Nanometer composition containing ceramide E as well as preparation method and application of nanometer composition

Through wrapping technology, active substances such as ceramide E are combined with hyaluronic acid and galactosomiasis-like bacteria fermentation products to form nanocompositions, solving the problem of shampoo destroying the scalp barrier and achieving better scalp repair and hair Improved gloss.

CN118986779APending Publication Date: 2024-11-22SOUTH CHINA INST OF COLLABORATIVE INNOVATION +1
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202411091166.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-09
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing shampoos can damage the sebum barrier when cleaning the scalp, causing sensitive and dryness to the scalp, and cationic conditioners may cause irritation and itching. The existing nourishing shampoos have poor moisturizing effects and cannot effectively repair the scalp barrier.

Method used

Through wrapping technology, active substances such as ceramide E and octanyl glycine are combined with hyaluronic acid and galactosomiae-like bacteria fermentation product filtrate to form nanocompositions, and auxiliary materials such as fat-soluble solvents and polyols are used to increase the water of these substances Phase dispersion and absorption effect form a nanocomposition to repair the scalp.

Benefits of technology

Improve the water solubility and dispersion of ceramide E and octanyl glycine, enhance its transdermal absorption and repair effect on the scalp, significantly improves the scalp barrier function, and improves the hair luster, and nanocompositions Good stability avoids stratification and rupture.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004986620870000071
    Figure BDA0004986620870000071
  • Figure BDA0004986620870000081
    Figure BDA0004986620870000081
  • Figure BDA0004986620870000101
    Figure BDA0004986620870000101
Patent Text Reader

Abstract

The invention belongs to the field of daily chemicals, and discloses a nano composition containing ceramide E as well as a preparation method and application of the nano composition. Fat-soluble active substances of ceramide and capryloyl glycine and water-soluble active substances of hyaluronic acid and galactose yeast-like bacterium fermentation product filtrate are combined, and a fat-soluble solvent, polyhydric alcohol, a wall material and a membrane material stabilizer are used as assistants; the nano composition containing both the water-soluble active substance and the fat-soluble active substance is formed. The ceramide, the capryloyl glycine, the low-molecular-weight hyaluronic acid and the galactose yeast-like bacterium fermentation product filtrate have a synergistic effect, so that the final product has very good effects of repairing a scalp barrier and improving hair luster.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of daily chemicals, and particularly relates to a nanocomposition containing ceramide E and a preparation method and application thereof. Background Art

[0002] At present, people usually take shampoo as the main care for their heads, and the care concept of scalp is still relatively weak. Although shampoo can clean our scalp and hair to make them clean, it also washes away the protective sebum on our scalp. Even the skin barrier of the scalp is sometimes damaged during the cleaning and scratching process. Cationic conditioners are added to the formula of some shampoos, which are also easy to cause certain stimulation to the scalp, thereby causing scalp itching. The itching of the scalp and the dryness of the scalp gradually destroy the barrier function of the head skin, and the problem of scalp sensitivity is becoming more and more serious. Although some shampoos with nourishing effects try to add moisturizing oils to their formulas to achieve the purpose of protecting the scalp, because the residence time of oils on the scalp is short and they have to be washed away in the end, the effect is very unsatisfactory, and the problem of scalp barrier damage is still not solved. Therefore, providing a raw material that can repair the scalp barrier has become one of the problems to be solved urgently. Summary of the invention

[0003] In order to overcome the above-mentioned shortcomings and deficiencies of the prior art, the primary purpose of the present invention is to provide a nanocomposition containing ceramide E.

[0004] Another object of the present invention is to provide a method for preparing the nanocomposition containing ceramide E. The present invention combines water-insoluble and water-soluble active substances through encapsulation technology to prepare a composition with good penetration-promoting and scalp repairing effects.

[0005] Another object of the present invention is to provide an application of the nanocomposition containing ceramide E.

[0006] The purpose of the present invention is achieved through the following solutions:

[0007] The invention provides a nanocomposition containing ceramide E. The nanocomposition comprises, by mass percentage, 1.5-3.0% ceramide E, 0.5-1.2% capryloyl glycine, 10-20% fat-soluble solvent, 2-6% polyol, 3-5% hyaluronic acid, 0.5-3.0% membrane material stabilizer, 1.2-2.0% phospholipid and the remainder galactose yeast-like bacteria fermentation product filtrate.

[0008] In some embodiments of the present invention, the nanocomposition includes, by mass percentage, 2% ceramide E, 0.8% capryloyl glycine, 15% fat-soluble solvent, 4% polyol, 4% hyaluronic acid, 1.5% membrane material stabilizer, 1.6% phospholipids and 71.1% galactose yeast fermentation product filtrate.

[0009] In some embodiments of the present invention, the fat-soluble solvent includes at least one of camellia oil, olive oil, jojoba seed oil, castor oil, hydrogenated castor oil, maleic acid-modified castor oil, and hydrogenated castor oil hydroxystearate.

[0010] In some embodiments of the present invention, the polyol includes at least one of propylene glycol, glycerol, butylene glycol, pentylene glycol, hexylene glycol, and dipropylene glycol.

[0011] In some embodiments of the present invention, the molecular weight of the hyaluronic acid is 400-1500 Da.

[0012] In some embodiments of the present invention, the film material stabilizer includes at least one of caprylic / capric triglyceride, oleic acid, linoleic acid, and octyldodecyl oleate.

[0013] In some embodiments of the present invention, the phospholipid comprises at least one of soy lecithin, hydrogenated soy lecithin, dipalmitoylphosphatidylcholine, palmitoylphosphatidylglycerol and egg yolk lecithin.

[0014] The present invention also provides a method for preparing a nanocomposition containing ceramide E, characterized by comprising:

[0015] (1) adding ceramide E and capryloyl glycine to a fat-soluble solvent and stirring uniformly to obtain an oil phase;

[0016] (2) adding hyaluronic acid to the filtrate of the fermentation product of galactosaccharomyces cerevisiae and polyol, stirring evenly to obtain an aqueous phase;

[0017] (3) adding the oil phase dropwise to the water phase and mixing them evenly to obtain a mixed solution;

[0018] (4) Adding phospholipids and membrane material stabilizers to the mixed solution, and obtaining a nanocomposite containing ceramide E after nano-processing.

[0019] In some embodiments of the present invention, the dropping speed in step (3) is 2-6 mL / min.

[0020] In some embodiments of the present invention, the nano-processing in step (4) is a high-speed shear dispersion process and a microfluidization homogenization process.

[0021] In some embodiments of the present invention, the rotation speed of the high-speed shear dispersion treatment is 6000-12000 rpm, and the time of the high-speed shear dispersion treatment is 10-30 min.

[0022] In some embodiments of the present invention, the homogenization pressure of the microfluidic homogenization process is 50-120 MPa, and the number of homogenization cycles is 2-10 times.

[0023] The present invention also provides an application of a nano-composition containing ceramide E in the preparation of daily chemicals, especially in hair care products.

[0024] In some embodiments of the present invention, the amount of the nanocomposition containing ceramide E added to the daily chemical product is 0.1-30.0% by mass.

[0025] Ceramide is a class of amide compounds formed by the dehydration of long-chain fatty acids and the amino group of sphingosine. Ceramide exists in all eukaryotic cells. As the main component of intercellular lipids in the stratum corneum of the skin, it accounts for more than 50% of sebum in the stratum corneum. It is an important component of the skin's physical barrier and is also involved in the regulation of cell life activities. It has multiple functions such as moisturizing, repairing and anti-aging. At present, common ceramides include ceramide 1 (ceramide EOS), ceramide 2 (ceramide NS), ceramide 3 (ceramide NP), etc. Ceramide E (cetyl-PG light ethyl palmitamide) is a modified and optimized molecular structure of natural ceramide 2. It has the characteristics of moisturizing, promoting the penetration of nutrients, and being easily absorbed by the skin, which can help repair the skin barrier.

[0026] Capryloylglycine is an amino acid ester compound. When used in daily chemicals, capryloylglycine can be used as a conditioner, detergent, etc. Capryloylglycine has good affinity and can promote the absorption of other active substances. It can improve the use effect of other active substances. Capryloylglycine has a strong inhibitory effect on Staphylococcus aureus and Propionibacterium acnes, and can also resist the excessive secretion of sebum, which has a more obvious effect on the prevention and treatment of acne.

[0027] Hyaluronic acid (HA) is a type of viscous polysaccharide composed of D-glucuronic acid (GlcUA) and N-acetylglucosamine (GlcNAc) linked by β-1,3 glycosidic bonds and β-1,4 glycosidic bonds to form unbranched disaccharide repeating units, commonly known as hyaluronic acid. Existing studies have shown that low molecular weight hyaluronic acid (Mr<1×10 4 ) has strong biological activity, can promote wound healing, promote angiogenesis and has immune regulation function, and low molecular weight hyaluronic acid can easily penetrate into the dermis, which is more conducive to the repair of the scalp barrier.

[0028] The filtrate of the fermentation product of galactosporium is obtained by fermentation of Trichosporon. The filtrate of the fermentation product of galactosporium is rich in vitamins, minerals, amino acids, organic acids, enzymes, and yeast peptides, and has the effects of exfoliating, enhancing the antibacterial ability of sebum (outside the stratum corneum), and moisturizing.

[0029] Compared with the prior art, the present invention has the following beneficial effects:

[0030] (1) The present invention combines ceramide, capryloyl glycine fat-soluble active substances and low molecular weight hyaluronic acid, galactose yeast fermentation product filtrate water-soluble active substances, and forms a nanocomposite containing both water-soluble active substances and fat-soluble active substances by using fat-soluble solvents, polyols, wall materials and membrane material stabilizers as auxiliary. When used as a nanocomposite, the fat-soluble ceramide E has a better transdermal absorption effect.

[0031] (2) Both ceramide and capryloyl glycine are fat-soluble compounds, which have the problems of low water solubility, poor water dispersibility, and difficulty in absorption and utilization in water. The present invention prepares a nanocomposite by encapsulating ceramide E and capryloyl glycine in liposomes, thereby improving the dispersibility of ceramide and capryloyl glycine in the aqueous phase system and being more conducive to transdermal absorption. In addition, the aqueous phase system of the nanocomposite also contains low molecular weight hyaluronic acid and galactosyl yeast fermentation product filtrate. Ceramide, capryloyl glycine, low molecular weight hyaluronic acid and galactosyl yeast fermentation product filtrate play a synergistic role, so that the final product has a good effect of repairing the scalp barrier and improving the gloss of hair.

[0032] (3) The nanocomposite prepared by the present invention improves the problems of low water solubility and poor water dispersibility of ceramide E and capryloyl glycine, and improves the application of ceramide E and capryloyl glycine in aqueous dosage form formulations.

[0033] (4) Adding a large amount of active substances to the aqueous phase system often easily leads to instability of the nanocomposite, resulting in demulsification and stratification. The present invention has found through a large number of experiments that the addition of a large amount of filtrate of the fermentation product of galactosyl yeast is not likely to cause fluctuations in the system, and the present invention has found that adding low molecular weight hyaluronic acid to the water-soluble active substance can improve the stability of the system and avoid the subsequent stratification and liposome rupture of the nanocomposite. DETAILED DESCRIPTION

[0034] The present invention is further described in detail below in conjunction with examples, but the embodiments of the present invention are not limited thereto.

[0035] If the specific conditions are not specified in the examples, the experiments were carried out under conventional conditions or conditions recommended by the manufacturer. If the manufacturers of the reagents or instruments are not specified, they are all conventional products that can be purchased commercially.

[0036] The ultra-low molecular weight hyaluronic acid used in the present invention is a low molecular weight hyaluronic acid prepared by enzymatic hydrolysis and purchased from Juwei (Wuxi) Biotechnology Co., Ltd. The weight distribution of the ultra-low molecular weight hyaluronic acid is 400-700Da, 700-900Da, and 1000-1500Da.

[0037] The filtrate of the fermentation product of galactose yeast-like bacteria used in the present invention was purchased from Dongguan Juwei New Material Technology Co., Ltd.

[0038] The hyaluronic acid with a molecular weight of 10000-15000 Da used in the comparative examples of the present invention was purchased from Juwei (Wuxi) Biotechnology Co., Ltd.

[0039] The filtrate of the bifid yeast fermentation product used in the comparative example of the present invention was purchased from Guangzhou Chaohui Biotechnology Co., Ltd.

[0040] Unless otherwise specified, all percentages mentioned in the present invention are by mass percentages.

[0041] Example 1

[0042] A nanocomposition containing ceramide E, comprising, by mass percentage:

[0043] 2% ceramide E, 0.8% capryloyl glycine, 15% hydrogenated castor oil, 4% 1,2-butylene glycol, 4% hyaluronic acid, 1.5% octyldodecanol oleate, 1.6% soy lecithin, and 71.1% galactosyl ferment filtrate.

[0044] Among them, the molecular weight of hyaluronic acid is 700-900Da.

[0045] The preparation method of the nanocomposite of ceramide E is as follows:

[0046] (1) adding ceramide E and capryloyl glycine to hydrogenated castor oil and stirring evenly to obtain an oil phase;

[0047] (2) adding hyaluronic acid to the filtrate of the fermentation product of galactosaccharomyces cerevisiae and 1,2-butanediol, stirring evenly to obtain an aqueous phase;

[0048] (3) adding the oil phase to the water phase at a rate of 4 mL / min and mixing well to obtain a mixed solution;

[0049] (4) Soybean lecithin and octyldodecyl oleate were added to the mixed solution, and after mixing, the solution was subjected to high-speed shear dispersion treatment for 20 min (rotation speed was 9000 rpm), and then subjected to microfluidization homogenization treatment at a homogenization pressure of 80 MPa for 6 times to obtain a nanocomposite containing ceramide E.

[0050] Example 2

[0051] A nanocomposition containing ceramide E, comprising, by mass percentage:

[0052] 1.5% ceramide E, 0.5% capryloyl glycine, 10% jojoba seed oil, 2% 1,2-pentanediol, 5% hyaluronic acid, 0.5% oleic acid, 1.2% palmitoyl phosphatidylglycerol, and 79.3% galactosyl ferment filtrate.

[0053] Among them, the molecular weight of hyaluronic acid is 1000-1500Da.

[0054] The preparation method of the nanocomposite of ceramide E is as follows:

[0055] (1) adding ceramide E and capryloyl glycine to jojoba seed oil and stirring evenly to obtain an oil phase;

[0056] (2) adding hyaluronic acid to the filtrate of the fermentation product of galactosaccharomyces cerevisiae and 1,2-pentanediol, stirring evenly to obtain an aqueous phase;

[0057] (3) adding the oil phase to the water phase at a rate of 6 mL / min and mixing well to obtain a mixed solution;

[0058] (4) Palmitoylphosphatidylglycerol and oleic acid were added to the mixed solution, and after mixing, the solution was subjected to high-speed shear dispersion treatment for 10 min (rotation speed of 6000 rpm), and then subjected to microfluidization homogenization treatment at a homogenization pressure of 120 MPa for 2 times to obtain a nanocomposite containing ceramide E.

[0059] Example 3

[0060] A nanocomposition containing ceramide E, comprising, by mass percentage:

[0061] 3.0% ceramide E, 1.2% capryloyl glycine, 20% maleic acid-modified castor oil, 6% glycerol, 3% hyaluronic acid, 3.0% caprylic / capric triglyceride, 2.0% egg yolk lecithin, and 61.8% galactosyl fermentation product filtrate.

[0062] Among them, the molecular weight of hyaluronic acid is 400-700Da.

[0063] The preparation method of the nanocomposite containing ceramide E is as follows:

[0064] (1) adding ceramide E and capryloyl glycine to maleic acid-modified castor oil and stirring uniformly to obtain an oil phase;

[0065] (2) adding hyaluronic acid to the filtrate of the fermentation product of galactosyl yeast and glycerol, stirring evenly to obtain an aqueous phase;

[0066] (3) adding the oil phase to the water phase at a rate of 2 mL / min and mixing well to obtain a mixed solution;

[0067] (4) Egg yolk lecithin and caprylic / capric triglyceride were added to the mixed solution, and after mixing, the solution was subjected to high-speed shear dispersion treatment for 30 min (rotation speed of 12000 rpm), and then subjected to microfluidization homogenization treatment at a homogenization pressure of 50 MPa for 10 times to obtain a nanocomposite containing ceramide E.

[0068] Embodiment 4-8

[0069] The preparation method of the nanocomposition containing ceramide E in Examples 4-8 is the same as that in Example 1, and only some parameters in the components are different from those in Example 1. The component table of Examples 1 and Examples 4-8 is as follows: Table 1:

[0070] Table 1

[0071]

[0072] Example 9

[0073] Example 9 provides a nanocomposition containing ceramide E, wherein Example 9 differs from Example 1 in that Example 9 replaces the 700-900Da hyaluronic acid in Example 1 with 400-700Da hyaluronic acid of the same mass ratio, and the remaining steps and parameters are the same as Example 1.

[0074] Example 10

[0075] Example 10 provides a nanocomposition containing ceramide E, wherein Example 10 differs from Example 1 in that, in Example 10, the hyaluronic acid of 700-900Da in Example 1 is replaced with hyaluronic acid of 1000-1500Da of the same mass ratio, and the remaining steps and parameters are the same as in Example 1.

[0076] Comparative Example 1

[0077] Comparative Examples 1-4 provide a nanocomposite. The preparation method of the nanocomposite is the same as that of Example 1. The components of the nanocomposite of Comparative Examples 1-4 are shown in Table 2 below.

[0078] Table 2

[0079]

[0080] Comparative Example 5

[0081] Comparative Example 5 provides a nanocomposition containing ceramide NPs, wherein the difference between Comparative Example 5 and Example 1 is that in Comparative Example 5, ceramide E in Example 1 is replaced with ceramide NPs of equal mass, and the remaining steps and parameters are the same as in Example 1.

[0082] Comparative Example 6

[0083] Comparative Example 6 provides a nanocomposition containing ceramide E, wherein the difference between Comparative Example 6 and Example 1 is that in Comparative Example 6, the filtrate of the fermentation product of the galactosaccharomyces cerevisiae-like bacteria in Example 1 is replaced with the filtrate of the fermentation product of the bifid yeast of the same mass, and the remaining steps and parameters are the same as in Example 1.

[0084] Comparative Example 7

[0085] Comparative Example 7 provides a nanocomposition containing ceramide E, wherein the difference between Comparative Example 7 and Example 1 is that in Comparative Example 7, the capryloyl glycine in Example 1 is replaced with salicylic acid of the same mass, and the remaining steps and parameters are the same as in Example 1.

[0086] Comparative Example 8

[0087] Comparative Example 8 provides a nanocomposition containing ceramide E, wherein the difference between Comparative Example 8 and Example 1 is that in Comparative Example 8, the 700-900Da hyaluronic acid in Example 1 is replaced with 10000-15000Da hyaluronic acid of the same mass, and the remaining steps and parameters are the same as in Example 1.

[0088] Comparative Example 9

[0089] Comparative Example 9 provides a nanocomposition containing ceramide E. The difference between Comparative Example 9 and Example 1 is that in Comparative Example 9, no membrane material stabilizer is added, and an equal mass of galactose yeast-like bacteria fermentation product filtrate is used instead, and the remaining steps and parameters are the same as those in Example 1.

[0090] Comparative Example 10

[0091] Comparative Example 10 provides a nanocomposition containing ceramide E, wherein the difference between Comparative Example 10 and Example 1 is that in Comparative Example 10, octyldodecyl oleate in Example 1 is replaced with cholesterol of the same mass, and the remaining steps and parameters are the same as in Example 1.

[0092] Comparative Example 11

[0093] In Comparative Example 11, a nanocomposition containing ceramide E was added, wherein, in Comparative Example 11, no polyol was added, and an equal mass of galactosyl yeast fermentation product filtrate was used instead, and the remaining steps and parameters were the same as those in Example 1.

[0094] Comparative Example 12

[0095] Comparative Example 12 provides a nanocomposition containing ceramide E, which includes, by mass percentage, 2% ceramide E, 0.8% capryloyl glycine, 15% hydrogenated castor oil, 4% 1,2-butylene glycol, 4% hyaluronic acid, 1.5% octyldodecanol oleate, 1.6% soy lecithin and 71.1% galactose yeast fermentation product filtrate.

[0096] Among them, the molecular weight of hyaluronic acid is 700-900Da.

[0097] The preparation method of the nanocomposite of ceramide E is as follows:

[0098] (1) adding ceramide E, capryloyl glycine, soybean lecithin and octyldodecyl oleate to hydrogenated castor oil and stirring uniformly to obtain an oil phase;

[0099] (2) adding hyaluronic acid to the filtrate of the fermentation product of galactosaccharomyces cerevisiae and 1,2-butanediol, stirring evenly to obtain an aqueous phase;

[0100] (3) adding the oil phase to the water phase at a rate of 4 mL / min and mixing well to obtain a mixed solution;

[0101] (4) The mixed solution was subjected to high-speed shear dispersion treatment for 20 min (rotation speed of 9000 rpm), and then subjected to microfluidization homogenization treatment at a homogenization pressure of 80 MPa for 6 times to obtain a nanocomposite containing ceramide E.

[0102] Test Example 1: Stability Test

[0103] Test samples: nanocomposites of Examples 1-10 and Comparative Examples 1-12.

[0104] Test steps: Take 10 mL of the test sample and put it in a colorless transparent PE sample bottle, seal the sample and place it indoors at room temperature and 45°C for 8 weeks, record the 0th week and the 4th week. Test the odor and delamination of the sample. The test results are shown in Table 3 below.

[0105] Table 3

[0106]

[0107]

[0108] The test results show that the nanocompositions of the embodiments of the present invention have good stability. The nanocompositions did not change after being placed at room temperature (25°C) and 45°C for 4 weeks. Some nanocompositions in the comparative example deteriorated to varying degrees after being placed at 25°C and 45°C for 4 weeks. Capryloyl glycine has a certain antibacterial effect. Capryloyl glycine is not added to the nanocomposition of comparative example 2, and the antibacterial performance of the system deteriorates and is prone to deterioration. Therefore, the nanocomposition of comparative example 2 has a sour taste after being placed at 45°C for 4 weeks. The nanocomposition of comparative example 3 does not add hyaluronic acid, and the composition shows stratification after being placed for 4 weeks, indicating that hyaluronic acid plays an important role in maintaining the stability of the system. Comparative Example 1 and Comparative Example 6 show that after replacing the filtrate of the fermentation product of galactose yeast-like bacteria with the filtrate of the fermentation product of bifid yeast, the compatibility of the filtrate of the fermentation product of bifid yeast with other substances in the system is poor, which easily causes the instability of the system. Comparative Example 7 replaces capryloyl glycine with salicylic acid of similar properties, and the prepared composition is still unstable. Comparative Example 8 replaces low molecular weight hyaluronic acid with high molecular weight hyaluronic acid, and the molecular weight of hyaluronic acid becomes large, which easily causes sedimentation and leads to instability of the system. Comparative Examples 9 and 10 are respectively not adding film material stability and replacing the film material stabilizer with cholesterol. In Comparative Example 11, no polyol is added, and the stability of the final nanocomposite is reduced, and stratification occurs, indicating that the type of film material stabilizer and whether polyol is added or not have a great influence on the stability of the final composition. The present invention preferably uses caprylic / capric triglyceride, oleic acid, linoleic acid, and octyl dodecanol oleate as the film material stabilizer of the nanocomposite of the present invention. Comparative Example 12 changes the preparation process of the nanocomposite, and the wall material and film material stabilizer are added in step (1), which will cause the prepared nanocomposite to change, causing instability of the system.

[0109] Test Example 2: Particle Size Test

[0110] The particle sizes of the nanocomposites of Examples 1-10 and Comparative Examples 1-10 were characterized by a Malvern Nano-ZS90 dynamic light scattering particle size analyzer. The test angle was 90° and the test temperature was 25°C. Three parallel experiments were performed for each group of experiments, and the arithmetic mean of the experimental results was taken.

[0111] The test results are shown in Table 4 below.

[0112] Table 4

[0113]

[0114]

[0115] The test results show that the composition prepared by the present invention is a nanocomposite, and the particle size of the composition in the embodiment is below 300nm. Among them, capryloyl glycine, hyaluronic acid and galactose yeast-like fermentation product filtrate are not added in Comparative Examples 2, 3, and 4, respectively, and Comparative Example 6 replaces the galactose yeast-like fermentation product filtrate with bifid yeast fermentation product filtrate, Comparative Example 7 replaces capryloyl glycine with salicylic acid, and Comparative Example 8 replaces hyaluronic acid with a molecular weight of 700-900Da with hyaluronic acid with a molecular weight of 10000-15000Da. The particle size of the nanocomposite finally obtained becomes larger, indicating that capryloyl glycine, hyaluronic acid (molecular weight 400-1500Da) and galactose yeast-like fermentation product filtrate are added to the system, which helps to reduce the particle size of the nanocomposite. Comparative Example 5 replaces ceramide E with ceramide NP, and the particle size of the nanocomposite finally obtained becomes larger, indicating that the system of the present invention is more suitable for encapsulating ceramide E, and the particle size of the nanocomposite finally obtained is also smaller. Comparative Example 9 does not add a film material stabilizer, Comparative Example 10 replaces the type of film material stabilizer from octyl dodecanol oleate with cholesterol, Comparative Example 11 does not add a polyol, and Comparative Example 12 adjusts the preparation process of the nanocomposite. The particle size of the nanocomposite finally prepared becomes larger, indicating that the type of film material stabilizer in the nanocomposite, whether polyol is added, and the preparation process have a great influence on the particle size of the final product. The film material stabilizer of the nanocomposite of the present invention is preferably at least one of caprylic / capric triglyceride, oleic acid, linoleic acid, and octyl dodecanol oleate.

[0116] Test Example 3: Encapsulation Efficiency Test

[0117] Test samples: nanocomposites of Examples 1-10 and Comparative Examples 1-12.

[0118] Test steps:

[0119] (1) Test of ceramide E encapsulation efficiency: 200 μL of the nanocomposition was taken and subjected to ultrafiltration centrifugation (9000 rpm, 30 min). 5 μL of the filtrate was measured by high performance liquid chromatography (HPLC, Shimadzu, Japan) to determine the concentration of ceramide E in the filtrate (standard curve method), and the concentration of ceramide E not encapsulated in the nanocomposition was obtained. Another nanocomposition was taken and added with a mixed solution of methanol and water. Ultrasonic demulsification was performed for 30 min at a ratio of sample: methanol: water = 1:4:5 (v / v). After filtering through a 0.45 μm organic filter membrane, 5 μL of the sample solution was taken and subjected to high performance liquid chromatography (HPLC, Shimadzu, Japan) to determine the concentration of ceramide E, and the concentration of ceramide E in the nanocomposition was obtained. The encapsulation efficiency (EE) of ceramide E in the nanocomposition was calculated according to formula (1).

[0120] (2) Capryloylglycine encapsulation efficiency test: Take 200 μL of the nanocomposition, and ultrafiltration centrifuge (9000 rpm, 30 min), take 5 μL of the filtrate and pass it through a high performance liquid chromatograph (HPLC, Shimadzu, Japan), and determine the concentration of capryloylglycine in the filtrate (standard curve method), that is, the concentration of capryloylglycine not encapsulated in the nanocomposition. Take another nanocomposition, add a mixed solution of methanol and water, and ultrasonically demulsify for 30 min according to the ratio of sample: methanol: water = 1:4:5 (v / v). After filtering through a 0.45 μm organic filter membrane, take 5 μL of the sample solution and pass it through a high performance liquid chromatograph (HPLC, Shimadzu, Japan), and determine the concentration of capryloylglycine, that is, the concentration of capryloylglycine in the nanocomposition. The encapsulation efficiency (EE) of capryloylglycine in the nanocomposition is calculated according to Formula 1.

[0121] Formula 1:

[0122] Wherein, C1 represents the concentration of unencapsulated ceramide E or octanoyl glycine in the sample; C0 represents the concentration of ceramide E or octanoyl glycine in the sample after ultrasonic demulsification of a mixed solution of methanol and deionized water.

[0123] The test results are shown in Table 5 below.

[0124] Table 5

[0125]

[0126]

[0127] The test results show that the nanocomposition of the embodiment of the present invention has a good encapsulation effect on ceramide E and octanoyl glycine, and the encapsulation rates of ceramide E and octanoyl glycine are both above 90%. The nanocomposition of the comparative example has a poor encapsulation effect on ceramide E and octanoyl glycine. In comparative example 1, ceramide E is not added, and correspondingly, the encapsulation effect of the composition on octanoyl glycine becomes worse. In comparative example 2, octanoyl glycine is not added, and correspondingly, the encapsulation effect of the composition on ceramide E becomes worse, indicating that the combined use of ceramide E and octanoyl glycine can improve the encapsulation effect of each other's active substances. In comparative example 4, no galactose yeast-like bacteria fermentation product filtrate is added, which corresponds to a large increase in the amount of ceramide E and octanoyl glycine, resulting in a very poor encapsulation effect of the composition on ceramide E and octanoyl glycine. The embedding effect of the nanocompositions of Comparative Examples 3 and 6 on ceramide E and capryloyl glycine is worse than that of Example 1, indicating that in the present invention, hyaluronic acid and galactose yeast fermentation product filtrate can promote the embedding of ceramide E and capryloyl glycine, and the final product has a high encapsulation rate for ceramide E and capryloyl glycine. After replacing ceramide E with ceramide NP in Comparative Example 5, the encapsulation rate of the nanocomposition on ceramide NP is only 79.6%, indicating that the nanocomposition of the present invention is more suitable for embedding ceramide E. Comparative Example 7 replaces capryloyl glycine with salicylic acid, and the embedding effect of the final composition on ceramide E and salicylic acid becomes worse, indicating that in the present invention, it is more suitable to combine capryloyl glycine with ceramide E to prepare a nanocomposition. Comparative Example 8 replaces hyaluronic acid with a molecular weight of 700-900Da with hyaluronic acid with a molecular weight of 10000-15000Da, and the embedding effect of the composition on ceramide E and capryloyl glycine becomes worse, indicating that the present invention is more suitable for preparing a nanocomposition using ultra-low molecular weight hyaluronic acid. Comparative Examples 9-11 respectively adjusted the film material stabilizer, polyol, etc., and the embedding effect of the final product on ceramide E and capryloyl glycine became worse. It shows that if the film material stabilizer is not added or the type of the film material stabilizer is changed, the wall material of the nanocomposite will also be changed, which ultimately affects the embedding effect of the final product. In Comparative Example 11, no polyol is added, and the flexibility of the prepared liposome wall material becomes worse, resulting in a poor embedding effect of the final product. The film material stabilizer of the nanocomposite of the present invention is preferably at least one of caprylic / capric triglyceride, oleic acid, linoleic acid, and octyl dodecanol oleate. The polyol is preferably at least one of propylene glycol, glycerol, butylene glycol, pentanediol, hexylene glycol, and dipropylene glycol. In Comparative Example 12, the preparation process of the nanocomposite was adjusted, and the encapsulation effect of the final product was very poor. The encapsulation rate of the nanocomposite for ceramide E was only 42.6%, and the encapsulation effect for capryloylglycine was only 50.3%. In order to prepare a composition with good encapsulation effect for ceramide E and capryloylglycine, the phospholipids and membrane material stabilizers should be mixed in the water phase and the oil phase before adding.

[0128] Test Example 4: Scalp Barrier Repair Test

[0129] Test samples: the nanocompositions of Examples 1-10 and Comparative Examples 1-12, and the composition (2% ceramide E, 0.8% capryloyl glycine, 4% hyaluronic acid (molecular weight 700-900Da) and 93.2% galactosyl yeast fermentation product filtrate were mixed evenly) were prepared into hair essences. Another base essence was prepared.

[0130] The preparation method of the hair essence is as follows: 10% of the nanocomposition or the composition, 1% of transparent xanthan gum, 0.1% of carbomer and 88.9% of deionized water are uniformly mixed at 40 DEG C, and the hair essence is obtained after cooling.

[0131] The preparation method of the matrix essence is as follows: 1% transparent xanthan gum, 0.1% carbomer and 98.9% deionized water are uniformly mixed at 40°C, and the matrix essence is obtained after cooling.

[0132] Test steps: 240 volunteers with damaged scalp were randomly divided into 24 groups, 10 people in each group, and each group used a test sample. Volunteers took 3-5ml of hair essence or matrix essence each time, applied it evenly on the scalp and hair, and massaged appropriately to promote absorption. Use it twice a day for 4 consecutive weeks. The scalp moisture loss rate was tested with the skin moisture loss tester TM300 before use and after 4 weeks of use, and the change rate of the scalp moisture loss rate was calculated.

[0133] The calculation method of the change rate of scalp moisture loss rate (A) is shown in Formula 2.

[0134] Formula 2:

[0135] Among them, A1 represents the scalp moisture loss rate after 4 weeks of use, and A0 represents the scalp moisture loss rate before use.

[0136] The test results are shown in Table 6 below.

[0137] Table 6

[0138]

[0139]

[0140] The scalp moisture loss rate is a negative value, indicating that after using the essence, the scalp moisture loss rate of the scalp is reduced, the scalp has a better water-locking effect, and the test product has a repairing effect. As shown in the test results in the above table, the essence added with the nanocomposition of the embodiment of the present invention has a good scalp repairing effect. After the volunteers used it for 4 weeks, the scalp moisture loss rate was reduced a lot. No active components were added to the matrix essence. After the volunteers used the matrix essence, the scalp moisture loss rate did not decrease, which also shows that the nanocomposition of the present invention has a good scalp repairing effect. The scalp repairing effect of Example 1 is better than that of Comparative Examples 1-8, indicating that in the present invention, ceramide E, capryloyl glycine, hyaluronic acid (molecular weight 400-1500Da) and galactose yeast-like fermentation product filtrate can synergize, so that the final product has a good scalp repairing effect. Without adding one of the four substances (Comparative Examples 1-4), or replacing ceramide E with ceramide NP (Comparative Example 5), replacing the filtrate of the fermentation product of galactosaccharomyces cerevisiae with the filtrate of the fermentation product of bifida yeast (Comparative Example 6), replacing capryloyl glycine with salicylic acid (Comparative Example 7), or replacing the hyaluronic acid with a molecular weight of 700-900Da with a hyaluronic acid with a molecular weight of 10000-15000Da (Comparative Example 8), the scalp repair effect of the final product becomes worse. Comparing Comparative Example 2 and Comparative Example 7, it can be seen that the scalp repair effect of adding salicylic acid to the system is worse than that of not adding capryloyl glycine, indicating that the addition of salicylic acid weakens the scalp repair effect of the entire composition. The scalp repairing effect of Example 1 is better than that of Comparative Examples 9-12, indicating that the type of film material stabilizer and the addition of polyols in the present invention affect the particle size of the final product and the embedding effect of ceramide E and capryloyl glycine, resulting in poor penetration effect and scalp repairing effect of the final product. Although the scalp repairing effects of Comparative Examples 9 and 10 are better than those of some comparative examples, Comparative Examples 9 and 10 have poor stability (see Test Example 1) and are not suitable for practical applications.

[0141] Test Example 5: Hair gloss test

[0142] Test sample: same as Example 4

[0143] Test steps:

[0144] (1) Hair bundle treatment: 240 hair bundles were randomly divided into 24 groups, each with 10 hair bundles, and each group of hair bundles used one test sample. The hair bundles were soaked in a 75wt% alcohol solution for 30 minutes, cleaned and then soaked in a 3wt% fatty alcohol polyoxyethylene ether sodium sulfate (AES) aqueous solution for 30 minutes, rinsed with tap water while smoothing the hair, washed, and hung at room temperature to dry naturally before use.

[0145] (2) Sample treatment: 1.5 mL of the test sample was gently and evenly applied to the upper, middle and lower sections of the hair bundle. The hair bundle was hung to dry naturally at room temperature for 5 consecutive days.

[0146] (3) Hair gloss test: Before using the sample and 5 days after using the sample, the gloss of the upper, middle and lower sections of the hair was tested, and the test results were averaged. The rate of change of the hair gloss before and after use was calculated, and the test results were averaged.

[0147] Test instrument: SAMBA HAIR hair gloss analysis system.

[0148] The calculation method of the glossiness change rate (B) is shown in Formula 3.

[0149] Formula 3:

[0150] Wherein, B1 represents the glossiness value of the hair after using the sample, and B0 represents the glossiness value of the hair after using the sample.

[0151] The test results are shown in Table 7 below.

[0152] Table 7

[0153] Group Glossiness change rate (%) Group Glossiness change rate (%) Matrix Essence -0.2 Composition 0.8 Example 1 29.5 Comparative Example 1 10.5 Example 2 24.7 Comparative Example 2 15.2 Example 3 21.8 Comparative Example 3 13.4 Example 4 25.2 Comparative Example 4 6.7 Example 5 27.0 Comparative Example 5 17.7 Example 6 29.1 Comparative Example 6 14.6 Example 7 27.3 Comparative Example 7 16.3 Example 8 28.8 Comparative Example 8 18.6 Example 9 29.3 Comparative Example 9 17.5 Example 10 27.9 Comparative Example 10 19.3 / / Comparative Example 11 19.5 / / Comparative Example 12 9.8

[0154] The test results show that after using the essence containing the nanocomposition of the embodiment of the present invention, the glossiness of the hair is greatly improved, and the glossiness change rate of the hair is increased by more than 20%. It shows that the nanocomposition of the present invention has a good effect of improving the glossiness of the hair. The glossiness change rate of Example 1 is higher than that of Comparative Examples 1-8, indicating that in the present invention, ceramide E, capryloyl glycine, hyaluronic acid (molecular weight 400-1500Da) and galactosaccharomyces fermentation product can synergize, so that the final product has a good effect of improving the glossiness of the hair. Without adding one of the four substances (Comparative Examples 1-4), or replacing ceramide E with ceramide NP (Comparative Example 5), replacing the filtrate of the galactosaccharomyces fermentation product with the filtrate of the bifid yeast fermentation product (Comparative Example 6), replacing capryloyl glycine with salicylic acid (Comparative Example 7), or replacing the hyaluronic acid with a molecular weight of 700-900Da with the hyaluronic acid with a molecular weight of 10000-15000Da (Comparative Example 8), the effect of improving the glossiness of the hair of the final product becomes worse. The scalp repairing effect of Example 1 is better than that of Comparative Examples 9-12, indicating that the type of film material stabilizer, whether polyols are added, and the order of feeding in the preparation process in the present invention all affect the hair lifting effect of the final product. The present invention preferably uses caprylic / capric triglyceride, oleic acid, linoleic acid, and octyl dodecanol oleate as the film material stabilizer of the nanocomposite of the present invention. The polyol is preferably at least one of propylene glycol, glycerol, butylene glycol, pentanediol, hexanediol, and dipropylene glycol. When preparing the nanocomposite, the phospholipid and the film material stabilizer are mixed in the water phase and the oil phase before being added.

[0155] The above embodiments are preferred implementation modes of the present invention, but the implementation modes of the present invention are not limited to the above embodiments. Any other changes, modifications, substitutions, combinations, and simplifications that do not deviate from the spirit and principles of the present invention should be equivalent replacement methods and are included in the protection scope of the present invention.

Claims

1. A nanocomposition containing ceramide E, characterized in that In terms of mass percentage, the nanocomposition comprises: 1.5-3.0% ceramide E, 0.5-1.2% capryloyl glycine, 10-20% fat-soluble solvent, 2-6% polyol, 3-5% hyaluronic acid, 0.5-3.0% membrane material stabilizer, 1.2-2.0% phospholipid and the remainder galactose yeast-like bacteria fermentation product filtrate.

2. The nanocomposition containing ceramide E according to claim 1, characterized in that In terms of mass percentage, the nanocomposition includes: 2% ceramide E, 0.8% capryloyl glycine, 15% fat-soluble solvent, 4% polyol, 4% hyaluronic acid, 1.5% membrane material stabilizer, 1.6% phospholipid and 71.1% galactose yeast-like bacteria fermentation product filtrate.

3. The nanocomposition containing ceramide E according to claim 1 or 2, characterized in that: The fat-soluble solvent includes at least one of camellia oil, olive oil, jojoba seed oil, castor oil, hydrogenated castor oil, maleic acid-modified castor oil, and hydrogenated castor oil hydroxystearate.

4. The nanocomposition containing ceramide E according to claim 1 or 2, characterized in that: The polyol includes at least one of propylene glycol, glycerol, butylene glycol, pentanediol, hexylene glycol and dipropylene glycol.

5. The nanocomposition containing ceramide E according to claim 1 or 2, characterized in that: The molecular weight of the hyaluronic acid is 400-1500Da.

6. The nanocomposition containing ceramide E according to claim 1 or 2, characterized in that: The membrane material stabilizer includes at least one of caprylic / capric triglyceride, oleic acid, linoleic acid, and octyldodecyl oleate; The phospholipids include at least one of soybean lecithin, hydrogenated soybean lecithin, dipalmitoylphosphatidylcholine, palmitoylphosphatidylglycerol and egg yolk lecithin.

7. A method for preparing a nanocomposition containing ceramide E according to any one of claims 1 to 6, characterized in that The following steps are involved: (1) adding ceramide E and capryloyl glycine to a fat-soluble solvent and stirring uniformly to obtain an oil phase; (2) adding hyaluronic acid to the filtrate of the fermentation product of galactosaccharomyces cerevisiae and polyol, stirring evenly to obtain an aqueous phase; (3) adding the oil phase dropwise to the water phase and mixing them evenly to obtain a mixed solution; (4) Adding phospholipids and membrane material stabilizers to the mixed solution, and obtaining a nanocomposite containing ceramide E after nano-processing.

8. The method for preparing the nanocomposition containing ceramide E according to claim 7, characterized in that: The nano-processing in step (4) is a high-speed shear dispersion process and a microfluidization homogenization process; the rotation speed of the high-speed shear dispersion process is 6000-12000rpm, and the time of the high-speed shear dispersion process is 10-30min; the homogenization pressure of the microfluidization homogenization process is 50-120MPa, and the number of homogenization cycles is 2-10 times.

9. Use of the nanocomposition containing ceramide E according to any one of claims 1 to 7 in daily chemical products, especially in hair care products.

10. The use of the nanocomposition containing ceramide E in daily chemicals according to claim 9, characterized in that: In terms of mass percentage, the nanocomposition containing ceramide E is added to the daily chemical product in an amount of 0.1-30.0%.

Citation Information

Cited By

  • Oil-control shampoo composition and preparation method thereof

    CN121533923A

  • An oil control shampoo composition and a method of making the same

    CN121533923B