Preparation method and application of multivalent metal catalyst
By using high mechanical strength support and suitable catalyst active substances in the preparation of polyvalent metal catalysts, combined with impregnation, drying, calcining and cooling steps, the problem of catalyst susceptibility to poisoning and inactivation is solved, and higher catalytic activity is achieved. Stability improves the safety and quality of the product.
Patent Information
- Application Number
- CN202411046664.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-19
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing polyvalent metal catalysts are susceptible to poisoning and inactivation, resulting in unstable catalytic activity, safety risks and quality problems.
Using high mechanical strength support and suitable catalyst active substances, a polyvalent metal catalyst is prepared by impregnation, drying, calcining and cooling steps, and solvent and water are removed during the drying process, and competitive adsorbent is added to uniformly distribute the active components, and Secondary calcination is used to improve the thermal stability of the catalyst.
It improves the safety and quality of polyvalent metal catalysts, avoids toxicity, enhances catalytic activity and thermal stability, and extends service life.
Smart Images

Figure CN118976483A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of metal catalyst preparation, and in particular to a preparation method and application of a multivalent metal catalyst. Background Art
[0002] Metal catalysts are heterogeneous catalysts with high catalytic activity and selectivity. Polyvalent metals refer to metals in which the element atoms in the compound can have different charge numbers. Common polyvalent metal catalysts include copper, iron, chromium, manganese, etc. They are widely used in chemical reactions such as hydrogenation, dehydrogenation, oxidation, reduction and cracking. The advantages of polyvalent metal catalysts include fast reaction rate and high catalytic efficiency. The existing technology has the following problems:
[0003] Because the copper element catalyst included in the existing multivalent metal catalyst has a fast reaction rate and high catalytic efficiency, it also has the disadvantage that the catalytic activity is easily poisoned and deactivated, which leads to safety risks and poor quality during catalysis. Summary of the Invention
[0004] The present invention provides a preparation method and application of a multivalent metal catalyst to solve the problems raised in the above background technology.
[0005] In order to solve the above technical problems, the technical solution adopted by the present invention is:
[0006] The preparation method and use of a multivalent metal catalyst include the following steps:
[0007] Step 1: Raw material preparation: Select appropriate carrier and catalyst active material, and carry out crushing and mixing pretreatment;
[0008] Step 2: Impregnation: Immerse the carrier in a solution of the catalyst active substance to evenly distribute the catalyst on the carrier surface;
[0009] Step 3: Drying: Dry the wet carrier to make the catalyst active material completely adhere to the carrier surface;
[0010] Step 4: Calcination: Place the carrier into a furnace and calcine at high temperature to completely fix the catalyst on the carrier;
[0011] Step 5: Cooling: After the calcination is completed, cool the furnace to room temperature and take out the catalyst.
[0012] A further improvement of the technical solution of the present invention is that: the carrier in step 1 requires high mechanical strength, suitable particle shape and size, appropriate surface area, pore structure, etc., good heat resistance, good thermal conductivity, sufficient water absorption, the carrier is inert, does not react chemically with the impregnation liquid, does not contain catalyst poisons and substances that cause side reactions, the raw materials are easily available, simple to prepare, and pollution-free, including alumina, silica gel, molecular sieve, activated carbon, diatomaceous earth, pumice, activated white clay, and carbon fiber. The catalyst active substance can be selected from ferric permanganate, potassium manganate, manganese sulfate, and manganese nitrate.
[0013] A further improvement of the technical solution of the present invention is that the carrier needs to be dehydrated and degassed before treatment. The specific steps are to place the carrier in an oven, dry it at 180°C for 4 hours, cool it to room temperature, and then degas it under inert gas for 1 hour.
[0014] A further improvement of the technical solution of the present invention is that: in the step 2, when the carrier component is easily eluted out of the aqueous solution, or when the active component to be loaded is insoluble in water, an alcohol or hydrocarbon solvent needs to be used. If the concentration is too high, the active component is unevenly distributed in the pores, and coarser metal particles with uneven particle size distribution are easily obtained; if the concentration is too low, one impregnation cannot meet the requirements, and multiple impregnations are required, which is time-consuming and labor-intensive. When the required loading amount is lower than the saturated adsorption amount, a dilute concentration impregnation solution should be used for impregnation, and the impregnation time should be extended or a competitive adsorbent should be used to ensure that the adsorbed active components are evenly distributed.
[0015] A further improvement of the technical solution of the present invention is that in step three, the catalyst is dried in a drying oven at about 80° C. for 10-12 hours to remove the solvent and water remaining in the impregnation process, thereby avoiding poisoning of the catalyst and making the catalyst reach a pure state, thereby better exerting its catalytic activity.
[0016] A further improvement of the technical solution of the present invention is that in step 4, microcrystal sintering is performed to improve the mechanical strength, remove volatile components in the carrier to form a stable structure, and enable the carrier to obtain a certain crystal form, grain size, pore structure and specific surface area.
[0017] A further improvement of the technical solution of the present invention is that after the catalyst is cooled and taken out in step 5, it needs to be post-processed, including washing with a washing device and secondary calcination to remove residual ions and substances and improve the specific surface area and thermal stability of the catalyst.
[0018] A further improvement of the technical solution of the present invention is that in step three, in addition to the active component, an appropriate amount of a second component can be added to the impregnation solution. The carrier adsorbs the second component while adsorbing the active component. The added second component is also called a competitive adsorbent. This effect is called competitive adsorption. Adding an appropriate amount of competitive adsorbent can make the active component evenly distributed. Commonly used competitive adsorbents include citric acid, tartaric acid, hydrochloric acid, oxalic acid, lactic acid, and trichloroacetic acid.
[0019] The preparation and use of multivalent metal catalysts are characterized by: including the chemical field and the energy field. In the polymerization reaction in the chemical field, the multivalent metal catalyst can promote the combination between monomers to form polymer materials. In the liquid phase oxidation reaction, the multivalent metal catalyst can introduce gaseous oxygen into the liquid phase to improve the reaction efficiency and selectivity. In the olefin hydrogenation reaction, the multivalent metal catalyst can react olefins with hydrogen to produce alkanes. In the energy field, it can catalyze the conversion of renewable energy and serve as an electrode catalyst in fuel cells to reduce the operating temperature and cost of fuel cells.
[0020] Due to the adoption of the above technical solution, the present invention has the following technical advancements compared to the prior art:
[0021] 1. The present invention provides a method for preparing and using a multivalent metal catalyst. By drying the wet carrier in a drying oven, the solvent and water remaining in the impregnation process are removed, thereby avoiding poisoning of the multivalent metal catalyst, making the multivalent metal catalyst reach a pure state, better exerting its catalytic activity, and making the obtained multivalent metal catalyst safer and of higher quality.
[0022] 2. The present invention provides a method for preparing and using a multivalent metal catalyst. The cooled catalyst is washed using a washing device and subjected to secondary calcination to remove residual ions and substances in the catalyst, thereby increasing the specific surface area and thermal stability of the catalyst.
[0023] 3. The present invention provides a method for preparing a multivalent metal catalyst and its use, wherein the active components are evenly distributed by adding competitive adsorbents such as citric acid, tartaric acid, hydrochloric acid, oxalic acid, lactic acid, and trichloroacetic acid to the impregnation solution. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 Schematic diagram of the structure of the present invention. DETAILED DESCRIPTION
[0025] The present invention is described in further detail below in conjunction with the embodiments:
[0026] Example 1
[0027] like Figure 1As shown, the present invention provides a method for preparing a multivalent metal catalyst, comprising the following steps:
[0028] Step 1: Raw material preparation: Select appropriate carrier and catalyst active material, and carry out crushing and mixing pretreatment;
[0029] Step 2: Impregnation: Immerse the carrier in a solution of the catalyst active substance to evenly distribute the catalyst on the carrier surface;
[0030] Step 3: Drying: Dry the wet carrier to make the catalyst active material completely adhere to the carrier surface;
[0031] Step 4: Calcination: Place the carrier into a furnace and calcine at high temperature to completely fix the catalyst on the carrier;
[0032] Step 5: Cooling: After the calcination is completed, cool the furnace to room temperature and take out the catalyst.
[0033] In this embodiment, since adsorption is an exothermic reaction, a high temperature of the impregnation liquid is not conducive to the adsorption of active components. However, if the temperature of the impregnation liquid is too low, the active components will be crystallized and precipitated. It should be controlled at an appropriate temperature. Step 2 adopts an excess impregnation method, in which the carrier is immersed in excess solution. The volume of the solution is greater than the volume of liquid that can be adsorbed by the carrier. The excess liquid is removed after a period of time. The impregnation process usually generates a large amount of adsorption heat, which increases the temperature of the impregnation liquid. Some impregnation liquids have a low pH value, which will adversely affect the structure and strength of the catalyst due to the action of the acid. The use of water blister treatment can reduce the impact of adsorption heat. The drying process can improve the thermal stability and moisture resistance of the catalyst and extend the service life of the catalyst. If residual substances exist in the catalyst for too long, it may cause the deactivation of the catalyst or reduce its activity.
[0034] Example 2
[0035] like Figure 1As shown, based on Example 1, the present invention provides a technical solution: Preferably, in the step 1, the carrier requires high mechanical strength, suitable particle shape and size, suitable surface area, pore structure, etc., good heat resistance, good thermal conductivity, sufficient water absorption, the carrier is inert, does not react chemically with the impregnation solution, does not contain catalyst poisons and substances that cause side reactions, the raw materials are easily available, the preparation is simple, and there is no pollution, including alumina, silica gel, molecular sieves, activated carbon, diatomaceous earth, pumice, activated white clay, and carbon fiber. The catalyst active substance can be selected from ferric permanganate, potassium manganate, manganese sulfate, and manganese nitrate. The carrier needs to be dehydrated and degassed before treatment. The specific steps are to place the carrier in an oven, dry it at 180°C for 4h, cool it to room temperature, and degas it under inert gas for 1h. In the step 2, when the carrier component is easily eluted in the aqueous solution, or when the active component to be loaded is insoluble in water, an alcohol or hydrocarbon solvent needs to be used. If the concentration is too high, the active component The components are unevenly distributed in the pores, and coarse metal particles with uneven particle size distribution are easily obtained; if the concentration is too low, one impregnation cannot meet the requirements, and multiple impregnations are required, which is time-consuming and labor-intensive. When the required loading capacity is lower than the saturated adsorption capacity, a dilute concentration impregnation solution should be used for impregnation, and the impregnation time should be extended or a competitive adsorbent should be used to uniformly distribute the adsorbed active components. In the step three, the solvent and water remaining in the impregnation process are removed by drying in a drying oven at about 80°C for 10-12 hours to avoid catalyst poisoning and to achieve a pure state of the catalyst, thereby better exerting its catalytic activity. In the step four, microcrystal sintering is performed to improve mechanical strength, remove volatile components in the carrier to form a stable structure, and enable the carrier to obtain a certain crystal form, grain size, pore structure and specific surface area. After the catalyst is cooled and removed in the step five, post-treatment is required, including washing with a washing device and secondary calcination to remove residual ions and substances and improve the specific surface area and thermal stability of the catalyst.
[0036] Example 3
[0037] like Figure 1 As shown, based on Example 1, the present invention provides a technical solution: Preferably, in step three, in addition to the active component, an appropriate amount of a second component can be added to the impregnation solution. The carrier adsorbs the second component while adsorbing the active component. The added second component is also called a competitive adsorbent. This effect is called competitive adsorption. Adding an appropriate amount of competitive adsorbent can make the active component evenly distributed. Commonly used competitive adsorbents include citric acid, tartaric acid, hydrochloric acid, oxalic acid, lactic acid, and trichloroacetic acid.
[0038] Example 4
[0039] like Figure 1As shown, based on Example 1, the present invention provides a use for the preparation of a multivalent metal catalyst, which is characterized in that it includes the chemical field and the energy field. In the polymerization reaction in the chemical field, the multivalent metal catalyst can promote the combination between monomers to form a polymer material. In the liquid phase oxidation reaction, the multivalent metal catalyst can introduce gaseous oxygen into the liquid phase to improve the reaction efficiency and selectivity. In the olefin hydrogenation reaction, the multivalent metal catalyst can react olefins with hydrogen to form alkanes. In the energy field, it can catalyze the conversion of renewable energy and serve as an electrode catalyst in a fuel cell to reduce the operating temperature and cost of the fuel cell.
[0040] The working principle of the method for preparing the multivalent metal catalyst will be described in detail below.
[0041] like Figure 1 As shown, the carrier is immersed in a liquid containing an active substance, and the active substance is gradually adsorbed on the surface of the carrier. When the impregnation equilibrium is reached, the remaining liquid is removed, and then drying, calcination, activation and other steps are carried out to finally obtain a polyvalent metal catalyst.
[0042] While the present invention has been generally described above, modifications and improvements are readily apparent to those skilled in the art. Therefore, modifications and improvements that do not depart from the spirit of the present invention are intended to be within the scope of the present invention.
Claims
1. Preparation method of multivalent metal catalyst, Features: The following steps are involved: Step 1: Raw material preparation: Select appropriate carrier and catalyst active material, and perform crushing and mixing pretreatment; Step 2: Impregnation: Immerse the carrier in a solution of the catalyst active substance so that the catalyst is evenly distributed on the surface of the carrier; Step 3: Drying: Dry the wet carrier so that the catalyst active substances are completely attached to the surface of the carrier; Step 4: Calcination: Place the carrier into a furnace and calcine at high temperature to completely fix the catalyst on the carrier; Step 5: Cooling: After the calcination is completed, cool the furnace to room temperature and take out the catalyst.
2. The method for preparing a multivalent metal catalyst according to claim 1, Features: The carrier in step 1 is required to have high mechanical strength, suitable particle shape and size, appropriate surface area, pore structure, etc., good heat resistance, good thermal conductivity, sufficient water absorption, the carrier is inert, does not react chemically with the impregnation solution, does not contain catalyst poisons and substances that cause side reactions, and has readily available raw materials, simple preparation, and no pollution. The carrier includes alumina, silica gel, molecular sieve, activated carbon, diatomaceous earth, pumice, activated clay, and carbon fiber. The catalyst active substance can be selected from ferric permanganate, potassium manganate, manganese sulfate, and manganese nitrate.
3. The method for preparing a multivalent metal catalyst according to claim 2, Features: The carrier needs to be dehydrated and degassed before treatment. The specific steps are to place the carrier in an oven, dry it at 180° C. for 4 hours, cool it to room temperature, and degas it under inert gas for 1 hour.
4. The method for preparing a multivalent metal catalyst according to claim 1, Features: In the step 2, when the carrier component is easily eluted out in the aqueous solution, or when the active component to be loaded is insoluble in water, alcohol or hydrocarbon solvents need to be used. If the concentration is too high, the active component is unevenly distributed in the pores, and coarser metal particles with uneven particle size distribution are easily obtained; if the concentration is too low, one impregnation cannot meet the requirements and multiple impregnations are required, which is time-consuming and labor-intensive. When the required loading amount is lower than the saturated adsorption amount, dilute concentration impregnation solution should be used for impregnation, and the impregnation time should be extended or a competitive adsorbent should be used to make the adsorbed active components evenly distributed.
5. The method for preparing a multivalent metal catalyst according to claim 1, Features: In step three, the catalyst is dried in a drying oven at about 80° C. for 10-12 hours to remove the residual solvent and water in the impregnation process, avoid poisoning of the catalyst, and make the catalyst reach a pure state, so as to better exert its catalytic activity.
6. The method for preparing a multivalent metal catalyst according to claim 1, Features: In the step 4, microcrystal sintering is performed to improve the mechanical strength, remove volatile components in the carrier to form a stable structure, and enable the carrier to obtain a certain crystal form, grain size, pore structure and specific surface area.
7. The method for preparing a multivalent metal catalyst according to claim 1, Features: After the catalyst is cooled and taken out in step 5, it needs to be post-processed, including washing with a washing device and secondary calcination to remove residual ions and substances and increase the specific surface area and thermal stability of the catalyst.
8. The method for preparing a multivalent metal catalyst according to claim 3, Features: In the step three, in addition to the active component, an appropriate amount of a second component can be added to the impregnation solution. The carrier adsorbs the second component while adsorbing the active component. The added second component is also called a competitive adsorbent. This effect is called competitive adsorption. Adding an appropriate amount of competitive adsorbent can make the active component evenly distributed. Commonly used competitive adsorbents include citric acid, tartaric acid, hydrochloric acid, oxalic acid, lactic acid, and trichloroacetic acid.
9. Preparation and use of multivalent metal catalysts, Features: Including the chemical field and the energy field, in the polymerization reaction in the chemical field, the multivalent metal catalyst can promote the combination of monomers to form polymer materials, in the liquid phase oxidation reaction, the multivalent metal catalyst can introduce gaseous oxygen into the liquid phase to improve the reaction efficiency and selectivity, in the olefin hydrogenation reaction, the multivalent metal catalyst can react olefins with hydrogen to generate alkanes, and in the energy field, it can catalyze the conversion of renewable energy and serve as an electrode catalyst in fuel cells to reduce the operating temperature and cost of fuel cells.