Etching method for removing chromium residues in PSM manufacturing process
By adjusting the bias voltage after main etching in the ICP machine, only chemical etching is used to remove chromium residues in the phase deflection mask, the phase error problem caused by chromium residues is solved, and efficient chromium residue removal is achieved, ensuring the product Quality and process efficiency.
Patent Information
- Application Number
- CN202410997185.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-12
AI Technical Summary
The existing phase deflection masks are prone to chromium residues during the etching process, resulting in phase errors and affecting wafer production yields. The existing methods require the removal of residues in combination with wet chemical etching, which has a long process time and high cost.
After the main etching is performed in the ICP machine, the bias voltage is adjusted to zero, and only chemical etching is used to remove chromium residues in the center. The radio frequency power supply of the ICP machine is used to generate reaction gas for physical bombardment and chemical reactions, ensuring the Mosi layer and the two Protection of silicon oxide layer.
Effectively remove chromium residues in the center of the photocoat, ensure product quality integrity, shorten process time and reduce costs, and ensure etching rate and product quality.
Smart Images

Figure CN118938613A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of photomask manufacturing process, and in particular to an etching method for removing chromium residues in a PSM process. Background Art
[0002] Phase Shift Mask (PSM) is a resolution enhancement technology that uses both the intensity and phase of light to form an image and obtain a higher resolution. For phase deflection masks, the product must ensure that there is no Cr on the surface of the Mosi in the pattern area. Cr on the surface of the Mosi will cause phase error and seriously affect the production yield of the wafer. Therefore, the control of surface Cr residue is crucial for mask production and is an important indicator of mask product yield and quality.
[0003] The etching of Cr on the existing phase shift mask is a combination of chemical etching and physical etching, usually using an ICP machine. The etching principle is that under the action of the etching gas (O2 / Cl2) at the upper electrode frequency of 13.56 MHz, the peripheral free electrons are easy to break free and become ions due to their light weight, and the remaining is polymer. Ions mainly play a role in physical bombardment, and polymers mainly play a role in chemical etching. The chemical etching direction of ICP plasma is rotary, and the physical bombardment of a smaller bias voltage and chemical etching synergistically enhance the etching rate. This part of the etching rate is about ten times that of chemical etching alone. Since the directionality of chemical etching is rotary, it is necessary to reduce the etching of silicon dioxide in the central area of the mask while ensuring that the phase (phase) and trans (penetration) of the phase shift mask meet the required standards. Therefore, the central position is prone to insufficient etching, resulting in such agglomerated but small-sized Cr residues (residual), which need to be removed by wet chemical etching, which greatly prolongs the process time and increases the cost. Summary of the invention
[0004] The present invention aims to provide a method to solve the existing problems.
[0005] The specific plan is as follows:
[0006] 1. An etching method for removing chromium residue in a PSM process, characterized in that it comprises the following steps:
[0007] S1. Providing a photomask substrate, wherein the substrate has a MoSi layer, the MoSi layer is covered with a Cr layer, and the Cr layer is further covered with a photoresist; after the photomask substrate is subjected to a pattern drawing, exposure and development process, the photoresist in the pattern area is removed;
[0008] S2, placing the photomask substrate into the ICP machine, using the radio frequency power supply of the ICP machine to generate highly reactive ions and electrons from the reaction gas, physically bombarding and chemically reacting the Cr layer, and etching away the Cr layer in the area not covered by the photoresist;
[0009] S3. After the main etching of the Cr layer is completed, the bias voltage of the ICP machine is adjusted to zero, and only the Cr residue in the center is removed by chemical etching.
[0010] Furthermore, in the process of step S2, the RF power of the ICP machine is 220-300w, the bias voltage is 10-20w, and the gas ratio is O2 : Cl2=1:6.
[0011] Furthermore, in the process of step S3, the RF power of the ICP machine is 220-300w, the bias voltage is 0, and the gas ratio is O2:Cl2=1:6.
[0012] Compared with the prior art, the etching method for removing chromium residues in the PSM process provided by the present invention has the following advantages: the etching method for removing chromium residues in the PSM process provided by the present invention is to adjust the bias voltage to zero after completing the main etching process in the ICP machine, and only use chemical etching to remove the central Cr residues. Since simple chemical etching only has chemical reactions, the time rate of chlorine oxygen plasma for the MoSi layer and the silicon dioxide layer is much lower than the etching rate of Cr. Therefore, this etching combination can be used to remove the central Cr residues while ensuring that the phase and penetration of the MoSi layer meet the requirements, thereby ensuring the integrity of product quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 A schematic diagram of the etching process flow is shown.
[0014] Figure 2 The schematic diagram shows the structure after completing the process of step S1.
[0015] Figure 3 The schematic diagram shows the structure after completing step S2 process.
[0016] Figure 4 The schematic diagram shows the structure after the step S3 process is completed.
[0017] Figure 5 This is the SEM image of sample 1.
[0018] Figure 6 This is the SEM image of sample 2. DETAILED DESCRIPTION
[0019] To further illustrate the various embodiments, the present invention provides drawings. These drawings are part of the disclosure of the present invention, which are mainly used to illustrate the embodiments and can be used in conjunction with the relevant descriptions in the specification to explain the operating principles of the embodiments. With reference to these contents, a person of ordinary skill in the art should be able to understand other possible implementations and advantages of the present invention. The components in the figures are not drawn to scale, and similar component symbols are generally used to represent similar components.
[0020] The present invention will now be further described with reference to the accompanying drawings and specific implementation methods.
[0021] The present invention provides an etching method for removing chromium residue in a PSM process, referring to Figure 1-Figure 4 The specific implementation of this method includes the following steps:
[0022] S1. Provide a photomask substrate, wherein the substrate 1 has a MoSi layer 2, the MoSi layer 2 is covered with a Cr layer 3, and the Cr layer is also covered with a photoresist 4. It should be noted that the substrate is usually made of quartz glass, and the formation of the MoSi layer and the Cr layer on the substrate, as well as the pattern drawing, exposure and development process are all existing technologies, and the specific process technology is not described in detail here. Figure 2 In the structure shown in FIG. 1 , the Cr layer on the MoSi layer that is not covered by the photoresist needs to be etched away.
[0023] S2. Place the photomask substrate into the ICP machine for etching. Specifically, the RF power of the ICP machine is used to make the reaction gas (O2 / Cl2) generate highly reactive ions and electrons to physically bombard and chemically react the Cr layer. The RF power is 220-300W, the bias voltage is 10-20W, the gas ratio is O2:Cl2=1:6, and the pressure is 3mtorr. The Cr layer and MoSi layer in the area not covered by the photoresist are etched away. The directionality of the chemical etching of the ICP machine is rotary. While ensuring that the phase (phase) and trans (penetration) of the phase shift mask meet the required standards, it is easy to under-etch in the center, resulting in agglomerated but small-sized Cr residues 5 (such as Figure 3 shown).
[0024] S3. After the main etching of the Cr layer is completed, the dry chemical etching time is extended in the ICP machine, that is, during this extended time, the bias voltage is adjusted to zero (so as not to use physical etching to protect the phase transfer Mosi layer), (RF power 220-300w, bias voltage 0w, gas ratio O2:Cl2=1:6, pressure 3mtorr, only chemical etching is used to remove the Cr residue in the center. Since the pure chemical etching has only chemical reaction, the etching rate of chlorine oxygen plasma for the Mosi layer is much lower than the etching rate of Cr. Therefore, this etching combination can only remove the Cr residue in the center, while ensuring that the phase and penetration of the Mosi layer meet the requirements, and ensure the integrity of product quality (such as Figure 4 shown).
[0025] The etching method for removing chromium residue in the PSM process provided by the present invention is to adjust the bias voltage to zero after completing the main etching process in the ICP machine without affecting the product properties, and only use chemical etching to remove the central Cr residue. Since the simple chemical etching only has chemical reaction, the time rate of chlorine oxygen plasma for the MoSi layer and the silicon dioxide layer is much lower than the etching rate of Cr. Therefore, this etching combination can be used to remove the central Cr residue under the premise of ensuring that the phase and penetration of the MoSi layer meet the requirements, thereby ensuring the integrity of product quality.
[0026] A comparative example is now used to prove that the method provided by the present invention can effectively remove Cr residues. Sample 1 is a photomask product made using an existing process, and sample 2 is a product made using the etching method provided by the present invention. The difference between the two is that after the Cr layer is etched, the bias voltage of the ICP machine is adjusted to zero for sample 2, and only simple chemical etching is used for etching, and the etching time is 6-8 minutes. The SEM image of the sample after etching is shown in FIG. Figure 5 and Figure 6 ,in Figure 5 is the SEM image of sample 1. Figure 6 This is the SEM image of sample 2. It can be seen from the image that sample 1 still has a lot of Cr residue in the central area, and sample 2 has almost no Cr residue in the central area, which proves that the method provided by the present invention can effectively remove Cr residue.
[0027] Although the present invention has been specifically shown and described in conjunction with the preferred embodiments, it should be understood by those skilled in the art that various changes may be made to the present invention in form and details without departing from the spirit and scope of the present invention as defined by the appended claims, all of which are within the scope of protection of the present invention.
Claims
1. An etching method for removing chromium residue in a PSM process, characterized in that: The following steps are involved: S1. Providing a photomask substrate, wherein the substrate has a MoSi layer, the MoSi layer is covered with a Cr layer, and the Cr layer is further covered with a photoresist; after the photomask substrate is subjected to a pattern drawing, exposure and development process, the photoresist in the pattern area is removed; S2, placing the photomask substrate into the ICP machine, using the radio frequency power supply of the ICP machine to generate highly reactive ions and electrons from the reaction gas, physically bombarding and chemically reacting the Cr layer, and etching away the Cr layer in the area not covered by the photoresist; S3. After the main etching of the Cr layer is completed, the bias voltage of the ICP machine is adjusted to zero, and only the Cr residue in the center is removed by chemical etching.
2. The etching method according to claim 1, characterized in that: In the process of step S2, the RF power of the ICP machine is 220-300w, the bias voltage is 10-20w, and the gas ratio is O2:Cl2=1:
6.