Method for manufacturing CIS
Through a plasma-free deposition process, multi-layer film is formed and side walls are etched to form, which solves the problem of white pixels in the CMOS image sensor chip and improves device performance.
Patent Information
- Application Number
- CN202411048061.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-15
AI Technical Summary
The problem with white pixels in existing CMOS image sensor chips is mainly caused by metal ions and lattice defects, which leads to an increase in the probability of electrons and holes recombination, affecting device performance.
A plasma-free deposition process is used to deposit and deposit multi-layer films on the semiconductor substrate and gate structure surfaces, including oxide layers and silicon nitride layers, and side walls are formed by etching to prevent metal ions from entering the pixel unit area and reduce white pixels. question.
By improving the quality of the film layer, the metal ions introduced in the subsequent process are blocked, the occurrence of white pixels is significantly reduced, and the performance of the CMOS image sensor chip is improved.
Smart Images

Figure CN118969808A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of semiconductor integrated circuit manufacturing, and in particular to a method for manufacturing a CIS. Background Art
[0002] With the continuous development of the semiconductor industry, the integrated circuit manufacturing process is just like Moore's Law (the number of integrated components on a chip doubles approximately every 18 months). The device density continues to increase, and the performance continues to improve. The popularization of computers, communications and consumer electronics has greatly improved economic productivity and quality of life. Among them, CMOS image sensor chips (CIS) are widely used, and the performance requirements of CIS products are also higher.
[0003] White pixel, or WP (White Pixel), is the most important performance parameter of CIS products. It refers to the output higher than the average output of surrounding pixels in a dark field environment. Generally, pixels with a DN value 50DN higher than the surrounding pixels are called white pixels.
[0004] The main reason for the formation of WP is that metal ions or lattice defects form highly active intermediate energy levels, which greatly increase the probability of electron and hole recombination, thus causing the problem of white pixels. Summary of the invention
[0005] The present application provides a method for manufacturing a CIS, which can improve the problem of white pixels in the related art.
[0006] In order to solve the technical problem in the background technology, the present application provides a method for manufacturing a CIS, and the method for manufacturing a CIS comprises the following steps:
[0007] Providing a semiconductor substrate including a pixel unit region, wherein a gate structure is formed on the semiconductor substrate;
[0008] Depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by a deposition process without plasma;
[0009] Depositing a second oxide layer on the first oxide layer by a plasma-free deposition process;
[0010] Depositing a first silicon nitride layer on the second oxide layer by a plasma-free deposition process;
[0011] Etching the first silicon nitride layer, the second oxide layer, and the first oxide layer to form first sidewall spacers located on both sides of the gate structure;
[0012] Depositing a third oxide layer by a plasma-free deposition process, wherein the third oxide layer covers the first sidewall spacer, the semiconductor substrate, and the exposed surface of the gate structure;
[0013] Depositing a second silicon nitride layer on the third oxide layer by a plasma-free deposition process;
[0014] The second silicon nitride layer and the third oxide layer are etched to form a second sidewall spacer covering the first sidewall spacer.
[0015] Optionally, the step of depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by a deposition process without plasma comprises:
[0016] A first oxide layer is deposited on the surface of the semiconductor substrate and the surface of the gate structure by a furnace deposition process.
[0017] Optionally, after the step of depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by a furnace tube deposition process is completed, the following steps are further performed:
[0018] The semiconductor substrate with the first oxide layer is cooled.
[0019] Optionally, the step of depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by a deposition process without plasma comprises:
[0020] A first oxide layer is deposited on the surface of the semiconductor substrate and the surface of the gate structure by an ALD process.
[0021] Optionally, after the step of depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by an ALD process is completed, the following steps are further performed:
[0022] The source drift region and the drain LDD region are lightly doped.
[0023] Optionally, the step of depositing a second oxide layer on the first oxide layer by a plasma-free deposition process comprises:
[0024] The second oxide layer is formed by depositing on the first oxide layer through a furnace tube deposition process, or the second oxide layer is formed by depositing on the first oxide layer through an ALD process.
[0025] Optionally, after the step of depositing the second oxide layer on the first oxide layer by a furnace tube deposition process is completed, the following steps are further performed:
[0026] The semiconductor substrate with the second oxide layer is cooled.
[0027] Optionally, the step of depositing a first silicon nitride layer on the second oxide layer by a plasma-free deposition process comprises:
[0028] The first silicon nitride layer is formed by depositing on the second oxide layer through a furnace deposition process, or the first silicon nitride layer is formed by depositing on the second oxide layer through an ALD process.
[0029] Optionally, after the step of depositing the first silicon nitride layer on the second oxide layer by a furnace deposition process is completed, the following steps are further performed:
[0030] The semiconductor substrate with the first silicon nitride layer is cooled.
[0031] Optionally, the step of depositing a third oxide layer by a deposition process without plasma, wherein the third oxide layer covers the first sidewall spacer, the semiconductor substrate, and the exposed surface of the gate structure, comprises:
[0032] A third oxide layer is deposited by a furnace tube deposition process, and the third oxide layer covers the exposed surface of the first side wall, the semiconductor substrate, and the gate structure, or a third oxide layer is deposited by an ALD process, and the third oxide layer covers the exposed surface of the first side wall, the semiconductor substrate, and the gate structure.
[0033] Optionally, the step of depositing a second silicon nitride layer on the third oxide layer by a plasma-free deposition process comprises:
[0034] The second silicon nitride layer is formed by depositing on the third oxide layer through a furnace deposition process, or the second silicon nitride layer is formed by depositing on the third oxide layer through an ALD process.
[0035] The technical solution of the present application has at least the following advantages: the present application improves the quality of the formed film layer by forming the first oxide layer, the second oxide layer, the first silicon nitride layer, the third oxide layer and the second silicon nitride layer through a deposition process without plasma, thereby avoiding lattice defects caused by plasma on the film layer. The high-quality film layer can block the metal ions introduced in the subsequent process from entering the pixel unit area, thereby reducing the problem of white pixels of the CIS device. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0037] Figure 1 A flow chart of a method for manufacturing a CIS provided in one embodiment of the present application is shown;
[0038] Figure 2 A schematic diagram of the cross-sectional structure of the device after step S2 is completed is shown;
[0039] Figure 3 A schematic diagram of the cross-sectional structure of the device after step S4 is completed is shown;
[0040] Figure 4 A schematic diagram of the cross-sectional structure of the device after step S5 is completed is shown;
[0041] Figure 5 FIG. 4 shows a schematic diagram of a cross-sectional structure of the device after step S7 is completed. DETAILED DESCRIPTION
[0042] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0043] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0044] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0045] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.
[0046] Figure 1A flow chart of a method for manufacturing a CIS according to an embodiment of the present application is shown. Figure 1 As can be seen from the figure, the manufacturing method of the CIS comprises the following steps:
[0047] Step S1: providing a semiconductor substrate including a pixel unit region, wherein a gate structure is formed on the semiconductor substrate.
[0048] Step S2: forming a first oxide layer by deposition on the surface of the semiconductor substrate and the surface of the gate structure through a deposition process without plasma.
[0049] Figure 2 The schematic diagram of the cross-sectional structure of the device after step S2 is completed is shown. Figure 2 As can be seen from the figure, a gate structure 200 is formed on the semiconductor substrate 100 , and a first oxide layer 310 is formed on the side surface of the gate structure 200 .
[0050] Exemplarily, the first oxide layer can be deposited on the surface of the semiconductor substrate and the surface of the gate structure by a furnace tube deposition process. After the first oxide layer is formed by the furnace tube deposition process, the temperature of the semiconductor device rises, which easily causes impurity ion drift in the doping region, thereby affecting the reliability of the device. Therefore, after the step of depositing the first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by the furnace tube deposition process is completed, the semiconductor substrate with the first oxide layer is also cooled to reduce the temperature of the device and weaken the impurity ion drift in the doping region.
[0051] Exemplarily, a first oxide layer may be deposited on the surface of the semiconductor substrate and the surface of the gate structure by an ALD process. Since the film layer produced by the ALD process is likely to cause the device to have a slow response speed, after the step of depositing the first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by an ALD process is completed, a light doping of the source end drift region and the drain end LDD region is performed. The doping concentration of the formed source end drift region 410 and the drain end LDD region 420 is lower than the doping concentration of the source end drift region and the drain end LDD region in conventional operation.
[0052] Step S3: forming a second oxide layer by depositing on the first oxide layer through a deposition process without plasma.
[0053] Illustratively, the second oxide layer may be formed by depositing on the first oxide layer through a furnace deposition process, or the second oxide layer may be formed by depositing on the first oxide layer through an ALD process.
[0054] After the second oxide layer is deposited on the first oxide layer by the furnace tube deposition process, the temperature of the semiconductor device rises, which easily causes impurity ion drift in the doping region, thereby affecting the reliability of the device. Therefore, after the step of depositing the second oxide layer on the first oxide layer by the furnace tube deposition process is completed, the semiconductor substrate with the second oxide layer is also cooled to reduce the temperature of the device and weaken the impurity ion drift in the doping region.
[0055] Step S4: forming a first silicon nitride layer by depositing on the second oxide layer through a plasma-free deposition process.
[0056] Reference Figure 3 , which shows a schematic diagram of the cross-sectional structure of the device after step S4 is completed. Figure 3 As can be seen in FIG. 1 , a second oxide layer 320 is formed on the first oxide layer 310 , and a first silicon nitride layer 330 is deposited on the second oxide layer 320 .
[0057] For example, the first silicon nitride layer may be formed by depositing on the second oxide layer through a furnace deposition process, or the first silicon nitride layer may be formed by depositing on the second oxide layer through an ALD process.
[0058] After the first silicon nitride layer is deposited on the second oxide layer by the furnace tube deposition process, the temperature of the semiconductor device rises, which easily causes impurity ion drift in the doping region, thereby affecting the reliability of the device. Therefore, after the step of depositing the first silicon nitride layer on the second oxide layer by the furnace tube deposition process is completed, the semiconductor substrate with the first silicon nitride layer is also cooled to reduce the temperature of the device and weaken the impurity ion drift in the doping region.
[0059] Step S5: etching the first silicon nitride layer, the second oxide layer, and the first oxide layer to form first sidewall spacers located on both sides of the gate structure.
[0060] Reference Figure 4 , which shows a schematic diagram of the cross-sectional structure of the device after step S5 is completed. Figure 4 It can be seen from the figure that the first spacer 300 composed of the first silicon nitride layer 330, the second oxide layer 320 and the first oxide layer 310 is located on both sides of the gate structure.
[0061] Step S6: forming a third oxide layer by a deposition process without plasma, wherein the third oxide layer covers the first spacer, the semiconductor substrate, and the exposed surface of the gate structure.
[0062] Exemplarily, a third oxide layer can be deposited by a furnace tube deposition process, and the third oxide layer covers the exposed surface of the first side wall, the semiconductor substrate, and the gate structure, or, a third oxide layer can be deposited by an ALD process, and the third oxide layer covers the exposed surface of the first side wall, the semiconductor substrate, and the gate structure.
[0063] After the third oxide layer is formed by the furnace tube deposition process, the temperature of the semiconductor device rises, which easily causes impurity ion drift in the doping area, thereby affecting the reliability of the device. Therefore, after the step of depositing the third oxide layer by the furnace tube deposition process is completed, the semiconductor substrate with the third oxide layer is also cooled to reduce the temperature of the device and weaken the impurity ion drift in the doping area.
[0064] Step S7: forming a second silicon nitride layer by depositing on the third oxide layer through a plasma-free deposition process.
[0065] For example, the second silicon nitride layer may be formed by depositing on the third oxide layer through a furnace deposition process, or the second silicon nitride layer may be formed by depositing on the third oxide layer through an ALD process.
[0066] After the second silicon nitride layer is deposited by the furnace tube deposition process, the temperature of the semiconductor device rises, which easily causes impurity ion drift in the doping region, thereby affecting the reliability of the device. Therefore, after the step of depositing the second silicon nitride layer by the furnace tube deposition process is completed, the semiconductor substrate with the second silicon nitride layer is also cooled to reduce the temperature of the device and weaken the impurity ion drift in the doping region.
[0067] Figure 5 The schematic diagram of the cross-sectional structure of the device after step S7 is completed is shown. Figure 5 It can be seen that the deposited third oxide layer 340 covers the exposed surfaces of the first spacer 300 , the semiconductor substrate 100 , and the gate structure 200 , and the second silicon nitride layer 350 covers the surface of the third oxide layer 340 .
[0068] Step S8: etching the second silicon nitride layer and the third oxide layer to form a second sidewall spacer covering the first sidewall spacer.
[0069] The present application improves the quality of the formed film layers by forming the first oxide layer, the second oxide layer, the first silicon nitride layer, the third oxide layer and the second silicon nitride layer using a plasma-free deposition process, thereby avoiding lattice defects caused by plasma on the film layers. The high-quality film layers can block metal ions introduced in subsequent processes from entering the pixel unit area, thereby reducing the problem of white pixels in the CIS device.
[0070] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection created by this application.
Claims
1. A method for manufacturing a CIS, characterized in that: The manufacturing method of the CIS comprises the following steps: Providing a semiconductor substrate including a pixel unit region, wherein a gate structure is formed on the semiconductor substrate; Depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by a deposition process without plasma; Depositing a second oxide layer on the first oxide layer by a plasma-free deposition process; Depositing a first silicon nitride layer on the second oxide layer by a plasma-free deposition process; Etching the first silicon nitride layer, the second oxide layer, and the first oxide layer to form first sidewall spacers located on both sides of the gate structure; Depositing a third oxide layer by a plasma-free deposition process, wherein the third oxide layer covers the first sidewall spacer, the semiconductor substrate, and the exposed surface of the gate structure; Depositing a second silicon nitride layer on the third oxide layer by a plasma-free deposition process; The second silicon nitride layer and the third oxide layer are etched to form a second sidewall spacer covering the first sidewall spacer.
2. The method for manufacturing a CIS according to claim 1, wherein: The step of depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by a deposition process without plasma comprises: A first oxide layer is deposited on the surface of the semiconductor substrate and the surface of the gate structure by a furnace deposition process.
3. The method for manufacturing a CIS according to claim 2, wherein: After the step of depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by a furnace tube deposition process is completed, the following steps are further performed: The semiconductor substrate with the first oxide layer is cooled.
4. The method for manufacturing a CIS according to claim 1, wherein: The step of depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by a deposition process without plasma comprises: A first oxide layer is deposited on the surface of the semiconductor substrate and the surface of the gate structure by an ALD process.
5. The method for manufacturing a CIS according to claim 4, wherein: After the step of depositing a first oxide layer on the surface of the semiconductor substrate and the surface of the gate structure by the ALD process is completed, the following steps are further performed: The source drift region and the drain LDD region are lightly doped.
6. The method for manufacturing a CIS according to claim 1, wherein: The step of depositing a second oxide layer on the first oxide layer by a plasma-free deposition process comprises: The second oxide layer is formed by depositing on the first oxide layer through a furnace tube deposition process, or the second oxide layer is formed by depositing on the first oxide layer through an ALD process.
7. The method for manufacturing a CIS according to claim 6, wherein: After the step of depositing the second oxide layer on the first oxide layer by the furnace tube deposition process is completed, the following steps are further performed: The semiconductor substrate with the second oxide layer is cooled.
8. The method for manufacturing a CIS according to claim 1, wherein: The step of depositing a first silicon nitride layer on the second oxide layer by a plasma-free deposition process comprises: The first silicon nitride layer is formed by depositing on the second oxide layer through a furnace deposition process, or the first silicon nitride layer is formed by depositing on the second oxide layer through an ALD process.
9. The method for manufacturing a CIS according to claim 8, wherein: After the step of depositing the first silicon nitride layer on the second oxide layer by the furnace deposition process is completed, the following steps are further performed: The semiconductor substrate with the first silicon nitride layer is cooled.
10. The method for manufacturing a CIS according to claim 1, wherein: The step of depositing a third oxide layer by a plasma-free deposition process, wherein the third oxide layer covers the first sidewall spacer, the semiconductor substrate, and the exposed surface of the gate structure, comprises: A third oxide layer is deposited by a furnace tube deposition process, and the third oxide layer covers the exposed surface of the first side wall, the semiconductor substrate, and the gate structure, or a third oxide layer is deposited by an ALD process, and the third oxide layer covers the exposed surface of the first side wall, the semiconductor substrate, and the gate structure.
11. The method for manufacturing a CIS according to claim 1, wherein: The step of depositing a second silicon nitride layer on the third oxide layer by a plasma-free deposition process comprises: The second silicon nitride layer is formed by depositing on the third oxide layer through a furnace deposition process, or the second silicon nitride layer is formed by depositing on the third oxide layer through an ALD process.