Method for forming component and plasma processing apparatus

By using laser scanning technology to irradiate the powders of different ceramic materials in the plasma processing device, the problem of long production cycles of complex structural components is solved, and the effect of high functionalization and shortening of time is achieved.

CN118969705APending Publication Date: 2024-11-15TOKYO ELECTRON LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411021692.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2018-05-15
Filing Date
2019-05-10
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

In plasma processing devices, the production cycle of components of complex structures is long, resulting in a long manufacturing process step and time-consuming.

Method used

A method is adopted to use powders of different ceramic materials in the plasma treatment device to irradiate energy beams through laser scanning technology to form components with complex structures, reduce the use of adhesives, and improve the bonding strength and heat conductivity of the material.

Benefits of technology

The manufacturing time of components is shortened, the thermal conductivity and bonding strength of the material are improved, the number of process steps is reduced, and the production of highly functional parts is achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118969705A_ABST
    Figure CN118969705A_ABST
Patent Text Reader

Abstract

The present invention provides a method for forming a component and a plasma processing apparatus, the method including a step of supplying a raw material of a first ceramic and a raw material of a second ceramic different from the first ceramic while irradiating the raw material of the first ceramic and the raw material of the second ceramic with an energy beam.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] (This application is a divisional application of application No. 201980004518.3 filed on May 10, 2019.) Technical Field

[0002] The present invention relates to a component forming method and a plasma processing device. Background Art

[0003] In recent years, components provided in plasma processing apparatuses have become more complex in structure in order to achieve higher functionality, and are sometimes manufactured by bonding or joining different materials (for example, see Patent Document 1).

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Publication No. 2018-46185 Summary of the invention

[0007] Technical problem to be solved by the invention

[0008] In the production of the above-mentioned parts, there are complex structures such as hollow structures, which require long production and development cycles, so the lead time for producing the parts increases, which has become a technical problem. It is required to reduce the number of steps in the manufacturing process of the parts and shorten the lead time.

[0009] With respect to the above technical problem, an object thereof is, in one aspect, to shorten the time taken to manufacture components.

[0010] Methods used to solve technical problems

[0011] In order to solve the above-mentioned technical problem, according to one embodiment, a method for forming a component used in a plasma processing device is provided, wherein the method for forming the component includes a process of supplying a raw material of a first ceramic and a raw material of a second ceramic different from the first ceramic, and irradiating the raw material of the first ceramic and the raw material of the second ceramic with an energy beam.

[0012] Effects of the Invention

[0013] According to one aspect of the present invention, the time required to manufacture components can be shortened. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a diagram showing an example of a plasma processing apparatus according to an embodiment.

[0015] Figure 2 yes Figure 1 An enlarged view of a portion of a mounting table of a plasma processing apparatus is shown.

[0016] Figure 3 This is a diagram showing an example of the structure of a 3D printer according to one embodiment.

[0017] Figure 4 This is a flowchart showing an example of a component forming process according to one embodiment.

[0018] Figure 5 It is a diagram for explaining a method of forming a component according to one embodiment. DETAILED DESCRIPTION

[0019] Hereinafter, the mode for implementing the present invention will be described with reference to the accompanying drawings. In addition, in this specification and the accompanying drawings, the same reference numerals are attached to substantially the same structure, and repeated description is omitted.

[0020] (Plasma processing device)

[0021] Figure 1 The plasma processing device 100 shown is an example of a capacitive coupling type plasma processing device. The plasma processing device 100 includes a processing container 112 and a mounting table 116. The processing container 112 has a substantially cylindrical shape, and its internal space becomes a processing chamber 112c. The processing container 112 is made of aluminum, for example. A ceramic coating having plasma resistance such as an acid-resistant aluminum film and / or an yttrium oxide film is formed on the surface of the internal space side of the processing container 112. The processing container 112 is grounded. An opening 112p for conveying a wafer W into or out of the processing chamber 112c is formed on the side wall of the processing container 112. The opening 112p can be opened and closed by a gate valve GV.

[0022] The mounting table 116 is configured to support the wafer W in the processing chamber 112c. The mounting table 116 has the functions of adsorbing the wafer W, adjusting the temperature of the wafer W, and transmitting high frequency to the susceptor 117 below the electrostatic chuck. The details of the mounting table 116 will be described later.

[0023] The plasma processing apparatus 100 includes an upper electrode 130. The upper electrode 130 is disposed in the upper opening of the processing container 112 and is disposed substantially parallel to the mounting table 116 functioning as the lower electrode. An insulating support component 132 is provided between the upper electrode 130 and the processing container 112.

[0024] The upper electrode 130 includes a top plate 134 and a support 136. The top plate 134 has a substantially disk shape. The top plate 134 may be conductive. The top plate 134 is formed of, for example, silicon or aluminum, and a plasma-resistant ceramic film is formed on its surface. A plurality of gas release holes 134a are formed in the top plate 134. The gas release holes 134a extend in a substantially vertical direction.

[0025] The support body 136 supports the top plate 134 in a detachable manner. The support body 136 is formed of, for example, aluminum. A gas diffusion chamber 136a is formed in the support body 136. A plurality of holes 136b extending from the gas diffusion chamber 136a are connected to the plurality of gas release holes 134a. The gas diffusion chamber 136a is connected to the pipe 138 via the port 136c. The pipe 138 is connected to the gas supply unit 139.

[0026] The plasma processing apparatus 100 includes an exhaust device 150 . The exhaust device 150 includes one or more pumps such as a turbomolecular pump and a dry pump, and a pressure regulating valve. The exhaust device 150 is connected to an exhaust port formed in the processing container 112 .

[0027] The plasma processing apparatus 100 includes a first control unit 151. A control program and recipe data for controlling various processes executed in the plasma processing apparatus 100 by a processor are stored in the storage unit of the first control unit 151. For example, a control program and recipe data for executing a plasma process such as an etching process in the plasma processing apparatus 100 are stored in the storage unit of the first control unit 151.

[0028] Below, refer to Figure 1 and Figure 2 , the mounting table 116 and the components of the plasma processing apparatus 100 attached to the mounting table 116 are described in detail. Figure 2 Yes Figure 1 The illustrated cross-sectional view is an enlarged view of a portion of the mounting table 116 of the plasma processing apparatus 100 .

[0029] The mounting table 116 includes a susceptor 117 and an electrostatic chuck 120. The susceptor 117 is formed of, for example, aluminum alloy (Al), titanium (Ti), silicon carbide (SiC), etc. The susceptor 117 is supported by a support part 114 extending upward from the bottom of the processing container 112. The support part 114 is an insulating part, for example, formed of oxidized aluminum (aluminum oxide). In addition, the support part 114 has a substantially cylindrical shape.

[0030] The base 117 is formed of a conductive metal such as aluminum. The base 117 has a substantially disk shape. The base 117 has a central portion 117a and a peripheral portion 117b. The central portion 117a has a substantially disk shape. The central portion 117a provides a first upper surface 117c of the base 117. The first upper surface 117c is a substantially circular surface.

[0031] The peripheral portion 117b is continuous with the central portion 117a and extends in the radial direction (relative to the axis Z extending in the vertical direction (refer to Figure 1 ) is located outside the central portion 117a in the radial direction and extends in the circumferential direction (in the circumferential direction relative to the axis Z). In one embodiment, the peripheral portion 117b and the central portion 117a together provide the lower surface 117d of the base 117. In addition, the peripheral portion 117b provides a second upper surface 117e. The second upper surface 117e is a strip-shaped surface that is located outside the first upper surface 117c in the radial direction and extends in the circumferential direction. In addition, the second upper surface 117e is located closer to the lower surface 117d than the first upper surface 117c in the vertical direction.

[0032] The base 117 is connected to a power supply 119. The power supply 119 is, for example, a power supply rod, and is connected to the lower surface 117d of the base 117. The power supply 119 is made of aluminum or an aluminum alloy. The power supply 119 is connected to the first high-frequency power supply 62 via the matching device 66. In addition, the power supply 119 is connected to the second high-frequency power supply 64 via the matching device 68.

[0033] A flow path 117f for a coolant (refrigerant) is formed in the base 117. The flow path 117f extends in the base 117 in a spiral shape, for example. A medium (coolant, heat medium) for temperature adjustment is supplied to the flow path 117f from a cooling unit. In one embodiment, a coolant, which is an example of the medium supplied to the flow path 117f, is a coolant that absorbs heat by evaporation to perform cooling. The coolant may be, for example, a hydrofluorocarbon-based coolant.

[0034] The electrostatic chuck 120 has an adsorption portion 123. The adsorption portion 123 is provided on a susceptor 121 on the susceptor 117. The susceptor 121 constitutes a lower electrode and is provided on the susceptor 117. The susceptor 121 has conductivity. The susceptor 121 may be made of ceramics that impart conductivity to aluminum nitride or silicon carbide, or may be made of metal (e.g., titanium).

[0035] The base 121 has a substantially disk shape. The base 121 has a central portion 121a and a peripheral portion 121b. The central portion 121a is substantially disk-shaped. The central portion 121a provides a first upper surface 121c of the base 121. The first upper surface 121c is a substantially circular surface.

[0036] The peripheral portion 121b is continuous with the central portion 121a, and extends in the circumferential direction on the outer side of the central portion 121a in the radial direction. In one embodiment, the peripheral portion 121b and the central portion 121a provide the lower surface 121d of the base 121. In addition, the peripheral portion 121b provides the second upper surface 121e. The second upper surface 121e is a strip-shaped surface, and extends in the circumferential direction on the outer side of the first upper surface 121c in the radial direction. In addition, the second upper surface 121e is located closer to the lower surface 121d than the first upper surface 121c in the vertical direction.

[0037] A boundary layer 129 is formed between the adsorption portion 123 and the base 121. The adsorption portion 123 has a substantially disk shape and is formed of ceramic. The ceramic constituting the adsorption portion 123 may have a thermal conductivity of 1×10 15 Ceramic with a volume resistivity of Ω·cm or more. As such ceramic, for example, alumina can be used.

[0038] The electrostatic chuck 120 includes a plurality of concentric regions RN relative to the axis Z, i.e., the central axis of the electrostatic chuck 120. In one embodiment, the electrostatic chuck 120 includes a first region R1, a second region R2, and a third region R3. The first region R1 intersects the axis Z, the third region R3 is a region including the edge of the electrostatic chuck 120, and the second region R2 is between the first region R1 and the third region R3. In one example, the first region R1 is a region from the center of the electrostatic chuck 120 to a radius of 120 mm, the second region R2 is a region from a radius of 120 mm to a radius of 135 mm in the electrostatic chuck 120, and the third region R3 is a region from a radius of 135 mm to a radius of 150 mm in the electrostatic chuck 120. In addition, the number of regions of the electrostatic chuck 120 may be any number greater than one.

[0039] The adsorption part 123 of the electrostatic chuck 120 has an electrode film 125 built therein. The electrode film 125 is electrically connected to a DC power source. When a DC voltage from the DC power source is applied to the electrode film 125, the adsorption part 123 generates an electrostatic force such as a Coulomb force, and the wafer W is held by the electrostatic force.

[0040] The adsorption portion 123 further has a plurality of built-in heaters HN. The plurality of heaters HN are respectively disposed in the plurality of regions RN of the electrostatic chuck. In one embodiment, the plurality of heaters HN include a first heater 156, a second heater 157, and a third heater 158. The first heater 156 is disposed in the first region R1, the second heater 157 is disposed in the second region R2, and the third heater 158 is disposed in the third region R3. The plurality of heaters HN are connected to a heater power supply.

[0041] A plurality of first elastic parts EM1 are provided between the base 121 and the base 117. The plurality of first elastic parts EM1 separate the electrostatic chuck 120 and the base 117 at an interval above. Each of the plurality of first elastic parts EM1 is an O-ring. The plurality of first elastic parts EM1 have different diameters from each other and are arranged concentrically with respect to the axis Z. In addition, the plurality of first elastic parts EM1 are provided below the boundary of adjacent regions of the electrostatic chuck 120 and the edge of the electrostatic chuck 120. In one embodiment, the plurality of first elastic parts EM1 include an elastic part 165, an elastic part 167, and an elastic part 169. The elastic part 165 is provided below the boundary between the first region R1 and the second region R2, the elastic part 167 is provided below the boundary between the second region R2 and the third region R3, and the elastic part 169 is provided below the edge of the electrostatic chuck 120.

[0042] The plurality of first elastic parts EM1 are partially arranged in the groove provided by the first upper surface 117c of the base 117, and are in contact with the first upper surface 117c and the lower surface 121d of the base 121. The plurality of first elastic parts EM1, together with the base 117 and the base 121, define a plurality of heat transfer spaces DSN between the first upper surface 117c of the base 117 and the lower surface 121d of the base 121. The plurality of heat transfer spaces DSN extend below each of the plurality of regions RN of the electrostatic chuck 120 and are separated from each other. In one embodiment, the plurality of heat transfer spaces DSN include a first heat transfer space DS1, a second heat transfer space DS2, and a third heat transfer space DS3. The first heat transfer space DS1 is located inside the elastic part 165, the second heat transfer space DS2 is located between the elastic part 165 and the elastic part 167, and the third heat transfer space DS3 is located between the elastic part 167 and the elastic part 169. As described later, a heat transfer gas (for example, He gas) is supplied to the plurality of heat transfer spaces DSN. In addition, the length in the vertical direction of each of the plurality of heat transfer spaces DSN is set to a length of, for example, 0.1 mm to 2.0 mm.

[0043] The plurality of first elastic parts EM1 are configured to have a thermal resistance higher than the thermal resistance of each of the plurality of heat transfer spaces DSN to which He gas is supplied. The thermal resistance of the plurality of heat transfer spaces DSN depends on the thermal conductivity of the heat transfer gas, the length in the vertical direction, and the area thereof. In addition, the thermal resistance of each of the plurality of first elastic parts EM1 depends on its thermal conductivity, its thickness in the vertical direction, and its area. Therefore, the material, thickness, and area of ​​each of the plurality of first elastic parts EM1 are determined according to the thermal resistance of each of the plurality of heat transfer spaces DSN. In addition, low thermal conductivity and high heat resistance can be required for the plurality of first elastic parts EM1. Therefore, the plurality of first elastic parts EM1 can be formed of, for example, perfluororubber.

[0044] The mounting table 116 has a fixing part 171. The fixing part 171 is formed of metal and is configured to be able to clamp the base 121 and the plurality of first elastic parts EM1 between the fixing part 171 and the base 117. The fixing part 171 is formed of a material having a low thermal conductivity, such as titanium, in order to suppress heat conduction between the base 121 and the base 117 via the fixing part 171.

[0045] In one embodiment, the fastening component 171 includes a cylindrical portion 171a and an annular portion 171b. The cylindrical portion 171a has a substantially cylindrical shape, and a first lower surface 171c is provided at its lower end. The first lower surface 171c is a strip-shaped surface extending in the circumferential direction.

[0046] The annular portion 171b has a substantially annular plate shape, is continuous with the inner source of the upper portion of the cylindrical portion 171a, and extends radially inward from the cylindrical portion 171a. The annular portion 171b provides a second lower surface 171d. The second lower surface 171d is a band-shaped surface extending in the circumferential direction.

[0047] The fixing part 171 is arranged so that the first lower surface 171c contacts the second upper surface 117e of the base 117, and the second lower surface 171d contacts the second upper surface 121e of the base 121. In addition, the fixing part 171 is fixed to the peripheral edge portion 117b of the base 117 by the bolt 173. By adjusting the screwing of the bolt 173 with respect to the fixing part 171, the amount of compression of the plurality of first elastic parts EM1 can be adjusted. Thus, the lengths of the plurality of heat transfer spaces DSN in the vertical direction can be adjusted.

[0048] In one embodiment, a second elastic part 175 is provided between the lower surface of the inner edge of the annular part 171b of the fixing part 171 and the second upper surface 121e of the base 121. The second elastic part 175 is an O-ring, and suppresses particles (for example, metal powder) that may be generated by friction between the second lower surface 171d of the fixing part 171 and the second upper surface 121e of the base 121 from moving to the adsorption part 123 side.

[0049] In addition, the second elastic part 175 generates a reaction force smaller than the reaction force generated by the plurality of first elastic parts EM1. In other words, the plurality of first elastic parts EM1 are configured so that the reaction force generated by the plurality of first elastic parts EM1 is larger than the reaction force generated by the second elastic part 175. Furthermore, the second elastic part 175 can be formed of perfluororubber, which is a material having high heat resistance and low thermal conductivity.

[0050] A heater 176 is provided on the fixing part 171. The heater 176 extends in the circumferential direction and is connected to a heater power source via a filter. The filter is provided to prevent high frequency from invading the heater power source.

[0051] The heater 176 is provided between the first film 180 and the second film 182. The first film 180 is provided on the fixing part 171 side relative to the second film 182. The first film 180 has a thermal conductivity lower than that of the second film 182. For example, the first film 180 may be a thermal spray film made of zirconium oxide, and the second film 182 may be a thermal spray film made of yttria. In addition, the heater 176 may be a thermal spray film made of tungsten.

[0052] An edge ring FR is provided on the second film 182. The edge ring FR is formed of, for example, Si. The edge ring FR is heated by the heat from the heater 176. In addition, most of the heat flux from the heater 176 does not go to the first film 180 but goes to the second film 182, and then goes to the edge ring FR via the second film 182. Therefore, the edge ring FR can be efficiently heated.

[0053] The base 117 of the mounting table 116, the fixing member 171, and the like are covered on their outer circumferences with one or more insulating members 186. The one or more insulating members 186 are formed of, for example, alumina or quartz.

[0054] As described above, in the mounting table 116, the base 117 and the base 121 are separated from each other by a plurality of first elastic parts EM1. In addition, in the mounting table 116, the base 121 and the adsorption part 123 are bonded without using an adhesive. Therefore, the temperature of the electrostatic chuck 120 can be set to a high temperature. In addition, the heat transfer gas supplied to the plurality of heat transfer spaces DSN can be used to perform heat exchange between the electrostatic chuck 120 and the base 117, so the temperature of the electrostatic chuck 120 can also be set to a low temperature. In addition, in the mounting table 116, the high-frequency power supply path to the base 121 of the electrostatic chuck 120 is ensured by the power supply body 119, the base 117 and the fixing part 171. In addition, the power supply body 119 is not directly connected to the base 121 of the electrostatic chuck 120, but is connected to the base 117, so aluminum or an aluminum alloy can be used as the constituent material of the power supply body 119. Therefore, even when a high frequency of 13.56 MHz or higher is used, the loss of the high frequency in the power supply body 119 can be suppressed.

[0055] In addition, as described above, in one embodiment, the second elastic member 175 is provided between the lower surface of the inner edge portion of the annular portion 171b of the fixing member 171 and the second upper surface 121e of the base 121. Since the second upper surface 121e of the peripheral portion 121b of the base 121 and the second lower surface 171d of the fixing member 171 are in contact with each other, friction occurs at their contact portion, and particles (for example, metal powder) may be generated. Even if such particles are generated, the second elastic member 175 can prevent the particles from being attached to the adsorption portion 123 and the wafer W placed on the adsorption portion 123.

[0056] Furthermore, the plurality of first elastic parts EM1 are configured so that the reaction force generated by the plurality of first elastic parts EM1 is greater than the reaction force generated by the second elastic part 175. Thus, the electrostatic chuck 120 and the susceptor 117 can be securely spaced apart.

[0057] In one embodiment, the plurality of first elastic parts EM1 are configured to have a higher thermal resistance than the thermal resistance of the plurality of heat transfer spaces DSN when He gas is supplied to the plurality of heat transfer spaces DSN. In addition, the plurality of first elastic parts EM1 are formed of, for example, perfluororubber. By using the plurality of first elastic parts EM1, heat conduction through the plurality of heat transfer spaces DSN is superior to heat conduction through the plurality of first elastic parts EM1 between the electrostatic chuck 120 and the base 117. Therefore, the temperature distribution of the electrostatic chuck 120 can be made uniform.

[0058] In one embodiment, the gas passage for heat transfer gas supplied between the wafer W and the adsorption unit 123 is formed without using an adhesive. In addition, the surface of the susceptor 121 that defines the storage space is covered with a coating, and an insulating elastic member is provided between the coating and the susceptor 117 to close the storage space, wherein a sleeve that constitutes a part of the gas passage is arranged in the storage space. Thus, it is possible to suppress the intrusion of plasma between the susceptor 121 and the susceptor 117 and the insulation breakdown of the susceptor 121 that follows.

[0059] Furthermore, according to the plasma processing apparatus 100 having the mounting table 116 described above, it is possible to perform plasma processing on the wafer W in a wide temperature range from low temperature to high temperature.

[0060] (3D printer configuration)

[0061] Below, refer to Figure 3 , an example of the structure of the 3D printer 200 is described. Figure 3 An example of the structure of a 3D printer 200 according to one embodiment is shown. The 3D printer 200 according to this embodiment is an example of a device for forming (manufacturing) a component used in a plasma processing device. However, the device for forming a component is not limited to Figure 3 The structure of the 3D printer 200 is shown.

[0062] In addition, in this embodiment, as an example of a component formed by the 3D printer 200, the mounting table 116 that functions as a lower electrode with a complex structure is cited for description. However, the component formed by the 3D printer 200 is not limited to this, and for example, it may be the upper electrode 130, or a component made of different materials or a component in which different materials that cannot be bonded are fixed together with bolts. In addition, any component may be used as long as it is a component disposed in the plasma processing apparatus 100.

[0063] The 3D printer 200 can form a three-dimensional object in the chamber 210. The 3D printer 200 of this embodiment stores three-dimensional data of the mounting table 116 for forming the three-dimensional object in a storage unit such as the RAM 256, and manufactures the mounting table 116 based on the three-dimensional data. The mounting table 116 is formed on the mounting surface of the processing table 202 of the platform. The processing table 202 can be raised and lowered, for example, gradually lowered, as the formation of the mounting table 116 progresses.

[0064] In this embodiment, the raw material storage unit 203 of the platform stores powder of the raw material for forming the mounting table 116. The raw material may be the same as the material of each component constituting the mounting table 116. For example, among the components constituting the mounting table 116, when the bases 117 and 121 are formed of an aluminum alloy and the electrostatic chuck 120 is formed of SiC, the powder of the aluminum alloy and the powder of SiC are stored separately in the raw material storage unit 203.

[0065] However, the material of the pedestals 117 and 121 is not limited to aluminum alloys, but may be ceramics such as SiC. In addition, the material of the electrostatic chuck 120 is not limited to SiC, but may be ceramics such as alumina. In the case where the pedestals 117 and 121 are formed of SiC and the electrostatic chuck 120 is formed of alumina, the powder of SiC and the powder of alumina are stored separately in the raw material storage unit 203. In addition, the raw materials of the materials constituting the pedestal 117, the pedestal 121, and the electrostatic chuck 120 are not limited to powdered form, but may be in the form of lines. In addition, in the present embodiment, the pedestal 117 and the electrostatic chuck 120 are formed of different materials.

[0066] The raw material powder is irradiated with an energy beam to melt the raw material powder while being supplied into the chamber 210. In the present embodiment, laser light A (optical laser) can be used as the irradiated energy beam.

[0067] Laser light A is output from the light source 206 and irradiated to a predetermined position determined by the laser scanning device 204 that performs two-dimensional scanning. The light source 206 and the laser scanning device 204 are preferably arranged outside the chamber 210. The laser scanning device 204 is driven by the laser driving unit 208 by the second control unit 250 to move to the predetermined position.

[0068] The laser scanning device 204 scans the laser A at least in the two-dimensional (XY) direction on the processing table 202. For example, the laser scanning device 204 is controlled to move the irradiation spot of the laser A on the processing table 202 based on the three-dimensional data representing the three-dimensional structure of the mounting table 116. Specifically, under the control of the second control unit 250, the laser scanning device 204 scans in the two-dimensional (XY) direction according to the progress of the formation of the parts such as the base 117, 121 and the electrostatic chuck 120 constituting the mounting table 116.

[0069] Second control unit 250 controls roller driving unit 207 to drive roller 205 , thereby supplying aluminum alloy powder, which is a material of susceptor 117 , and / or SiC powder, which is a material of electrostatic chuck 120 , to laser scanning space 209 .

[0070] In addition, it is preferable that the temperature of the raw material storage unit 203 is adjusted by a heating device. In addition, it is preferable that a mechanism capable of supplying an inert gas and exhausting the inside of the chamber 210 is provided in the chamber 210 .

[0071] The laser A scanned in two dimensions by the laser scanning device 204 is irradiated to the irradiation area on the processing table 202 through the top of the chamber 210, for example, the laser transmission window 211 provided just above the center of the processing table 202. The laser A heats the aluminum alloy powder and / or SiC powder on the processing table 202 (see Figure 3 B), the powder is melted and solidified to form the mounting table 116. In this way, the base 117 and the electrostatic chuck 120 are three-dimensionally formed in sequence, and the manufacturing of the mounting table 116 is completed.

[0072] The second control unit 250 includes a CPU 252, a ROM 254, and a RAM 256. The second control unit 250 controls the supply of the raw material powder from the raw material storage unit 203 and the lifting and lowering of the processing table 202. In addition, the second control unit 250 controls the lighting of the light source 206, the scanning of the laser scanning device 204, and the roller driving unit 207 and the laser driving unit 208. Thus, the second control unit 250 controls the operation of the manufacturing stage 116.

[0073] The control program executed by the CPU 252 is stored in, for example, the ROM 254. The CPU 252 executes the control program based on, for example, the three-dimensional data stored in the RAM 256, thereby controlling the manufacturing of the mounting table 116. In addition, the control program may be stored in a fixed storage medium, or in a removable computer-readable storage medium such as various flash memories or optical (magnetic) disks.

[0074] In addition, the second control unit 250 has a display 258 and an input device 260 such as a keyboard or a pointing device. The display 258 is used to display the progress of the production of the mounting table 116. The input device 260 is used to input instructions to start or stop the production of the mounting table 116 or control parameters when setting.

[0075] The three-dimensional data is data for making the stage 116, and is stored in a storage unit such as the RAM 256. The three-dimensional data includes data on the three-dimensional structure of the susceptor 117, the hollow structure such as the flow path 117f in the susceptor 117, the susceptor 121 and the electrostatic chuck 120, and various parts constituting the stage 116. In addition, the three-dimensional data includes data on the three-dimensional structure of the electrostatic chuck 120, the heater HN and the electrode film 125 embedded in the electrostatic chuck 120. In addition, the three-dimensional data includes data on the boundary layer 129 formed between the susceptors 117, 121 and the electrostatic chuck 120.

[0076] (3D printer operation)

[0077] Next, an example of the operation of the 3D printer 200 will be described with reference to Figure 4 and Figure 5 While explaining. Figure 4 This is a flowchart showing an example of a forming process of a component using the 3D printer 200 according to one embodiment. Figure 5 It is a diagram for explaining a method of forming a component according to one embodiment.

[0078] When the present process starts, the second control unit 250 acquires the three-dimensional data stored in the RAM 256 (step S10). Based on the three-dimensional data, the second control unit 250 supplies the powder of the aluminum alloy to the laser scanning space 209 while irradiating the powder with laser (step S12). At this time, the second control unit 250 controls the roller driving unit 207 to move the roller 205 to supply the powder of the aluminum alloy to the laser scanning space 209. Moreover, the second control unit 250 controls the laser driving unit 208 to move the laser scanning device 204 to a specified position, irradiates the laser to the powder of the aluminum alloy, and melts and solidifies the powder of the aluminum alloy. Then, the second control unit 250 repeatedly performs the action of using the roller 205 to supply the powder of the aluminum alloy and using the laser to melt and solidify it. Thus, the second control unit 250 completes the formation of the bases 117 and 121 (step S14).

[0079] Figure 5(1) shows a part of the process of forming the base 117, 121. This process is an example of the first process, which forms the base by supplying an example of a metal raw material, that is, aluminum alloy powder, while irradiating the powder with laser. Thus, the hollow structure of the flow path 117f inside the base 117 can be precisely formed based on the three-dimensional data.

[0080] return Figure 4 Then, the second control unit 250 supplies the aluminum alloy powder and the SiC powder to the laser scanning space 209 while changing the ratio (step S16). At this time, the second control unit 250 supplies the aluminum alloy powder in a manner that gradually decreases the ratio from 100% and continuously changes to 0% based on the three-dimensional data. In addition, the second control unit 250 supplies the SiC powder in a manner that gradually increases the ratio from 0% and continuously changes to 100% based on the three-dimensional data.

[0081] As a result, the ratio of the aluminum alloy powder and the SiC powder supplied to the laser scanning space 209 changes from a state where the aluminum alloy is more than the SiC powder to a state where the SiC is more than the aluminum alloy. The second control unit 250 repeatedly performs the following operations: using the roller 205 to supply the aluminum alloy powder and the SiC powder in a predetermined ratio to the laser scanning space 209, and irradiating the aluminum alloy powder and the SiC powder with laser light to melt and solidify them. As a result, the second control unit 250 completes the formation of the boundary layer 129 (step S18).

[0082] Figure 5 (2) shows an example of a process for forming the boundary layer 129. This process is an example of the second process, in which a powder prepared by configuring a powder of an aluminum alloy, an example of a metal raw material, and a powder of SiC, an example of a ceramic raw material, in a predetermined ratio is supplied to the susceptor 121 and the powder is irradiated with a laser to form a boundary layer on the susceptor.

[0083] return Figure 4 Next, the second control unit 250 supplies SiC powder to the laser scanning space 209 while irradiating the powder with laser (step S20). The second control unit 250 repeatedly performs the operation of supplying SiC powder using the roller 205 and melting and solidifying it with laser. As a result, the ceramic layer forming the adsorption portion 123 of the electrostatic chuck 120 is formed below the heating layer (step S22).

[0084] Figure 5 (3) is an example of a ceramic layer forming step. This step is an example of a third step, in which a ceramic layer (adsorption portion 123 ) is formed on the boundary layer 129 by supplying SiC powder, an example of a ceramic raw material, while irradiating the powder with laser light.

[0085] return Figure 4 Next, the second control unit 250 supplies the powder of the raw material of the heater to the laser scanning space 209 while irradiating the powder with laser (step S24). The second control unit 250 supplies the powder of the raw material of the heater HN using the roller 205 and melts and solidifies it with laser to form a heating layer in the adsorption unit 123.

[0086] Figure 5 (4) shows an example of a step of forming the heater HN. This step is an example of the fourth step, in which the heater HN is formed by irradiating the raw material of the heater HN with an energy beam while supplying the raw material of the heater HN.

[0087] return Figure 4 Next, the second control unit 250 supplies SiC powder to the laser scanning space 209 while irradiating the powder with laser (step S26). The second control unit 250 repeatedly supplies SiC powder using the roller 205 and melts and solidifies it using laser. Thus, the ceramic layer of the adsorption unit 123 is formed to below the electrode film (step S28).

[0088] Next, the second control unit 250 supplies the powder of the electrode film raw material to the laser scanning space 209 while irradiating the powder with laser (step S30). The second control unit 250 supplies the powder of the electrode film raw material using the roller 205 and melts and solidifies it with laser to form an electrode layer in the electrostatic chuck 120.

[0089] Figure 5 (5) shows an example of a step of forming an electrode layer (electrode film 125). This step is an example of a fifth step, in which the electrode film 125 is formed by irradiating the raw material of the electrode film 125 with laser light while supplying the raw material of the electrode film 125.

[0090] return Figure 4 Next, the second control unit 250 supplies SiC powder to the laser scanning space 209 while irradiating the powder with laser (step S32). The second control unit 250 repeatedly performs the operation of supplying SiC powder using the roller 205 and melting and solidifying it with laser. Thus, the remaining ceramic layer of the adsorption unit 123 is formed (step S34), and the present process ends. Thus, Figure 5 The formation of the adsorption portion 123 of the electrostatic chuck 120 shown in (6) is completed, and the manufacturing of the mounting table 116 is completed.

[0091] According to the above-mentioned component forming method, a boundary layer 129 formed by changing the material ratio of each part of the base 121 and the adsorption part 123 is provided between the base 121 and the adsorption part 123. At this time, the boundary layer 129 formed by mixing the materials of the base 121 and the adsorption part 123 of different materials in a predetermined ratio can be formed into a smooth and gradual shape. As a result, the adhesive layer of the mounting table 116 can be eliminated. As a result, the thermal conductivity between the different materials of the mounting table 116 can be increased, and the thermal characteristics can be improved.

[0092] Regarding the ratio of each material of the boundary layer 129, the closer to the base 121, the higher the ratio of the aluminum alloy as the material of the base 121 than the ratio of SiC as the material of the adsorption portion 123. Conversely, the closer to the adsorption portion 123, the higher the ratio of SiC as the material of the adsorption portion 123 than the ratio of the aluminum alloy as the material of the base 121.

[0093] Thus, the boundary layer 129 is formed by melting, solidifying, and laminating materials in which the ratio of aluminum alloy and SiC changes gradually. The formation of the boundary layer 129 in which the ratio of different materials changes gradually and is laminated is called "inclined lamination".

[0094] In the step of forming the boundary layer 129, by stacking the boundary layer 129 between the base 121 and the adsorption unit 123 at an angle, the thermal conductivity between the different materials of the mounting table 116 can be improved compared to the case where the inclined stacking is not performed. In addition, in the step of forming the boundary layer 129, the number of manufacturing steps can be reduced by removing the adhesive layer that bonds the base 121 and the adsorption unit 123, and the time required for manufacturing can be shortened.

[0095] Then, by arranging the flow path structure, the wiring structure, etc. in three dimensions, it is possible to realize a high-level functionality of the mounting table 116 .

[0096] In addition, in the 3D printer 200, each process may be performed in the order of the first process → the second process → the third process, or in the order of the third process → the second process → the first process. Thus, the upper electrode 130 that functions as an upper electrode can be manufactured by the 3D printer 200, similarly to the mounting table 116 that functions as a lower electrode.

[0097] (Changes in the boundary layer)

[0098] The boundary layer 129 is not limited to the inclined layer stacking in which the ratio of the aluminum alloy powder to the SiC powder changes linearly in a slope shape (gradual shape). The boundary layer 129 may be an inclined layer stacking in a step shape in which the ratio of the aluminum alloy powder to the SiC powder changes in a step shape. In addition, the inclination (ratio of each material) of the boundary layer 129 may also be changed according to the linear expansion coefficient of each material of the base 121 and the adsorption part 123.

[0099] (Types of 3D printers)

[0100] In addition, in the present embodiment, a powder bed melting type 3D printer is used as an example of a 3D printer 200 for manufacturing the mounting table 116. The powder bed melting type 3D printer repeatedly forms a component by spreading a powdered raw material on the processing table 202 and melting it with a laser or the like, and then spreading a powdered raw material again and melting it with a laser or the like. Therefore, the powder bed melting type 3D printer is suitable for manufacturing a structure of the mounting table 116 and the upper electrode 130 having a pre-formed three-dimensional structure with a clear structure and a complex structure such as a hollow structure.

[0101] However, the 3D printer 200 is not limited to the 3D printer of the above structure, and may be, for example, a directional energy type 3D printer, or a 3D printer using other methods. As the 3D printer used, for example, a binder jet type 3D printer, a sheet stacking type 3D printer, a photopolymerization curing (photoforming) type 3D printer, and a material extrusion (thermal melt stacking) type 3D printer can be cited.

[0102] In addition, when the material of the component to be manufactured is a resin material or a ceramic, in the process of supplying the raw material of the resin material and irradiating the energy beam by the 3D printer, ultraviolet rays can be used as the energy beam. Therefore, according to the component forming method of this embodiment, not only components made of metal materials but also components made of resin or ceramic materials can be formed. As a 3D printer in which the material of the component is a resin or a ceramic material, a material jetting type 3D printer that uses ultraviolet rays to cure the resin ejected from the inkjet head and stack them can be cited as an example.

[0103] (Layered structure of different ceramics)

[0104] Finally, the manufacture of a component having a stacked structure of different ceramics using a 3D printer is briefly described. For example, when the material of the base 121 is SiC and the material of the adsorption portion 123 is alumina, the mounting table 116 is an example of a component having a stacked structure of different ceramics. In this case, the material of the base 121 is an example of a raw material of the first ceramic, and the material of the adsorption portion 123 is an example of a raw material of a second ceramic different from the first ceramic.

[0105] Thus, in the method of forming a component having a stacked structure of different ceramics using the 3D printer 200, first, a process of supplying a raw material of the first ceramic and the second ceramic while irradiating the raw material with an energy beam is performed. Figure 3 The second control unit 250 irradiates the SiC powder with ultraviolet light based on the three-dimensional data while supplying the SiC powder to the laser scanning space 209. The energy beam irradiated in this step and the following steps is not limited to ultraviolet light, and may be light of other frequency bands.

[0106] Next, a process of supplying the raw material of the first ceramic and the raw material of the second ceramic while irradiating the raw materials with an energy beam is performed. For example, the second control unit 250 supplies SiC powder and aluminum oxide powder to the laser scanning space 209 based on the three-dimensional data while irradiating the SiC powder and aluminum oxide powder with ultraviolet rays.

[0107] Finally, a process of supplying the other raw material of the first ceramic and the second ceramic while irradiating the raw material with an energy beam is performed. For example, based on the three-dimensional data, the second control unit 250 supplies aluminum oxide powder to the laser scanning space 209 while irradiating the aluminum oxide powder with ultraviolet rays. Thus, the 3D printer 200 is used to form the mounting table 116 having a stacked structure of the SiC base 121, the boundary layer 129, and the aluminum oxide adsorption unit 123.

[0108] In the process of supplying two kinds of ceramic powders while irradiating ultraviolet rays, the second control unit 250 changes the ratio of SiC powder and alumina powder and supplies them to the laser scanning space 209 while irradiating the powder with ultraviolet rays. At this time, the second control unit 250 supplies the powder in a manner that gradually decreases the ratio of SiC powder, which is the same material as the base 121, from 100% based on the three-dimensional data and continuously changes it to 0%. In addition, the second control unit 250 supplies the powder in a manner that gradually increases the ratio of alumina powder, which is the same material as the electrostatic suction cup 120, from 0% based on the three-dimensional data and continuously changes it to 100%. In addition, the manufacturing order can be the order of base 121→boundary layer 129→adsorption unit 123, or the order of adsorption unit 123→boundary layer 129→base 121.

[0109] Thus, the ratio of SiC powder and alumina powder supplied to the laser scanning space 209 is changed from a state with more SiC to a state with more alumina while being supplied to the laser scanning space 209. The second control unit 250 repeatedly performs the operation of irradiating the SiC and alumina powders with the changed ratio with ultraviolet light to melt and solidify them. Thus, the boundary layer 129 formed between the SiC base 121 and the alumina adsorption part 123 is stacked obliquely.

[0110] In the above-mentioned manufacturing process, the thermal conductivity between different materials of the mounting table 116 can be improved by obliquely stacking the boundary layer 129 between the base 121 and the adsorption part 123. In addition, in the above-mentioned manufacturing process, the adhesive layer that adheres the base 121 and the adsorption part 123 is removed by obliquely stacking the boundary layer 129, thereby reducing the number of manufacturing processes and shortening the manufacturing time.

[0111] The above described the component forming method and the plasma processing device using the above embodiment, but the component forming method and the plasma processing device of the present invention are not limited to the above embodiment, and various modifications and improvements can be made within the scope of the present invention. The contents described in the above multiple embodiments can be combined within the scope of no contradiction.

[0112] The plasma processing apparatus of the present invention can also be applied to any type of Capacitively Coupled Plasma (CCP), Inductively Coupled Plasma (ICP), Radial Line Slot Antenna, Electron Cyclotron Resonance Plasma (ECR), and Helicon Wave Plasma (HWP).

[0113] In this specification, a wafer W is described as an example of a substrate. However, the substrate is not limited thereto, and may be various substrates used for LCD (Liquid Crystal Display), FPD (Flat Panel Display), CD substrate, printed circuit board, etc.

[0114] The present international application claims the benefit of priority based on Japanese Patent Application No. 2018-094128, filed on May 15, 2018, the entire contents of which are incorporated herein by reference.

[0115] Description of Reference Numerals

[0116] 62 No.1 High Frequency Power Supply

[0117] 64 2nd high frequency power supply

[0118] 100 Plasma treatment device

[0119] 112 Processing Container

[0120] 116 Loading table

[0121] 117 Base

[0122] 120 Electrostatic chuck

[0123] 121 Base

[0124] 123 Adsorption Department

[0125] 125 Electrode membrane

[0126] 129 Boundary Layer

[0127] 130 Upper electrode

[0128] 139 Gas supply unit

[0129] 151 First Control Unit

[0130] 200 3D printers

[0131] 202 Processing Station

[0132] 203 Raw Materials Storage Department

[0133] 204 Laser Scanning Device

[0134] 205 roller

[0135] 206 Light Source

[0136] 207 Roller drive unit

[0137] 208 Laser drive unit

[0138] 209 Laser Scanning Space

[0139] 210 Chamber

[0140] 250 Second Control Unit

[0141] HN heater.

Claims

1. A mounting table, characterized in that: include: a base formed of a conductive material; An electrostatic chuck formed of ceramic material and disposed on the base; a boundary layer disposed between the base and the electrostatic chuck, The boundary layer comprises a mixture of the conductive material and the ceramic material, The ratio of the conductive material to the ceramic material in the mixture changes in the boundary layer from the susceptor to the electrostatic chuck.

2. The mounting table according to claim 1, wherein: The ratio of the conductive material to the ceramic material in the mixture gradually decreases from the base toward the electrostatic chuck.

3. The mounting table according to claim 2, wherein: The ratio of the conductive material to the ceramic material in the mixture decreases linearly from the base toward the electrostatic chuck.

4. The mounting table according to claim 2, wherein: The ratio of the conductive material to the ceramic material in the mixture decreases in a step-like manner from the base toward the electrostatic chuck.

5. The mounting table according to claim 3, characterized in that: The ratio of the conductive material in the mixture to the ceramic material decreases from 100% to 0% toward the electrostatic chuck.

6. The mounting table according to claim 4, wherein: The ratio of the conductive material in the mixture to the ceramic material decreases from 100% to 0% toward the electrostatic chuck.

7. The mounting table according to claim 3, wherein: The boundary layer is formed by melting and solidification.

8. The mounting table according to claim 4, wherein: The boundary layer is formed by melting and solidification.

9. The mounting table according to claim 3, wherein: The conductive component is aluminum alloy, aluminum nitride, silicon carbide or titanium, The ceramic is aluminum oxide or silicon carbide.

10. The mounting table according to claim 4, wherein: The conductive component is aluminum alloy, aluminum nitride, silicon carbide or titanium, The ceramic is aluminum oxide or silicon carbide.

11. A component for a plasma processing device, characterized in that: include: a first component formed of a first material; a second component formed of a second material; and a boundary layer provided between the first component and the second component, The boundary layer comprises a mixture of the first material and the second material, The ratio of the first material to the second material in the mixture changes in the boundary layer from the first member to the second member.

12. The component for a plasma processing apparatus according to claim 11, wherein: The ratio of the first material to the second material in the mixture gradually decreases from the first component to the second component.

13. The component for a plasma processing apparatus according to claim 12, wherein: The ratio of the first material to the second material in the mixture decreases linearly from the first member to the second member.

14. The component for a plasma processing apparatus according to claim 12, wherein: The ratio of the first material to the second material in the mixture decreases in a step-like manner from the first member toward the second member.

15. The component for a plasma processing apparatus according to claim 13, wherein: The ratio of the first material to the second material in the mixture decreases from 100% to 0% toward the second component.

16. The component for a plasma processing apparatus according to claim 14, wherein: The ratio of the first material to the second material in the mixture decreases from 100% to 0% toward the second component.

17. The component for a plasma processing apparatus according to claim 13, wherein: The boundary layer is formed by melting and solidification.

18. The component for a plasma processing apparatus according to claim 14, wherein: The boundary layer is formed by melting and solidification.

19. The component for a plasma processing apparatus according to claim 13, wherein: The first material is aluminum alloy, aluminum nitride, silicon carbide or titanium, The second material is aluminum oxide or silicon carbide.

20. The component for a plasma processing apparatus according to claim 14, wherein: The first material is aluminum alloy, aluminum nitride, silicon carbide or titanium, The second material is aluminum oxide or silicon carbide.

21. A plasma processing device, characterized in that: include: Plasma processing vessels; a plasma generating unit for performing plasma processing in the plasma processing container; and A component disposed in the plasma processing container, The member is formed of a first ceramic and a second ceramic different from the first ceramic, and includes a boundary layer formed while changing the compounding ratio of the first ceramic and the second ceramic.

22. The plasma processing apparatus according to claim 21, wherein: The component includes a first ceramic layer formed of the first ceramic and a second ceramic layer formed of the second ceramic, The boundary layer is provided between the first ceramic layer and the second ceramic layer.

23. The plasma processing device according to claim 21 or 22, characterized in that: The boundary layer is formed while changing the mixing ratio of the first ceramic and the second ceramic continuously or stepwise.

24. The plasma processing apparatus according to claim 21 or 22, characterized in that: The first ceramic is alumina, The second ceramic is silicon carbide.

25. A plasma processing device, characterized in that: include: Plasma processing vessels; a plasma generating unit for performing plasma processing in the plasma processing container; and A component disposed in the plasma processing container, The member is formed of metal and ceramics and includes a boundary layer formed while changing the respective ratios of the metal and the ceramics.

26. The plasma processing apparatus according to claim 25, wherein: The component includes a metal layer formed of the metal and a ceramic layer formed of the ceramic, The boundary layer is disposed between the metal layer and the ceramic layer.

27. The plasma processing apparatus according to claim 26, wherein: The ceramic layer has a heating layer inside.

28. The plasma processing apparatus according to claim 26 or 27, characterized in that: The ceramic layer has an electrode layer inside.

29. The plasma processing apparatus according to claim 26 or 27, characterized in that: The metal layer has a flow path formed therein.

30. The plasma processing apparatus according to claim 25 or 26, characterized in that: The boundary layer is formed while changing the mixing ratio of the metal and the ceramic continuously or stepwise.

31. The plasma processing apparatus according to claim 25 or 26, wherein: The metal is aluminum, The ceramic is aluminum oxide or silicon carbide.

32. A component for a plasma processing device, characterized in that: The ceramic is formed of a first ceramic and a second ceramic different from the first ceramic, and includes a boundary layer formed while changing the mixing ratio of the first ceramic and the second ceramic.

33. The component for a plasma processing apparatus according to claim 32, wherein: include: a first ceramic layer formed of the first ceramic; and a second ceramic layer formed of the second ceramic, The boundary layer is provided between the first ceramic layer and the second ceramic layer.

34. The component for a plasma processing apparatus according to claim 32 or 33, characterized in that: The boundary layer is formed while changing the mixing ratio of the first ceramic and the second ceramic continuously or stepwise.

35. The component for a plasma processing apparatus according to claim 32 or 33, characterized in that: The first ceramic is alumina, The second ceramic is silicon carbide.

36. A component for a plasma processing device, characterized in that: The invention is formed of metal and ceramic and includes a boundary layer formed by changing the mixing ratio of the metal and the ceramic.

37. The component for a plasma processing apparatus according to claim 36, wherein: include: a metal layer formed of the metal; and a ceramic layer formed of the ceramic, The boundary layer is disposed between the metal layer and the ceramic layer.

38. The component for a plasma processing apparatus according to claim 37, wherein: The ceramic layer has a heating layer inside.

39. The component for a plasma processing apparatus according to claim 37 or 38, characterized in that: The ceramic layer has an electrode layer inside.

40. The component for a plasma processing apparatus according to claim 37 or 38, characterized in that: The metal layer has a flow path formed therein.

41. The component for a plasma processing apparatus according to claim 36 or 37, characterized in that: The boundary layer is formed while changing the mixing ratio of the metal and the ceramic continuously or stepwise.

42. The component for a plasma processing apparatus according to claim 36 or 37, wherein: The metal is aluminum, The ceramic is aluminum oxide or silicon carbide.

43. A method for forming an electrostatic chuck, characterized in that: include: A first step of spreading only the raw material of silicon carbide and the raw material of aluminum oxide on a processing table and irradiating the raw material of silicon carbide and the raw material of aluminum oxide with ultraviolet light to melt and solidify them, In the first step, the raw material of silicon carbide and the raw material of aluminum oxide are spread on the processing table while changing their respective ratios only in the vertical direction.

44. The method for forming an electrostatic chuck according to claim 43, wherein: include: A second step of spreading only one of silicon carbide and aluminum oxide on the processing table and irradiating the raw material with ultraviolet light to melt and solidify only one of silicon carbide and aluminum oxide; and A third step of irradiating the raw material with ultraviolet light while spreading only the raw material of the other of silicon carbide and aluminum oxide on the processing table to melt and solidify only the other of silicon carbide and aluminum oxide, The second step is performed before the first step, The third step is performed after the first step.

45. A method for forming a mounting table, wherein the mounting table is a mounting table used in a plasma processing device, the method comprising: A first step of forming a base by irradiating the metal raw material with laser light to melt and solidify the metal raw material while only the metal raw material is spread on the processing table; A second step of forming a boundary layer on the susceptor by irradiating the metal raw material and the ceramic raw material with laser light to melt and solidify the metal raw material and the ceramic raw material while only the metal raw material and the ceramic raw material are spread on the processing table on the susceptor; and In a third step of forming a ceramic layer by irradiating the ceramic raw material with laser light to melt and solidify the ceramic raw material while only the ceramic raw material is spread on the processing table, In the second step, the raw material of the metal and the raw material of the ceramic are spread on the processing table while changing their respective ratios only in the vertical direction.

46. ​​The method for forming a mounting table according to claim 45, wherein: In the second step, the metal raw material and the ceramic raw material are supplied onto the susceptor while changing their mixing ratio continuously or stepwise.

47. The method for forming a mounting table according to claim 45, wherein: The first step, the second step, and the third step are performed in this order.

48. The method for forming a mounting table according to claim 45, wherein: The steps are performed in the order of the third step, the second step, and the first step.

49. The method for forming a mounting table according to claim 45, wherein: The method further includes a fourth step of irradiating the raw material of the heater with laser light while supplying the raw material of the heater to form a heating layer.

50. The method for forming a mounting table according to claim 45, wherein: The method further includes a fifth step of forming the electrode film by irradiating the raw material of the electrode film with laser light while supplying the raw material of the electrode film.

51. The method for forming a mounting table according to claim 45, wherein: A flow path is formed in the base.

52. The method for forming a mounting table according to claim 45, wherein: The raw material is in powder form.

53. A plasma processing device, characterized in that: include: Plasma processing vessels; a plasma generating unit for generating plasma for performing plasma treatment on a substrate in the plasma processing device; and An electrostatic chuck is arranged in a plasma processing device. The electrostatic chuck has a boundary layer, which is formed by changing the respective ratios of the silicon carbide raw material and the aluminum oxide raw material only in the longitudinal direction while spreading them on the processing table in a process of spreading only the silicon carbide raw material and the aluminum oxide raw material on the processing table while irradiating the silicon carbide raw material and the aluminum oxide raw material with ultraviolet rays.

54. The plasma processing apparatus according to claim 53, wherein: The electrostatic chuck further comprises a first layer and a second layer, The first layer is formed by spreading only one of silicon carbide and aluminum oxide on the processing table and irradiating the raw material with ultraviolet light to melt and solidify only one of silicon carbide and aluminum oxide. The second layer is formed by spreading only the raw material of the other of silicon carbide and aluminum oxide on the processing table and irradiating the raw material with ultraviolet rays to melt and solidify only the other of silicon carbide and aluminum oxide. The boundary layer is arranged between the first layer and the second layer.

55. A plasma processing device, characterized in that: include: Plasma processing vessels; a plasma generating unit for generating plasma for performing plasma treatment on a substrate in the plasma processing device; and A mounting table is arranged in a plasma processing device, The mounting platform has a first layer, a boundary layer and a second layer, The first layer is formed by a first step of spreading only the metal raw material on the processing table and irradiating the metal raw material with laser to melt and solidify the metal raw material to form a base. The boundary layer is formed by a second step of spreading only the metal raw material and the ceramic raw material on the processing table on the base and irradiating the metal raw material and the ceramic raw material with laser to melt and solidify the metal raw material and form a boundary layer on the base. The second layer is formed by a third step of spreading the ceramic raw material on the processing table and irradiating the ceramic raw material with laser to melt and solidify the ceramic raw material to form a ceramic layer. The boundary layer is formed by spreading the raw materials of the metal and the raw materials of the ceramics on the processing table while changing their respective ratios only in the vertical direction in the second step.

56. The plasma processing apparatus according to claim 55, wherein: The boundary layer is formed while continuously or stepwise changing the ratio of the metal raw material and the ceramic raw material supplied onto the susceptor.

57. The plasma processing apparatus according to claim 55, wherein: The mounting table is formed by performing the first step, the second step, and the third step in this order.

58. The plasma processing apparatus according to claim 55, wherein: The mounting table is formed by performing the third step, the second step, and the first step in this order.

59. The plasma processing apparatus according to claim 55, wherein: The mounting table further includes a heating layer formed by a fourth step of forming the heating layer by irradiating the raw material of the heater with laser light while supplying the raw material of the heater.

60. The plasma processing apparatus according to claim 55, wherein: The mounting table further includes an electrode layer formed by a fifth step of forming an electrode film by irradiating the raw material of the electrode film with laser light while supplying the raw material of the electrode film.

61. The plasma processing apparatus according to claim 55, wherein: A flow path is formed in the base.

62. The plasma processing apparatus according to claim 55, wherein: The raw material is in powder form.