Low-transfer low-precipitation silica gel protective film and preparation method thereof

By using silicone systems and carbon nanowhisker-loaded diatomaceous earth in semiconductor packaging, the problem of silicon transfer and precipitation in silicone protective film is solved, and the effect of low transfer and low precipitation is achieved, improving the quality and stability of packaging products sex.

CN118956329AActive Publication Date: 2024-11-15SUZHOU AOBEIXIN MATERIAL TECH LTD CO
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410990804.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-15
Estimated Expiration
2044-07-23

AI Technical Summary

Technical Problem

During semiconductor packaging, the existing silicone protective film has problems with silicon transfer and silicone oil precipitation, which affects the quality of the packaging product.

Method used

Using silicone system, silicone pressure-sensitive adhesive is prepared by methylvinyl silicone rubber, methyl hydrogen-containing MQ resin and other materials, and is subjected to high-temperature vacuum deselected small molecule treatment, combined with diatomaceous earth loaded with carbon nanowhiskers to improve the glue The dispersion and stability of the silicone oil can be reduced.

Benefits of technology

It significantly reduces silicone oil precipitation and silicon transfer, improves the heat resistance and stability of the protective film, and achieves the effect of low transfer and low precipitation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004958814740000101
    Figure BDA0004958814740000101
  • Figure BDA0004958814740000111
    Figure BDA0004958814740000111
Patent Text Reader

Abstract

The invention provides a low-transfer low-precipitation silica gel protective film and a preparation method thereof. Comprising the following steps: adding methyl vinyl silicone rubber, methyl hydrogen-containing MQ resin, a platinum catalyst and a solvent which are subjected to high-temperature vacuum distillation to remove small molecules into a reaction kettle, and heating and refluxing while stirring to obtain a prepolymer; adding the prepolymer, high-hydrogen-content silicone oil, an adhesion promoter, a platinum catalyst and a solvent into a glue mixing barrel, and uniformly stirring and dispersing to obtain an organic silicon pressure-sensitive adhesive; the preparation method comprises the following steps: taking a PI base material, carrying out corona treatment, coating an organic silicon pressure-sensitive adhesive on the PI base material, curing in a drying oven, overlapping a base film, and curing to obtain the low-transfer low-precipitation silica gel protective film. Firstly, raw materials are subjected to high-temperature vacuum micromolecule removal, the content of micromolecules is reduced, silicone oil precipitation is reduced from the source, and silicon transfer is reduced; pre-polymerization and curing are carried out in advance, the whole adhesive layer is integrated, silicone oil precipitation is reduced, and silicon transfer is reduced; and finally, by adding the diatomite loaded with the carbon nanowhiskers, the precipitation of silicon is further reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of silica gel films, and in particular to a low-transfer and low-precipitation silica gel protective film and a preparation method thereof. Background Art

[0002] In the field of semiconductor packaging, there is a packaging form that is particularly popular in the market, that is, QFN (Quad-Flat No-leads Package) packaging. QFN packaging is widely used in a variety of electronic products due to its compact size and excellent electrical performance. In the QFN packaging process, the QFN packaging protective film plays a key role, especially in ensuring the positioning accuracy of the lead frame and protecting the stability during the packaging process. The QFN packaging protective film is a single-sided tape made of polyimide (PI) as the base material and coated with an adhesive. At present, most of the protective films on the market use acrylic adhesives, but acrylic acid is not resistant to high temperatures. It is easy to have residual glue or even powder after high temperatures, which seriously affects the quality of the packaged products. Silicone pressure-sensitive adhesive has good high temperature resistance and stable adhesiveness. Generally, there will be no residual glue, which is very suitable for QFN packaging protective film. The current silicone protective film also has some problems, such as severe silicon transfer and silicone oil precipitation, which affects the QFN packaging back-end process. Therefore, it is of great significance to prepare a low transfer and low precipitation silicone protective film for semiconductor packaging. Summary of the invention

[0003] Technical problems to be solved: In view of the above technical problems, the purpose of the present invention is to provide a low-transfer and low-precipitation silicone protective film and a preparation method thereof. First, an organic silicon system is established, and methyl vinyl silicone rubber, methyl hydrogenated MQ resin and other materials are used to prepare an organic silicon pressure-sensitive adhesive. The raw materials are subjected to high-temperature vacuum de-small molecule removal to reduce the small molecule content, thereby reducing silicone oil precipitation and silicon transfer from the source; the organic silicon pressure-sensitive adhesive is pre-polymerized in advance and then solidified, and the entire adhesive layer is integrated to reduce silicone oil precipitation and silicon transfer; then, diatomaceous earth loaded with carbon nanowhiskers is added, and the huge specific surface area of ​​diatomaceous earth itself is utilized to improve the dispersibility and stability of the pressure-sensitive adhesive, thereby reducing silicon precipitation. At the same time, due to the porous characteristics of diatomaceous earth, sufficient nucleation sites can be provided to promote the one-dimensional directional growth of polyaniline nanowhiskers. After carbonization, a large amount of carbon nanofibers are loaded on the surface of the diatomaceous earth, which can improve the internal structure and interfacial bonding force of the pressure-sensitive adhesive and further reduce silicon precipitation.

[0004] Technical solution: A low transfer and low precipitation silicone protective film, including a PI substrate, a silicone pressure-sensitive adhesive and a base film, the silicone pressure-sensitive adhesive layer is located between the PI substrate and the base film, and the silicone pressure-sensitive adhesive includes the following weight components: 30 to 90 parts of methyl vinyl silicone rubber, 5 to 20 parts of methyl hydrogenated MQ resin, 0.5 to 3 parts of high hydrogenated silicone oil, 1.5 to 5 parts of diatomaceous earth loaded with carbon nano whiskers, 0.5 to 2 parts of adhesion promoter, 0.5 to 3 parts of platinum catalyst, and 150 to 400 parts of solvent. Furthermore, the molecular weight of the methyl vinyl silicone rubber is 700,000 to 1,000,000, and the vinyl mole fraction is 0.1 to 1.0%. Before use, the small molecules are removed by high-temperature vacuum distillation to make the volatile content less than 0.1%. Furthermore, the M / Q value of the methyl hydrogen-containing MQ resin is 0.7-0.9, and the active hydrogen content is 0.02-0.5%; the active hydrogen content of the high hydrogen-containing silicone oil is 1.2-1.6%. Furthermore, the preparation method of the diatomaceous earth loaded with carbon nano whiskers is as follows: S1: preparing a hydrochloric acid solution of aniline monomer with a concentration of 0.1-0.2 mol / L; S2: Take diatomaceous earth and dry it, use it as a base, add aniline monomer hydrochloric acid solution, and mix well; S3: adding ammonium persulfate solution for polymerization, and keeping the temperature at 5°C for 4 hours after the addition is completed, so as to orient the growth of polyaniline nanowhiskers; S4: Take out and wash with water and ethanol in sequence; S5: vacuum drying at 60°C; S6: Annealing at 850-950° C. for 2 h in a vacuum tube furnace with nitrogen protection to obtain diatomaceous earth loaded with carbon nanowhiskers. Furthermore, the diatomaceous earth particle size is 2 to 100 μm. Furthermore, the molar ratio of the aniline monomer to ammonium persulfate is 4:(1-3). Furthermore, the adhesion promoter is an organic siloxane with an epoxide; the platinum catalyst is one of a platinum-vinylsiloxane complex catalyst, an alcohol-modified chloroplatinic acid catalyst and a platinum acetylene complex, wherein the platinum content is 2000 to 8000 ppm. Furthermore, the adhesion promoter is 3-glycidyloxypropyltriethoxysilane or trimethoxy[2-(7-oxabicyclo[4.1.0]hept-3-yl)ethyl]silane. Furthermore, the platinum-vinylsiloxane complex catalyst is bis(1,3-divinyl-1,1,3,3-tetramethyldisiloxane) platinum; the alcohol-modified chloroplatinic acid catalyst is an ethanol-modified chloroplatinic acid catalyst; and the platinum acetylene-based complex is a bis(alkyne)(cyclodiene-based) platinum complex. Furthermore, the solvent is one or more of toluene, xylene, ethyl acetate, butyl acetate, n-heptane, 120# solvent oil, and butanone. The method for preparing the low transfer and low precipitation silica gel protective film comprises the following steps: (1) adding methyl vinyl silicone rubber, methyl hydrogenated MQ resin, platinum catalyst and solvent to a reaction kettle, and heating and refluxing for 1 hour under stirring to obtain a prepolymer; (2) adding the prepolymer to a mixing barrel, adding a solvent, stirring and dispersing for 10 minutes, adding diatomaceous earth loaded with carbon nano whiskers and high hydrogen silicone oil under stirring, and continuing to stir for 5 minutes; adding an adhesion promoter under stirring, and continuing to stir for 5 minutes; adding a platinum catalyst under stirring, and continuing to stir and disperse for 20 minutes, until the feed liquid is evenly mixed, to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate is taken, subjected to corona treatment, coated with a silicone pressure-sensitive adhesive and cured in an oven, and a base film is superimposed and aged to obtain a low transfer and low precipitation silicone protective film. Furthermore, the corona treatment condition is: power is 1.5 kW. Furthermore, the aging process in step (3) is as follows: aging temperature is 30 to 85° C., and aging time is 24 to 72 hours. The application of the above-mentioned low transfer and low precipitation silicone protective film in semiconductor packaging. Beneficial effects: 1. The present invention firstly establishes an organic silicon system, adopts methyl vinyl silicone rubber, methyl hydrogenated MQ resin and other materials to prepare an organic silicon pressure-sensitive adhesive, removes small molecules from the raw materials at high temperature and vacuum, reduces the small molecule content, reduces the silicone oil precipitation from the source, and reduces the silicon transfer; 2. The organic silicone pressure-sensitive adhesive of the present invention is pre-polymerized in advance and then cured, and the entire adhesive layer is integrated, which reduces the precipitation of silicone oil and reduces silicon transfer; 3. The present invention adds diatomaceous earth loaded with carbon nano whiskers, and utilizes the huge specific surface area of ​​diatomaceous earth itself to improve the dispersibility and stability of the pressure-sensitive adhesive, thereby reducing the precipitation of silicon. At the same time, due to the porous characteristics of diatomaceous earth, sufficient nucleation sites can be provided to promote the one-dimensional directional growth of polyaniline nano whiskers. After carbonization, a large amount of carbon nanofibers are loaded on the surface of diatomaceous earth, which can improve the internal structure and interface bonding force of the pressure-sensitive adhesive and further reduce the precipitation of silicon. 4. The diatomaceous earth loaded with carbon nano whiskers of the present invention has a three-dimensional porous structure, which can prevent its own agglomeration, so that it is more evenly dispersed in the pressure-sensitive adhesive. At the same time, the surface of the diatomaceous earth contains a large number of different types of hydroxyl groups, which can be well combined with the pressure-sensitive adhesive. 5. After the protective film is coated in the present invention and matured, the reaction can be more complete, and the silicone oil precipitation and silicon transfer can be further reduced. 6. In addition, the thermal stability of conventional silicone pressure-sensitive adhesives is poor, and diatomaceous earth loaded with carbon nanowhiskers can also improve the heat resistance of pressure-sensitive adhesives. DETAILED DESCRIPTION The present invention proposes a low transfer and low precipitation silica gel protective film and a preparation method thereof. In order to make the purpose, technical scheme and effect of the present invention clearer and more specific, the present invention will be further described in detail with reference to the embodiments below. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention. Example 1 The preparation method of diatomaceous earth loaded with carbon nano whiskers is as follows: S1: prepare 80 mL of 0.15 mol / L aniline monomer hydrochloric acid solution; S2: Take 5g of diatomaceous earth with a particle size of 2 to 100μm and dry it, use it as a substrate, add aniline monomer hydrochloric acid solution, and mix well; S3: Add ammonium persulfate solution dropwise for polymerization, and after the addition is completed, keep warm at 5℃ for 4h to grow polyaniline nano whiskers in a directional manner; the molar ratio of aniline monomer to ammonium persulfate is 2:1; S4: Take out and wash with water and ethanol in sequence; S5: vacuum drying at 60°C; S6: Annealing at 900° C. for 2 h in a vacuum tube furnace with nitrogen protection to obtain diatomaceous earth loaded with carbon nanowhiskers. Example 2 A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Example 3 A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.1%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Example 4 A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 20 parts of methyl hydrogenated MQ resin, 0.2 parts of platinum catalyst, and 70 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 180 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.75, and an active hydrogen content of 0.1%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Example 5 A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 60 parts of methyl vinyl silicone rubber from which small molecules have been removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.2 parts of platinum catalyst, and 70 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1.5 parts of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.5%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.1%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Example 6 A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 1.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Example 7 A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 2.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Example 8 A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Example 9 A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 70° C. for 48 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Comparative Example 1 The difference between this embodiment and embodiment 2 is that the methyl vinyl silicone rubber is not subjected to high-temperature vacuum distillation, and no prepolymerization is performed during the preparation of the glue. Specifically: A method for preparing a silicone protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber that has not been subjected to high-temperature vacuum distillation to remove small molecules and 10 parts of methyl hydrogenated MQ resin are added to a mixing barrel, and then 210 parts of solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogenated silicone oil are added, and stirring is continued for 5 minutes; under stirring, 1.2 parts of adhesion promoter are added, and stirring is continued for 5 minutes; under stirring, 1.1 parts of platinum catalyst are added, and stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain an organic silicone pressure-sensitive adhesive; (2) A PI substrate was taken and subjected to a corona treatment at a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Comparative Example 2 The difference between this embodiment and embodiment 2 is that no prepolymerization is performed during the preparation of the glue, specifically: A method for preparing a silicone protective film comprises the following steps: (1) Take 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, add them into a mixing barrel, add 210 parts of solvent, stir and disperse for 10 minutes, add 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogenated silicone oil under stirring, and continue stirring for 5 minutes; add 1.2 parts of adhesion promoter under stirring, and continue stirring for 5 minutes; add 1.1 parts of platinum catalyst under stirring, and continue stirring and dispersing for 20 minutes until the material liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (2) Take a PI substrate, subject it to a corona treatment with a power of 1.5 kW, coat the silicone pressure-sensitive adhesive thereon and cure it in an oven, overlay a base film, and age it at 85°C for 72 hours to obtain a silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Comparative Example 3 The difference between this embodiment and embodiment 2 is that the methyl vinyl silicone rubber is not subjected to high temperature vacuum distillation, as follows: A method for preparing a silicone protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber that has not been subjected to high-temperature vacuum distillation to remove small molecules, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent were added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate was taken and subjected to a corona treatment at a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Comparative Example 4 The difference between this embodiment and embodiment 2 is that the methyl vinyl silicone rubber is not subjected to high-temperature vacuum distillation, no prepolymerization is performed during the preparation of the glue, and the prepared protective film is not matured. Specifically: A method for preparing a silicone protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber that has not been subjected to high-temperature vacuum distillation to remove small molecules and 10 parts of methyl hydrogenated MQ resin are added to a mixing barrel, and then 210 parts of solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogenated silicone oil are added, and stirring is continued for 5 minutes; under stirring, 1.2 parts of adhesion promoter are added, and stirring is continued for 5 minutes; under stirring, 1.1 parts of platinum catalyst are added, and stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain an organic silicone pressure-sensitive adhesive; (2) A PI substrate is taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive is coated thereon and cured in an oven. A base film is superimposed without curing to obtain a silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Comparative Example 5 The difference between this embodiment and embodiment 2 is that the protective film is not cured, specifically: A method for preparing a silicone protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of the prepolymer are added to a mixing barrel, 150 parts of the solvent are added, and the mixture is stirred and dispersed for 10 minutes. Under stirring, 3.5 parts of diatomaceous earth loaded with carbon nano whiskers and 1 part of high hydrogen silicone oil are added, and the stirring is continued for 5 minutes; under stirring, 1.2 parts of an adhesion promoter are added, and the stirring is continued for 5 minutes; under stirring, 1 part of a platinum catalyst is added, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate is taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive is coated thereon and cured in an oven. A base film is superimposed without curing to obtain a silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogenated MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the active hydrogen content of the high hydrogenated silicone oil is 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Comparative Example 6 The difference between this embodiment and embodiment 2 is that diatomaceous earth loaded with carbon nano whiskers is not added, specifically: A method for preparing a low-transfer and low-precipitation silica gel protective film comprises the following steps: (1) 50 parts of methyl vinyl silicone rubber from which small molecules are removed by high-temperature vacuum distillation, 10 parts of methyl hydrogenated MQ resin, 0.1 parts of platinum catalyst, and 60 parts of solvent are added to a reaction kettle, and heated to 150° C. and refluxed for 1 hour under stirring to obtain a prepolymer; (2) 100 parts of prepolymer are added to a mixing barrel, 150 parts of solvent are added, and the mixture is stirred and dispersed for 10 minutes. 1 part of high hydrogen silicone oil is added under stirring, and the stirring is continued for 5 minutes. 1.2 parts of adhesion promoter are added under stirring, and the stirring is continued for 5 minutes. 1 part of platinum catalyst is added under stirring, and the stirring is continued for 20 minutes until the feed liquid is evenly mixed to obtain a silicone pressure-sensitive adhesive. (3) A PI substrate was taken and subjected to a corona treatment with a power of 1.5 kW. A silicone pressure-sensitive adhesive was coated thereon and cured in an oven. A base film was superimposed and aged at 85° C. for 72 h to obtain a low transfer and low precipitation silicone protective film. Among them, the methyl vinyl silicone rubber used has a molecular weight of 700,000, a vinyl molar fraction of 0.1%, and a volatile content of 0.05%; the methyl hydrogen-containing MQ resin M / Q=0.7, and an active hydrogen content of 0.05%; the high hydrogen-containing silicone oil has an active hydrogen content of 1.6%; the adhesion promoter is 3-glycidyloxypropyltriethoxysilane; the platinum catalyst is a platinum-vinylsiloxane complex catalyst, and the platinum content is 5000ppm; the solvent is a mixture of 120# solvent oil, ethyl acetate, and butanone in a volume ratio of 1:1:2. Take the protective film obtained in each embodiment and comparative example, remove the base film, obtain a sample, and test the silicon transfer rate and silicon precipitation respectively and record the test results. Among them: 1. The silicon transfer test method is: stick the protective film to a clean test steel plate, put it in a 70℃ oven for 20 hours, cool it for 2 hours, remove the protective film, directly stick NITTO 31B tape, let it stand for 20 minutes, test the peel strength with a tensile machine, and get the peel strength F1. The blank value is sticking NITTO 31B tape to a clean test steel plate, let it stand for 20 minutes, and test the peel strength with a tensile machine to get the peel strength F2. Transfer rate = (1-F1 / F2)*100% 2.2. The silicon precipitation test method is: take a circular copper foil with a diameter of 2 cm to test the dry silicon content on the copper foil surface, and obtain the dry silicon content F3; cut the protective film into a circular copper foil with a diameter of 2 cm and stick it on the surface of the copper foil, put it in a 200°C oven and bake it for 6 hours. After cooling, remove the protective film and test the dry silicon content on the copper foil surface to obtain the dry silicon content F4. Silicon precipitation = (F4-F3)*100% Table 1 As can be seen from Table 1, the protective film obtained in the embodiment of the present invention has a very small silicon transfer, less than 5.5%, and a silicon precipitation, less than 1.0%, which is not obvious, achieving low transfer and low precipitation.

Claims

1. A low transfer and low precipitation silicone protective film, comprising a PI substrate, an organic silicone pressure-sensitive adhesive and a base film, wherein the organic silicone pressure-sensitive adhesive layer is located between the PI substrate and the base film, and is characterized in that: The organic silicone pressure-sensitive adhesive comprises the following components by weight: 30-90 parts of methyl vinyl silicone rubber, 5-20 parts of methyl hydrogenated MQ resin, 0.5-3 parts of high hydrogenated silicone oil, 1.5-5 parts of diatomaceous earth loaded with carbon nano whiskers, 0.5-2 parts of adhesion promoter, 0.5-3 parts of platinum catalyst and 150-400 parts of solvent.

2. The low transfer and low precipitation silica gel protective film according to claim 1, characterized in that: The molecular weight of the methyl vinyl silicone rubber is 700,000 to 1,000,000, and the vinyl mole fraction is 0.1 to 1.0%. Before use, the small molecules are removed by high-temperature vacuum distillation to make the volatile content less than 0.1%.

3. The low transfer and low precipitation silica gel protective film according to claim 1, characterized in that: The M / Q value of the methyl hydrogen-containing MQ resin is 0.7-0.9, and the active hydrogen content is 0.02-0.5%; the active hydrogen content of the high hydrogen-containing silicone oil is 1.2-1.6%.

4. The low transfer and low precipitation silica gel protective film according to claim 1, characterized in that: The preparation method of the diatomaceous earth loaded with carbon nano whiskers is as follows: S1: preparing a hydrochloric acid solution of aniline monomer with a concentration of 0.1-0.2 mol / L; S2: Take diatomaceous earth and dry it, use it as a base, add aniline monomer hydrochloric acid solution, and mix well; S3: adding ammonium persulfate solution for polymerization, and keeping the temperature at 5°C for 4 hours after the addition is completed, so as to orient the growth of polyaniline nanowhiskers; S4: Take out and wash with water and ethanol in sequence; S5: vacuum drying at 60°C; S6: Annealing at 850-950° C. for 2 h in a vacuum tube furnace with nitrogen protection to obtain diatomaceous earth loaded with carbon nanowhiskers.

5. The low transfer and low precipitation silica gel protective film according to claim 4, characterized in that: The molar ratio of the aniline monomer to ammonium persulfate is 4:(1-3).

6. The low transfer and low precipitation silica gel protective film according to claim 1, characterized in that: The adhesion promoter is an organic siloxane with epoxide; the platinum catalyst is one of a platinum-vinylsiloxane complex catalyst, an alcohol-modified chloroplatinic acid catalyst and a platinum acetylene complex, wherein the platinum content is 2000-8000ppm.

7. The low transfer and low precipitation silica gel protective film according to claim 1, characterized in that: The solvent is one or more of toluene, xylene, ethyl acetate, butyl acetate, n-heptane, 120# solvent oil, and butanone.

8. A method for preparing a low transfer and low precipitation silica gel protective film according to any one of claims 1 to 7, comprising the following steps: (1) adding methyl vinyl silicone rubber, methyl hydrogenated MQ resin, platinum catalyst and solvent to a reaction kettle, and heating and refluxing for 1 hour under stirring to obtain a prepolymer; (2) adding the prepolymer to a mixing barrel, adding a solvent, stirring and dispersing for 10 minutes, adding diatomaceous earth loaded with carbon nano whiskers and high hydrogen silicone oil under stirring, and continuing to stir for 5 minutes; adding an adhesion promoter under stirring, and continuing to stir for 5 minutes; adding a platinum catalyst under stirring, and continuing to stir and disperse for 20 minutes, until the feed liquid is evenly mixed, to obtain a silicone pressure-sensitive adhesive; (3) A PI substrate is taken, subjected to corona treatment, coated with a silicone pressure-sensitive adhesive and cured in an oven, and a base film is superimposed and aged to obtain a low transfer and low precipitation silicone protective film.

9. The method for preparing a low transfer and low precipitation silica gel protective film according to claim 8, characterized in that: The aging process in step (3) is as follows: aging temperature is 30-85° C., and aging time is 24-72 hours.

10. Use of the low transfer and low precipitation silica gel protective film according to any one of claims 1 to 7 in semiconductor packaging.

Citation Information

Patent Citations

  • SBS-containing flame-retardant modified plastic and preparation method thereof

    CN106700381A

  • Anticorrosive paint on trailer surface

    CN108715715A

  • Trailer coating spraying technology

    CN108745838A

  • Organic silicon pressure-sensitive adhesive for AF anti-fingerprint screen

    CN109880584A

  • Low-climbing organic silicon pressure-sensitive adhesive and preparation method and application thereof

    CN113388362A