Electron barrier layer compound with long parallel ring structure and organic electroluminescent device thereof
By using electron barrier layer compounds with long ring structures in organic electroluminescent devices, the problem of insufficient heat resistance and stability of the electron barrier material is solved, the life and efficiency of the device are improved, and the driving voltage is reduced.
Patent Information
- Application Number
- CN202411035883.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-19
AI Technical Summary
The heat resistance and film phase stability of the electronic barrier materials in existing organic electroluminescent devices are poor, resulting in a shortened device life, a high driving voltage and low efficiency.
Using electron barrier layer compounds with long ring structures, including electron-rich adamantane structure, dibenzo five-membered ring structures connected with single bonds of nitrogen atoms, and three-dimensional stereosamantane structures, to improve the charge resistance and thermal stability of the compound. , and fine-tune the energy band gap by substituents to improve interface properties.
It improves the hole mobility and life of the device, reduces the driving voltage, improves the device efficiency, and effectively prevents molecular crystallization and extends the service life.
Smart Images

Figure CN118978476A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of organic electroluminescent materials, and in particular relates to an electron blocking layer compound with a long parallel ring structure and an organic electroluminescent device thereof. Background Art
[0002] The classic double-injection organic electroluminescent device consists of three layers: a hole transport layer, a light-emitting layer, and an electron transport layer. Holes are transported to the light-emitting layer through the hole transport layer and combine with electrons in the electron transport layer to form excitons, which then emit light. Organic electroluminescent devices can be adjusted to obtain various required lights by changing the composition of the light-emitting layer as needed.
[0003] Most of the materials used in organic electroluminescent devices are pure organic matter or organometallic complexes, which can be divided into hole injection materials, hole transport materials, carrier blocking materials, luminescent materials, electron transport materials, electron injection materials, etc. according to their uses. Among them, carrier blocking materials are divided into electron blocking materials and hole blocking materials. In organic electroluminescent devices, hole blocking materials are often directly replaced by electron transport materials or directly removed. For top-emitting devices, electron blocking materials adjust the microcavity length and affect the exciton formation area, which is an indispensable component of the device. The heat resistance and amorphousness of electron blocking materials will have a crucial impact on the life of the device. Materials with poor heat resistance are prone to decomposition during the evaporation process, polluting the evaporation cavity and damaging the life of the device; materials with poor film phase stability will crystallize during the use of the device, reducing the service life of the device. Therefore, the electron blocking material is required to have a high film phase stability and decomposition temperature during use. Summary of the invention
[0004] In order to solve the problems existing in the background technology, the first object of the present invention is to provide an electron blocking layer compound having a long parallel ring structure, and the technical solution is as follows:
[0005] An electron blocking layer compound having a long parallel ring structure has a structure shown in the following general formula I:
[0006]
[0007] Wherein X is selected from a single bond, CR 1 R 2 , O, S or S(=O)2; Y is selected from CR 3 R 4 , O, S; Z is selected from a single bond, CR 5 R 6 , O, S or S(=O)2;
[0008] R 1 To R 6are the same or different from each other and are independently selected from hydrogen, C1 to C 10 Alkyl, C6~C 30 The aryl group; R 7 To R 10 are the same or different from each other and are independently selected from deuterium, cyano, amine, halogen, C1-C 10 Alkyl, C6~C 30 The aryl group, n is independently selected from 0 to the maximum number of sites that can be substituted in the ring.
[0009] As a preferred embodiment of the present invention, X is selected from a single bond, CR 1 R 2 , O, S; Z is selected from a single bond, CR 5 R 6 , O, S.
[0010] As a preferred embodiment of the present invention, when X is a single bond, Z is a single bond; X is CR 1 R 2 When Z is CR 5 R 6 ; When X is O, Z is O; When X is S, Z is S; General Formula I is represented by the following formulas (1-1) to (1-4):
[0011]
[0012] As a preferred embodiment of the present invention, the R 1 , R 2 The same as each other, selected from methyl or phenyl: the R 3 , R 4 are the same as each other and are methyl; the R 5 , R 6 The same as each other is methyl; n is 0.
[0013] As a preferred embodiment of the present invention, the structure of the general formula I is as follows:
[0014]
[0015]
[0016]
[0017] Another object of the present invention is to provide an organic electroluminescent device, comprising a first electrode, a second electrode and an organic material layer arranged therebetween, wherein the organic material layer comprises a carrier blocking layer, and the preparation material of the carrier blocking layer comprises at least one of the above-mentioned electron blocking layer compounds having a long parallel ring structure.
[0018] As a preferred embodiment of the present invention, the organic electroluminescent device is applied to a flat panel display device or a flexible display device.
[0019] The beneficial effects of the present invention are as follows:
[0020] The electron blocking layer compound with a long parallel ring structure provided by the present invention comprises an electron-rich adamantane structure, a long parallel ring structure connected to adamantane by a single bond of a nitrogen atom, and a dibenzo pentacyclic structure connected to the long parallel ring structure by a nitrogen atom. The charge resistance of the compound is improved by connecting with a nitrogen atom, wherein the long parallel ring structure containing at least six rings makes the molecule as a whole extremely planar rigid, which is beneficial to improve the mobility of holes, thereby improving the life of the device. In addition, the three-dimensional adamantane structure introduced has both rigidity, which can adjust the thermal stability of the compound, and can effectively prevent the aggregation between molecules. The film phase stability is strong, making the compound difficult to crystallize. The dibenzo pentacyclic structure that can rotate freely on the outside plays a spatial distortion role of the compound, and has strong functionalization. It can be matched with the energy level of an organic electroluminescent device by replacing it. Moreover, the compound provided by the present invention has a relatively deep HOMO energy level compared to the comparative compound, so that the injection barrier between the hole transport material and the host material is smaller, which is beneficial to reduce the driving voltage of the device, and effectively improves the device efficiency, thereby improving the life of the device.
[0021] In addition, by introducing various substituents into the core structure, the energy band gap can be fine-tuned while improving the interfacial properties between organic materials, diversifying the uses of the materials. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:
[0023] Figure 1 is the DSC spectrum of the prepared compound 1;
[0024] Figure 2 The chem3D geometry optimization diagram of the prepared compound 1;
[0025] Figure 3 This is a comparison chart of the lifespan of the organic electroluminescent devices in device example 1 and device comparative example 1;
[0026] Figure 4 The voltage-current density comparison diagram of the single carrier device prepared using compound 1 and comparative compound 1. DETAILED DESCRIPTION
[0027] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0028] If the specific conditions are not specified in the embodiments, they are carried out under conventional conditions or conditions recommended by the manufacturer. The reagents or instruments used without indicating the manufacturer are all conventional products that can be purchased commercially. Some reaction compounds are purchased from commodity suppliers (Zhengzhou Alpha Chemical Co., Ltd.), and some compounds that cannot be directly purchased are prepared by simple reactions of commercially available raw materials. The percentages all refer to mass percentages, and the temperatures are degrees Celsius (℃). Such method principles, operating procedures, conventional post-treatments, silica gel columns, recrystallization purification and other means are well known to synthesizers in the art, and the synthesis process can be fully realized to obtain the target product. The reactions in each preparation embodiment are generally carried out under positive pressure of nitrogen or argon.
[0029] Preparation Example
[0030] Example 1: Preparation of Compound 1
[0031]
[0032] Synthesis of compound 1-3: Compound 1-1 (8.6 g, 16 mmol), compound 1-2 (4.6 g, 16 mmol), palladium acetate (0.2 g, 1 mmol), sodium tert-butoxide (3.1 g, 32 mmol), bis(diphenylphosphino)-1,1'-binaphthyl (0.6 g, 1 mmol) and toluene (45 mL) were placed in a 100 mL reactor. The mixture was refluxed for 2 hours under stirring. After the reaction was completed, the mixture was filtered, and the filtrate was concentrated and purified by column chromatography to obtain compound 1-3 (9.2 g, yield 82%);
[0033] Synthesis of compound 1: Compound 1-3 (17.4 g, 25 mmol), Pd(OAc)2 (0.22 g, 1 mmol), PCy3HBF4 (0.74 g, 2 mmol) and K2CO3 (0.41 g, 3 mmol) were dispersed in DMAc and reacted at 130°C for 24 h. After cooling to room temperature, the filter cake was filtered under reduced pressure, and the crude product was purified by silica gel column chromatography (DCM as eluent) to obtain compound 1 (10.7 g, yield 79%), MS: 617.45.
[0034] Example 2: Preparation of Compound 5
[0035]
[0036] Synthesis of compound 5-3: The synthesis method is the same as that of compound 1-3, except that compound 1-1 is replaced by compound 5-1, and compound 1-2 is replaced by compound 5-2;
[0037] Synthesis of compound 5: n-BuLi (0.70 g, 11 mmol) was slowly dripped into a dry t-BuPh solution of compound 5-3 (7.1 g, 10 mmol) under N2 atmosphere, reacted at 0°C for 2 h, t-BuPh solution of acetone (0.64 g, 11 mmol) was slowly dripped into it, and then naturally warmed to room temperature. The reaction was quenched with H2O, the organic layer solvent was removed by rotary evaporation, the crude product was purified by Al2O3 column chromatography (ethyl acetate / petroleum ether, volume ratio 1:10), and recrystallized from THF and MeOH to obtain an intermediate; HCl was slowly dripped into a CH3COOH solution of the intermediate and stirred for 10 min, the filter cake was quickly vacuum filtered, washed with MeOH, and then recrystallized from THF and MeOH to obtain compound 5 (5.4 g, yield 80%), MS: 675.46.
[0038] Example 3: Preparation of Compound 9
[0039]
[0040] Synthesis of compound 9-3: The synthesis method is the same as that of compound 1-3, except that compound 1-1 is replaced by compound 9-1, and compound 1-2 is replaced by compound 9-2;
[0041] Synthesis of compound 9: Compound 9-3 (36 g, 50 mmol), potassium carbonate (13.8 g, 100 mmol) and N-methyl-2-pyrrolidone (800 mL) were added to a 2L three-necked flask and stirred at 150°C for 12 hours. After the reaction was completed, the reaction product was separated, the organic layer was concentrated under reduced pressure, separated by column chromatography, and dried to obtain compound 9 (23.0 g, yield 72%), MS: 639.40.
[0042] Example 4: Preparation of Compound 11
[0043]
[0044] Synthesis of compound 11-3: The synthesis method is the same as that of compound 1-1, except that compound 11-1 is used to replace compound 1-1, and compound 11-2 is used to replace compound 1-2;
[0045] Synthesis of compound 11-4: Under N2 atmosphere, LaCl3·2LiCl (3.6 g, 11 mmol) in THF was kept at -50°C for 15 min, and n-BuLi (0.70 g, 11 mmol) was added dropwise, and the reaction was carried out at -50°C for 30 min to obtain n-Bu2LaCl·4LiCl solution. Compound 11-3 (7.0 g, 10 mmol) in THF (10 mL) was added dropwise to n-Bu2LaCl·4LiCl solution, kept at -50°C for 5 min, and reacted at 0°C for 30 min. I2 (25.38 g, 100 mmol) was added, and the reaction was carried out at room temperature for 1 h. The reaction was quenched with water, washed three times with DCM, and the organic solvent was removed by rotary evaporation. The crude product was purified by silica gel column chromatography (DCM / petroleum ether, volume ratio 1:5), and recrystallized with DCM and methanol to obtain compound 11-4 (5.1 g, yield 78%);
[0046] Synthesis of compound 11: Under N2 atmosphere, compound 11-4 (8.8 g, 10 mmol), sulfur powder (0.64 g, 20 mmol), KOH (2.24 g, 40 mmol) were dispersed in DMSO and reacted at 110°C for 24 h. The reaction was quenched with water, washed three times with DCM, and the organic solvent was removed by rotary evaporation. The crude product was purified by silica gel column chromatography (DCM / petroleum ether, volume ratio 1:10), and recrystallized from DCM and methanol to obtain compound 11 (5.2 g, yield 79%), MS: 655.34.
[0047] Example 5: Preparation of Compound 22
[0048]
[0049] Synthesis of compound 22-3: The synthesis method is the same as that of compound 1-1, except that compound 22-1 is used to replace compound 1-1, and compound 22-2 is used to replace compound 1-2;
[0050] Synthesis of compound 22: The synthesis method is the same as that of compound 5, except that compound 22-3 is used to replace compound 5-3, MS: 825.55.
[0051] Example 6: Preparation of Compound 32
[0052]
[0053] Synthesis of compound 32-3: The synthesis method is the same as that of compound 1-1, except that compound 32-1 is used to replace compound 1-1, and compound 32-2 is used to replace compound 1-2;
[0054] Synthesis of compound 32-4: The synthesis method is the same as that of compound 11-4, except that compound 11-3 is replaced by compound 32-3;
[0055] Synthesis of compound 32: The synthesis method is the same as that of compound 11, except that compound 11-4 is replaced by compound 32-4, MS: 623.39.
[0056] Example 7: Preparation of Compound 44
[0057]
[0058] Synthesis of compound 44-3: The synthesis method is the same as that of compound 1-1, except that compound 44-1 is used to replace compound 1-1, and compound 44-2 is used to replace compound 1-2;
[0059] Synthesis of compound 44: The synthesis method is the same as that of compound 11-4, except that compound 44-3 is used to replace compound 11-3;
[0060] Synthesis of compound 44: The synthesis method was the same as that of compound 11, except that compound 44-4 was used to replace compound 11-4, MS: 639.35.
[0061] In addition, it should be noted that other compounds of the present application can be obtained by referring to the synthesis methods of the above-listed embodiments and existing synthesis methods, so they will not be listed one by one here.
[0062] Device Embodiment
[0063] Preparation of Device Example 1:
[0064] A glass substrate coated with ITO (indium tin oxide) as a thin film with a thickness of 1000 angstroms was placed in distilled water in which a detergent was dissolved and ultrasonically cleaned. After the ITO was cleaned for 30 minutes, ultrasonic cleaning was repeated twice with distilled water for 10 minutes, and then the substrate was ultrasonically cleaned with isopropyl alcohol, acetone and methanol solvents, dried, transferred to a plasma cleaner for cleaning for 5 minutes, and then transferred to a vacuum depositor;
[0065] On the ITO transparent electrode, the compound [HI] was thermally vacuum deposited to a thickness of 100 angstroms to form a hole injection layer; the compound [HT] was vacuum deposited to 800 angstroms on the hole injection layer to form a hole transport layer; the compound 1 was vacuum deposited to a thickness of 50 angstroms on the hole transport layer to form an electron blocking layer (also called a light-emitting auxiliary layer); the compound [BH] and the compound [BD] were vacuum deposited to a thickness of 200 angstroms at a ratio of 97:3 on the electron blocking layer to form a light-emitting layer; the compound [ET] and the compound [LiQ] (lithium quinoline) were vacuum deposited at a ratio of 1:1 to form an electron transport layer with a thickness of 300 angstroms; yttrium (Yb) and magnesium silver (1:9) were sequentially deposited on the electron transport layer to a thickness of 10 angstroms and 1000 angstroms, respectively, to form a cathode. The vacuum degree during deposition was maintained at 1×10 -7 Up to 5×10 -8 Entrust.
[0066] Preparation of device examples 2-11:
[0067] When forming the electron blocking layer, the compound shown in Table 1 was used instead of the compound 1 in Example 1, and an organic electroluminescent device was prepared by the same method as Example 1.
[0068] Preparation of Comparative Examples 1 and 2:
[0069] An organic electroluminescent device was prepared in the same manner as in Example 1, except that Comparative Compound 1 and Comparative Compound 2 were used instead of Compound 1 in Example 1 when forming the electron blocking layer.
[0070] The structure of the compound used in the above preparation process is as follows:
[0071]
[0072] The HOMO value of each compound was calculated by Gaussian calculation software; for the organic electroluminescent devices manufactured using each compound as an electron blocking layer in the embodiments and comparative examples, the ... 2 The driving voltage and current efficiency were measured at a current density of 50 mA / cm 2 The time required for the brightness to decrease to 97% of the initial brightness (LT97) was measured at a current density of 1.5 Å. The results are shown in Table 1 below:
[0073] Table 1
[0074]
[0075]
[0076] In Table 1 above, compared with the comparative example, under the same current density, it can be seen that the current efficiency of the device embodiment is greatly improved, the driving voltage is reduced, and the service life is improved. For example Figure 3 The lifespan comparison diagram of the devices prepared in Comparative Example 1 and Example 1, J = 50 mA / cm 2 At this current density, the brightness drops to 970cd / m 2 The life of the device prepared in Example 1 is longer than that of the device prepared in Comparative Example 1. Figure 4 The voltage-current density diagram of the single carrier device prepared using compound 1 and comparative compound 1, with the structure of [ITOglass / / HI:HT(3:97,10nm) / compound 1 or comparative compound 1(50nm) / HI:HT(3:97,10nm) / Al(150nm)]. It can be seen that the hole mobility of the single carrier device prepared using compound 1 is better than that of comparative compound 1. Figure 2 The molecular structure diagram of compound 1 of the present invention adjusted by chem3D shows more intuitively that the planar rigidity of the compound structure is good and its glass transition temperature is high (see Figure 1 , Tg value 134.68°C), so the film forming stability is very good during the thermal evaporation process, which is beneficial to improving the life of the device; in addition, compared with the comparative example compounds, the compounds provided in the present application have a deeper HOMO energy level and can better form ohmic contact with the main material, which is beneficial to reducing the driving voltage of the device and effectively improving the device efficiency, thereby improving the life of the device and having broad application prospects.
Claims
1. An electron blocking layer compound having a long parallel ring structure, characterized in that: It has the structure shown in the following general formula I: Wherein X is selected from a single bond, CR 1 R 2 , O, S or S(=O)2; Y is selected from CR 3 R 4 , O, S; Z is selected from a single bond, CR 5 R 6 , O, S or S(=O)2; R 1 To R 6 are the same or different from each other and are independently selected from hydrogen, C1 to C 10 Alkyl, C6~C 30 The aryl group; R 7 To R 10 are the same or different from each other and are independently selected from deuterium, cyano, amine, halogen, C1-C 10 Alkyl, C6~C 30 The aryl group, n is independently selected from 0 to the maximum number of sites that can be substituted in the ring.
2. The electron blocking layer compound having a long parallel ring structure according to claim 1, characterized in that: The X is selected from a single bond, CR 1 R 2 , O, S; Z is selected from a single bond, CR 5 R 6 , O, S.
3. The electron blocking layer compound having a long parallel ring structure according to claim 2, characterized in that: When X is a single bond, Z is a single bond; X is CR 1 R 2 When Z is CR 5 R 6 ; When X is O, Z is O; When X is S, Z is S; General Formula I is represented by the following formulas (1-1) to (1-4):
4. The electron blocking layer compound having a long parallel ring structure according to claim 3, characterized in that: The R 1 , R 2 The same as each other, selected from methyl or phenyl: the R 3 , R 4 are the same as each other and are methyl; the R 5 , R 6 The same as each other are methyl; n is 0.
5. The electron blocking layer compound having a long parallel ring structure according to claim 1, characterized in that: The structure of the general formula I is as follows:
6. An organic electroluminescent device, characterized in that: It comprises a first electrode, a second electrode and an organic material layer arranged therebetween, wherein the organic material layer comprises a carrier blocking layer, and the preparation material of the carrier blocking layer comprises at least one electron blocking layer compound having a long parallel ring structure as described in any one of claims 1-5.
7. The organic electroluminescent device according to claim 6, characterized in that: The organic electroluminescent device is applied to a flat panel display device or a flexible display device.