Repair method for improving wear resistance of end face of turbine rotor blade
Through induction brazing technology and brazing preparation, a high-bound wear-resistant layer is formed, which solves the problem of poor wear resistance on the end surface of the turbine rotor blade, and achieves better wear resistance and high temperature stability. It is suitable for aircraft engine blades Repair.
Patent Information
- Application Number
- CN202411192144.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-11-19
AI Technical Summary
After the existing laser cladding repair, the wear resistance of the end surface of the turbine rotor blade is still poor, and the bonding performance of conventional coatings is poor, making it difficult to meet the needs of high temperature and wear.
The wear-resistant layer is prepared by induction brazing technology. Through the steps of brazing preparation, pre-welding treatment, pre-weld protection, coating of brazing, induction brazing and post-welding grinding, a high-bonding wear-resistant layer is formed, using nickel-based The solder of powder and CBN particles achieves metallurgical bonding, and the wear-resistant layer shape is ensured through a contoured guardrail.
It significantly improves the wear resistance of the blade, enhances the wear resistance of the blade tip, ensures the stability of the blade under high temperature and wear conditions, saves energy, heats local areas, and facilitates automated production.
Smart Images

Figure CN118977058A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of blade repair, in particular to a repair method for improving the wear resistance of a turbine rotor blade end surface. Background Art
[0002] Turbine rotor blades are key components of aircraft engines and are used in harsh environments. The service environment of the blade tip is even worse than that of the blade body. Not only do they have to withstand high temperatures and drastic changes in working stress, they are also prone to corrosion and wear, which greatly reduces the engine efficiency and blade service life. Therefore, the blade tip material needs to be protected.
[0003] Wear is usually repaired by laser cladding, but the wear resistance after repair is consistent with that of the substrate. Wear will still occur during the operation of the engine, and the wear resistance of the blade end face still needs to be improved. In order to improve the wear resistance of the blade end face after repair, conventional wear-resistant coatings are usually applied to the repaired part in the prior art. The coating methods include electroplating and cold spraying, but the bonding performance is poor in the later stage of coating. Therefore, it is necessary to study a repair method with good bonding strength, high temperature resistance and wear resistance. Summary of the invention
[0004] The purpose of the present invention is to provide a repair method for improving the wear resistance of the end face of a turbine rotor blade, so as to solve the problem that the wear resistance of the end face of the blade is still poor after the blade tip is repaired by the existing laser cladding method.
[0005] In order to solve the above technical problems, the present invention adopts the following technical solutions: A repair method for improving the wear resistance of the end face of a turbine rotor blade comprises the following steps: S1, preparation of solder; S2, pre-welding treatment; S3, pre-welding protection; S4, coating of solder; S5, induction brazing; S6, post-welding grinding; S7, non-destructive testing.
[0006] The method of the present invention adopts induction brazing to prepare the wear-resistant layer, realizes metallurgical bonding, has good bonding force, better meets the need of blade scraping during operation, effectively solves the problem of blade tip wear, and is of great significance for controlling the gap between turbine rotor blades and seals. At the same time, induction brazing only heats local areas to save energy and facilitate automated production. The non-destructive testing is to inspect the repaired blades using fluorescent testing, X-ray testing and other methods.
[0007] As a further preferred embodiment of the present invention, the brazing filler metal preparation in step S1 is specifically to mix nickel-based powder, CBN particles and flux to prepare the brazing filler metal.
[0008] As a further preferred embodiment of the present invention, the nickel-based powder, CBN particles and flux in step S1 are prepared in the following mass proportions: 10-15 parts of nickel-based powder, 10-15 parts of CBN particles and 2-6 parts of flux. After the nickel-based powder, CBN particles and flux are prepared, they are stirred evenly to make a paste solder.
[0009] The brazing filler metal used in this solution contains CBN particles, so it has high wear resistance. The nickel-based powder is consistent with the material of the blade tip to be repaired, so the two are very compatible.
[0010] As a further preferred embodiment of the present invention, the nickel-based powder is mixed with the following raw materials in parts by mass: 20 parts of cobalt, 10 parts of chromium, 10 parts of tungsten, 2 parts of aluminum, 3 parts of boron and 55 parts of nickel.
[0011] As a further preference of the present invention, the pre-welding treatment in step S2 includes a coating removal treatment and a grinding treatment performed in sequence, wherein the coating removal treatment specifically adopts a chemical method or a mechanical method or a combination of a chemical method and a mechanical method to remove the surface coating; the grinding treatment specifically grinds the 5-8 mm range around the blade tip to be welded to a metallic luster, removes carbon deposits, oxides and dirt, and grinds the blade tip surface to make it smooth and clean it with alcohol.
[0012] As a further preferred embodiment of the present invention, the pre-weld protection in step S3 is specifically to use a high-temperature alloy plate to make a guardrail along the blade tip surface morphology, and the guardrail is fixed to the blade by energy storage spot welding.
[0013] The use of a contoured guardrail fits well with the blade profile and can effectively ensure the shape of the wear-resistant layer. The energy storage spot welding specifically uses an energy storage electric welder to weld it to the blade.
[0014] As a further preferred embodiment of the present invention, the brazing filler metal coating in step S4 is specifically coating the brazing filler metal prepared in step S1 onto the guardrail of the blade end surface.
[0015] As a further preferred embodiment of the present invention, the temperature during induction brazing in step S5 is 1000-1300° C. and maintained for 5-30 minutes, and cooled to room temperature after the induction brazing is completed.
[0016] The brazing temperature and insulation are 1000~1300℃, and the insulation time is about 25 minutes, which has better bonding. Because after reaching the above temperature, the brazing filler metal melts and has good fluidity. Sufficient insulation time can promote the mutual diffusion between the brazing filler metal and the blade matrix. If this time is exceeded, some components in the brazing filler metal will be lost, and too long insulation time will affect the performance of the blade matrix.
[0017] As a further preferred embodiment of the present invention, the post-weld grinding in step S6 specifically involves grinding away excess material in the weld and shaping the weld to a specified profile size of the blade.
[0018] Compared with the prior art, the present invention can achieve at least one of the following beneficial effects: 1. The method of the present invention adopts induction brazing to prepare the wear-resistant layer, realizes metallurgical bonding, has good bonding strength, better meets the need for blade scraping during operation, and effectively solves the problem of blade tip wear.
[0019] 2. It is of great significance to control the gap between turbine rotor blades and seals.
[0020] 3. The contoured guardrail fits well with the blade surface and can effectively ensure the shape of the wear-resistant layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 This is a schematic diagram of the preparation position of the wear-resistant layer of the blade of the present invention. DETAILED DESCRIPTION
[0023] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0024] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0025] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features of the embodiments may be combined with each other.
[0026] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.
[0027] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, or the positions or positional relationships in which the product of the invention is usually placed when in use, or the positions or positional relationships commonly understood by those skilled in the art, which are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.
[0028] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "install", "connect", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. Specific embodiment 1: Figure 1 A repair method for improving the wear resistance of the end face of a turbine rotor blade is shown, comprising the following steps: S1, brazing material preparation; S2, pre-welding treatment; S3, pre-welding protection; S4, brazing material coating; S5, induction brazing; S6, post-welding grinding; S7, non-destructive testing.
[0030] The method of the present invention adopts induction brazing to prepare the wear-resistant layer, realizes metallurgical bonding, has good bonding force, better meets the need of blade scraping during operation, effectively solves the problem of blade tip wear, and is of great significance for controlling the gap between turbine rotor blades and seals. At the same time, induction brazing only heats local areas to save energy and facilitate automated production. The non-destructive testing is to inspect the repaired blades using fluorescent testing, X-ray testing and other methods. Specific embodiment 2: This embodiment further illustrates step S1 on the basis of specific embodiment 1. The preparation of the solder in step S1 is to mix nickel-based powder, CBN particles and flux to prepare the solder. Specific embodiment 3: This embodiment further illustrates step S1 on the basis of specific embodiment 2. The nickel-based powder, CBN particles and flux in step S1 are prepared in the following mass proportions: 10 parts of nickel-based powder, 10 parts of CBN particles and 6 parts of flux. After the nickel-based powder, CBN particles and flux are prepared, they are stirred evenly to make a paste solder. Specific embodiment 4: This embodiment further illustrates step S1 on the basis of specific embodiment 2. The nickel-based powder, CBN particles and flux in step S1 are prepared in the following mass proportions: 15 parts of nickel-based powder, 15 parts of CBN particles and 5 parts of flux. After the nickel-based powder, CBN particles and flux are prepared, they are stirred evenly to make a paste solder. Specific embodiment 5: This embodiment further illustrates step S1 on the basis of specific embodiment 2. The nickel-based powder, CBN particles and flux in step S1 are prepared in the following mass proportions: 12 parts of nickel-based powder, 12 parts of CBN particles and 2 parts of flux. After the nickel-based powder, CBN particles and flux are prepared, they are stirred evenly to form a paste solder. Specific embodiment 6: This embodiment further illustrates the nickel-based powder on the basis of Specific Embodiment 2. The nickel-based powder is mixed with the following raw materials in parts by mass: 20 parts of cobalt, 10 parts of chromium, 10 parts of tungsten, 2 parts of aluminum, 3 parts of boron and 55 parts of nickel. Specific embodiment 7: This embodiment further illustrates step S2 on the basis of specific embodiment 1. The pre-welding treatment in step S2 includes a coating removal treatment and a grinding treatment performed in sequence. The coating removal treatment specifically adopts a chemical method or a mechanical method or a combination of a chemical method and a mechanical method to remove the surface coating. The grinding treatment specifically grinds the 5 mm range around the blade tip to be welded to a metallic luster, removes carbon deposits, oxides and dirt, and grinds the blade tip surface to make it smooth and clean it with alcohol. Specific embodiment 8: This embodiment further illustrates step S2 on the basis of specific embodiment 1. The pre-welding treatment in step S2 includes a coating removal treatment and a grinding treatment performed in sequence. The coating removal treatment specifically adopts a chemical method or a mechanical method or a combination of a chemical method and a mechanical method to remove the surface coating. The grinding treatment specifically grinds the 7 mm range around the blade tip to be welded to a metallic luster, removes carbon deposits, oxides and dirt, and grinds the blade tip surface to make it smooth and clean it with alcohol. Specific embodiment 9: This embodiment further illustrates step S2 on the basis of specific embodiment 1. The pre-welding treatment in step S2 includes a coating removal treatment and a grinding treatment performed in sequence. The coating removal treatment specifically adopts a chemical method or a mechanical method or a combination of a chemical method and a mechanical method to remove the surface coating. The grinding treatment specifically grinds the 8 mm range around the blade tip to be welded to a metallic luster, removes carbon deposits, oxides and dirt, and grinds the blade tip surface to make it smooth and clean it with alcohol. Specific embodiment 10: This embodiment further explains step S3 based on specific embodiment 1. The pre-weld protection in step S3 is to use a high-temperature alloy plate to make a guardrail along the blade tip surface morphology, and the guardrail is fixed to the blade by energy storage spot welding.
[0040] The use of a contoured guardrail fits well with the blade profile and can effectively ensure the shape of the wear-resistant layer. The energy storage spot welding specifically uses an energy storage electric welder to weld it to the blade. Specific embodiment 11: This embodiment further explains step S4 on the basis of specific embodiment 1. The coating of the solder in step S4 is specifically to coat the solder prepared in step S1 into the guardrail of the blade end surface. Specific embodiment 12: This embodiment further illustrates step S5 on the basis of specific embodiment 1. In step S5, the temperature during induction brazing is 1300° C. and maintained for 10 minutes. After the induction brazing is completed, the temperature is cooled to room temperature. Specific embodiment 13: This embodiment further illustrates step S5 on the basis of specific embodiment 1. In step S5, the temperature during induction brazing is 1200° C. and maintained for 5 minutes. After the induction brazing is completed, the temperature is cooled to room temperature. Specific embodiment 14: This embodiment further illustrates step S5 on the basis of specific embodiment 1. In step S5, the temperature during induction brazing is 1000° C. and maintained for 30 minutes. After the induction brazing is completed, the temperature is cooled to room temperature. Specific embodiment 15: This embodiment further explains step S6 on the basis of specific embodiment 1. The post-weld grinding in step S6 specifically includes grinding away excess material in the weld and shaping the weld to a specified profile size of the blade.
[0046] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A repair method for improving the wear resistance of the end surface of a turbine rotor blade, characterized in that: The method comprises the following steps: S1, preparation of solder; S2, pre-welding treatment; S3, pre-welding protection; S4, coating of solder; S5, induction brazing; S6, post-welding grinding; and S7, non-destructive flaw detection.
2. The repair method for improving the wear resistance of the end surface of a turbine rotor blade according to claim 1, characterized in that: The preparation of the solder in step S1 specifically involves mixing nickel-based powder, CBN particles, and flux to prepare the solder.
3. The repair method for improving the wear resistance of the end surface of a turbine rotor blade according to claim 2, characterized in that: The nickel-based powder, CBN particles and flux in step S1 are prepared in the following mass proportions: 10-15 parts of nickel-based powder, 10-15 parts of CBN particles and 2-6 parts of flux. After the nickel-based powder, CBN particles and flux are prepared, they are stirred evenly to form a paste solder.
4. The repair method for improving the wear resistance of the end surface of a turbine rotor blade according to claim 3 is characterized in that: The nickel-based powder is mixed with the following raw materials in parts by weight: 20 parts of cobalt, 10 parts of chromium, 10 parts of tungsten, 2 parts of aluminum, 3 parts of boron and 55 parts of nickel.
5. The repair method for improving the wear resistance of the end surface of a turbine rotor blade according to claim 1, characterized in that: The pre-welding treatment in step S2 includes a coating removal treatment and a grinding treatment performed in sequence. The coating removal treatment specifically adopts a chemical method or a mechanical method or a combination of a chemical method and a mechanical method to remove the surface coating; the grinding treatment specifically grinds the 5-8 mm range around the blade tip to be welded to a metallic luster, removes carbon deposits, oxides and dirt, and grinds the blade tip surface to make it smooth and clean it with alcohol.
6. The repair method for improving the wear resistance of the end surface of a turbine rotor blade according to claim 1, characterized in that: The pre-welding protection in step S3 is specifically to use a high-temperature alloy plate to make a guardrail along the blade tip surface morphology, and the guardrail is fixed to the blade by energy storage spot welding.
7. The repair method for improving the wear resistance of the end surface of a turbine rotor blade according to claim 6, characterized in that: The solder coating in step S4 is specifically coating the solder prepared in step S1 to the guardrail of the blade end surface.
8. The repair method for improving the wear resistance of the end surface of a turbine rotor blade according to claim 1, characterized in that: The temperature during induction brazing in step S5 is 1000-1300° C. and maintained for 5-30 minutes. After the induction brazing is completed, the material is cooled to room temperature.
9. The repair method for improving the wear resistance of the end surface of a turbine rotor blade according to claim 1, characterized in that: The post-weld grinding in step S6 specifically involves grinding away excess material in the weld and shaping the blade to a specified profile size.
Citation Information
Patent Citations
Preparing method of titanium fire resistance coating
CN107138878A
Preparation method of high temperature alloy surface wear-resisting oxidation-resistant coating
CN107794528A
Method of brazing wear-resistant alloy on damping boss of low-pressure rotor blade
CN110977071A
Aero-engine high-pressure turbine working blade crown repairing method
CN113478167A
High-strength and high-wear-resistance composite brazing coating for repairing water turbine blade
CN113667973A