Electrophoresis electronic paper, isolating membrane applied to electrophoresis electronic paper and manufacturing method of isolating membrane

By setting an isolation film containing electron-withdrawing and electron-donating groups on the electrode surface of electrophoretic electronic paper, the problem of pigment electrophoretic particle adsorption is solved, the service life of electronic paper is extended, and the manufacturing process is simplified.

CN118938557AInactive Publication Date: 2024-11-12GUANGZHOU OED TECH INC +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202310530552.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-10
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In existing electrophoretic electronic paper, pigment electrophoretic particles are easily adsorbed onto the common electrode and pixel electrode, leading to irreversible display effects and affecting the lifespan.

Method used

An isolation film is provided on the surface of the common electrode and/or pixel electrode of the electrophoretic electronic paper. The isolation film material contains electron-withdrawing groups and electron-donating groups to prevent the adsorption of pigment electrophoretic particles.

Benefits of technology

It effectively avoids the adsorption of pigment electrophoretic particles to electrodes, extends the service life of electronic paper, and has a simple manufacturing method with high feasibility and economy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118938557A_ABST
    Figure CN118938557A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides an isolating membrane applied to electrophoresis electronic paper, and aims to solve the problem of adsorption of surface metal oxide and charge particles of at least one of a common electrode or a pixel electrode of the electrophoresis electronic paper. The isolating membrane is arranged on the surface of at least one of a common electrode and a pixel electrode of the electrophoresis electronic paper and used for isolating pigment electrophoresis particles from being adsorbed by any one of the common electrode and the pixel electrode, and the molecular structure of the isolating membrane material simultaneously comprises an electron withdrawing group and an electron donating group. Therefore, the problem that the pigment electrophoretic particles are adsorbed with electrodes of the display cavity is solved, and the service life of the electronic paper is prolonged. In addition, the manufacturing method adopted by the invention is relatively simple, can be compatible with an existing manufacturing process, and has relatively high feasibility and economical efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of electrophoretic display, and in particular, to an electrophoretic electronic paper and an isolation film applied to the electrophoretic electronic paper, an isolation film applied to the electrophoretic electronic paper, and a manufacturing method thereof. Background Art

[0002] Electrophoretic electronic paper is a high-tech display technology that displays images and text by placing a large number of tiny charged particles in a tiny space and making them move under the control of the field. These tiny charged particles are usually colloidal particles with a diameter of several hundred nanometers, submicron, or 1-5 microns. These particles are generally called pigment electrophoretic particles, which are wrapped in a solution and stored in a cavity. Two electrodes above and below the cavity apply an electric field to the pigment electrophoretic particles, and they move perpendicular to the direction of the electric field, thereby changing their color.

[0003] Generally, the upper electrode is called the common electrode and the lower electrode is called the pixel electrode. Due to the relationship between the above-mentioned electrode materials, these pigment electrophoretic particles have a probability of being adsorbed on the electrode. Even if the electric field is changed, this adsorption effect cannot be eliminated, which leads to irreversible display effects and seriously affects the service life of the electronic paper.

[0004] Therefore, it is urgent to provide a new electrophoretic electronic paper structure to solve the above technical problems. Summary of the invention

[0005] In order to solve the defects of the prior art, the present invention aims to solve the problem of adsorption of charged particles by at least one surface metal oxide in the common electrode or pixel electrode of electrophoretic electronic paper.

[0006] The first aspect of the present invention provides an isolation film for use in electrophoretic electronic paper, characterized in that the isolation film is arranged on the surface of the common electrode and / or pixel electrode of the electrophoretic electronic paper, and is used to isolate the pigment electrophoretic particles from being adsorbed by either the common electrode or the pixel electrode, and the molecular structure of the isolation film material contains both electron-withdrawing groups and electron-donating groups.

[0007] Optionally, the isolation film has a thickness of 0.001 to 25 microns.

[0008] Optionally, the ratio between the electron donating group and the electron withdrawing group in the isolation membrane is 1:5 to 5:1.

[0009] Optionally, the ratio between the electron donating group and the electron withdrawing group in the isolation membrane is controlled to be 1:2 to 2:1.

[0010] Optionally, the transmittance of the isolation film disposed on the surface of the common electrode is greater than or equal to 80%.

[0011] Optionally, the volume resistivity of the isolation film is less than or equal to 10 15 Ω·cm.

[0012] A second aspect of the present invention provides an electrophoretic electronic paper, comprising an electrophoretic display cavity surrounded by a common electrode, a pixel electrode and an edge sealing structure, wherein the display cavity comprises at least two pigment electrophoretic particles and a solution, wherein the pigment electrophoretic particles are wrapped by the solution, and an isolation film as described above is applied, wherein the isolation film is arranged on the surface of the common electrode and / or the pixel electrode.

[0013] Optionally, the electrophoretic display cavities are separated by a plurality of transparent isolation members, and the electrophoretic display cavities separated by the transparent isolation members are connected or disconnected.

[0014] Optionally, the cross-section of the transparent isolation member is a regular shape, such as a square, a circle, a triangle, a trapezoid, a pentagon, a hexagon, an ellipse or other shapes and irregular shapes.

[0015] A third aspect of the present invention provides a method for manufacturing electrophoretic electronic paper, using the isolation film as described above.

[0016] Compared with the prior art, the present invention has the following beneficial effects:

[0017] Compared with the background technology, the isolation film provided by the present invention is arranged on the surface of the common electrode and / or pixel electrode of the electrophoretic electronic paper, and is used to isolate the pigment electrophoretic particles from being adsorbed by either the common electrode or the pixel electrode. The molecular structure of the isolation film material contains both electron-withdrawing groups and electron-donating groups. This avoids the problem of adsorption of the pigment electrophoretic particles on the electrodes of the display cavity. This prolongs the service life of the electronic paper. In addition, the manufacturing method adopted by the present invention is relatively simple, compatible with existing manufacturing processes, and has high feasibility and economy. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 A schematic diagram of the structure of an embodiment of an electrophoretic electronic paper of the present invention;

[0019] Figure 2 This is a schematic structural diagram of another embodiment of an electrophoretic electronic paper of the present invention;

[0020] Figure 3 This is a schematic structural diagram of another embodiment of an electrophoretic electronic paper of the present invention. DETAILED DESCRIPTION

[0021] First, the technical terms and inventive concepts in the text are explained:

[0022] In order to solve the problem of adsorption of metal oxides and pigment electrophoretic particles on the electrode surface of electrophoretic electronic paper in the background technology, the applicant's invention is to use a certain material to isolate the pigment electrophoretic particles from the electrode without affecting the display effect. The isolation layer can be attached between the pigment electrophoretic particles and the common electrode, and the isolation layer is not adsorbed by the pigment electrophoretic particles.

[0023] A first aspect of an embodiment of the present invention provides an isolation film applied to electrophoretic electronic paper, wherein the isolation film is arranged on the surface of at least one of a common electrode or a pixel electrode of the electrophoretic electronic paper, and is used to isolate pigment electrophoretic particles from being adsorbed by either the common electrode or the pixel electrode, and the molecular structure of the isolation film material contains both electron-withdrawing groups and electron-donating groups.

[0024] In this embodiment, the ratio between the electron donating group and the electron withdrawing group in the isolation membrane is controlled to be 1:5 to 5:1, preferably 1:2 to 2:1. Different types of compounds and functional groups can be used to control the ratio of the electron donating group and the electron withdrawing group of the isolation membrane. For example, functional groups such as nitro, carbonyl, and methyl can be used to adjust the charge properties of the isolation membrane surface. The following are several possible compounds and functional groups:

[0025] (1) Fluoroaniline: Contains fluorophenyl and amine functional groups, which can make the surface electron-withdrawing;

[0026] (2) Aniline: Contains phenyl and amine functional groups, which can make the surface electron-donating;

[0027] (3) Organic amines: including seven categories: fatty amines, alcohol amines, amides, alicyclic amines, aromatic amines, naphthyl amines, and other amines.

[0028] (4) Acrylic acid: It contains carboxyl functional groups, which can form negative charges on the surface, making the surface electron-withdrawing;

[0029] (5) Methacrylic acid: It contains carboxyl and methyl functional groups, which can form positively charged acidic functional groups on the surface, making the surface electron-donating.

[0030] Electron donating groups and electron withdrawing groups are concepts in organic chemistry that describe the relative electron affinities between different functional groups in some organic molecules. Usually, there are electron donating groups and electron withdrawing groups in organic molecules, and their relative ratios will affect the properties of the molecules. Some common electron donating groups include -NH2, -NHR, -NR1R2, -N +R1R2R3, or other functional groups containing amine, imino, amide, etc., which can donate electrons to the center of the molecule, making the molecule positively charged. Some common electron-withdrawing groups include -C=O, -NO2, -CN, -F, -Cl, -Br, -I, -COOH, -SO3H, -SH, -C≡CH, -OCH3, -OH, -C6H5, -CH=CH2, etc., which can attract electrons from the center of the molecule, making the molecule negatively charged.

[0031] The selected material is prepared by solution method or vapor deposition method. The solution method is to add the selected material to an appropriate amount of solvent and stir it thoroughly until the material is completely dissolved. The vapor deposition method includes physical vapor deposition (PVD, Physical Vapor Deposition) and chemical vapor deposition (CVD, Chemical Vapor Deposition).

[0032] It should be noted that the physical vapor deposition technology in this application refers to the technology of using physical methods to vaporize the surface of the material source (solid or liquid) into gaseous atoms or molecules, or partially ionize into ions under vacuum conditions, and deposit a thin film with some special functions on the surface of the substrate through a low-pressure gas (or plasma) process. Physical vapor deposition is one of the main surface treatment technologies. PVD coating technology is mainly divided into three categories: vacuum evaporation coating, vacuum sputtering coating and vacuum ion coating. The main methods of physical vapor deposition are: vacuum evaporation, sputtering coating, arc plasma coating, ion plating and molecular beam epitaxy. The corresponding vacuum coating equipment includes vacuum evaporation coating machine, vacuum sputtering coating machine and vacuum ion coating machine. Physical vapor deposition technology can deposit metal films, alloy films, compounds, ceramics, semiconductors, polymer films, etc. Chemical vapor deposition is a chemical technology that uses one or more gas phase compounds or single substances containing film elements to chemically react on the surface of the substrate to form a thin film. The materials deposited by chemical vapor deposition can be oxides, sulfides, nitrides, carbides, or binary or multinary inter-element compounds in groups III-V, II-IV, and IV-VI, and their physical functions can be precisely controlled by the deposition process of vapor phase doping. The methods for preparing thin films also include slit or dye coating, or spraying, evaporation, ion beam deposition, etc.

[0033] The second invention of the present invention provides an electronic paper, please refer to the following Figure 1 , a first embodiment of an electrophoretic electronic paper of the present application, its structure sequentially comprises:

[0034] A transparent cover plate 1, a common electrode 2, a first isolation film 3, an electrophoretic display cavity 4 and a pixel electrode 5.

[0035] The electrophoretic display cavity 4 further comprises a transparent barrier 43, pigment electrophoretic particles 41 and electrophoretic liquid 42. The plurality of transparent barriers 43 divide the electrophoretic display cavity 4 into a plurality of display units, which are connected to each other. Each display unit is filled with electrophoretic liquid 42, in which the pigment electrophoretic particles 41 are immersed.

[0036] It should be noted that the transmittance of the first barrier film 3 is greater than or equal to 80%.

[0037] Preferably, the isolation film has a thickness of 0.001 to 25 microns.

[0038] It should be noted that in actual manufacturing, the cross section of the transparent spacer may be a regular shape, such as a square, a circle, a triangle, a trapezoid, a pentagon, a hexagon, an ellipse or other shapes and irregular shapes.

[0039] The second embodiment of the electrophoretic electronic paper of the present application is different from the above-mentioned embodiment in that the electrophoretic display units separated by the transparent isolation member are not connected to each other. The other structures are the same and will not be described in detail.

[0040] See below Figure 2 The third embodiment of the electrophoretic electronic paper of the present application is different from the first embodiment in that it also includes a second isolation film 6, which is arranged on the surface of the pixel electrode 5 to further prevent the pigment electrophoretic particles 42 from being adsorbed and combined with the pixel electrode 5. Since the second isolation film 6 is located under the electrophoretic display cavity, it will not affect the display effect and can be limited to be transparent or opaque.

[0041] The fourth embodiment of an electrophoretic electronic paper of the present application differs from the second embodiment in that it also includes a second isolation film 6, which is arranged on the surface of the pixel electrode 5 to further prevent the pigment electrophoretic particles 42 from being adsorbed and combined with the pixel electrode 5. Since the second isolation film 6 is located under the electrophoretic display cavity, it will not affect the display effect. It can be limited to be transparent or opaque, and the specific material may include the manufacturing material of the first isolation film 3. In practical applications, the specific material can be formed into an isolation film on the upper surface of the pixel electrode and the surface of the transparent barrier by evaporation. The isolation film material has been described in the previous embodiment and will not be described again.

[0042] A third aspect of the present invention provides an electronic paper manufacturing method, comprising:

[0043] 1. Preparation of pigment electrophoretic particles:

[0044] The electrophoretic pigment particles in the present application are positively charged or negatively charged or electrically neutral. The pigments include titanium white, zinc barium white, zinc oxide, silicon dioxide, iron black, carbon black, chromite, chromate, silicate, chromium oxide green, lead chrome green, copper, titanium yellow, chrome yellow, iron yellow, lead chrome green, manganese violet, iron blue, cobalt blue, zinc white, cadmium yellow, cadmium red, barium sulfate, molybdenum orange, ultramarine, azure blue, emerald green, emerald green, etc. The pigment of the charged pigment particles can be micronized, and the particle size is preferably 0.01-5 microns. The pigment of the neutral pigment particles can also be micronized, and the particle size is preferably 0.1-1 microns. The methods of the micronization process include grinding and crushing, ultrasound, solvent dispersion and other methods, and the related equipment may include colloid mills, ball mills, freeze crushers, ultrasonic machines, etc. In addition, the pigments of the neutral pigment particles and the charged pigment particles can be surface treated by physical or chemical methods to increase their stability in the solvent. The physical method mainly includes physical adsorption of polymers, surfactants, etc. on the surface of the pigment particles, and the chemical method mainly includes silane modification of the surface of the pigment particles, polymer grafting or chemical bonding of other small molecule compounds or surfactant compounds on the surface of the particles. The low polarity dispersing solvent can be aromatic hydrocarbons such as toluene, benzene, xylene, etc. and halogenated hydrocarbons such as chloroform, tetrachloroethylene, etc. In general, the number of carbon atoms of aromatic hydrocarbons and halogenated hydrocarbons is less than 30. The non-polar dispersing solvent can be straight-chain, branched and cyclic aliphatic hydrocarbons such as n-hexane, nonane, decanane, synthetic isomerized paraffin, synthetic paraffin, synthetic cycloalkane, synthetic alkane, cyclohexane, etc. and halogenated hydrocarbons such as carbon tetrachloride, etc. In general, the number of carbon atoms of aliphatic hydrocarbons and halogenated hydrocarbons is less than 30. The electrophoretic display liquid containing electrically neutral pigment particles can also have good display performance, which is specifically manifested as follows: the neutral pigment particles are used as an efficient dye to produce the background color of the electrophoretic liquid, but do not participate in the electrophoretic behavior of the particles under the action of the electric field. Under the action of the electric field, only the charged pigment particles move. The charged pigment particles move up and down in the microcapsule, combined with the background color produced by the neutral pigment particles, so that the observer has a visual color change, thereby achieving the purpose of display.

[0045] The electrophoretic display liquid is filled around the pigment electrophoretic particles, and the electrophoretic display liquid includes: 5-30 parts by weight of negatively or positively charged pigment particles, or 5-30 parts by weight of neutral pigment particles of a different color from the charged pigment particles; 20-70 parts by weight of low polarity and / or non-polar dispersion solvents. It can also include 0.1-10 parts by weight of a thickening stabilizer. The electrophoretic display liquid containing neutral electrophoretic display particles preferably consists of: 40-60 parts by weight of the dispersion solvent; 10-20 parts by weight of the charged pigment particles; 10-20 parts by weight of the neutral pigment particles; and 0.5-5 parts by weight of the thickening stabilizer. The listed composition ranges are examples listed only for the convenience of explaining the composition of the electrophoretic display liquid. These numbers do not mean that the composition of each component is limited to the listed composition ranges. In the actual electrophoretic display liquid, the composition of each component can also be in a larger range. Meanwhile, the components in the electrophoretic display liquid are not limited to the components listed above, but may also include other components required for preparing the electrophoretic display liquid and the display device, such as but not limited to charge control agents such as OLOA11000, surface tension control agents such as Span80, wetting and dispersing agents such as polyether-modified trisiloxane and other silicone surfactants, and their combinations. Various compositions or other components listed in other parts of this patent are also applicable to the situation described.

[0046] The electrophoretic display liquid containing neutral electrophoretic particles can achieve the purpose of display by controlling the electrophoretic behavior of only one particle, fundamentally avoiding the problem of mutual adsorption and agglomeration of positive and negative electrophoretic particles, thereby improving the electrophoretic display performance and repeatability, and greatly simplifying the reaction process and preparation process. Compared with electrophoretic materials produced by other methods, since the electrophoretic liquid is composed of charged pigment particles and neutral pigment particles, there is no attraction process between the charged pigment particles due to the existence of positive and negative charges, thereby fundamentally avoiding the agglomeration between particles caused by different charges. Because there is no charge attraction between particles, the chemical treatment process for charged pigment particles and neutral pigment particles also becomes simple, and no multi-step synthesis steps are required, thereby effectively simplifying the reaction process. At the same time, due to the simplicity of the internal particle interaction force of the electrophoretic display liquid, the preparation process of the electrophoretic display liquid has also been simplified accordingly, and no additional components need to be added, avoiding cumbersome preparation processes, thereby greatly improving the preparation efficiency and production repeatability of the electrophoretic display liquid, and greatly saving material costs.

[0047] The thickening stabilizer is selected from polymethyl methacrylate, polyethylene, polypropylene, polystyrene, rubbers such as polyisoprene, polyisobutylene or mixtures thereof, preferably polyisoprene, polyisobutylene and / or other agents.

[0048] 2. Prepare electrophoresis solution, specifically including:

[0049] 1) Prepare neutral pigment particles; the weight proportions of each reactant for synthesizing neutral pigment particles are: 30-60% dispersion solvent, 20-35% polymer monomer, 20-35% pigment, 0.1-5% coupling agent, 0.001-5% polymer reaction chain initiator; preferably, 40-50% dispersion solvent, 25-30% polymer monomer, 25-30% pigment, 0.5-3% coupling agent, and 0.1-3% polymer reaction chain initiator. The synthesis method of neutral pigment particles is characterized in that the electrical neutrality of the pigment particles is controlled by surface treatment of the pigment particles and by surface grafting of neutral polymers. The particles synthesized by this method have good dispersibility, high suspension stability, high color covering rate, no charge, no aggregation, and no charge attraction with charged pigment particles to induce agglomeration between particles. This synthesis method is applicable to a variety of inorganic oxides, inorganic salts, and composite inorganic salt pigments. The polymer monomer is a low polar or non-polar small molecule that can undergo polymer polymerization, including but not limited to methacrylates, olefins or dienes such as styrene, butadiene, halogenated olefins such as vinyl chloride, and their mixtures and derivatives. The best choice is acrylate, methacrylate such as lauryl methacrylate, styrene, and their mixtures and derivatives. The pigment includes but is not limited to titanium white, lithopone, zinc oxide, silicon dioxide, iron black, carbon black, chromite, chromate, silicate, chromium oxide green, lead chrome green, copper oxide, titanium yellow, chrome yellow, iron yellow, lead chrome green, manganese violet, iron blue, cobalt blue, zinc white, cadmium yellow, cadmium red, barium sulfate, molybdenum orange, ultramarine, azure blue, emerald green, emerald green, etc., and its particle size should be less than 10 microns, preferably 0.01-5 microns, and the best choice is 0.1-1 micron. The coupling agent needs to be selected as a coupling agent with unsaturated functional groups that can undergo polymer reactions. It includes but is not limited to titanate coupling agents and aluminate coupling agents, etc. Among them, the preferred coupling agent is titanate coupling agent, and the unsaturated functional group includes double bonds, triple bonds, conjugated double bonds and other functional groups. The polymer reaction chain initiator selection includes but is not limited to: azo chain initiators such as azobisisobutyronitrile (AIBN) and azobisisoheptanenitrile, etc., organic peroxide initiators such as dibenzoyl peroxide (BPO), dodecyl peroxide, diisopropyl peroxide, ditert-butyl peroxide, tert-butyl perbenzoate, tert-butyl peroxypivalate, diisopropyl peroxydicarbonate, dicyclohexyl peroxydicarbonate, isopropylbenzene hydroperoxide, tert-butyl hydroperoxide, and various oil-soluble oxidation-reduction chain initiators, etc., and the best selection is azobisisobutyronitrile, azobisisoheptanenitrile, dibenzoyl peroxide (BPO), diisopropyl peroxide. Diisopropyl peroxide, dicyclohexyl peroxydicarbonate, isopropylbenzene hydroperoxide, tert-butyl hydroperoxide, and various oil-soluble oxidation-reduction chain initiators, etc., and the best selection is azobisisobutyronitrile, azobisisoheptanenitrile, dibenzoyl peroxide (BPO), diisopropyl peroxide.

[0050] The synthesis reaction of the neutral pigment particles of the present invention can be carried out in a temperature range of 35-120 degrees Celsius, and the optimal reaction temperature is 70-85 degrees Celsius. The reaction time can be 4-48 hours, and the optimal reaction time is 12-16 hours. The reaction can be carried out in an air environment or under the protection of an inert gas, and the optimal reaction environment is to carry out under the protection of nitrogen or helium. The collection of the product can be collected by centrifugation after the reaction is completed. The centrifugation is generally carried out at 2000-5000RPM, preferably 3500-4000RPM, and then it is best to use an organic solvent such as toluene to wash the collected precipitate several times to obtain a neutral pigment particle product. The synthesis of the charged pigment particles comprises: mixing 20-35 of pigment particles with 20-35 of polymer monomer, 0.1-5 of coupling agent and 0.001-5 of polymer reaction chain initiator in 30-60 of dispersion solvent in a temperature range of 30-120 degrees, by weight, and reacting for 12-16 hours under nitrogen protection. The coupling agent for preparing the charged pigment particles is generally selected from silane, which tends to form charged particles.

[0051] 2) Preparation of charged pigment particles: The process for preparing charged particles is basically similar to the process for preparing neutral particles mentioned above, wherein the coupling agent for preparing positively or negatively charged particles is silane, but the functional groups are different, the electron-withdrawing group is negatively charged, and the electron-donating group is positively charged, so that the charged behavior of the particles can be controlled. For example: a coupling agent with an electron-withdrawing functional group such as an acrylic functional group makes the particles negatively charged, while a coupling agent with an electron-donating functional group such as an amino group makes the particles positively charged.

[0052] 3) preparing an electrophoretic display liquid: mixing 5-30 parts by weight of charged pigment particles with 20-70 parts by weight of a dispersing solvent, and performing ultrasonic dispersion, the ultrasonic dispersion time is generally 10-60 minutes, preferably 20-30 minutes, to obtain a dispersion liquid; then placing 5-30 parts by weight of neutral pigment particles in the dispersion liquid under ultrasonic conditions, and continuing ultrasonic dispersion, the ultrasonic dispersion time is generally 10-60 minutes, preferably 20-30 minutes, to obtain an electrophoretic display liquid. At this time, if the dispersion liquid is fully mixed, the obtained electrophoretic display liquid has a better effect.

[0053] Preferably, the step of preparing the electrophoretic display liquid may further include the step of adding 0.1-10 parts by weight of a thickening stabilizer to the electrophoretic display liquid. Wherein, the step of adding the thickening stabilizer is specifically: 5-30 parts by weight of charged pigment particles are mixed with 18-60 parts by weight of a dispersion solvent, and ultrasonic dispersion is performed to obtain a dispersion liquid. Then, 5-30 parts by weight of neutral pigment particles are placed in the dispersion liquid under ultrasonic state, and ultrasonic dispersion is continued to form a solution by dissolving 0.1-10 parts by weight of a thickening stabilizer in 2-10 parts by weight of a dispersion solvent, and then the solution is added to the above dispersion liquid to obtain an electrophoretic display liquid. Wherein, the electrophoretic display liquid is preferably composed of: the total weight of the dispersion solvent is 40-60; the weight of the charged pigment particles is 10-20; the weight of the neutral pigment particles is 10-20; the weight of the thickening stabilizer is 0.5-5. The synthesis method of the neutral pigment particles comprises: mixing the pigment particles with a polymer monomer, a coupling agent and a polymer reaction chain initiator in a dispersion solvent, and reacting them at a temperature range of 30-120 degrees for 4-48 hours.

[0054] The dispersion solvent for preparing the neutral pigment particles and the charged pigment particles includes various non-polar and / or low-polar organic solvents and mixtures thereof. The low-polar dispersion solvent includes but is not limited to various aromatic hydrocarbons such as toluene, benzene, xylene, and halogenated hydrocarbons such as but not limited to chloroform, tetrachloroethylene, etc.; the non-polar dispersion solvent includes but is not limited to various straight-chain, branched and cyclic aliphatic hydrocarbons such as but not limited to n-hexane, nonane, deoxynane, synthetic isomerized paraffin (Isopar), synthetic paraffin (Norpar), synthetic cycloalkanes (Nappar), synthetic alkanes (Varsol / Naphtha), cyclohexane and halogenated hydrocarbons such as but not limited to carbon tetrachloride, etc.

[0055] The thickening stabilizer for preparing the electrophoretic display liquid can be a non-polar polymer, including but not limited to polymethyl methacrylate, polyethylene, polypropylene, rubbers such as polyisoprene, polyisobutylene, etc., among which polymethyl methacrylate, polyisoprene, and polyisobutylene are the best choices.

[0056] In addition, other ingredients required for preparing electrophoretic display liquid and display device may be added when preparing electrophoretic display liquid, such as but not limited to charge control agent, surface tension control agent, dispersing wetting agent and their combination.

[0057] 3. Combine the electrophoretic liquid prepared in the second step with the transparent barrier to produce an electrophoretic display cavity.

[0058] In this embodiment, the electrophoretic electronic paper manufactured by the above manufacturing method has good separation and conductivity, and can avoid the adsorption problem of metal oxides and charged particles on the surface of the common electrode. At the same time, the electrophoretic electronic paper has a long service life and low maintenance cost.

[0059] Although the preferred embodiments of the present application have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications falling within the scope of the present application.

[0060] Obviously, those skilled in the art can make various changes and modifications to the present application without departing from the spirit and scope of the present application. Thus, if these modifications and variations of the present application fall within the scope of the claims of the present application and their equivalents, the present application is also intended to include these modifications and variations.

Claims

1. An isolation film used for electrophoretic electronic paper, characterized in that: The isolation film is arranged on the surface of at least one of the common electrode or the pixel electrode of the electrophoretic electronic paper to isolate the electrophoretic pigment particles from being adsorbed by either the common electrode or the pixel electrode. The molecular structure of the isolation film material contains both electron-withdrawing groups and electron-donating groups.

2. The isolation film for electrophoretic electronic paper according to claim 1, characterized in that: The thickness of the isolation film is 0.001 to 25 microns.

3. The isolation film for electrophoretic electronic paper according to claim 1, characterized in that: The ratio between the electron donating group and the electron withdrawing group in the isolation film is controlled to be 1:5 to 5:

1.

4. The isolation film for electrophoretic electronic paper according to claim 1, characterized in that: The ratio between the electron donating group and the electron withdrawing group in the isolation film is controlled to be 1:2 to 2:

1.

5. The isolation film for electrophoretic electronic paper according to claim 1, characterized in that: The transmittance of the isolation film disposed on the surface of the common electrode is greater than or equal to 80%.

6. The isolation film for electrophoretic electronic paper according to claim 1, characterized in that: The volume resistivity of the isolation film is less than or equal to 10 15 Ω·cm.

7. An electrophoretic electronic paper, comprising an electrophoretic display cavity surrounded by a common electrode, a pixel electrode and an edge sealing structure, wherein the display cavity comprises at least two kinds of pigment electrophoretic particles and a solution, wherein the pigment electrophoretic particles are wrapped by the solution, characterized in that: The isolation film according to any one of claims 1 to 6 is applied, and the isolation film is arranged on the surface of the common electrode and / or the pixel electrode.

8. The electrophoretic electronic paper according to claim 7, characterized in that: The electrophoretic display cavities are separated by a plurality of transparent isolation members, and the electrophoretic display cavities separated by the transparent isolation members are connected or disconnected.

9. The electrophoretic electronic paper according to claim 8, characterized in that: The cross section of the transparent isolation piece is a regular shape, such as a square, a circle, a triangle, a trapezoid, a pentagon, a hexagon, an ellipse or other shapes and irregular shapes.

10. A method for manufacturing electrophoretic electronic paper, characterized in that: Use the isolation film as claimed in any one of claims 1 to 6.

Citation Information

Patent Citations

  • Difference electric charge color electrophoresis type display device

    CN107065375A

  • Method and composition for improving performance of cataphoresis display

    CN1469177A

  • Electrophoretic particle, electrophoretic particle dispersion liquid, image display medium, and image display

    JP2010271638A

  • Electrode protection film for electrophoretic displays

    US20050264869A1