Method for improving discharge rate of waste smooth shell battery

By controlling the depth at which the photovoltaic cells are inserted into conductive particles, the contact area and resistance of the cells are adjusted, thus solving the problems of safety and low efficiency in the process of processing waste photovoltaic cells. This achieves a safe, efficient, and low-cost discharge method suitable for large-scale processing.

CN118943550APending Publication Date: 2024-11-12SHENZHEN JIECHENG NICKEL COBALT NEW ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411062187.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Existing technologies for processing waste photovoltaic cells suffer from safety issues, high costs, low discharge efficiency, and uncontrollable states, making them particularly unsuitable for mass production.

Method used

By controlling the depth of the photovoltaic cell inserted into the conductive particles, the contact area and resistance of the cell are adjusted. The conductive particles and the conductive plate form an equivalent resistance, thereby controlling the discharge rate. Graphite particles or carbon steel balls are used as conductive particles, and conductive metal sheets are used as conductive plates. Discharge is achieved by connecting them with wires.

Benefits of technology

It achieves a safe and efficient discharge process, reduces processing costs, is suitable for large-scale processing of waste photovoltaic cells, and is environmentally friendly and pollution-free, showing good application prospects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118943550A_ABST
    Figure CN118943550A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of waste battery treatment, in particular to a method for improving the discharge rate of a waste smooth shell battery. According to the method provided by the invention, the contact area and the corresponding resistance of the light-shell battery are regulated and controlled by controlling the depth of the light-shell battery inserted into the conductive particles, so that the discharge rate of the waste light-shell battery is controlled, and the problems of unsafety, low discharge efficiency and the like in the treatment process of the light-shell battery are avoided; besides, the method for treating the waste light-shell batteries is simple and easy to operate, is suitable for treating the waste light-shell batteries on a large scale, is favorable for realizing efficient treatment of the light-shell batteries, is green and environment-friendly, does not generate waste liquid, and can be used for recycling raw materials, so that the cost of discharging by using materials such as saline water is reduced, and the utilization rate of the waste light-shell batteries is increased. And the method has no pollution to the environment and has a relatively good application prospect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of waste battery treatment, and in particular to a method for improving the discharge rate of waste bare shell batteries. Background Art

[0002] Cylindrical batteries are used in combination as the cells of automotive power batteries and have a large production scale. And the cylindrical batteries currently used are mainly light shell batteries. The basic structure of light shell batteries includes positive electrode, negative electrode, diaphragm and electrolyte, which is the same as ordinary lithium-ion batteries. Their outer shells are usually made of aluminum or steel instead of harder packaging materials. This design makes them lighter in weight and lower in cost. In summary, light shell batteries have many advantages and good application prospects.

[0003] With the increasing application of bare shell batteries in the field of automotive power batteries, the treatment of retired bare shell batteries has also attracted more and more attention. In the process of treating waste batteries, it is usually necessary to first perform crushing treatment and then discharge treatment. For example, Chinese patent application CN108134153A discloses a method for treating waste lithium-ion batteries (rejected), which uses salt water discharge, alkali solution spraying crushing, electrolyte dissolution, filtration and other processes to treat waste lithium-ion batteries. For example, Chinese patent application CN108110356B (authorized) discloses a fully automatic waste lithium-ion battery recycling process and system, which uses salt water immersion discharge, crushing by a pulverizer, and separation of active material powder and copper / aluminum fragments to recycle waste lithium-ion batteries. However, the above-mentioned treatment method for conventional waste batteries is not suitable for bare shell batteries. This is because the treatment of bare shell batteries compared to conventional batteries has certain particularities.

[0004] When two bare shell batteries collide with each other, sparks may occur, so the retired bare shell batteries need to be discharged independently before being crushed, which brings certain insecurities to the treatment of bare shell batteries. And although the traditional salt water discharge is simple and easy to operate, it is expensive and has poor discharge efficiency, is not suitable for mass production and use, and is not green and low-carbon and environmentally friendly; in addition, the state of the discharge process is uncontrollable, and the discharge endpoint monitoring is difficult to achieve, which has always been a pain point in the industry. Therefore, a method for waste bare shell batteries with high safety and high discharge efficiency is urgently needed. Summary of the invention

[0005] The present invention provides a method for improving the discharge rate of waste bare shell batteries. By controlling the depth of the bare shell batteries inserted into conductive particles, the contact area and corresponding resistance of the bare shell batteries are regulated, thereby controlling the discharge rate of the waste bare shell batteries, thereby avoiding the problems of unsafety, low discharge efficiency, etc. in the treatment process of the bare shell batteries.

[0006] In a first aspect, a method for improving the discharge rate of waste bare shell batteries is provided, comprising the following steps:

[0007] Conductive particles are placed on the lower conductive plate, the light-shell battery is inserted into the conductive particles, the upper conductive plate is connected to the positive electrode of the light-shell battery, and the upper conductive plate and the lower conductive plate are connected with a wire for discharge, and then the change of the wire current is detected to detect the change of the discharge state and the discharge end point.

[0008] The present invention forms an equivalent resistance by contacting the negative electrode of the light-shell battery with the conductive particles, and the conductive particles contact the conductive plate. The deeper the insertion depth, the smaller the resistance and the faster the discharge efficiency. The shell of the present invention controls the discharge rate of the light-shell battery by controlling the insertion depth of the light-shell battery.

[0009] Specifically, the resistance of the conductive particles is within 0.8Ω; the resistance of the conductive particles is controlled, and the conductive particles must have good conductive properties;

[0010] Specifically, the conductive particles are graphite particles or carbon steel balls, preferably graphite particles, because graphite particles have good stability and are not easily oxidized, which will affect the resistance value and thus the discharge effect. The conductive particles can also be selected from other conductive particles with good stability as needed.

[0011] Specifically, the conductive particles are spherical and have a diameter of 4 to 8 mm.

[0012] Specifically, the conductive plate is a conductive metal sheet.

[0013] Specifically, the conductive metal sheet includes but is not limited to one of a copper sheet, an aluminum sheet, a copper alloy and an aluminum alloy.

[0014] Specifically, the wire is one wire or multiple wires.

[0015] Specifically, there is one light shell battery.

[0016] Specifically, there are a plurality of light-shell cells, and the plurality of light-shell cells are placed in the same direction between the two conductive plates.

[0017] Specifically, there are gaps between the light-shell batteries; if there are no gaps between the light-shell batteries, two light-shell batteries that are closely attached will be directly connected to each other on the surfaces of the light-shell batteries, resulting in a battery short circuit.

[0018] Specifically, the plurality of conductors are connected in parallel; and the plurality of conductors are provided to play a shunting role.

[0019] Specifically, there is a gap between the negative electrode of the bare shell battery and the conductive plate; the negative electrode of the bare shell battery cannot directly contact the conductive plate, and direct contact may cause risks.

[0020] Specifically, the current carrying capacity of the wire is greater than the discharge current of the battery; this is because it is necessary to ensure that the current carrying capacity of the wire is large enough, otherwise it will cause safety problems.

[0021] The depth of the light shell battery inserted into the conductive particles is within 3 / 5 of the height of the light shell battery.

[0022] In a second aspect, a device for executing the method for improving the discharge rate of waste bare shell batteries is provided, the device comprising a conductive plate, a wire and conductive particles, the conductive plate comprising an upper conductive plate and a lower conductive plate, the wire connecting the upper conductive plate and the lower conductive plate, the conductive particles being placed on the lower conductive plate and not in contact with the upper conductive plate.

[0023] The beneficial effects of the present invention are as follows:

[0024] 1. The present invention controls the depth of light-shell batteries inserted into conductive particles, regulates the contact area and corresponding resistance of the light-shell batteries, and thus controls the discharge rate of waste light-shell batteries, thereby avoiding the problems of unsafety and low discharge efficiency of light-shell batteries during the treatment process;

[0025] 2. The method for treating waste light shell batteries provided by the present invention is simple and easy to operate, and is suitable for treating waste light shell batteries in large quantities, which is conducive to realizing efficient treatment of light shell batteries. In addition, the method provided by the present invention is green and environmentally friendly, does not generate waste liquid, and the raw materials can be reused repeatedly, which not only reduces the cost of discharging using materials such as salt water, but also has no pollution to the environment and has good application prospects. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is the discharge principle diagram of the light shell battery in Example 6;

[0027] Figure numerals: 1. Conductive plate, 2. Light-shell battery, 3. Conductive particles, 4. Wire. DETAILED DESCRIPTION

[0028] The technical solution of the present application will be described clearly and completely below in conjunction with the embodiments. Obviously, the described embodiments are part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.

[0029] The present invention provides a method for improving the discharge rate of waste bare shell batteries, comprising the following steps:

[0030] Conductive particles are placed on the lower conductive plate, the light-shell battery is inserted into the conductive particles, the upper conductive plate is connected to the positive electrode of the light-shell battery, and the upper conductive plate and the lower conductive plate are connected with a wire to discharge, and then the change in the wire current is detected to detect the change in the discharge state and the end point of the discharge. The present invention inserts the light-shell battery into the conductive particles so that the negative electrode of the light-shell battery contacts the conductive particles, and the conductive particles contact the lower conductive plate to form an equivalent resistance. The deeper the insertion depth, the smaller the resistance and the faster the discharge efficiency. Therefore, the present invention can control the discharge rate of the light-shell battery by controlling the insertion depth of the light-shell battery.

[0031] Specifically, the resistance of the conductive particles is within 0.8Ω, for example, 0.8Ω, 0.6Ω and 0.4Ω; by controlling the resistance of the conductive particles, the conductive particles have better conductivity and thus better discharge effect;

[0032] More specifically, the conductive particles can be graphite particles or carbon steel balls; graphite particles have better stability, are not easily oxidized, and have better effects; carbon steel balls will oxidize after being left for a period of time, which will affect the resistance of the conductive particles and further affect the discharge effect.

[0033] More specifically, the conductive particles can be selected to be spherical with a particle diameter of 4 to 8 mm; selecting small-diameter spherical conductive particles is beneficial to providing a larger release surface area when the light-shell battery contacts the conductive particles, thereby promoting current transfer; in addition, small-diameter conductive particles can better fill the space, making the current distribution more uniform, which is beneficial to reduce local overheating, and can reduce local discharge caused by electric field concentration and effectively control the voltage rebound behavior of the battery after discharge, thereby reducing the safety hazards caused by voltage relaxation.

[0034] Specifically, the upper conductive plate and the lower conductive plate are both conductive metal sheets, such as copper sheets, aluminum sheets, copper alloys or aluminum alloys; the conductive metal sheets have good electrical conductivity, which is more conducive to improving discharge efficiency.

[0035] Specifically, the wire is one wire or multiple wires, for example, 1, 5, or 10. The selection of the number of wires mainly affects the safety of the entire processing process. In principle, the number of wires is sufficient as long as the discharge current is less than the sum of the current carrying capacities of all wires, that is, the discharge current is allowed to pass safely. For example, even if multiple light-shell batteries are discharged at the same time, when the current carrying capacity of one wire is large enough to carry it, even one wire can be used; when the current carrying capacity of one wire is not enough to carry the current passing during discharge, multiple wires can be selected as needed to be connected in parallel for shunting to ensure the safety of the processing process.

[0036] Specifically, there are one or more light-shell batteries, for example, 2, 10 or 20; but if the number of waste light-shell batteries to be processed is multiple in order to improve the processing efficiency, the multiple light-shell batteries should be placed in the same direction between the two conductive plates. There are gaps between the multiple light-shell batteries, and the size of the gaps is not limited here; the gaps are set because if there are no gaps between the multiple light-shell batteries, two light-shell batteries that are closely attached will be directly connected due to the surface of the light-shell batteries, resulting in a battery short circuit.

[0037] Specifically, there is a gap between the negative electrode of the bare shell battery and the conductive plate; the gap is left because the negative electrode of the bare shell battery and the conductive plate cannot be in direct contact, and direct contact will cause risks.

[0038] Specifically, the depth of the light-shell battery inserted into the conductive particles is within 3 / 5 of the battery height, for example, it can be 0, 1 / 5, 2 / 5 or 3 / 5. When the light-shell battery is inserted to different depths, the corresponding light-shell battery has different discharge rates. The greater the insertion depth, the smaller the equivalent resistance formed, and the greater the discharge rate.

[0039] The present invention provides a device for executing the above-mentioned method for improving the discharge rate of waste bare shell batteries, the device comprises a conductive plate, a wire and conductive particles, the conductive plate comprises an upper conductive plate and a lower conductive plate, the wire connects the upper conductive plate and the lower conductive plate, the conductive particles are placed on the lower conductive plate and do not contact the upper conductive plate. When the device is used, the bare shell battery to be processed is placed between the upper conductive plate and the lower conductive plate and does not contact the lower conductive plate.

[0040] The present application is further described below through specific examples and comparative examples. The following examples and comparative examples all provide a method for increasing the discharge rate of waste bare shell batteries.

[0041] It should be noted that the following embodiments and comparative examples were tested with 18650 model bare shell batteries, all of which were fully charged and had a height of 65 mm. The insertion depth involved in the present application refers to the length of the bare shell battery inserted into the conductive particles, which can also be understood as the length of the battery part immersed in the conductive particles after the conductive particles are inserted.

[0042] Discharge time and maximum discharge temperature measurement method:

[0043] (1) The discharge time in the embodiments and comparative examples is measured as follows:

[0044] During the entire discharge process, the voltage of the bare shell battery was continuously monitored using a voltmeter, and then the time taken for the bare shell battery to discharge below 1V was monitored;

[0045] (2) The method for measuring the maximum discharge temperature in the embodiments and comparative examples is:

[0046] During the discharge process, an infrared thermometer was used to measure the maximum temperature of the light shell battery during discharge.

[0047] Examples 1 to 4 and Comparative Example 1

[0048] A method for improving the discharge rate of waste bare shell batteries, comprising the following steps:

[0049] A copper plate is used as a lower conductive plate, graphite particles (4 to 8 mm) are placed on the lower conductive plate, a light shell battery is inserted into the graphite particles, the copper plate is used as an upper conductive plate, the upper conductive plate is connected to the positive electrode of the light shell battery, and the upper and lower conductive plates are connected with a wire for discharge, and then the change in the wire current is detected to detect the change in the discharge state and the discharge end point.

[0050] Example 1 Example 2 Example 3 Example 4 Comparative Example 1 Insertion depth (mm) 0 6.5 13 26 52 Discharge time (h) 12.1 9.0 8.0 6.2 - Maximum discharge temperature (℃) 60.2 70.4 79.9 80.1 -

[0051] It can be seen from the above data that as the insertion depth gradually increases, the discharge time becomes shorter and the discharge efficiency improves, but the corresponding maximum discharge temperature increases; when the insertion depth reaches 52mm, the temperature rises rapidly to 80°C within 3s after discharge, which is likely to cause a safety accident, resulting in the inability to test the discharge time and maximum discharge temperature.

[0052] Example 5

[0053] A method for improving the discharge rate of waste bare shell batteries, comprising the following steps:

[0054] An aluminum alloy sheet is used as a lower conductive plate, a carbon steel ball is placed on the lower conductive plate, a bare shell battery is inserted into the carbon steel ball with an insertion depth of 26 mm, the aluminum alloy sheet is used as an upper conductive plate, the upper conductive plate is connected to the positive electrode of the bare shell battery, and a wire is used to connect the upper conductive plate and the lower conductive plate for discharge, and then the change in the wire current is detected to detect the change in the discharge state and the discharge end point.

[0055] After testing, it was found that the discharge time of Example 5 was 18.2 h, and the maximum discharge temperature was 85.6° C. This was mainly because as the discharge time increased, the conductive particles were gradually oxidized, which increased the internal resistance of the conductive particles, and thus caused the discharge rate to gradually slow down.

[0056] Example 6

[0057] A method for improving the discharge rate of waste bare shell batteries, comprising the following steps:

[0058] A copper alloy sheet is used as a lower conductive plate 1, spherical graphite particles are placed on the lower conductive plate 1 as conductive particles 3, two light-shell batteries 2 are inserted into the conductive particles 3, a gap is left between the two light-shell batteries 2, and the insertion depth of the two light-shell batteries 2 is 6.5 mm, and then the copper alloy sheet is used as an upper conductive plate 1, the upper conductive plate 1 is connected to the positive electrodes of the two light-shell batteries 2, and the upper conductive plate 1 and the lower conductive plate 1 are connected with a wire 4, and discharge is performed, and then the current change of the wire 4 is detected to detect the change of the discharge state and the discharge end point.

[0059] After testing, the discharge time and the maximum discharge temperature of the treatment process of Example 6 were tested, and it was measured that the discharge time in Example 6 was 9.3h and the maximum discharge temperature was 71.6°C.

[0060] Example 7

[0061] A method for improving the discharge rate of waste bare shell batteries comprises the following steps:

[0062] An aluminum sheet is used as a lower conductive plate, graphite particles are placed on the lower conductive plate, 10 light-shell batteries are inserted into the graphite particles, and gaps are left between the 10 light-shell batteries. The insertion depth of the 10 light-shell batteries is 13 mm. Then the aluminum sheet is used as an upper conductive plate, the upper conductive plate is connected to the positive electrodes of the 10 light-shell batteries, and the upper conductive plate and the lower conductive plate are connected with a wire for discharge, and then the change in the wire current is detected to detect the change in the discharge state and the discharge end point.

[0063] The test method of Example 3 was used to test the discharge time and the maximum discharge temperature of the treatment process of Example 6. The discharge time in Example 6 was measured to be 9.3 h, and the maximum discharge temperature was 81.0° C.

[0064] Comparative Example 2

[0065] A method for improving the discharge rate of waste bare shell batteries, comprising the following steps:

[0066] A bare shell battery was inserted into a 10wt% salt water pool for discharge, and the discharge time was about 5 days. Since the discharge was carried out in water, the temperature change was small and could not be measured. Since this method was used for discharge, the valuable black powder in the bare shell battery was leached into the salt water during the discharge process, resulting in material loss and high subsequent salt water treatment costs.

[0067] In addition, after calculation and comparison, the processing cost of comparative example 2 is about 800-900 yuan / ton, while the processing cost of embodiments 1-4 is about 400.05 yuan / ton. It can be seen that the method of the present invention can greatly reduce the processing cost of waste bare shell batteries and has good application prospects.

[0068] In summary, the method of the present invention is used to treat waste bare shell batteries, which can greatly reduce the discharge time of the waste bare shell batteries and has a high treatment efficiency; and the treatment process can control the discharge rate, and the treatment process is relatively safe; the process can greatly reduce the treatment cost, which is conducive to large-scale treatment of waste bare shell batteries and is conducive to the commercial promotion and application of the method.

[0069] It should be noted that, in the present application, the terms "comprise", "include" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises one ..." does not exclude the presence of other identical elements in the process, method, article or device including the element. In the present application, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically specified.

[0070] The above description is only a specific implementation of the present application, so that those skilled in the art can understand or implement the present application. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein can be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application will not be limited to the embodiments shown herein, but will conform to the widest range consistent with the principles and novel features applied for herein.

Claims

1. A method for increasing the discharge rate of waste bare shell batteries, characterized in that: The following steps are involved: Conductive particles are placed on the lower conductive plate, the light-shell battery is inserted into the conductive particles, the upper conductive plate is connected to the positive electrode of the light-shell battery, and the upper conductive plate and the lower conductive plate are connected with a wire for discharge, and then the change of the wire current is detected to detect the change of the discharge state and the discharge end point.

2. The method for improving the discharge rate of waste bare shell batteries according to claim 1, characterized in that: The resistance of the conductive particles is within 0.8Ω.

3. The method for improving the discharge rate of waste bare shell batteries according to claim 2, characterized in that: The conductive particles are graphite particles or carbon steel balls.

4. The method for improving the discharge rate of waste bare shell batteries according to claim 1, characterized in that: The conductive plate is a conductive metal sheet.

5. The method for improving the discharge rate of waste bare shell batteries according to claim 1, characterized in that: The wire is one wire or multiple wires.

6. The method for increasing the discharge rate of waste bare shell batteries according to any one of claims 1 to 5, characterized in that: The light shell battery has one or more.

7. The method for increasing the discharge rate of waste bare shell batteries according to claim 6, characterized in that: There are gaps between the plurality of light housing cells.

8. The method for increasing the discharge rate of waste bare shell batteries according to claim 1, characterized in that: There is a gap between the negative electrode of the light shell battery and the conductive plate.

9. The method for increasing the discharge rate of waste bare shell batteries according to claim 1, characterized in that: The depth of the light shell battery inserted into the conductive particles is within 3 / 5 of the height of the light shell battery.

10. The method for increasing the discharge rate of waste bare shell batteries according to claim 1, characterized in that: The device for executing the method for improving the discharge rate of waste bare shell batteries comprises a conductive plate, a wire and conductive particles, wherein the conductive plate comprises an upper conductive plate and a lower conductive plate, the wire connects the upper conductive plate and the lower conductive plate, and the conductive particles are placed on the lower conductive plate and do not contact the upper conductive plate.