B: Transfer occurs 120 seconds after printing, but not 150 seconds

[0210] C: Transfer occurs even 150 seconds after printing

[0211] 4.2.2. Smoking

[0212] The inkjet ink compositions of Examples and Comparative Examples were used to transfer the sublimation transfer paper EPSON DS Transfer Multi-Purpose (manufactured by Seiko Epson Corporation) using PX-G930 (manufactured by Seiko Epson Corporation) at an ink adhesion amount of 8±0.5 mg / inch. 2 Then, the full pattern was printed by using a desktop automatic sublimation transfer press AF-54TEN (manufactured by Itsumi Co., Ltd.) at 200°C for 40 seconds at 465 g / cm 2 The transfer was performed onto a polyester 100% cloth Carl·Dry (Toray Industries, Inc.) by applying a pressure of , and the smoke generation after the transfer was visually evaluated. The evaluation was performed according to the following criteria, and the results are recorded in Table 6.

[0213] A: No smoke is generated after transfer

[0214] B: Smoke is generated after transfer, but disappears within 5 seconds

[0215] C: Smoke is generated after transfer and lasts for more than 5 seconds

[0216] 4.2.3. Intermittent spraying stability

[0217] Using the inkjet ink compositions of the examples and comparative examples, the head voltage was adjusted to a dot weight of 6±0.5 ng using PX-G930 (manufactured by Seiko Epson Corporation), and 700 idle runs were performed with the pre-ejection off. Then, a nozzle check pattern was printed to evaluate the presence or absence of ink droplet landing deviation. The evaluation was performed according to the following criteria, and the results are recorded in Table 6.

[0218] AA: No missing or distorted dots

[0219] A: Less than 80% of nozzles are distorted

[0220] B: More than 80% of the nozzles are distorted

[0221] C: More than 50% of the nozzles do not spray

[0222] 4.2.4. Blockage recovery

[0223] After filling the ink of each example into PX-G930 (manufactured by Seiko Epson Corporation), the lid was opened and placed in a constant temperature room at a temperature of 40°C and a humidity of 20% for 5 days. After that, the cleaning operation was performed three times at room temperature (the ink suction amount was 4g, 2g, and 2g, respectively), and the number of nozzles that did not recover was counted. The evaluation was performed according to the following criteria, and the results are recorded in Table 6.

[0224] A: No unrecovered nozzles

[0225] B: More than 1 and less than 10 nozzles have not been restored

[0226] C: More than 11 nozzles have not been restored

[0227] 4.2.5. Color rendering

[0228] The inkjet ink compositions of Examples and Comparative Examples were used to transfer the sublimation transfer paper EPSON DS Transfer Multi-Purpose (manufactured by Seiko Epson Corporation) using PX-G930 (manufactured by Seiko Epson Corporation) at an ink adhesion amount of 8±0.5 mg / inch. 2 Then, the full pattern was printed by using a desktop automatic sublimation transfer press AF-54TEN (manufactured by Itsumi Co., Ltd.) at 200°C for 40 seconds at 465 g / cm 2 The OD value on the fabric was measured by applying a pressure of 100% polyester Carl Dry (Toray Industries, Inc.). The measurement conditions were light source D65 and concentration state T. The evaluation was performed according to the following criteria, and the results are recorded in Table 6.

[0229] AA: OD value is above 1.55

[0230] A: OD value is 1.50 or more and less than 1.55

[0231] B: OD value is 1.45 or more and less than 1.50

[0232] C: OD value is less than 1.45

[0233] Evaluation results

[0234] It can be seen from Tables 2 to 6 that the inkjet ink compositions of each embodiment comprising: a sublimable dye; a sugar alcohol having 4 or more OH groups; a diol having 2 or 3 carbon atoms; a penetrating moisturizer selected from one or more of glycol monoethers, diols having 4 or more carbon atoms, amides and (poly)glycerol ethers; and glycerol in an amount of 1 mass % or less relative to the total mass of the composition have good paper drying properties and are not prone to smoking.

[0235] The present invention includes structures that are substantially the same as the structures described in the embodiments, for example, structures with the same functions, methods and results or structures with the same purposes and effects. In addition, the present invention includes structures that replace non-essential parts of the structures described in the embodiments. In addition, the present invention includes structures that can achieve the same effects as the structures described in the embodiments or structures that achieve the same purposes. In addition, the present invention includes structures that add known technologies to the structures described in the embodiments.

[0236] The following contents are derived from the above-mentioned embodiment and modification examples.

[0237] The inkjet ink composition comprises:

[0238] Sublimation dyes;

[0239] Sugar alcohols, with more than 4 OH groups;

[0240] Diols, with 2 or 3 carbon atoms;

[0241] A penetrating moisturizer selected from one or more of glycol monoethers, diols having 4 or more carbon atoms, amides and (poly)glycerol ethers; and

[0242] The content of glycerol is 1% by mass or less based on the total mass of the inkjet ink composition.

[0243] According to the inkjet ink composition, sugar alcohols containing 4 or more OH groups are not easily volatilized at a temperature of 220°C or less, and are not easily smoked when heated. In addition, according to the inkjet ink composition, by using a diol having 2 or 3 carbon atoms with high drying properties and low viscosity and a penetrating moisturizer in combination, low smoke generation and paper surface drying properties can be achieved. In addition, according to the inkjet ink composition, smoke generation is suppressed because the content of glycerol is 1% by mass or less.

[0244] In the above inkjet ink composition,

[0245] The surface tension of a 10 mass % aqueous solution of the osmotic moisturizing agent may be 45 mN / m or more and 67 mN / m or less.

[0246] According to the inkjet ink composition, color development, intermittent ejection stability and clogging recovery are more excellent. Since the surface tension is more appropriate, the permeability is more appropriate, and the color development of the obtained image is better. In addition, since the viscosity and / or evaporation thickening property are also better, the clogging recovery and / or intermittent ejection stability are also better.

[0247] In the above inkjet ink composition,

[0248] The content of the penetrating moisturizing agent may be 5% by mass or less relative to the total mass of the inkjet ink composition.

[0249] The inkjet ink composition has better clogging recovery and color development properties and also has excellent storage stability.

[0250] In the above inkjet ink composition,

[0251] At least one selected from polyglycerols and betaines may be further included.

[0252] The inkjet ink composition has better intermittent ejection stability. Polyglycerols and betaines have low evaporation thickening properties, and the intermittent ejection stability can be improved by adding a small amount of them.

[0253] In the above inkjet ink composition,

[0254] The content of the diol having 2 or 3 carbon atoms may be 5% by mass or more and 15% by mass or less based on the total mass of the inkjet ink composition.

[0255] According to this inkjet ink composition, smoke generation can be further suppressed, and paper surface drying properties and intermittent ejection can also be further improved.

[0256] In the above inkjet ink composition,

[0257] The viscosity of a 60 mass % aqueous solution of the sugar alcohol may be 35 mPa·s or less.

[0258] According to this inkjet ink composition, the ink is less susceptible to the evaporation thickening property of sugar alcohol, and the intermittent ejection stability is further improved.

[0259] In the above inkjet ink composition,

[0260] The content of the sugar alcohol may be 3% by mass or more and 15% by mass or less relative to the total mass of the inkjet ink composition.

[0261] According to the inkjet ink composition, in addition to the above-mentioned effects, clogging recovery property, color development property, and intermittent ejection stability can be well balanced.

[0262] In the above inkjet ink composition,

[0263] The penetrating moisturizer may comprise (poly)glycerol ethers.

[0264] According to this inkjet ink composition, smoke generation is reduced and the above-mentioned effects are made more remarkable.

[0265] In the above inkjet ink composition,

[0266] The weight average molecular weight of the (poly)glyceryl ethers may be 300 or more and 800 or less.

[0267] According to this inkjet ink composition, smoke generation can be further suppressed, and the color development property of the image can be further improved.

[0268] Inkjet recording methods include:

[0269] A recording step of attaching any of the above-mentioned inkjet ink compositions to a sheet-like recording medium;

[0270] a transfer step of placing the recording surface of the sheet-like recording medium on an object to be dyed, heating the recording surface at a temperature of 150° C. to 220° C. to transfer the sublimation dye to the object to be dyed by sublimation; and

[0271] The peeling step is to peel the sheet-like recording medium from the dyeing object after the image transfer.

[0272] According to this inkjet recording method, since the sublimation transfer temperature is 150° C. or higher and 220° C. or lower, volatilization of sugar alcohol is suppressed and generation of smoke is suppressed.

[0273] Inkjet recording methods include:

[0274] A recording step of attaching any of the above-mentioned inkjet ink compositions to a sheet-like recording medium;

[0275] a drying step of heating the sheet-like recording medium to which the inkjet ink composition is attached at a temperature of 50° C. or higher; and

[0276] In the recovery step, the dried sheet-shaped recording medium is wound into a roll.

[0277] According to the inkjet recording method, the drying step of heating at a temperature of 50° C. or higher causes the glycol to evaporate, so that the paper surface dries well and smoke generation during transfer can be suppressed. In addition, since the above-mentioned inkjet ink composition is used, the paper surface dries well and print-through is unlikely to occur.

[0278] The inkjet recording device comprises:

[0279] An inkjet head that allows any of the above inkjet ink compositions to adhere to a sheet-like recording medium;

[0280] a heater for heating the sheet-like recording medium at a temperature of 50° C. or higher; and

[0281] The sheet-like recording medium is wound into a roll.

[0282] According to this inkjet recording apparatus, since the above-mentioned inkjet ink composition is used, the drying property of the paper surface on the recording medium is also good, and even if it is wound into a roll, it is difficult to cause print-through.

Claims

1. An inkjet ink composition, characterized in that Include: Sublimation dyes; Sugar alcohols, with more than 4 OH groups; Diols, with 2 or 3 carbon atoms; A penetrating moisturizer selected from one or more of glycol monoethers, diols having 4 or more carbon atoms, amides and (poly)glycerol ethers; and The content of glycerol is 1% by mass or less based on the total mass of the inkjet ink composition.

2. The inkjet ink composition according to claim 1, characterized in that The surface tension of a 10 mass % aqueous solution of the above-mentioned penetrating moisturizing agent is 45 mN / m or more and 67 mN / m or less.

3. The inkjet ink composition according to claim 1, characterized in that The content of the penetrating moisturizing agent is 5% by mass or less relative to the total mass of the inkjet ink composition.

4. The inkjet ink composition according to claim 1, characterized in that The invention further comprises at least one selected from polyglycerols and betaines.

5. The inkjet ink composition according to claim 1, characterized in that The content of the diol having 2 or 3 carbon atoms is 5% by mass or more and 15% by mass or less based on the total mass of the inkjet ink composition.

6. The inkjet ink composition according to claim 1, characterized in that The viscosity of a 60 mass % aqueous solution of the sugar alcohol is 35 mPa·s or less.

7. The inkjet ink composition according to claim 1, characterized in that The content of the sugar alcohol is 3% by mass or more and 15% by mass or less relative to the total mass of the inkjet ink composition.

8. The inkjet ink composition according to claim 1, characterized in that The penetrating moisturizer comprises (poly)glycerol ethers.

9. The inkjet ink composition according to claim 8, characterized in that The weight average molecular weight of the (poly)glyceryl ethers is 300 or more and 800 or less.

10. An inkjet recording method, characterized in that: include: A recording step of attaching the inkjet ink composition according to any one of claims 1 to 9 to a sheet-like recording medium; a transfer step of placing the recording surface of the sheet-like recording medium on an object to be dyed, heating the recording surface at a temperature of 150° C. to 220° C. to transfer the sublimation dye to the object to be dyed by sublimation; as well as The peeling step is to peel the sheet-like recording medium from the dyeing object after the image transfer.

11. An inkjet recording method, characterized in that: include: A recording step of attaching the inkjet ink composition according to any one of claims 1 to 9 to a sheet-like recording medium; a drying step of heating the sheet-like recording medium to which the inkjet ink composition is attached at a temperature of 50° C. or higher; and In the recovery step, the dried sheet-shaped recording medium is wound into a roll.

12. An inkjet recording device, characterized in that: Include: An inkjet head that allows the inkjet ink composition according to any one of claims 1 to 9 to adhere to a sheet-like recording medium; a heater for heating the sheet-like recording medium at a temperature of 50° C. or higher; and The sheet-like recording medium is wound into a roll.