Metaacidic potassium cocoyl glycinate powder as well as preparation method and application thereof

By adjusting the pH value of potassium cocoyl glycine and using specific pH regulators, combined with scraper drying method, the problem of slow dissolution of potassium cocoyl glycine powder is solved, and the efficiency and cost of cleanser production are improved. benefit.

CN118948643APending Publication Date: 2024-11-15SHANGHAI CHEERMORE COSMETICS CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411030751.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing potassium cocoyl glycine powder has high pH, ​​slow dissolution speed and lots of foam during dissolution, resulting in high energy consumption and increased cost during the preparation of cleanser.

Method used

By adjusting the pH value of cocoyl glycine potassium to 6.00-7.00, using anhydrous citric acid, lactic acid or citric acid as the pH regulator, and using scraper drying method to prepare acidic potassium glycine powder to improve its dissolution and defoaming properties.

Benefits of technology

The dissolution rate and defoaming rate of cocoyl glycine potassium powder are significantly improved, the energy consumption and cost of cleanser production are reduced, and the technical bias of better dissolution performance of alkaline powders in the prior art is overcome.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention relates to meta-acidic potassium cocoyl glycinate powder and a preparation method and application thereof.According to the meta-acidic potassium cocoyl glycinate powder, firstly, the pH value of liquid potassium cocoyl glycinate is adjusted to 6.00-7.00 through a pH adjusting agent, then scraping and drying are conducted, then smashing or grinding is conducted, and the meta-acidic potassium cocoyl glycinate powder is obtained, the potassium cocoyl glycinate powder is a slightly acidic potassium cocoyl glycinate powder with high dissolution efficiency and dissolution defoaming efficiency, the average particle size of the potassium cocoyl glycinate powder is 188-233 microns, the dissolution rate is 0.42-1.88 g / min, and the dissolution defoaming rate is 0.32-0.56 g / min. When the potassium cocoyl glycinate powder is used as one of the raw materials for producing the facial cleanser, the dissolving and defoaming time can be reduced by 45.0% compared with the slightly alkaline potassium cocoyl glycinate powder, so that the energy consumption in the production process is effectively reduced, the production cost of facial cleanser enterprises is reduced, and the production efficiency is relatively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of cosmetic raw materials, and more specifically, to a slightly acidic potassium cocoyl glycinate powder and a preparation method and application thereof. Background Art

[0002] In the potassium cocoyl glycinate cleanser, the raw material potassium cocoyl glycinate powder is mainly used as a foaming agent in the cosmetic cleanser, because it is required to have good solubility and foaming properties when used as a foaming agent.

[0003] If rich foam is required, a sufficient amount of potassium cocoyl glycinate needs to be added to the cleanser. However, the effective concentration of commercially available liquid potassium cocoyl glycinate is generally 26-33%, which cannot achieve a high proportion of effective activity in the cleanser. Therefore, it is necessary to add potassium cocoyl glycinate solid powder to ensure a sufficient total amount of surfactant in the cleanser.

[0004] However, in the prior art, the solid powder of potassium cocoyl glycinate has a high pH value, is generally alkaline, is fluffy, has a low bulk density, and has a low dissolution efficiency, that is, a slow dissolution rate. At the same time, the defoaming time during the dissolution process is long, resulting in high energy consumption and an increase in the preparation cost of the potassium cocoyl glycinate cleanser.

[0005] Furthermore, during the preparation of the facial cleanser, high pH, ​​i.e. alkaline potassium cocoyl glycinate powder is added. When the pH of the system is high, most of the potassium cocoyl glycinate exists in the system in the form of salt, and has high solubility. When the pH is low, potassium cocoyl glycinate will partially decompose and exist in the system in the form of cocoyl glycine, and its solubility is reduced. Therefore, it is generally believed that during the preparation of the facial cleanser, high pH, ​​i.e. alkaline potassium cocoyl glycinate powder has better solubility performance.

[0006] In summary, the current high pH, ​​i.e. alkaline potassium cocoyl glycinate powder has technical problems such as slow dissolution speed, high foam during dissolution, and difficulty in defoaming, so that when it is used in the preparation of facial cleansers, the heating time is long, the energy consumption is high, and the production cost is increased. Summary of the invention

[0007] In order to solve the technical problems of the above-mentioned alkaline potassium cocoyl glycinate powder, such as slow dissolution speed, high foam during dissolution, and difficulty in defoaming, the present application provides a slightly acidic potassium cocoyl glycinate powder, a preparation method and application thereof.

[0008] Technical principle of this application There will be some cocoyl glycine in the potassium cocoyl glycinate raw material, which will lower the pH value and increase the proportion of cocoyl glycine. The solubility of cocoyl glycine is worse than that of potassium cocoyl glycinate, which increases the hydrophobicity of the raw material powder to a certain extent, making it difficult for the powder to be wetted on the outside first, and then wrapping the unwetted powder in the middle to form a gel.

[0009] The technical solution of this application In a first aspect, the present application provides a method for preparing a slightly acidic potassium cocoyl glycinate powder, using the following technical scheme: A method for preparing a slightly acidic potassium cocoyl glycinate powder, the steps are as follows: First, the pH value of the liquid potassium cocoyl glycinate is adjusted to 6.00-7.00 with a pH adjuster, and then dried, and finally crushed or ground to an average particle size of 188-233 μm to obtain a slightly acidic potassium cocoyl glycinate powder; The liquid potassium cocoyl glycinate used above has a pH value of 8.00-9.00 and is produced by Changsha Puji Biotechnology Co., Ltd.; The pH regulator is one or a combination of two or more of anhydrous citric acid, lactic acid or monosodium citrate; The drying is carried out by a blade drying method.

[0010] By adopting the above technical scheme, due to the synergistic effect of a special pH regulator and a blade drying method in the preparation process, the finally obtained slightly acidic potassium cocoyl glycinate powder has a large average particle size but good solubility and also has good solubility and defoaming performance. The average particle size is 188-233 μm and the bulk density is 0.51-0.73 g / cm 3 , the dissolution rate is 0.42-1.88g / min, and the dissolution and defoaming rate is 0.32-0.56g / min.

[0011] Preferably, the pH regulator used in the preparation process is anhydrous citric acid, lactic acid or monosodium citrate; By adopting the above scheme, when anhydrous citric acid, lactic acid or monosodium citrate is used as a pH regulator in the preparation process, the dissolution rate of the finally obtained slightly acidic potassium cocoyl glycinate powder can reach 0.77-1.88 g / min, and the dissolution and defoaming rate is 0.32-0.56 g / min. Compared with the slightly alkaline potassium cocoyl glycinate powder of the prior art, under the same conditions, its dissolution rate is relatively increased by 286%, and the dissolution and defoaming rate is relatively increased by 87%, which shows that the slightly acidic potassium cocoyl glycinate powder obtained by the preparation method of the present application has good solubility and also has good dissolution and defoaming performance.

[0012] More preferably, the pH regulator used in the preparation process is anhydrous citric acid; When anhydrous citric acid is used as a pH regulator in the preparation process, the dissolution rate of the obtained slightly acidic potassium cocoyl glycinate powder can reach up to 1.88 g / min, and the dissolution and defoaming rate can reach up to 0.56 g / min.

[0013] The above drying adopts the scraper drying method, and the temperature of the drying process is controlled at 100-110°C, preferably at 105°C. Too high a process control temperature will cause the powder to turn yellow, and too low a process control temperature will prolong the drying time.

[0014] By adopting the above technical scheme, the use of the scraper drying method and the use of a special pH regulator in the preparation process synergistically enhance the solubility and dissolution and defoaming properties of the finally obtained slightly acidic potassium cocoyl glycinate powder.

[0015] In a second aspect, the present application provides a slightly acidic potassium cocoyl glycinate powder obtained by the preparation method of the above-mentioned slightly acidic potassium cocoyl glycinate powder.

[0016] By adopting the above technical scheme, the acidic potassium cocoyl glycinate powder has its hydrophobic properties changed due to its acidic nature, and the finally obtained potassium cocoyl glycinate powder has better solubility and better foaming effect.

[0017] A slightly acidic potassium cocoyl glycinate powder with an average particle size of 188-233 μm and a bulk density of 0.51-0.73 g / cm 3 , the dissolution rate is 0.42-1.88g / min, and the dissolution and defoaming rate is 0.32-0.56g / min. That is, although it has a large average particle size, it has good dissolution performance and dissolution and defoaming performance.

[0018] In a third aspect, the present application provides the use of the above-mentioned slightly acidic potassium cocoyl glycinate powder as a foaming agent in a cosmetic facial cleanser, wherein the amount used is calculated by mass ratio, and the slightly acidic potassium cocoyl glycinate powder: the total mass of raw materials used in the facial cleanser is 10-30:100, preferably the slightly acidic potassium cocoyl glycinate powder: the total mass of raw materials used in the facial cleanser is 20-30:100, and more preferably the slightly acidic potassium cocoyl glycinate powder: the total mass of raw materials used in the facial cleanser is 30:100.

[0019] Using the above technical solution, That is, when the slightly acidic potassium cocoyl glycinate powder of the present application is used as a foaming agent in the production of facial cleansing milk, the production energy consumption of the enterprise can be reduced, the production cost can be further reduced, and the production efficiency of the enterprise can be improved.

[0020] Beneficial technical effects of this application The slightly acidic potassium cocoyl glycinate powder of the present application adopts a special pH regulator and a blade drying method in the preparation process to cooperate with each other, and the finally obtained slightly acidic potassium cocoyl glycinate powder has the characteristics of large particle size, large bulk density, good solubility, and also has good solubility and defoaming performance. The particle size is 188-233 μm and the bulk density is 0.51-0.73 g / cm 3 , the dissolution rate is 0.42-1.88g / min, and the dissolution and defoaming rate is 0.32-0.56g / min.

[0021] Furthermore, the slightly acidic potassium cocoyl glycinate powder of the present application is compared with the slightly alkaline potassium cocoyl glycinate powder of the prior art. Under the same conditions, the dissolution rate is increased by 286%, that is, the potassium cocoyl glycinate powder has better solubility in slightly acidic conditions. This shows that the slightly acidic potassium cocoyl glycinate powder of the present application overcomes the technical prejudice generally believed in the prior art that solid potassium cocoyl glycinate powder has better solubility in slightly alkaline pH.

[0022] Furthermore, since the slightly acidic potassium cocoyl glycinate powder of the present application has a better dissolution effect although the average particle size of the particles is relatively large, the technical prejudice commonly believed in the prior art that the smaller the particle size of the potassium cocoyl glycinate powder, the better the dissolution effect.

[0023] Furthermore, since the slightly acidic potassium cocoyl glycinate powder of the present application has better foaming performance, it can be used as a foaming agent in the production of facial cleansers. At the same time, since it has a good dissolution and defoaming rate, it can effectively reduce the energy consumption of the production process, thereby reducing the production cost of facial cleansers companies and improving the production efficiency of the companies. DETAILED DESCRIPTION

[0024] The technical solution of the present application is described in detail below with reference to the embodiments, but the present application is not limited thereto.

[0025] The raw material specifications and manufacturer information used in each example of this application are as follows: 1. Liquid potassium cocoyl glycinate, pH 8.00-9.00, produced by Changsha Puji Biotechnology Co., Ltd.; 2. Sodium lauroamphoacetate, model MIRANOL ULTRA L-32, produced by Solvay 3. Glyceryl stearate, model number is Cutina GMS-V, produced by BASF of Germany; 4. Acrylic acid (ester) copolymer, model EMUL 34C, produced by Tianci Company; 5. Ethylene glycol distearate, model: Cithrol TMEGDS, produced by Croda; 6. PCA sodium, model AJIDEW NL-50, produced by Ajinomoto Co., Ltd. of Japan; 7. The water is pure water with a pH value of 7.0; 8. Anhydrous citric acid, lactic acid, monosodium citrate, and glycerol are commercially available; The equipment used in each embodiment of this application: Drum scraper dryer, model HG-600; produced by Changzhou Jialimei Drying Equipment Co., Ltd.; Fluidized bed dryer, model FG-0.5; produced by Changzhou Runyao Drying Equipment Co., Ltd. Spray dryer, model YM-8000B; manufactured by Shanghai Yuming Instrument Co., Ltd.; Crusher: Model RT-N04; manufactured by Rongcong Precision Technology Co., Ltd. Grinding equipment: glass mortar, model 150mm; manufactured by Huaou Glass; The particle size of the acidic potassium cocoyl glycinate powder or alkaline potassium cocoyl glycinate powder obtained in each example of the present application is measured using a laser particle size analyzer, model HORIBA LA-960V2, produced by HORIBA Co., Ltd. of Japan; The bulk density (rough measurement) test method of the acidic potassium cocoyl glycinate powder or the alkaline potassium cocoyl glycinate powder obtained in each example of the present application is measured according to the tap density determination method-fixed volume method, using a 100 ml cylindrical measuring cup.

[0026] The solubility and dissolution and defoaming properties (including dissolution rate and dissolution and defoaming rate) of the slightly acidic potassium cocoyl glycinate powder obtained in each example of the present application are determined by the following method: The raw materials used to prepare the test solution are calculated based on 100g of the test solution. The composition and content of the raw materials used to prepare the test solution are as follows: Preparation of test solution: First, add 30g of glycerin into a container, then add 12g of water, then add 30g of slightly acidic potassium cocoyl glycinate powder, and finally add 28g of water, control the temperature to 85-90°C and the rotation speed to 50-60rpm for stirring until the slightly acidic potassium cocoyl glycinate powder is completely dissolved and the foam is completely eliminated, to obtain a test solution, i.e., a solution containing slightly acidic potassium cocoyl glycinate; The calculation formula of the dissolution rate of the slightly acidic potassium cocoyl glycinate powder = the amount of the slightly acidic potassium cocoyl glycinate powder contained in the test solution (g) / the time taken for the slightly acidic potassium cocoyl glycinate powder to be completely dissolved (min); The calculation formula of the dissolution and defoaming rate of the slightly acidic potassium cocoyl glycinate powder = the amount of the slightly acidic potassium cocoyl glycinate powder contained in the test solution (g) / the time (min) taken for the slightly acidic potassium cocoyl glycinate powder to be completely dissolved until the foam is completely eliminated.

[0027] Example 1 A slightly acidic potassium cocoyl glycinate powder is prepared by the following steps: The pH value of the liquid potassium cocoyl glycinate is adjusted to 6.73 by a pH regulator, and then a blade dryer is used to control the temperature to 105° C. for blade drying, and then the powder is crushed and ground to obtain a slightly acidic potassium cocoyl glycinate powder with an average particle size of 189 μm; The pH value of the liquid potassium cocoyl glycinate is 8.00-9.00, and it is produced by Changsha Puji Biotechnology Co., Ltd.; the pH regulator is anhydrous citric acid.

[0028] The bulk density of the acidic potassium cocoyl glycinate powder obtained above was measured to be 0.73 g / cm 3 ; During the solubility test of the above-obtained slightly acidic potassium cocoyl glycinate powder, the slightly acidic potassium cocoyl glycinate powder was completely dissolved after stirring for 21 minutes, and the foam was completely eliminated after defoaming for 33 minutes. The total time for dissolution and defoaming was 54 minutes. The dissolution rate was calculated to be 1.43 g / min, and the dissolution and defoaming rate was 0.56 g / min.

[0029] Comparative Example 1 of Example 1 A slightly alkaline potassium cocoyl glycinate, which is different from Example 1 in that: liquid potassium cocoyl glycinate is directly used, the temperature is controlled to be 105° C. for drying, and then crushed and ground in sequence, that is, pH adjustment is not performed by a pH adjuster during the preparation process, to obtain a slightly alkaline potassium cocoyl glycinate powder with an average particle size of 189 μm; The liquid potassium cocoyl glycinate has a pH value of 8.00-9.00 and is produced by Changsha Puji Biotechnology Co., Ltd.

[0030] According to the dissolution performance test method of the slightly acidic potassium cocoyl glycinate powder of the present application, the slightly alkaline potassium cocoyl glycinate powder obtained above was tested. During the test process, the slightly alkaline potassium cocoyl glycinate powder obtained above was used to replace the slightly acidic potassium cocoyl glycinate powder in the test method. During the dissolution performance test process, the slightly alkaline potassium cocoyl glycinate powder obtained above was completely dissolved when stirred for 82 minutes, and the foam was completely eliminated after defoaming for 15 minutes. The total time for dissolution and defoaming was 97 minutes. After calculation, its dissolution rate was 0.37g / min, and the dissolution and defoaming rate was 0.30g / min.

[0031] The alkaline potassium cocoyl glycinate powder obtained above was measured to have a bulk density of 0.59 g / cm 3 .

[0032] The average particle size, bulk density, dissolution efficiency and dissolution defoaming rate of the slightly acidic potassium cocoyl glycinate powder obtained in Example 1 and the slightly alkaline potassium cocoyl glycinate powder obtained in Comparative Example 1 of Example 1 are summarized in the following table: The solubility performance of the slightly acidic potassium cocoyl glycinate powder obtained in the above-mentioned embodiment 1 and the slightly alkaline potassium cocoyl glycinate powder obtained in the comparative example 1 of embodiment 1 is compared. It can be seen that relative to the slightly alkaline potassium cocoyl glycinate powder, when the drying method, drying temperature and average particle size of the potassium cocoyl glycinate powder are the same, the solubility performance and dissolution and defoaming performance of the slightly acidic potassium cocoyl glycinate powder obtained in embodiment 1 are better, that is, the dissolution rate of the slightly acidic potassium cocoyl glycinate powder is increased by 286% compared with the slightly alkaline potassium cocoyl glycinate powder, and the dissolution and defoaming rate is increased by 87%. It is shown that the slightly acidic potassium cocoyl glycinate powder of the present application overcomes the technical prejudice that the slightly alkaline potassium cocoyl glycinate powder has better solubility performance generally believed in the prior art. Further, the improvement of the dissolution and defoaming rate is not as good as the improvement of the dissolution rate, which also shows that the slightly acidic potassium cocoyl glycinate powder of the present application has a good foaming effect, which is conducive to its application as a foaming agent in facial cleansing milk.

[0033] The slightly acidic potassium cocoyl glycinate powder obtained in the above-mentioned Example 1 and the slightly alkaline potassium cocoyl glycinate powder obtained in the comparative example 1 of Example 1 were tested for solubility performance (the solubility performance test of the slightly alkaline potassium cocoyl glycinate powder obtained in the comparative example 1 of Example 1 was carried out according to the test method for the solubility performance and dissolution and defoaming performance (including dissolution rate and dissolution and defoaming rate) of the slightly acidic potassium cocoyl glycinate powder of the present application, except that the slightly acidic potassium cocoyl glycinate powder was replaced with the slightly alkaline potassium cocoyl glycinate powder obtained in the comparative example 1 of Example 1). The same amount of 30 g of the slightly acidic potassium cocoyl glycinate powder obtained in Example 1 and the slightly alkaline potassium cocoyl glycinate powder obtained in the comparative example 1 of Example 1 were completely dissolved, and the time taken for the powder to be completely dissolved until the foam was completely eliminated was shown in the following table: Comparing the dissolution of the potassium cocoyl glycinate powder obtained by the above-mentioned Example 1 and the comparative example 1 of Example 1, it can be seen that: when the amounts of potassium cocoyl glycinate powder, glycerin and water are the same, and the same rotation speed and temperature conditions are controlled during the dissolution process, the time taken for dissolution and defoaming is completely different when potassium cocoyl glycinate powder with different pH is used, that is, the time required for dissolution by the acidic potassium cocoyl glycinate powder of Example 1 of the present application is relatively shortened by (82-21min) / 82min*100%=74% compared with the alkaline potassium cocoyl glycinate powder in the comparative example 1 of Example 1. This shows that the different pH values ​​of potassium cocoyl glycinate powder directly affect its dissolution rate. Analysis shows that the reason may be that in the acidic potassium cocoyl glycinate powder, part of the potassium cocoyl glycinate exists in the raw material in the form of cocoyl glycine, which reduces the hydrophilicity of the powder, and is not prone to the phenomenon of external water absorption and internal drying to form micelles, making the powder easier to slowly and evenly combine with water; the time used for defoaming after dissolution is relatively increased by 120%, which further shows that the acidic potassium cocoyl glycinate powder obtained in the present application has a better foaming effect and is more conducive to its use as a foaming agent in facial cleansers.

[0034] Comparative Example 2 of Example 1 A slightly acidic potassium cocoyl glycinate powder is different from Example 1 in that the drying is carried out by a boiling drying method, and the temperature of the drying chamber and the air inlet are controlled to be 105° C. during the drying process to carry out boiling drying, thereby obtaining a slightly acidic potassium cocoyl glycinate powder with an average particle size of 170 μm.

[0035] Comparative Example 3 of Example 1 A slightly acidic potassium cocoyl glycinate powder is different from Example 1 in that a spray dryer is used for drying, and the temperature is controlled at 105° C. for spray drying to obtain a slightly acidic potassium cocoyl glycinate powder with an average particle size of 150 μm.

[0036] The particle size, bulk density, dissolution rate and defoaming rate of the slightly acidic potassium cocoyl glycinate powder obtained by the scraper method in the above-mentioned Example 1, the boiling drying method in the comparative example 2 of Example 1, and the spray drying method in the comparative example 3 of Example 1 are shown in the following table: The average particle size, bulk density, and dissolution rate of the slant-acidic potassium cocoyl glycinate powder obtained by the above-mentioned Example 1 and the comparative examples 2-3 of Example 1 are compared. It can be seen that under the same pH value, the average particle size of the slant-acidic potassium cocoyl glycinate powder prepared by the blade drying method is large, the bulk density is larger, and the dissolution rate of the powder prepared by the spray drying method is higher than that of the powder prepared by the blade drying method, but the dissolution and defoaming rate of the powder prepared by the blade drying method is the highest. This shows that the use of the blade drying method in the preparation process of the slant-acidic potassium cocoyl glycinate powder of the present application and the use of a special pH regulator synergistically enhance the solubility and dissolution and defoaming properties of the slant-acidic potassium cocoyl glycinate powder finally obtained.

[0037] Example 2 A slightly acidic potassium cocoyl glycinate powder, the difference being that the anhydrous citric acid used as a pH regulator in the preparation process is replaced by lactic acid; the rest is the same as in Example 1, and the slightly acidic potassium cocoyl glycinate powder is finally obtained.

[0038] Example 3 A slightly acidic potassium cocoyl glycinate powder, the difference being that the anhydrous citric acid used as a pH regulator in the preparation process is replaced by monosodium citric acid; the rest is the same as in Example 1, and the slightly acidic potassium cocoyl glycinate powder is finally obtained.

[0039] Example 4 A slightly acidic potassium cocoyl glycinate powder is different from Example 1 in that the anhydrous citric acid used as a pH regulator in its preparation process is replaced by a complex of anhydrous citric acid and monosodium citrate, and the used complex of anhydrous citric acid and monosodium citrate is calculated by mass ratio, that is, citric acid: monosodium citrate is 1:1; the rest is the same as Example 1, and finally the slightly acidic potassium cocoyl glycinate powder is obtained.

[0040] Example 5 A slightly acidic potassium cocoyl glycinate powder, the difference being that anhydrous citric acid used as a pH regulator in its preparation process is replaced by a complex of anhydrous citric acid and lactic acid, and the used complex of anhydrous citric acid and lactic acid is calculated by mass ratio, that is, anhydrous citric acid:lactic acid is 1:1; the rest is the same as in Example 1, and finally the slightly acidic potassium cocoyl glycinate powder is obtained.

[0041] The average particle size, bulk density, dissolution rate and dissolution defoaming rate of the acidic potassium cocoyl glycinate powder obtained in the above Examples 1-5, when the pH adjuster is anhydrous citric acid, lactic acid, monosodium citric acid, a 1:1 complex of citric acid and monosodium citrate, and a 1:1 complex of citric acid and lactic acid, respectively, are tested, and the test results of the average particle size, bulk density, dissolution rate and dissolution defoaming rate of the alkaline potassium cocoyl glycinate powder obtained in the control example of Example 1 are listed in the following table: By comparing the dissolution rate and dissolution and defoaming rate of the slightly acidic potassium cocoyl glycinate powder obtained in Examples 1-5 in the above table, it can be seen that the pH regulator used in the preparation process of the slightly acidic potassium cocoyl glycinate powder of the present application is preferably anhydrous citric acid, lactic acid or monosodium citrate, and particularly preferably anhydrous citric acid. When anhydrous citric acid is used as the pH adjuster in Example 1, the dissolution rate and dissolution defoaming rate of the partially acidic potassium cocoyl glycinate powder obtained are respectively increased by 43% and 30% compared with those when lactic acid is used as the pH adjuster in Example 2, the dissolution rate and dissolution defoaming rate of the partially acidic potassium cocoyl glycinate powder obtained are respectively increased by 86% and 75% compared with those when monosodium citric acid is used as the pH adjuster in Example 3, the dissolution efficiency and dissolution defoaming rate of the partially acidic potassium cocoyl glycinate powder obtained are respectively increased by 240% and 70% compared with those when the pH adjuster in Example 4 is a complex of anhydrous citric acid and monosodium citrate, and the dissolution rate and dissolution defoaming rate of the partially acidic potassium cocoyl glycinate powder obtained are respectively increased by 138% and 27% compared with those when the pH adjuster in Example 5 is a complex of anhydrous citric acid and lactic acid.

[0042] Further, by comparing the bulk density of the slightly acidic potassium cocoyl glycinate powder obtained in Examples 1-5 in the above table, it can be seen that when the pH regulator of Example 1 uses anhydrous citric acid, the bulk density of the slightly acidic potassium cocoyl glycinate powder finally obtained when the pH regulator of Example 2 uses lactic acid is increased by 28%, the bulk density of the slightly acidic potassium cocoyl glycinate powder obtained when the pH regulator of Example 3 uses monosodium citric acid is increased by 9%, the bulk density of the slightly acidic potassium cocoyl glycinate powder obtained when the pH regulator of Example 4 uses a complex of anhydrous citric acid and monosodium citric acid is increased by 43%, and the bulk density of the slightly acidic potassium cocoyl glycinate powder obtained when the pH regulator of Example 5 uses a complex of anhydrous citric acid and lactic acid is increased by 43%. This shows that when the slightly acidic potassium cocoyl glycinate powder of the present application is used as a foaming agent in a facial cleanser, the slightly acidic potassium cocoyl glycinate powder can be put into the pot all at once without overflowing.

[0043] Further, by comparing the average particle size and dissolution rate of the slightly acidic potassium cocoyl glycinate powder obtained in Examples 1-5 in the above table with the slightly alkaline potassium cocoyl glycinate powder obtained in the control example of Example 1, it can be seen that although the slightly acidic potassium cocoyl glycinate powder of the present application has a larger average particle size, it has a good dissolution effect, thereby overcoming the technical prejudice in the prior art that the smaller the particle size, the better the dissolution effect.

[0044] Example 6 A slightly acidic potassium cocoyl glycinate powder, the difference being that the average particle size after crushing and grinding during the preparation process is different; the other aspects are the same as those in Example 1, and finally the slightly acidic potassium cocoyl glycinate powder is obtained.

[0045] The average particle size, bulk density, dissolution rate and dissolution defoaming rate of the slightly acidic potassium cocoyl glycinate powder obtained in Example 6 above were tested, and the test results of the average particle size, bulk density, dissolution rate and dissolution defoaming rate of the slightly acidic potassium cocoyl glycinate powder obtained in Example 1 are listed in the following table: It can be seen from the above table that when the pH regulator is anhydrous citric acid and other preparation conditions are the same, the dissolution rate is different when the final product particle size is different. The larger the particle size, the greater the dissolution rate. When the average particle size increases by 4.76%, the dissolution rate increases by 31.47%, which further shows that the slightly acidic potassium cocoyl glycinate powder of the present application can achieve a larger particle size and a better dissolution effect, that is, it overcomes the technical prejudice generally believed in the prior art that the smaller the particle size of the powder particles, the better the dissolution effect.

[0046] Example 7 A slightly acidic potassium cocoyl glycinate powder is different from Example 1 in that a pH regulator is used in the preparation process to adjust the pH value of liquid cocoyl glycine to 6.50, and the other steps are the same as those in Example 1, and finally the slightly acidic potassium cocoyl glycinate powder is obtained.

[0047] Example 8 A slightly acidic potassium cocoyl glycinate powder is different from that in Example 1 in that a pH regulator is used in the preparation process to adjust the pH value of liquid potassium cocoyl glycinate to 7.00, and the rest is the same as in Example 1, and finally the slightly acidic potassium cocoyl glycinate powder is obtained.

[0048] Example 9 A slightly acidic potassium cocoyl glycinate powder is different from that in Example 1 in that a pH regulator is used in the preparation process to adjust the pH value of liquid cocoyl glycine to 6.00, and the rest is the same as in Example 1, and finally the slightly acidic potassium cocoyl glycinate powder is obtained.

[0049] The average particle size, bulk density, dissolution rate and dissolution defoaming rate of the slightly acidic potassium cocoyl glycinate powder obtained in the above Examples 7-9 were detected, and compared with the average particle size, bulk density, dissolution rate and dissolution defoaming rate of the slightly acidic potassium cocoyl glycinate powder obtained in Example 1. The results are shown in the following table: The results in the above table show that when anhydrous citric acid is used as the pH regulator, the pH values ​​are adjusted to 6.73, 6.50, 7.00 and 6.00 respectively. The obtained slightly acidic potassium cocoyl glycinate powder can achieve good dissolution rate and dissolution defoaming rate when the average particle size is basically the same.

[0050] Application Example 1 A cream-forming amino acid facial cleanser containing slightly acidic potassium cocoyl glycinate, the raw material composition and content thereof are as follows (the total composition is 100%), calculated by mass percentage: The balance is water; The above-mentioned slightly acidic potassium cocoyl glycinate powder is the slightly acidic potassium cocoyl glycinate powder obtained in Example 1.

[0051] The preparation method of the above-mentioned cream-forming amino acid cleanser containing slightly acidic potassium cocoyl glycinate comprises the following steps: Add glycerin to a container, then add 30% water of the total water mass, then add slightly acidic potassium cocoyl glycinate powder, turn on the mixer at 50-60rpm to stir evenly, then add sodium lauroylamphoacetate, glyceryl stearate, ethylene glycol distearate, then control the temperature to 85-90°C and the rotation speed to 50-60rpm for stirring for 0.9h, at which time the slightly acidic potassium cocoyl glycinate powder is completely dissolved and the foam is completely eliminated, then immediately cool to 50-60°C, add sodium PCA, anhydrous citric acid, acrylic acid (ester) copolymer and the remaining water, stir and mix, then continue to cool to room temperature under stirring to obtain a cream-forming amino acid cleanser containing slightly acidic potassium cocoyl glycinate.

[0052] Comparative Example of Application Example 1 A cream-forming amino acid facial cleanser containing alkaline potassium cocoyl glycinate powder, the raw material composition and content of which are as follows (the total composition is 100%), calculated by mass percentage: The balance is water; The alkaline potassium cocoyl glycinate powder is the alkaline potassium cocoyl glycinate powder obtained in Comparative Example 1.

[0053] The preparation method of the above-mentioned cream-forming amino acid cleanser containing alkaline potassium cocoyl glycinate comprises the following steps: Add glycerin to a container, then add water that accounts for 30% of the total water mass, then add alkaline potassium cocoyl glycinate powder, turn on the mixer at 50-60rpm and stir evenly, then add sodium lauroylamphoacetate, glyceryl stearate, ethylene glycol distearate, then control the temperature to 85-90°C and the rotation speed to 50-60rpm for stirring for 1.62h, at which time the alkaline potassium cocoyl glycinate powder is completely dissolved and the foam is completely eliminated, then immediately cool to 50-60°C, add sodium PCA, anhydrous citric acid, acrylic acid (ester) copolymer and the remaining water, stir and mix, then continue to cool to room temperature under stirring to obtain a cream-forming amino acid cleanser containing alkaline potassium cocoyl glycinate.

[0054] The final products of the above-mentioned Application Example 1 and the control example of Application Example 1 were observed in terms of product appearance and foam performance. The results showed that the comprehensive weighted scores were similar. By comparing the observation results, it can be seen that there is little difference in the appearance and foam performance of the final products.

[0055] Further, in the above-mentioned application example 1, in the preparation process of the paste-type amino acid cleanser of the reference example of application example 1, when the amount of cocoyl glycine potassium powder used is the same, when a kind of slant-acid cocoyl glycine potassium powder of the present application is used as a foaming agent for the production of cleanser, only 0.9h can be used to reach the state that the slant-acid cocoyl glycine potassium powder is completely dissolved and the foam is completely eliminated, and when the slant-alkaline cocoyl glycine potassium powder is used as a foaming agent for the production of cleanser, 1.62h is required to reach the state that the slant-alkaline cocoyl glycine potassium powder is completely dissolved and the foam is completely eliminated. Thus, it is shown that when the amount of use is the same, a kind of slant-acid cocoyl glycine potassium powder of the present application, the time of its complete dissolution and complete elimination of foam relative to the slant-alkaline cocoyl glycine potassium powder in the prior art is reduced by 45.0%, which also verifies that a kind of slant-acid cocoyl glycine potassium powder of the present application has good dissolution and defoaming performance, so it can reduce the production energy consumption of the enterprise, further reduce the production cost, and improve the production efficiency of the enterprise.

[0056] Application Example 2 A cream-forming amino acid facial cleanser containing slightly acidic potassium cocoyl glycinate, the raw material composition and content thereof are as follows (the total composition is 100%), calculated by mass percentage: The balance is water; The above-mentioned slightly acidic potassium cocoyl glycinate powder is the slightly acidic potassium cocoyl glycinate powder obtained in Example 1.

[0057] The preparation method of the above-mentioned cream-forming amino acid facial cleanser containing the slightly acidic potassium cocoyl glycinate obtained in Example 1 is the same as that of Application Example 1, and finally a cream-forming amino acid facial cleanser containing the slightly acidic potassium cocoyl glycinate is obtained.

[0058] Application Example 3 A cream-forming amino acid facial cleanser containing slightly acidic potassium cocoyl glycinate, the raw material composition and content thereof are as follows (the total composition is 100%), calculated by mass percentage: The balance is water; The above-mentioned slightly acidic potassium cocoyl glycinate powder is the slightly acidic potassium cocoyl glycinate powder obtained in Example 1.

[0059] The cream-type amino acid facial cleanser products containing slightly acidic potassium cocoyl glycinate finally obtained in the above-mentioned application examples 1, 2, and 3, when the usage amounts of the slightly acidic potassium cocoyl glycinate powder as a raw material are 30%, 20%, and 10%, respectively, the obtained slightly acidic potassium cocoyl glycinate cream-type amino acid facial cleanser can meet the use requirements of cosmetics in terms of foaming performance, but the foam expression and cleaning power of application examples 1 and 2 are significantly better than those of application example 3, and the foam expression and cleaning power of application example 1 are more significantly better than those of application example 2.

[0060] In summary, the acidic potassium cocoyl glycinate powder of the present application has good solubility and fast dissolution and defoaming rate, although its average particle size is large. Therefore, when it is used as one of the raw materials to prepare a paste-forming amino acid high-foaming facial cleanser containing potassium cocoyl glycinate powder, production energy can be effectively saved and the production cost of the facial cleanser manufacturer can be reduced.

Claims

1. A method for preparing a slightly acidic potassium cocoyl glycinate powder, characterized in that The steps of its preparation process are as follows: First, the pH value of the liquid potassium cocoyl glycinate is adjusted to 6.00-7.00 with a pH regulator, then dried, and finally crushed or ground to obtain a slightly acidic potassium cocoyl glycinate powder; The pH regulator is one of anhydrous citric acid, lactic acid or monosodium citrate or a combination of two or more thereof.

2. The method for preparing a slightly acidic potassium cocoyl glycinate powder as claimed in claim 1, wherein The pH regulator is anhydrous citric acid, lactic acid or monosodium citrate.

3. The method for preparing a slightly acidic potassium cocoylglycinate powder as claimed in claim 1, wherein The liquid potassium cocoyl glycinate used in the preparation has a pH value of 8.00-9.

00.

4. The method for preparing a slightly acidic potassium cocoylglycinate powder as claimed in claim 3, wherein The liquid potassium cocoyl glycinate used in the preparation is produced by Changsha Puji Biotechnology Co., Ltd.

5. The method for preparing a slightly acidic potassium cocoyl glycinate powder as claimed in claim 1, wherein The drying is carried out by a blade drying method, and the temperature during the drying process is controlled at 100-110°C.

6. The method for preparing a slightly acidic potassium cocoylglycinate powder as claimed in claim 5, wherein The temperature of the drying process is controlled at 105°C.

7. A slant-acidic potassium cocoyl glycinate powder obtained by the preparation method of a slant-acidic potassium cocoyl glycinate powder as described in any one of claims 1 to 6.

8. The acidic potassium cocoyl glycinate powder according to claim 7, having an average particle size of 188-233 μm and a bulk density of 0.51-0.73 g / cm 3 , the dissolution rate is 0.42-1.88g / min, and the dissolution and defoaming rate is 0.32-0.56g / min.

9. The use of the slightly acidic potassium cocoyl glycinate powder as claimed in claim 7 as a foaming agent in a cosmetic facial cleanser, characterized in that The dosage is calculated based on the mass ratio of the slightly acidic potassium cocoyl glycinate powder to the total mass of the raw materials used in the cleanser in a ratio of 10-30:

100.

10. The use of the slightly acidic potassium cocoyl glycinate powder as claimed in claim 9 as a foaming agent in a cosmetic facial cleanser, characterized in that The dosage is calculated based on the mass ratio of the slightly acidic potassium cocoyl glycinate powder to the total mass of the raw materials used in the cleanser in a ratio of 20-30:100.

Citation Information

Cited By

  • Transparent weakly acidic system containing potassium cocoyl glycinate and application thereof

    CN122075323A