Semiconductor device and manufacturing method thereof

By forming depletion-mode and enhancement-mode device regions on the substrate respectively, and by utilizing the design of passivation layer and gate structure, the process compatibility problem of depletion-mode and enhancement-mode GaN HEMT devices is solved, and device integration and performance improvement are achieved.

CN118969796AInactive Publication Date: 2024-11-15SHANGHAI XINWEI SEMICON CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411056090.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the existing technology, the processes for depletion-mode and enhancement-mode GaN HEMT devices are incompatible, making it difficult to achieve effective integration of integrated circuits.

Method used

Depletion-type and enhancement-type device regions are formed on the substrate, and a second gate structure is covered by a passivation layer to form a first gate structure as a gate dielectric layer. Combined with the arrangement of source and drain metals, the integration of depletion-type and enhancement-type devices is achieved.

Benefits of technology

It achieves efficient integration of depletion-mode and enhancement-mode devices, reduces parasitic parameters, and improves device performance such as switching speed and power consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118969796A_ABST
    Figure CN118969796A_ABST
Patent Text Reader

Abstract

The invention provides a semiconductor device and a manufacturing method thereof, and the semiconductor device comprises a substrate which comprises a depletion type device region and an enhancement type device region; the second gate structure is formed on the substrate in the enhanced device region; the passivation layer is formed on the substrate in the depletion type device region and the enhancement type device region, and the passivation layer covers the second gate structure; the first gate structure is formed on the passivation layer in the depletion type device region, and the passivation layer between the first gate structure and the substrate is used as a gate dielectric layer; the first gate structure is formed on the substrate, the second gate structure is formed on the substrate, the first source metal, the first drain metal, the second source metal and the second drain metal are formed on the substrate on the two sides of the first gate structure, and the second source metal and the second drain metal are formed on the substrate on the two sides of the second gate structure. According to the technical scheme, the depletion type device and the enhancement type device can be integrated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a semiconductor device and a manufacturing method thereof. Background Art

[0002] Due to the compatibility issues between GaN HEMT (High Electron Mobility Transistor) power devices and silicon-based drive circuits, in order to further reduce parasitic parameters, it is necessary to develop GaN integrated circuits. For mature silicon-based integrated circuits, low static power consumption and high operating frequency CMOS integrated circuits can be realized based on enhanced NMOS and PMOS devices; however, due to the low activation rate and large device damage under high doping of P-type GaN HEMT devices, enhanced PMOS devices have not been realized. Therefore, at this stage, direct-coupled integrated circuits are mostly realized based on depletion-mode (D-mode) HEMT devices and enhancement-mode (E-mode) HEMT devices. However, due to the large differences in the structures of depletion-mode HEMT devices and enhancement-mode HEMT devices, the conventional process for realizing enhancement-mode HEMT devices is not compatible with the process of depletion-mode HEMT devices, which is not conducive to integration.

[0003] Therefore, how to integrate depletion-mode devices and enhancement-mode devices is a problem that needs to be solved urgently. Summary of the invention

[0004] The object of the present invention is to provide a semiconductor device and a manufacturing method thereof, so that a depletion-mode device and an enhancement-mode device are integrated.

[0005] To achieve the above object, the present invention provides a semiconductor device, comprising:

[0006] A substrate, including a depletion mode device region and an enhancement mode device region;

[0007] A second gate structure is formed on the substrate in the enhancement mode device region;

[0008] A passivation layer is formed on the substrate in the depletion-mode device region and the enhancement-mode device region, and the passivation layer covers the second gate structure;

[0009] A first gate structure is formed on the passivation layer in the depletion-mode device region, wherein the passivation layer between the first gate structure and the substrate serves as a gate dielectric layer;

[0010] A first source metal, a first drain metal, a second source metal, and a second drain metal, wherein the first source metal and the first drain metal are formed on the substrate at both sides of the first gate structure, and the second source metal and the second drain metal are formed on the substrate at both sides of the second gate structure.

[0011] Optionally, the substrate further includes an enhanced power device region, and the semiconductor device further includes:

[0012] A third gate structure is formed on the substrate in the enhanced power device region, and the passivation layer is also formed on the substrate in the enhanced power device region and the third gate structure;

[0013] A third source metal and a third drain metal are formed on the substrate at two sides of the third gate structure.

[0014] Optionally, the first gate structure includes a first metal gate layer, and the second gate structure and the third gate structure each include a nitride gate layer and a second metal gate layer from bottom to top.

[0015] Optionally, the first gate structure, the second gate structure and the third gate structure each further include a third metal gate layer, and the third metal gate layer is formed on the first metal gate layer and the second metal gate layer.

[0016] Optionally, the semiconductor device further includes:

[0017] At least one field plate is formed on the passivation layer in the enhancement mode power device region.

[0018] Optionally, the base includes a substrate, and a buffer layer, a channel layer, and a barrier layer formed from bottom to top on the substrate.

[0019] The present invention also provides a method for manufacturing a semiconductor device, comprising:

[0020] Providing a substrate, the substrate comprising a depletion-type device region and an enhancement-type device region;

[0021] A second gate structure, a passivation layer and a first gate structure are formed, wherein the second gate structure is formed on the substrate in the enhancement device region; the passivation layer is formed on the substrate in the depletion device region and the enhancement device region, and the passivation layer covers the second gate structure; the first gate structure is formed on the passivation layer in the depletion device region, and the passivation layer between the first gate structure and the substrate serves as a gate dielectric layer;

[0022] A first source metal, a first drain metal, a second source metal and a second drain metal are formed, wherein the first source metal and the first drain metal are formed on the substrate on both sides of the first gate structure, and the second source metal and the second drain metal are formed on the substrate on both sides of the second gate structure.

[0023] Optionally, the substrate further includes an enhanced power device region, and the method for manufacturing the semiconductor device further includes:

[0024] forming a third gate structure on the substrate in the enhanced power device region, wherein the passivation layer is also formed on the substrate in the enhanced power device region and the third gate structure;

[0025] A third source metal and a third drain metal are formed on the substrate at two sides of the third gate structure.

[0026] Optionally, the steps of forming the second gate structure, the passivation layer, the first gate structure and the third gate structure include:

[0027] Forming a nitride gate layer and a second metal gate layer stacked on the substrate of the enhancement mode device region and the enhancement mode power device region;

[0028] Forming a passivation layer on the substrate in the depletion-mode device region, the enhancement-mode device region and the enhancement-mode power device region, wherein the passivation layer covers the nitride gate layer and the second metal gate layer;

[0029] A first metal gate layer is formed on the passivation layer in the depletion device region, so that the first gate structure includes the first metal gate layer, and the second gate structure and the third gate structure both include the nitride gate layer and the second metal gate layer.

[0030] Optionally, the step of forming the second gate structure, the first gate structure and the third gate structure further includes:

[0031] A third metal gate layer is formed on the first metal gate layer and the second metal gate layer, so that the first gate structure, the second gate structure and the third gate structure all further include the third metal gate layer.

[0032] Optionally, the method for manufacturing the semiconductor device further includes:

[0033] At least one field plate is formed on the passivation layer in the enhancement mode power device region.

[0034] Optionally, the base includes a substrate, and a buffer layer, a channel layer, and a barrier layer formed from bottom to top on the substrate.

[0035] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:

[0036] 1. The semiconductor device of the present invention comprises: a substrate including a depletion-type device region and an enhancement-type device region; a second gate structure formed on the substrate in the enhancement-type device region; a passivation layer formed on the substrate in the depletion-type device region and the enhancement-type device region, the passivation layer covering the second gate structure; a first gate structure formed on the passivation layer in the depletion-type device region, the passivation layer between the first gate structure and the substrate serving as a gate dielectric layer; a first source metal, a first drain metal, a second source metal and a second drain metal, the first source metal and the first drain metal being formed on the substrate on both sides of the first gate structure, the second source metal and the second drain metal being formed on the substrate on both sides of the second gate structure, so that a depletion-type device and an enhancement-type device can be integrated.

[0037] 2. The manufacturing method of the semiconductor device of the present invention comprises: providing a substrate, the substrate comprising a depletion-type device region and an enhancement-type device region; forming a second gate structure, a passivation layer and a first gate structure, the second gate structure being formed on the substrate in the enhancement-type device region; the passivation layer being formed on the substrate in the depletion-type device region and the enhancement-type device region, the passivation layer covering the second gate structure; the first gate structure being formed on the passivation layer in the depletion-type device region, the passivation layer between the first gate structure and the substrate serving as a gate dielectric layer; forming a first source metal, a first drain metal, a second source metal and a second drain metal, the first source metal and the first drain metal being formed on the substrate on both sides of the first gate structure, the second source metal and the second drain metal being formed on the substrate on both sides of the second gate structure, so that a depletion-type device and an enhancement-type device can be integrated. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 is a schematic diagram of a semiconductor device according to an embodiment of the present invention;

[0039] Figure 2 is a flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present invention;

[0040] Figure 3a to Figure 3j yes Figure 2 A device schematic diagram of a method for manufacturing a semiconductor device is shown.

[0041] Among them, Figure 1 to Figure 3j The reference numerals are described as follows:

[0042] 10-substrate; 101-buffer layer; 102-channel layer; 103-barrier layer; 104-nitride layer; 105-second metal layer; 111-first metal gate layer; 112-nitride gate layer; 113-second metal gate layer; 114-third metal gate layer; 12-passivation layer; 131-first source metal; 132-first drain metal; 133-second source metal; 134-second drain metal; 135-third source metal; 136-third drain metal; 141-first insulating dielectric layer; 142-second insulating dielectric layer; 15-field plate; 161-first interlayer dielectric layer; 162-second interlayer dielectric layer; 171-conductive plug; 172-first metal layer. DETAILED DESCRIPTION

[0043] In order to make the purpose, advantages and features of the present invention more clear, the semiconductor device and the manufacturing method thereof proposed by the present invention are further described in detail below in conjunction with the accompanying drawings. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.

[0044] An embodiment of the present invention provides a semiconductor device, comprising: a substrate, comprising a depletion-type device region and an enhancement-type device region; a second gate structure, formed on the substrate in the enhancement-type device region; a passivation layer, formed on the substrate in the depletion-type device region and the enhancement-type device region, the passivation layer covering the second gate structure; a first gate structure, formed on the passivation layer in the depletion-type device region, the passivation layer between the first gate structure and the substrate serving as a gate dielectric layer; a first source metal, a first drain metal, a second source metal, and a second drain metal, the first source metal and the first drain metal being formed on the substrate on both sides of the first gate structure, the second source metal and the second drain metal being formed on the substrate on both sides of the second gate structure.

[0045] See below Figure 1 The semiconductor device provided by this embodiment is described in more detail. Figure 1 It is a schematic diagram of a longitudinal cross-section of a semiconductor device.

[0046] The substrate includes a depletion type device region A1 and an enhancement type device region A2.

[0047] The depletion-type device region A1 is used to form a depletion-type device, and the enhancement-type device region A2 is used to form an enhancement-type device.

[0048] The base includes a substrate 10 and a buffer layer 101 , a channel layer 102 and a barrier layer 103 formed from bottom to top on the substrate 10 .

[0049] The substrate 10 may be made of any appropriate semiconductor material, including but not limited to Si, SiGe, SiGeC, SiC, GaAs, GaN, InAs, InP or sapphire, the buffer layer 101 may be made of GaN or AlGaN, the channel layer 102 may be made of GaN, and the barrier layer 103 may be made of AlGaN.

[0050] The second gate structure is formed on the substrate in the enhancement mode device region A2.

[0051] The passivation layer 12 is formed on the substrate of the depletion-mode device region A1 and the enhancement-mode device region A2 , and the passivation layer 12 covers the second gate structure.

[0052] The material of the passivation layer 12 may include at least one of AlN, Al2O3, SiO2 and SiN.

[0053] The first gate structure is formed on the passivation layer 12 of the depletion-mode device region A1 , and the passivation layer 12 between the first gate structure and the substrate serves as a gate dielectric layer.

[0054] The first source metal 131 and the first drain metal 132 are formed on the substrate of the depletion device region A1 on both sides of the first gate structure, and the second source metal 133 and the second drain metal 134 are formed on the substrate of the enhancement device region A2 on both sides of the second gate structure.

[0055] In one embodiment, the substrate further includes an enhanced power device region A3, and the semiconductor device further includes:

[0056] A third gate structure is formed on the substrate of the enhanced power device area A3, and the passivation layer 12 is also formed on the substrate of the enhanced power device area A3 and the third gate structure;

[0057] A third source metal 135 and a third drain metal 136 are formed on the substrate of the enhanced power device region A3 at both sides of the third gate structure.

[0058] The first source metal 131 , the first drain metal 132 , the second source metal 133 , the second drain metal 134 , the third source metal 135 and the third drain metal 136 all penetrate the passivation layer 12 and contact the barrier layer 103 .

[0059] The enhancement mode power device region A3 is used to form an enhancement mode power device.

[0060] In one embodiment, the depletion-mode device, the enhancement-mode device and the enhancement-mode power device may all be HEMT (High Electron Mobility Transistor) devices.

[0061] The threshold voltage of the depletion-mode device is less than 0V, and the threshold voltage of the enhancement-mode device and the enhancement-mode power device is greater than 0V.

[0062] In one embodiment, the first gate structure includes a first metal gate layer 111 , and the second gate structure and the third gate structure each include a nitride gate layer 112 and a second metal gate layer 113 from bottom to top.

[0063] Preferably, the first gate structure, the second gate structure and the third gate structure all further include a third metal gate layer 114, and the third metal gate layer 114 is formed on the first metal gate layer 111 and the second metal gate layer 113. By providing the third metal gate layer 114, the thickness of the first gate structure, the second gate structure and the third gate structure is increased, thereby reducing the parasitic gate resistance.

[0064] The materials of the first metal gate layer 111, the second metal gate layer 113 and the third metal gate layer 114 may include at least one of metal (such as titanium, aluminum or tungsten), metal nitride (titanium nitride or tungsten nitride) and metal silicide, and the material of the nitride gate layer 112 may include GaN, AlN or AlGaN.

[0065] Preferably, the lengths of the first gate structure, the second gate structure and the third gate structure are all 0.1 μm to 2 μm, so that the performance (such as switching speed, power consumption, etc.) of the depletion-mode device, the enhancement-mode device and the enhancement-mode power device is better. The length refers to the length in the direction from the first source metal 131 to the first drain metal 132.

[0066] Preferably, the thickness of the passivation layer 12 is 0-100 nm, so as to reduce the dynamic on-resistance of the depletion-mode device, the enhancement-mode device and the enhancement-mode power device.

[0067] Preferably, the semiconductor device further comprises: at least one field plate 15 formed on the passivation layer 12 of the enhanced power device region A3. By providing the field plate 15 on the enhanced power device region A3, the withstand voltage of the enhanced power device can be improved.

[0068] When the semiconductor device includes at least two layers of the field plates 15 , an insulating dielectric layer is formed between adjacent layers of the field plates 15 , and the projections of the adjacent layers of the field plates 15 in a direction perpendicular to the substrate surface may overlap or not overlap.

[0069] exist Figure 1 In the illustrated embodiment, the semiconductor device further includes a first insulating dielectric layer 141 and a second insulating dielectric layer 142, wherein the first insulating dielectric layer 141 is formed on the passivation layer 12, and the first insulating dielectric layer 141 covers the first metal gate layer 111, and the field plate 15 is formed on the first insulating dielectric layer 141 of the enhanced power device area A3, and the second insulating dielectric layer 142 is formed on the first insulating dielectric layer 141, and the second insulating dielectric layer 142 covers the field plate 15. In other embodiments, the field plate 15 may also be formed between the passivation layer 12 and the first insulating dielectric layer 141 of the enhanced power device area A3.

[0070] In one embodiment, in the depletion-mode device area A1, the third metal gate layer 114 penetrates the second insulating dielectric layer 142 and the first insulating dielectric layer 141 and then contacts the first metal gate layer 111; in the enhancement-mode device area A2 and the enhancement-mode power device area A3, the third metal gate layer 114 penetrates the second insulating dielectric layer 142, the first insulating dielectric layer 141 and the passivation layer 12 and then contacts the second metal gate layer 113. The top surface of the third metal gate layer 114 is flush with or higher than the top surface of the second insulating dielectric layer 142.

[0071] In one embodiment, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136 all penetrate the second insulating dielectric layer 142, the first insulating dielectric layer 141 and the passivation layer 12 and then contact the barrier layer 103, and the top surfaces of the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136 are flush with or higher than the top surface of the second insulating dielectric layer 142.

[0072] The field plate 15 may be made of at least one of metal (such as titanium, aluminum or tungsten), metal nitride (titanium nitride or tungsten nitride) and metal silicide. The field plate 15 may be made of the same material as or different from the first metal gate layer 111 .

[0073] The semiconductor device further includes an interlayer dielectric layer and a metal interconnect structure, wherein the interlayer dielectric layer is formed on the second insulating dielectric layer 142, and the interlayer dielectric layer covers the third metal gate layer 114, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136, the third metal gate layer 114, the field plate 15, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136. The metal interconnection structure may be formed in the interlayer dielectric layer on the drain metal 134, the third source metal 135, and the third drain metal 136, and the top surface of the interlayer dielectric layer exposes a part of the structure of the metal interconnection structure, so that the first gate structure, the second gate structure, the third gate structure, the field plate 15, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135, and the third drain metal 136 are led out through the metal interconnection structure. The metal interconnection structures on the third metal gate layer 114, the field plate 15, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135, and the third drain metal 136 may be connected or not connected.

[0074] The interlayer dielectric layer may include a stacked multi-layer structure, and the metal interconnect structure may include a multi-layer conductive plug 171 and a multi-layer first metal layer 172. Figure 1 In the illustrated embodiment, the interlayer dielectric layer includes a first interlayer dielectric layer 161 and a second interlayer dielectric layer 162 from bottom to top, the metal interconnect structure includes a multi-layer conductive plug 171 and a multi-layer first metal layer 172, the first metal layers 172 of adjacent layers are electrically connected through the conductive plug 171, and the bottom-most first metal layer 172 is electrically connected to the third metal gate layer 114, the field plate 15, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136 through the conductive plug 171.

[0075] In one embodiment, the metal interconnect structure can also lead out the substrate 10, such as Figure 1As shown, the conductive plug 171 is also formed on the substrate 10, and the conductive plug 171 penetrates the second interlayer dielectric layer 162, the first interlayer dielectric layer 161, the second insulating dielectric layer 142, the first insulating dielectric layer 141, the passivation layer 12, the barrier layer 103, the channel layer 102 and the buffer layer 101 and is electrically connected to the substrate 10, and the first metal layer 172 electrically connected to the conductive plug 171 is formed on the second interlayer dielectric layer 162.

[0076] In addition, an isolation structure (not shown) is formed between any adjacent regions of the depletion mode device region A1, the enhancement mode device region A2 and the enhancement mode power device region A3. The isolation structure may be an ion doped region or a groove.

[0077] From the above content, it can be seen that since the passivation layer 12 is formed on the substrate of the depletion-type device area A1 and the enhancement-type device area A2, the passivation layer 12 covers the second gate structure; the passivation layer 12 between the first gate structure of the depletion-type device area A1 and the substrate serves as a gate dielectric layer, thereby realizing the integration of depletion-type devices and enhancement-type devices.

[0078] Furthermore, when the substrate further includes the enhancement mode power device region A3, the passivation layer 12 is also formed on the substrate and the third gate structure of the enhancement mode power device region A3, thereby realizing the integration of depletion mode devices, enhancement mode devices and enhancement mode power devices.

[0079] In summary, the semiconductor device provided by the present invention includes: a substrate, including a depletion device region and an enhancement device region; a second gate structure, formed on the substrate in the enhancement device region; a passivation layer, formed on the substrate in the depletion device region and the enhancement device region, the passivation layer covering the second gate structure; a first gate structure, formed on the passivation layer in the depletion device region, the passivation layer between the first gate structure and the substrate serving as a gate dielectric layer; a first source metal, a first drain metal, a second source metal and a second drain metal, the first source metal and the first drain metal being formed on the substrate on both sides of the first gate structure, the second source metal and the second drain metal being formed on the substrate on both sides of the second gate structure. The semiconductor device of the present invention enables the integration of depletion devices and enhancement devices.

[0080] An embodiment of the present invention provides a method for manufacturing a semiconductor device. Figure 2 , Figure 2 1 is a flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present invention, wherein the method for manufacturing a semiconductor device comprises:

[0081] Step S1, providing a substrate, wherein the substrate comprises a depletion-type device region and an enhancement-type device region;

[0082] Step S2, forming a second gate structure, a passivation layer and a first gate structure, wherein the second gate structure is formed on the substrate in the enhancement device region; the passivation layer is formed on the substrate in the depletion device region and the enhancement device region, and the passivation layer covers the second gate structure; the first gate structure is formed on the passivation layer in the depletion device region, and the passivation layer between the first gate structure and the substrate serves as a gate dielectric layer;

[0083] Step S3, forming a first source metal, a first drain metal, a second source metal and a second drain metal, wherein the first source metal and the first drain metal are formed on the substrate on both sides of the first gate structure, and the second source metal and the second drain metal are formed on the substrate on both sides of the second gate structure.

[0084] See below Figure 3a to Figure 3j The method for manufacturing the semiconductor device provided in this embodiment is described in more detail. Figure 3a to Figure 3j It is a schematic diagram of a longitudinal cross-section of a semiconductor device.

[0085] According to step S1, Figure 3a As shown, a substrate is provided, wherein the substrate includes a depletion type device region A1 and an enhancement type device region A2.

[0086] The depletion-type device region A1 is used to form a depletion-type device, and the enhancement-type device region A2 is used to form an enhancement-type device.

[0087] The base includes a substrate 10 and a buffer layer 101 , a channel layer 102 and a barrier layer 103 formed from bottom to top on the substrate 10 .

[0088] The substrate 10 may be made of any appropriate semiconductor material, including but not limited to Si, SiGe, SiGeC, SiC, GaAs, GaN, InAs, InP or sapphire, the buffer layer 101 may be made of GaN or AlGaN, the channel layer 102 may be made of GaN, and the barrier layer 103 may be made of AlGaN.

[0089] According to step S2, a second gate structure, a passivation layer 12 and a first gate structure are formed, wherein the second gate structure is formed on the substrate of the enhancement device area A2; the passivation layer 12 is formed on the depletion device area A1 and the substrate of the enhancement device area A2, and the passivation layer 12 covers the second gate structure; the first gate structure is formed on the passivation layer 12 of the depletion device area A1, and the passivation layer 12 between the first gate structure and the substrate serves as a gate dielectric layer.

[0090] The material of the passivation layer 12 may include at least one of AlN, Al2O3, SiO2 and SiN.

[0091] According to step S3, a first source metal 131, a first drain metal 132, a second source metal 133 and a second drain metal 134 are formed, the first source metal 131 and the first drain metal 132 are formed on the substrate of the depletion device area A1 on both sides of the first gate structure, and the second source metal 133 and the second drain metal 134 are formed on the substrate of the enhancement device area A2 on both sides of the second gate structure.

[0092] In one embodiment, the substrate further includes an enhanced power device region A3, and the method for manufacturing the semiconductor device further includes:

[0093] Forming a third gate structure on the substrate of the enhanced power device area A3, and the passivation layer 12 is also formed on the substrate of the enhanced power device area A3 and the third gate structure;

[0094] A third source metal 135 and a third drain metal 136 are formed on the substrate of the enhanced power device region A3 at both sides of the third gate structure.

[0095] The enhancement mode power device region A3 is used to form an enhancement mode power device.

[0096] In one embodiment, the depletion-mode device, the enhancement-mode device and the enhancement-mode power device may all be HEMT (High Electron Mobility Transistor) devices.

[0097] The threshold voltage of the depletion-mode device is less than 0V, and the threshold voltage of the enhancement-mode device and the enhancement-mode power device is greater than 0V.

[0098] In one embodiment, the steps of forming the second gate structure, the passivation layer 12, the first gate structure and the third gate structure include: first, Figure 3aAs shown, a nitride layer 104 and a second metal layer 105 are sequentially formed on the substrate of the depletion mode device region A1, the enhancement mode device region A2 and the enhancement mode power device region A3; then, as shown in FIG. Figure 3b As shown, the nitride layer 104 and the second metal layer 105 are etched to form a nitride gate layer 112 and a second metal gate layer 113 stacked from bottom to top on the substrate of the enhancement device area A2 and the enhancement power device area A3; then, as shown Figure 3c As shown, a passivation layer 12 is formed on the substrate of the depletion device region A1, the enhancement device region A2 and the enhancement power device region A3, and the passivation layer 12 covers the nitride gate layer 112 and the second metal gate layer 113; then, as shown Figure 3d As shown, a first metal gate layer 111 is formed on the passivation layer 12 of the depletion device area A1, so that the first gate structure includes the first metal gate layer 111, and the second gate structure and the third gate structure both include the nitride gate layer 112 and the second metal gate layer 113.

[0099] Preferably, the method for manufacturing the semiconductor device further comprises: Figure 3e As shown, at least one field plate 15 is formed on the passivation layer 12 of the enhanced power device region A3. By providing the field plate 15 on the enhanced power device region A3, the withstand voltage of the enhanced power device can be improved.

[0100] When the semiconductor device includes at least two layers of the field plates 15 , an insulating dielectric layer is formed between adjacent layers of the field plates 15 , and the projections of the adjacent layers of the field plates 15 in a direction perpendicular to the substrate surface may overlap or not overlap.

[0101] exist Figure 3e In the illustrated embodiment, after forming the first metal gate layer 111 and before forming the field plate 15, a first insulating dielectric layer 141 is further formed on the passivation layer 12, the first insulating dielectric layer 141 covers the first metal gate layer 111, and the field plate 15 is formed on the first insulating dielectric layer 141 of the enhanced power device region A3; after forming the field plate 15, a second insulating dielectric layer 142 is further formed on the first insulating dielectric layer 141, the second insulating dielectric layer 142 covers the field plate 15. In other embodiments, the field plate 15 may also be formed between the passivation layer 12 and the first insulating dielectric layer 141 of the enhanced power device region A3. In this case, preferably, the field plate 15 between the passivation layer 12 and the first insulating dielectric layer 141 is formed simultaneously with the first metal gate layer 111 to simplify the process.

[0102] Preferably, the steps of forming the second gate structure, the first gate structure and the third gate structure further include: Figure 3f As shown, a third metal gate layer 114 is formed on the first metal gate layer 111 and the second metal gate layer 113, so that the first gate structure, the second gate structure and the third gate structure all include the third metal gate layer 114. Figure 3f In the illustrated embodiment, the second insulating dielectric layer 142 and the first insulating dielectric layer 141 on the first metal gate layer 111 are etched to form a first through hole (not shown) exposing the first metal gate layer 111, and the second insulating dielectric layer 142, the first insulating dielectric layer 141 and the passivation layer 12 on the second metal gate layer 113 are etched to form a second through hole (not shown) exposing the second metal gate layer 113, and then metal material is filled into the first through hole and the second through hole to form the third metal gate layer 114. The top surface of the third metal gate layer 114 is flush with or higher than the top surface of the second insulating dielectric layer 142.

[0103] By providing the third metal gate layer 114 , the thicknesses of the first gate structure, the second gate structure and the third gate structure are increased, thereby reducing the parasitic gate resistance.

[0104] The materials of the first metal gate layer 111, the second metal gate layer 113, the third metal gate layer 114 and the field plate 15 may include at least one of metal (e.g., titanium, aluminum or tungsten), metal nitride (titanium nitride or tungsten nitride) and metal silicide, and the material of the nitride gate layer 112 may include GaN, AlN or AlGaN.

[0105] The material of the field plate 15 is the same as or different from the material of the first metal gate layer 111 .

[0106] Preferably, the lengths of the first gate structure, the second gate structure and the third gate structure are all 0.1 μm to 2 μm, so that the performance (such as switching speed, power consumption, etc.) of the depletion-mode device, the enhancement-mode device and the enhancement-mode power device is better. The length refers to the length in the direction from the first source metal 131 to the first drain metal 132.

[0107] Preferably, the thickness of the passivation layer 12 is 0-100 nm, so as to reduce the dynamic on-resistance of the depletion-mode device, the enhancement-mode device and the enhancement-mode power device.

[0108] In one embodiment, the steps of forming the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136 may include: Figure 3g As shown, the second insulating dielectric layer 142, the first insulating dielectric layer 141 and the passivation layer 12 on both sides of the first gate structure, the second gate structure and the third gate structure are etched to form a plurality of third through holes (not shown) exposing the barrier layer 103, and metal material is filled into the third through holes to form the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136. The top surfaces of the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136 are flush with or higher than the top surface of the second insulating dielectric layer 142.

[0109] The method for manufacturing the semiconductor device further includes: forming an interlayer dielectric layer and a metal interconnect structure, wherein the interlayer dielectric layer is formed on the second insulating dielectric layer 142, and the interlayer dielectric layer covers the third metal gate layer 114, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136, the third metal gate layer 114, the field plate 15, the first source metal 131, the first drain metal 132, the second source metal 133, The metal interconnection structure may be formed in the interlayer dielectric layer on the second drain metal 134, the third source metal 135 and the third drain metal 136, and the top surface of the interlayer dielectric layer exposes a part of the structure of the metal interconnection structure, so as to lead out the first gate structure, the second gate structure, the third gate structure, the field plate 15, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136 through the metal interconnection structure. The metal interconnection structures on the third metal gate layer 114, the field plate 15, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136 may be connected or not connected.

[0110] The interlayer dielectric layer may include a stacked multi-layer structure, and the metal interconnect structure may include a multi-layer conductive plug 171 and a multi-layer first metal layer 172. Figure 3h~Figure 3j The steps of forming the interlayer dielectric layer and the metal interconnect structure may include: Figure 3h As shown, a first interlayer dielectric layer 161 is formed on the second insulating dielectric layer 142, and then a conductive plug 171 is formed in the first interlayer dielectric layer 161 on the third metal gate layer 114, the field plate 15, the first source metal 131, the first drain metal 132, the second source metal 133, the second drain metal 134, the third source metal 135 and the third drain metal 136; then, as shown Figure 3i As shown, a first metal layer 172 is formed on the first interlayer dielectric layer 161, and the first metal layer 172 is electrically connected to the conductive plug 171; then, as shown in FIG. Figure 3j As shown, a second interlayer dielectric layer 162 is formed on the first interlayer dielectric layer 161, and a plurality of conductive plugs 171 are formed in the second interlayer dielectric layer 162, and a first metal layer 172 is formed on the second interlayer dielectric layer 162; then, the above steps are repeated to form the interlayer dielectric layer and the metal interconnection structure.

[0111] In one embodiment, the metal interconnect structure can also lead out the substrate 10, such as Figure 3j As shown, the conductive plug 171 is also formed on the substrate 10, and the conductive plug 171 penetrates the second interlayer dielectric layer 162, the first interlayer dielectric layer 161, the second insulating dielectric layer 142, the first insulating dielectric layer 141, the passivation layer 12, the barrier layer 103, the channel layer 102 and the buffer layer 101 and is electrically connected to the substrate 10, and the first metal layer 172 electrically connected to the conductive plug 171 is formed on the second interlayer dielectric layer 162.

[0112] In addition, an isolation structure (not shown) is formed between any adjacent regions of the depletion mode device region A1, the enhancement mode device region A2 and the enhancement mode power device region A3. The isolation structure may be an ion doped region or a groove.

[0113] From the above content, it can be seen that since the passivation layer 12 is formed on the substrate of the depletion-type device area A1 and the enhancement-type device area A2, the passivation layer 12 covers the second gate structure; the passivation layer 12 between the first gate structure of the depletion-type device area A1 and the substrate serves as a gate dielectric layer, thereby realizing the integration of depletion-type devices and enhancement-type devices.

[0114] Furthermore, when the substrate further includes the enhancement mode power device region A3, the passivation layer 12 is also formed on the substrate and the third gate structure of the enhancement mode power device region A3, thereby realizing the integration of depletion mode devices, enhancement mode devices and enhancement mode power devices.

[0115] In summary, the manufacturing method of the semiconductor device provided by the present invention includes: providing a substrate, the substrate including a depletion device region and an enhancement device region; forming a second gate structure, a passivation layer and a first gate structure, the second gate structure is formed on the substrate in the enhancement device region; the passivation layer is formed on the substrate in the depletion device region and the enhancement device region, and the passivation layer covers the second gate structure; the first gate structure is formed on the passivation layer in the depletion device region, and the passivation layer between the first gate structure and the substrate serves as a gate dielectric layer; forming a first source metal, a first drain metal, a second source metal and a second drain metal, the first source metal and the first drain metal are formed on the substrate on both sides of the first gate structure, and the second source metal and the second drain metal are formed on the substrate on both sides of the second gate structure. The manufacturing method of the semiconductor device of the present invention enables the integration of depletion-type devices and enhancement-type devices.

[0116] The above description is only a description of the preferred embodiments of the present invention, and is not intended to limit the scope of the present invention. Any changes or modifications made by a person skilled in the art in the field of the present invention based on the above disclosure shall fall within the scope of protection of the claims.

Claims

1. A semiconductor device, characterized in that: include: A substrate, including a depletion mode device region and an enhancement mode device region; A second gate structure is formed on the substrate in the enhancement mode device region; A passivation layer is formed on the substrate in the depletion-mode device region and the enhancement-mode device region, and the passivation layer covers the second gate structure; A first gate structure is formed on the passivation layer in the depletion-mode device region, wherein the passivation layer between the first gate structure and the substrate serves as a gate dielectric layer; A first source metal, a first drain metal, a second source metal, and a second drain metal, wherein the first source metal and the first drain metal are formed on the substrate at both sides of the first gate structure, and the second source metal and the second drain metal are formed on the substrate at both sides of the second gate structure.

2. The semiconductor device according to claim 1, wherein The substrate further includes an enhanced power device region, and the semiconductor device further includes: A third gate structure is formed on the substrate in the enhanced power device region, and the passivation layer is also formed on the substrate in the enhanced power device region and the third gate structure; A third source metal and a third drain metal are formed on the substrate at two sides of the third gate structure.

3. The semiconductor device according to claim 2, wherein: The first gate structure includes a first metal gate layer, and the second gate structure and the third gate structure each include a nitride gate layer and a second metal gate layer from bottom to top.

4. The semiconductor device according to claim 3, characterized in that The first gate structure, the second gate structure and the third gate structure each further include a third metal gate layer, and the third metal gate layer is formed on the first metal gate layer and the second metal gate layer.

5. The semiconductor device according to claim 1, wherein: The semiconductor device further comprises: At least one field plate is formed on the passivation layer in the enhancement mode power device region.

6. The semiconductor device according to any one of claims 1 to 5, wherein: The base includes a substrate, and a buffer layer, a channel layer and a barrier layer formed from bottom to top on the substrate.

7. A method for manufacturing a semiconductor device, characterized in that: include: Providing a substrate, the substrate comprising a depletion-type device region and an enhancement-type device region; forming a second gate structure, a passivation layer and a first gate structure, wherein the second gate structure is formed on the substrate in the enhancement mode device region; The passivation layer is formed on the substrate of the depletion-type device region and the enhancement-type device region, and the passivation layer covers the second gate structure; the first gate structure is formed on the passivation layer of the depletion-type device region, and the passivation layer between the first gate structure and the substrate serves as a gate dielectric layer; A first source metal, a first drain metal, a second source metal and a second drain metal are formed, wherein the first source metal and the first drain metal are formed on the substrate on both sides of the first gate structure, and the second source metal and the second drain metal are formed on the substrate on both sides of the second gate structure.

8. The method for manufacturing a semiconductor device according to claim 7, wherein: The substrate further includes an enhanced power device region, and the method for manufacturing the semiconductor device further includes: forming a third gate structure on the substrate in the enhanced power device region, wherein the passivation layer is also formed on the substrate in the enhanced power device region and the third gate structure; A third source metal and a third drain metal are formed on the substrate at two sides of the third gate structure.

9. The method for manufacturing a semiconductor device according to claim 8, wherein: The steps of forming the second gate structure, the passivation layer, the first gate structure and the third gate structure include: Forming a nitride gate layer and a second metal gate layer stacked on the substrate of the enhancement mode device region and the enhancement mode power device region; Forming a passivation layer on the substrate in the depletion-mode device region, the enhancement-mode device region and the enhancement-mode power device region, wherein the passivation layer covers the nitride gate layer and the second metal gate layer; A first metal gate layer is formed on the passivation layer in the depletion device region, so that the first gate structure includes the first metal gate layer, and the second gate structure and the third gate structure both include the nitride gate layer and the second metal gate layer.

10. The method for manufacturing a semiconductor device according to claim 9, wherein: The steps of forming the second gate structure, the first gate structure and the third gate structure also include: A third metal gate layer is formed on the first metal gate layer and the second metal gate layer, so that the first gate structure, the second gate structure and the third gate structure all further include the third metal gate layer.

11. The method for manufacturing a semiconductor device according to claim 7, wherein: The method for manufacturing the semiconductor device further includes: At least one field plate is formed on the passivation layer in the enhancement mode power device region.

12. The method for manufacturing a semiconductor device according to any one of claims 7 to 11, wherein: The base includes a substrate, and a buffer layer, a channel layer and a barrier layer formed from bottom to top on the substrate.

Citation Information

Patent Citations

  • Semiconductor circuit based on gate protection and semiconductor device

    CN111916451A

  • Integrated enhanced and depletion mode HEMT device and production method thereof

    CN113053826A

  • Integrated enhancement / depletion mode HEMT and method for manufacturing the same

    US20190267469A1

  • Integrated depletion and enhancement mode gallium nitride high-electron mobility transistors

    US20240063219A1