Ejection cover and rocket engine thereof
By designing a spherical multi-layer composite ejection cover, the problems of complex structure and low reliability in cold launch technology are solved, and efficient ejection and engine ignition processes are achieved, reducing maintenance costs and risks.
Patent Information
- Application Number
- CN202411031191.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-12
AI Technical Summary
In the existing cold launch technology, the structure for ejection has problems such as complex structure, high cost of use, low reliability, and cumbersome use and maintenance.
Design a spherical ejection cover, which is cured by multi-layer composite material, bonded to the inner surface of the nozzle diffusion section, can withstand ejection gas under high pressure, prevent gas from entering the engine, and under low pressure when the engine is ignited Break into small pieces to avoid damage to the launcher.
The ejection structure is simplified, the cost of use is reduced, reliability and maintenance ease is improved, while ensuring the normal ignition and operation of the engine, avoiding the risk of large-scale impact.
Smart Images

Figure CN118936235A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of rocket equipment, and in particular to an ejection cover and a rocket engine thereof. Background Art
[0002] As a missile launch method, cold launch technology does not rely on the rocket engine's own power (hot launch) to launch the missile from the launch tube, but uses external power such as compressed air, gas, high-pressure cold air, etc. to eject the missile from the launch tube. After reaching a certain height, the missile engine ignites to propel the missile to continue flying. Cold launch is increasingly widely used due to its simple structure, good versatility, light weight, high safety, and strong launch adaptability.
[0003] Cold launch has specific sealing requirements for the projectile structure. A sealing ring or adapter is required between the projectile and the launch tube to achieve the functions of sealing, buffering and guiding. In order to adapt to the pressure of ejection, the projectile needs to be equipped with a special tail cover or ejector and separation mechanism to meet the requirements of cold launch. Usually, the specially designed ejection structure has the characteristics of complex structure, high cost, low reliability, and cumbersome use and maintenance. Summary of the invention
[0004] The present application provides an ejection cover and a rocket engine thereof, which can solve the problems in the related art that the ejection structure has a complex structure, high use cost, low reliability, and cumbersome use and maintenance.
[0005] In a first aspect, an embodiment of the present application provides an ejection cover, comprising: a gas action portion and a bonding portion, wherein the gas action portion is a spherical structure; the bonding portion is a cylindrical structure and is arranged on one side of the gas action surface, and the bonding portion is used to bond with the nozzle by an adhesive; wherein the gas action portion and the bonding portion are integrally formed and are formed by curing and stacking multiple layers of composite materials. The ejection cover is bonded to the inner surface of the nozzle diffusion section. Since the gas action part is a spherical structure, when the projectile is launched, high-pressure gas is generated to act on the concave surface of the gas action part. The ejection cover bears the high pressure in the positive direction, preventing the ejection gas from entering the engine and pushing the launch tube at the ejection point of the projectile; when the projectile is ejected out of the tube and the engine ignites, the engine gas acts on the convex surface of the gas action part, and the ejection cover bears a low pressure of 1 to 3 MPa in the reverse direction; the ejection cover is formed by curing and forming composite material layers. When the pressure reaches a certain value, the ejection cover loses its stability and structure is damaged. It breaks into small fragments under the action of gas, which does not affect the normal ignition and pressure building of the engine. The ejection cover fragments are scattered due to the action of the gas plume, and will not form large pieces to hit the launch tube and cause damage.
[0006] In combination with the first aspect, in one implementation, the number of composite material plies is obtained based on a correction factor, an actual thickness of the ejection cover, and a single-layer thickness.
[0007] In combination with the first aspect, in one embodiment, the actual number of layers of the ejection cover is obtained according to the design thickness of the ejection cover and the design evaluation thickness of the ejection cover for reverse compression instability;
[0008] The ejection cover design thickness is obtained according to the front pressure bearing design pressure, spherical radius, and material tensile strength;
[0009] The reverse pressure instability design evaluation thickness of the ejection cover is obtained according to the reverse instability design pressure, the spherical radius, the material elastic modulus and the material Poisson's ratio.
[0010] In combination with the first aspect, in one embodiment, each layer of the composite material ply includes multiple pieces of composite material ply, and the multiple pieces of composite material ply are spliced together to form the composite material ply, and the surface of the composite material ply is coated with an adhesive layer.
[0011] In combination with the first aspect, in one embodiment, in the same layer of composite material ply, two adjacent pieces of composite material ply partially overlap, and the overlapping portion forms a lap joint.
[0012] In combination with the first aspect, in one implementation, the overlap width is 20 to 30 mm.
[0013] In combination with the first aspect, in one embodiment, multiple sheets of composite material pavement in the same composite material pavement layer are arranged in parallel, which not only improves the laying consistency of the composite material pavement, but also enables the glass fiber twill fabric to exert its bulk tensile properties.
[0014] In combination with the first aspect, in one embodiment, in two adjacent layers of composite material ply, one layer of composite material ply is rotated in a set direction and at a set angle relative to the other layer of composite material ply. To ensure that the thickness of each part of the ejection cover is consistent
[0015] In combination with the first aspect, in one implementation, the set angle is 25° to 35°.
[0016] In combination with the first aspect, in one implementation, the number of composite material plies is 5 to 8, which can not only meet certain positive compression resistance, but also ensure sufficiently low reverse explosion resistance, while ensuring the lightness of the structure.
[0017] In a second aspect, an embodiment of the present application provides a rocket engine, comprising: an ejection cover and a nozzle as described above, wherein the ejection cover is arranged at the nozzle outlet.
[0018] The beneficial effects brought by the technical solution provided in the embodiments of the present application include:
[0019] The embodiment of the present application provides an ejection cover and a rocket engine thereof, wherein the ejection cover is bonded to the inner surface of the nozzle diffusion section. Since the gas action part is a spherical structure, when the projectile is launched, high-pressure gas is generated to act on the concave surface of the gas action part, and the ejection cover bears the high pressure in the positive direction, preventing the ejection gas from entering the engine and pushing the launch tube at the ejection point of the projectile; when the projectile is ejected out of the tube and the engine is ignited, the engine gas acts on the convex surface of the gas action part, and the ejection cover bears a low pressure of 1 to 3 MPa in the reverse direction; the ejection cover is formed by curing and forming a composite material layer. When the pressure reaches a certain value, the ejection cover loses its stability and is structurally damaged. It breaks into small fragments under the action of the gas, which does not affect the normal ignition and pressure building of the engine. The fragments of the ejection cover are scattered due to the action of the gas plume, and will not form large pieces to hit the launch tube and cause damage. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0021] Figure 1 A schematic diagram of the overall structure provided for an embodiment of the present application;
[0022] Figure 2 A schematic diagram of the overall structure provided for an embodiment of the present application;
[0023] Figure 3 A schematic diagram of an ejection cover and a nozzle provided in an embodiment of the present application;
[0024] Figure 4 A schematic diagram of an ejection cover and a nozzle provided in an embodiment of the present application;
[0025] Figure 5 A schematic diagram of the overlap portion provided in an embodiment of the present application.
[0026] In the figure: 1. Gas action part; 2. Adhesive part; 3. Overlap part; 4. Nozzle diffusion section shell; 5. Diffusion section insulation layer. DETAILED DESCRIPTION
[0027] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0028] See also Figures 1 to 5 The embodiment of the present application provides an ejection cover and a rocket engine thereof, which can solve the problems in the related art that the ejection structure has a complex structure, high use cost, low reliability, and cumbersome use and maintenance.
[0029] As a missile launch method, cold launch technology does not rely on the rocket engine's own power (hot launch) to launch the missile from the launch tube, but uses external power such as compressed air, gas, high-pressure cold air, etc. to eject the missile from the launch tube. After reaching a certain height, the missile engine ignites to propel the missile to continue flying. Cold launch is increasingly widely used due to its simple structure, good versatility, light weight, high safety, and strong launch adaptability.
[0030] Cold launch has specific sealing requirements for the projectile structure. A sealing ring or adapter is required between the projectile and the launch tube to achieve the functions of sealing, buffering and guiding. In order to adapt to the pressure of ejection, the projectile needs to be equipped with a special tail cover or ejector and separation mechanism to meet the requirements of cold launch. Usually, the specially designed ejection structure has the characteristics of complex structure, high cost, low reliability, and cumbersome use and maintenance.
[0031] Aiming at the problems that the ejection structure has a complex structure, high cost of use, low reliability, and cumbersome use and maintenance. In the first aspect, the embodiment of the present application provides an ejection cover and a rocket engine thereof, which comprises: a gas action part 1 and a bonding part 2, wherein the gas action part 1 is a spherical structure; the bonding part 2 is a cylindrical structure and is arranged on one side of the gas action surface, and the bonding part 2 is used to bond with the nozzle by an adhesive; wherein the gas action part 1 and the bonding part 2 are integrally formed, and are formed by curing a multi-layer composite material layer.
[0032] In the present application, the ejection cover is bonded to the inner surface of the nozzle diffusion section. Since the gas action part 1 is a spherical structure, when the projectile is launched, high-pressure gas is generated to act on the concave surface of the gas action part 1, and the ejection cover bears the high pressure in the positive direction, preventing the ejection gas from entering the engine and pushing the launch tube where the projectile is ejected; when the projectile is ejected out of the tube and the engine is ignited, the engine gas acts on the convex surface of the gas action part 1, and the ejection cover bears a low pressure of 1 to 3 MPa in the reverse direction; the ejection cover is formed by curing the composite material ply. When the pressure reaches a certain value, the ejection cover loses its stability and the structure is damaged. It breaks into small fragments under the action of the gas, which does not affect the normal ignition and pressure building of the engine. The ejection cover fragments are scattered due to the action of the gas plume, and will not form large pieces to hit the launch tube and cause damage. Among them, Figure 3 X represents engine gas, and Y represents ejection gas.
[0033] The ejection cover adopts the thin shell theory to calculate the actual thickness of the ejection cover, and is designed based on the low-pressure instability failure characteristics of the composite structure:
[0034] Specifically, the ejection cover design thickness is obtained according to the front pressure bearing design pressure, spherical radius, and material tensile strength:
[0035] Based on the formula: h1 = P*R / σ, the ejection cover design thickness h1 is obtained, where P is the front pressure design pressure, R is the spherical radius, and σ is the tensile strength of the material;
[0036] The reverse pressure instability design evaluation thickness of the ejection cover is obtained according to the reverse instability design pressure, spherical radius, material elastic modulus and material Poisson's ratio:
[0037] Based on the formula: The reverse pressure instability design evaluation thickness h' of the ejection cover is obtained, where P' is the reverse instability design pressure, E is the elastic modulus of the material, V is the Poisson's ratio of the material, and R is the spherical radius.
[0038] By adjusting and optimizing the values of P and P', h1 and h' are calculated to ensure that the absolute value of the difference between h1 and h' is less than 0.10 mm. When the absolute value of the difference between h1 and h' is less than 0.10 mm, the design thickness h1 of the ejection cover is the actual thickness h of the ejection cover.
[0039] Furthermore, the number of composite material plies is obtained according to the correction factor, the actual thickness of the ejection cover and the thickness of the single ply:
[0040] Based on the formula: n = ζ × h / tn, the number of composite material plies n is obtained, where ζ is the correction factor, tn is the thickness of a single layer, and h is the actual thickness of the ejection cover.
[0041] In this embodiment, the number of composite material plies is designed to be 5 to 8, which can meet certain positive compressive strength and ensure sufficiently low reverse explosion resistance, while ensuring the lightness of the structure. In other embodiments, the number of composite material plies can be designed and calculated as needed.
[0042] On the basis of the above embodiments, in this embodiment, each layer of the composite material ply includes multiple pieces of composite material ply, and the multiple pieces of composite material ply are spliced together to form the composite material ply, and the surface of the composite material ply is coated with an adhesive layer.
[0043] Specifically, in this embodiment, the composite material paving material is made of glass fiber twill, quartz fiber cloth or nylon fiber cloth; preferably, glass fiber twill is used, and the easily ablated glass fiber twill is used for paving, so that the material can better adapt to the geometric structure, and the glass fiber twill is easily ablated and blown away by the engine gas after reverse explosion. The adhesive layer painted on the surface is made of materials such as epoxy resin or modified phenolic resin.
[0044] After the adhesive layer is applied to the surface of the composite material pavement for impregnation, it is laid layer by layer on the tooling surface. In the present embodiment, each layer of composite material pavement is formed by laying three composite material pavements, and multiple pieces of composite material pavements in the same layer of composite material pavement are arranged in parallel, that is, multiple pieces of composite material pavements are overlapped in parallel. In order to ensure the firmness of the overlap, in the same layer of composite material pavement, two adjacent pieces of composite material pavements are partially overlapped, and the overlapping part forms an overlap portion 3. In the present embodiment, the width of the overlap portion 3 is set to 20 to 30 mm. Each layer in the ejection cover is provided with parallel overlapping edges, which not only makes the laying consistency of the composite material pavement better, but also enables the glass fiber twill cloth to exert its body tensile properties.
[0045] On the basis of the above embodiment, in this embodiment, in two adjacent composite material plies, one of the composite material plies is rotated at a set angle in a set direction relative to the other composite material ply.
[0046] Specifically, in order to ensure that the thickness of each part of the ejection cover is consistent, when laying the composite material, the composite material in the second layer of composite material is rotated at a set angle relative to the composite material in the first layer of composite material, and the composite material in the third layer of composite material is rotated at a set angle relative to the composite material in the second layer of composite material... and so on, until all composite material layers are laid. It should be noted that when the first rotation is to set the angle clockwise, each subsequent layer of composite material rotates clockwise; when the first rotation is to set the angle counterclockwise, each subsequent layer of composite material rotates counterclockwise. In this embodiment, the set angle is 25° to 35°.
[0047] After the composite material ply is laid, a vacuum bag is used for evacuation and curing is performed in an autoclave. After the ejection cover is cured and formed, the edge is trimmed to ensure sufficient width of the bonding portion 2, usually ensuring that the width of the bonding portion 2 is 30 to 50 mm.
[0048] After the ejection cover is manufactured, the bonding portion 2 of the ejection cover is polished and coated with adhesive, and the bonding portion 2 is bonded to the inner surface of the diffusion section insulation layer 5 of the engine nozzle by using a tool for centering and cured.
[0049] During the storage period of the device, the ejection cover can act as a plug on the nozzle. During launch, the ejection device works, generating high-pressure gas, which acts on the concave surface of the ejection cover, pushing the missile body out of the launch tube, and the ejection cover plays a role of sealing and pressure bearing; after the missile is ejected out of the tube, the engine ignites and works, and the high-temperature gas acts on the convex surface of the ejection cover, breaking the ejection cover into small fragments and scattering, while the nozzle works normally. At this time, the ejection cover plays a role in maintaining ignition pressure and low-pressure crushing.
[0050] In a second aspect, an embodiment of the present application provides a rocket engine, comprising:
[0051] The ejection cover and nozzle provided in any of the above embodiments of the present application, wherein the ejection cover is arranged at the nozzle outlet.
[0052] The nozzle comprises a nozzle diffuser shell 4 , and a diffuser heat insulation layer 5 is arranged inside the nozzle diffuser shell 4 .
[0053] In the present application, the ejection cover is bonded to the inner surface of the nozzle diffusion section. Since the gas action part 1 is a spherical structure, when the projectile is launched, high-pressure gas is generated to act on the concave surface of the gas action part 1, and the ejection cover bears the high pressure in the positive direction, preventing the ejection gas from entering the engine and pushing the launch tube at the ejection point of the projectile; when the projectile is ejected out of the tube, the engine ignites and works, and the engine gas acts on the convex surface of the gas action part 1, and the ejection cover bears a low pressure of 1 to 3 MPa in the reverse direction; the ejection cover is formed by curing and forming a composite material layer. When the pressure reaches a certain value, the ejection cover loses its stability and the structure is damaged. It breaks into small fragments under the action of the gas, which does not affect the normal ignition and pressure building of the engine. The fragments of the ejection cover are scattered due to the action of the gas plume, and will not form large pieces to hit the launch tube and cause damage.
[0054] Among them, the ejection cover adopts thin shell theory to calculate the actual thickness of the ejection cover, and is designed based on the low-pressure instability and failure characteristics of the composite structure.
[0055] Specifically, the ejection cover design thickness is obtained according to the front pressure bearing design pressure, spherical radius, and material tensile strength:
[0056] Based on the formula: h1 = P*R / σ, the ejection cover design thickness h1 is obtained, where P is the front pressure design pressure, R is the spherical radius, and σ is the tensile strength of the material;
[0057] The reverse pressure instability design evaluation thickness of the ejection cover is obtained according to the reverse instability design pressure, spherical radius, material elastic modulus and material Poisson's ratio:
[0058] Based on the formula: The reverse pressure instability design evaluation thickness of the ejection cover is obtained, where P' is the reverse instability design pressure, E is the elastic modulus of the material, V is the Poisson's ratio of the material, and R is the spherical radius.
[0059] By adjusting and optimizing the values of P and P', h1 and h' are calculated to ensure that the absolute value of the difference between h1 and h' is less than 0.10 mm. When the absolute value of the difference between h1 and h' is less than 0.10 mm, the design thickness h1 of the ejection cover is the actual thickness h of the ejection cover.
[0060] Furthermore, the number of composite material plies is obtained according to the correction factor, the actual thickness of the ejection cover and the thickness of the single ply:
[0061] Based on the formula: n = ζ × h / tn, the number of composite material plies n is obtained, where ζ is the correction factor, tn is the thickness of a single layer, and h is the actual thickness of the ejection cover.
[0062] In this embodiment, the number of composite material plies is designed to be 5 to 8, which can meet certain positive compressive strength and ensure sufficiently low reverse explosion resistance, while ensuring the lightness of the structure. In other embodiments, the number of composite material plies can be designed and calculated as needed.
[0063] On the basis of the above embodiments, in this embodiment, each layer of the composite material ply includes multiple pieces of composite material ply, and the multiple pieces of composite material ply are spliced together to form the composite material ply, and the surface of the composite material ply is coated with an adhesive layer.
[0064] Specifically, in this embodiment, the composite material paving material is made of glass fiber twill, quartz fiber cloth or nylon fiber cloth; preferably, glass fiber twill is used, and the easily ablated glass fiber twill is used for paving, so that the material can better adapt to the geometric structure, and the glass fiber twill is easily ablated and blown away by the engine gas after reverse explosion. The adhesive layer painted on the surface is made of materials such as epoxy resin or modified phenolic resin.
[0065] After the adhesive layer is applied to the surface of the composite material pavement for impregnation, it is laid layer by layer on the tooling surface. In this embodiment, each layer of composite material pavement is paved with three composite material pavements, and multiple pieces of composite material pavements in the same layer of composite material pavement are arranged in parallel, that is, multiple pieces of composite material pavements are overlapped in parallel. In order to ensure the firmness of the overlap, in the same layer of composite material pavement, two adjacent pieces of composite material pavement are partially overlapped, and the overlapping part forms an overlap portion 3. In this embodiment, the width of the overlap portion 3 is set to 20 to 30 mm. Each layer in the ejection cover is provided with parallel overlapping edges, which not only makes the laying consistency of the composite material pavement better, but also enables the glass fiber twill cloth to exert its body tensile properties.
[0066] On the basis of the above embodiment, in this embodiment, in two adjacent composite material plies, one of the composite material plies is rotated at a set angle in a set direction relative to the other composite material ply.
[0067] Specifically, in order to ensure that the thickness of each part of the ejection cover is consistent, when laying the composite material, the composite material in the second layer of composite material is rotated at a set angle relative to the composite material in the first layer of composite material, and the composite material in the third layer of composite material is rotated at a set angle relative to the composite material in the second layer of composite material... and so on, until all composite material layers are laid. It should be noted that when the first rotation is to set the angle clockwise, each subsequent layer of composite material rotates clockwise; when the first rotation is to set the angle counterclockwise, each subsequent layer of composite material rotates counterclockwise. In this embodiment, the set angle is 25° to 35°.
[0068] After the composite material ply is laid, a vacuum bag is used for evacuation and curing is performed in an autoclave. After the ejection cover is cured and formed, the edge is trimmed to ensure sufficient width of the bonding portion 2, usually ensuring that the width of the bonding portion 2 is 30 to 50 mm.
[0069] After the ejection cover is manufactured, the bonding portion 2 of the ejection cover is polished and coated with adhesive, and the bonding portion 2 is bonded to the inner surface of the diffusion section insulation layer 5 of the engine nozzle by using a tool for centering and cured.
[0070] During the storage period of the device, the ejection cover can act as a plug on the nozzle. During launch, the ejection device works, generating high-pressure gas, which acts on the concave surface of the ejection cover, pushing the missile body out of the launch tube, and the ejection cover plays a role of sealing and pressure bearing; after the missile is ejected out of the tube, the engine ignites and works, and the high-temperature gas acts on the convex surface of the ejection cover, breaking the ejection cover into small fragments and scattering, while the nozzle works normally. At this time, the ejection cover plays a role in maintaining ignition pressure and low-pressure crushing.
[0071] In the description of the present application, it should be noted that the terms "upper", "lower", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application. Unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be a connection between the two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the present application can be understood according to the specific circumstances.
[0072] It should be noted that, in this application, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.
[0073] The above description is only a specific implementation of the present application, so that those skilled in the art can understand or implement the present application. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein can be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application will not be limited to the embodiments shown herein, but will conform to the widest range consistent with the principles and novel features applied for herein.
Claims
1. A ejection cover, characterized in that: It includes: A gas action part (1), wherein the gas action part (1) is a spherical structure; A bonding portion (2), the bonding portion (2) being a cylindrical structure and being arranged on one side of the gas action surface, the bonding portion (2) being used for bonding with the nozzle by means of an adhesive; The gas action portion (1) and the bonding portion (2) are integrally formed and are formed by stacking and curing multiple layers of composite material.
2. The ejection cover according to claim 1, characterized in that: The number of composite material plies is obtained according to a correction factor, an actual thickness of the ejection cover and a single-layer ply thickness.
3. The ejection cover according to claim 2, characterized in that: The actual number of layers of the ejection cover is obtained according to the design thickness of the ejection cover and the design evaluation thickness of the ejection cover under reverse pressure instability; The ejection cover design thickness is obtained according to the front pressure bearing design pressure, spherical radius, and material tensile strength; The reverse pressure instability design evaluation thickness of the ejection cover is obtained according to the reverse instability design pressure, the spherical radius, the material elastic modulus and the material Poisson's ratio.
4. The ejection cover according to claim 1, characterized in that: Each layer of the composite material ply comprises a plurality of pieces of composite material ply, and the plurality of pieces of composite material ply are spliced together to form the composite material ply, and the surface of the composite material ply is coated with an adhesive layer.
5. The ejection cover according to claim 4, characterized in that: In the same layer of composite material ply, two adjacent composite material ply materials partially overlap, and the overlapping portion forms an overlap portion (3).
6. The ejection cover according to claim 5, characterized in that: The overlap portion (3) has a width of 20 to 30 mm.
7. The ejection cover according to claim 4, characterized in that: Multiple pieces of composite material in the same layer of composite material layup are arranged in parallel.
8. The ejection cover according to claim 7, characterized in that: In two adjacent layers of composite material plies, one layer of composite material plies is rotated at a set angle in a set direction relative to the other layer of composite material plies.
9. The ejection cover according to claim 8, characterized in that: The setting angle is 25° to 35°.
10. A rocket engine, characterized in that: It includes: The ejection cover according to any one of claims 1 to 9; The ejection cover is arranged at the nozzle outlet.
Citation Information
Patent Citations
Rubber blanking cap of guided missile engine exhaust nozzle
CN104696110A
Solid rocket engine jet pipe blanking cap and forming and bonding method thereof
CN117469054A
One-way pressure-bearing sealing cover
CN221096683U