Method for preparing planar superfine densely-arranged grooves and nanowires without high-precision photoetching
Through mask plate lithography and PECVD technology, plane tight drain trenches are formed under high-precision lithography conditions, combined with plasma processing and plane solid-liquid solid growth technology, ultra-fine tight drain nanowires under wafer-free substrates are realized Growth solves the limitations of nanowire integration in the prior art and realizes a low-cost and high-quality nanowire array.
Patent Information
- Application Number
- CN202411090297.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-08-09
AI Technical Summary
The prior art is difficult to achieve the growth of ultrafine crystalline nanowire channels without high-precision lithography and wafer-free substrates, which limits the application of large-scale integration and three-dimensional integration of nanowires.
The edge pattern is defined by mask plate lithography technology, vertical side walls are formed by dry etching, dielectric layers of different thicknesses are deposited cyclically and alternately, top dielectric layers are removed by CMP technology, plane tight drainage trenches are formed, and plasma is passed. The treatment forms catalytic metal nanoparticles, and combines planar solid-liquid solid-growth technology to achieve nanowire growth without high-precision lithography.
Under 2 micron precision lithography conditions, a growth groove array below 15nm is achieved, and a nanowire array of about 10nm is grown, breaking through the limitations of lithography technology and achieving large-scale integration and three-dimensional integration of nanowires at low cost and low accuracy , provides high-quality crystalline silicon channels.
Smart Images

Figure CN118969600A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for preparing planar ultrafine closely packed grooves and nanowires without high-precision photolithography, and more specifically to a method for preparing planar ultrafine closely packed nanowire arrays (Nanowire Arrays) by using plasma enhanced chemical vapor deposition (PECVD) lamination preparation technology, which is suitable for the field of microelectronics and three-dimensional integration. Background Art
[0002] As a typical one-dimensional nanomaterial, crystalline silicon nanowires have great application value in nanoelectronic devices, optoelectronic devices, quantum electronics, flexible / stretchable electronics and bioelectronics. At present, the growth of nanowires mainly uses the planar solid-liquid-solid (IPSLS) growth mode, which uses hydrogenated amorphous silicon film as a precursor, and metal catalyst nanoparticles absorb amorphous silicon to grow crystalline silicon nanowire structures. At the same time, the IPSLS growth mode can achieve limited regulation of nanowire diameter under a double-sided restricted growth channel.
[0003] However, currently, large-scale, ultra-fine and densely packed nanowire arrays that can be positioned and integrated rely on high-precision lithography technology and high-quality wafer substrates, which are limited by technical barriers and high costs. At the same time, three-dimensional integrated back-end devices lack high-lattice quality wafers.
[0004] The applicant's research group has previously applied for patent CN 114400248 A, a method for accurately guiding the growth of nanowires with highly uniform diameters. The patent also mentions the generation of nanowires by planar closely packed grooves; however, the planar groove morphology of the patent is to define the guiding grooves by photolithography graphics, and the groove width and the distance between the spacer layers are directly limited by the photolithography accuracy and are micrometers wide. In addition, the patent limits the growth of nanowires by confined etching of amorphous silicon.
[0005] How to realize ultra-fine and densely packed crystalline nanowire channels without high-precision lithography and wafer substrate is a technical challenge that our research group needs to solve in the near future. The mastery of this technology has important scientific research and industrialization value. Summary of the invention
[0006] The present application proposes a method for preparing planar ultra-fine and densely packed grooves and growing nanowires without high-precision lithography, which can realize a growth groove array below 15nm under 2-micron precision lithography conditions, and then grow a nanowire array of about 10nm, which is conducive to the realization of low-cost, low-precision nanowire large-scale integrated devices and multi-field applications.
[0007] The present application provides a method for preparing planar ultrafine closely spaced grooves and nanowires without high-precision photolithography, characterized in that it comprises the following steps: 1) using a mask plate lithography technology to define an edge pattern on a substrate, and using a dry etching process to etch the substrate to form a protruding morphology with a vertical sidewall; 2) Using the edge pattern defined in the first step as a substrate, two different dielectric layers are cyclically and alternately deposited on the substrate; the alternating dielectric layers of different thicknesses can be designed and deposited according to the requirements of the nanowire diameter and spacing, and the thickness of the film determines the width and spacing of the grooves; 3) using a CMP process to remove the dielectric layer stacked in a vertical direction on the top of the edge pattern, and exposing the two dielectric layers stacked in a horizontal direction; 4) Treating the surface with a corrosive liquid having different etching rates for the two dielectric layers to form planar closely packed growth grooves; 5) Using the planar close-packed growth groove formed in step 4 as the substrate, the catalytic metal is defined again using the mask plate photolithography technology, and a strip-shaped catalytic metal layer is locally deposited through evaporation or sputtering process; 6) Raising the temperature to above the melting point of the catalytic metal, introducing reducing gas plasma for treatment, so that the catalytic metal layer is transformed into separated metal nanoparticles; 7) Lowering the temperature below the melting point of the catalytic metal particles, depositing an amorphous semiconductor precursor thin film layer on the entire surface of the structure; then raising the temperature to an appropriate temperature so that the nano metal particles melt again, and the front end thereof begins to absorb the amorphous layer, while crystalline nanowires are deposited at the rear end. Under the guidance of the growth grooves, the nanowires grow along the planar closely packed guide channels; 8) The remaining amorphous semiconductor precursor is removed by etching processes such as hydrogen plasma, ICP or RIE to obtain planar densely packed nanowires.
[0008] Preferably, the substrate material in step 1) is crystalline silicon, glass, aluminum foil, silicon nitride, silicon oxide, silicon carbide or sapphire.
[0009] Preferably, the materials of the two different dielectric layers in step 2) are silicon nitride, silicon oxide, aluminum oxide or silicon carbide, and the deposition technology is PECVD or ALD.
[0010] Preferably, the corrosive liquid in step 4) is hydrofluoric acid, hot phosphoric acid, silicon oxide, aluminum oxide, silicon nitride or silicon oxide for silicon nitride and silicon oxide stacking, and hydrochloric acid is used for wet etching.
[0011] Preferably, the catalytic metal in step 5) is one of In, Sn, Bi, Ga or a metal alloy thereof.
[0012] Preferably, the precursor layer in step 7) is amorphous silicon a-Si, amorphous germanium a-Ge, amorphous carbon aC or other amorphous alloy layer, and a heterogeneous stacked layer (such as a-Ge / a-Si) structure thereof.
[0013] The technical solution provided by this application has at least the following technical effects or advantages: 1) The present invention combines the stacked structure and CMP process on the vertical sidewall, and does not require high-precision lithography to produce a planar ultra-fine densely packed groove structure, and prepares a locatable planar ultra-fine densely packed nanowire through a planar solid-liquid-solid (IPSLS) nanowire growth method. At the same time, arraying is achieved through programming guidance technology, that is, as long as the diameter of the nanowire and the thickness of the spacer layer are controlled by depositing different thicknesses of the dielectric layer, the subsequent planar line width can be made below 20nm using 2um lithography, and the required lithography accuracy is lower than the 90nm lithography accuracy required by the SAQP technology. The present invention is expected to break through the key technical bottleneck that has long been unable to prepare planar ultra-fine nanowires on a large scale due to the limitation of lithography technology. It can realize planar ultra-fine nanowire arrays without wafer substrates under low thermal budget and micron-level lithography accuracy, and can provide high-quality crystalline silicon channels for back-end devices and three-dimensional integration.
[0014] 2) The present invention does not require a high-quality crystal lattice wafer as a substrate, which provides a wider range of substrate material choices and can serve three-dimensional integration. In the absence of a wafer substrate, ultra-fine densely packed grooves can be easily prepared. Combined with the IPSLS growth mode, high-quality ultra-fine densely packed crystalline silicon nanowire channels can be provided for application in back-end devices.
[0015] 3) The present invention utilizes IPSLS growth technology and trench confinement to grow an ultrafine silicon nanowire array with a diameter less than 10 nanometers and a spacing less than 10 nm. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 This is a diagram showing the preparation process of planar ultrafine densely packed nanowires provided in Example 1 of the present invention. Figure 1 The guide pattern is defined on the substrate by photolithography, and the vertical sidewall trench is etched by ICP. Figure 1 b PECVD cyclic deposition of two dielectric layers, Figure 1 c CMP process removes the top layer of the pattern and flattens it. Figure 1 d. Corrosive solution wet etching of the growing trench, Figure 1 A strip-shaped catalytic metal layer is deposited at one end of the e-channel. Figure 1 f Hydrogen plasma treatment catalyzes the metal layer to form metal droplets, which cover the amorphous precursor layer, grow nanowires, and then etch the amorphous silicon.
[0017] Figure 2 For Example 1 of the present invention, Figure 1 a structure to Figure 1 b Schematic diagram of the specific process of the structure. Figure 2 The process a→b→c is cycled N times to obtain Figure 2 N-layer stacked structure in d.
[0018] Figure 3 In Example 1 of the present invention Figure 1 d. Figure 1 f Enlarged cross-section diagram, Figure 3 a is a smooth growth groove obtained after selective etching with the corrosive liquid. Figure 3 b is Figure 3 aNanowires are grown through grooves. Figure 3 c is the growth groove obtained when the etching solution has extremely high selectivity. The extremely high selectivity means that the etching solution does not react with one material film or the reaction rate is much lower than that of the other film. Figure 3 d is Figure 3 c Nanowires are grown through grooves.
[0019] Figure 4 This is a flow chart of Example 2 of the present invention for achieving planar ultra-fine and closely packed growth of grooves and nanowires with higher density on the sidewalls of multiple grooves. DETAILED DESCRIPTION
[0020] In order to better understand the above technical solution, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods. Example
[0021] like Figure 1-Figure 3 As shown: This embodiment provides a method for preparing planar ultra-fine dense grooves and nanowires without high-precision photolithography, and the steps are as follows: 1) Using silicon wafers, glass, compounds (such as silicon nitride, silicon oxide, silicon oxynitride) or other metal materials as substrates, using low-precision mask plate lithography technology to define edge patterns on the substrate, and using dry etching processes such as inductively coupled plasma etching (ICP) to anisotropically etch the substrate to form a protruding morphology with a vertical sidewall, such as Figure 1 As shown in a; 2) Using the pattern formed in the first step as the substrate, two different dielectric layers are cyclically deposited on the substrate using the PECVD process. The good conformality of the PECVD process allows the dielectric layers to form alternating dense layers on the vertical sidewalls. Alternating dielectric layers of different thicknesses can be designed and deposited according to the requirements of the nanowire diameter and spacing. The thickness of the film determines the width and spacing of the grooves, such as Figure 1 As shown in b; Figure 2 The process a→b→c is cycled N times to obtain Figure 2 N-layer stacked structure in d; 3) Use CMP process to remove the vertically stacked dielectric layer on the top of the pattern and expose the two dielectric layers that alternate in the horizontal direction, such as Figure 1 As shown in c; 4) Treat the surface with a corrosive liquid having different etching rates for the two dielectric layers, preferably with an etching rate ratio higher than 2, to form planar closely packed growth grooves, such as Figure 1 d- Figure 1 f; if the selected corrosive liquid can react to both dielectric layers, but the etching rate is different, it is easy to obtain a smooth arc-shaped groove morphology, such as Figure 3 In Figure 3 a. Figure 3 b. If the selected corrosive liquid only reacts with one dielectric layer, the etching effect on the other dielectric layer is negligible, and it is easy to obtain a rectangular cross-section groove morphology, such as Figure 3 c. Figure 3 d; Therefore, this technical solution can prepare grooves with different morphologies to meet different needs; 5) Using the planar close-packed growth grooves formed in the previous step as the substrate, the catalytic metal is defined perpendicular to the groove direction using the mask lithography technology again, and a strip-shaped catalytic metal layer is locally deposited by evaporation or sputtering process; 6) In the PECVD vacuum system, the temperature is raised to above the melting point of the catalytic metal, and a reducing gas plasma is introduced for treatment to transform the catalytic metal layer into separated metal nanoparticles; 7) Lower the temperature to below the melting point of the catalytic metal particles, and deposit a thin film layer of amorphous semiconductor precursor on the entire surface of the structure; then raise the temperature to an appropriate temperature so that the nanometal particles melt again, and begin to absorb the amorphous layer at the front end, while crystalline nanowires are deposited at the rear end; due to the guiding effect of the limiting channel, the nanowires will grow along the densely packed guiding channels in the plane; 8) The remaining amorphous semiconductor precursor is removed by etching processes such as hydrogen plasma, ICP or RIE to obtain planar densely packed nanowires.
[0022] This embodiment combines the stacked structure and CMP process on the vertical sidewalls to prepare a planar ultra-fine densely packed groove structure without high-precision lithography, and prepares a positionable planar ultra-fine densely packed nanowire through a planar solid-liquid-solid (IPSLS) nanowire growth method, and realizes arraying through programming guidance technology (as long as the diameter of the nanowire and the thickness of the spacer layer are controlled by depositing dielectric layers of different thicknesses). The present invention is expected to break through the key technical bottleneck of the long-term inability to prepare planar ultra-fine nanowires on a large scale due to the limitations of lithography technology. It can realize planar ultra-fine nanowire arrays on substrates without wafers under low thermal budgets and low lithography precision, and can be used on a large scale in the back end of three-dimensional integration. Example
[0023] like Figure 4 As shown: the preparation method of this embodiment is the same as that of embodiment 1, except that in this embodiment, the substrate is etched to form a protruding morphology with two vertical sidewalls, and two planar closely packed nanowires are prepared at the same time. By analogy, the present invention can also prepare multiple planar closely packed nanowire structures at the same time as needed.
[0024] The method for defining ultra-fine guide grooves provided in Examples 1 and 2 of the present invention is equivalent to using micron-level photolithography combined with PECVD thin film deposition technology, which can obtain nanometer-level groove width and spacing on the plane, replacing high-cost and high-precision photolithography such as DUV and EUV. At the same time, compared with the self-aligned quadruple patterning technology (SAQP), there is no need for multiple cycles of deposition and etching. The technical solution ensures the precise control of the guide groove width and spacing while the process steps are relatively simple and stable. The width of the guide groove and the distance of the spacer layer in the embodiment are determined by the thickness of the deposited film, with an accuracy of several nanometers to tens of nanometers. Even if 2um photolithography is used, the subsequent plane line width can reach less than 20nm. Compared with the prior art, this method has outstanding technical advantages.
[0025] The above description is only a preferred embodiment of the present invention. It should be pointed out that a person skilled in the art can make several improvements without departing from the principle of the present invention, and these improvements should also be regarded as within the protection scope of the present invention.
Claims
1. A method for preparing planar ultra-fine closely spaced grooves and nanowires without high-precision photolithography. It is characterized in that The steps include: 1) defining an edge pattern on a substrate using a mask lithography technique, and etching the substrate using a dry etching process to form a protruding morphology with a vertical sidewall; 2) using the edge pattern defined in the first step as a substrate, cyclically and alternately depositing two different dielectric layers on the substrate; 3) using a CMP process to remove the dielectric layer stacked in a vertical direction on the top of the edge pattern, and exposing the two dielectric layers stacked in a horizontal direction; 4) Treating the surface with a corrosive liquid having different etching rates for the two dielectric layers to form planar closely packed growth grooves; 5) Using the planar close-packed growth groove formed in step 4 as the substrate, the catalytic metal is defined again using the mask plate photolithography technology, and a strip-shaped catalytic metal layer is locally deposited through evaporation or sputtering process; 6) Raising the temperature to above the melting point of the catalytic metal, introducing reducing gas plasma for treatment, so that the catalytic metal layer is transformed into separated metal nanoparticles; 7) Lowering the temperature below the melting point of the catalytic metal particles, depositing an amorphous semiconductor precursor thin film layer on the entire surface of the structure; then raising the temperature to an appropriate temperature so that the nano metal particles melt again, and the front end thereof begins to absorb the amorphous layer, while crystalline nanowires are deposited at the rear end. Under the guidance of the growth grooves, the nanowires grow along the planar closely packed guide channels; 8) The remaining amorphous semiconductor precursor is removed by etching processes such as hydrogen plasma, ICP or RIE to obtain planar densely packed nanowires.
2. The method for preparing planar ultrafine closely spaced grooves and nanowires without high-precision photolithography according to claim 1, Features: The substrate material in step 1) is crystalline silicon, glass, aluminum foil, silicon nitride, silicon oxide, silicon carbide or sapphire.
3. The method for preparing planar ultrafine closely spaced grooves and nanowires without high-precision photolithography according to claim 1, Features: In the step 2), the materials of the two different dielectric layers are silicon nitride, silicon oxide, aluminum oxide or silicon carbide, and the deposition technology is PECVD or ALD.
4. The method for preparing planar ultrafine closely spaced grooves and nanowires without high-precision photolithography according to claim 1, Features: The corrosive liquid in step 4) is hydrofluoric acid, hot phosphoric acid, silicon oxide, aluminum oxide, silicon nitride or silicon oxide for silicon nitride and silicon oxide for silicon oxide stacking, and hydrochloric acid is used for wet etching.
5. The method for preparing planar ultrafine closely spaced grooves and nanowires without high-precision photolithography according to claim 1, It is characterized in that The catalytic metal in step 5) is one of In, Sn, Bi, Ga or a metal alloy thereof.
6. The method for preparing planar ultrafine closely spaced grooves and nanowires without high-precision photolithography according to claim 1, It is characterized in that In the step 7), the precursor layer is one of amorphous silicon a-Si, amorphous germanium a-Ge, amorphous carbon a-C, or a heterogeneous stacked structure thereof.
Citation Information
Patent Citations
Method for guiding and growing three-dimensional slope nanowire array by using heterogeneous alternating lamination step
CN108217591A
Method of preparing three-dimensional super-stretchable crystalline nanowire
CN110767537A
Planar superlattice nanowire field effect transistor and preparation method thereof
CN113130325A
Preparation method of anti-crosstalk self-limiting superfine densely-arranged crystalline silicon nanowire
CN113968571A
Cited By
Universal preparation method and device for metal micro-nano structure
CN121571660A
A general method and device for preparing metal micro-nano structures
CN121571660B