High-temperature-resistant and high-humidity-resistant capacitor and preparation method thereof
Patent Information
- Application Number
- CN202411121829.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-12
AI Technical Summary
The existing capacitors are insufficient in high temperature and high humidity environments, resulting in deterioration of electrical parameters and failure of functions. The existing waterproof materials have poor moisture and gas permeability, poor mechanical properties, poor heat dissipation performance, as well as anti-mold, anti-corrosion and anti-salt spray capabilities. Limited, and the impregnation and spraying processes have problems such as pore blockage, uneven thickness, risk of organic solvent peeling and shrinkage pressure.
The vacuum air phase deposition process is used to deposit the Parelin material on the capacitor core or packaging surface to form a dense protective film layer, which is enhanced by plasma cleaning and silane coupling agent pretreatment, and is cracked at high temperature to form The monomers are polymerized and deposited to avoid solvent and thermal stress problems.
It realizes a protective film with high coverage, no pinholes and good airtightness, enhances the waterproof performance and high temperature and humidity resistance of the capacitor, avoids changes in electrical parameters and functional failures, and extends the life of the capacitor.
Smart Images

Figure CN118942913A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of capacitor preparation, and in particular relates to a high temperature and high humidity resistant capacitor and a preparation method thereof. Background Art
[0002] The existing organic polymer chip tantalum capacitors and organic polymer laminated aluminum capacitors have structures such as Fig. 9 , 10 As shown, due to its non-airtight packaging in the form of molded and the use of easily absorbent conductive polymer as the cathode electrolyte layer of the capacitor, it is a moisture-sensitive electronic component. Moisture-sensitive devices are affected by temperature and humidity during storage, installation, and use. For example, when water vapor enters, reflow soldering installation will cause the capacitor to crack. At the same time, the electrical parameters of the capacitor core are very likely to deteriorate under the presence of water vapor conditions, resulting in its functional failure. With the emergence of high temperature, high humidity, and high salt fog application environments such as islands, caves, and oceans, organic polymer chip tantalum capacitors and organic polymer laminated aluminum capacitors produced by current processes can no longer guarantee long life and high reliability. In order to solve this problem, some manufacturers have focused on the research of high temperature and humidity resistant organic polymer chip tantalum capacitors and organic polymer laminated aluminum capacitors, and launched "double 85" (85℃, 85%RH) products. The main solution is to impregnate or spray waterproof materials to enhance the sealing of the capacitor and the moisture resistance of the core.
[0003] Patent document with publication number CN112164591A discloses a manufacturing method for improving the high temperature and high humidity tolerance of laminated aluminum electrolytic capacitors. In the patent, the capacitors after molded packaging are immersed in a silicone solution to prevent water vapor from entering the core and causing parameter degradation.
[0004] Patent document with publication number CN110459406A discloses a solid electrolytic capacitor for use under high temperature and high humidity conditions. In the patent, a hydrophobic elastomer material composed of silicone, fluoropolymer, etc. is coated on the capacitor core body to improve the core's waterproofness.
[0005] Patent document with publication number CN110233052A discloses a capacitor and a method for preparing the same. In the patent, the surface of the capacitor core group is coated or impregnated with an elastomeric material to enhance the waterproofness.
[0006] Disadvantages of existing capacitor waterproof materials:
[0007] 1. The waterproof materials selected in the prior art, such as organic polysiloxane, organic fluorine polymer, silicone and other materials, have relatively poor moisture and gas permeability and limited water blocking ability;
[0008] 2. The mechanical properties of the film after forming are poor. When the film is molded and injected for packaging, it cannot withstand the impact of the molding material and is easy to fall off, and the effect of full coverage cannot be achieved;
[0009] 3. The heat dissipation performance is relatively poor. When the capacitor is working, the heat generated cannot be dissipated in time, which will cause heat accumulation and reduce the lifespan;
[0010] 4. The ability to resist mildew, corrosion, salt spray, acid and alkali is limited.
[0011] Disadvantages of existing dipping, spraying or brushing processes:
[0012] 1. Liquid coating forms a protective layer on the surface of the device by dipping, spraying or brushing. In this process, it is easy to block small pores, produce bubbles, thick thickness, uneven thickness, etc., thus failing to achieve a better waterproof effect.
[0013] 2. The liquid coating contains a large amount of organic solvents. When it is processed by dipping, brushing and other processes, there is a risk of peeling between the layers of the capacitor core;
[0014] 3. When the liquid coating is cured at high temperature, there will be shrinkage pressure, resulting in insufficient coverage at the edges of the capacitor. Summary of the invention
[0015] In order to solve the above technical problems, the present invention provides a high temperature and high humidity resistant capacitor and a preparation method thereof.
[0016] The present invention is achieved through the following technical solutions.
[0017] The present invention provides a method for preparing a high temperature and high humidity resistant capacitor, comprising the steps of depositing a parylene material on a surface of a capacitor core or a surface of a package body using a vacuum vapor deposition process to form a protective film layer.
[0018] Preferably, a method for preparing a high temperature and high humidity resistant capacitor comprises the following steps:
[0019] S1: shielding the lead frame;
[0020] S2: Processing the lead frame;
[0021] S3: plasma cleaning;
[0022] S4: silane coupling agent pretreatment;
[0023] S5: Perform vacuum vapor deposition process, and then perform molding packaging after deposition. The subsequent production process is the same as that of conventional organic polymer tantalum chip capacitors and organic polymer laminated aluminum capacitors.
[0024] Preferably, the step S1 comprises: shielding the capacitor leads to be bonded to the lead frame to form a shielding layer, wherein the shielding material is polytetrafluoroethylene tape.
[0025] Preferably, the step S2 comprises: etching a groove at the junction of the lead frame and the epoxy resin by laser to enhance the bonding force of the parylene material, and this step can be processed before the capacitor core is bonded to the lead frame;
[0026] The step S3 includes: using argon gas in plasma cleaning.
[0027] Preferably, the groove has a width of 2 μm to 20 μm, a depth of 2 μm to 20 μm, an interval between each groove of 2 μm to 20 μm, and the groove is a rectangular parallelepiped or an elliptical cylinder.
[0028] Preferably, step S4 comprises: spraying or dipping a silane coupling agent on the surface of the lead frame at the treatment location, and then drying and solidifying, wherein the concentration of the silane coupling agent comprises 0.5%wt-20%wt, the solvent comprises one or more of water, ethanol, n-butanol, acetone, ether, and xylene, and the silane coupling agent comprises one or more of γ-aminopropyltriethoxysilane, γ-glycidyloxypropyltrimethoxysilane, γ-(methacryloyloxy)propyltrimethoxysilane, monoaminoethyl)γ-aminopropyltrimethoxy(ethyl)silane, and Nβ-(aminoethyl)γ-aminopropylmethyldimethoxysilane;
[0029] Preferably, step S4 comprises: preparing a silane coupling agent solution with a weight percentage of 1% to 10% using a solvent, immersing the assembled lead frame in the silane coupling agent solution for 10s to 300s, and then drying in an oven at 60°C to 120°C for 10min to 60min.
[0030] Preferably, the vacuum vapor deposition process in step S5 comprises the following steps:
[0031] S1: vaporizing and sublimating the solid parylene dimer material at a temperature of 90 to 130°C;
[0032] S2: cleaving the parylene dimer at a temperature of 660-700°C to form parylene monomers;
[0033] S3: Parylene monomers are polymerized and deposited on the surface of the capacitor at 25-35°C, eventually forming a dense protective film layer.
[0034] Preferably, the protective film layer has a thickness of 1 μm to 100 μm.
[0035] A capacitor prepared by the above preparation method.
[0036] The beneficial effects of the present invention are:
[0037] The protective film of the present invention is prepared by vacuum vapor deposition process, and is a conformal polymer film coating grown by active small molecules on the surface of the substrate, so the coverage on the surface of the coating material is high, and dead corners are avoided.
[0038] The deposition process of the present invention is to heat and gasify the xylene ring dimer and then pyrolyze it into free gas phase molecules at high temperature, and then instantly adsorb it on the substrate under vacuum and room temperature conditions to form a film, thereby forming a protective film with good airtightness. Since the material does not contain solvent, it overcomes the disadvantage of the solvent-based coating used in the past that many tiny pinholes are left due to the evaporation of the solvent during the drying process, and can provide a truly pinhole-free protective film.
[0039] Parylene coating can be applied to product surfaces of various shapes, including sharp edges, cracks and inner surfaces. Because there is no liquid in the deposition process of Parylene coating, there will be no problems such as hanging flow, bubbles, bridged meniscus, and uneven thickness that occur during the coating process of liquid coating. Deposition at room temperature will not cause thermal stress to sensitive parts of the product to be coated, and there is no solvent, so it will not damage the coated device. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 It is a process flow chart of the present invention;
[0041] Figure 2 is a schematic diagram of the shielding layer and the groove of the present invention;
[0042] Figure 3 is a schematic diagram of the shielding layer and the groove of the present invention;
[0043] Figure 4 It is a schematic structural diagram of the protective film layer of the present invention;
[0044] Figure 5 It is a schematic structural diagram of the protective film layer of the present invention;
[0045] Figure 6 This is a physical picture of a capacitor prepared by the process of the present invention;
[0046] Figure 7 This is a physical picture of a capacitor prepared by the process of the present invention;
[0047] Figure 8 This is a physical picture of a capacitor prepared by the process of the present invention;
[0048] Fig. 9 This is a diagram of the structure of an organic polymer chip tantalum capacitor;
[0049] Fig.10 Organic polymer chip aluminum capacitor structure diagram;
[0050] In the figure: 1- shielding layer, 2- groove. DETAILED DESCRIPTION
[0051] The technical solution of the present invention is further described below, but the scope of protection claimed is not limited to the description.
[0052] A method for preparing a high temperature and high humidity resistant capacitor comprises the steps of depositing a parylene material on the surface of a capacitor core or a packaging body by a vacuum vapor deposition process to form a complete and dense protective film layer.
[0053] A method for preparing a high temperature and high humidity resistant capacitor comprises the following steps:
[0054] S1: shielding the lead frame;
[0055] S2: Processing the lead frame;
[0056] S3: plasma cleaning;
[0057] S4: silane coupling agent pretreatment;
[0058] S5: Perform vacuum vapor deposition process, perform molding and packaging after deposition, remove the shielding layer after packaging, and the subsequent production process is the same as that of conventional organic polymer chip tantalum capacitors and organic polymer laminated aluminum capacitors. The shielding layer can also be omitted, and the protective film layer at this location can be removed by sandblasting, laser, grinding, etc. after molding and packaging.
[0059] The step S1 includes: shielding the capacitor lead that needs to be bonded to the lead frame to form a shielding layer 1 to prevent the parylene coating from being deposited on the lead. The shielding material is a polytetrafluoroethylene tape. The advantages of the tape are high temperature resistance, stable chemical properties, good acid and alkali resistance, moderate adhesion, and it is not easy for the lead frame to have residual glue when the tape is removed.
[0060] The step S2 includes: etching a groove 2 at the junction of the lead frame and the epoxy resin by laser to enhance the bonding force of the parylene material. This step can be performed before the capacitor core is bonded to the lead frame. The groove 2 has a width of 2 μm to 20 μm and a depth of 2 μm to 20 μm. Each groove is spaced 2 μm to 20 μm apart. The groove 2 is a rectangular parallelepiped or an elliptical cylinder.
[0061] The step S3 includes: using plasma cleaning to remove surface pollutants, which can significantly enhance the adhesion of the surface. Argon is used in plasma cleaning. The principle is that in a vacuum chamber, a radio frequency power source is ignited under a certain pressure to generate a high-energy disordered plasma. The plasma bombards the surface of the cleaned product. The active plasma performs a dual effect of physical bombardment and chemical reaction on the cleaned object, so that the surface material of the cleaned object is converted into particles and gaseous substances, which are discharged through vacuum pumping to achieve the cleaning purpose. During the cleaning process, the power is 100w~300w, the pressure is 0.15Torr~0.22Torr, the time is 10s~60s, and the gas flow rate is 3cc / min~10cc / min. The cleaning principle is as follows:
[0062] Ar+e→Ar + +2e - →Ar + +Cx
[0063] The step S4 comprises: spraying or dipping a silane coupling agent on the surface of the lead frame where the lead frame is to be treated, and then drying and solidifying. The concentration of the silane coupling agent comprises 0.5%wt to 20%wt, preferably 1%wt to 10%wt, and particularly preferably 2%wt to 5%wt. The solvent comprises one or more of water, ethanol, n-butanol, acetone, ether, and xylene. The type of silane coupling agent comprises: the silane coupling agent comprises: one or more of γ-aminopropyltriethoxysilane, γ-glycidyloxypropyltrimethoxysilane, γ-(methacryloyloxy)propyltrimethoxysilane, monoaminoethyl)γ-aminopropyltrimethoxysilane, and Nβ-(aminoethyl)γ-aminopropylmethyldimethoxysilane.
[0064] The step S4 comprises: preparing a silane coupling agent solution with a weight percentage of 1% to 10% using a solvent, immersing the assembled lead frame in the silane coupling agent solution for 10s to 300s, and then drying in an oven at 60°C to 120°C for 10min to 60min.
[0065] The vacuum vapor deposition process in step S5 comprises the following steps:
[0066] S1: vaporizing and sublimating the solid parylene dimer material at a temperature of 90 to 130°C;
[0067] S2: The sublimated dimer gas enters the cracking chamber, and the parylene dimer is cracked at a temperature of 660-700°C. The molecular bonds of the dimer are broken to form active parylene monomers with two dangling bonds.
[0068] S3: Parylene monomer is polymerized and deposited on the surface of the capacitor in a vacuum deposition chamber at 25-35°C, eventually forming a dense protective film layer.
[0069] The thickness of the protective film layer is 1 μm to 100 μm, particularly preferably 5 μm to 50 μm, and further preferably 10 μm to 20 μm. The protective film layer has good waterproof performance.
[0070] Embodiment 1:
[0071] like Figure 1-8 As shown, a method for preparing a high temperature and high humidity resistant capacitor includes the steps of depositing a parylene material on the surface of a capacitor core or a packaging body using a vacuum vapor deposition process to form a protective film layer.
[0072] A method for preparing a high temperature and high humidity resistant capacitor comprises the following steps:
[0073] S1: shielding the lead frame;
[0074] S2: Processing the lead frame;
[0075] S3: plasma cleaning;
[0076] S4: silane coupling agent pretreatment;
[0077] S5: Perform vacuum vapor deposition process, and then perform molding packaging after deposition. The subsequent production process is the same as that of conventional organic polymer tantalum chip capacitors and organic polymer laminated aluminum capacitors.
[0078] The step S1 includes: shielding the capacitor leads that need to be bonded to the lead frame to form a shielding layer 1, and the shielding material is polytetrafluoroethylene tape.
[0079] The step S2 comprises: etching a groove 2 at the junction of the lead frame and the epoxy resin by laser to enhance the bonding force of the parylene material, and this step can be performed before the capacitor core is bonded to the lead frame;
[0080] The step S3 includes: using argon gas in plasma cleaning.
[0081] The groove 2 has a width of 10 μm and a depth of 10 μm, and each groove is spaced 15 μm apart. The groove 2 is an elliptical cylinder.
[0082] The step S4 comprises: spraying or dipping a silane coupling agent on the surface of the lead frame treatment area, and then drying and solidifying, wherein the concentration of the silane coupling agent is 10%wt, the solvent comprises water, ethanol, n-butanol, acetone, ether, and xylene, and the silane coupling agent comprises: γ-aminopropyl triethoxysilane, γ-glycidyloxypropyl trimethoxysilane, γ-(methacryloyloxy)propyl trimethoxysilane, monoaminoethyl)γ-aminopropyl trimethoxy(ethyl)silane, and Nβ-(aminoethyl)γ-aminopropyl methyldimethoxysilane;
[0083] Step S4 includes: preparing a 6% by weight silane coupling agent solution using a solvent, immersing the assembled lead frame in the silane coupling agent solution for 180 seconds, and then drying in a 90° C. oven for 40 minutes.
[0084] The vacuum vapor deposition process in step S5 comprises the following steps:
[0085] S1: vaporizing and sublimating the solid parylene dimer material at a temperature of 110°C;
[0086] S2: cleaving the parylene dimer at 680°C to form parylene monomers;
[0087] S3: Parylene monomers are polymerized and deposited on the surface of the capacitor at 28°C, eventually forming a dense protective film layer.
[0088] The thickness of the protective film layer is 10 μm to 20 μm.
[0089] Comparative Example 1:
[0090] The conductive polymer laminated aluminum capacitor prepared using the existing technology includes the following steps: assembling (assembling aluminum foil and welding it to steel bars for mass production) → chemical repair (repairing the dielectric layer damaged by cutting) → polymerization (coating with conductive high polymer to form the cathode layer of the capacitor) → impregnating graphite and silver paste to lead out the cathode → lamination (according to the capacity design, bonding the multi-layer aluminum capacitor core to the lead frame to lead out the positive and negative electrodes of the capacitor) → molding (epoxy resin packaging) → aging and other screening → finished product measurement → taping packaging.
[0091] Comparative Example 2:
[0092] The conductive polymer tantalum capacitor prepared using the existing technology includes the following steps: tantalum powder pressing and molding → sintering (capacitor anode body formation) → forming (capacitor dielectric layer formation) → polymerization (coating with conductive high polymer, capacitor cathode layer formation) → impregnation with graphite and silver paste to lead out the cathode → bonding (bonding to the lead frame to lead out the positive and negative electrodes of the capacitor) → molding (epoxy resin encapsulation) → aging and screening after aging → finished product measurement → taping packaging.
[0093] like Fig. 9 , 10 As shown, the capacitors prepared in Example 1, Comparative Examples 1 and 2 were subjected to high temperature and high humidity tests, wherein the method of Example 1 was used to prepare organic polymer chip aluminum capacitors and organic polymer chip tantalum capacitors, respectively, and the results are shown in Table 1 and Table 2:
[0094] Table 1 Comparison of high temperature and high humidity parameters of laminated aluminum 25V33μF-D shell
[0095]
[0096] As shown in Table 1, the electrical parameters of the 25V33μF-D shell specification laminated aluminum capacitor prepared by conventional process and prepared by the present invention are compared after applying DC voltage for 1000 hours under the conditions of 85°C and 85% RH. It can be seen that the capacitor prepared by conventional process has cracked and failed after 1000 hours, while the present invention can make the electrical parameters of the capacitor sample still change very little after being powered on and working for 1000 hours under the conditions of 85°C and 85% RH.
[0097] Table 2 Comparison of high temperature and high humidity parameters of organic polymer chip tantalum capacitor 50V68μF-F1 shell
[0098]
[0099]
[0100] As shown in Table 2, there is a comparison of electrical parameters of 50V68μF-F1 shell specification organic polymer chip tantalum capacitors prepared by conventional process and prepared by the present invention after applying DC voltage for 1000 hours at 85°C and 85% RH. It can be seen that the capacitor prepared by conventional process has short-circuited and failed after 1000 hours, while the present invention can make the electrical parameters of the capacitor sample still change very little after being powered on and working for 1000 hours at 85°C and 85% RH.
Claims
1. A method for preparing a high temperature and high humidity resistant capacitor, characterized in that: The method comprises the steps of using a vacuum vapor deposition process to deposit the parylene material on the surface of the capacitor core or the surface of the package to form a protective film layer.
2. The method for preparing a high temperature and high humidity resistant capacitor according to claim 1, characterized in that: The following steps are involved: S1: shielding the lead frame; S2: Processing the lead frame; S3: plasma cleaning; S4: silane coupling agent pretreatment; S5: Perform vacuum vapor deposition process, and then perform molding packaging after deposition. The subsequent production process is the same as that of conventional organic polymer tantalum chip capacitors and organic polymer laminated aluminum capacitors.
3. The method for preparing a high temperature and high humidity resistant capacitor according to claim 2, characterized in that: The step S1 comprises: shielding the capacitor leads that need to be bonded to the lead frame to form a shielding layer (1), wherein the shielding material is polytetrafluoroethylene tape.
4. The method for preparing a high temperature and high humidity resistant capacitor according to claim 2, characterized in that: The step S2 comprises: etching a groove (2) at the junction of the lead frame and the epoxy resin by laser to enhance the bonding force of the parylene material, and this step can be performed before the capacitor core is bonded to the lead frame; The step S3 includes: using argon gas in plasma cleaning.
5. The method for preparing a high temperature and high humidity resistant capacitor according to claim 4, characterized in that: The groove (2) has a width of 2 μm to 20 μm and a depth of 2 μm to 20 μm, each groove is spaced 2 μm to 20 μm apart, and the groove (2) is a rectangular parallelepiped or an elliptical cylinder.
6. The method for preparing a high temperature and high humidity resistant capacitor according to claim 2, characterized in that: The step S4 comprises: spraying or dipping a silane coupling agent on the surface of the lead frame where the lead frame is to be treated, and then drying and solidifying. The concentration of the silane coupling agent comprises 0.5%wt to 20%wt. The solvent comprises one or more of water, ethanol, n-butanol, acetone, ether, and xylene. The silane coupling agent comprises one or more of γ-aminopropyltriethoxysilane, γ-glycidyloxypropyltrimethoxysilane, γ-(methacryloyloxy)propyltrimethoxysilane, monoaminoethyl)γ-aminopropyltrimethoxysilane, and Nβ-(aminoethyl)γ-aminopropylmethyldimethoxysilane.
7. The method for preparing a high temperature and high humidity resistant capacitor according to claim 2, characterized in that: Step S4 includes: preparing a silane coupling agent solution with a weight percentage of 1% to 10% using a solvent, immersing the assembled lead frame in the silane coupling agent solution for 10s to 300s, and then drying in an oven at 60°C to 120°C for 10min to 60min.
8. The method for preparing a high temperature and high humidity resistant capacitor according to claim 1, characterized in that: The vacuum vapor deposition process in step S5 comprises the following steps: S1: vaporizing and sublimating the solid parylene dimer material at a temperature of 90 to 130°C; S2: cleaving the parylene dimer at a temperature of 660-700°C to form parylene monomers; S3: Parylene monomers are polymerized and deposited on the surface of the capacitor at 25-35°C, eventually forming a dense protective film layer.
9. The method for preparing a high temperature and high humidity resistant capacitor according to claim 8, characterized in that: The thickness of the protective film layer is 1 μm to 100 μm.
10. A capacitor prepared by the preparation method according to any one of claims 1 to 9.