Preparation method of high-purity molybdenum dioxide dichloride
By heating the molybdenum pentachloride raw material in a tube reactor and purifying it using a metal nanopore filtration device, the problems of low yield and low purity of molybdenum dichloride dioxide were solved, and high-efficiency and environmentally friendly high-purity preparation was achieved. Reduced production costs.
Patent Information
- Application Number
- CN202411183642.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-15
AI Technical Summary
The existing synthesis methods of molybdenum dichloride and molybdenum dioxide have problems of low yield, low purity and high production costs.
Heat the high-purity molybdenum pentachloride raw material in a tube reactor, and oxygen reaction is introduced under argon protection. Then, the dichloro-molybdenum dioxide gas is collected and purified through a metal nanopore filtration device to achieve high purity. Preparation of molybdenum dichloride dioxide.
It improves production yield, reduces energy consumption and operating costs, ensures high purity and environmental protection of the product, reduces the use of toxic gases, and extends the service life of the filter device.
Smart Images

Figure CN118954594A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of preparing high-purity molybdenum dichloride dioxide, and in particular to a method for preparing high-purity molybdenum dichloride dioxide, belonging to the technical field of chemistry. Background Art
[0002] Molybdenum dioxide dichloride is an important inorganic chemical widely used in chemical industry, metallurgy and materials science. High-purity molybdenum dioxide dichloride has a wide range of applications in electronic materials. Its electrical conductivity, optical properties, chemical stability and thermal stability make it one of the ideal materials for preparing high-performance electronic devices. Storage chips and logic chips after 5nm need Mo source instead of W. Because of its better dielectric constant, molybdenum dioxide dichloride is tested as one of the best molybdenum sources and is used as one of the molybdenum sources for chemical vapor deposition of molybdenum-containing materials.
[0003] The synthetic method of molybdenum dioxide dichloride is as follows at present: (1)MoOCl4+ O(Si(CH3)3)2→MoO2Cl2+ 2ClSi(CH3)3 (2) MoO2 + Cl2 → MoO2Cl2 (3) Mo + O2 + Cl2 → MoO2Cl2 (4) MoO3+C+Cl2→MoO2Cl2 The above-mentioned traditional synthesis methods have problems such as low yield, low purity or high production cost. Summary of the invention
[0004] The present invention aims to provide a method for preparing high-purity molybdenum dioxide dichloride, in particular a method for purifying molybdenum dioxide dichloride.
[0005] To achieve the purpose of the present invention, the following technical scheme is adopted: a method for preparing high-purity molybdenum dioxide dichloride, comprising the following steps: S1: Put high-purity molybdenum pentachloride raw material into a tubular reactor, pass argon gas for protection, heat to 200-400°C, turn off the argon gas, pass oxygen into the tubular reactor, react for 4-6 hours, obtain molybdenum dioxide dichloride gas and molybdenum pentachloride gas, turn off the oxygen, pass argon gas, collect and cool the above gases through a cooler, and obtain a crude product of a mixture of molybdenum dioxide dichloride solid and molybdenum pentachloride solid; S2: Under the protection of argon, the crude product is added into the purification device from the feed port, wherein the purification device is equipped with a metal nanopore filter device, the feed port is located below the metal nanopore filter device, and the discharge port is located above the metal nanopore filter device. The temperature in the purification device is heated to not less than 200°C to sublime molybdenum dioxide dichloride, and molybdenum dioxide dichloride vapor is separated. The vapor passes through the metal nanopore filter device and flows out from the discharge port to obtain high-purity molybdenum dioxide dichloride. The molybdenum pentachloride solid is separated and reused.
[0006] Furthermore, the purity of the high-purity molybdenum dichloride is ≥99.99%.
[0007] Furthermore, the oxygen gas flow rate is: 100-220mL / min.
[0008] Furthermore, the pore size of the metal nanopore filter device is 2-20nm.
[0009] Further; the purity of the high-purity molybdenum dichloride in step S2 is greater than 5N.
[0010] Compared with the prior art, the beneficial effects of the present invention are as follows: the preparation reaction of the present invention is a one-step reaction, and the reaction temperature is relatively low, and unreacted molybdenum pentachloride can be repeatedly reacted, thereby improving the production yield and reducing unnecessary waste; no toxic gas is used in the preparation reaction process of the present invention, which greatly guarantees the life safety of operators; the present invention uses a metal nanopore filter device to filter and purify the crude molybdenum dioxide dichloride product, and has a nanometer-level filter pore size, which can effectively intercept tiny particles, organic matter, inorganic matter and other impurities in the gas, ensuring that the purity of the gas reaches a high standard, and in the filtering process, no chemical agent is needed, thereby achieving true green environmental protection, and the efficient filtering capacity reduces the energy consumption in the production process, saving a large amount of energy costs for the enterprise; and the metal nanopore filter device has a long service life, reduces the frequency and cost of replacing the filter, has low maintenance costs, and reduces the operating costs of the enterprise. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 Schematic diagram of the metal nanopore filtration device of the present invention. DETAILED DESCRIPTION
[0012] In order to more fully explain the implementation of the present invention, implementation examples of the present invention are provided. These implementation examples are merely elaborations of the present invention and do not limit the scope of the present invention.
[0013] In a specific embodiment, ICP-MS is used to analyze and detect the metal ion impurity content of the product. Example 1
[0014] A preparation method and purification device of high-purity molybdenum dioxide dichloride, comprising the following steps: S1: Mix multiple batches of 10kg molybdenum pentachloride raw materials with a purity of more than 99.99%, pass argon gas protection, put them into a tubular reactor and heat them to 200°C, turn off the argon gas, and then pass dry oxygen into the tubular reactor at a flow rate of 150mL / min to react to obtain molybdenum dioxide dichloride gas and a small amount of molybdenum pentachloride gas. After reacting for 4 hours, turn off the oxygen, pass argon gas, and collect these gases through a cooler to obtain molybdenum dioxide dichloride solid and a small amount of molybdenum pentachloride solid. ; S2: Under the protection of argon, the crude product is sublimated at a temperature of 200°C to separate molybdenum dioxide dichloride vapor. The waste residue in the vapor falls into the waste solid collector of the purification device. The molybdenum dioxide dichloride vapor is filtered and purified by a purification device with a metal nanopore size of 20nm and a heat preservation temperature of 200°C. Finally, 6.80kg (theoretical 7.27kg) of high-purity molybdenum dioxide dichloride product is obtained, with a direct yield of up to 93.53%. The waste residue such as molybdenum pentachloride in the waste solid collector repeats the step S1 operation. Example 2
[0015] A preparation method and purification device of high-purity molybdenum dioxide dichloride, comprising the following steps: S1: Mix multiple batches of 10kg molybdenum pentachloride raw materials with a purity of more than 99.99%, pass argon gas protection, put them into a tubular reactor and heat them to 200°C, turn off the argon gas, and then pass dry oxygen into the tubular reactor at a flow rate of 150mL / min to react to obtain molybdenum dioxide dichloride gas and a small amount of molybdenum pentachloride gas. After reacting for 5 hours, turn off the oxygen, pass argon gas, collect these gases through a cooler, and obtain molybdenum dioxide dichloride solid and a small amount of molybdenum pentachloride solid. ; S2: Under the protection of argon, the crude product is sublimated at a temperature of 200°C to separate molybdenum dioxide dichloride vapor. The waste residue in the vapor falls into the waste solid collector of the purification device. The molybdenum dioxide dichloride vapor is filtered and purified by a purification device with a metal nanopore size of 10nm and a heat preservation temperature of 200°C. Finally, 6.42kg (theoretical 7.27kg) of high-purity molybdenum dioxide dichloride product is obtained, with a direct yield of up to 88.30%. The waste residue such as molybdenum pentachloride in the waste solid collector repeats the step S1 operation. Example 3
[0016] A preparation method and purification device of high-purity molybdenum dioxide dichloride, comprising the following steps: S1: Mix multiple batches of 10kg molybdenum pentachloride raw materials with a purity of more than 99.99%, pass argon gas protection, put them into a tubular reactor and heat them to 200°C, turn off the argon gas, and then pass dry oxygen into the tubular reactor at a flow rate of 150mL / min to obtain molybdenum dioxide dichloride gas and a small amount of molybdenum pentachloride gas. After reacting for 6 hours, turn off the oxygen, pass argon gas, collect these gases through a cooler, and obtain molybdenum dioxide dichloride solid and a small amount of molybdenum pentachloride solid. ; S2: Under the protection of argon, the crude product is sublimated at a temperature of 200°C to separate molybdenum dioxide dichloride vapor. The waste residue in the vapor falls into the waste solid collector of the purification device. The molybdenum dioxide dichloride vapor is filtered and purified by a purification device with a metal nanopore size of 2nm and a heat preservation temperature of 200°C. Finally, 5.16kg (theoretical 7.27kg) of high-purity molybdenum dioxide dichloride product is obtained, with a direct yield of up to 70.78%. The waste residue such as molybdenum pentachloride in the waste solid collector repeats the step S1 operation. Example 4
[0017] A method for preparing high-purity molybdenum dioxide dichloride, comprising the following steps: S1: Mix multiple batches of 10kg molybdenum pentachloride raw materials with a purity of more than 99.99%, pass argon gas protection, put them into a tubular reactor and heat them to 300°C, turn off the argon gas, and then pass dry oxygen into the tubular reactor at a flow rate of 150mL / min to obtain molybdenum dioxide dichloride gas and a small amount of molybdenum pentachloride gas. After reacting for 5 hours, turn off the oxygen, pass argon gas, collect these gases through a cooler, and obtain molybdenum dioxide dichloride solid and a small amount of molybdenum pentachloride solid. ; S2: Under the protection of argon, the crude product is sublimated at a temperature of 200°C to separate molybdenum dioxide dichloride vapor. The waste residue in the vapor falls into the waste solid collector of the purification device. The molybdenum dioxide dichloride vapor is filtered and purified by a purification device with a metal nanopore size of 10nm and a heat preservation temperature of 200°C. Finally, 6.75kg (theoretical 7.27kg) of high-purity molybdenum dioxide dichloride product is obtained, with a direct yield of up to 92.85%. The waste residue such as molybdenum pentachloride in the waste solid collector repeats the step S1 operation. Example 5
[0018] A method for preparing high-purity molybdenum dioxide dichloride comprises the following steps: S1: Mix multiple batches of 10kg molybdenum pentachloride raw materials with a purity of more than 99.99%, pass argon gas protection, put them into a tubular reactor and heat them to 300°C, turn off the argon gas, and then pass dry oxygen into the tubular reactor at a flow rate of 150mL / min to obtain molybdenum dioxide dichloride gas and a small amount of molybdenum pentachloride gas. After reacting for 5 hours, turn off the oxygen, pass argon gas, collect these gases through a cooler, and obtain molybdenum dioxide dichloride solid and a small amount of molybdenum pentachloride solid. ; S2: Under the protection of argon, the crude product is sublimated at a temperature of 200°C to separate molybdenum dioxide dichloride vapor. The waste residue in the vapor falls into the waste solid collector of the purification device. The molybdenum dioxide dichloride vapor is filtered and purified by a purification device with a metal nanopore size of 2nm and a heat preservation temperature of 200°C. Finally, 6.31kg (theoretical 7.27kg) of high-purity molybdenum dioxide dichloride product is obtained, with a direct yield of up to 86.80%. The waste residue such as molybdenum pentachloride in the waste solid collector repeats the operation of step S1. Example 6
[0019] A method for preparing high-purity molybdenum dioxide dichloride, comprising the following steps: S1: Mix multiple batches of 10kg molybdenum pentachloride raw materials with a purity of more than 99.99%, pass argon gas for protection, put them into a tubular reactor and heat them to 400°C, turn off the argon gas, and then pass dry oxygen into the tubular reactor at a flow rate of 150mL / min to obtain molybdenum dioxide dichloride gas and a small amount of molybdenum pentachloride gas. After reacting for 5h, turn off the oxygen, pass argon gas, collect these gases through a cooler, and obtain molybdenum dioxide dichloride solid and a small amount of molybdenum pentachloride solid; S2: Under the protection of argon, the crude product is sublimated at a temperature of 200°C to separate molybdenum dioxide dichloride vapor. The waste residue in the vapor falls into the waste solid collector of the purification device. The molybdenum dioxide dichloride vapor is filtered and purified by a purification device with a metal nanopore size of 10nm and a heat preservation temperature of 200°C. Finally, 6.83kg (theoretical 7.27kg) of high-purity molybdenum dioxide dichloride product is obtained, with a direct yield of up to 93.95%. The waste residue such as molybdenum pentachloride in the waste solid collector repeats the operation of step S1. Example 7
[0020] A method for preparing high-purity molybdenum dioxide dichloride, comprising the following steps: S1: Mix multiple batches of 10kg molybdenum pentachloride raw materials with a purity of more than 99.99%, pass argon gas protection, put them into a tubular reactor and heat them to 400°C, turn off the argon gas, and then pass dry oxygen into the tubular reactor at a flow rate of 150mL / min to obtain molybdenum dioxide dichloride gas and a small amount of molybdenum pentachloride gas. After reacting for 5 hours, turn off the oxygen, pass argon gas, collect these gases through a cooler, and obtain molybdenum dioxide dichloride solid and a small amount of molybdenum pentachloride solid. ; S2: Under the protection of argon, the crude product is sublimated at a temperature of 200°C to separate molybdenum dioxide dichloride vapor. The waste residue in the vapor falls into the waste solid collector of the purification device. The molybdenum dioxide dichloride vapor is filtered and purified by a purification device with a metal nanopore size of 2nm and a heat preservation temperature of 200°C. Finally, 6.50kg (theoretical 7.27kg) of high-purity molybdenum dioxide dichloride product is obtained, with a direct yield of up to 89.41%. The waste residue such as molybdenum pentachloride in the waste solid collector repeats the step S1 operation.
[0021] The following table 1 is a summary table of process conditions, yields and purities of Examples 1-7
[0022] Table 2 below shows the metal ion impurity content of the products analyzed by ICP-MS in some embodiments. (Unit: ppm)
[0023] The present invention also provides a purification device for high-purity molybdenum dichloride (i.e. the above-mentioned purification device), as shown in the attached Figure 1 As shown, the purification device includes a filter tank 1, an electric ball valve 3, a waste solid collector 2, a waste solid cleaning port 4, an armored thermocouple 5, a discharge port 7, a feed port 14, an oil inlet 13, an oil outlet 8, a filter device installation and regeneration port 9, a heat transfer oil interlayer 10, and a metal nanopore filter device 12; The filter tank body 1 is a hollow cylindrical body made of corrosion-resistant Hastelloy; the filter tank body is fixed by a support 1; The electric ball valve 3 is arranged at the bottom of the filter tank and connected to the waste solid collector, and is used to seal the filter tank and clean the waste solid collector; The waste solid cleaning port is arranged at the lower side of the filter tank; The armored thermocouple is arranged at the lower middle part of the filter tank; The feed port is arranged at the lower end of the filter tank, and the discharge port is arranged at the higher end of the filter tank; the oil inlet is arranged at the lower end of the filter tank, and the oil outlet is arranged at the higher end of the filter tank; The heat transfer oil interlayer is arranged around the filter tank; The filter device installation and regeneration port is arranged at the top of the filter tank; The metal nanopore filter device is arranged above the middle of the filter tank body, and the metal nanopore filter device is installed on the filter element fixing plate 11. The pore size of the metal nanopore filter device is 2-20nm.
[0024] When the above purification device is used, the crude product enters from the feed port 14, the heat transfer oil is heated to 200°C, and the sublimated molybdenum dioxide dichloride vapor passes through the metal nanoporous filter device and then comes out from the discharge port 7, and the waste residue falls into the waste solid collector of the purification device for collection.
[0025] After describing the implementation mode of the present invention in detail, people familiar with the technology can clearly understand that various changes and modifications can be made without departing from the scope and spirit of the above-mentioned patent application. Any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention are within the scope of the technical solution of the present invention, and the present invention is not limited to the implementation mode of the examples given in the specification.
Claims
1. A method for preparing high-purity molybdenum dioxide dichloride, Features The steps include: S1: Put high-purity molybdenum pentachloride raw material into a tubular reactor, pass argon gas for protection, heat to 200-400°C, turn off the argon gas, pass oxygen into the tubular reactor, react for 4-6 hours, obtain molybdenum dioxide dichloride gas and molybdenum pentachloride gas, turn off the oxygen, pass argon gas, collect and cool the above gases through a cooler, and obtain a crude product of a mixture of molybdenum dioxide dichloride solid and molybdenum pentachloride solid; S2: Under the protection of argon, the crude product is added into the purification device from the feed port, wherein the purification device is equipped with a metal nanopore filter device, the feed port is located below the metal nanopore filter device, and the discharge port is located above the metal nanopore filter device. The temperature in the purification device is heated to not less than 200°C to sublime molybdenum dioxide dichloride, and molybdenum dioxide dichloride vapor is separated. The vapor passes through the metal nanopore filter device and flows out from the discharge port to obtain high-purity molybdenum dioxide dichloride. The molybdenum pentachloride solid is separated and reused.
2. A method for preparing high-purity molybdenum dioxide dichloride according to claim 1, Features: The purity of the high-purity molybdenum dichloride is ≥99.99%.
3. A method for preparing high-purity molybdenum dioxide dichloride according to claim 1, Features: The oxygen gas flow rate is: 100-220mL / min.
4. A method for preparing high-purity molybdenum dioxide dichloride according to claim 1, Features: The pore size of the metal nanopore filter device is 2-20 nm.
5. A method for preparing high-purity molybdenum dioxide dichloride according to claim 1, Features: The purity of the high-purity molybdenum dioxide dichloride in step S2 is greater than 5N.
Citation Information
Cited By
Production process of electronic grade dichloromolybdenum dioxide
CN121405130A
Synthesis method of dichloromolybdenum dioxide
CN121948546A