Cured film forming method, method for manufacturing substrate for imprint mold, method for manufacturing imprint mold, method for manufacturing resistant structure, method for forming pattern, method for forming hard mask, method for forming insulating film, and method for manufacturing semiconductor device
By using a curable resin with siloxane bond and polymerizable functional groups to form a protective film, the problem of damage to the light shielding part of the imprint mold during the etching and cleaning process is solved, and a simpler process and higher stability are achieved.
Patent Information
- Application Number
- CN202380031542.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-31
- Filing Date
- 2023-03-24
- Publication Date
- 2024-11-15
AI Technical Summary
During the etching process and cleaning process of the existing imprint mold, the light-shielding part is easily damaged, which makes it unable to effectively play the role of a protective film, and the process of forming a protective film is complicated.
Using a curable resin containing silicone bonds and polymerizable functional groups, the organic components are decomposed by plasma treatment or oxidation treatment to form a protective film, and the curable resin is supplied to the non-patterned parts of the imprint mold to form a protective film to ensure light shading. protection of department.
The protective film is formed more easily, the process complexity is reduced, the damage resistance of the light shielding part is improved, and the stability and functionality of the imprint mold in the manufacturing process are ensured.
Smart Images

Figure CN118974885A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for forming a cured film, a method for manufacturing a substrate for an imprint mold, a method for manufacturing an imprint mold, a method for manufacturing a concave-convex structure, a method for forming a pattern, a method for forming a hard mask, a method for forming an insulating film, and a method for manufacturing a semiconductor device. Background Art
[0002] In the manufacture of semiconductor devices, nanoimprint lithography is known as a technology for transferring fine patterns. Nanoimprint lithography is a technology that allows an imprint mold with a transfer pattern of fine concave and convex shapes formed on the surface to contact with a resin supplied to a transferred substrate such as a semiconductor wafer, and then solidifies the resin to transfer the concave and convex shapes of the transfer pattern of the imprint mold to the resin. As methods of nanoimprint lithography, there are hot imprinting methods that use thermal energy to transfer the concave and convex shapes of the transfer pattern to the resin, and photoimprinting methods that solidify the resin by exposure. In applications that require high alignment accuracy, photoimprinting methods that are not affected by expansion and contraction caused by heating are mainly used.
[0003] In the imprint mold used for nanoimprint lithography, a mesa-like height difference structure is provided on the main surface of the base so that only a specified area (pattern area) of the transfer pattern formed with a concave-convex shape is in contact with the resin supplied to the transferred substrate, and a transfer pattern is formed on the upper surface of the mesa-like height difference structure. It should be noted that in the imprint mold of such a structure, the upper surface of the mesa-like height difference structure becomes the pattern area. The height difference of the mesa-like height difference structure (the height from the main surface of the base to the upper surface of the height difference structure) is determined by the mechanical accuracy of the imprint device used, but is usually about 30μm.
[0004] In addition, if the pattern density of the transfer pattern in the imprint mold increases, the close contact area between the imprint mold and the resin increases, so when the imprint mold and the resin are demolded, a force is required to counteract the friction between the two. In particular, the transfer pattern for semiconductor use has a small size (dimension) and a high pattern density, so demolding requires a large force. Therefore, the following method is known: by forming a recessed portion on the back side of the imprint mold (the side opposite to the side where the transfer pattern is formed), the thickness of the template of the specified area (including the pattern area) where the transfer pattern is formed becomes thinner and easier to bend, and when demolding, the pattern area of the imprint mold is convexly bent toward the side of the transferred substrate, and the outer edge of the transfer area is sequentially partially demolded.
[0005] In the photoimprinting method, in order to suppress the unintentional solidification of the resin in the non-transfer area located outside the area where the transfer pattern is transferred, it is proposed to form a second height difference structure on the first height difference structure of the imprinting mold, and to provide a shading portion in the non-pattern portion (a portion different from the transfer pattern area) of the upper surface of the first height difference structure, which is the area outside the second height difference structure (see patent document 1).
[0006] Prior art literature
[0007] Patent Literature
[0008] Patent Document 1: Japanese Patent Application Publication No. 2018-56545
[0009] Patent Document 2: International Publication No. 2020 / 203472 Pamphlet Summary of the invention
[0010] Problems to be solved by the invention
[0011] An imprint mold having a first height difference structure and a second height difference structure and having a shading portion in a non-pattern portion (a portion different from a transfer pattern region) is manufactured, for example, by preparing an imprint mold substrate having a second height difference structure on the first height difference structure, and after forming a transfer pattern in the transfer pattern region, forming a shading portion in the non-pattern portion (refer to patent document 1). If a shading portion is provided in the non-pattern portion of the imprint mold substrate having the first height difference structure and the second height difference structure, and a transfer pattern is formed in the transfer pattern region of the imprint mold substrate, the shading portion may sometimes be damaged in the etching process, the cleaning process, etc. in the process of manufacturing the above-mentioned imprint mold, and therefore, the shading portion in the manufactured imprint mold may not be able to perform the desired function. In order to solve such a problem, it is considered to form a protective film on the shading portion to suppress damage to the shading portion, but in order to form a protective film on the shading portion only provided in the non-pattern portion such as the imprint mold substrate, for example, it is necessary to go through processes such as sputtering and patterning, and the process of forming the shading portion is cumbersome.
[0012] In view of the above-mentioned problems, the object of the present invention is to provide: a cured film forming method that can form a cured film that can be used as a protective film such as the above-mentioned in a simpler way, and a manufacturing method for a substrate for an imprint mold, a manufacturing method for an imprint mold, a manufacturing method for a concave-convex structure, a pattern forming method, a hard mask forming method, an insulating film forming method and a manufacturing method for a semiconductor device using the cured film forming method.
[0013] Means for solving problems
[0014] To achieve such an object, as one embodiment of the present invention, there is provided a method for forming a cured film, comprising: a step of supplying a curable resin to a substrate, the curable resin comprising a polymerizable compound having a siloxane bond in a molecule and at least one polymerizable functional group, a polymerization initiator, and a reactive crosslinking agent; a step of curing the curable resin; and a step of subjecting the cured curable resin to a plasma treatment or an oxidation treatment to decompose an organic component contained in the curable resin so that a siloxane polymerized portion remains, thereby forming a cured film.
[0015] The polymerizable compound may have a spherical structure in which the polymerizable functional group extends outward from the siloxane polymer portion as the center.
[0016] The ratio of oxygen atoms bonded to a single silicon atom among oxygen atoms bonded to silicon atoms contained in the polymerizable compound may be 10 mol % or less, and the curable resin may contain substantially no solvent and have a viscosity of 20 cPs or less.
[0017] The content of the reactive crosslinking agent in the curable resin may be 49% by mass to 79% by mass.
[0018] The process of curing the curable resin may include: a contact process of bringing the mold close to the substrate to allow the curable resin to expand between the substrate and the mold to form a formed resin layer; a curing process of curing the formed resin layer; and a demolding process of detaching the mold from the cured formed resin layer.
[0019] The amount of the curable resin supplied to the substrate can be determined based on the following mathematical formula (1) which represents the relationship between the thickness T0 of the resin layer to be formed, the thickness T of the cured film, and the decomposition treatment time t for decomposing the organic component.
[0020] [Number 1]
[0021]
[0022] In the above mathematical formula (1), Ab ct represents "the amount of reduction per unit time of the film thickness of the formed resin layer in the initial stage of the decomposition treatment of the above-mentioned organic component that varies with the above-mentioned decomposition treatment time t", αt represents "the amount of reduction per unit time of the film thickness of the above-mentioned formed resin layer that does not substantially vary with the above-mentioned decomposition treatment time t", A represents "the amount of reduction per unit time of the film thickness of the above-mentioned formed resin layer in the initial stage of the decomposition treatment of the above-mentioned organic component", b and c are "coefficients representing the reduction of the exponential function of the film thickness of the above-mentioned formed resin layer", b>1 and c<0.
[0023] It may be that a cured film forming region where the cured film is formed and a cured film non-forming region where the cured film is not formed are set on the substrate, and the curable resin is supplied to the cured film forming region in an amount determined based on the mathematical formula (1) so that the thickness T of the cured film exceeds 0, and the curable resin is supplied to the cured film non-forming region in an amount determined based on the mathematical formula (1) so that the thickness T of the cured film becomes less than 0.
[0024] It may be that the mold has a concave-convex structure including a concave portion, the formed resin layer has a transfer structure and a residual film portion, the transfer structure includes a convex portion to which the concave portion of the concave-convex structure is transferred, and the amount of the curable resin supplied to the substrate is determined based on the depth of the concave portion of the concave-convex structure and the thickness of the residual film portion, as well as the mathematical formula (1).
[0025] It can be that the above-mentioned mold has a concave-convex structure with a minimum size of less than 100nm, and the above-mentioned formed resin layer has a transfer structure on which the above-mentioned concave-convex structure is transferred, so that the above-mentioned cured film has a pattern with a size smaller than the minimum size of the above-mentioned concave-convex structure; or it can be that the above-mentioned substrate has a first surface and a second surface located on the opposite side of the first surface, and the above-mentioned substrate has at least one material layer made of a material different from the material of the above-mentioned substrate on at least the above-mentioned first surface, and the above-mentioned curable resin is supplied to the above-mentioned material layer.
[0026] As one embodiment of the present invention, a cured film is provided, which is a cured film formed by the above-mentioned cured film forming method, and has a concentration gradient in which the concentration of silicon (Si) atoms is highest near the surface of the cured film and the concentration of silicon (Si) atoms is lowest near the substrate in the composition distribution along the thickness direction of the cured film.
[0027] The composition distribution along the thickness direction of the cured film may have a concentration distribution in which the concentration of carbon (C) atoms is lowest near the surface of the cured film and is highest near the substrate.
[0028] As one embodiment of the present invention, a method for manufacturing a substrate for an imprint mold is provided, which comprises: a process of preparing a multi-stage mold substrate, wherein the multi-stage mold substrate comprises a base, a first height difference structure, a second height difference structure and a light shielding film, wherein the base has a first surface and a second surface located on the opposite side of the first surface, the first height difference structure protrudes from the first surface of the base, the second height difference structure protrudes from the upper surface of the first height difference structure, and the light shielding film is located on the upper surface of the first height difference structure; supplying a curable resin to the light shielding film and the upper surface of the second height difference structure to form a first curable resin layer on the light shielding film, and forming a second curable resin layer on the upper surface of the second height difference structure The invention relates to a process for forming a first curable resin layer and a second curable resin layer, wherein the curable resin comprises a polymerizable compound having a siloxane bond in a molecule and at least one polymerizable functional group, a polymerization initiator and a reactive cross-linking agent; and a process for subjecting the first curable resin layer and the second curable resin layer after curing to a plasma treatment or an oxidation treatment to decompose the organic components contained in the curable resin so that the siloxane polymerization part remains, thereby forming a protective film on the light-shielding film, and removing the second curable resin layer, wherein the thickness of the second curable resin layer is less than that of the first curable resin layer and is a thickness that is removed during the formation of the protective film.
[0029] The method may include forming a light shielding material layer on the upper surface of the second height difference structure of the multi-stage mold substrate, and removing the light shielding material layer by etching after removing the second curable resin layer.
[0030] As one embodiment of the present invention, a method for manufacturing an imprint mold is provided, which includes: a process of forming a first hard mask layer on the above-mentioned protective film of the imprint mold substrate manufactured by the above-mentioned method, and forming a second hard mask layer on the upper surface of the above-mentioned second height difference structure; a process of forming a mask pattern on the above-mentioned second hard mask layer; a process of etching the above-mentioned second hard mask layer by using the above-mentioned mask pattern as a mask, thereby forming a hard mask pattern on the upper surface of the above-mentioned second height difference structure, and removing the above-mentioned first hard mask layer; and a process of etching the upper surface of the above-mentioned second height difference structure by using the above-mentioned hard mask pattern as a mask, thereby forming a concave-convex pattern on the upper surface of the above-mentioned second height difference structure, and removing the above-mentioned protective film.
[0031] As one embodiment of the present invention, there is provided a method for manufacturing a concave-convex structure, characterized in that it comprises: a process of preparing a substrate having a first surface and a second surface located on the opposite side of the first surface; a process of forming a core material pattern having a convex pattern on the above-mentioned first surface; a process of supplying a curable resin to the above-mentioned core material pattern, wherein the curable resin comprises a polymerizable compound having a siloxane bond and at least one polymerizable functional group in the molecule, a polymerization initiator and a reactive cross-linking agent; a process of contacting a template with the above-mentioned curable resin supplied to the above-mentioned core material pattern and curing the same, thereby forming a solid The process of forming a curable resin layer, wherein the curable resin layer covers the top and side wall of the above-mentioned convex pattern of the above-mentioned core material pattern, and the above-mentioned first surface exposed from between adjacent above-mentioned convex patterns; subjecting the portion of the above-mentioned curable resin layer covering the side wall of the above-mentioned convex pattern to plasma treatment or oxidation treatment, decomposing the organic components contained in the above-mentioned curable resin to leave the siloxane polymerization part, and removing the portion covering the top of the above-mentioned convex pattern and the portion covering the above-mentioned first surface exposed from between adjacent above-mentioned convex patterns, thereby forming a side wall pattern; and the process of removing the above-mentioned core material pattern.
[0032] As one embodiment of the present invention, a pattern forming method is provided, which comprises: a step of preparing a substrate having a first surface and a second surface located on the opposite side of the first surface; a step of discretely dropping a curable resin onto the first surface of the substrate, wherein the curable resin comprises a polymerizable compound having a siloxane bond in a molecule and at least one polymerizable functional group, a polymerization initiator, and a reactive cross-linking agent; a step of curing the discretely dropped curable resin; and a step of performing a plasma treatment or an oxidation treatment on the cured curable resin to decompose the organic component contained in the curable resin and leave a siloxane polymerization part, thereby forming a cured film pattern.
[0033] As one embodiment of the present invention, a pattern forming method is provided, which comprises: a step of preparing a substrate having a first surface and a second surface located on the opposite side of the first surface; a step of supplying a curable resin to the first surface of the substrate, wherein the curable resin comprises a polymerizable compound having a siloxane bond in a molecule and having at least one polymerizable functional group, a polymerization initiator and a reactive cross-linking agent; a step of bringing a mold close to the substrate and curing the curable resin spread between the substrate and the mold to form a formed resin layer; a step of separating the mold from the formed resin layer; a step of forming a resist layer having a thickness distribution on the formed resin layer; a step of etching the formed resin layer using the resist layer as a mask to form a resin pattern; and a step of performing a plasma treatment or an oxidation treatment on the resin pattern to decompose the organic component contained in the curable resin and leave the siloxane polymerization part to form a cured film pattern.
[0034] As one embodiment of the present invention, a hard mask forming method is provided, which is a method for forming a hard mask in an arbitrary area on a substrate formed with a metal film, the hard mask forming method comprising: a process of supplying a curable resin onto the above-mentioned metal film, the curable resin comprising a polymerizable compound having a siloxane bond in a molecule and having at least one polymerizable functional group, a polymerization initiator and a reactive cross-linking agent; a process of bringing a mold close to the above-mentioned substrate to cure the above-mentioned curable resin spread between the above-mentioned substrate and the above-mentioned mold, thereby forming a formed resin layer; and a process of subjecting the above-mentioned formed resin layer to plasma treatment or oxidation treatment to decompose the organic components contained in the above-mentioned curable resin to leave the siloxane polymerization part, thereby forming a hard mask.
[0035] As one embodiment of the present invention, an insulating film forming method is provided, which is a method for forming an insulating film in an insulating film forming region on a substrate, the insulating film forming method comprising: a process of supplying a curable resin to the above-mentioned insulating film forming region, the curable resin comprising a polymerizable compound having a siloxane bond in a molecule and at least one polymerizable functional group, a polymerization initiator and a reactive cross-linking agent; a process of curing the above-mentioned curable resin; and a process of performing plasma treatment or oxidation treatment on the above-mentioned cured curable resin to decompose the organic components contained in the above-mentioned curable resin and leave the siloxane polymerization part, thereby forming the above-mentioned insulating film.
[0036] As one embodiment of the present invention, a method for manufacturing a semiconductor device is provided, wherein the semiconductor device has the following structure: on the first surface side of a substrate having a first surface and a second surface located on the opposite side of the first surface, a semiconductor layer, an insulating film and a wiring are stacked in sequence from the first surface side, and the manufacturing method includes: a process of forming the semiconductor layer on the first surface, the semiconductor layer having a channel region and a source / drain region, the source / drain region including a contact portion contacting the wiring; and a process of forming the insulating film on the channel region and the region other than the contact portion by the above-mentioned method.
[0037] Effects of the Invention
[0038] According to the present invention, there can be provided a method for forming a cured film which can be used as a protective film such as the above-mentioned in a simpler way, and a method for manufacturing a substrate for an imprint mold, a method for manufacturing an imprint mold, a method for manufacturing a concave-convex structure, a pattern forming method, a hard mask forming method, a method for forming an insulating film, and a method for manufacturing a semiconductor device using the cured film forming method. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1AIt is a cut end view schematically showing one step of the cured film forming method according to one embodiment of the present invention.
[0040] Figure 1B The following is a schematic diagram showing the steps of a cured film forming method according to one embodiment of the present invention. Figure 1A A cutting end view of a process.
[0041] Figure 1C The following is a schematic diagram showing the steps of a cured film forming method according to one embodiment of the present invention. Figure 1B A cutting end view of a process.
[0042] Figure 1D The following is a schematic diagram showing the steps of a cured film forming method according to one embodiment of the present invention. Figure 1C A cutting end view of a process.
[0043] Figure 2A It is a cut end view schematically showing one step of another mode of the cured film forming method according to one embodiment of the present invention.
[0044] Figure 2B This is a schematic diagram showing another aspect of the cured film forming method according to one embodiment of the present invention. Figure 2A A cutting end view of a process.
[0045] Figure 2C This is a schematic diagram showing another aspect of the cured film forming method according to one embodiment of the present invention. Figure 2B A cutting end view of a process.
[0046] Figure 2D This is a schematic diagram showing another aspect of the cured film forming method according to one embodiment of the present invention. Figure 2C A cutting end view of a process.
[0047] Figure 3A It is a cut end view schematically showing one step of a method for producing a substrate for an imprint mold according to one embodiment of the present invention.
[0048] Figure 3B The following is a schematic diagram showing a method for manufacturing an imprint mold substrate according to an embodiment of the present invention. Figure 3A A cutting end view of a process.
[0049] Figure 3C The following is a schematic diagram showing a method for manufacturing an imprint mold substrate according to an embodiment of the present invention. Figure 3B A cutting end view of a process.
[0050] Figure 3DThe following is a schematic diagram showing a method for manufacturing an imprint mold substrate according to an embodiment of the present invention. Figure 3C A cutting end view of a process.
[0051] Figure 3E The following is a schematic diagram showing a method for manufacturing an imprint mold substrate according to an embodiment of the present invention. Figure 3D A cutting end view of a process.
[0052] Figure 3F The following is a schematic diagram showing a method for manufacturing an imprint mold substrate according to an embodiment of the present invention. Figure 3E A cutting end view of a process.
[0053] Figure 4A This is a cut end view schematically showing one step of a method for producing an imprint mold according to one embodiment of the present invention.
[0054] Figure 4B The following is a schematic diagram of a method for manufacturing an imprint mold according to an embodiment of the present invention. Figure 4A A cutting end view of a process.
[0055] Figure 4C The following is a schematic diagram of a method for manufacturing an imprint mold according to an embodiment of the present invention. Figure 4B A cutting end view of a process.
[0056] Figure 4D The following is a schematic diagram of a method for manufacturing an imprint mold according to an embodiment of the present invention. Figure 4C Cutting end view of a process.
[0057] Figure 4E The following is a schematic diagram of a method for manufacturing an imprint mold according to an embodiment of the present invention. Figure 4D A cutting end view of a process.
[0058] Figure 4F The following is a schematic diagram of a method for manufacturing an imprint mold according to an embodiment of the present invention. Figure 4F A cutting end view of a process.
[0059] Figure 5A It is a cut end view schematically showing one step of a method for producing a concavo-convex structure body according to one embodiment of the present invention.
[0060] Figure 5B The following is a schematic diagram of a method for manufacturing a concavo-convex structure body according to an embodiment of the present invention. Figure 5A A cutting end view of a process.
[0061] Figure 5CThe following is a schematic diagram of a method for manufacturing a concavo-convex structure body according to an embodiment of the present invention. Figure 5B A cutting end view of a process.
[0062] Figure 5D The following is a schematic diagram of a method for manufacturing a concavo-convex structure body according to an embodiment of the present invention. Figure 5C A cutting end view of a process.
[0063] Figure 5E The following is a schematic diagram of a method for manufacturing a concavo-convex structure body according to an embodiment of the present invention. Figure 5D Cutting end view of a process.
[0064] Fig. 6A It is a process of a method for manufacturing a concavo-convex structure body as one embodiment of the present invention. Figure 5A A top view of the process is shown.
[0065] Figure 6B It is a process of a method for manufacturing a concavo-convex structure body as one embodiment of the present invention. Figure 5B A top view of the process is shown.
[0066] Figure 6C It is a process of a method for manufacturing a concavo-convex structure body as one embodiment of the present invention. Figure 5C A top view of the process is shown.
[0067] Fig.6D It is a process of a method for manufacturing a concavo-convex structure body as one embodiment of the present invention. Figure 5D A top view of the process is shown.
[0068] Fig. 6E It is a process of a method for manufacturing a concavo-convex structure body as one embodiment of the present invention. Figure 5E A top view of the process is shown.
[0069] Fig. 7A This is a cut end view schematically showing one step of a pattern forming method according to one embodiment of the present invention.
[0070] Figure 7B The following is a schematic diagram showing a pattern forming method according to an embodiment of the present invention. Fig. 7A A cutting end view of a process.
[0071] Fig. 8A This is a cut end view schematically showing one step of another mode of the pattern forming method according to one embodiment of the present invention.
[0072] Figure 8BA schematic diagram of another embodiment of the pattern forming method of the present invention is shown in the following Fig. 8A A cutting end view of a process.
[0073] Figure 8C A schematic diagram of another embodiment of the pattern forming method of the present invention is shown in the following Figure 8B A cutting end view of a process.
[0074] Fig. 9A This is a cut end view schematically showing one step of a method for manufacturing a semiconductor device according to one embodiment of the present invention.
[0075] Fig. 9B The following is a schematic diagram of a method for manufacturing a semiconductor device according to an embodiment of the present invention. Fig. 9A A cutting end view of a process.
[0076] Fig.10 It is a graph showing the results of Example 1, Reference Example 1 and Reference Example 2. DETAILED DESCRIPTION
[0077] Embodiments of the present invention will be described with reference to the drawings.
[0078] In the accompanying drawings, for easy understanding, the shape, scale, aspect ratio, etc. of each part are sometimes changed from the real object or exaggeratedly shown. In this specification, etc., the numerical range represented by "~" refers to the range of each numerical value recorded before and after the "~" as the lower limit and upper limit. In this specification, etc., the terms such as "film", "sheet", "plate" are not distinguished from each other based on the difference in the name. For example, "plate" is a concept that also includes components that can be generally called "sheet" or "film".
[0079] [Cured Film Formation Method]
[0080] The method for forming a cured film of the present embodiment includes the step of supplying a curable resin 2 to a substrate 3 (see Figure 1A , Figure 2A ); a step of curing the curable resin 2 (refer to Figure 1B , Figure 1C , Figure 2B , Figure 2C );And the step of forming a cured film 1 (refer to Figure 1D , Figure 2D ).
[0081] The curable resin 2 in this embodiment includes a polymerizable compound having an organic component and an inorganic component in the molecule. The inorganic component contains SiO X(X is 1 or more), and the polymerizable compound only needs to have a siloxane bond as an inorganic component and only needs to have at least one polymerizable functional group.
[0082] For the polymerizable compound contained in the curable resin 2 in the present embodiment, the ratio of oxygen atoms bonded to a single silicon atom among oxygen atoms bonded to silicon atoms contained in the polymerizable compound may be 10 mol% or less. As the polymerizable compound, polymers, oligomers, etc. having tetrafunctional silane, trifunctional silane, difunctional silane, and monofunctional silane as structural units may be used alone or in combination of multiple types.
[0083] In the present embodiment, it is preferable to use a resin mainly containing trifunctional silane and difunctional silane as structural units, in view of the desired properties of the curable resin 2 .
[0084] In the polymerizable compound of this embodiment, the ratio of oxygen atoms bonded to a single silicon atom among oxygen atoms bonded to silicon atoms contained in the polymerizable compound may be 10 mol % or less, preferably 7 mol % or less, and particularly preferably 5 mol % or less.
[0085] The oxygen atom bonded to a single silicon atom refers to an oxygen atom in which one of the two bonds of the oxygen atom is bonded to silicon, and refers to an oxygen atom in which both of the two bonds of the oxygen atom are not bonded to silicon. The other bond of the oxygen atom is not particularly limited as long as it is bonded to a group other than silicon, and is particularly preferably bonded to hydrogen or an alkyl group having 1 to 4 carbon atoms.
[0086] In this embodiment, by making the ratio of oxygen atoms bonded to a single silicon atom as described above, that is, the ratio of highly reactive functional groups such as hydroxyl (-OH) and alkoxy (-OR, R is an alkyl group having 1 to 4 carbon atoms) bonded to silicon atoms within the above range, the stability of the curable resin over time can be improved, and the thickening during storage can be suppressed. In addition, for the same reason, the reaction with the surface of the flat mold described later can also be suppressed, thereby achieving an excellent effect of peeling off the flat mold.
[0087] The reason why the highly reactive functional group exists in a certain proportion in the polymerizable compound is presumed to be unreacted oxygen atoms remaining in the manufacturing process of the polymerizable compound. As the reason for the remaining unreacted oxygen atoms, when the highly reactive functional group is an alkoxy group (-OR, R is an alkyl group having 1 to 4 carbon atoms), it is believed that the hydrolysis of the alkoxy group of the raw material has not proceeded, and when the highly reactive functional group is a hydroxyl group (-OH), it is believed that the polymerization reaction has not been completely carried out due to steric hindrance or the like.
[0088] In this embodiment, the ratio of oxygen atoms bonded to a single silicon atom represents the number of oxygen atoms bonded to a single silicon atom when the number of oxygen atoms bonded to silicon atoms of the polymerizable compound is 100. The ratio can be determined by using 29 The value was calculated by analyzing the spectrum with Si-NMR.
[0089] Specifically, when a polymerizable compound including a siloxane structure having a trifunctional silane as a structural unit is analyzed using NMR, four peaks are observed: a component in which none of the three oxygen atoms bonded to a silicon atom is bonded to other silicon atoms, a component in which one of the three oxygen atoms bonded to a silicon atom is bonded to other silicon atoms, a component in which two of the three oxygen atoms bonded to a silicon atom are bonded to other silicon atoms, and a component in which all of the three oxygen atoms bonded to a silicon atom are bonded to other silicon atoms.
[0090] The value obtained by integrating the four peaks, that is, the ratio of the respective areas is defined as T 0 ~T 3 In the case of , the ratio (mol %) of oxygen atoms bonded to a single silicon atom can be calculated according to the following formula (2).
[0091] [Number 2]
[0092]
[0093] In addition, when the polymerizable compound contains a siloxane structure having a difunctional silane as a structural unit, three peaks are observed: a component in which both of the two oxygen atoms bonded to the silicon atom are not bonded to other silicon atoms, a component in which one of the two oxygen atoms bonded to the silicon atom is bonded to other silicon atoms, and a component in which both of the two oxygen atoms bonded to the silicon atom are bonded to other silicon atoms.
[0094] The value obtained by integrating the three peaks, that is, the ratio of the respective areas is defined as D 0 ~D 2 In the case of , the ratio (mol %) of oxygen atoms bonded to a single silicon atom can be calculated according to the following formula (3).
[0095] [Number 3]
[0096]
[0097] Furthermore, when the polymerizable compound contains a siloxane structure having a tetrafunctional silane as a structural unit, five peaks are observed: a component in which none of the four oxygen atoms bonded to a silicon atom are bonded to other silicon atoms, a component in which one of the four oxygen atoms bonded to a silicon atom is bonded to other silicon atoms, a component in which two of the four oxygen atoms bonded to a silicon atom are bonded to other silicon atoms, a component in which three of the four oxygen atoms bonded to a silicon atom are bonded to other silicon atoms, and a component in which all of the four oxygen atoms bonded to a silicon atom are bonded to other silicon atoms.
[0098] The value obtained by integrating the five peaks, that is, the ratio of the respective areas, is defined as Q 0 ~Q 4 In the case of , the ratio (mol %) of oxygen atoms bonded to a single silicon atom can be calculated according to the following formula (4).
[0099] [Number 4]
[0100]
[0101] For example, when the curable resin 2 contains the polymerizable compound having two structural units of trifunctional silane and difunctional silane, the ratio (mol %) of oxygen atoms bonded to a single silicon atom can be calculated from the following formula (5).
[0102] [Number 5]
[0103]
[0104] The weight average molecular weight (Mw) of the polymerizable compound may be within a range of 500 to 100,000, preferably 600 to 50,000, and particularly preferably 700 to 20,000.
[0105] The weight average molecular weight (Mw) is a polystyrene-equivalent molecular weight measured by gel permeation chromatography (GPC), and is a value measured under the following conditions after pressure filtration using a membrane filter having a pore size of 0.2 μm.
[0106] (condition)
[0107] ·Device: Water 2695
[0108] Sample volume: about 10 mg of sample per 3 mL of solvent
[0109] Injection volume: 5μL
[0110] Guard column: LF-G (Shodex)
[0111] Column: GPC LF-804×3 (Shodex)
[0112] Column temperature: 40℃
[0113] Mobile phase: tetrahydrofuran
[0114] Flow rate: 1.0mL / min
[0115] Detector: Differential refractometer (Water 2414)
[0116] Molecular weight calibration: polystyrene conversion
[0117] The polymerizable compound has a polymerizable functional group constituting at least a part of the organic component. The polymerizable functional group is a functional group capable of undergoing a polymerization reaction, and is not particularly limited as long as the polymerization reaction is carried out by external stimulation. For example, acryloyl, methacryloyl, acryloyloxy, methacryloyloxy, epoxy, oxetane, vinyl ether, etc., which undergo a polymerization reaction by light irradiation, heat, heat accompanying light irradiation, the action of a photoacid generator, etc., can be used. If it is such a polymerizable functional group, the stability during synthesis and storage, the reactivity during curing are good, and the raw materials are easy to obtain.
[0118] In the present embodiment, from the viewpoint of the curing speed and the wide range of the selection of physical properties, an acryloyl group and a methacryloyl group are particularly preferred.
[0119] In the polymerizable compound, when the polymerizable group directly bonded to the silicon atom is bulky, if the reactivity changes due to steric hindrance, sometimes affecting the curability, etc., the molecular weight of the polymerizable group directly bonded to the silicon atom can be in the range of 20 to 500, preferably in the range of 25 to 400. It should be noted that in the present embodiment, the polymerizable group refers to a group containing a polymerizable functional group. As such a polymerizable group, as a preferred embodiment, the structure shown below can be cited.
[0120] [Chemical formula 1]
[0121]
[0122] R1 represents "a substituted or unsubstituted alkyl chain having 1 to 10 carbon atoms", and R2 represents "a substituted or unsubstituted alkyl chain having 1 to 3 carbon atoms, or a hydrogen atom". In addition, both R1 and R2 may be linear or branched.
[0123] It is sufficient that at least one of the polymerizable functional groups is bonded to the structural unit of the polymerizable compound, but the present invention is not limited thereto, and a structure in which two or more polymerizable functional groups are bonded may be used.
[0124] As the structural unit having a polymerizable group of the polymerizable compound in the present embodiment, for example, the following structural units can be mentioned.
[0125] Examples of the trifunctional structural unit include 3-acryloxypropyltrimethoxysilane, 3-acryloxypropyltriethoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-methacryloxypropyltriethoxysilane, vinyltrimethoxysilane, vinyltriethoxysilane, allyltrimethoxysilane, allyltriethoxysilane, styryltrimethoxysilane, styryltriethoxysilane, 3-glycidoxypropyltrimethoxysilane, 3-glycidoxypropyltriethoxysilane, 2-(3,4-epoxycyclohexyl)ethyltrimethoxysilane, 2-(3,4-epoxycyclohexyl)ethyltriethoxysilane, 3-ethyl-3-[3'-(trimethoxysilyl)propyl]methyloxetane, 3-ethyl-3-[3'-(triethoxysilyl)propyl]methyloxetane, 3-(3'-(trimethoxysilyl)propyl]methyloxetane, etc., among which 3-acryloxypropyltrimethoxysilane, 3-acryloxypropyltriethoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-methacryloxypropyltriethoxysilane, vinyltrimethoxysilane, vinyltriethoxysilane, 3-glycidoxypropyltrimethoxysilane, 3-glycidoxypropyltriethoxysilane, 2-(3,4-epoxycyclohexyl)ethyltrimethoxysilane, 2-(3,4-epoxycyclohexyl)ethyltriethoxysilane, 3-ethyl-3-[3'-(trimethoxysilyl)propyl]methyloxetane, 3-ethyl-3-[3'-(triethoxysilyl)propyl]methyloxetane, etc. are preferably used.
[0126] Examples of the bifunctional structural unit include 3-acryloxypropyl(methyl)dimethoxysilane, 3-acryloxypropyl(methyl)diethoxysilane, 3-methacryloxypropyl(methyl)dimethoxysilane, 3-methacryloxypropyl(methyl)diethoxysilane, vinyl(methyl)dimethoxysilane, vinyl(methyl)diethoxysilane, allyl(methyl)dimethoxysilane, allyl(methyl)diethoxysilane, styryl(methyl)dimethoxysilane, styryl(methyl)diethoxysilane, silane, 3-glycidoxypropylmethyldiethoxysilane, 3-glycidoxypropylmethyldimethoxysilane, 2-(3,4-epoxycyclohexyl)ethyl(methyl)dimethoxysilane, 2-(3,4-epoxycyclohexyl)ethyl(methyl)diethoxysilane, 3-ethyl-3-[3'-(methyldimethoxysilyl)propyl]methyloxetane, 3-ethyl-3-[3'-(methyldiethoxysilyl)propyl]methyloxetane, dimethoxymethylvinylsilane, diethoxymethylvinylsilane, etc. Among them, 3-acryloxypropyl(methyl)dimethoxysilane, 3-acryloxypropyl(methyl)diethoxysilane, 3-methacryloxypropyl(methyl)dimethoxysilane, 3-methacryloxypropyl(methyl)diethoxysilane, vinyl(methyl)dimethoxysilane, vinyl(methyl)diethoxysilane, 3-glycidoxypropylmethyldiethoxysilane, 3-glycidoxypropylmethyldimethoxysilane, 2-(3,4-epoxycyclohexyl)ethyl(methyl)dimethoxysilane, 2-(3,4-epoxycyclohexyl)ethyl(methyl)diethoxysilane, 3-ethyl-3-[3'-(methyldimethoxysilyl)propyl]methyloxetane, 3-ethyl-3-[3'-(methyldiethoxysilyl)propyl]methyloxetane, and the like are preferably used.
[0127] Relative to the structural unit having a polymerizable group, a structural unit without a polymerizable group can also be used in combination. As the structural unit without a polymerizable group, as a trifunctional structural unit, trimethoxy (methyl) silane, triethoxy (methyl) silane, methyl tripropoxy silane, tributoxy (methyl) silane, methyl triphenoxy silane, ethyl trimethoxy silane, triethoxy (ethyl) silane, ethyl tripropoxy silane, tributoxy (ethyl) silane, ethyl triphenoxy silane, trimethoxy (propyl) silane, triethoxy (propyl) silane, tripropoxy (propyl) silane, tributoxy ] cyclohexyltrimethoxysilane, triethoxy(methyl)silane, triethoxy(methyl)silane, ethyltrimethoxysilane, triethoxy(ethyl)silane, trimethoxy(phenyl)silane, triethoxy(phenyl)silane, phenyltripropoxysilane, tributoxy(phenyl)silane, triphenoxy(phenyl)silane, cyclohexyltrimethoxysilane, triethoxy(methyl)silane, ethyltrimethoxysilane, triethoxy(ethyl)silane, trimethoxy(phenyl)silane, triethoxy(phenyl)silane, cyclohexyltrimethoxysilane, cyclohexyltriethoxysilane, tripropoxy(cyclohexyl)silane, cyclohexyltributoxysilane, cyclohexyltriphenoxysilane, etc. Among them, trimethoxy(methyl)silane, triethoxy(methyl)silane, ethyltrimethoxysilane, triethoxy(ethyl)silane, trimethoxy(phenyl)silane, triethoxy(phenyl)silane, cyclohexyltrimethoxysilane, cyclohexyltriethoxysilane, etc. can be preferably used.
[0128] As the bifunctional structural unit, preferably used are dimethoxydimethylsilane, diethoxydimethylsilane, methylphenyldimethoxysilane, methylphenyldiethoxysilane, cyclohexyl(dimethoxy)methylsilane, cyclohexyldiethoxymethylsilane, dimethoxydiphenylsilane, diethoxydiphenylsilane, dimethoxymethylvinylsilane, diethoxymethylvinylsilane and the like.
[0129] In this embodiment, the structure of the polymerizable compound is not particularly limited. However, if it is a polymerizable compound having a spherical structure described later or a polyhedral siloxane oligomer having an incompletely condensed skeleton, it is preferred because it can be made into a curable resin 2 with a sufficiently low viscosity even if it does not substantially contain a solvent. In particular, if it is a polymerizable compound having a spherical structure, it is preferred from the viewpoints of thermal stability, processing uniformity, etc.
[0130] The spherical structure refers to a structure in which a polymerizable functional group extends outward from a polymerized portion having a high degree of polymerization. For example, in the case of a polymerizable compound having a spherical structure such as a dendrimer, the ratio of oxygen atoms bonded to a single silicon atom among oxygen atoms bonded to silicon atoms contained in the polymerizable compound is 10 mol% or less, and the viscosity of the curable resin 2 can be sufficiently reduced by adding only a small amount of solvent or low-viscosity material.
[0131] As polymerizable compounds having a spherical structure, polymerizable compounds having trifunctional silane as a structural unit can be cited. Among them, polymerizable compounds having only trifunctional silane as a structural unit are preferred. Polymerizable compounds having such a spherical structure can be cited, for example, as a mixture of one or more of hexamers to 36-mers (molecular weight of 1000 to 6300) of trifunctional silanes having polymerizable functional groups. It should be noted that the molecular weight of the polymerizable compound having a spherical structure can be in the range of 2000 to 6000, and can also preferably be in the range of 2000 to 3000.
[0132] In the case of a siloxane containing a trifunctional silane, it generally has the following structure: 3 / 2 The siloxane polymerization part with high siloxane polymerization degree of the unit is the center, and the polymerizable functional group extends outward. Regarding such a spherical structure polymerizable compound, the siloxane polymerization degree in the siloxane polymerization part can be higher than 90%, particularly can be set to 95% or more, and further can be set to 97% or more, so the ratio of oxygen atoms bonded to a single silicon atom in oxygen atoms bonded to silicon atoms contained in the polymerizable compound is 10 mol% or less.
[0133] This is presumably due to the following reasons. That is, when the hydrolysis reaction of trifunctional silane is carried out under alkaline conditions, OH - Nucleophilic reaction to Si atom. One hydrolyzable group (alkoxy group) is hydrolyzed, thereby reducing the steric hindrance of Si atom, so the hydrolysis reaction rate increases, and -Si(OH)3 is generated in which all three hydrolyzable groups (alkoxy groups) are hydrolyzed. All OH groups of -Si(OH)3 can be condensed, so a high-density and high-polymerization siloxane structure is formed three-dimensionally.
[0134] Specifically, it has a spherical structure represented by the following formula: It should be noted that the following formula is a schematic diagram of a polymerizable compound having a spherical structure, and the polymerizable compound having a spherical structure includes an octamer of trifunctional silane having an acryloxypropyl group and a 3-methacryloxypropyl group as polymerizable groups.
[0135] [Chemical formula 2]
[0136]
[0137] In the formula, SiO 1.5 Indicates that it contains SiO 3 / 2 The siloxane polymer part of the unit.
[0138] In the present invention, the polymerizable compound having a spherical structure may be a polymerizable compound having no oxygen atom, nitrogen atom, phosphorus atom or sulfur atom in the bonding group between the siloxane polymer part constituting the main skeleton of the spherical structure and the polymerizable functional group, or a polymerizable compound having a silicon atom (e.g., SiO 3 / 2 A polymerizable compound having no oxygen atom, nitrogen atom, phosphorus atom or sulfur atom between the silicon atom of the unit) and the polymerizable functional group.
[0139] Examples of the bonding group between the silicon atom and the polymerizable functional group in the siloxane polymer portion include a divalent hydrocarbon group that does not contain an oxygen atom, a nitrogen atom, a phosphorus atom, and a sulfur atom, preferably a linear alkylene group, and more preferably -(CH2) n -(n is an integer from 1 to 9).
[0140] The polymerizable compound having a spherical structure can be obtained by subjecting a hydrolyzable silane composition containing at least a hydrolyzable silane to a hydrolysis-condensation reaction under alkaline conditions.
[0141] Specifically, the reaction can be carried out by putting a solvent and silane as a raw material into a reactor, adding an alkaline substance as a catalyst, and dripping water while stirring. Examples of alkaline catalysts include sodium hydroxide, potassium hydroxide, lithium hydroxide, potassium carbonate (K2CO3), sodium carbonate, ammonia, etc., and the pH is set to 8 to 13, and typically it can be carried out at room temperature to 100°C.
[0142] The above-mentioned silane as raw material can be any one or more of tetrafunctional hydrolyzable silane, trifunctional hydrolyzable silane, difunctional hydrolyzable silane and monofunctional hydrolyzable silane, preferably tetrafunctional hydrolyzable silane or trifunctional hydrolyzable silane, particularly preferably trifunctional hydrolyzable silane. In addition, only one hydrolyzable silane can be used, or two or more can be used in combination.
[0143] Thus, by using a basic catalyst as the catalyst in the synthesis step, the polymerizable compound obtained in the hydrolysis condensation reaction has a high condensation degree. Therefore, it is easy to obtain a polymerizable compound having a spherical structure in which the ratio of oxygen atoms bonded to a single silicon atom among oxygen atoms bonded to silicon atoms is reduced, particularly to 10 mol% or less.
[0144] In addition, the polymerizable compound in this embodiment may be a polyhedral siloxane oligomer having an incompletely condensed skeleton. Since such a polymerizable compound has a regular structure, the proportion of oxygen atoms bonded to a single silicon atom in the oxygen atoms bonded to silicon atoms contained in the polymerizable compound is 10 mol% or less. In addition, the viscosity of the curable resin can be sufficiently reduced.
[0145] As the polyhedral siloxane oligomer having an incompletely condensed skeleton bonded with a polymerizable functional group, there can be mentioned: an incompletely condensed type in which a polyhedral siloxane oligomer having a completely condensed skeleton lacks one vertex, one edge or one face. As the polyhedral siloxane oligomer having an incompletely condensed skeleton bonded with a polymerizable functional group, a polyhedral siloxane oligomer represented by the following formula is particularly preferred.
[0146] [Chemical formula 3]
[0147]
[0148] In the formula, R 3 is a monovalent hydrocarbon group, R 4 R is a -Si- polymerizable group bonded to the oxygen atom in the formula, a hydrogen atom, a metal ion such as Na or Li, or a tetraalkylammonium ion (the alkyl group includes a methyl group, an ethyl group, a propyl group, a butyl group, etc.). 3 It is a monovalent hydrocarbon group, preferably an alkyl group having 1 to 5 carbon atoms or a phenyl group, and specific examples thereof include an ethyl group, a butyl group, and a phenyl group.
[0149] The polymerizable compound can be obtained by reacting a compound containing a polymerizable functional group with a polyhedral siloxane oligomer having an incompletely condensed skeleton in which hydrogen atoms, hydroxyl groups, or organic groups other than polymerizable functional groups are bonded to silicon atoms.
[0150] The polyhedral siloxane oligomer having an incompletely condensed skeleton as a raw material has hydrogen atoms, hydroxyl groups, or organic groups other than polymerizable functional groups bonded to silicon atoms located at the vertices. Examples of organic groups other than polymerizable functional groups include alkoxy groups, alkyl groups, and phenyl groups.
[0151] The reaction of the above raw materials with the compound containing a polymerizable functional group may be a conventionally known reaction, for example, an addition reaction of a hydrogen atom directly bonded to silicon with a compound containing a polymerizable functional group having an unsaturated double bond; a reaction of a hydroxyl group (OH group) or an alkoxy group (OR group) directly bonded to silicon with a compound containing a polymerizable functional group capable of forming a siloxane bond, etc.
[0152] The curable resin 2 in the present embodiment may contain a polymerization initiator. Examples of the polymerization initiator include photopolymerization initiators and thermal polymerization initiators, and photopolymerization initiators are particularly preferred.
[0153] A photopolymerization initiator is a substance that generates a reactive species that causes a polymerization reaction of a polymerizable compound by light stimulation. Specifically, a photoradical generator that generates free radicals by light stimulation, a photoacid generator that generates protons by light stimulation, etc. can be cited. A photoradical generator is a polymerization initiator that generates free radicals by light (charged particle beams such as infrared rays, visible rays, ultraviolet rays, far ultraviolet rays, X-rays, electron beams, etc., radiation), and is mainly used in the case where the polymerizable compound is a free radical polymerizable compound. On the other hand, a photoacid generator is a polymerization initiator that generates an acid (proton) by light, and is mainly used in the case where the polymerizable compound is a cationic polymerizable compound.
[0154] As the photoradical generator, for example, 2,4,6-trimethyldiphenylphosphine oxide, 2,2-dimethoxy-2-phenylacetophenone, 2-methyl-1-[4-(methylthio)phenyl]-2-morpholino-propane-1-one, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-1-butanone, 2-(dimethylamino)-2-[(4-methylphenyl)methyl]-1-[4-(4-morpholino)phenyl]-1-butanone, 2-hydroxy-2-methyl-1-phenyl-propane-1-one, 2-hydroxy-2-methyl-1-phenyl-propane-1-one, etc. can be cited, but it is not limited to these. It should be noted that these photoradical generators can be used alone or in combination of two or more.
[0155] Examples of the photoacid generator include onium salt compounds, sulfone compounds, sulfonate compounds, sulfonimide compounds, and diazomethane compounds, but the photoacid generator is not limited to these.
[0156] The thermal polymerization initiator is a compound that generates the above-mentioned polymerization factor (free radical, cation, etc.) by heat. Specifically, the thermal polymerization initiator includes a thermal free radical generator that generates free radicals by heat, a proton (H + ) etc. The thermal radical generator is mainly used when the polymerizable compound is a radical polymerizable compound. On the other hand, the thermal acid generator is mainly used when the polymerizable compound is a cationic polymerizable compound.
[0157] As thermal free radical generators, organic peroxides, azo compounds, etc. can be cited. As organic peroxides, peroxyesters such as tert-hexyl peroxyisopropyl monocarbonate, tert-hexyl peroxy-2-ethylhexanoate, tert-butyl peroxy-3,5,5-trimethylhexanoate, tert-butyl peroxyisopropyl carbonate, peroxyketals such as 1,1-bis(tert-hexylperoxy)3,3,5-trimethylcyclohexane, diacyl peroxides such as lauroyl peroxide, etc. can be cited, but are not limited to these. In addition, as azo compounds, azonitriles such as 2,2'-azobisisobutyronitrile, 2,2'-azobis(2-methylbutyronitrile), and 1,1'-azobis(cyclohexane-1-carbonitrile) can be cited, but are not limited to these.
[0158] Examples of the thermal acid generator include known iodonium salts, sulfonium salts, phosphonium salts, ferrocenes, etc. Specifically, examples include diphenyliodonium hexafluoroantimonate, diphenyliodonium hexafluorophosphate, diphenyliodonium hexafluoroborate, triphenylsulfonium hexafluoroantimonate, triphenylsulfonium hexafluorophosphate, and triphenylsulfonium hexafluoroborate, but the examples are not limited thereto.
[0159] The content of the polymerization initiator in the curable resin 2 is not particularly limited, but can be in the range of 0.5% by mass to 20% by mass, and can be in the range of 1% by mass to 10% by mass, based on the above-mentioned polymerizable compound.
[0160] The curable resin 2 in the present embodiment may be substantially free of solvent. By being substantially free of solvent, it is possible to suppress the deterioration of flatness and poor curing caused by the bubbling of solvent on the surface during curing. Here, "substantially free of solvent" means: no solvent other than solvents that are not intentionally included, such as impurities. That is, for example, relative to the curable resin 2 as a whole, the content of the solvent in the curable resin 2 is preferably 0.01% by mass or less, and more preferably 0.001% by mass or less. It should be noted that the solvent refers to a solvent used in a conventional resin composition, a photoresist, etc. That is, the type of solvent is not particularly limited as long as it is a solvent that dissolves and uniformly disperses the curable resin 2 and does not react with the curable resin 2.
[0161] Curable resin 2 may include a reactive crosslinking agent. As a reactive crosslinking agent, it is a reactive crosslinking agent having a polymerizable functional group, for example, a reactive crosslinking agent having more than two polymerizable functional groups can be cited. As a polymerizable functional group, a group containing an ethylenically unsaturated bond, an epoxy group, etc. can be exemplified, and a group containing an ethylenically unsaturated bond is suitable. As a group containing an ethylenically unsaturated bond, (meth)acryloyl, vinyl, etc. can be exemplified, more preferably (meth)acryloyl, and further preferably acryloyl. In addition, (meth)acryloyl is preferably (meth)acryloyloxy. Two or more polymerizable groups can be contained in one molecule, and two or more polymerizable groups of the same type can also be contained.
[0162] As a photopolymerizable monomer (bifunctional monomer) having two polymerizable functional groups, for example, trimethylolpropane di(meth)acrylate, ethylene glycol di(meth)acrylate, tetraethylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate, polypropylene glycol di(meth)acrylate, 1,4-butylene glycol di(meth)acrylate, 1,6-hexanediol di(meth)acrylate, neopentyl glycol di(meth)acrylate, bis(hydroxymethyl)tricyclodecane di(meth)acrylate, etc. can be cited. As a commercial product of the bifunctional monomer, for example, Light Acrylate 3EG-A, 4EG-A, 9EG-A, NP-A, DCP-A, BP-4EAL, BP-4PA (above, manufactured by Kyoeisha Chemical Co., Ltd.) can be cited. In addition, from the viewpoint of compatibility, a polyfunctional monomer having a siloxane structure is preferred.
[0163] The content of the reactive crosslinking agent is not particularly limited, and can be within a range of 0% to 99% by mass, preferably 5% to 80% by mass, and particularly preferably 49% to 79% by mass, in the curable resin 2.
[0164] The curable resin 2 may also contain other components in addition to the above-mentioned polymerizable compound, polymerization initiator, and reactive crosslinking agent. As other components, for example, surfactants, release agents, silane coupling agents, photosensitizers, antioxidants, organometallic coupling agents, polymerization inhibitors, ultraviolet absorbers, light stabilizers, anti-aging agents, plasticizers, adhesion promoters, photobase generators, colorants, elastomer particles, photoacid proliferators, basic compounds, other flow regulators, defoamers, dispersants and other components can be cited as needed. The content of other components is not particularly limited, and is preferably less than 5% by mass in the curable resin 2, and particularly preferably less than 3% by mass.
[0165] The viscosity of the curable resin 2 can be 20 cPs or less, preferably 10 cPs or less, and more preferably 7 cPs or less. On the other hand, the lower limit of the viscosity is not particularly limited, and can be set to 1 cPs or more, preferably 1.5 cPs or more. Since the viscosity of the curable resin 2 is very low, it is possible to suppress the generation of bubbles on the concave-convex structure and apply it with good filling properties. In addition, if it is such a low viscosity, it can be applied by inkjet. It should be noted that the viscosity of the curable resin 2 is the value of 25°C and 1000 (1 / s) when the curable resin 2 is dripped on the disc plate using AR-G2 manufactured by TA Instruments under a measurement environment of 25°C and 40% RH, so that the shear rate of a standard steel cone with a diameter of 40 mm becomes 10 to 1000 (1 / s), and 25°C and 1000 (1 / s).
[0166] The contact angle of the curable resin 2 relative to the surface of the standard resist is preferably 20° or less, and more preferably 15° or less. Regarding the contact angle, specifically, the curable resin 2 can be dripped on the surface of the standard resist under a normal pressure atmosphere of a temperature of 25°C and a humidity of 33%, and then measured after 5 seconds using a contact angle measuring device (manufactured by Kyowa Interface Science Co., Ltd., automatic contact angle meter DM-501). As a standard resist, for example, as long as it is a layer formed by using an acrylic acid-styrene (Japanese: アクリルースチレン) copolymer (organic resist resin) as a base resin.
[0167] If the curable resin 2 has a contact angle relative to the standard resist layer, for example, when used as a reversal layer material in a reversal process, the wettability to the core pattern formed by the resist composition becomes good, so that the coating can be applied with better filling performance. When the curable resin 2 shows the above-mentioned contact angle relative to the standard resist, even if the composition of the organic resist material actually used as the core pattern is different from that of the standard resist, good wettability is exhibited.
[0168] The surface free energy of the curable resin 2 is preferably 20 mJ / m 2 Above and 70mJ / m 2 Below, particularly preferably 25mJ / m 2 Above and 50mJ / m 2 If it is within the above range, for example, since it is possible to suppress the compatibility with the core material pattern formed of the organic resist material and to sufficiently wet and spread on the core material pattern, it is preferable.
[0169] In the cured film forming method of the present embodiment, the substrate 3 to which the curable resin 2 is supplied is not particularly limited, and may be, for example, a glass substrate such as a quartz glass substrate, a soda-lime glass substrate, a fluorite substrate, a calcium fluoride substrate, a magnesium fluoride substrate, a barium borosilicate glass, an aminoborosilicate glass, an aluminosilicate glass, or an alkali-free glass substrate; a transparent substrate such as a resin substrate such as a polycarbonate substrate, a polypropylene substrate, a polyethylene substrate, a polymethyl methacrylate substrate, a polyethylene terephthalate substrate; a semiconductor substrate such as a silicon substrate, a GaAs substrate, an InP substrate, a GaN substrate, a GaP substrate, a SiC substrate; a metal-based substrate such as a stainless steel substrate, an aluminum substrate, a copper substrate, an iron substrate; a metal-deposited substrate formed by evaporating a metal such as gold, silver, copper, ITO, chromium, etc. on the surface of a glass substrate, etc. In addition, it may be a laminated substrate formed by laminating two or more substrates arbitrarily selected from the above. It should be noted that in the present embodiment, "transparent" means that the transmittance of light with a wavelength of 300nm to 450nm is 70% or more, preferably 90% or more.
[0170] The substrate 3 has a first surface 3A and a second surface 3B located on the opposite side thereof. The curable resin 2 is supplied to the first surface 3A of the substrate 3 (see Figure 1A , Figure 2A ). The method of supplying the curable resin 2 to the first surface 3A of the substrate 3 is not particularly limited. For example, the curable resin 2 can be discretely supplied to the first surface 3A of the substrate 3 by an inkjet method, or the curable resin 2 can be applied to the first surface 3A of the substrate 3 using a coating machine such as a spin coater or a spray coater.
[0171] The mold 4 is brought close to the curable resin 2 supplied to the first surface 3A of the substrate 3, and the curable resin 2 is spread between the substrate 3 and the mold 4 to form a molded resin layer 5 (contact step, see Figure 1B , Figure 2B ).
[0172] The mold 4 can be composed of, for example, a glass substrate such as a quartz glass substrate, a soda-lime glass substrate, a fluorite substrate, a calcium fluoride substrate, a magnesium fluoride substrate, an acrylic glass substrate, a resin substrate such as a polycarbonate substrate, a polypropylene substrate, a polyethylene substrate, a polyethylene terephthalate substrate, a transparent substrate such as a stacked substrate formed by stacking two or more substrates selected arbitrarily from them, and the like.
[0173] The mold 4 may be a flat mold having a first surface 4A and a second surface 4B located on the opposite side thereof, wherein the first surface 4A is a flat surface (see Figure 1A ), or a mold having a concave-convex structure 41 including a concave portion 42 formed on the first surface 4A (see Figure 2A)。The shape of the concavo-convex structure 41 formed on the first surface 4A of the mold 4 is not particularly limited, and examples thereof include a spaced shape (in Japanese: スペース状), a hole shape (in Japanese: ホール状), etc. The size of the concavo-convex structure 41 is also not particularly limited. For example, in the case of the spaced concavo-convex structure 41, the length in the short side direction of the concave portion 42 may be about 10 nm to 100 nm, and in the case of the hole-shaped concavo-convex structure, the maximum diameter of the concave portion 42 may be about 10 nm to 100 nm. It should be noted that the maximum diameter of the hole-shaped concave portion 42 is, for example, the diameter of the circle when the top view shape of the concave portion 42 is circular, and the length of the diagonal of the square when the top view shape of the concave portion 42 is square. The respective sizes of the plurality of concave portions 42 included in the concavo-convex structure 41 of the mold 4 may be different. In this case, the minimum size (the smallest size) among the plurality of concave portions 42 may be 100 nm or less.
[0174] While the mold 4 is in contact with the resin layer 5 to be formed (curable resin 2), the resin layer 5 to be formed is cured (curing step). The method of curing the resin layer 5 to be formed may be appropriately selected according to the curing type of the curable resin 2 constituting the resin layer 5 to be formed. For example, if the curable resin 2 is a photocurable type, light (such as ultraviolet rays, electron beams, etc.) may be irradiated on the resin layer 5 to be formed (curable resin 2)隔着 the mold 4. If the curable resin 2 is a thermosetting type, heat may be applied to the resin layer 5 to be formed (curable resin 2). In the case where the curable resin 2 is a thermoplastic type, the mold 4 is brought into contact with the resin layer 5 to be formed softened by heating and directly cooled, whereby the resin layer 5 to be formed is cured.
[0175] The film thickness of the cured resin layer 5 to be formed is important for forming the cured film 1 (refer to Figure 1D , Figure 2D ). As described later, by performing an etching treatment on the cured resin layer 5 to be formed (curable resin 2), the organic components in the resin layer 5 to be formed (curable resin 2) are decomposed, and the inorganic components containing a siloxane polymer part as the main component remain and are concentrated, thereby forming the cured film 1. By performing an etching treatment on the resin layer 5 to be formed, while the inorganic components are bonded to each other, the inorganic components are separated. If the film thickness of the resin layer 5 to be formed is relatively thin, most of the inorganic components are separated, and it is difficult to form the cured film 1. However, by making the film thickness of the resin layer 5 to be formed relatively thick, the inorganic components bonded to each other are concentrated, and a cured film 1 having a desired film thickness can be formed.
[0176] Therefore, the film thickness of the formed resin layer 5 after curing can be appropriately set to a degree that can form a cured film 1 having a desired film thickness. For example, based on the following mathematical formula (1) representing the relationship between the film thickness T0 of the formed resin layer 5 after curing, the film thickness T of the cured film 1 to be formed, and the decomposition treatment time t for decomposing the organic component, the supply amount of the curable resin 2 supplied to the first surface 3A of the substrate 3 is determined to form a formed resin layer 5 having a predetermined film thickness T0.
[0177] [Number 6]
[0178]
[0179] In the above mathematical formula (1), Ab ct represents "the amount of reduction per unit time of the film thickness of the formed resin layer 5 that changes with the decomposition treatment time t at the initial stage of the decomposition treatment of the organic component", αt represents "the amount of reduction per unit time of the film thickness of the formed resin layer 5 that does not substantially change with the decomposition treatment time t", A represents "the amount of reduction per unit time of the film thickness of the formed resin layer 5 at the initial stage of the decomposition treatment of the organic component", b and c are "coefficients representing the reduction of the exponential function of the film thickness of the formed resin layer 5", b>1 and c<0. If the absolute values of the coefficients b and c both increase, the amount of reduction per unit time of the film thickness of the formed resin layer 5 that changes with the decomposition treatment time t increases. The coefficients b and c change according to the conditions when the organic components of the formed resin layer 5 are decomposed, and can be appropriately set according to the conditions.
[0180] The above mathematical formula (1) includes a component that changes in the film thickness of the formed resin layer 5 in an exponential function and a component that changes in a linear function. It can be said that the component that changes in an exponential function represents a state in which inorganic components that are bonded to each other are concentrated and gradually remain as the decomposition treatment time t passes. On the other hand, it can be said that the component that changes in a linear function represents a state in which the film thickness of the formed resin layer 5 decreases substantially in proportion to the decomposition treatment time t due to physical etching.
[0181] It should be noted that the "initial stage of decomposition treatment of organic components" is determined based on the type of organic components contained in the formed resin layer 5 (curable resin 2), the conditions for the etching treatment of the formed resin layer 5, etc. For example, it can be about 10 seconds to 300 seconds from the start of the etching treatment of the formed resin layer 5, and preferably about 10 seconds to 60 seconds from the start of the etching treatment.
[0182] After the cured molded resin layer 5 is separated from the mold 4 (mold release process, see Figure 1C , Figure 2C), the shaped resin layer 5 (curable resin 2) is etched to form a cured film 1 (refer to Figure 1D , Figure 2D ). The etching treatment applied to the formed resin layer 5 may be a dry etching treatment (plasma treatment) in which oxygen, nitrogen, argon, chlorine, or a mixed gas of two or more thereof is used for etching in a discharge plasma atmosphere in a vacuum chamber, or a wet etching treatment (oxidation treatment) in which the formed resin layer 5 is etched by contacting an etching liquid such as sulfuric acid or hydrogen peroxide having an oxidizing power. Through these etching treatments, the organic components can be decomposed, and the inorganic components can be bonded and concentrated to each other. As a result, a cured film 1 mainly containing inorganic components can be formed.
[0183] When the cured film 1 is formed on the first surface 3A of the substrate 3, a cured film forming region 31 where the cured film 1 is formed and a cured film non-forming region 32 where the cured film 1 is not formed can be set on the first surface 3A of the substrate 3, and the curable resin 2 is supplied to the cured film forming region 31 in an amount determined based on the above mathematical formula (1) so that the film thickness T of the cured film 1 exceeds 0, and the curable resin 2 is supplied to the cured film non-forming region 32 in an amount determined based on the above mathematical formula (1) so that the film thickness T of the cured film 1 becomes 0 or less, thereby forming the formed resin layer 5. For example, Figures 2A to 2D As shown, when the molded resin layer 5 is formed using a mold 4 having a concavo-convex structure 41 including concave portions 42, the convex portions 51 of the molded resin layer 5 are formed corresponding to the concave portions 42, and the concave portions (residual film portions) 52 of the molded resin layer 5 are formed corresponding to the convex portions between adjacent concave portions 42. Therefore, the region where the convex portions 51 of the molded resin layer 5 should be located is set as the cured film forming region 31, and the region where the concave portions (residual film portions) 52 should be located is set as the cured film non-forming region 32. Then, the height of the convex portions 51 of the molded resin layer 5 and the thickness of the concave portions (residual film portions) 52 of the molded resin layer 5 are determined based on the above mathematical formula (1), and the molded resin layer 5 is formed so that the convex portions 51 of the molded resin layer 5 remain as the cured film 1 and the concave portions (residual film portions) 52 of the molded resin layer 5 disappear. Thus, it is possible to form a structure such as Figure 2D The patterned cured film 1 is shown.
[0184] The cured film 1 thus formed mainly contains inorganic components, more specifically, mainly contains SiO X (X is 1 or more). The term “mainly contains” means that the cured film 1 may contain an organic component. In other words, it includes the concept that the content of the inorganic component in the cured film 1 is greater than the content of the inorganic component in the curable resin 2 .
[0185] The film thickness T of the cured film 1 is thinner than the film thickness T0 of the formed resin layer 5. This is because the organic components in the formed resin layer 5 (curable resin 2) are decomposed and the inorganic components are also separated by the etching process for forming the cured film 1. Figure 2D The size of the patterned cured film 1 (the size of the convex pattern) is smaller than the size of the patterned formed resin layer 5 (see Figure 2C That is, by forming the cured film 1 using the mold 4 having the concavo-convex structure 41 , the cured film 1 including the convex pattern having a size smaller than the minimum size of the concave portion 42 of the concavo-convex structure 41 of the mold 4 can be formed.
[0186] It should be noted that in the cured film forming method of the present embodiment, at least one material layer made of a material different from the material constituting the substrate 3 may be provided on the first surface 3A of the substrate 3 on which the cured film 1 is formed, and the cured film 1 may be formed on the material layer. The material layer is not particularly limited, and examples thereof include a hard mask layer made of metal chromium or the like, a semiconductor layer made of a P-type semiconductor such as boron-doped silicon or arsenic-doped silicon or the like, and a conductive film layer made of ITO or the like.
[0187] [Method for manufacturing substrate for imprint mold]
[0188] The manufacturing method of the substrate for the imprint mold of the present embodiment is described. It should be noted that, in the present embodiment, a method for manufacturing the following imprint mold substrate 10 is cited as an example, wherein the imprint mold substrate 10 comprises: a base 11 having a first surface 11A and a second surface 11B located on the opposite side of the first surface 11A; a first height difference structure 12 protruding from the first surface 11A of the base 11; a second height difference structure 13 protruding from the upper surface portion 12A of the first height difference structure 12; a shading film 14 located on the upper surface portion 12A of the first height difference structure 12; and a cured film 1 as a protective film 15 located on the shading film 14, but the manufacturing method is not limited to the manufacturing method of the substrate 10 for the imprint mold in this manner.
[0189] In this embodiment, first, a multi-stage mold substrate 10' (see Figure 3A). The multi-stage mold substrate 10' comprises: a base 11 having a first surface 11A and a second surface 11B located on the opposite side of the first surface 11A; a first height difference structure 12 protruding from the first surface 11A of the base 11; a second height difference structure 13 protruding from an upper surface portion 12A of the first height difference structure 12; and a light shielding film 14 located on the first surface 11A of the base 11, the upper surface portion 12A of the first height difference structure 12, and the upper surface portion 13A of the second height difference structure 13. A recessed portion 16 is formed on the second surface 11B of the base 11, and the recessed portion 16 has a size that can physically cover the outer edge of the first height difference structure 12 when viewed from above.
[0190] The base 11 can be any substrate that is common as a substrate for an imprint mold, for example, a glass substrate such as a quartz glass substrate, a soda-lime glass substrate, a fluorite substrate, a calcium fluoride substrate, a magnesium fluoride substrate, a barium borosilicate glass, an aminoborosilicate glass, an aluminosilicate glass or other alkali-free glass substrate, a polycarbonate substrate, a polypropylene substrate, a polyethylene substrate, a polymethyl methacrylate substrate, a polyethylene terephthalate substrate or other resin substrate, a transparent substrate such as a stacked substrate formed by stacking two or more substrates selected arbitrarily from them, or the like.
[0191] The plan view shape of the base 11 is not particularly limited, and may be, for example, a substantially rectangular shape, etc. When the base 11 is formed of a quartz glass substrate generally used for photoimprinting, the plan view shape of the base 11 is generally a substantially rectangular shape.
[0192] The size of the base 11 (size when viewed from above) is not particularly limited, but when the base 11 is formed of the above-mentioned quartz glass substrate, the size of the base 11 is, for example, about 152 mm×152 mm. In addition, the thickness of the base 11 can be appropriately set in the range of about 300 μm to 10 mm, for example, in consideration of strength, handling adaptability, etc.
[0193] The first height difference structure 12 protruding from the first surface 11A of the base 11 is provided at the approximate center of the base 11 in a plan view. The first height difference structure 12 has an upper surface portion 12A, and the light shielding film 14 is located on the upper surface portion 12A. In the present embodiment, by arranging the light shielding film 14 on the upper surface portion 12A of the first height difference structure 12, the imprint mold 20 (see FIG. 1 ) manufactured using the imprint mold substrate 10 is Figure 4F ) in the imprint process, only the resin to which the concave-convex pattern 21 of the imprint mold 20 is transferred (the resin directly below the second level difference structure 13) can be cured.
[0194] The second height difference structure 13 protruding from the upper surface portion 12A of the first height difference structure 12 is provided at the approximate center of the base portion 11 (first height difference structure 12) in a plan view. The second height difference structure 13 has an upper surface portion 13A, and a light shielding film 14 is located on the upper surface portion 13A. The light shielding film 14 is removed in a subsequent process. The upper surface portion 13A of the second height difference structure 13 is formed on the imprint mold 20 (see Figure 4F ) constitutes a pattern area in which a concave-convex pattern 21 is formed.
[0195] In a plan view, the outer contour shape of the upper surface portion 12A of the first height difference structure 12 and the outer contour shape of the upper surface portion 13A of the second height difference structure 13 are substantially rectangular. The size (dimension) of the upper surface portion 13A of the second height difference structure 13 is determined by using the imprint mold 20 (see Figure 4F ) is appropriately set, for example, to about 30 mm × 25 mm. The size (dimension) of the outer contour of the upper surface portion 12A of the first height difference structure 12 is about 10 μm to 4000 μm larger than the size (dimension) of the upper surface portion 13A of the second height difference structure 13. That is, the width W of the upper surface portion 12A of the first height difference structure 12 is about 10 μm to 4000 μm. 12A It can be set to about 5μm to 2000μm.
[0196] The protruding height T of the first step structure 12 12 (The length between the first surface 11A of the base 11 and the upper surface portion 12A of the first height difference structure 12, which is parallel to the thickness direction of the base 11) is not particularly limited as long as the purpose of providing the substrate 10 for the imprint mold manufactured in this embodiment with the first height difference structure 12 can be achieved, and for example, it can be set to about 10μm to 30μm.
[0197] The length T between the upper surface portion 12A of the first step structure 12 and the upper surface portion 13A of the second step structure 13 parallel to the thickness direction of the base 11 is 13 (The protruding height T of the second height difference structure 13 13 ) is not particularly limited, and can be set to, for example, about 1 μm to 5 μm.
[0198] A recessed portion 16 of a predetermined size is formed on the second surface 11B of the base 11. By forming the recessed portion 16, an imprint mold 20 (see Figure 4F), especially when the base 11, especially the upper surface portion 13A of the second height difference structure 13, is bent during the imprinting process of the base 11, especially when the base 11 is in contact with the imprinting resin and when the imprinting mold 20 is peeled off. As a result, when the upper surface portion 13A of the second height difference structure 13 (the concave-convex pattern 21 formed on the upper surface portion 13A) is brought into contact with the imprinting resin, it is possible to suppress the situation where gas is trapped between the concave-convex pattern 21 formed on the first upper surface portion 311 of the convex structure portion 3 and the imprinting resin, and the imprinting mold 20 can be easily peeled off from the transfer pattern obtained by transferring the concave-convex pattern 21 to the imprinting resin.
[0199] The top view shape of the recessed portion 16 is preferably a substantially circular shape. By being substantially circular, during the imprint process, particularly when the upper surface portion 13A of the second height difference structure 13 is brought into contact with the imprint resin or when the imprint mold 20 is peeled off from the imprint resin, the upper surface portion 13A of the second height difference structure 13 of the imprint mold 20 can be substantially uniformly curved within its surface.
[0200] The size of the recessed portion 16 when viewed from above is not particularly limited as long as it is such that the first height difference structure 12 is included in the projection area of the recessed portion 16 projected onto the first surface 11A side of the base 11. If the projection area is such a size that the first height difference structure 12 cannot be included, the entire surface of the upper surface portion 13A of the second height difference structure 13 of the imprint mold 20 may not be effectively bent.
[0201] The light shielding film 14 may be formed of a material that can be used in the imprint mold 20 (see Figure 4F ) is used to shield the light (such as UV light, etc.) irradiated to the imprint mold 20 during the imprint process, for example, metals such as chromium, titanium, tantalum, silicon, and aluminum; chromium compounds such as chromium nitride, chromium oxide, and chromium oxynitride, tantalum oxide, tantalum oxynitride, tantalum oxide boride (Japanese: acid boronization tantal), tantalum oxynitride boride (Japanese: acid oxyboration tantal) and other tantalum compounds, titanium nitride, silicon nitride, silicon oxynitride, etc. In addition, the film thickness of the light shielding film 14 is not particularly limited as long as it is a thickness that can shield the light. It should be noted that the light shielding film 14 can be formed by a conventionally known method, such as a sputtering method.
[0202] Next, the curable resin 2 is supplied onto the light shielding film 14 located on the upper surface portion 12A of the first step structure 12 and the light shielding film 14 located on the upper surface portion 13A of the second step structure 13 of the multi-stage mold substrate 10' (see Figure 3B), a predetermined template 17 is brought into contact with the curable resin 2 and cured, thereby forming a first curable resin layer 18 on the light shielding film 14 located on the upper surface portion 12A of the first height difference structure 12, and forming a second curable resin layer 19 on the light shielding film 14 located on the upper surface portion 13A of the second height difference structure 13 (see Figure 3C Then, the template 17 is separated from the cured first curable resin layer 18 and the second curable resin layer 19 (see Figure 3D ).
[0203] The first curable resin layer 18 is used to form a cured film 1 as a protective film 15 by a subsequent process. On the other hand, the second curable resin layer 19 is removed without remaining in the subsequent process of forming the cured film 1. By subjecting the layer containing the curable resin 2 to an etching treatment, the inorganic components contained in the curable resin 2 are bonded to each other and the inorganic components are separated. If the film thickness of the layer containing the curable resin 2 is relatively thin, most of the inorganic components are separated and it is difficult to form a cured film 1, but by making the film thickness relatively thick, the inorganic components bonded to each other are concentrated, and a cured film 1 with a desired film thickness can be formed. Therefore, the first curable resin layer 18 is formed with a film thickness that can form the cured film 1 as the protective film 15, and on the other hand, the second curable resin layer 19 is formed with a film thickness that disappears by the etching treatment in the subsequent process. That is, the curable resin 2 is supplied in such a manner that the film thickness of the second curable resin layer 19 is smaller than the film thickness of the first curable resin layer 18, thereby forming the first curable resin layer 18 and the second curable resin layer 19. Specifically, the supply amount of the curable resin 2 supplied to the upper surface portion 12A of the first height difference structure 12 and the supply amount of the curable resin 2 supplied to the upper surface portion 12A of the second height difference structure 13 can be determined by the above mathematical formula (1).
[0204] The method for curing the first curable resin layer 18 and the second curable resin layer 19 may be appropriately selected according to the curing type of the curable resin 2 constituting the first curable resin layer 18 and the second curable resin layer 19. For example, if the curable resin 2 is a photocurable type, the first curable resin layer 18 and the second curable resin layer 19 (curable resin 2) may be irradiated with light (e.g., ultraviolet rays, electron beams, etc.) through the template 17. If the curable resin 2 is a thermosetting type, heat may be applied to the first curable resin layer 18 and the second curable resin layer 19 (curable resin 2).
[0205] The template 17 has a convex portion 171 having a square ring shape in a plan view and a concave portion 172 surrounded by the convex portion 171. The convex portion 171 corresponds to the upper surface portion 12A of the first height difference structure 12 of the multi-stage mold substrate 10', and the concave portion 172 surrounded by the convex portion 171 corresponds to the upper surface portion 13A of the second height difference structure 13 of the multi-stage mold substrate 10'. The protruding height of the convex portion 171 can be appropriately set so that the first curable resin layer 18 and the second curable resin layer 19 are formed with a predetermined film thickness.
[0206] Next, the first curable resin layer 18 and the second curable resin layer 19 (curable resin 2) are etched to remove the second curable resin layer 19 and form a cured film 1 as a protective film 15 on the light shielding film 14 located on the upper surface portion 12A of the first step structure 12 (see FIG. 1 ). Figure 3E The etching process may be dry etching (plasma treatment) in which etching is performed using oxygen, nitrogen, argon, chlorine, or a mixed gas of two or more thereof in a discharge plasma atmosphere in a vacuum chamber, or wet etching (oxidation treatment) in which etching is performed by bringing an etching solution such as sulfuric acid or hydrogen peroxide into contact with the first curable resin layer 18 and the second curable resin layer 19.
[0207] As described above, the film thickness of the first curable resin layer 18 is set to such an extent that the organic components can be decomposed by the above-mentioned etching process, and the inorganic components can be bonded and concentrated with each other, and as a result, the cured film 1 mainly containing the inorganic components can be formed. On the other hand, the film thickness of the second curable resin layer 19 is set to such an extent that it can be eliminated by the above-mentioned etching process. Therefore, by the above-mentioned etching process, the cured film 1 is formed on the light shielding film 14 located on the upper surface portion 12A of the first step structure 12. On the other hand, the second curable resin layer 19 is removed from the light shielding film 14 located on the upper surface portion 13A of the second step structure 13, and the light shielding film 14 is exposed.
[0208] Finally, the light shielding film 14 located on the first surface 11A of the base 11 and the light shielding film 14 located on the upper surface portion 13A of the second step structure 13 are removed by dry etching using, for example, a chlorine-based (Cl2+O2) gas (see Figure 3F ). On the light shielding film 14 located on the upper surface portion 12A of the first height difference structure 12, a layer mainly composed of SiO is formed. X(X is 1 or more) as a protective film 15. The cured film 1 has low reactivity with respect to the chlorine-based (Cl2+O2) gas that can etch the light-shielding film 14, and thus can protect the light-shielding film 14 located on the upper surface portion 12A of the first level difference structure 12. Therefore, according to the present embodiment, the imprint mold substrate 10 in which the light-shielding film 14 and the protective film 15 are sequentially stacked on the upper surface portion 12A of the first level difference structure 12 can be manufactured.
[0209] It should be noted that, in the above-mentioned embodiment, the method of manufacturing the imprint mold substrate 10 using the multi-stage mold substrate 10' in which the light shielding film 14 is located on the upper surface portion 13A of the second height difference structure 13 is cited as an example, but it is not limited to this method. For example, the imprint mold substrate 10 may also be manufactured using the multi-stage mold substrate 10' in which the light shielding film 14 does not exist on the upper surface portion 13A of the second height difference structure 13. In this case, the second curable resin layer 19 may not be formed on the upper surface portion 13A of the second height difference structure 13.
[0210] [Method for manufacturing imprint mold]
[0211] A method for manufacturing the imprint mold in this embodiment will be described.
[0212] First, prepare Figure 3A to Figure 3F The imprint mold substrate 10 manufactured as shown in the figure has a hard mask layer 22 formed on the first surface 11A of the base 11 of the imprint mold substrate 10, the protective film 15 located on the upper surface portion 12A of the first height difference structure 12, and the upper surface portion 13A of the second height difference structure 13. Figure 4A The hard mask layer 22 includes a first hard mask layer 221 formed on the protective film 15 , a second hard mask layer 222 formed on the upper surface portion 13A of the second height difference structure 13 , and a third hard mask layer 223 formed on the first surface 11A of the base 11 .
[0213] As materials constituting the hard mask layer 22, for example, there can be mentioned metals such as chromium, titanium, tantalum, silicon, and aluminum; chromium compounds such as chromium nitride, chromium oxide, and chromium oxynitride; tantalum compounds such as tantalum oxide, tantalum oxynitride, tantalum oxide boride, and tantalum oxyboride; titanium nitride, silicon nitride, silicon oxynitride, etc., which can be used alone or in combination of any two or more selected ones.
[0214] The second hard mask layer 222 is used to form a mask pattern used when etching is performed to form the concave-convex pattern 21 on the upper surface portion 13A of the second height difference structure 13. In addition, the third hard mask layer 223 is used to form a mask pattern used when etching is performed to form the alignment mark 23 on the first surface 11A of the base 11. Therefore, the constituent material of the hard mask layer 22 can be selected in consideration of the etching selectivity, etc., according to the constituent material of the base 11. For example, when the base 11 is made of quartz glass, chromium oxide or the like can be appropriately selected as the material constituting the hard mask layer 22.
[0215] The thickness of the hard mask layer 22 is appropriately set in consideration of the etching selectivity according to the constituent material of the base 11. For example, when the base 11 is made of quartz glass and the hard mask layer 22 is made of chromium oxide, the thickness of the hard mask layer 22 can be appropriately set within a range of about 0.5 nm to 200 nm.
[0216] The method for forming the hard mask layer 22 (the first hard mask layer 221 , the second hard mask layer 222 , and the third hard mask layer 223 ) is not particularly limited, and examples thereof include known film forming methods such as sputtering, PVD (Physical Vapor Deposition), and CVD (Chemical Vapor Deposition).
[0217] Next, droplets of the imprint resin 23 are discretely supplied onto the second hard mask layer 222 by an inkjet method (see Figure 4B At the same time, the imprint resin 23 is dripped onto the third hard mask layer 223 (see Figure 4B ). Droplets of the imprint resin 23 are arranged on the upper surface portion 13A (second hard mask layer 222) of the second height difference structure 13 according to the pattern density of the concave-convex pattern of the master mold 24 used to form the resin pattern 231 on the second hard mask layer 222. The imprint resin 23 dropped onto the third hard mask layer 223 is arranged according to the position and size of the alignment mark 23 formed on the first surface 11A of the base 11.
[0218] The concavo-convex pattern formed on the pattern surface 24A of the main mold 24 is brought into contact with the imprint resin 23 supplied to the second hard mask layer 222, and the imprint resin 23 is spread between the pattern surface 24A of the main mold 24 and the upper surface portion 13A of the second height difference structure 13 (the second hard mask layer 222). The imprint resin 23 between the pattern surface of the main mold 24 and the upper surface portion 13A of the second height difference structure 13 (the second hard mask layer 222) and the imprint resin 23 on the first surface 11A of the base 11 (the third hard mask layer 223) are cured. Thus, the concavo-convex pattern of the main mold 24 can be transferred to the imprint resin 23 on the second hard mask layer 222 to form a resin pattern 231, and a resist pattern 232 can be formed on the third hard mask layer 223 (see Figure 4C ).
[0219] The imprint resin 23 (resist material) is not particularly limited, and resin materials commonly used in imprint processing (such as ultraviolet curable resins, thermosetting resins, etc.) can be used. The imprint resin 23 may also contain a release agent for easily separating from the main mold 24, a sealing agent for improving the adhesion between the second height difference structure 13 of the imprint mold substrate 10 and the upper surface portion 13A (the second hard mask layer 222), and the like.
[0220] Next, the cured imprint resin 23 is separated from the master mold 24 to form a resin pattern 231, and the residual film portion of the resin pattern 231 is removed as needed (see Figure 4D In this way, the resin pattern 231 to which the concavo-convex pattern of the master mold 24 is transferred can be formed on the second height difference structure 13 (second hard mask layer 222 ) of the imprint mold substrate 10 .
[0221] The resin pattern 231 is used as a mask, and the second hard mask layer 222 formed on the upper surface portion 13A of the second height difference structure 13 formed on the imprint mold substrate 10 is etched by dry etching using, for example, a chlorine-based (Cl2+O2) etching gas to form a hard mask pattern 22P1 (see Figure 4E At the same time, the third hard mask layer 223 is etched using the resist pattern 232 as a mask to form a hard mask pattern 22P2 (see Figure 4E It should be noted that the first hard mask layer 221 located on the upper surface portion 12A of the first level structure 12 is removed by etching, and the protective film 15 is exposed (see Figure 4E ).
[0222] The imprint mold substrate 10 is subjected to dry etching using the hard mask patterns 22P1 and 22P2 as masks to form a concavo-convex pattern 21 on the upper surface portion 13A of the second height difference structure 13 and to form an alignment mark 23 on the first surface 11A of the base 11, thereby manufacturing the imprint mold 20 (see Figure 4F ). At this time, SiO X The protective film 15 mainly composed of (X is 1 or more) is etched and removed simultaneously with the imprint mold substrate 10. The dry etching of the imprint mold substrate 10 can be performed by appropriately selecting an etching gas according to the type of constituent material of the imprint mold substrate 10. As the etching gas, for example, a fluorine-based gas or the like can be used.
[0223] [Method for producing concavoconvex structure body]
[0224] A method for producing the concavo-convex structure body in this embodiment will be described.
[0225] The method for manufacturing a concave-convex structure in the present embodiment is a method for manufacturing a concave-convex structure composed of a line and gap-shaped (Japanese: line and space-shaped) sidewall pattern formed along the sidewall of a resist pattern, and is a method for manufacturing a concave-convex structure by a so-called sidewall method. Usually, in the case of manufacturing a concave-convex structure by a sidewall method, a sidewall material film is formed on the sidewall of a resist pattern that becomes a core material by an ALD method or the like, and a sidewall pattern is formed by etching the sidewall material film. In this case, the sidewall pattern formed along the sidewall of the core material becomes annular (annular in top view), so in order to form a line and gap-shaped sidewall pattern, a process called ring cutting is required. In the method for manufacturing a concave-convex structure in the present embodiment, there is a feature that the process called ring cutting is not required.
[0226] First, a substrate 31 having a first surface 31A and a second surface 31B located on the opposite side thereof and having a resist pattern on the first surface 31A is prepared. The resist pattern can be formed, for example, by imprint lithography using a mold, electron beam lithography using an electron beam drawing device, photolithography using a photomask having a predetermined opening and a light shielding portion, etc. The resist pattern plays a role as a core material pattern 32 for forming a sidewall pattern 36 described later.
[0227] When the sidewall pattern 36 functions as an etching mask for etching the substrate 31, the height (thickness) of the sidewall pattern 36 is required to be a height (thickness) at which the sidewall pattern 36 does not disappear during the etching process of the substrate 31, based on the etching selectivity ratio of the materials that respectively constitute the sidewall pattern 36 and the substrate 31.
[0228] On the other hand, the core material pattern 32 is formed by thinning the resist pattern by etching, so the height (thickness) of the core material pattern 32 is lower (thinner) than the height (thickness) of the resist pattern. Therefore, considering the thinning amount in the process of forming the core material pattern described later, it is necessary to make the height (thickness) of the resist pattern higher (thicker) than the height (thickness) required for the sidewall pattern 36.
[0229] Next, the resist pattern formed on the first surface 31A of the substrate 31 is subjected to a thinning process to form a thin core pattern 32. The thinning process of the resist pattern can be performed by, for example, wet etching, dry etching, or a combination thereof.
[0230] Next, droplets of the sidewall material 33 are dropped onto the core pattern 32 (see Figure 5A , Fig. 6A ). As the side wall material 33, the curable resin 2 in this embodiment is used. The position and number of the droplets of the side wall material 33, and the size of the droplets (amount of one drop) can be set as follows, that is, when the mold 34 is brought into contact with the side wall material 33 in the subsequent process, the side wall material 33 spread between the mold 34 and the core material pattern 32 will not completely cover the core material pattern 32, and at least will not reach the two ends of the length direction of the core material pattern 32 when viewed from above.
[0231] The mold 34 having the convex pattern 341 is brought into contact with the drop of the sidewall material 33 dropped onto the core material pattern 32, and the sidewall material 33 is spread between the mold 34 and the core material pattern 32. In this state, the sidewall material 33 is solidified, thereby forming a sidewall material film 35 (see Figure 5B , Figure 6B Then, the mold 34 is separated from the solidified side wall material film 35 (refer to Figure 5C , Figure 6C ).
[0232] The convex pattern 341 of the mold 34 only needs to have a size (length in the short side direction when viewed from above) that allows it to be inserted between adjacent core material patterns 32 and to form a predetermined gap between the side walls of the core material patterns 32. By inserting the convex pattern 341 having such a size between adjacent core material patterns 32, the mold 34 is brought into contact with the side wall material 33 and solidified, thereby forming a side wall material film 35 that covers the side walls and top of the core material patterns 32 and the first surface 31A of the substrate 31 exposed between the adjacent core material patterns 32.
[0233] Next, the sidewall material film 35 is subjected to an etching process (dry etching process using oxygen, nitrogen, argon, chlorine, or a mixture of two or more of these gases) to form a sidewall pattern 36 on the sidewall of the core pattern 32 (see Figure 5D , Fig.6D ). If the curable resin 2 constituting the sidewall material film 35 is etched, the sidewall material film 35 disappears because the portion located on the top of the core material pattern 32 is relatively thin. In addition, the sidewall material film 35 also disappears in the portion located on the first surface 31A of the substrate 31 exposed between the adjacent core material patterns 32. On the other hand, since the portion along the side wall of the core material pattern 32 is a relatively thick film, the organic component is decomposed, and the inorganic component is bonded and concentrated, forming a cured film 1 as the sidewall pattern 36.
[0234] Then, the core pattern 32 (see FIG. 1 ) on which the sidewall pattern 36 is formed is removed by ashing (plasma ashing using a gas containing oxygen, etc.). Figure 5E , Fig. 6E ). Thus, only the core material pattern 32 can be removed, leaving the side wall pattern 36 on the first surface 31A of the substrate 31. In this way, a concave-convex structure 30 having a line and gap-shaped side wall pattern 36 formed on the first surface 31A of the substrate 31 can be manufactured. It should be noted that the side wall pattern 36 can also be formed on a hard mask layer (not shown) formed on the first surface 31A of the substrate 31 and made of Cr or the like.
[0235] [Pattern Formation Method]
[0236] The pattern forming method in this embodiment is described. It should be noted that as the pattern forming method in this embodiment, a method for manufacturing a convex lens substrate is listed (refer to Figure 7A to Figure 7B ) and a method for manufacturing a Fresnel lens substrate (refer to Figure 8A to Figure 8C ) is used as an example for explanation, but is not limited to this method.
[0237] [Method for manufacturing convex lens substrate]
[0238] In the method for manufacturing the convex lens substrate 60, a base material 61 having a first surface 61A and a second surface 61B located on the opposite side thereof is prepared, and a drop of a curable resin 2 is dripped onto the first surface 61A of the base material 61 (see Fig. 7A Since each drop of the dripped curable resin 2 will constitute the convex lens 62 in the convex lens substrate 60, the dripping configuration and size (amount of one drop) of the drop of the curable resin 2 can be appropriately set according to the configuration and size of the convex lens 62 required in the convex lens substrate 60 to be manufactured.
[0239] Next, the droplets of curable resin 2 are subjected to etching treatment (dry etching treatment using oxygen, nitrogen, argon, chlorine, or a mixture of two or more thereof as etching gas, or wet etching treatment using an etching solution such as sulfuric acid or hydrogen peroxide). This etching treatment can decompose the organic components in the curable resin 2, and bond and condense the inorganic components, thereby forming a convex lens 62 mainly composed of inorganic components (see Figure 7B ). In this way, the convex lens substrate 60 having the convex lenses 62 as the cured film 1 can be manufactured.
[0240] [Method for manufacturing Fresnel lens substrate]
[0241] In the method for manufacturing a Fresnel lens substrate, a substrate 71 having a first surface 71A and a second surface 71B located on the opposite side thereof is prepared, and a curable resin layer 72 containing a curable resin 2 is formed on the first surface 71A of the substrate 71. The curable resin layer 72 can be formed by, for example, dropping a liquid drop of the curable resin 2 onto the first surface 71A of the substrate 71, and curing the curable resin 2 while bringing a mold (not shown) having a flat surface into contact with the liquid drop of the curable resin 2.
[0242] A photoresist layer is formed on the curable resin layer 72, and grayscale exposure is performed on the photoresist layer, for example, at a predetermined grayscale number, thereby forming a resin layer 73 having a thickness distribution (for example, a resin layer 73 having a sawtooth shape in cross section) (see Fig. 8A ).
[0243] Next, the curable resin layer 72 is etched using the resin layer 73 as a mask, thereby transferring the shape of the resin layer 73 to the curable resin layer 72 (see Figure 8B ). In this embodiment, a curable resin layer 72 having a sawtooth-shaped cross section is formed. This etching may be dry etching using a fluorine-based gas or the like, for example.
[0244] Finally, the curable resin layer 72 having a sawtooth-shaped cross section is subjected to dry etching using oxygen, nitrogen, argon, chlorine, or a mixture of two or more thereof as an etching gas, or wet etching using sulfuric acid, hydrogen peroxide, or the like as an etching liquid. This etching process can decompose the organic components in the curable resin 2, and generate bonding and concentration of inorganic components, so that a Fresnel lens 74 mainly composed of inorganic components can be formed (see Figure 8C ). In this way, the Fresnel lens substrate 70 having the Fresnel lens 74 as the cured film 1 can be manufactured.
[0245] [Method for manufacturing semiconductor device]
[0246] A method for manufacturing the semiconductor device in this embodiment will be described.
[0247] The semiconductor device manufactured in this embodiment has the following structure: on the first surface side of a substrate having a first surface and a second surface located on the opposite side thereof, a semiconductor layer, an insulating film, and wiring are stacked in order from the first surface side. The manufacturing method of the semiconductor device includes: forming a semiconductor layer 82 on the first surface 81A side of a substrate 81, the semiconductor layer 82 having a channel region 821 and a source / drain region 822 including a contact portion contacting with the wiring (see Fig. 9A ); and forming an insulating film 83 on an insulating film forming region including the channel region 821 and a region other than the contact portion (refer to Fig. 9B ).
[0248] The process of forming the insulating film 83 includes: a process of supplying the curable resin 2 to the insulating film forming region; a process of curing the curable resin 2; and a process of forming the insulating film 83 by decomposing the organic components in the cured curable resin 2 and leaving the inorganic components. According to the present embodiment, the insulating film 83 can be formed by a simple method by curing the curable resin 2 supplied to the insulating film forming region and subjecting the curable resin 2 to a predetermined etching process (dry etching process or wet etching process using oxygen, nitrogen, argon, chlorine, or a mixture of two or more thereof).
[0249] The embodiments described above are described to facilitate understanding of the present invention, and are not described to limit the present invention. Therefore, each element disclosed in the above embodiments also includes all design changes and equivalents belonging to the technical scope of the present invention.
[0250] The cured film forming method of the above embodiment can be used as a hard mask forming method for forming a cured film 1 functioning as a hard mask layer on a metal film such as a quartz glass substrate on which a metal film such as a Cr film is formed. Such a hard mask forming method may include, for example, the steps of supplying the above curable resin 2 to the metal film, Figure 1B The mold 4 shown in the figure is brought into contact with the curable resin 2 and cured to form a molded resin layer 5, and the molded resin layer 5 is subjected to a predetermined etching process to decompose the organic component and bond and condense the inorganic component to form a cured film 1.
[0251] Example
[0252] Hereinafter, the present invention will be described in further detail with reference to Examples and the like, but the present invention is not limited at all to the following Examples and the like.
[0253] [Example 1]
[0254] A curable resin 2 is applied to a quartz glass substrate and cured while a flat plate mold is pressed from above to form a 150 nm thick shaped resin layer 5. The shaped resin layer 5 is subjected to dry etching using a chlorine-based (Cl2+O2) gas (etching time: 1555 seconds) to form a cured film 1 with a thickness of 95 nm. Fig.10 The relationship between the etching time and the film thickness (nm) of the formed resin layer 5 is shown in FIG. Fig.10 In the graph shown, the black circles (●) are the results of Example 1, the hollow diamonds (◇) are the results of Reference Example 1 described later, and the white circles (○) are the results of Reference Example 2 described later. Fig.10 As shown, after the etching time has passed for about 300 seconds, the variation of the film thickness of the exponential function is almost not observed. Based on this result, it was confirmed that by using a curable resin 2 to form a formed resin layer 5 having a predetermined initial film thickness, and subjecting the formed resin layer 5 to a predetermined etching treatment, the organic components can be decomposed, and the inorganic components can be bonded and concentrated, thereby forming a cured film 1 mainly containing inorganic components. The organic components contained in the formed resin layer 5 are decomposed by the above-mentioned dry etching treatment, while the inorganic components are not decomposed by the above-mentioned dry etching treatment. In the initial stage of the dry etching treatment (for example, within 300 seconds from the start of the dry etching treatment), it is believed that mainly the organic components are decomposed. At this time, it is believed that the inorganic components are bonded and concentrated, but a part of the inorganic components are physically etched. Therefore, in the initial stage of the dry etching treatment, the film thickness reduction per unit time of the formed resin layer 5 is relatively large (refer to Fig.10 On the other hand, it is considered that after most of the organic components contained in the formed resin layer 5 are decomposed (after 300 seconds from the start of the dry etching process), the bonding and concentration of the inorganic components proceed, and a part of the inorganic components are physically etched. Therefore, the film thickness reduction per unit time of the formed resin layer 5 becomes relatively small (refer to Fig.10 ).
[0255] Regarding the relationship between the initial film thickness T0 of the formed resin layer 5 and the film thickness T of the cured film 1, the decrease per unit time of the film thickness of the formed resin layer 5 that changes according to the decomposition treatment time t of the organic component is defined as Ab. ct, when the amount of reduction per unit time of the film thickness of the formed resin layer 5 that does not substantially change according to the decomposition treatment time t is defined as αt, the amount of reduction per unit time of the film thickness of the formed resin layer in the initial stage of the decomposition treatment of the organic component, i.e., A, can be calculated as the amount of change per unit time based on, for example, the amount of change in the film thickness of the formed resin layer 5 when the formed resin layer 5 is subjected to an etching treatment in a short time of less than 30 seconds. In addition, α can be calculated as the amount of change per unit time by measuring the amount of change in the film thickness of the formed resin layer 5 after the etching treatment of the formed resin layer 5 continues and the amount of reduction per unit time of the film thickness of the formed resin layer 5 does not substantially change according to the decomposition treatment time t. The coefficients b and c of the exponential function phenomenon representing the film thickness of the formed resin layer 5 can be derived by appropriately adjusting the numerical values so as to be suitable for the change in the film thickness of the formed resin layer 5. However, since the numerical values vary depending on the conditions of the decomposition treatment, the above mathematical formula (1) can be appropriately derived according to the material of the formed resin layer 5 (curable resin 2), etching treatment conditions, etc.
[0256] In the above-mentioned Example 1, a composition containing 20% by mass of the polymerizable compound having a spherical structure shown below, a reactive crosslinking agent (difunctional acrylate containing dimethylsiloxane, 79% by mass), and a photopolymerization initiator (Omnirad907, 1% by mass) was used as the curable resin 2. It should be noted that in a measurement environment of 25°C and 40% RH, using AR-G2 manufactured by TA Instruments, the curable resin was dripped on a disk plate, and the value of the shear rate of a standard steel cone of 40 mm in diameter at 25°C and 1000 (1 / s) was changed to 6.4 cPs at 25°C and 1000 (1 / s), which can be coated by inkjet.
[0257] [Chemical formula 4]
[0258]
[0259] In the formula, SiO 1.5 Indicates that it contains SiO 3 / 2 The siloxane polymer part of the unit.
[0260] The above polymerizable compound was synthesized as follows.
[0261] 11.7 g of 3-acryloxypropyltrimethoxysilane was dissolved in 93.9 g of acetone and heated to 50°C. A mixed solution of 13.5 g of ion exchange water and 0.07 g of potassium carbonate (K2CO3) was added dropwise thereto and stirred at 50°C for 5 hours. The obtained reaction solution was washed and extracted with saturated brine and chloroform. The volatile components were removed to obtain the above-mentioned polymerizable compound having a spherical structure.
[0262] [Reference Example 1]
[0263] When the cured film 1 was formed in the same manner as in Example 1 except that the film thickness of the formed resin layer 5 was changed to 40.5 nm, the disappearance of the formed resin layer 5 was confirmed at 330 seconds of dry etching (see Fig.10 ).
[0264] [Reference Example 2]
[0265] When the cured film 1 was formed in the same manner as in Example 1 except that the film thickness of the formed resin layer 5 was changed to 27.3 nm, the disappearance of the formed resin layer 5 was confirmed at 120 seconds of dry etching (see Fig.10 ).
[0266] [Reference Example 3]
[0267] When the cured film 1 was formed in the same manner as in Example 1 except that a composition containing 35% by mass of the above-mentioned polymerizable compound having a spherical structure, a reactive crosslinking agent (difunctional acrylate containing dimethylsiloxane, 64% by mass) and a photopolymerization initiator (Omnirad907, 1% by mass) was used as the curable resin, the variation of the film thickness decreased more rapidly than in Example 1, and the variation of the film thickness was not observed over time (not shown). It should be noted that the viscosity of the curable resin measured in the same manner as in Example 1 was 20 cPs, and it can be applied by inkjet.
[0268] [Reference Example 4]
[0269] When a cured film 1 was formed in the same manner as in Example 1 except that a composition containing 50% by mass of the above-mentioned polymerizable compound having a spherical structure, a reactive crosslinking agent (difunctional acrylate containing dimethylsiloxane, 49% by mass) and a photopolymerization initiator (Omnirad 907, 1% by mass) was used as a curable resin, the variation in film thickness decreased more rapidly than in Reference Example 3, and no variation in film thickness was observed over time (not shown). It should be noted that the viscosity of the curable resin measured in the same manner as in Example 1 was 54 cPs, and it was not possible to apply it by inkjet, so it was applied by spin coating.
[0270] [Example 2] Example of manufacturing an imprint mold
[0271] Prepare Figure 3A The multi-stage mold substrate 10' made of a quartz glass substrate shown in FIG. 1 is coated with the curable resin 2 used in Example 1 on the upper surface portion 12A of the first height difference structure 12 and the upper surface portion 13A of the second height difference structure 13. Figure 3C The template 17 shown is pressed against the curable resin 2, and the curable resin 2 is irradiated with ultraviolet rays to be cured, thereby forming a first curable resin layer 18 and a second curable resin layer 19. It should be noted that the supply amount of the curable resin 2 is adjusted based on the above mathematical formula (1) so that the film thickness of the first curable resin layer 18 becomes 80nm and the film thickness of the second curable resin layer 19 becomes 30nm.
[0272] Next, the first curable resin layer 18 and the second curable resin layer 19 are subjected to dry etching treatment (etching time 300 seconds) using chlorine-based (Cl2+O2) gas to remove the second curable resin layer 19, and a cured film 1 (film thickness 40 nm) is formed as a protective film 15 on the shading film 14 located on the upper surface portion 12A of the first height difference structure 12, thereby producing a substrate 10 for an imprint mold.
[0273] Next, a hard mask layer 22 containing metal Cr is formed on the first surface 11A of the base 11 of the imprint mold substrate 10, the protective film 15 located on the upper surface portion 12A of the first step structure 12, and the upper surface portion 13A of the second step structure 13 (see Figure 4A ), droplets of the imprint resin 23 are discretely supplied onto the second hard mask layer 222 by inkjet method (refer to Figure 4B ). Then, the concavo-convex pattern of the master mold 24 is transferred to the imprint resin 23 supplied to the second hard mask layer 222 to form a resin pattern 231, and the second hard mask layer 222 is etched using the resin pattern 231 as a mask to form a hard mask pattern 22P1. Then, the imprint mold substrate 10 is dry-etched using the hard mask pattern 22P1 as a mask to form a concavo-convex pattern 21 on the upper surface portion 13A of the second height difference structure 13, thereby manufacturing the imprint mold 20.
[0274] [Example 3] Example of manufacturing a concave-convex structure body based on the sidewall method
[0275] As a substrate having a first surface 31A and a second surface 31B located on the opposite side thereof, a synthetic quartz glass substrate having an outer shape of 6 inches square and a thickness of 0.25 inches was prepared. An electron beam sensitive resist was applied to the first surface 31A of the quartz glass substrate by spin coating, and the resist layer was subjected to electron beam drawing and developed to form a resist pattern having a line and space shape with a pattern width of 48 nm, a height of 59 nm, a half pitch of 52 nm, and a line length of 10 μm.
[0276] Next, the resist pattern was thinned by dry etching with oxygen plasma to form a core pattern 32 with a pattern width of 26 nm and a height of 48 nm, and droplets of curable resin 2 were dropped on the core pattern 32 as the sidewall material 33. As the curable resin 2, the curable resin used in Example 1 was used.
[0277] The mold 34 having a convex pattern 341 with a pattern width of 26 nm and a height of 55 nm is brought into contact with a drop of the curable resin 2 dripped onto the core material pattern 32, and the curable resin 2 is spread between the mold 34 and the core material pattern 32, and is cured by irradiating ultraviolet rays, thereby forming a side wall material film 35 (see Figure 5B , Figure 6B ). Then, the side wall material film 35 after solidification is separated from the mold 34 (refer to Figure 5C , Figure 6C ).
[0278] Next, the side wall material film 35 is subjected to an etching process (dry etching process using chlorine (Cl2+O2) gas (etching time 300 seconds)) to decompose the organic components and bond and condense the inorganic components, thereby forming a side wall pattern 36 with a pattern width of 26nm and a height of 23nm on the side wall of the core material pattern 32 (see Figure 5D , Fig.6D Then, the core pattern 32 having the sidewall pattern 36 formed thereon is removed by plasma ashing using an oxygen-containing gas (see Figure 5E , Fig. 6E ) to manufacture a concave-convex structure 30 having a sidewall pattern 36 in the shape of lines and gaps.
[0279] [Example 4] Surface composition analysis based on XPS
[0280] The same operation as in Example 1 was performed except that the film thickness of the formed resin layer 5 was changed to 39 nm and the dry etching process was performed until the film thickness became 24 nm, to form a cured film 1, and the surface composition analysis of the cured film 1 was performed by X-ray photoelectron spectroscopy (XPS). In addition, the surface composition analysis based on X-ray photoelectron spectroscopy (XPS) was also performed on the formed resin layer 5 before the dry etching process. As a result, the composition ratio (%) of the elements in the cured film 1 and the formed resin layer 5 is as shown in Table 1 below.
[0281] [Table 1]
[0282]
[0283] (Others: N, etc.)
[0284] From the results shown in Table 1, it was confirmed that the cured film formed by the dry etching process had a concentration gradient in which the concentration of silicon (Si) atoms was high near the surface of the cured film and the concentration of silicon (Si) atoms was low toward the inside of the cured film along the thickness direction of the cured film. In addition, it was confirmed that the cured film formed by the dry etching process had a concentration gradient in which the concentration of carbon (C) atoms was low near the surface of the cured film and the concentration of carbon (C) atoms was high toward the inside of the cured film along the thickness direction of the cured film.
[0285] Description of Reference Numerals
[0286] 1…cured film
[0287] 2…Curing resin
[0288] 10…Substrates for imprint molds
[0289] 20…Imprinting mold
[0290] 30…Concave-convex structure
[0291] 60…Convex lens substrate
[0292] 70…Fresnel lens substrate
Claims
1. A method for forming a cured film, comprising: include: A step of supplying a curable resin to the substrate, wherein the curable resin comprises a polymerizable compound having a siloxane bond in a molecule and having at least one polymerizable functional group, a polymerization initiator, and a reactive crosslinking agent; A step of curing the curable resin; as well as The cured curable resin is subjected to a plasma treatment or an oxidation treatment to decompose an organic component contained in the curable resin and leave a siloxane polymerized portion, thereby forming a cured film.
2. The cured film forming method according to claim 1, in, The polymerizable compound has a spherical structure with the siloxane polymer part as the center and the polymerizable functional group extending outward.
3. The cured film forming method according to claim 1 or 2, in, Among the oxygen atoms bonded to silicon atoms contained in the polymerizable compound, the proportion of oxygen atoms bonded to a single silicon atom is 10 mol % or less, The curable resin contains substantially no solvent and has a viscosity of 20 cPs or less.
4. The method for forming an effect film according to any one of claims 1 to 3, in, The content of the reactive crosslinking agent contained in the curable resin is 49% by mass to 79% by mass.
5. The cured film forming method according to any one of claims 1 to 4, in, The step of curing the curable resin includes: A contact step of bringing the mold close to the substrate and spreading the curable resin between the substrate and the mold to form a molded resin layer; a curing step of curing the formed resin layer; and A demolding step of releasing the mold from the cured resin layer to be molded.
6. The cured film forming method according to claim 5, in, Based on the thickness T of the resin layer to be formed 0 , the thickness T of the cured film, and the decomposition treatment time t for decomposing the organic component, to determine the amount of the curable resin supplied to the substrate, In the above mathematical formula (1), Ab ct represents "the amount of reduction per unit time of the film thickness of the formed resin layer in the initial stage of the decomposition treatment of the organic component that varies with the decomposition treatment time t", αt represents "the amount of reduction per unit time of the film thickness of the formed resin layer that does not substantially vary with the decomposition treatment time t", A represents "the amount of reduction per unit time of the film thickness of the formed resin layer in the initial stage of the decomposition treatment of the organic component", b and c are "coefficients representing the reduction of the exponential function of the film thickness of the formed resin layer", b>1 and c<0.
7. The cured film forming method according to claim 6, in, A cured film forming region where the cured film is formed and a cured film non-forming region where the cured film is not formed are set on the substrate, The curable resin is supplied to the cured film forming region in an amount determined based on the mathematical formula (1) so that the thickness T of the cured film exceeds 0, and the curable resin is supplied to the cured film non-forming region in an amount determined based on the mathematical formula (1) so that the thickness T of the cured film becomes less than 0.
8. The cured film forming method according to claim 6 or 7, in, The mold has a concavo-convex structure including a concave portion, The resin layer to be formed has a transfer structure and a residual film portion, wherein the transfer structure includes a convex portion to which the concave portion of the concavo-convex structure is transferred, The amount of the curable resin supplied to the substrate is determined based on the depth of the concave portion of the concavo-convex structure, the thickness of the residual film portion, and the mathematical formula (1).
9. The cured film forming method according to claim 5, in, The mold has a concave-convex structure with a minimum size of less than 100 nm, The shaped resin layer has a transfer structure to which the concavo-convex structure is transferred, The cured film forming method forms the cured film having a pattern having a size smaller than a minimum size of the concavo-convex structure.
10. The cured film forming method according to any one of claims 1 to 9, in, The substrate has a first surface and a second surface located on the opposite side of the first surface, and the substrate has at least one material layer made of a material different from that of the substrate on at least the first surface. The cured film forming method supplies the curable resin onto the material layer.
11. A cured film formed by the cured film forming method according to any one of claims 1 to 10, In the composition distribution along the thickness direction of the cured film, there is a concentration gradient in which the concentration of silicon (Si) atoms is highest near the surface of the cured film and lowest near the substrate.
12. The cured film according to claim 11, in, In the composition distribution along the thickness direction of the cured film, the concentration of carbon (C) atoms near the surface of the cured film is the lowest and the concentration of carbon (C) atoms near the substrate is the highest.
13. A method for manufacturing a substrate for an imprint mold, wherein include: A step of preparing a multi-stage mold substrate, the multi-stage mold substrate comprising a base, a first height difference structure, a second height difference structure, and a light shielding film, the base having a first surface and a second surface located on the opposite side of the first surface, the first height difference structure protruding from the first surface of the base, the second height difference structure protruding from the upper surface of the first height difference structure, and the light shielding film located on the upper surface of the first height difference structure; A step of supplying a curable resin onto the light shielding film and the upper surface of the second height difference structure to form a first curable resin layer on the light shielding film and a second curable resin layer on the upper surface of the second height difference structure, and curing the first curable resin layer and the second curable resin layer, wherein the curable resin comprises a polymerizable compound having a siloxane bond and at least one polymerizable functional group in the molecule, a polymerization initiator, and a reactive crosslinking agent; as well as a step of subjecting the cured first curable resin layer and the second curable resin layer to a plasma treatment or an oxidation treatment to decompose the organic components contained in the curable resins so as to leave the siloxane polymerized part, thereby forming a protective film on the light shielding film, and removing the second curable resin layer; The second curable resin layer has a thickness smaller than that of the first curable resin layer and is of a thickness sufficient to be removed during formation of the protective film.
14. The method for manufacturing an imprint mold substrate according to claim 13, in, forming a light shielding material layer on the upper surface of the second height difference structure of the multi-stage mold substrate, After removing the second curable resin layer, the method includes removing the light shielding material layer by etching.
15. A method for manufacturing an imprinting mold, wherein include: A step of forming a first hard mask layer on the protective film of the imprint mold substrate manufactured by the method according to claim 13 or 14, and forming a second hard mask layer on the upper surface of the second step structure; forming a mask pattern on the second hard mask layer; A step of etching the second hard mask layer using the mask pattern as a mask to form a hard mask pattern on the upper surface of the second height difference structure and remove the first hard mask layer; as well as A step of etching the upper surface of the second level difference structure using the hard mask pattern as a mask to form a concavo-convex pattern on the upper surface of the second level difference structure, and removing the protective film.
16. A method for manufacturing a concavo-convex structure, comprising: A step of preparing a substrate having a first surface and a second surface located on the opposite side of the first surface; forming a core material pattern having a convex pattern on the first surface; A step of supplying a curable resin onto the core material pattern, wherein the curable resin comprises a polymerizable compound having a siloxane bond in a molecule and having at least one polymerizable functional group, a polymerization initiator, and a reactive crosslinking agent; A step of forming a curable resin layer by bringing the template into contact with the curable resin supplied onto the core material pattern and curing the curable resin layer, wherein the curable resin layer covers the top and side wall portions of the convex patterns of the core material pattern and the first surface exposed between adjacent convex patterns; A step of subjecting a portion of the curable resin layer covering the sidewall portion of the convex pattern to a plasma treatment or an oxidation treatment to decompose an organic component contained in the curable resin so that a siloxane polymerization portion remains, and removing a portion covering the top of the convex pattern and a portion covering the first surface exposed between adjacent convex patterns, thereby forming a sidewall pattern; as well as A step of removing the core material pattern.
17. A pattern forming method, comprising: A step of preparing a substrate having a first surface and a second surface located on the opposite side of the first surface; A step of discretely dropping a curable resin onto the first surface of the substrate, the curable resin comprising a polymerizable compound having a siloxane bond in a molecule and having at least one polymerizable functional group, a polymerization initiator, and a reactive crosslinking agent; A step of curing the discretely dropped curable resin; as well as The cured curable resin is subjected to plasma treatment or oxidation treatment to decompose the organic component contained in the curable resin and leave the siloxane polymerized part, thereby forming a cured film pattern.
18. A pattern forming method, comprising: A step of preparing a substrate having a first surface and a second surface located on the opposite side of the first surface; A step of supplying a curable resin to the first surface of the substrate, the curable resin comprising a polymerizable compound having a siloxane bond in a molecule and having at least one polymerizable functional group, a polymerization initiator, and a reactive crosslinking agent; a step of bringing a mold close to the substrate and curing the curable resin spread between the substrate and the mold to form a molded resin layer; a step of separating the mold from the molded resin layer; forming an anti-etching layer having a thickness distribution on the formed resin layer; a step of etching the resin layer to be formed by using the resist layer as a mask to form a resin pattern; and The resin pattern is subjected to plasma treatment or oxidation treatment to decompose the organic component contained in the curable resin to leave the siloxane polymerized part, thereby forming a cured film pattern.
19. A method for forming a hard mask, which is a method for forming a hard mask in an arbitrary region on a substrate having a metal film formed thereon, the hard mask forming method comprising: A step of supplying a curable resin onto the metal film, the curable resin comprising a polymerizable compound having a siloxane bond in a molecule and having at least one polymerizable functional group, a polymerization initiator, and a reactive crosslinking agent; a step of bringing a mold close to the substrate and curing the curable resin spread between the substrate and the mold to form a molded resin layer; as well as The step of subjecting the resin layer to be formed to a plasma treatment or an oxidation treatment to decompose the organic component contained in the curable resin and leave a siloxane polymerized portion, thereby forming a hard mask.
20. An insulating film forming method, which is a method of forming an insulating film in an insulating film forming region on a substrate, the insulating film forming method include: A step of supplying a curable resin to the insulating film forming region, the curable resin comprising a polymerizable compound having a siloxane bond in a molecule and having at least one polymerizable functional group, a polymerization initiator, and a reactive crosslinking agent; A step of curing the curable resin; as well as The step of subjecting the cured curable resin to a plasma treatment or an oxidation treatment to decompose an organic component contained in the curable resin and leave a siloxane polymerized portion, thereby forming the insulating film.
21. A method for manufacturing a semiconductor device, in, The semiconductor device has a structure in which a semiconductor layer, an insulating film, and wiring are stacked in order from the first surface side on the first surface side of a substrate having a first surface and a second surface located on the opposite side of the first surface, and the manufacturing method includes: forming the semiconductor layer on the first surface, the semiconductor layer having a channel region and a source / drain region, the source / drain region including a contact portion contacting the wiring; and The step of forming the insulating film on the channel region and the region excluding the contact portion by the method according to claim 20.
Citation Information
Cited By
Imprint method
TWI915154B