Infrared model simulation method for orthotropic carbon fibers of plain weave structure

By constructing a detailed multi-layer fiber braided structure model in the finite element modeling of composite materials, the problem of detection result error in the existing technology is solved, more accurate temperature change curves and detection accuracy are achieved, and non-destructive detection of composite materials is laid. The basis of

CN118983031APending Publication Date: 2024-11-19GUILIN UNIV OF ELECTRONIC TECH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411008342.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The prior art fails to fully consider the specific characteristics of the carbon fiber braided structure in the finite element modeling of composite materials, resulting in errors in the detection results and cannot accurately reflect the actual performance of the material.

Method used

采用平织结构正交各向异性碳纤维的红外模型仿真方法,通过构建详细的多层纤维编织结构模型,设置材料参数和热激励,进行数值模拟以绘制温度分布图,并改变纤维层间距以模拟结构变化。

Benefits of technology

A more accurate temperature change curve is achieved, providing a solid foundation for non-destructive testing and evaluation of composite materials, reducing experimental costs and improving detection accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983031A_ABST
    Figure CN118983031A_ABST
Patent Text Reader

Abstract

The invention provides an infrared model simulation method for orthotropic carbon fibers of a plain weave structure. The property of the orthotropic carbon fibers on temperature conduction and the influence of structural changes and internal pore defects on the surface temperature of a composite material are studied. The method comprises the following steps: defining material basic attributes of carbon fibers and epoxy resin and geometric parameters of a model according to the actual size of a carbon fiber plate, and establishing a three-dimensional weaving geometric model; the pore defect is added in the structure, the influence of the defect on the surface temperature in the nondestructive testing process is truly simulated, the influence possibly caused by the internal change of the structure is considered, and a certain guiding value is achieved for actual nondestructive testing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an infrared model simulation method for orthotropic carbon fibers with a plain weave structure, and belongs to the technical field of nondestructive testing and evaluation of composite materials. Background Art

[0002] Carbon fiber reinforced polymer composites have been widely used in many production and life fields such as aerospace, military, navigation, medical, automobile manufacturing, construction and electronic technology due to their many superior properties such as low density, light weight, high strength, high temperature resistance, low thermal expansion coefficient and good fatigue resistance. In the production and use of CFRP composite materials, various types of defects will appear, which will shorten the life of the material during its use. In order to inspect and test the type, quantity, size and other defects inside the material without damaging or affecting the performance of the object being tested, infrared detection technology came into being. When performing infrared detection on samples, it is very important to clarify the material properties of the sample being tested, such as its own thermal conductivity, specific heat capacity, density, elastic modulus, shear modulus, etc. In addition to these fixed material properties, the geometric size and structure of the material, the interlayer arrangement, and the ratio of carbon fiber to epoxy resin will also affect the test results. In order to clarify the impact of these variable factors on the test, material simulation is indispensable before formal testing.

[0003] Composite materials are made of a variety of different materials, usually containing two or more materials, with complex internal structures, and composite materials are generally anisotropic materials, which are more difficult to analyze in finite element modeling. The traditional finite element modeling method for composite materials is equivalent modeling, which simplifies the finite element model of composite materials and improves the modeling efficiency and calculation efficiency to a certain extent, but it will inevitably lead to errors in the results and cannot accurately reflect the true performance of composite materials.

[0004] After investigation, it was found that in the current research, the specific structure of the braided fabric has not been taken into account in the final result for the modeling of carbon fiber braided multilayer composite materials. Simplified fiber structures are used, or the orientation of fibers is simply divided using the software's built-in functions. In the present invention, a more detailed multilayer fiber braided fabric structure is constructed in the software. By applying this structure calculation, the final result will be closer to the actual data. Summary of the invention

[0005] The purpose of the present invention is to provide an infrared model simulation method of orthotropic carbon fibers with a plain weave structure, which has reasonable design, low experimental cost and high precision, and the final result obtained will be closer to the actual data.

[0006] The object of the present invention is achieved in that:

[0007] Step 1, establishing an epoxy resin substrate and its carbon fiber composite material model;

[0008] Step 2: Set the material parameters, thermal excitation, boundary and constraint conditions in the model, set the curve coordinates and divide the grid;

[0009] Step 3: Add thermal excitation to the front and back of the model to study the properties of orthotropic carbon fibers on temperature conduction;

[0010] Step 4: Add defects to the model, perform numerical simulation and draw a surface temperature distribution diagram of the model with defects inside;

[0011] Step 5, changing the fiber layer spacing in the model, performing numerical simulation and drawing the surface temperature curve of the model when the structure changes;

[0012] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific steps of step 1 include:

[0013] (1) Construct a single carbon fiber model and form a single-layer carbon fiber woven structure through a series of Boolean geometric operations;

[0014] (2) The single-layer carbon fiber woven structure undergoes a series of geometric operations and is translated by a certain phase (retaining the initial object) to obtain a multi-layer carbon fiber woven structure;

[0015] (3) Construct an epoxy resin base model and inject epoxy resin into the multi-layer fiber woven structure to obtain the overall structure.

[0016] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific steps of step 2 include:

[0017] (1) Setting the thermophysical parameters of carbon fiber and epoxy values ​​in the model;

[0018] (2) Write the continuous infrared light source equation into the local variables and set the irradiation area and power density;

[0019] (3) Set the material edge temperature, convective heat flux, and boundary heat source in the boundary conditions of the solid heat transfer module.

[0020] (4) Add curvilinear coordinates in the physical field, select the diffusion method, and set the two ends of the fiber as the inlet and outlet respectively.

[0021] (5) The simulation model is divided into four different areas: carbon fiber finite element domain area, epoxy resin finite element domain area, infinite element area and defect area.

[0022] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific steps of step 3 include:

[0023] (1) Set the same Gaussian point heat source on the front and back of the model.

[0024] (2) Perform numerical simulation and draw the temperature distribution diagram of the model surface

[0025] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific steps of step 4 include:

[0026] (1) Add a sphere inside the model and set the coordinates and radius of the sphere as variables.

[0027] (2) Set the material of the sphere to air.

[0028] (3) Perform numerical simulation and draw a surface temperature distribution diagram of the model with internal defects.

[0029] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific steps of step 5 include:

[0030] (1) Change the fiber layer spacing in the model.

[0031] (2) Perform numerical simulation and draw the surface temperature curve of the model when the structure changes.

[0032] Furthermore, in step 1, the geometric parameters of the carbon fiber composite material plate are actually measured, and the geometric model of the braided structure carbon fiber reinforced polymer material is established by finite element software.

[0033] Furthermore, in step 2, the heat transfer coefficient of the material is set to 10, and the material type is set to solid.

[0034] Furthermore, in step 3, a Gaussian point light source is used to illuminate the fiber bundles in different directions on the front and back sides respectively, and the power density of the Gaussian point light source is set to 10000w / m2.

[0035] Furthermore, in step 4, the spheres added inside the model are regarded as pore defects, and the radius and burial depth of the defects can be changed. Six defects are set in the model, three of which have a radius of 0.3 mm and defect depths of 0.1 mm, 0.2 mm, and 0.3 mm respectively; the other three defects have a depth of 0.3 mm and a radius of 0.1 mm, 0.2 mm, and 0.3 mm respectively.

[0036] Furthermore, in step 5, the depth of the first carbon fiber braided layer from the surface and the spacing between the carbon fiber braided layers are changed respectively, and then numerical simulation is performed to obtain the surface temperature curve of the model when the structure changes.

[0037] The beneficial effects of the present invention are:

[0038] 1. The infrared model simulation method of a plain-woven orthotropic carbon fiber provided by the present invention takes into account the influence of internal defects on the surface temperature of the model.

[0039] 2. The infrared model simulation method of plain-woven orthotropic carbon fiber proposed in the present invention takes into account the influence of the depth of the first carbon fiber braided layer from the surface and the change of the spacing between the carbon fiber braided layers on the surface temperature. It can more accurately and effectively give the temperature change curve over time when the layer spacing changes, laying a solid foundation for the subsequent non-destructive testing and evaluation of composite materials. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 The present invention is a flow chart of an infrared model simulation method for orthotropic carbon fibers with a plain weave structure.

[0041] Figure 2 It is the geometric model of a single carbon fiber.

[0042] Figure 3 It is a single-layer woven carbon fiber geometry model.

[0043] Figure 4 It is a multi-layer woven carbon fiber geometry model.

[0044] Figure 5 It is the geometric model of epoxy resin substrate and its carbon fiber composite material.

[0045] Figure 6 It is the surface temperature distribution thermal map of the front and back sides of the model receiving thermal excitation respectively.

[0046] Figure 7 It is the surface temperature simulation result of the model with pore defects.

[0047] Figure 8 It is the simulation result of the model surface temperature when the interlayer spacing changes. DETAILED DESCRIPTION

[0048] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.

[0049] It should be understood that the terms such as “having”, “including” and “comprising” used herein do not exclude the existence or addition of one or more other elements or combinations thereof.

[0050] A method for analyzing defects of multi-layer carbon fiber reinforced polymer materials based on heat transfer, characterized in that it includes the following steps:

[0051] Step 1, establishing an epoxy resin substrate and its carbon fiber composite material model;

[0052] Step 2: Set the material parameters, thermal excitation, boundary and constraint conditions in the model, set the curve coordinates and divide the grid;

[0053] Step 3: Add defects to the model, perform numerical simulation and draw a surface temperature distribution diagram of the model with defects inside;

[0054] Step 4, changing the fiber layer spacing in the model, performing numerical simulation and drawing the surface temperature curve of the model when the structure changes;

[0055] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific steps of step 1 include:

[0056] (1) Construct a single carbon fiber model and form a single-layer carbon fiber woven structure through a series of Boolean geometric operations;

[0057] (2) The single-layer carbon fiber woven structure undergoes a series of geometric operations and is translated by a certain phase (retaining the initial object) to obtain a multi-layer carbon fiber woven structure;

[0058] (3) Construct an epoxy resin base model and inject epoxy resin into the multi-layer fiber woven structure to obtain the overall structure.

[0059] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that: the specific method of step (1) of step 1 is:

[0060] Using the sweep operation in the geometry module of the finite element simulation software, the swept surface is an ellipse with a major axis of a mm and a minor axis of b mm. T is the length of one undulation cycle of the fiber, and the equation of the edge to be followed is:

[0061] After sweeping, a single carbon fiber model is obtained. Then the model is translated and the initial object is retained to obtain the second fiber model. The translation displacement is the distance between the two fibers. Then the second fiber is mirrored and the point on the reflection surface is The normal vector of the reflection plane is (0,0,1), and a new mirror fiber is obtained. Array operations are performed on the initial fiber and the mirror fiber respectively. The sizes and displacements of the two arrays are (1,4,1), (0,a,0) and (1,3,1), (0,a,0) respectively.

[0062] Rotate both fiber arrays by 90 degrees and keep the original object I1. The points on the rotation axis are Finally, the initial object I1 is mirrored, and the points on the reflection surface are The normal vector of the reflection plane is (0,0,1), thus obtaining a single-layer woven carbon fiber structure model.

[0063] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that: the specific method of step (2) of step 1 is:

[0064] Using the mirror operation for the single-layer model, the points on the reflection surface are The normal vector of the reflection plane is (0,0,1), the initial object I2 is retained, and the mirror image M1 of the single-layer model is obtained; the initial object I2 is translated on the z-axis with a displacement of 2×hy to obtain a double-layer model, M1 is translated on the z-axis with a displacement of 4×hy, and the initial object is retained, I2 is translated on the z-axis with a displacement of 4×hy, and the initial object is retained, thus obtaining a multi-layer carbon fiber woven structure.

[0065] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific steps of step 2 include:

[0066] (1) Setting the thermophysical parameters of carbon fiber and epoxy values ​​in the model;

[0067] (2) Write the continuous infrared light source equation into the local variables and set the irradiation area and power density;

[0068] (3) Set the material edge temperature and convective heat flux in the boundary conditions of the solid heat transfer module.

[0069] (4) Add curvilinear coordinates in the physical field, select the diffusion method, and set the two ends of the fiber as the inlet and outlet respectively.

[0070] (5) The simulation model is divided into four different areas: carbon fiber finite element domain area, epoxy resin finite element domain area, infinite element area and defect area.

[0071] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that: the specific method of step (4) of step 2 is:

[0072] (1) The curve coordinates of the carbon fiber part are calculated using the steady-state method, and the calculated curve coordinates are substituted into the next step of transient calculation of solid heat transfer.

[0073] (2) The transient method was used to heat the multilayer woven carbon fiber epoxy resin model and the multilayer woven carbon fiber epoxy resin composite model containing defects for 40 seconds, and the surface temperature of the multilayer woven carbon fiber epoxy resin model was calculated.

[0074] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific method of step 3 is:

[0075] (1) The same Gaussian point heat source is set on the front and back of the model, and the point heat source irradiates the transverse and longitudinal fiber bundles respectively.

[0076] (2) Perform numerical simulation and draw the temperature distribution diagram of the model surface

[0077] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific method of step 4 is:

[0078] A sphere with variable radius and burial depth of defects was added inside the model. Six defects were set in the model, three of which had a radius of 0.3 mm and defect depths of 0.1 mm, 0.2 mm, and 0.3 mm respectively; the other three had a depth of 0.3 mm and a radius of 0.1 mm, 0.2 mm, and 0.3 mm respectively.

[0079] The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1 is characterized in that the specific method of step 5 is:

[0080] The depth of the first carbon fiber braided layer from the surface and the spacing between carbon fiber braided layers were changed respectively, and then numerical simulation was carried out to obtain the surface temperature curve of the model when the structure changed.

Claims

1. An infrared model simulation method for orthotropic carbon fiber with a plain weave structure. The method is characterized by: The following steps are involved: Step 1, establishing an epoxy resin substrate and its carbon fiber composite material model; Step 2: Set the material parameters, thermal excitation, boundary and constraint conditions in the model, set the curve coordinates and divide the grid; Step 3: Add thermal excitation to the front and back of the model to study the properties of orthotropic carbon fibers on temperature conduction; Step 4: Add defects to the model, perform numerical simulation and draw a surface temperature distribution diagram of the model with defects inside; Step 5: Change the fiber layer spacing in the model, perform numerical simulation, and draw the model surface temperature curve when the structure changes.

2. The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1, characterized in that: The specific steps of step 1 include: (1) Construct a single carbon fiber model and form a single-layer carbon fiber woven structure through a series of Boolean geometric operations; (2) The single-layer carbon fiber woven structure undergoes a series of geometric operations and is translated by a certain phase (retaining the initial object) to obtain a multi-layer carbon fiber woven structure; (3) Construct an epoxy resin base model and inject epoxy resin into the multi-layer fiber woven structure to obtain the overall structure.

3. The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1, characterized in that: The specific steps of step 2 include: (1) Setting the thermophysical parameters of carbon fiber and epoxy values ​​in the model; (2) Write the continuous infrared light source equation into the local variables and set the irradiation area and power density; (3) Set the material edge temperature, convective heat flux, and boundary heat source in the boundary conditions of the solid heat transfer module. (4) Add curvilinear coordinates in the physical field, select the diffusion method, and set the two ends of the fiber as the inlet and outlet respectively. (5) The simulation model is divided into four different areas: carbon fiber finite element domain area, epoxy resin finite element domain area, infinite element area and defect area.

4. The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1, characterized in that: The specific steps of step 3 include: (1) Set the same Gaussian point heat source on the front and back of the model. (2) Perform numerical simulation and draw the temperature distribution diagram of the model surface.

5. The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1, characterized in that: The specific steps of step 4 include: (1) Add a sphere inside the model and set the coordinates and radius of the sphere as variables. (2) Set the material of the sphere to air. (3) Perform numerical simulation and draw a surface temperature distribution diagram of the model with internal defects.

6. The infrared model simulation method of a plain woven orthotropic carbon fiber according to claim 1, characterized in that: The specific steps of step 5 include: (1) Change the fiber layer spacing in the model. (2) Perform numerical simulation and draw the surface temperature curve of the model when the structure changes.

Citation Information

Patent Citations

  • A parameterized modeling method of laminated composite plate imitating mother-of-pearl

    CN108959786A

  • Linear friction welding numerical simulation method for introducing initial defects

    CN111639448A

  • Estimation model for heat conductivity coefficient probability distribution characteristics of braided structure composite material

    CN115630540A

  • Method for predicting high and low temperature mechanical properties of linen fiber composite material

    CN116386776A

  • Fiber paving layer mode conversion metamaterial structure

    CN213808600U