Epoxy resin curing agent and preparation method thereof
By combining epoxy resin, dodecyl primary amine and 4,4'-diaminodicyclohexylmethane in the preparation method, the high temperature resistance and compatibility problems of existing epoxy resin curing agents are solved, and the problem of high temperature resistance and compatibility of the existing epoxy resin curing agents is realized. The good high temperature resistance and flexibility of the epoxy resin curing agent are simplified, and the preparation process is improved and the performance of the epoxy resin curing agent is improved.
Patent Information
- Application Number
- CN202411359601.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-27
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-09-27
AI Technical Summary
The existing epoxy resin curing agent has high toxicity, low reaction activity, high temperature resistance, high brittleness after curing, high environmental humidity, and poor compatibility and solubility with epoxy resin, affecting the final product. performance.
Using a preparation method of an epoxy resin curing agent, by adding epoxy resin, dodecyl primary amine and 4,4'-diaminodicyclohexylmethane at room temperature, stirring and cooling in water bath, and adding water-free Ethanol and ethyl acetate are used as solvents to control the solid content and prepare an epoxy resin curing agent with good high temperature resistance and flexibility.
It realizes good compatibility and epoxy resin of epoxy resin, improves the high temperature resistance and flexibility of the curing agent, solves the problems of poor compatibility with the curing agent and epoxy resin and the coating brittleness, and the preparation process Simple and environmentally friendly.
Smart Images

Figure FT_1 
Figure FT_2
Abstract
Description
Technical Field The present invention relates to the field of chemical materials, in particular to the field of polymer materials, and more particularly to an epoxy resin curing agent and a preparation method thereof. Background Art In the field of chemical materials, acrylic glue is widely used in many industries, such as automobile manufacturing, electronic appliances and construction industries, due to its excellent water resistance, environmental corrosion resistance and anti-discoloration performance; however, as electronic products continue to develop in the direction of multifunctionality, small and lightweight and / or high performance, acrylic esters are also introduced into certain high temperature resistant functional groups (such as epoxy functional groups, etc.). Epoxy resin (EP) has excellent various properties due to its special molecular structure, such as high dimensional stability, corrosion resistance, high adhesion, excellent medium resistance, etc. It is one of the most widely used resins and has been widely used in various industries. Epoxy resin is a thermoplastic resin with a linear structure. It cannot be used alone. When used, a curing agent needs to be added. It is only useful when it undergoes a cross-linking reaction with the curing agent to form an insoluble or infusible macromolecular polymer with a three-dimensional network structure. Therefore, the structure and performance of the curing agent are very important to epoxy resin, so the development of various new curing agents is very important to expand the application of epoxy resin. There are many types of epoxy resin curing agents, mainly polyamines, isocyanates, anhydrides, imidazoles and polythiols, among which amine curing agents are the most widely used curing agents, including aliphatic polyamines, alicyclic polyamines, low molecular weight polyamides, etc. Existing commercial curing agents have many disadvantages, such as high toxicity, low reactivity, not resistant to high temperatures, brittle coating after curing, and great influence of environmental humidity, etc.; and most epoxy resin curing agents have poor solubility in epoxy resin, resulting in uneven mixing, affecting the performance of the final product. Therefore, how to develop an epoxy resin curing agent compatible with epoxy resin is a technical problem that needs to be solved in the near future by technicians in this field. Summary of the invention The technical problem to be solved by the present invention is to avoid the deficiencies of the above-mentioned prior art and provide an epoxy resin curing agent and a preparation method thereof. The epoxy resin curing agent prepared by the present invention has a large number of benzene rings, dodecyl groups, etc. on its chain, so the epoxy resin curing agent has good high temperature resistance and flexibility, and has good compatibility with epoxy resin.
[0004] The technical solution adopted by the present invention to solve the technical problem is: Provided is a method for preparing an epoxy resin curing agent, comprising the following steps: Step A: adding a certain amount of epoxy resin and a certain amount of the first mixed solvent to a reaction bottle at room temperature, stirring evenly, and then adding a certain amount of dodecyl primary amine to react epoxy end-capping, stirring in a water bath at a certain temperature, stirring and reacting for a period of time to obtain a first mixed solution; Step B: Then, 4,4'-diaminodicyclohexylmethane is added to the first mixed solution in step A, and after heating to another certain temperature, stirring is continued in a water bath, stirring and reacting for another period of time, and then naturally cooling to room temperature to obtain a second mixed solution; Step C: Add the second mixed solvent to the second mixed solution in step B to make its solid content reach a certain value, stir evenly, and obtain the epoxy resin curing agent. After bottling, seal and put into a refrigerator for refrigeration.
[0005] In step A, the mass ratio of the epoxy resin to dodecyl primary amine is 1:(0.3-0.4).
[0006] In step A, the temperature in the water bath is 50-100°C.
[0007] In step B, the mass ratio of 4,4'-diaminodicyclohexylmethane to epoxy resin is (0.2-0.4):1.
[0008] In step A and step C, the first mixed solvent and the second mixed solvent both include anhydrous ethanol and ethyl acetate, and the mass ratio of anhydrous ethanol to ethyl acetate is (0.4-1):1.
[0009] The temperature of the water bath in step B is 5-10°C higher than the temperature of the water bath in step A.
[0010] In step C, the solid content is 25% to 50%.
[0011] In step A, the dodecyl primary amine can be replaced by laurylamine dipropylene diamine, 1-aminotetradecane, octadecyl primary amine or hexamethylene diamine.
[0012] The present invention also provides an epoxy resin curing agent, which is obtained according to the above preparation method. Specifically, the epoxy resin curing agent comprises epoxy resin, dodecyl primary amine and 4,4'-diaminodicyclohexylmethane.
[0013] Compared with the prior art, the epoxy resin curing agent and the preparation method thereof of the present invention have the following beneficial effects: 1. The present invention contains more high temperature resistant monomers or groups in the molecular combination, which can provide good temperature resistance, such as epoxy resin E51; 2. The flexible monomer used in the molecular combination of the present invention is an amine monomer, which has good flexibility and makes the molecular chain of the curing agent easy to move, thereby giving the curing agent good flexibility; for example, dodecyl primary amine, laurylamine dipropylene diamine, 1-aminotetradecane, octadecyl primary amine or hexamethylenediamine are used.
[0014] 3. Another end-capping monomer used in the molecular matching of the present invention is an alicyclic amine monomer, which can provide more reaction sites and can also achieve better epoxy resin reaction according to the designed molecular chain structure, such as 4,4'-diaminodicyclohexylmethane; Fourth, in the molecular combination of the present invention, the material is a polymer material with a molecular weight in the range of 10,000 to 20,000, has good compatibility with epoxy resin, and can cure epoxy resin at room temperature; 5. The epoxy resin curing agent of the present invention is firstly prepared by chain extension of bisphenol A epoxy resin containing a large number of benzene rings and amine monomers containing flexible groups, with excess epoxy resin, and finally end-capped with alicyclic amine monomers. The preparation process is simple to operate.
[0015] Therefore, the epoxy resin curing agent prepared by the present invention has good high temperature resistance and flexibility, and has good compatibility with epoxy resin; it can effectively solve the problems of the curing agent and epoxy resin being not resistant to high temperatures, poor compatibility, and strong rigidity of the molecular chain leading to brittle coatings. The synthesis method of the epoxy resin curing agent is simple and environmentally friendly, and provides a new idea for the subsequent research on curing agents. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 This is a list of various properties of new glue prepared by using the epoxy resin curing agent prepared in Example 1 of the present invention; Figure 2 The following is a table showing various properties of new glue prepared by using the epoxy resin curing agent prepared in Example 2 of the present invention. DETAILED DESCRIPTION
[0017] The present invention will be further described in detail below in conjunction with the accompanying drawings.
[0018] A method for preparing an epoxy resin curing agent comprises the following steps: Step A: Under room temperature conditions, which generally refers to 21°C to 25°C, a certain amount of epoxy resin and a certain amount of the first mixed solvent are added to the reaction bottle, stirred evenly, and then a certain amount of dodecyl primary amine is added to react epoxy end-capping, and stirred in a water bath at a certain temperature, the temperature in the water bath is 50 to 100°C, for example, the temperature in the water bath is maintained at 60°C, and stirred for a period of time, the period of time is 10 to 30 hours, for example, stirring reaction for 12 hours, to obtain a first mixed solution, the first mixed solution is generally a colorless, transparent, viscous solution; the reaction bottle generally adopts a four-necked flask equipped with a reflux condenser, a constant pressure dropping funnel, a stirring device and a thermometer; the mass ratio of the epoxy resin to the dodecyl primary amine is 1: (0.3 to 0.4); the amount of the first mixed solvent is at least enough to ensure that the epoxy resin and the dodecyl primary amine can be completely dissolved, generally speaking, the total mass ratio of the first mixed solvent to the epoxy resin and the dodecyl primary amine is (0.7 to 1): 1; the first mixed solvent is mainly a cosolvent, generally speaking, Amines can be dissolved in alcohols, and epoxy resins can be dissolved in ethyl acetate. Therefore, ethyl acetate and alcohols can be selected to form a first mixed solvent. For example, the first mixed solvent includes anhydrous ethanol and ethyl acetate. In the early stage of the reaction, alcohols (anhydrous ethanol) are used as co-solvents, which is very beneficial for dissolving amine substances. In the first mixed solution, the mass ratio of anhydrous ethanol to ethyl acetate is (0.4-1):1; the epoxy resin can be an epoxy resin of model E51; Step B: Then, 4,4'-diaminodicyclohexylmethane is added to the first mixed solution of step A, and the temperature is raised to another predetermined temperature, which is 5-10°C higher than the temperature in the water bath of step A. For example, if the temperature in the water bath of step A is maintained at 60°C, the temperature in the water bath of step B is maintained at 65°C-70°C, and stirring is continued in the water bath for another period of time, which is 10-30 hours, for example, stirring for 12 hours, and then naturally cooled to room temperature to obtain a second mixed solution, which is an amino-terminated polymer; in step B, the mass ratio of 4,4'-diaminodicyclohexylmethane to epoxy resin is (0.2-0.4):1; Step C: Add the second mixed solvent to the second mixed solution in step B to make its solid content reach a certain value, stir evenly, and the epoxy resin curing agent is obtained. After bottling, seal and put into the refrigerator for refrigeration. The purpose of refrigeration is to extend the shelf life of the epoxy resin curing agent. In this step C, the solid content is 25% to 50%, for example, the solid content reaches 40%. The second mixed solvent is also mainly a cosolvent. Generally speaking, amines can be dissolved in alcohols and epoxy resins can be dissolved in ethyl acetate. Therefore, ethyl acetate and alcohols can be selected to form a second mixed solvent. For example, the second mixed solvent includes anhydrous ethanol and ethyl acetate. In the second mixed solution, the mass ratio of anhydrous ethanol to ethyl acetate is (0.4 to 1):1.
[0019] The present invention also provides an epoxy resin curing agent obtained by the above preparation method. Specifically, the epoxy resin curing agent of the present invention comprises epoxy resin, dodecyl primary amine and 4,4'-diaminodicyclohexylmethane. The mass ratio of the epoxy resin, dodecyl primary amine and 4,4'-diaminodicyclohexylmethane is 1: (0.3-0.4): (0.2-0.4).
[0020] The dodecyl primary amine can be replaced by laurylamine dipropylene diamine, 1-aminotetradecane, octadecyl primary amine or hexamethylene diamine. Example
[0021] A method for preparing an epoxy resin curing agent comprises the following steps: Step A: at room temperature, add 90 grams of epoxy resin of model E51 and 90 grams of a first mixed solvent into a reaction bottle, wherein the first mixed solvent is a mixed solvent of anhydrous ethanol and ethyl acetate, wherein anhydrous ethanol accounts for 50% of the total mass of the first mixed solvent, and ethyl acetate accounts for 50% of the total mass of the first mixed solvent. After stirring evenly, add 28 grams of dodecyl primary amine to react epoxy end-capping, stir in a water bath at 60° C., stir and react for 12 hours to obtain a first mixed solution, which is generally a colorless, transparent, viscous solution; the reaction bottle generally uses a four-necked flask equipped with a reflux condenser, a constant pressure dropping funnel, a stirring device and a thermometer; Step B: Then, 32 g of 4,4'-diaminodicyclohexylmethane was added to the first mixed solution in step A, the temperature of the water bath was raised to 65°C, stirring was continued in the water bath, the reaction was stirred for 12 hours, and then naturally cooled to room temperature to obtain a second mixed solution, which was an amine-terminated polymer; Step C: Add a second mixed solvent to the second mixed solution of step B. The second mixed solvent is a mixed solvent of anhydrous ethanol and ethyl acetate, wherein anhydrous ethanol accounts for 50% of the total mass of the second mixed solvent, and ethyl acetate accounts for 50% of the total mass of the second mixed solvent, so that the solid content reaches 40%. Stir evenly to obtain an epoxy resin curing agent. After bottling, seal and put it in a refrigerator for refrigeration; GPC detection obtains a polymer with a weight average molecular weight of about 10,000 and a viscosity of 800-900 cps. GPC (Gel Permeation Chromatography) is a liquid chromatography technique mainly used to separate and determine the molecular weight and molecular weight distribution of polymers. Cps is a unit of viscosity, the full name is centipoise, which is often used to indicate the viscosity of a fluid.
[0022] Experimental results: Prepare 8 grams of homemade epoxy resin glue, 0.1 grams, 0.2 grams and 0.3 grams of epoxy resin curing agent prepared in Example 1, and 0.08 grams of DMP-30, respectively, and mix them into new glue; Figure 1 As shown, from this Figure 1 It can be seen that: the state of the newly prepared glue is visually "clear", indicating that the new glue can be dissolved in the epoxy resin glue; the 210°C high temperature resistance effect is "very good", indicating that the new glue has strong high temperature resistance; whether there is residual glue is "no residual glue"; therefore, the epoxy resin curing agent prepared in this embodiment 1 has good high temperature resistance and flexibility, and can be dissolved in the epoxy resin glue; DMP-30 is a catalyst for epoxy resin curing, namely: 2,4,6-tris(dimethylaminomethyl)phenol. Example
[0023] A method for preparing an epoxy resin curing agent comprises the following steps: Step A: at room temperature, add 90 grams of epoxy resin of model E51 and 90 grams of a first mixed solvent into a reaction bottle, wherein the first mixed solvent is a mixed solvent of anhydrous ethanol and ethyl acetate, wherein anhydrous ethanol accounts for 50% of the total mass of the first mixed solvent, and ethyl acetate accounts for 50% of the total mass of the first mixed solvent. After stirring evenly, add 34 grams of dodecyl primary amine to react epoxy end-capping, stir in a water bath at 60° C., stir and react for 12 hours to obtain a first mixed solution, which is generally a colorless, transparent, viscous solution; the reaction bottle generally uses a four-necked flask equipped with a reflux condenser, a constant pressure dropping funnel, a stirring device and a thermometer; Step B: Then, 19 g of 4,4'-diaminodicyclohexylmethane was added to the first mixed solution in step A, the temperature of the water bath was raised to 65°C, stirring was continued in the water bath, the reaction was stirred for 12 hours, and then naturally cooled to room temperature to obtain a second mixed solution, which was an amine-terminated polymer; Step C: Add a second mixed solvent to the second mixed solution in step B, wherein the second mixed solvent is a mixed solvent of anhydrous ethanol and ethyl acetate, wherein anhydrous ethanol accounts for 50% of the total mass of the second mixed solvent, and ethyl acetate accounts for 50% of the total mass of the second mixed solvent, so that the solid content reaches 40%, and stir evenly to obtain an epoxy resin curing agent, which is bottled and sealed and placed in a refrigerator for refrigeration; after GPC testing, a polymer with a weight average molecular weight of about 15,000 and a viscosity of 3000 to 3300 cps is obtained.
[0024] Experimental results: Prepare 8 grams of homemade epoxy resin glue, 0.1 grams, 0.2 grams and 0.3 grams of the curing agent prepared in Example 2, and 0.08 grams of DMP-30, respectively, and mix them into new glue; Figure 2 As shown, from this Figure 2 It can be seen that: the state of the newly prepared glue is visually "clear", indicating that the new glue can be dissolved in the epoxy resin glue; the 210°C high temperature resistance effect is "very good", indicating that the new glue has strong high temperature resistance; whether there is residual glue is "no residual glue"; therefore, the curing agent prepared in this embodiment 2 has good high temperature resistance and flexibility, and can be dissolved in epoxy resin glue.
[0025] The above-mentioned embodiments only express the preferred implementation modes of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the patent scope of the present invention. It should be pointed out that, for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, all equivalent changes and modifications made to the scope of the claims of the present invention should belong to the scope covered by the claims of the present invention.
Claims
1. A method for preparing an epoxy resin curing agent, characterized in that: The following steps are involved: Step A: Add a certain amount of epoxy resin and a certain amount of the first mixed solvent to a reaction bottle at room temperature, stir evenly, then add a certain amount of dodecyl primary amine to react epoxy end-capping, stir in a water bath at a certain temperature, and react for a period of time to obtain a first mixed solution; Step B: 4,4'-diaminodicyclohexylmethane is then added to the first mixed solution in step A, and the mixture is heated to another predetermined temperature, and then stirred in a water bath for another period of time, and then naturally cooled to room temperature to obtain a second mixed solution; Step C: Add the second mixed solvent to the second mixed solution in step B to make its solid content reach a certain value, stir evenly, and obtain the epoxy resin curing agent. After bottling, seal and refrigerate.
2. The method for preparing an epoxy resin curing agent according to claim 1, wherein: In step A, the mass ratio of the epoxy resin to the dodecyl primary amine is 1:(0.3-0.4).
3. The method for preparing the epoxy resin curing agent according to claim 1, wherein: In step A, the temperature in the water bath is 50-100°C.
4. The method for preparing an epoxy resin curing agent according to claim 1, wherein: In step B, the mass ratio of 4,4'-diaminodicyclohexylmethane to epoxy resin is (0.2-0.4):
1.
5. The method for preparing the epoxy resin curing agent according to claim 1, wherein: In step A and step C, the first mixed solvent and the second mixed solvent both include anhydrous ethanol and ethyl acetate, and the mass ratio of anhydrous ethanol to ethyl acetate is (0.4-1):
1.
6. The method for preparing an epoxy resin curing agent according to claim 1, wherein: The temperature of the water bath in step B is 5-10° C. higher than the temperature of the water bath in step A.
7. The method for preparing an epoxy resin curing agent according to claim 1, wherein: In step C, the solid content is 25% to 50%.
8. The method for preparing an epoxy resin curing agent according to claim 1, wherein: In step A, the dodecyl primary amine can be replaced by laurylamine dipropylene diamine, 1-aminotetradecane, octadecyl primary amine or hexamethylenediamine.
9. An epoxy resin curing agent, characterized in that: The epoxy resin curing agent obtained by the preparation method according to any one of claims 1 to 8, specifically, the epoxy resin curing agent comprises epoxy resin, dodecyl primary amine and 4,4'-diaminodicyclohexylmethane.
10. The epoxy resin curing agent according to claim 9, characterized in that: The dodecyl primary amine can be replaced by laurylamine dipropylene diamine, 1-aminotetradecane, octadecyl primary amine or hexamethylenediamine.
Citation Information
Patent Citations
Hardeners for cold-curing epoxy systems
CN105246939A
Liquid composition and epoxy resin curing agent using the same
JP2016190949A
Curing agents for epoxy resins based on 1,2-diaminocyclohexane
US5508373A
Mixture of cyanoalkylated polyamine and accelerator as latent hardener for epoxy resins
WO2015158684A1