Glass cover plate and photovoltaic module
By providing an inward recessed portion at an appropriate depth on the first surface of the glass cover plate of the photovoltaic module, stress is dispersed, and the problem of cracks or breakage of the glass cover plate under impact is solved, and the service life of the photovoltaic module is extended.
Patent Information
- Application Number
- CN202411008404.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-07-25
AI Technical Summary
The glass cover plate of photovoltaic modules is prone to cracks or breakage when impacted, affecting the service life of the module.
A plurality of inwardly recessed depressions are provided on the first surface of the glass cover plate. The ratio of the depth of the depression to the thickness of the glass body is between 0.005≤D1/D2≤0.015, which enhances the structural strength of the glass cover plate, disperses the stress, and improves the strength of the glass cover plate. Impact resistance.
Without increasing the thickness and weight of the glass cover, the impact resistance of the glass cover is improved, the risk of cracks or breakage is reduced, and the life of the photovoltaic module is extended.
Smart Images

Figure CN118943221A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of photovoltaic cell technology, and in particular to a glass cover plate and a photovoltaic module. Background Art
[0002] Photovoltaic modules convert solar energy into electrical energy by absorbing sunlight. Photovoltaic modules include glass cover, film, battery cells, backplane and other components. Among them, the glass cover is located at the top of the photovoltaic module. When hail or other objects fall on the surface of the glass cover, the glass cover is easily cracked or even broken by the impact, thus affecting the normal operation of the photovoltaic module. Summary of the invention
[0003] The embodiments of the present application provide a glass cover plate and a photovoltaic module, which are intended to improve the structural strength of the glass cover plate and extend the service life of the photovoltaic module.
[0004] The present application provides a glass cover plate for a photovoltaic module, wherein the glass cover plate comprises:
[0005] A glass body, wherein along the thickness direction of the glass cover plate, the glass body has a first surface and a second surface that are oppositely arranged, the first surface is provided with a plurality of evenly distributed recessed portions, and a gap is formed between the recessed portions located at the edge and the edge of the glass body;
[0006] Along the thickness direction of the glass cover plate, a ratio of a depth D1 of the recessed portion to a thickness D2 of the glass body satisfies: 0.005≤D1 / D2≤0.015.
[0007] In a possible design, a distance D3 between the recessed portion located at the edge position and the edge of the glass body satisfies: 2 mm ≤ D3 ≤ 8.5 mm.
[0008] In a possible design, the depth D1 of the recessed portion satisfies: 10 μm≤D1≤30 μm.
[0009] In a possible design, a cross section of the recessed portion gradually decreases along a direction from the first surface to the second surface.
[0010] In a possible design, along the thickness direction of the glass cover plate, the cross section of the recessed portion is one or more of a circle, a triangle, a rectangle, and a polygon.
[0011] In a possible design, the glass cover plate further includes a porous nano-silicon dioxide film layer, and the porous nano-silicon dioxide film layer is disposed on the first surface.
[0012] In a possible design, the refractive index of the porous nano-silica film layer is 1.28-1.30;
[0013] The thickness of the porous nano-silicon dioxide film layer is 100nm-130nm.
[0014] In a possible design, the glass cover plate further includes a dense silicon dioxide film layer and a porous nano silicon dioxide film layer;
[0015] The dense silicon dioxide film layer is arranged on the first surface, and the porous nano silicon dioxide film layer is arranged on the dense silicon dioxide film layer.
[0016] In a possible design, the refractive index of the porous nano-silica film layer is 1.18-1.20, and the thickness of the porous nano-silica film layer is 100nm-120nm;
[0017] The refractive index of the dense silicon dioxide film layer is 1.38-1.40, and the thickness of the dense silicon dioxide film layer is 70nm-90nm.
[0018] The embodiment of the present application further provides a photovoltaic module, the photovoltaic module comprising a first cover plate, a first adhesive film, a battery pack, a second adhesive film and a second cover plate which are stacked, the first cover plate being the glass cover plate described above, or the first cover plate and the second cover plate being the glass cover plates described above; the first surface of the glass cover plate being a side away from the battery pack;
[0019] The battery pack includes a plurality of electrically connected battery cells.
[0020] In the embodiment of the present application, embossing is performed on the first surface to form a plurality of inwardly concave portions on the first surface. Without increasing the thickness and weight of the glass cover plate, the structural strength of the glass cover plate is enhanced, and the stress is dispersed (the stress is concentrated on the edge of the concave portion, the stress concentration is reduced, and the stress concentration degree of the glass cover plate is reduced), thereby improving the impact resistance of the glass cover plate, reducing the risk of cracks or breakage of the glass cover plate due to impact, and being conducive to extending the life of the glass cover plate and the photovoltaic module.
[0021] It should be understood that the foregoing general description and the following detailed description are exemplary only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 A schematic diagram of the cross-sectional structure of a photovoltaic module provided in this application in a specific embodiment;
[0023] Figure 2 A schematic cross-sectional view of a glass body provided in the present application in a specific embodiment;
[0024] Figure 3 A cross-sectional schematic diagram of the glass body provided in the present application in another specific embodiment;
[0025] Figure 4 A cross-sectional schematic diagram of the glass body provided in the present application in another specific embodiment;
[0026] Figure 5 A cross-sectional schematic diagram of the glass body provided in the present application in another specific embodiment;
[0027] Figure 6 This is a top view schematic diagram of the glass body provided in this application;
[0028] Figure 7 A schematic cross-sectional view of a glass cover provided in the present application in a specific embodiment;
[0029] Figure 8 A cross-sectional schematic diagram of the glass body provided in the present application in another specific embodiment;
[0030] Fig. 9 The light transmittance curves of the glass body provided in this application when uncoated, single-coated, and double-coated.
[0031] Reference numerals:
[0032] 1- Photovoltaic modules;
[0033] 11- glass cover;
[0034] 111- glass body;
[0035] 111a-first surface;
[0036] 111a1 - recessed portion;
[0037] 111a2 - marginal position;
[0038] 111b- second surface;
[0039] 111c-edge;
[0040] 112-porous nano-silicon dioxide film layer;
[0041] 113- dense silicon dioxide film layer;
[0042] 12- first cover plate;
[0043] 13- first adhesive film;
[0044] 14-battery pack;
[0045] 15- second adhesive film;
[0046] 16- Second cover plate.
[0047] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the present application and, together with the description, serve to explain the principles of the present application. DETAILED DESCRIPTION
[0048] In order to better understand the technical solution of the present application, the embodiments of the present application are described in detail below with reference to the accompanying drawings.
[0049] It should be clear that the described embodiments are only part of the embodiments of the present application, rather than all the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.
[0050] The terms used in the embodiments of the present application are only for the purpose of describing specific embodiments, and are not intended to limit the present application. The singular forms "a", "said" and "the" used in the embodiments of the present application and the appended claims are also intended to include plural forms, unless the context clearly indicates other meanings.
[0051] It should be understood that the term "and / or" used in this article is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0052] It should be noted that the directional words such as "upper", "lower", "left", and "right" described in the embodiments of the present application are described at the angles shown in the accompanying drawings and should not be understood as limiting the embodiments of the present application. In addition, in the context, it is also necessary to understand that when it is mentioned that an element is connected to another element "upper" or "lower", it can not only be directly connected to another element "upper" or "lower", but also indirectly connected to another element "upper" or "lower" through an intermediate element.
[0053] like Figure 1 The schematic cross-sectional view of the photovoltaic module 1 is shown, and the photovoltaic module 1 includes a first cover plate 12, a first adhesive film 13, a battery group 14, a second adhesive film 15, and a second cover plate 16 which are stacked. That is, the photovoltaic module 1 is composed of the first cover plate 12, the first adhesive film 13, the battery group 14, the second adhesive film 15, and the second cover plate 16 which are laminated and packaged. Among them, the photovoltaic module 1 can be a single-glass module, that is, the first cover plate 12 is a glass cover plate 11 facing the light source, which is used to transmit sunlight. Alternatively, the photovoltaic module 1 can be a double-glass module, and the first cover plate 12 and the second cover plate 16 are both glass cover plates 11 facing the light source, which are used to transmit sunlight.
[0054] During the lamination process of the photovoltaic module 1, the first adhesive film 13 and the second adhesive film 15 are used to encapsulate the battery pack 14 to prevent the external environment from affecting the performance of the battery pack 14, and at the same time can also bond the first cover plate 12, the second cover plate 16 and the battery pack 14 into a whole.
[0055] The materials of the first adhesive film 13 and the second adhesive film 15 may be the same or different. For example, the materials of the first adhesive film 13 and the second adhesive film 15 may be one of materials such as ethylene-vinyl acetate copolymer (EVA), polyolefin elastomer (POE), polyvinyl butyral (PVB), etc., and may also be EPE adhesive film (EVA-POE-EVA co-extruded structure) or EP adhesive film (EVA-EP co-extruded structure).
[0056] The battery pack 14 includes a plurality of electrically connected battery cells. Specifically, the battery pack 14 includes a plurality of battery strings connected in series or in parallel. The battery string is formed by connecting a plurality of battery cells in series, and adjacent battery cells are connected by welding strips.
[0057] This embodiment does not limit the structure of the battery cell. The types of battery cells include but are not limited to Passivated Emitter Rear Cell (PERC), Tunnel Oxide Passivated Contact (TOPCon), Heterojunction with Intrinsic Thin-film (HJT), Interdigitated Back Contact (IBC), perovskite battery, etc.
[0058] For PERC cells, along the thickness direction, PERC cells include front surface metal silver electrode, front surface silicon nitride passivation layer, phosphorus layer emitter, P-type base silicon layer, local aluminum back field, metal aluminum back electrode, back passivation layer (Al2O3 / SiNx). PERC cells use a passivation film to passivate the back, replacing the full aluminum back field, enhancing the internal back reflection of light in the silicon base, reducing the recombination rate on the back, and increasing the efficiency of the cell by 0.5%-1%.
[0059] For TOPCon cells, along the thickness direction, TOPCon cells include metal silver electrodes, front surface silicon nitride passivation layers, boron-doped emitters, N-type base silicon layers, diffused doping layers, ultra-thin silicon oxide, doped polysilicon, silicon nitride, and metal silver electrodes. The back of the cell is composed of a layer of ultra-thin silicon oxide (1nm to 2nm) and a layer of phosphorus-doped microcrystalline amorphous mixed Si film, which together form a passivation contact structure. This structure can block the recombination of minority carrier holes and increase the open circuit voltage and short circuit current of the cell. The ultra-thin oxide layer allows majority electrons to tunnel into the polysilicon layer while blocking the recombination of minority carrier holes. The good passivation effect of ultra-thin silicon oxide and heavily doped silicon film causes the energy band on the silicon wafer surface to bend, thereby forming a field passivation effect, greatly increasing the probability of electron tunneling, reducing contact resistance, and increasing the open circuit voltage and short circuit current of the cell, thereby improving the cell conversion efficiency.
[0060] For HJT cells, along the thickness direction, the HJT cells include a front low-temperature silver electrode, a front conductive film, an N-type amorphous silicon film, an intrinsic amorphous silicon film, an N-type base silicon layer, an intrinsic amorphous silicon film, a P-type amorphous silicon film, a back conductive film, and a back low-temperature silver electrode.
[0061] For IBC cells, along the thickness direction, IBC cells include silicon nitride anti-layer, N+ front surface field, N-type base silicon layer, P+ emitter, N+ back field, aluminum oxide passivation layer, silicon nitride anti-reflection layer, and metal silver electrode. IBC cells use ion implantation technology to obtain P and N regions with good uniformity and precisely controllable junction depth. There is no grid line blocking on the front of the cell, which can eliminate the shading current loss of the metal electrode and achieve the maximum utilization of incident photons. The short-circuit current can be increased by about 7% compared with conventional solar cells; due to the back contact structure, there is no need to consider the grid line blocking problem, and the grid line ratio can be appropriately widened, thereby reducing the series resistance and having a high fill factor; the surface passivation and surface light trapping structure can be optimized to obtain a lower front surface recombination rate and surface reflection.
[0062] For perovskite cells, along the thickness direction, the perovskite cell includes substrate material, conductive film, electron transport layer (titanium dioxide), perovskite absorption layer (hole transport layer), and metal cathode. Perovskite materials have a high light absorption coefficient and a long carrier diffusion distance. After the photons absorbed by the perovskite material are converted into electrons, they are easily collected by the electrode with low loss, so they can generate higher photoelectric voltage and current, making perovskite show higher photoelectric conversion efficiency.
[0063] The battery cell can adopt a multi-busbar solution, which can shorten the current conduction path, reduce internal losses, and thus improve the power of the photovoltaic module 1, while also reducing the cost of the photovoltaic module 1; it can also adopt a busbar-free solution, replacing the original busbar with a welding ribbon and directly connecting it to the fine grid, which can greatly reduce the silver paste consumption, thereby reducing the cost of the photovoltaic module 1.
[0064] The structure of the glass cover plate (first cover plate / first cover plate and second cover plate) will be described in detail below with reference to the accompanying drawings.
[0065] like Figure 2 The figure shows a cross-sectional schematic diagram of a glass body 111 in an embodiment. The glass cover plate 11 includes the glass body 111. Along the thickness direction Z of the glass cover plate 11, the glass body 111 has a first surface 111a and a second surface 111b that are arranged opposite to each other. The first surface 111a is a light-facing surface on the glass body 111 that is away from the battery group 14 and is located at the outermost side of the photovoltaic module 1. Therefore, the first surface 111a is easily impacted, causing the glass cover plate 11 to crack or even break.
[0066] To this end, in this embodiment, the first surface 111a of the glass cover plate 11 is punched to form a plurality of reinforcement structures on the first surface 111a of the glass cover plate 11. Specifically, the first surface 111a is embossed to form a plurality of inwardly concave portions 111a1.
[0067] In this embodiment, a recessed portion 111a1 is provided on the first surface 111a to enhance the structural strength of the glass body 111 and disperse the stress (concentrate the stress on the edge of the recessed portion 111a1, reduce stress concentration, and reduce the degree of stress concentration in the glass body 111) without increasing the thickness and weight of the glass body 111, thereby improving the impact resistance of the glass body 111 and reducing the risk of cracks or breakage of the glass body 111 due to impact, which is beneficial to extending the life of the glass cover 11 and the photovoltaic module 1.
[0068] It should be noted that the recessed portion 111a1 in this embodiment is formed by punching the first surface 111a of the glass body 111, and a part of the structure of the first surface 111a is recessed toward the second surface 111b. Instead of providing a protruding structure on the first surface 111a and punching a recess on the protruding structure to form the recessed portion 111a1, or providing a protruding portion on the first surface 111a and forming the recessed portion 111a1 by the recess between adjacent protruding portions.
[0069] Please continue to refer to Figure 2 Along the thickness direction Z of the glass cover plate 11 , the ratio of the depth D1 of the recessed portion 111 a 1 to the thickness D2 of the glass body 111 satisfies: 0.005≤D1 / D2≤0.015.
[0070] For example, the ratio of the depth D1 of the recessed portion 111a1 to the thickness D2 of the glass body 111 may be 0.005, 0.006, 0.007, 0.008, 0.009, 0.010, 0.011, 0.012, 0.013, 0.014, 0.015, or the like.
[0071] In this embodiment, the ratio of the depth D1 of the recessed portion 111a1 to the thickness D2 of the glass body 111 should not be too large or too small. If D1 / D2 is too large (e.g., greater than 0.015), the depth of the recessed portion 111a1 is too large, resulting in a thinner structure of the glass body 111 below the recessed portion 111a1, which reduces the strength of the structure and may break under pressure during the lamination process. If D1 / D2 is too small (e.g., less than 0.005), the depth of the recessed portion 111a1 is too small, resulting in the first surface 111a of the glass body 111 not being provided with the recessed portion 111a1 and the impact resistance being not significantly improved after the recessed portion 111a1 is provided.
[0072] Therefore, when the ratio of the depth D1 of the recessed portion 111a1 to the thickness D2 of the glass body 111 satisfies: 0.005≤D1 / D2≤0.015, the impact resistance of the first surface 111a of the glass body 111 can be enhanced while the structural strength of the glass body 111 below the recessed portion 111a1 can be ensured.
[0073] The depth D1 of the recessed portion 111 a 1 satisfies: 10 μm≤D1≤30 μm.
[0074] Illustratively, the depth D1 of the recessed portion 111 a 1 may be 10 μm, 12 μm, 14 μm, 16 μm, 18 μm, 20 μm, 22 μm, 24 μm, 26 μm, 28 μm, 30 μm, or the like.
[0075] In this embodiment, the depth D1 of the recessed portion 111a1 should be neither too large nor too small. If D1 is too large (e.g., greater than 30 μm), the structure of the glass body 111 below the recessed portion 111a1 is thinner, which reduces the strength of the structure and may break under the pressure during the lamination process. If D1 is too small (e.g., less than 10 μm), the impact resistance of the first surface 111a of the glass body 111 is not significantly improved when the recessed portion 111a1 is not provided or when the recessed portion 111a1 is provided.
[0076] Therefore, when the depth D1 of the recessed portion 111a1 satisfies: 10 μm≤D1≤30 μm, the impact resistance of the first surface 111a of the glass body 111 can be enhanced while the structural strength of the glass body 111 below the recessed portion 111a1 can be ensured.
[0077] For further information, please refer to Figure 2 , there is a gap D3 between the recessed portion 111a1 at the edge position 111a2 and the edge 111c of the glass body 111. The edge 111c refers to the edge position of the outer periphery of the first surface 111a, the edge position 111a2 refers to the edge position 111a2 of the region where the multiple recessed portions 111a1 on the first surface 111a are located (indicated by the dotted box area in the figure), and the recessed portion 111a1 at the edge position 111a2 refers to the recessed portion 111a1 located at the outermost periphery among the multiple recessed portions 111a1. In this embodiment, the edge 111c of the glass body 111 is not provided with the recessed portion 111a1, so as to avoid the edge 111c of the glass body 111 being notched, and to make the edge 111c of the glass body 111 the original thickness of the glass body 111, so as to ensure the connection strength between the edge position 111a2 of the photovoltaic module 1 and the frame.
[0078] Specifically, the interval D3 between the recessed portion 111a1 located at the edge position 111a2 and the edge 111c of the glass body 111 satisfies: 2mm≤D3≤8.5mm.
[0079] Exemplarily, the interval D3 between the recessed portion 111a1 at the edge position 111a2 and the edge 111c of the glass body 111 may be 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm, 5mm, 5.5mm, 6mm, 6.5mm, 7mm, 7.5mm, 8mm, 8.5mm, etc.
[0080] In this embodiment, the interval D3 between the recessed portion 111a1 located at the edge position 111a2 and the edge 111c of the glass body 111 should not be too large. If D3 is too large (e.g., greater than 8.5 mm), the distance between the recessed portion 111a1 located at the edge position 111a2 on the first surface 111a and the edge 111c of the first surface 111a will be larger, resulting in a larger area on the first surface 111a where the recessed portion 111a1 is not provided, thereby affecting the structural strength of the area of the first surface 111a close to the edge 111c.
[0081] Meanwhile, in this embodiment, 2 mm ≤ D3 is defined, and an error value is reserved for the processing of the recessed portion 111 a 1 located at the edge position 111 a 2 , so as to avoid the edge 111 c of the glass body 111 being notched due to the processing error.
[0082] Alternatively, please refer to Figure 3 , Figure 31 is a cross-sectional schematic diagram of another embodiment of the glass body 111. In some embodiments, the entire surface of the first surface 111a of the glass body 111 may be provided with a recessed portion 111a1. That is, the interval D3 between the recessed portion 111a1 located at the edge position 111a2 and the edge 111c of the glass body 111 satisfies: 0mm≤D3≤8.5mm. However, in this embodiment, when the interval D3 between the recessed portion 111a1 located at the edge position 111a2 and the edge 111c of the glass body 111 is equal to 0mm, the thickness of the edge 111c of the glass body 111 is still the original thickness D2 of the glass body 111.
[0083] Please continue to refer to Figure 2 , along the direction from the first surface 111a to the second surface 111b, the cross section of the recessed portion 111a1 gradually decreases, which facilitates the processing and forming of the recessed portion 111a1.
[0084] In some embodiments, there may be a gap between adjacent recessed portions 111a1 of the first surface 111a, such as Figure 2 Alternatively, adjacent recessed portions 111a1 of the first surface 111a are arranged closely together, as shown in FIG. Figure 4 As shown, Figure 4 1 is a schematic cross-sectional view of another embodiment of the glass body 111. The arrangement of the recessed portions 111a1 on the first surface 111a can be set according to actual conditions, and is not specifically limited in this embodiment.
[0085] In some embodiments, along the thickness direction Y perpendicular to the glass cover plate 11, the cross section of the recessed portion 111a1 may be triangular, arc-shaped, trapezoidal, etc. For details, please refer to Figure 1 and Figure 5 , Figure 1 The cross section of the middle recessed portion 111a1 along the thickness direction Y perpendicular to the glass cover plate 11 is a triangle. Figure 5 The cross section of the middle recessed portion 111a1 along the thickness direction Y perpendicular to the glass cover plate 11 is arc-shaped. Alternatively, the cross section of the recessed portion 111a1 along the thickness direction Y perpendicular to the glass cover plate 11 may also be other shapes, which are not limited in this embodiment.
[0086] In some embodiments, along the thickness direction Z of the glass cover plate 11, the cross section of the recessed portion 111a1 may be one or more of a circle, a triangle, a rectangle, and a polygon. Figure 6, the cross section of the recessed portion 111a1 along the thickness direction Z of the glass cover plate 11 is circular or square, and there is a gap between adjacent recessed portions 111a1. Among them, when the cross section of the recessed portion 111a1 along the thickness direction Z of the glass cover plate 11 is circular, the recessed portion 111a1 can be a cone, a semicircle or other structure. When the cross section of the recessed portion 111a1 along the glass cover plate 11 is triangular, the recessed portion 111a1 can be a triangular pyramid structure. When the cross section of the recessed portion 111a1 along the glass cover plate 11 is a quadrilateral, the recessed portion 111a1 can be a quadrangular pyramid structure. Alternatively, the recessed portion 111a1 can also be other shapes, which are not limited in this embodiment.
[0087] like Figure 7 The figure shows a cross-sectional schematic diagram of a glass cover plate 11 in an embodiment. The glass cover plate 11 includes a glass body 111 and a porous nano-silicon dioxide film layer 112. The glass body 111 has a first surface 111a, and the porous nano-silicon dioxide film layer 112 is disposed on the first surface 111a.
[0088] The porous nano-silicon dioxide film layer 112 is mainly composed of porous nano-silicon dioxide. Based on the optical principle of film coating, nano-technology is used to set the film thickness at one-fourth of the sensitive wavelength of the solar cell, so as to achieve the interference and elimination of the reflected light of the solar light wave on the film surface and the glass surface, thereby increasing the transmittance. In this regard, the porous nano-silicon dioxide film layer 112 has the effect of increasing transmittance and reducing reflection. The porous nano-silicon dioxide film layer 112 is covered on the first surface 111a to reduce the light reflection of the glass cover plate 11, improve the light transmittance of the glass cover plate 11, reduce light loss, effectively improve the light energy utilization rate and service life of the photovoltaic module 1, and efficiently utilize solar energy.
[0089] In addition, the porous nano-silica film layer 112 has excellent light transmittance, anti-reflection performance and high thermal resistance, while also having certain anti-attenuation and hydrophobicity, and has a self-cleaning function to avoid the reduction of power generation efficiency of the photovoltaic module 1 caused by dirt on the surface of the glass cover 11.
[0090] The refractive index of the porous nano-silicon dioxide film layer 112 is 1.28-1.30, and the thickness of the porous nano-silicon dioxide film layer 112 is 100 nm-130 nm.
[0091] Exemplarily, the refractive index of the porous nano-silica film layer 112 is 1.28, 1.29, 1.3, and the thickness of the porous nano-silica film layer 112 is 100nm, 120nm, 130nm. Preferably, the refractive index of the porous nano-silica film layer 112 is 1.3, and the thickness of the porous nano-silica film layer 112 is 110nm.
[0092] In this embodiment, when the refractive index of the porous nano-silica film layer 112 is 1.28-1.30 and the thickness of the porous nano-silica film layer 112 is 100nm-130nm, the light transmittance of the glass cover plate 11 can be improved, light loss can be reduced, and the power of the photovoltaic module 1 can be increased.
[0093] It should be noted that the first surface 111a of the glass body 111 is provided with a recessed portion 111a1, so the first surface 111a is uneven. After the porous nano-silicon dioxide film 112 is plated on the first surface 111a, the porous nano-silicon dioxide film 112 is also uneven.
[0094] like Figure 8 The figure shows a cross-sectional schematic diagram of a glass cover plate 11 in another embodiment, wherein the glass cover plate 11 comprises a glass body 111, a dense silicon dioxide film layer 113 and a porous nano-silicon dioxide film layer 112, wherein the glass body 111 has a first surface 111a, the dense silicon dioxide film layer 113 is disposed on the first surface 111a, and the porous nano-silicon dioxide film layer 112 is disposed on the dense silicon dioxide film layer 113. In this embodiment, two film layers are disposed to reduce the propagation loss of reflected light and reduce the reflectivity.
[0095] In order to further illustrate that the transmittance of the glass cover 11 is improved when the glass body 111 in the present application is provided with a single film layer (porous nano-silica film layer 112) and a double film layer (dense silica film layer 113 and porous nano-silica film layer 112), the present application records and compares the transmittance of the glass body 111 when there is no film layer, a single film layer (porous nano-silica film layer 112) and a double film layer (dense silica film layer 113 and porous nano-silica film layer 112).
[0096] It should be noted that other parameters of the glass body 111 are the same whether it is provided with no film layer, a single film layer, or a double film layer, and are not described one by one here.
[0097] Please refer to Fig. 9 ,like Fig. 9 The figure shows the light transmittance curves when the glass body 111 is provided with no film layer, a single film layer, and a double film layer. Fig. 9 It can be seen that in the figure, the horizontal axis is the wavelength of light, the vertical axis is the transmittance, the blue line is the transmittance curve of the glass body 111 without a coating layer, the orange line is the transmittance curve of the glass body 111 coated with a single layer of film (porous nano-silica film layer 112), and the gray line is the transmittance curve of the glass body 111 coated with a double layer of film (dense silica film layer 113 and porous nano-silica film layer 112).
[0098] The average light transmittance of the glass body 111 is 91.61, the average light transmittance of the glass body 111 coated with a single layer of film is 93.94, and the average light transmittance of the glass body 111 coated with a double layer of film is 94.29.
[0099] It can be seen that compared with the glass body 111 without coating, the glass body 111 coated with a single layer of film shows a higher light transmittance. Compared with the glass body 111 coated with a single layer of film, the glass body 111 coated with a double layer of film shows a higher light transmittance.
[0100] Therefore, when the glass body 111 is coated with a double-layer film, the light transmittance of the glass cover plate 11 can be further improved. That is, the synergistic effect of the dense silicon dioxide film layer 113 and the porous nano-silicon dioxide film layer 112 can improve the utilization rate of light energy and enhance the photoelectric conversion efficiency. At the same time, the two film layers provided on the glass body 111 are conducive to improving the anti-fouling performance of the glass cover plate 11, thereby reducing the possibility that the surface dirt of the glass cover plate 11 affects the power generation efficiency of the photovoltaic module 1.
[0101] The refractive index of the porous nano-silicon dioxide film layer 112 is 1.18-1.20, and the thickness of the porous nano-silicon dioxide film layer 112 is 100nm-120nm. The refractive index of the dense silicon dioxide film layer 113 is 1.38-1.40, and the thickness of the dense silicon dioxide film layer is 70nm-90nm.
[0102] For example, the refractive index of the porous nano-silicon dioxide film layer 112 may be 1.18, 1.19, 1.20, etc., and the thickness of the porous nano-silicon dioxide film layer 112 may be 100 nm, 110 nm, 120 nm, etc. The refractive index of the dense silicon dioxide film layer 113 may be 1.38, 1.39, 1.40, etc., and the thickness of the dense silicon dioxide film layer may be 70 nm, 80 nm, 90 nm, etc.
[0103] In this embodiment, the refractive index of the porous nano-silica film layer 112 is 1.18-1.20, the thickness of the porous nano-silica film layer 112 is 100nm-120nm, the refractive index of the dense silica film layer 113 is 1.38-1.40, and the thickness of the dense silica film layer is 70nm-90nm, which can further improve the transmittance of the glass cover 11, reduce light loss, and increase the power of the photovoltaic module 1.
[0104] It should be noted that the first surface 111a of the glass body 111 is provided with a recessed portion 111a1, so the first surface 111a is uneven. After the dense silicon dioxide film layer 113 is plated on the first surface 111a, after the porous nano-silicon dioxide film layer 112 is plated on the dense silicon dioxide film layer 113, the dense silicon dioxide film layer 113 and the porous nano-silicon dioxide film layer 112 are also uneven.
[0105] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.
Claims
1. A glass cover plate for a photovoltaic module (1), It is characterized in that The glass cover plate (11) comprises: A glass body (111), along a thickness direction (Z) of the glass cover plate (11), the glass body (111) having a first surface (111a) and a second surface (111b) arranged opposite to each other, the first surface (111a) being provided with a plurality of evenly distributed recessed portions (111a1), and a gap being provided between the recessed portions (111a1) located at edge positions (111a2) and an edge (111c) of the glass body (111); Along the thickness direction (Z) of the glass cover plate (11), the ratio of the depth D1 of the recessed portion (111a1) to the thickness D2 of the glass body (111) satisfies: 0.005≤D1 / D2≤0.
015.
2. The glass cover plate according to claim 1, It is characterized in that The interval D3 between the recessed portion (111a1) located at the edge position (111a2) and the edge (111c) of the glass body (111) satisfies: 2mm≤D3≤8.5mm.
3. The glass cover plate according to claim 1, It is characterized in that The depth D1 of the recessed portion (111a1) satisfies: 10 μm≤D1≤30 μm.
4. The glass cover plate according to claim 1, It is characterized in that Along the direction from the first surface (111a) to the second surface (111b), the cross section of the recessed portion (111a1) gradually decreases.
5. The glass cover plate according to claim 1, It is characterized in that Along the thickness direction (Z) of the glass cover plate (11), the cross section of the recessed portion (111a1) is one or more of circular, triangular, rectangular and polygonal.
6. The glass cover plate according to claim 1, It is characterized in that The glass cover plate (11) further comprises a porous nano-silicon dioxide film layer (112), and the porous nano-silicon dioxide film layer (112) is arranged on the first surface (111a).
7. The glass cover plate according to claim 6, It is characterized in that The refractive index of the porous nano-silicon dioxide film layer (112) is 1.28-1.30; The thickness of the porous nano-silicon dioxide film layer (112) is 100nm-130nm.
8. The glass cover plate according to claim 1, It is characterized in that The glass cover plate (11) further comprises a dense silicon dioxide film layer (113) and a porous nano silicon dioxide film layer (112); The dense silicon dioxide film layer (113) is arranged on the first surface (111a), and the porous nano silicon dioxide film layer (112) is arranged on the dense silicon dioxide film layer (113).
9. The glass cover plate according to claim 8, It is characterized in that The refractive index of the porous nano-silicon dioxide film layer (112) is 1.18-1.20, and the thickness of the porous nano-silicon dioxide film layer (112) is 100 nm-120 nm; The refractive index of the dense silicon dioxide film layer (113) is 1.38-1.40, and the thickness of the dense silicon dioxide film layer (133) is 70nm-90nm.
10. A photovoltaic module, It is characterized in that The photovoltaic module (1) comprises a first cover plate (12), a first adhesive film (13), a battery group (14), a second adhesive film (15) and a second cover plate (16) which are stacked, the first cover plate (12) being the glass cover plate (11) according to any one of claims 1 to 9, or the first cover plate (12) and the second cover plate (16) being the glass cover plates (11) according to any one of claims 1 to 9; the first surface (111a) of the glass cover plate (11) is the side away from the battery group (14); The battery pack (14) includes a plurality of electrically connected battery cells.
Citation Information
Patent Citations
Homogeneous double-layer SiO2 and polytetrafluoroethylene composited self-cleaning anti-reflective film, and preparation method thereof
CN106526719A
Conductive glass antireflection film design and preparation method
CN108155253A
High-definition flicker-free etched glass as well as manufacturing process and application thereof
CN111333340A
Cover plate glass for photovoltaic module, photovoltaic module with cover plate glass and photovoltaic system with cover plate glass
CN216818354U
Method for forming low-reflection film and member with low-reflection film
JP2013228643A