Dielectric layer structure for RRAM device, RRAM device and preparation method thereof
By adopting a stacked structure of the first dielectric layer, the second dielectric layer and the third dielectric layer in the RRAM device, the influence of temperature changes on the dielectric constant is solved, and the dielectric constant instability of the RRAM device at high temperatures is solved. The problem of improving data retention capabilities and overall reliability.
Patent Information
- Application Number
- CN202411099811.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-19
AI Technical Summary
The dielectric layer structure of RRAM devices is unstable at high temperatures, resulting in an increase in programming voltage, affecting the uniformity of the device, erase reliability and data retention capabilities.
Using a stacked structure of the first dielectric layer, the second dielectric layer and the third dielectric layer, the first dielectric layer and the third dielectric layer are used to reduce the influence of temperature changes on the dielectric constant of the second dielectric layer to ensure that The dielectric layer structure remains amorphous at high temperatures, thereby improving the data retention capability and overall reliability of RRAM devices.
Through the stacked structure design, interface interaction is suppressed, the thermal stability and crystallization temperature of the dielectric layer are improved, heat generation is reduced, data retention ability and overall reliability are improved, and device stability and storage density are enhanced.
Smart Images

Figure CN118984648A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a dielectric layer structure for a RRAM device, a RRAM device and a preparation method thereof. Background Art
[0002] As a non-volatile memory device, resistive random access memory (RRAM) has the advantages of simple structure, high storage density and low power consumption. However, the performance of RRAM devices is often limited by the high temperature stability of the dielectric layer structure. In the related art, the dielectric constant of the ALO (aluminum-doped aluminum oxide) dielectric layer structure is unstable at high temperature. The dielectric constant increases with the increase of temperature, which easily leads to an increase in programming voltage, making the uniformity of RRAM devices worse, and generating more heat, affecting the erase reliability and data retention ability of RRAM devices. Summary of the invention
[0003] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, one object of the present invention is to provide a dielectric layer structure for an RRAM device, which helps to maintain the high temperature performance of the dielectric layer structure, thereby facilitating the improvement of the data retention capability and overall reliability of the RRAM device.
[0004] Another object of the present invention is to provide a RRAM device.
[0005] Another object of the present invention is to provide a method for preparing a RRAM device.
[0006] According to an embodiment of the first aspect of the present invention, a dielectric layer structure for an RRAM device includes: a first dielectric layer, a second dielectric layer, and a third dielectric layer arranged in sequence, wherein the dielectric constant of the first dielectric layer and the dielectric constant of the third dielectric layer are both greater than the dielectric constant of the second dielectric layer, and the first dielectric layer and the third dielectric layer are used to reduce the influence of temperature change on the dielectric constant of the second dielectric layer; a side of any one of the first dielectric layer and the third dielectric layer away from the second dielectric layer is connected to the upper electrode of the RRAM device, and a side of the other of the first dielectric layer and the third dielectric layer away from the second dielectric layer is connected to the lower electrode of the RRAM device.
[0007] According to the dielectric layer structure for the RRAM device according to the embodiment of the present invention, a first dielectric layer, a second dielectric layer and a third dielectric layer stacked structure are sequentially arranged, and the first dielectric layer and the third dielectric layer are used to reduce the influence of temperature change on the dielectric constant of the second dielectric layer, so that the dielectric layer structure can maintain an amorphous state at a higher temperature, which helps to maintain the high temperature performance of the dielectric layer structure, thereby facilitating the improvement of the data retention capability and overall reliability of the RRAM device.
[0008] According to some embodiments of the present invention, the first dielectric layer, the second dielectric layer and the third dielectric layer are all oxygen-rich metal oxides.
[0009] According to some embodiments of the present invention, the first dielectric layer and / or the third dielectric layer comprises a compound with a molecular formula of AOx, wherein A is one of Hf, Ta, Ru, Zr, Ti and a rare earth element, O is an oxygen element, and x is a relative amount of the oxygen element;
[0010] And / or, the second dielectric layer includes a compound with a molecular formula of BOy, wherein B is one of Al, Ta, Ru, Zr, Ti, a transition metal element or a rare earth element, O is an oxygen element, and y is a relative amount of the oxygen element.
[0011] According to some embodiments of the present invention, the thickness of the second dielectric layer is d1, the thickness of the first dielectric layer is d2, and the thickness of the third dielectric layer is d3, wherein d1, d2 and d3 satisfy: 1 / 4d1≤d2≤d1, 1 / 4d1≤d3≤d1.
[0012] According to some embodiments of the present invention, d1 satisfies: 5A≤d1≤40A.
[0013] According to some embodiments of the present invention, the roughness of the first dielectric layer and / or the roughness of the third dielectric layer is 5A-20A; and / or the roughness of the second dielectric layer is 5A-30A.
[0014] According to an embodiment of the second aspect of the present invention, an RRAM device comprises: a lower metal interconnection layer; a lower electrode, wherein the lower electrode is arranged on one side of the lower metal interconnection layer in a thickness direction; and a dielectric layer structure, wherein the dielectric layer structure is a dielectric layer structure for an RRAM device according to an embodiment of the first aspect of the present invention, wherein the dielectric layer structure is arranged on a side of the lower electrode away from the lower metal interconnection layer.
[0015] According to some embodiments of the present invention, a metal ion supply layer, an upper electrode and a protective layer are sequentially provided on the side of the dielectric layer structure away from the lower electrode, and the metal ion supply layer is used to provide metal ions to the second dielectric layer of the dielectric layer structure, and the metal of the metal ion supply layer is the same as the metal of the second dielectric layer.
[0016] According to some embodiments of the present invention, a fourth dielectric layer is disposed on the sidewalls of the dielectric layer structure, the metal ion supply layer, the upper electrode and the protective layer.
[0017] According to some embodiments of the present invention, a protective layer is provided on an outer wall of the fourth dielectric layer.
[0018] According to some embodiments of the present invention, the thickness of the metal ion supply layer is 100A to 500A.
[0019] According to a third aspect of the present invention, a method for preparing a RRAM device comprises the following steps: depositing a first dielectric layer, a second dielectric layer and a third dielectric layer in sequence on a side of the lower electrode away from the lower metal interconnection layer.
[0020] According to some embodiments of the present invention, a metal ion supply layer, an upper electrode and a protective layer are sequentially deposited on a side of the third dielectric layer away from the lower electrode, and then etched to obtain the third dielectric layer.
[0021] According to some embodiments of the present invention, a fourth dielectric layer is deposited on the side walls of the first dielectric layer, the second dielectric layer, the third dielectric layer, the metal ion supply layer, the upper electrode and the protective layer, and the protective layer is then deposited on the outer side wall of the fourth dielectric layer.
[0022] According to some embodiments of the present invention, the deposition method is atomic layer deposition or chemical vapor deposition.
[0023] According to some embodiments of the present invention, during the deposition process, the oxygen flow rate is 10 sccm to 60 sccm, the inert gas flow rate is 80 sccm to 200 sccm, the power is 500w to 1500w, the process pressure is 3.5mT to 10mT, and the temperature is less than 270°C.
[0024] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:
[0026] Figure 1 is a schematic diagram of a dielectric layer structure according to an embodiment of the present invention;
[0027] Figure 2 is a partial schematic diagram of a RRAM device according to an embodiment of the present invention;
[0028] Figure 3 yes Figure 2 Schematic diagram of a local portion of a RRAM device and a dielectric layer structure shown in ;
[0029] Figure 4 is a partial schematic diagram of a RRAM device according to an embodiment of the present invention;
[0030] Figure 5is a schematic diagram of a RRAM device according to an embodiment of the present invention.
[0031] Reference numerals:
[0032] 100: dielectric layer structure;
[0033] 1: first dielectric layer; 2: second dielectric layer; 3: third dielectric layer;
[0034] 200: RRAM devices;
[0035] 201: lower metal interconnect layer; 202: lower electrode; 2021: tungsten layer; 202: titanium nitride layer; 203: metal ion supply layer; 204: upper electrode; 205: protective layer; 206: fourth dielectric layer. DETAILED DESCRIPTION
[0036] Reference below Figure 1-Figure 5 A dielectric layer structure 100 for a RRAM device 200 according to an embodiment of the first aspect of the present invention is described. The first dielectric layer 1, the second dielectric layer 2, and the third dielectric layer 3 are stacked and matched in sequence, and the first dielectric layer 1 and the third dielectric layer 3 are used to reduce the influence of temperature change on the dielectric constant of the second dielectric layer 2, thereby improving the dielectric constant stability of the dielectric layer structure 100 at high temperature and enhancing the high temperature stability of the RRAM device 200.
[0037] like Figure 1-Figure 5 As shown, the dielectric layer structure 100 for the RRAM device 200 according to the first embodiment of the present invention comprises a first dielectric layer 1, a second dielectric layer 2 and a third dielectric layer 3 arranged in sequence, wherein the dielectric constant of the first dielectric layer 1 and the dielectric constant of the third dielectric layer 3 are both greater than the dielectric constant of the second dielectric layer 2, and the first dielectric layer 1 and the third dielectric layer 3 are used to reduce the influence of temperature change on the dielectric constant of the second dielectric layer 2. The side of any one of the first dielectric layer 1 and the third dielectric layer 3 away from the second dielectric layer 2 is connected to the upper electrode 204 of the RRAM device 200, and the side of the other one of the first dielectric layer 1 and the third dielectric layer 3 away from the second dielectric layer 2 is connected to the lower electrode 202 of the RRAM device 200.
[0038] Specifically, along the direction from the lower electrode 202 to the upper electrode 204 of the RRAM device 200, the first dielectric layer 1, the second dielectric layer 2, and the third dielectric layer 3 are sequentially arranged; or, the third dielectric layer 3, the second dielectric layer 2, and the first dielectric layer 1 are sequentially arranged. Thus, the dielectric layer structure 100 in the RRAM device 200 can be stably and reliably arranged between the upper electrode 204 and the lower electrode 202, which is conducive to applying different driving voltages to the upper electrode 204 and the lower electrode 202, so that the RRAM device 200 can be switched between different resistance states, that is, from a low resistance state to a high resistance state, or from a high resistance state to a low resistance state.
[0039] The dielectric constant of the second dielectric layer 2 is relatively small, while the dielectric constants of the first dielectric layer 1 and the third dielectric layer 3 are relatively large, which is conducive to reducing the influence of temperature change on the dielectric constant of the second dielectric layer 2, especially the influence of high temperature on the dielectric layer structure 100, so that the dielectric layer structure 100 can remain amorphous at a relatively high temperature, which is conducive to maintaining the high temperature performance of the dielectric layer structure 100. As a result, the dielectric constant stability of the dielectric layer structure 100 is improved, which is conducive to improving the consistency of the dielectric layer structure 100, making the conductivity of the dielectric layer structure 100 regular, and further conducive to improving the data retention capability and overall reliability of the RRAM device 200.
[0040] Among them, the dielectric constant of the first dielectric layer 1 and / or the dielectric constant of the third dielectric layer 3 can be controlled to be greater than 1.5 times the dielectric constant of the second dielectric layer 2, and the multiple can specifically be 1.5, 1.8, 2.0, 2.5, etc., so as to obtain a dielectric layer structure with high dielectric constant stability.
[0041] The performance of the dielectric layer structure 100 can be further improved by designing the laminated structure of the dielectric layer structure 100. Specifically, the laminated structure can effectively suppress the interaction between interfaces and improve the thermal stability and crystallization temperature of the dielectric layer structure 100. Selecting a material with a high dielectric constant (high-k) can reduce the equivalent oxide thickness (EOT) without changing the physical thickness, thereby achieving a reduction in the size of the transistor. At the same time, it also helps to improve the potential barrier and energy gap of the dielectric layer structure 100 and reduce the interface state density and defects.
[0042] The first dielectric layer 1, the second dielectric layer 2 and the third dielectric layer 3 are stacked in sequence, and also have the following advantages:
[0043] In terms of stability: the interaction between interface layers is suppressed. The first dielectric layer 1 or the third dielectric layer 3 is separated from the second dielectric layer 2 and the corresponding upper electrode 204 or lower electrode 202. The second dielectric layer 2 can effectively prevent the interaction between the first dielectric layer 1 and the third dielectric layer 3 and the Si substrate, suppress the occurrence of crystallization, and is conducive to maintaining the good insulation performance of the dielectric layer structure 100.
[0044] Storage density: A dielectric layer structure 100 with the same thickness can provide a larger capacitance, thereby facilitating the realization of the same storage capacity in a smaller area, and further facilitating the miniaturization and high-density integration of the RRAM device 200 .
[0045] In terms of thermal damage: the dielectric layer structure 100 does not increase with the increase of temperature, and its programming voltage does not increase either, so that the heat generated by the dielectric layer structure 100 is reduced, thereby reducing the thermal damage of the RRAM device 200.
[0046] In terms of electric field: the stacked structure of the first dielectric layer 1 , the second dielectric layer 2 , and the third dielectric layer 3 can distribute the electric field more evenly, reduce local high electric field areas, and reduce the possibility of breakdown, thereby improving the stability and reliability of the RRAM device 200 .
[0047] Improved surface smoothness: With the stacked structure of the first dielectric layer 1 , the second dielectric layer 2 , and the third dielectric layer 3 , the dielectric layer structure 100 exhibits atomic-level smoothness after annealing, which helps to reduce leakage and improve the overall performance of the RRAM device 200 .
[0048] In summary, the RRAM device 200 using the stacked structure of the first dielectric layer 1, the second dielectric layer 2 and the third dielectric layer 3 has higher data retention capability, better reliability and better environmental adaptability, which is conducive to the dielectric layer structure 100 providing more stable and efficient performance during use.
[0049] According to the dielectric layer structure 100 for the RRAM device 200 of the embodiment of the present invention, a first dielectric layer 1, a second dielectric layer 2 and a third dielectric layer 3 are sequentially arranged in a stacked structure, and the first dielectric layer 1 and the third dielectric layer 3 are used to reduce the influence of temperature change on the dielectric constant of the second dielectric layer 2, so that the dielectric layer structure 100 can maintain an amorphous state at a higher temperature, which helps to maintain the high temperature performance of the dielectric layer structure 100, thereby facilitating the improvement of the data retention capability and overall reliability of the RRAM device 200.
[0050] According to some embodiments of the present invention, the first dielectric layer 1 , the second dielectric layer 2 , and the third dielectric layer 3 are all oxygen-rich metal oxides.
[0051] In the above embodiment, the oxygen-rich metal oxide can be a metal oxide with excess oxygen or a metal oxide with saturated oxygen. When y>zx / 2, wherein M is a metal element, O is an oxygen element, x is the relative amount of the metal element, y is the relative amount of the oxygen element, z is the valence of the metal element, and according to the stoichiometric ratio, y≥zx / 2. Thus, it is beneficial to ensure the conductivity and storage density of the first dielectric layer 1, the second dielectric layer 2, and the third dielectric layer 3, and it is beneficial to improve the stability and usability of the dielectric layer structure 100. When y>zx / 2, the oxygen-rich metal oxide includes superoxide, peroxide, or oxide with a high oxygen content; when y=zx / 2, the oxygen-rich metal oxide includes a metal oxide with a saturated oxygen content.
[0052] Further, the first dielectric layer 1 and / or the third dielectric layer 3 include a compound with a molecular formula of AOx, wherein A is one of Hf, Ta, Ru, Zr, Ti and rare earth elements, O is an oxygen element, and x is the relative amount of the oxygen element; and / or, the second dielectric layer 2 includes a compound with a molecular formula of BOy, wherein B is one of Al, Ta, Ru, Zr, Ti, a transition metal element or a rare earth element, O is an oxygen element, and y is the relative amount of the oxygen element.
[0053] Hafnium oxide, ruthenium oxide, zirconium oxide, titanium oxide and oxides of rare earth elements all have the advantages of high melting point, strong chemical stability and high dielectric constant. By doping with rare earth elements, for example, by doping with rare earth elements such as lanthanum (La) and neodymium (Nd), the thermal stability and dielectric constant of the dielectric layer structure 100 can be improved. Or by doping with transition metal elements, such as doping with transition metal elements such as hafnium (Hf) and zirconium (Zr), the crystallization temperature of the dielectric layer structure 100 can be increased, and the electrical properties of the dielectric layer structure 100 can be improved. Aluminum oxide has high thermal stability, chemical inertness, high hardness and wear resistance. At the same time, aluminum oxide has a high dielectric constant and can effectively store charge. Doping elements such as Al into the second dielectric layer 2 can significantly increase the crystallization temperature of the dielectric layer structure 100, so that the dielectric layer structure 100 can remain amorphous at a higher temperature, thereby helping to maintain the high temperature performance of the RRAM device 200.
[0054] Therefore, by using the above-mentioned first dielectric layer 1, second dielectric layer 2 and third dielectric layer 3, by controlling the dielectric constant of the first dielectric layer 1 and the dielectric constant of the third dielectric layer 3 to be greater than the dielectric constant of the second dielectric layer 2, it is beneficial to improve the thermal stability and crystallization temperature of the dielectric layer structure 100.
[0055] For example, when the second dielectric layer 2 includes aluminum oxide, and the first dielectric layer 1 and the third dielectric layer 3 each include at least one of hafnium oxide and zirconium oxide, the relative dielectric constant of aluminum oxide is about 9, the relative dielectric constant of hafnium oxide is about 25, and the relative dielectric constant of zirconium oxide is about 27.
[0056] According to some embodiments of the present invention, referring to Figure 1 , the thickness of the second dielectric layer 2 is d1, the thickness of the first dielectric layer 1 is d2, and the thickness of the third dielectric layer 3 is d3, wherein d1, d2 and d3 satisfy: 1 / 4d1≤d2≤d1, 1 / 4d1≤d3≤d1, so that the thicknesses of the first dielectric layer 1, the second dielectric layer 2 and the third dielectric layer 3 can be set more reasonably, which is beneficial for the dielectric layer structure 100 to achieve a larger storage capacity in a smaller area, and is beneficial for reducing local high electric field areas and reducing the possibility of breakdown, thereby improving the stability and reliability of the RRAM device 200.
[0057] In the above embodiment, the thickness d2 of the first dielectric layer 1 and the thickness d3 of the third dielectric layer 3 may be equal or unequal, and the present application does not limit this.
[0058] According to C=εS / 4πkd, where C is capacitance, in farads (F); ε is dielectric constant; d is the distance between the two plates, in meters (m). When the capacitance remains unchanged, d increases, and the dielectric constant ε of the dielectric layer structure 100 increases. At the same time, as the temperature rises, the molecular activity inside the dielectric layer structure 100 is enhanced, causing the dielectric constant to change. Therefore, limiting the stacking arrangement of the dielectric layer structure 100, and / or the thickness of the first dielectric layer 1, the second dielectric layer 2, and the third dielectric layer 3 is beneficial to reducing the influence of temperature on the dielectric constant of the dielectric layer structure 100, thereby reducing the influence of temperature changes on programming voltage changes, and improving the influence of temperature changes on programming voltage uniformity.
[0059] Wherein, d1 satisfies: 5A≤d1≤40A. When the thickness of the second dielectric layer 2 is less than 5A, the thickness of the second dielectric layer 2 is relatively small, which increases the processing difficulty of the dielectric layer structure 100; when the thickness of the second dielectric layer 2 is greater than 40A, the thickness of the second dielectric layer 2 is relatively large, and within the limited thickness of the dielectric layer structure 100, the thickness of the first dielectric layer 1 and the third dielectric layer 3 is reduced, which is easy to affect the improvement of the high-temperature stability of the dielectric constant of the dielectric layer structure 100. Therefore, by setting the thickness of the second dielectric layer 2 at 5A≤d1≤40A, the setting of the thickness of the second dielectric layer 2 is more reasonable, which is conducive to improving the high-temperature stability of the dielectric constant of the dielectric layer structure 100 and giving full play to the effect of the dielectric layer structure 100.
[0060] The roughness of the first dielectric layer 1 and / or the roughness of the third dielectric layer 3 is 5A to 20A. When the roughness of the first dielectric layer 1 and the roughness of the third dielectric layer 3 are less than 5A, the roughness of the first dielectric layer 1 and the roughness of the third dielectric layer 3 are both small, the stability of the connection between the first dielectric layer 1 and the third dielectric layer 3 and the second dielectric layer 2 is poor, and the processing difficulty of the dielectric layer structure 100 is increased; when the roughness of the first dielectric layer 1 and the roughness of the third dielectric layer 3 are greater than 20A, the roughness of the first dielectric layer 1 and the roughness of the third dielectric layer 3 are large, and the rough first dielectric layer 1 and the third dielectric layer 3 are prone to cause additional scattering, affecting the carrier mobility, thereby easily reducing the electrical performance of the RRAM device 200. Therefore, by setting the roughness of the first dielectric layer 1 and the roughness of the third dielectric layer 3 to 5A-20A, the roughness of the first dielectric layer 1 and the roughness of the third dielectric layer 3 are relatively reasonable, which can meet the requirements of stable connection with the second dielectric layer 2 and is conducive to ensuring the electrical performance of the RRAM device 200, thereby improving the reliability of the RRAM device 200.
[0061] The roughness of the second dielectric layer 2 is 5A to 30A. When the roughness of the second dielectric layer 2 is less than 5A, the roughness of the second dielectric layer 2 is small, which is easy to reduce the connection stability and reliability of the second dielectric layer 2 with the first dielectric layer 1 and the third dielectric layer 3; when the roughness of the second dielectric layer 2 is greater than 30A, the roughness of the second dielectric layer 2 is large, and the rough second dielectric layer 2 is easy to cause additional scattering, affecting the carrier mobility. Therefore, by setting the roughness of the second dielectric layer 2 to 5A to 30A, the roughness of the second dielectric layer 2 is more reasonable, which satisfies the stable connection with the first dielectric layer 1 and the third dielectric layer 3, and is conducive to ensuring the electrical performance of the RRAM device 200, thereby improving the reliability of the RRAM device 200.
[0062] Reference Figure 2-Figure 5 The RRAM device 200 according to the second aspect of the present invention comprises a lower metal interconnection layer 201, a lower electrode 202 and a dielectric layer structure 100. The lower electrode 202 is disposed on one side in the thickness direction of the lower metal interconnection layer 201. The dielectric layer structure 100 is a dielectric layer structure 100 for the RRAM device 200 according to the first aspect of the present invention, and the dielectric layer structure 100 is disposed on a side of the lower electrode 202 away from the lower metal interconnection layer 201.
[0063] The lower electrode 202 includes a tungsten layer 2021 and / or a titanium nitride layer 202. However, it is not limited thereto. The titanium nitride layer 202 has good conductivity and can effectively transmit current, thereby improving the overall performance of the RRAM device 200. The tungsten layer 2021 is conducive to reducing the cumulative effect of metal elements in the lower electrode 202 (in multiple formation processes, the lower electrode 202 will be continuously diffused into the second dielectric layer 2 under the cumulative effect of the electric field.), and through the first dielectric layer 1 and the third dielectric layer 3, it is conducive to optimizing the second dielectric layer 2, that is, blocking the diffusion of tungsten (W) into the second dielectric layer 2.
[0064] The RRAM device 200 according to the embodiment of the present invention uses the dielectric layer structure 100 for the RRAM device 200 , which is beneficial to improving the conductivity uniformity and reliability of the RRAM device 200 in a high temperature environment.
[0065] Further, a metal ion supply layer 203, an upper electrode 204 and a protective layer 205 are sequentially provided on a side of the dielectric layer structure 100 away from the lower electrode 202. The metal ion supply layer 203 is used to provide metal ions to the second dielectric layer 2 of the dielectric layer structure 100. The metal of the metal ion supply layer 203 is the same as the metal of the second dielectric layer 2. For example, when the second dielectric layer 2 includes aluminum oxide, the metal of the metal ion supply layer 203 includes aluminum. Such a configuration is conducive to using the metal ion supply layer 203 to provide metal ions to the second dielectric layer 2, so as to provide supplementary metal ions to the dielectric layer structure 100, extend the service life of the RRAM device 200, and improve the use effect of the RRAM device 200. The upper electrode 204 cooperates with the dielectric layer structure 100 and the lower electrode 202 to achieve a reliable conductive connection of the RRAM device 200. The protection layer 205 may be used to protect the upper electrode 204 , the metal ion supply layer 203 and the dielectric layer structure 100 , thereby improving the use safety of the RRAM device 200 and extending the service life of the RRAM device 200 .
[0066] In addition, a fourth dielectric layer 206 is provided on the side walls of the dielectric layer structure 100, the metal ion supply layer 203, the upper electrode 204 and the protective layer 205. The fourth dielectric layer 206 is conducive to isolating the side walls of the dielectric layer structure 100, the metal ion supply layer 203, the upper electrode 204 and the protective layer 205 from the outside, protecting the side walls of the dielectric layer structure 100, the metal ion supply layer 203, the upper electrode 204 and the protective layer 205, thereby improving the use safety and stability of the dielectric layer structure 100, the metal ion supply layer 203, the upper electrode 204 and the protective layer 205. Among them, the fourth dielectric layer 206 can be an AlO layer, a SiN layer, etc. It is not specifically limited here.
[0067] Furthermore, a protective layer 205 is disposed on the outer wall of the fourth dielectric layer 206 . Thus, the fourth dielectric layer 206 is protected by the protective layer 205 to prevent the fourth dielectric layer 206 from being damaged, thereby facilitating the improvement of the service life of the fourth dielectric layer 206 .
[0068] According to some embodiments of the present invention, the thickness of the metal ion supply layer 203 is 100A to 500A. When the thickness of the metal ion supply layer 203 is less than 100A, the metal ion supply layer 203 provides less metal ions to the dielectric layer structure 100, which is difficult to meet the needs of the dielectric layer structure 100; when the thickness of the metal ion supply layer 203 is greater than 500A, the thickness of the metal ion supply layer 203 is large, resulting in an increase in cost, while increasing the volume of the RRAM device 200 and reducing the applicability of the RRAM device 200. Therefore, by setting the thickness of the metal ion supply layer 203 to 100A to 500A, the thickness of the metal ion supply layer 203 is relatively reasonable, which is conducive to controlling the cost and volume of the RRAM device 200 while meeting the needs of the metal ions provided to the dielectric layer structure 100, so as to improve the market competitiveness of the RRAM device 200.
[0069] Reference Figure 2-Figure 5 , a method for preparing a RRAM device 200 according to an embodiment of the third aspect of the present invention comprises the following steps:
[0070] A first dielectric layer 1 , a second dielectric layer 2 and a third dielectric layer 3 are sequentially deposited on a side of the lower electrode 202 away from the lower metal interconnection layer 201 .
[0071] The method for preparing the RRAM device 200 according to the embodiment of the present invention is conducive to achieving efficient and uniform doping, ensuring that the thickness and quality of the deposited first dielectric layer 1, second dielectric layer 2 and third dielectric layer 3 are optimal, so as to improve the quality of the RRAM device 200.
[0072] Further, after the metal ion supply layer 203, the upper electrode 204 and the protective layer 205 are sequentially deposited on the side of the third dielectric layer 3 away from the lower electrode 202, etching is performed to obtain the third dielectric layer 3. The metal ion supply layer 203 is conducive to providing metal ions to the dielectric layer structure 100. The protective layer 205 is arranged on the side of the upper electrode 204 away from the metal ion supply layer 203 to protect the upper electrode 204. Etching is conducive to selectively removing part of the material to form a characteristic profile to meet the size and precision requirements of the RRAM device 200.
[0073] Furthermore, a fourth dielectric layer 206 is deposited on the sidewalls of the first dielectric layer 1, the second dielectric layer 2, the third dielectric layer 3, the metal ion supply layer 203, the upper electrode 204 and the protective layer 205, and then the protective layer 205 is deposited on the outer sidewall of the fourth dielectric layer 206. Thus, the protective layer 205 is used to protect the first dielectric layer 1, the second dielectric layer 2, the third dielectric layer 3, the metal ion supply layer 203 and the upper electrode 204 in the circumferential direction, so as to improve the structural integrity of the RRAM device 200 and improve the quality of the RRAM device 200.
[0074] Furthermore, the deposition method is atomic layer deposition (ALD) or chemical vapor deposition (CVD). Atomic layer deposition uses an alternating, self-limiting surface reaction process to deposit materials, which is conducive to accurately controlling the thickness and composition of the film, and the formed film has a high uniformity and good step coverage. By forming a stacked structure of the dielectric layer structure 100 through atomic layer deposition, the change in temperature will not easily change the dielectric constant of the dielectric layer structure 100 after the stack design, which is conducive to forming a programming voltage with higher consistency, so that the electrical properties of the dielectric layer structure 100 will be more regular and uniform, and show a more stable dielectric constant at high temperature, which is conducive to improving the data retention capability and overall reliability of the RRAM device 200.
[0075] Chemical vapor deposition uses a gaseous precursor to react chemically with the surface of the lower electrode 202 at high temperature, thereby forming a solid film on the lower electrode 202. Chemical vapor deposition has a fast film-forming speed, can be carried out under normal pressure or low vacuum conditions, and the film layer formed by CVD has good bonding with the substrate. In addition, by adjusting the flow rate of various gas raw materials, the composition of the product can be finely controlled. Therefore, the use of chemical vapor deposition to deposit the first dielectric layer 1, the second dielectric layer 2, and the third dielectric layer 3 is conducive to improving the deposition effect and the deposition efficiency.
[0076] Furthermore, during the deposition process, the oxygen flow rate is 10 sccm to 60 sccm, the inert gas flow rate is 80 sccm to 200 sccm, the power is 500 w to 1500 w, the process pressure is 3.5 mT to 10 mT, and the temperature is less than 270°C. Thus, the deposition process is reacted in an inert gas atmosphere, which is beneficial to avoid the occurrence of side reactions and improve the quality of the deposited first dielectric layer 1, the second dielectric layer 2, and the third dielectric layer 3. By controlling the oxygen flow rate, the inert gas flow rate, the power, the process pressure, and the temperature during the deposition process, the deposition accuracy is improved, and the quality of the first dielectric layer 1, the second dielectric layer 2, and the third dielectric layer 3 formed by deposition is improved, so as to improve the quality of the RRAM device 200, thereby improving the market competitiveness of the RRAM device 200.
[0077] The present application does not specifically limit the selection of inert gas. In some embodiments, the inert gas may be argon. Argon is chemically inert and highly stable and can be used as a carrier gas or scavenging gas in the reaction process to help transport oxygen and remove residues while preventing pollutants from contaminating the reaction.
[0078] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example.
[0079] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. A dielectric layer structure for a RRAM device, characterized in that: include: A first dielectric layer, a second dielectric layer, and a third dielectric layer are sequentially arranged, wherein the dielectric constant of the first dielectric layer and the dielectric constant of the third dielectric layer are both greater than the dielectric constant of the second dielectric layer, and the first dielectric layer and the third dielectric layer are used to reduce the influence of temperature change on the dielectric constant of the second dielectric layer; A side of any one of the first dielectric layer and the third dielectric layer away from the second dielectric layer is connected to the upper electrode of the RRAM device, and a side of the other one of the first dielectric layer and the third dielectric layer away from the second dielectric layer is connected to the lower electrode of the RRAM device.
2. The dielectric layer structure for RRAM device according to claim 1, characterized in that: The first dielectric layer, the second dielectric layer and the third dielectric layer are all oxygen-rich metal oxides.
3. The dielectric layer structure for RRAM device according to claim 2, characterized in that: The first dielectric layer and / or the third dielectric layer comprises a compound with a molecular formula of AOx, wherein A is one of Hf, Ta, Ru, Zr, Ti and a rare earth element, O is an oxygen element, and x is a relative amount of the oxygen element; And / or, the second dielectric layer includes a compound with a molecular formula of BOy, wherein B is one of Al, Ta, Ru, Zr, Ti, a transition metal element or a rare earth element, O is an oxygen element, and y is a relative amount of the oxygen element.
4. The dielectric layer structure for RRAM device according to claim 1, characterized in that: The thickness of the second dielectric layer is d1, the thickness of the first dielectric layer is d2, and the thickness of the third dielectric layer is d3, wherein d1, d2, and d3 satisfy: 1 / 4d1≤d2≤d1, 1 / 4d1≤d3≤d1.
5. The dielectric layer structure for RRAM device according to claim 4, characterized in that: The d1 satisfies: 5A≤d1≤40A.
6. The dielectric layer structure for RRAM device according to claim 1, characterized in that: The roughness of the first dielectric layer and / or the roughness of the third dielectric layer is 5A to 20A; and / or The roughness of the second dielectric layer is 5A-30A.
7. A RRAM device, characterized in that: include: a lower metal interconnect layer; A lower electrode, the lower electrode being arranged on one side in the thickness direction of the lower metal interconnect layer; A dielectric layer structure, wherein the dielectric layer structure is a dielectric layer structure for a RRAM device according to any one of claims 1 to 6, and the dielectric layer structure is arranged on a side of the lower electrode away from the lower metal interconnection layer.
8. The RRAM device according to claim 7, characterized in that: A metal ion supply layer, an upper electrode and a protective layer are sequentially arranged on one side of the dielectric layer structure away from the lower electrode. The metal ion supply layer is used to provide metal ions to the second dielectric layer of the dielectric layer structure. The metal of the metal ion supply layer is the same as the metal of the second dielectric layer.
9. The RRAM device according to claim 8, characterized in that: A fourth dielectric layer is disposed on the side walls of the dielectric layer structure, the metal ion supply layer, the upper electrode and the protective layer.
10. The RRAM device according to claim 9, characterized in that: The outer wall of the fourth dielectric layer is provided with a protective layer.
11. The RRAM device according to claim 8, characterized in that: The thickness of the metal ion supply layer is 100 Å to 500 Å.
12. The method for preparing a RRAM device according to any one of claims 7 to 11, characterized in that: The steps include: A first dielectric layer, a second dielectric layer and a third dielectric layer are sequentially deposited on a side of the lower electrode away from the lower metal interconnection layer.
13. The method for preparing a RRAM device according to claim 12, characterized in that: The third dielectric layer is obtained by sequentially depositing a metal ion supply layer, an upper electrode and a protective layer on a side away from the lower electrode and then etching the layer.
14. The method for preparing a RRAM device according to claim 13, characterized in that: A fourth dielectric layer is deposited on the sidewalls of the first dielectric layer, the second dielectric layer, the third dielectric layer, the metal ion supply layer, the upper electrode and the protective layer, and then the protective layer is deposited on the outer sidewall of the fourth dielectric layer.
15. The method for preparing a RRAM device according to any one of claims 12 to 14, characterized in that: The deposition method is atomic layer deposition or chemical vapor deposition.
16. The method for preparing a RRAM device according to claim 15, characterized in that: During the deposition process, the oxygen flow rate is 10 sccm to 60 sccm, the inert gas flow rate is 80 sccm to 200 sccm, the power is 500w to 1500w, the process pressure is 3.5mT to 10mT, and the temperature is less than 270°C.