Beneficiation equipment and beneficiation method for fluorite and scheelite associated ore
By designing ore dressing equipment for fluorite and syringe associated ore, using X-ray imaging detection and multi-stage crushing process, one-time sorting of fluorite and syringe is realized, solving the problems of difficulty and high cost of sorting of associated ore, and improving the problem of improved Concentrate grade and recovery rate.
Patent Information
- Application Number
- CN202411330328.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-24
- Publication Date
- 2024-11-19
AI Technical Summary
The separation of fluorite and syringe tungsten ore is difficult. The existing technology requires two different ore dressing equipment, which leads to high cost and high concentration impurities, making it difficult to obtain high-grade fluorite and syringe tungsten concentrate.
A mineral processing equipment including crushing barrels, sorting barrels, flotation barrels and acid-leaching barrels was designed. Through X-ray imaging detection and multi-stage crushing process, one-time sorting of fluorite and syringe are realized, simplifying the sorting process and improving the efficiency.
The recovery rate of fluorite and scheelite is improved, the sorting process is simplified, the cost is reduced, the concentrate obtained is of high grade, and the recovery rate of fluorite is significantly improved.
Smart Images

Figure CN118976592A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of mineral separation, and in particular to a mineral separation device and a mineral separation method for fluorite and scheelite associated minerals. Background Art
[0002] Fluorite ore usually contains high mud content and impurity minerals coexist with fluorite, so it is difficult to separate fluorite. Especially when fluorite is coexisting with scheelite, since both fluorite and scheelite are high-value minerals, the existing beneficiation technology requires the use of two different beneficiation equipment to separate scheelite and fluorite ores, which not only leads to high costs, but also the separation process for fluorite and scheelite co-ordinating ores is usually more complicated. When the existing beneficiation process is used to beneficiate fluorite and scheelite co-ordinating ores, the obtained concentrate contains more impurities, making it difficult to obtain high-grade fluorite and scheelite concentrates. Summary of the invention
[0003] In view of the above analysis, the present application aims to provide a fluorite and scheelite associated ore beneficiation equipment and a scheelite beneficiation method, which can separate fluorite and scheelite at one time and improve the separation efficiency of fluorite and scheelite associated ore.
[0004] The purpose of this application is mainly achieved through the following technical solutions:
[0005] On the one hand, the embodiment of the present application provides a fluorite and scheelite associated ore beneficiation equipment, including:
[0006] A first crushing barrel, used for crushing the ore to a first preset particle size to obtain coarse ore;
[0007] A sorting barrel is connected to the first crushing barrel, the sorting barrel comprises a sorting device, a first sorting outlet, a second sorting outlet and a third sorting outlet, the sorting device sorts the coarse ore into coarse scheelite ore and coarse fluorite ore by X-rays; the coarse scheelite ore and the coarse fluorite ore fall into the first sorting outlet and the second sorting outlet in sequence;
[0008] The second crushing barrel is connected to the first sorting outlet and is used to crush the coarse scheelite ore into a second preset particle size;
[0009] A third crushing barrel is connected to the second sorting outlet and is used to crush the coarse fluorite ore into a third preset particle size;
[0010] A flotation barrel, connected to the second crushing barrel, is used to float out scheelite concentrate and scheelite tailings;
[0011] The acid leaching barrel is connected to the flotation gate and the third crushing barrel and is used to acid leach the scheelite tailings and fluorite rough ore into fluorite concentrate.
[0012] According to one aspect of the embodiment of the present application, the first crushing barrel includes: a first feed port, a first crushing device and a first discharge port, the first feed port is located at the top of the first crushing barrel, and the first discharge port is located at the bottom of the first crushing barrel; the first discharge port is provided with a bottom plate inclined relative to both the vertical direction and the horizontal direction, the bottom plate is provided with a plurality of first openings smaller than the first preset particle size, and the diameter of the first discharge port is 1-1.5 times the first preset particle size; the second crushing barrel includes a second feed port, a second crushing device and a second discharge port, the second feed port is connected to the first sorting discharge port The second discharge port is provided with a bottom plate inclined relative to both the vertical and horizontal directions, the bottom plate is provided with a plurality of second openings smaller than the second preset particle size, and the diameter of the second discharge port is 1-1.5 times the second preset particle size; the third crushing barrel includes a third feed port, a third crushing device and a third discharge port, and the third feed port is connected to the first sorting discharge port; the third discharge port is provided with a bottom plate inclined relative to both the vertical and horizontal directions, the bottom plate is provided with a plurality of third openings smaller than the third preset particle size, and the diameter of the third discharge port is 1-1.5 times the third preset particle size.
[0013] According to one aspect of an embodiment of the present application, the sorting device includes: an X-ray emitting component for irradiating X-rays to the coarse ore; an imaging component for acquiring an image of the coarse ore reflecting the X-rays; an analyzing component for analyzing the image to obtain the content of scheelite and the content of fluorite in the coarse ore; and a guiding component for changing the falling direction of the coarse ore according to the content of scheelite and the content of fluorite.
[0014] According to one aspect of an embodiment of the present application, the sorting barrel also includes: a conveying component that conveys coarse ore in a horizontal direction; a guide component that is rotatably arranged at the end of the conveying component; a first sorting discharge port, a second sorting discharge port and a third sorting discharge port that are vertically and parallelly arranged in a horizontal direction below the guide component.
[0015] According to one aspect of an embodiment of the present application, a recovery pipeline is provided below the bottom plate of the first discharge port of the first crushing barrel, and the recovery pipeline is connected to the second feed port of the second crushing barrel.
[0016] On the other hand, an embodiment of the present application provides a method for beneficiating fluorite and scheelite associated ores, characterized in that the beneficiation equipment for fluorite and scheelite associated ores according to one aspect of an embodiment of the present application is used; the method for beneficiating fluorite and scheelite associated ores includes: step 1, crushing the ore to a first preset particle size to form a coarse ore; step 2, sorting the coarse ore by X-rays to obtain coarse scheelite ore and coarse fluorite ore; step 3, crushing the coarse scheelite ore to a second preset particle size to form fine scheelite ore, and crushing the coarse fluorite ore to a third preset particle size to form fine fluorite ore; step 4, flotation of the fine scheelite ore to obtain scheelite concentrate and scheelite tailings; step 5, acid leaching the scheelite tailings and the fluorite fine ore together to obtain fluorite concentrate.
[0017] According to another aspect of the embodiment of the present application, in step 1, the particle size of the coarse ore is 1-1.5 times the first preset particle size.
[0018] According to another aspect of the embodiment of the present application, in step 2, the coarse ore is irradiated with X-rays and an image is taken, and the fluorite content and the scheelite content in the coarse ore are determined based on the attenuation of the X-rays in the image; when the scheelite content is greater than or equal to a first threshold value, the corresponding coarse ore is sorted as coarse scheelite ore, and when the scheelite content is less than the first threshold value and the fluorite content is greater than or equal to a second threshold value, the corresponding coarse ore is sorted as coarse fluorite ore.
[0019] According to another aspect of the embodiment of the present application, in step 4, after the fine scheelite ore is floated, the sink is the scheelite concentrate and the float is the scheelite tailings.
[0020] According to another aspect of the embodiment of the present application, in step 5, after the scheelite tailings and the fluorite fine ore are acid-leached together, the undissolved matter is the fluorite concentrate.
[0021] Compared with the prior art, the present invention has at least one of the following beneficial effects:
[0022] (a) The present application uses the first crushing barrel to crush the ore into suitable sizes, so that in the subsequent X-ray sorting, the scheelite content and fluorite content can be obtained more accurately, thereby making the sorting process of the sorting barrel more accurate and reliable.
[0023] (b) In the present application, after the flotation of the coarse scheelite ore, the scheelite tailings containing fluorite are acid-leached together with the fluorite fine ore to obtain fluorite concentrate, thereby fully obtaining the fluorite in the ore and improving the recovery rate of the fluorite.
[0024] (c) The present application adopts an integrated device that can separate fluorite and scheelite from fluorite and scheelite associated ores at one time, thereby simplifying the separation process, improving the separation efficiency, and obtaining a high-grade concentrate.
[0025] In the present application, the above-mentioned technical solutions can also be combined with each other to achieve more preferred combination solutions. Other features and advantages of the present application will be described in the subsequent description, and some advantages can become obvious from the description, or can be understood by practicing the present application. The purpose and other advantages of the present application can be realized and obtained through the contents particularly pointed out in the description and the drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] The accompanying drawings are only for the purpose of illustrating specific embodiments and are not to be considered as limiting the present application. The same reference symbols denote the same components throughout the accompanying drawings.
[0027] Figure 1 A schematic diagram of the structure of a ore dressing device for fluorite and scheelite associated ores according to an embodiment of the present application;
[0028] Figure 2 A structural schematic diagram of the first crushing barrel of the ore dressing equipment for fluorite and scheelite associated ores in the embodiment of the present application.
[0029] Figure 3 A structural schematic diagram of the second crushing barrel and the third crushing barrel of the ore dressing equipment for fluorite and scheelite associated ores in the embodiment of the present application.
[0030] Figure 4 This is a schematic diagram of the internal structure of the second crushing barrel and the third crushing barrel of the ore dressing equipment for fluorite and scheelite associated ores in the embodiment of the present application.
[0031] Figure 5 A flow chart of the beneficiation method of fluorite and scheelite associated ores according to an embodiment of the present application.
[0032] Reference numerals:
[0033] 1. The first crushing barrel; 11. The first discharge port;
[0034] 2. Sorting barrel; 21. X-ray emission assembly; 22. Imaging assembly; 23. Guide assembly; 24. Conveying assembly; 25. First sorting outlet; 26. Second sorting outlet;
[0035] 3. Second crushing barrel; 31. Second discharge port;
[0036] 4. The third crushing barrel; 41. The third discharge port;
[0037] 5. Flotation tank;
[0038] 6. Acid leaching barrel. DETAILED DESCRIPTION
[0039] The preferred embodiments of the present application are described in detail below in conjunction with the accompanying drawings, wherein the accompanying drawings constitute a part of the present application and are used together with the embodiments of the present application to illustrate the principles of the present application, and are not used to limit the scope of the present application.
[0040] In the description of the embodiments of the present application, it should be noted that, unless otherwise clearly specified and limited, the term "connected" should be understood in a broad sense, for example, it can be a fixed connection, or a detachable connection, or an integral connection can be a mechanical connection, or an electrical connection can be a direct connection, or it can be indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0041] The terms "top", "bottom", "above", "lower", and "on" used throughout the description are relative to the relative positions of components of a device, such as the relative positions of the top and bottom substrates within a device. It is understood that devices are multifunctional regardless of their orientation in space.
[0042] Example 1
[0043] The applicant discovered that in the process of sorting fluorite ore to obtain fluorite, the fluorite ore is usually associated with scheelite. Considering that the utilization value of scheelite is also relatively high, it is necessary to sort out fluorite and scheelite separately for the associated ores of fluorite and scheelite. Usually, fluorite and scheelite are sorted separately for the associated ores of fluorite and scheelite. During the sorting process, there will be a small amount of loss of scheelite and fluorite, so the recovery rate is low. In order to improve the recovery rate, it is often necessary to add more sorting steps, resulting in a decrease in sorting efficiency.
[0044] In view of the above analysis, the applicant proposed a beneficiation equipment and method for fluorite and scheelite associated ore, firstly crushing the ore into coarse ore by a first crushing barrel, sorting the coarse ore into coarse scheelite ore and coarse fluorite ore by a combination of a sorting barrel, crushing the coarse scheelite ore into fine scheelite ore by a second crushing barrel, crushing the coarse fluorite ore into fine fluorite ore by a third crushing barrel, sorting the fine scheelite ore into scheelite concentrate and scheelite tailings by a flotation barrel, and forming fluorite concentrate from the scheelite tailings and fluorite fine ore by an acid leaching barrel. The use of integrated equipment combined with X-ray imaging detection can realize the separation of fluorite and scheelite in fluorite and scheelite associated ore at one time, simplifying the separation process and improving the separation efficiency. After the flotation of the coarse scheelite ore, the scheelite tailings containing fluorite are acid-leached together with the fluorite fine ore to obtain the fluorite concentrate, thereby fully obtaining the fluorite in the ore and improving the recovery rate of fluorite.
[0045] Figure 1 A structural schematic diagram of the ore dressing equipment for fluorite and scheelite associated ores according to an embodiment of the present application. Figure 2 A structural schematic diagram of the first crushing barrel of the ore dressing equipment for fluorite and scheelite associated ores in the embodiment of the present application. Figure 3 A structural schematic diagram of the second crushing barrel and the third crushing barrel of the ore dressing equipment for fluorite and scheelite associated ores in the embodiment of the present application. Figure 4 This is a schematic diagram of the internal structure of the second crushing barrel and the third crushing barrel of the ore dressing equipment for fluorite and scheelite associated ores in the embodiment of the present application.
[0046] Specifically, refer to Figures 1 to 4 The embodiment of the present application provides a ore dressing device for fluorite and scheelite associated ore, comprising:
[0047] The first crushing barrel 1 is used to crush the ore to a first preset particle size to obtain coarse ore;
[0048] The sorting barrel 2 is connected to the first crushing barrel 1, and the sorting barrel 2 includes a sorting device, a first sorting outlet 25, a second sorting outlet 26 and a third sorting outlet. The sorting device sorts the coarse ore into coarse scheelite ore and coarse fluorite ore by X-rays; the coarse scheelite ore and the coarse fluorite ore fall into the first sorting outlet 25 and the second sorting outlet 26 in sequence;
[0049] The second crushing barrel 3 is connected to the first sorting outlet 25 and is used to crush the coarse scheelite ore into a second preset particle size;
[0050] The third crushing barrel 4 is connected to the second sorting outlet 26 and is used to crush the coarse fluorite ore into a third preset particle size;
[0051] The flotation tank 5 is connected to the second crushing tank 3 and is used for floating out the scheelite concentrate and scheelite tailings;
[0052] The acid leaching tank 6 is connected to the flotation gate and the third crushing tank 4, and is used for acid leaching the scheelite tailings and the fluorite coarse ore to form fluorite concentrate.
[0053] The embodiment of the present application adopts a multi-stage barrel structure from top to bottom as a whole, and the first crushing barrel 1, the sorting barrel 2, the second crushing barrel 3, the third crushing barrel 4, the flotation barrel 5 and the acid leaching barrel 6 are arranged from top to bottom.
[0054] In the process of mineral processing, the gravity of the ore itself can be used to improve the sorting efficiency and save the sorting cost.
[0055] The first crushing barrel 1 is used to pre-treat the ore and crush the ore to a first preset particle size so that the overall size of the coarse ore obtained after crushing is basically the same, which is convenient for the subsequent X-ray sorting of the sorting barrel 2. The first preset particle size can be determined according to the X-ray detection capability of the sorting barrel 2, and it is necessary to be able to obtain the content of fluorite and scheelite in the coarse ore after X-ray detection.
[0056] The sorting barrel 2 sorts the coarse ore into coarse scheelite ore and coarse fluorite ore through X-ray detection. The sorting device can display the process of X-ray detection, irradiate the coarse ore with X-rays, obtain the image of the X-rays, analyze the attenuation effect in the X-ray image, and thus determine the mineral composition and content in the coarse ore. In other words, the sorting device can sort the coarse ore into coarse scheelite ore and coarse fluorite ore according to the content of fluorite and scheelite. Since the particle size of the coarse ore is basically the same, the error generated by a single coarse ore particle during the sorting process is basically the same, making the sorting result more scientific and reliable. After sorting, the coarse scheelite ore falls into the first sorting discharge port 25, and the coarse fluorite ore falls into the second sorting discharge port 26. In addition, since the sorting barrel 2 can simultaneously sort the coarse scheelite ore and the coarse fluorite ore, the multiple sorting process is omitted, so the embodiment of the present application can greatly simplify the sorting process and reduce the sorting cost.
[0057] The second crushing barrel 3 is used to further crush the coarse scheelite ore to obtain fine scheelite ore with a smaller particle size, so as to facilitate the subsequent scheelite flotation process.
[0058] The third crushing barrel 4 is used to further crush the fluorite coarse ore to obtain fluorite fine ore with a smaller particle size, so as to facilitate the subsequent fluorite acid leaching process. It should be noted that the crushing of the scheelite coarse ore by the second crushing barrel 3 and the crushing of the fluorite coarse ore by the third crushing barrel 4 can be carried out synchronously and in parallel to further improve the ore dressing efficiency of the embodiment of the present application.
[0059] The flotation tank 5 uses flotation to recover scheelite concentrate from scheelite fine ore. During the flotation process, the scheelite concentrate will settle in the flotation reagent, while the scheelite tailings containing fluorite components will float on the surface of the flotation reagent. The scheelite tailings can be recovered together with the fluorite fine ore to improve the recovery rate of the embodiment of the present application.
[0060] Acid leaching barrel 6 is generally used to recover fluorite concentrate in the form of acid leaching. The impurities in the scheelite tailings after flotation and the fluorite fine ore after crushing are mainly carbonates. Therefore, the carbonate impurities can be removed by acid leaching, and the insoluble matter obtained is the fluorite concentrate.
[0061] It can be understood that the fluorite and scheelite associated ore dressing equipment of the embodiment of the present application has a unified shell, and the first crushing barrel 1, the separation barrel 2, the second crushing barrel 3, the third crushing barrel 4, the flotation barrel 5, and the acid leaching barrel 6 are all arranged in the unified shell and arranged in sequence from top to bottom to provide a stable environment for the ore dressing process. For ease of understanding, in the embodiment of the present application, Figures 1 to 4 The shell is hidden in the middle.
[0062] The embodiment of the present application adopts an integrated device, and can separate fluorite and scheelite from fluorite and scheelite associated ore at one time through X-ray imaging detection during separation, thereby simplifying the separation process, improving separation efficiency, and reducing separation costs. After the flotation of the coarse scheelite ore, the scheelite tailings containing fluorite are acid-leached together with the fluorite fine ore to obtain fluorite concentrate, thereby fully obtaining the fluorite in the ore and improving the recovery rate of fluorite.
[0063] Further, the first crushing barrel 1 includes: a first feed port, a first crushing device and a first discharge port 11, the first feed port is located at the top of the first crushing barrel 1, and the first discharge port 11 is located at the bottom of the first crushing barrel 1; the first discharge port 11 is provided with a bottom plate inclined relative to both the vertical direction and the horizontal direction, the bottom plate is provided with a plurality of first openings smaller than the first preset particle size, and the diameter of the first discharge port 11 is 1-1.5 times the first preset particle size; the second crushing barrel 3 includes a second feed port, a second crushing device and a second discharge port 31, and the second feed port is connected to the first sorting discharge port 25; The second discharge port 31 is provided with a bottom plate inclined relative to both the vertical and horizontal directions, the bottom plate is provided with a plurality of second openings smaller than the second preset particle size, and the diameter of the second discharge port 31 is 1-1.5 times the second preset particle size; the third crushing barrel 4 includes a third feed port, a third crushing device and a third discharge port 41, and the third feed port is connected to the first sorting discharge port 25; the third discharge port 41 is provided with a bottom plate inclined relative to both the vertical and horizontal directions, the bottom plate is provided with a plurality of third openings smaller than the third preset particle size, and the diameter of the third discharge port 41 is 1-1.5 times the third preset particle size.
[0064] The main body of the first crushing barrel 1 is cylindrical, and the bottom is an inclined bottom plate. The bottom plate is provided with a plurality of first openings smaller than the first preset particle size, so that the particles with smaller particle size after crushing will directly fall from the first opening to form the first tailings, and the coarse ore with substantially the same particle size obtained after crushing will fall from the first discharge port 11, and the particle size of the obtained coarse ore is substantially 1-1.5 times the first preset particle size. Rotating crushing blades can be arranged inside the crushing barrel to crush the ore. Similarly, the main body of the second crushing barrel 3 is cylindrical, and the bottom is an inclined bottom plate. The bottom plate is provided with a plurality of second openings smaller than the second preset particle size, so that the particles with smaller particle size after crushing will directly fall from the second opening to form the second tailings, and the fine scheelite ore with substantially the same particle size obtained after crushing will fall from the second discharge port 31, and the particle size of the fine scheelite ore is substantially 1-1.5 times the second preset particle size. Rotating crushing blades can be arranged inside the crushing barrel to crush the coarse scheelite ore. The main body of the third crushing barrel 4 is cylindrical, and the bottom is an inclined bottom plate, and the bottom plate is provided with a plurality of third openings smaller than the third preset particle size, so that the particles with smaller particle size after crushing will directly fall from the third openings to form the third tailings, and the fluorite fine ore with basically the same particle size obtained after crushing will fall from the third discharge port 41, and the particle size of the obtained fluorite fine ore is basically 1-1.5 times the third preset particle size. Rotating crushing blades can be arranged inside the crushing barrel to crush the fluorite coarse ore.
[0065] Furthermore, the sorting device includes: an X-ray emitting component 21, used to irradiate X-rays to the coarse ore; an imaging component 22, used to obtain an image of the coarse ore reflecting the X-rays; an analysis component, used to analyze the image to obtain the content of scheelite and the content of fluorite in the coarse ore; a guide component 23, used to change the falling direction of the coarse ore according to the content of scheelite and the content of fluorite.
[0066] The sorting device performs sorting by X-ray detection. The X-ray emitting component 21 can emit X-rays toward the coarse ore, and the coarse ore will reflect the X-rays. The imaging component 22 shoots the coarse ore to obtain an X-ray image of the coarse ore. Different mineral components in the coarse ore correspond to different attenuation degrees of the reflected X-rays. The analysis component determines the attenuation degree of the X-rays based on the obtained X-ray image, thereby determining the content of scheelite and the content of fluorite in the coarse ore. According to the content of scheelite and the content of fluorite in the coarse ore, the guide component 23 adjusts the falling direction of the coarse ore so that the coarse scheelite ore falls into the first sorting outlet 25, and the coarse fluorite ore falls into the second sorting outlet 26. Among them, when the scheelite content is greater than or equal to the first threshold value, the corresponding coarse ore is sorted as coarse scheelite ore, and when the scheelite content is less than the first threshold value and the fluorite content is greater than or equal to the second threshold value, the corresponding coarse ore is sorted as coarse fluorite ore. Therefore, crude scheelite ore may contain fluorite, but crude fluorite ore basically does not contain scheelite. After the scheelite concentrate is recovered by flotation, the scheelite tailings may contain fluorite. Simultaneous acid leaching of the scheelite tailings and fluorite fine ore can improve the recovery rate of fluorite and ensure the recovery rate of scheelite.
[0067] Furthermore, the sorting barrel 2 also includes: a conveying component 24, which conveys coarse ore in the horizontal direction; a guide component 23 rotatably arranged at the end of the conveying component 24; a first sorting discharge port 25, a second sorting discharge port 26 and a third sorting discharge port are vertically and parallelly arranged below the guide component 23 in the horizontal direction.
[0068] During X-ray detection, the conveying assembly 24 can keep the coarse ore stable, thereby ensuring the accuracy of sorting. The guide assembly 23 changes the falling position of the coarse ore by rotating, so that the coarse scheelite ore falls into the first sorting outlet 25 and the coarse fluorite ore falls into the second sorting outlet 26, thereby achieving the purpose of sorting.
[0069] It should be noted that the sorting barrel 2 also includes a third sorting outlet. When the scheelite content is less than the first threshold value and the fluorite content is less than the second threshold value, the coarse ore basically does not contain scheelite and / or fluorite, and the guide component 23 causes it to fall from the third sorting outlet to form sorting tailings.
[0070] Furthermore, a recovery pipeline is provided below the bottom plate of the first discharge port 11 of the first crushing barrel 1 , and the recovery pipeline is connected to the second feed port of the second crushing barrel 3 .
[0071] The small-particle first tailings that fall from the first opening of the bottom plate in the first crushing barrel 1 have not been sorted by the sorting barrel 2, and therefore may still contain a small amount of fluorite and / or scheelite. After the first tailings are introduced into the second crushing barrel 3 through the recovery pipeline, they are further crushed along with the crude scheelite, and then through flotation and / or acid leaching, the fluorite and / or scheelite in the first tailings can be recovered, thereby further improving the recovery rate of the embodiment of the present application.
[0072] Figure 5 A flow chart of the beneficiation method of fluorite and scheelite associated ores according to an embodiment of the present application.
[0073] refer to Figure 5 The embodiment of the present application also provides a method for beneficiating fluorite and scheelite associated ore, using the beneficiation equipment for fluorite and scheelite associated ore of the above embodiment of the present application. The method for beneficiating fluorite and scheelite associated ore includes:
[0074] Step 1: crushing the ore to a first preset particle size to form coarse ore.
[0075] The ore is crushed by the first crushing barrel 1, and the particle size of the coarse ore obtained after crushing is basically the same, which can be 1-1.5 times the first preset particle size. The particle size of the coarse ore obtained after crushing is basically the same, so that the result of the subsequent X-ray sorting of the sorting barrel 2 is more accurate and reliable. The first crushing barrel 1 can also obtain a first tailing with a smaller particle size than the coarse ore.
[0076] Step 2: sorting the coarse ore by X-ray to obtain coarse scheelite ore and coarse fluorite ore.
[0077] The coarse ore is sorted into coarse scheelite ore and coarse fluorite ore by sorting barrel 2. The coarse ore is irradiated with X-rays and an image is taken. The fluorite content and the scheelite content in the coarse ore are determined according to the attenuation of the X-rays in the image. When the scheelite content is greater than or equal to the first threshold, the corresponding coarse ore is sorted into coarse scheelite ore; when the scheelite content is less than the first threshold and the fluorite content is greater than or equal to the second threshold, the corresponding coarse ore is sorted into coarse fluorite ore; when the scheelite content is less than the first threshold and the fluorite content is less than the second threshold, the corresponding coarse ore is sorted into sorting tailings.
[0078] Step 3: crushing the coarse scheelite ore to a second preset particle size to form fine scheelite ore, and crushing the coarse fluorite ore to a third preset particle size to form fine fluorite ore.
[0079] The coarse scheelite ore is crushed by the second crushing barrel 3, and the particle size of the fine scheelite ore obtained after crushing is basically the same, which can be 1-1.5 times the second preset particle size. The coarse fluorite ore is crushed by the third crushing barrel 4, and the particle size of the fine fluorite ore obtained after crushing is basically the same, which can be 1-1.5 times the third preset particle size. The crushing process of the coarse scheelite ore and the crushing process of the coarse fluorite ore can be synchronized and parallel. When the coarse scheelite ore is crushed, the first tailings that may contain scheelite and / or fluorite can be introduced to improve the recovery rate of scheelite and fluorite.
[0080] Step 4: flotation the scheelite fine ore to obtain scheelite concentrate and scheelite tailings.
[0081] The scheelite fine ore is floated by the flotation tank 5. After the scheelite fine ore is floated, the sediment is scheelite concentrate and the float is scheelite tailings. The scheelite concentrate can be directly used for further utilization of scheelite. The scheelite tailings may contain fluorite, which is recovered together with the fluorite fine ore.
[0082] Step 5: acid-leach the scheelite tailings and fluorite fine ore together to obtain fluorite concentrate.
[0083] The acid leaching process is carried out by the acid leaching barrel 6. After the scheelite tailings and the fluorite fine ore are acid-leached together, the undissolved matter is the fluorite concentrate. The impurities in the scheelite tailings and the fluorite fine ore are mainly carbonates. After acid leaching, the impurities are dissolved, and the remaining undissolved matter is the fluorite concentrate. The fluorite concentrate can be directly used for further utilization of fluorite.
[0084] Illustratively, the beneficiation equipment and beneficiation method of the fluorite and scheelite associated ore of the embodiment of the present application were used to carry out pre-enrichment industrial tests on the associated low-grade fluorite in the Bayan Obo mining area, realizing the comprehensive recovery of low-grade fluorite resources. Among them, an industrial test line with a daily processing capacity of 1,000 tons was built in combination with the beneficiation equipment of the fluorite and scheelite associated ore of the embodiment of the present application. During the test, the grade of the selected fluorite (CaF2) was 7%-8%, and the grade of the concentrate fluorite was 20%-21%, which was higher than the industrial grade, the enrichment ratio was 150%, and the fluorite grade enrichment effect was significant. At the same time, the fluorite grade of the tailings produced during the test was about 5%-6%, which was lower than the fluorite content (9%) of the current fluorite beneficiation tailings.
[0085] In summary, the embodiments of the present application provide a beneficiation device and a beneficiation method for fluorite and scheelite associated ores. The present application uses a first crushing barrel to crush the ore into suitable sizes, so that in the subsequent X-ray sorting, the scheelite content and fluorite content can be obtained more accurately, thereby making the sorting process of the sorting barrel more accurate and reliable. In the present application, after the flotation of the scheelite coarse ore, the scheelite tailings containing fluorite are acid-leached together with the fluorite fine ore to obtain fluorite concentrate, thereby fully obtaining the fluorite in the ore and improving the recovery rate of fluorite. The present application uses an integrated device to achieve the sorting of fluorite and scheelite in fluorite and scheelite associated ores at one time, which simplifies the sorting process, improves the sorting efficiency, and the obtained concentrate has a high grade.
[0086] The above is only a preferred specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily conceived by any technician familiar with the technical field within the technical scope disclosed in the present application should be covered within the protection scope of the present application.
Claims
1. A ore dressing equipment for fluorite and scheelite associated ore, characterized in that: include: A first crushing barrel, used for crushing the ore to a first preset particle size to obtain coarse ore; a sorting barrel connected to the first crushing barrel, the sorting barrel comprising a sorting device, a first sorting outlet, a second sorting outlet and a third sorting outlet, the sorting device sorting the coarse ore into coarse scheelite ore and coarse fluorite ore by X-rays; the coarse scheelite ore and the coarse fluorite ore fall into the first sorting outlet and the second sorting outlet in sequence; A second crushing barrel, connected to the first sorting outlet, is used to crush the coarse scheelite ore into a second preset particle size; a third crushing barrel, connected to the second sorting outlet, for crushing the fluorite coarse ore into a third preset particle size; A flotation tank connected to the second crushing tank, used for floating out scheelite concentrate and scheelite tailings; The acid leaching tank is connected to the flotation gate and the third crushing tank, and is used for acid leaching the scheelite tailings and the fluorite coarse ore to form fluorite concentrate.
2. The ore dressing equipment for fluorite and scheelite associated ore according to claim 1 is characterized in that: The first crushing barrel comprises: a first feed port, a first crushing device and a first discharge port, wherein the first feed port is located at the top of the first crushing barrel, and the first discharge port is located at the bottom of the first crushing barrel; the first discharge port is provided with a bottom plate inclined relative to both the vertical direction and the horizontal direction, the bottom plate is provided with a plurality of first openings smaller than the first preset particle size, and the diameter of the first discharge port is 1-1.5 times of the first preset particle size; The second crushing barrel comprises a second feed port, a second crushing device and a second discharge port, the second feed port is connected to the first sorting discharge port; the second discharge port is provided with a bottom plate inclined relative to both the vertical direction and the horizontal direction, the bottom plate is provided with a plurality of second openings smaller than the second preset particle size, and the diameter of the second discharge port is 1-1.5 times of the second preset particle size; The third crushing barrel includes a third feed port, a third crushing device and a third discharge port, and the third feed port is connected to the first sorting discharge port; the third discharge port is provided with a bottom plate inclined relative to both the vertical and horizontal directions, and the bottom plate is provided with a plurality of third openings smaller than the third preset particle size, and the diameter of the third discharge port is 1-1.5 times the third preset particle size.
3. The ore dressing equipment for fluorite and scheelite associated ore according to claim 2, characterized in that: The sorting device comprises: An X-ray emitting assembly, used for emitting X-rays to the rough ore; An imaging component for acquiring an image of X-rays reflected by the rough ore; An analysis component, used for analyzing the image to obtain the content of scheelite and the content of fluorite in the rough ore; A guide assembly is used to change the falling direction of the rough ore according to the content of scheelite and the content of fluorite.
4. The ore dressing equipment for fluorite and scheelite associated ore according to claim 2, characterized in that: The sorting barrel also includes: A conveying assembly conveys the coarse ore in a horizontal direction; the guide assembly is rotatably arranged at the end of the conveying assembly; the first sorting outlet, the second sorting outlet and the third sorting outlet are vertically and parallelly arranged below the guide assembly in a horizontal direction.
5. The ore dressing equipment for fluorite and scheelite associated ore according to claim 4, characterized in that: A recovery pipeline is provided below the bottom plate of the first discharge port of the first crushing barrel, and the recovery pipeline is connected to the second feed port of the second crushing barrel.
6. A method for beneficiating fluorite and scheelite associated ore, characterized in that: Ore dressing equipment using the fluorite and scheelite associated ore as described in claims 1 to 5; The ore dressing method of the fluorite and scheelite associated ore comprises: Step 1, crushing the ore to a first preset particle size to form coarse ore; Step 2, sorting the coarse ore by X-ray to obtain coarse scheelite ore and coarse fluorite ore; Step 3, crushing the scheelite coarse ore to a second preset particle size to form scheelite fine ore, and crushing the fluorite coarse ore to a third preset particle size to form fluorite fine ore; Step 4, flotation the scheelite fine ore to obtain scheelite concentrate and scheelite tailings; Step 5: acid-leach the scheelite tailings and fluorite fine ore together to obtain fluorite concentrate.
7. The ore dressing method of fluorite and scheelite associated ore according to claim 6, characterized in that: In step 1, the particle size of the coarse ore is 1-1.5 times the first preset particle size.
8. The ore dressing method of fluorite and scheelite associated ore according to claim 7, characterized in that: In step 2, the coarse ore is irradiated with X-rays and an image is taken, and the fluorite content and the scheelite content in the coarse ore are determined based on the attenuation of the X-rays in the image; when the scheelite content is greater than or equal to a first threshold, the corresponding coarse ore is sorted as coarse scheelite ore; when the scheelite content is less than the first threshold and the fluorite content is greater than or equal to a second threshold, the corresponding coarse ore is sorted as coarse fluorite ore.
9. The ore dressing method of fluorite and scheelite associated ore according to claim 8, characterized in that: In the step 4, after the scheelite fine ore is floated, the sink is the scheelite concentrate and the float is the scheelite tailings.
10. The ore dressing method of fluorite and scheelite associated ore according to claim 9, characterized in that: In step 5, after the scheelite tailings and the fluorite fine ore are acid-leached together, the undissolved matter is the fluorite concentrate.