Injection mold for preparing injection molding part identification and preparation method

Through injection mold and reset rod technology, combined with the use of hard and soft rubber, the problem of easy scratching of the shell marking of electronic products is solved, and the scratch resistance and durability of the labeling of injection molded parts is achieved, and the appearance and performance of the product is improved.

CN118990924APending Publication Date: 2024-11-22TONGDA (XIAMEN) PRECISION RUBBER & PLASTIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411150016.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing electronic product housing logos are prone to scratches or scratches, lacking scratch resistance and durability.

Method used

The injection mold is used to process the injection molding part marking process, and the retractable reset rod is used to form the insertion zone and soft rubber runner, combining the use of hard rubber and soft rubber to ensure the different colors of the marking frame and rubber encapsulation zone, and adjust it through the reset rod. Soft rubber flow rate, fill the glue wrap area.

Benefits of technology

Good scratch resistance and durability of injection molded parts are achieved, and it is more wear-resistant, chemical corrosion-resistant, adhesion and sense of layering than the prior art surface coating structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118990924A_ABST
    Figure CN118990924A_ABST
Patent Text Reader

Abstract

According to the injection mold and the preparation method, a reset rod extends out of the cavity wall of a movable mold core, so that it is guaranteed that the end, facing a cavity of the movable mold core, of the reset rod extends into a closed part of a mark skeleton during injection molding of an injection molding part skeleton; then, the reset rod retracts during injection molding of the rubber coating area, so that the end, facing the cavity of the movable mold core, of the reset rod leaves the insertion area, a soft rubber runner penetrating through the cavity wall of the closed part is formed, and after soft rubber is injected, the soft rubber runner is closed. According to the injection molding part identification, the rubber coating areas on the inner side and the side of the identification framework can be filled with the soft rubber, the color of the identification framework and the color of the rubber coating areas are different, and therefore the injection molding part identification can be machined through the injection molding technology, and compared with an identification of a surface coating structure in the prior art, the injection molding part identification has good scratch resistance and durability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of injection molding, and in particular to an injection mold and a preparation method for preparing injection molded part markings. Background Art

[0002] Common electronic products on the market, such as ear-hook headphones, have logos of various colors on the surface of their shells, abbreviated as Logo in English. Generally, the shell is injection molded, and then different patterns of logos are formed on the surface of the shell through processing techniques such as spray printing, pad printing or patching. However, after a period of use, the logo is easily scratched or scraped off. Therefore, this type of logo is not scratch-resistant and durable. Summary of the invention

[0003] To this end, the present invention provides an injection mold and a preparation method for preparing injection molded part markings to solve the above problems. The injection molded part markings are processed through an injection molding process and have good scratch resistance and durability.

[0004] To achieve the above purpose, the technical solution provided by the present invention is as follows:

[0005] The present invention provides an injection mold for preparing injection molded part identification, comprising a first mold and a second mold, and also comprising a movable mold core respectively matched with the first mold and the second mold; the injection molded part comprises an injection molded part skeleton and a rubber-coated area wrapping the injection molded part skeleton, the injection molded part skeleton has a protruding identification skeleton, the identification skeleton has a closed sealing part, the sealing part has a cavity opening outward, and the colors of the identification skeleton and the rubber-coated area are set differently from each other; the movable molds of the first mold and the second mold respectively have installation cavities for positioning with the movable mold core, and the movable mold core is detachably arranged in the installation cavities of the movable molds of the first mold and the second mold; the first mold is used to cooperate in molding the injection molded part skeleton, and the second mold is used to cooperate in wrapping the injection molded part with soft glue The plastic part skeleton forms the rubber-coated area, and the rubber-coated area is exposed on the outward side of the identification skeleton; a retractable reset rod is arranged in the movable mold core, and the reset rod corresponds to the closed part; when the injection molded part skeleton is injection molded in the first mold, the reset rod extends out of the cavity wall of the movable mold core, so that the reset rod extends into the closed part of the identification skeleton toward the end of the cavity of the movable mold core, and forms an insertion area, and the insertion area laterally penetrates the inner and outer surfaces of the cavity wall of the closed part; when the rubber-coated area is injection molded in the second mold, the reset rod is retracted so that the reset rod leaves the insertion area toward the end of the cavity of the movable mold core, so as to form a soft rubber flow channel penetrating the cavity wall of the closed part, thereby ensuring that the inner and side rubber-coated areas of the identification skeleton are filled with soft rubber, and the injection molded part identification is formed at the same time.

[0006] Furthermore, the reset rod includes an insert pin and a reset spring sleeved on the insert pin; a limit plate for limiting the extension distance of the insert pin is arranged in the movable mold core to adjust the flow rate of the soft rubber flowing through the soft rubber flow channel.

[0007] Furthermore, the movable mold of the first mold is provided with a movable platen for abutting the reset rod, so as to ensure that the reset rod is abutted by the movable platen and abuts against the limit plate during injection molding in the first mold.

[0008] Furthermore, when the reset rod retracts and resets, one end of the reset rod facing away from the cavity of the movable mold core protrudes out of the bottom of the movable mold core, and the movable mold of the second mold is provided with a clearance groove for allowing the protruding part of the reset rod to protrude from the bottom of the movable mold core to ensure that the reset rod retracts and resets.

[0009] Furthermore, positioning pins for guiding and positioning the movable mold core are arranged in the mounting cavities of the movable molds of the first mold and the second mold, and the movable mold core is provided with positioning grooves matching the positioning pins.

[0010] Furthermore, the injection molded part includes a metal wire arranged at one end of the injection molded part frame, and the rubber coating area includes a first rubber coating area for wrapping the metal wire and a second rubber coating area for wrapping the injection molded part frame; the second mold is a two-color mold, and the fixed mold of the two-color mold is provided with two independent cavities to correspond one to one to the first rubber coating area and the second rubber coating area.

[0011] The present invention provides a method for preparing an injection molded part logo, wherein the injection mold for preparing an injection molded part logo is used to prepare the injection molded part logo, the injection molded part comprises an injection molded part skeleton and a rubber-coated area that wraps the injection molded part skeleton, the injection molded part skeleton has a protruding logo skeleton, the logo skeleton has a closed sealing portion, and the sealing portion has a cavity opening outward, comprising the following steps: S1, inserting a movable mold core into an installation cavity of a movable mold of a first mold, and then locking the movable mold core; S2, closing the first mold, and extending a retractable reset rod arranged in the movable mold core out of a cavity wall of the movable mold core to ensure that a protruding distance of the reset rod protruding from the cavity wall of the movable mold core is less than a thickness of the sealing portion of the logo skeleton itself, and then performing hard glue injection molding to obtain an injection molded part having a first color. The mold skeleton is formed by inserting the reset rod toward one end of the mold skeleton into the closed part of the identification skeleton to form an insertion area, and the insertion area laterally penetrates the inner and outer surfaces of the cavity wall of the closed part; S3, the movable mold core carrying the mold skeleton is moved out after the first mold is opened, and then the movable mold core carrying the mold skeleton is inserted into the installation cavity of the movable mold of the second mold, and then the movable mold core is locked; S4, the second mold is closed, and the reset rod is retracted to ensure that the end of the reset rod toward the injection molded part skeleton is away from the insertion area, and a soft glue flow channel penetrating the cavity wall of the closed part is formed, and then the soft glue with a second color is injected and wrapped around the mold skeleton to ensure that the inner and side glue-wrapped areas of the identification skeleton are filled with the soft glue, thereby obtaining an injection molded part with an injection molded part identification.

[0012] Furthermore, the reset rod includes an insert pin and a reset spring sleeved on the insert pin; a limit plate is provided in the movable mold core to limit the extension distance of the insert pin so as to adjust the flow rate of the soft rubber flowing through the soft rubber flow channel; when the reset rod retracts and resets, one end of the reset rod away from the cavity of the movable mold core protrudes out of the bottom of the movable mold core, and the movable mold of the second mold is provided with a makeshift groove for making way for the protruding part of the reset rod to protrude from the bottom of the movable mold core, so as to ensure the retraction and reset of the reset rod.

[0013] Furthermore, the movable mold core is positioned and installed by positioning pins provided in the installation cavities of the movable molds of the first mold and the second mold respectively.

[0014] Furthermore, the injection molded part includes a metal wire arranged at one end of the injection molded part skeleton, and the rubber coating area includes a first rubber coating area for coating the metal wire and a second rubber coating area for coating the injection molded part skeleton; the second mold is a two-color mold, and the fixed mold of the two-color mold is provided with a first rubber coating cavity corresponding to the first rubber coating area and a second rubber coating cavity corresponding to the second rubber coating area; the movable mold core moved out of the first mold is first inserted into the first rubber coating cavity of the second mold, and then the second mold is closed to coat the metal wire and form the first rubber coating area, while ensuring the precise positioning of the metal wire during molding; then the second mold is opened, and the movable mold of the second mold with the movable mold core is rotated to align the movable mold core on the movable mold of the second mold with the second mold The second mold cavity, and then the second mold is closed again to coat the injection molded part skeleton with rubber and form the second rubber coating area.

[0015] The technical solution provided by the present invention has the following beneficial effects:

[0016] The reset rod is extended out of the cavity wall of the movable mold to ensure that when the injection molded part skeleton is injection molded, the reset rod extends into the closed part of the identification skeleton toward the end of the cavity of the movable mold to form an insertion area that laterally penetrates the inner and outer surfaces of the cavity wall of the closed part. Then, when the encapsulated area is injection molded, the reset rod is retracted to allow the reset rod to leave the insertion area toward the end of the cavity of the movable mold to form a soft glue flow channel that penetrates the cavity wall of the closed part. After the soft glue is injected, it can be ensured that the inner and side encapsulated areas of the identification skeleton are filled with soft glue, and the colors of the identification skeleton and the encapsulated areas are different from each other. In this way, the injection molded part logo can be processed through the injection molding process. Compared with the logo with a surface coating structure in the prior art, the injection molded part logo of the present invention has good scratch resistance and durability. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 The figure is a flow chart of the method for preparing the injection molded part mark in the first embodiment;

[0018] Figure 2 The figure shows the state of the moving mold core when the reset rod is lifted up in the first mold in the first embodiment;

[0019] Figure 3 Shown Figure 2 A magnified schematic diagram of area A in the middle;

[0020] Figure 4 The figure shows a cross-sectional view of the movable mold core when the reset rod is lifted up in the first mold in the first embodiment;

[0021] Figure 5 Shown Figure 4 A magnified schematic diagram of area B in the middle;

[0022] Figure 6 The figure shows the state of the moving mold core when the reset rod is retracted in the first mold in the first embodiment;

[0023] Figure 7 Shown Figure 6 Enlarged schematic diagram of area C in the middle;

[0024] Figure 8 The figure shows a schematic diagram of the soft glue flowing through the soft glue channel in the second mold in the first embodiment;

[0025] Fig. 9 The figure shows a partial appearance of the injection molded part in the first embodiment. DETAILED DESCRIPTION

[0026] To further illustrate the various embodiments, the present invention provides drawings. These drawings are part of the disclosure of the present invention, which are mainly used to illustrate the embodiments and can be used in conjunction with the relevant descriptions in the specification to explain the operating principles of the embodiments. With reference to these contents, a person of ordinary skill in the art should be able to understand other possible implementations and advantages of the present invention. The components in the figures are not drawn to scale, and similar component symbols are generally used to represent similar components.

[0027] The present invention will now be further described with reference to the accompanying drawings and specific implementation methods.

[0028] Embodiment 1

[0029] Reference Figure 1 As shown, embodiment 1 provides a method for preparing an injection molded part mark, and uses an injection mold to prepare an injection molded part mark, the injection molded part includes an injection molded part frame and a Fig. 9 The encapsulation area 4 shown, such as Figure 7 and Fig. 9 As shown, the injection molded part skeleton has a protruding identification skeleton 2, the identification skeleton 2 has a closed sealing portion, and the sealing portion has a cavity 21 open to the outside, and the injection molded part skeleton adopts hard glue such as PC material, and the rubber-coated area 4 adopts soft glue such as TPE material.

[0030] The injection mold includes a first mold and a second mold, and also includes a mold that matches the first mold and the second mold respectively. Figure 2 and Figure 4 The movable mold core 1 shown in the figure, the first mold is used to cooperate with the molding of the injection molded part frame, the second mold is used to cooperate with the soft glue to wrap the injection molded part frame to form the glue-encapsulated area 4, the side of the logo frame 2 facing outward exposes the glue-encapsulated area 4, and the colors of the logo frame 2 and the glue-encapsulated area 4 are set differently from each other to ensure that the injection molded part can be directly displayed after processing. Fig. 9 The native color of the molded part logo is shown.

[0031] The movable molds of the first mold and the second mold respectively have mounting cavities for cooperating with the movable mold core 1 for positioning. The movable mold core 1 is detachably disposed in the mounting cavities of the movable molds of the first mold and the second mold.

[0032] A retractable reset rod 11 is provided in the movable mold core 1, and the reset rod 11 corresponds to the closed portion. Specifically, Figure 4 The reset rod 11 shown includes an insert pin 111 and a reset spring 112 sleeved on the insert pin 111, and a limit plate is provided in the movable mold core 1 to limit the extension distance of the insert pin 111 so as to adjust the subsequent flow rate of the soft rubber flowing through the soft rubber flow channel 3, and the movable mold of the first mold is provided with a movable mold plate for resisting the reset rod 11 to ensure that the reset rod 11 is resisted by the movable mold plate of the first mold and abuts against the limit plate during injection molding in the first mold.

[0033] like Figures 2 to 7 As shown, when the molded part skeleton is injection molded in the first mold, the distance between the limiting plate and the abutting wall of the insert pin 111 is preset, and the insert pin 111 is pushed against the movable mold plate of the first mold until the abutting wall of the insert pin 111 abuts against the limiting plate to complete the limiting. At this time, the extension distance of the insert pin 111 extending from the cavity wall 12 of the movable mold core 1 is limited to a fixed value to ensure that the channel width of the soft glue flow channel 3 is large enough, thereby ensuring that the soft glue flow rate flowing through the soft glue flow channel 3 meets the injection molding requirements of the molded part skeleton. And the reset rod 11 extends out of the cavity wall 12 of the movable mold core 1, so that the insert pin 111 of the reset rod 11 extends into the closed part of the identification skeleton 2 toward the upper end of the cavity of the movable mold core 1, and forms an insertion area that laterally penetrates the inner and outer surfaces of the cavity wall of the closed part to prevent the hard glue from filling the insertion area.

[0034] like Figure 8 As shown, when the rubber-coated area 4 is injection molded in the second mold, the insert pin 111 of the reset rod 11 is retracted. At this time, the insert pin 111 of the reset rod 11 is away from the lower end of the cavity of the movable mold core 1 and protrudes out of the bottom of the movable mold core 1. The movable mold of the second mold is provided with a recess for the protruding part of the reset rod 11 protruding out of the bottom of the movable mold core 1, so as to ensure that the reset rod 11 is not pushed against by the movable mold of the second mold, and to achieve retraction and reset, thereby ensuring that the reset rod 11 leaves the insertion area toward the upper end of the cavity of the movable mold core 1, so as to form a soft rubber flow channel 3 that penetrates the cavity wall of the closed part, thereby ensuring that the rubber-coated area 4 on the inside and side of the logo skeleton 2 is filled with soft rubber, and the injection molded part logo is formed at the same time.

[0035] The method for preparing the injection molded part mark of this embodiment specifically comprises the following steps:

[0036] Step S1, insert the movable mold core 1 into the mounting cavity of the movable mold of the first mold, then lock the movable mold core 1, and set a positioning pin for guiding and positioning the movable mold core 1 in the mounting cavity of the movable mold of the first mold, and the movable mold core 1 is provided with a positioning groove matching the positioning pin, and the positioning pin and the positioning groove cooperate with each other to ensure that the movable mold core 1 is accurately installed in the mounting cavity of the movable mold of the first mold, and then the cylinder assembly is used to lock the movable mold core 1 in the mounting cavity of the movable mold of the first mold.

[0037] Step S2, close the first mold, and extend the reset rod 11 in the movable mold core 1 out of the cavity wall 12 of the movable mold core 1 to ensure that the protruding distance of the reset rod 11 from the cavity wall 12 of the movable mold core 1 is less than the thickness of the closed part of the identification skeleton 2 itself, such as the protruding distance of the reset rod 11 is 0.3mm, and then hard glue injection molding is performed from the fixed mold side of the first mold to obtain an injection molded part skeleton with a first color, and at this time, the reset rod 11 is inserted into the closed part of the identification skeleton 2 toward one end of the injection molded part skeleton to form an insertion area, and the insertion area laterally penetrates the inner and outer surfaces of the cavity wall of the closed part, and the height of the insertion area is equal to the protruding distance of the reset rod 11.

[0038] Step S3, the movable mold core 1 carrying the injection molded part skeleton is moved out after the first mold is opened, and then the movable mold core 1 carrying the injection molded part skeleton is inserted into the mounting cavity of the movable mold of the second mold, and then the movable mold core 1 is locked, and a positioning pin for guiding and positioning the movable mold core 1 is arranged in the mounting cavity of the movable mold of the second mold. The positioning pin and the positioning groove cooperate with each other to ensure that the movable mold core 1 is accurately installed in the mounting cavity of the movable mold of the second mold, and then the movable mold core 1 is locked in the mounting cavity of the movable mold of the second mold through the cylinder assembly.

[0039] Step S4, closing the second mold and retracting the reset rod 11 to ensure that the end of the reset rod 11 facing the injection molded part skeleton is away from the insertion area, and a soft glue flow channel 3 is formed that penetrates the cavity wall of the closed part. At this time, the channel height of the soft glue flow channel 3 is equal to the protruding distance of the reset rod 11, so that the channel height of the soft glue channel can be ensured to be large enough and the time required for subsequent soft glue injection molding can be short enough, thereby ensuring that the injection molded part logo will not have undesirable phenomena such as under-injection. After that, the soft glue having a second color is injected from the fixed mold side of the second mold and wrapped around the injection molded part skeleton to ensure that the inner and side glue-encapsulated areas 4 of the logo skeleton 2 are filled with soft glue, thereby obtaining a logo having the following characteristics: Fig. 9 The injection molded part shown is an injection molded part with an injection molded part logo.

[0040] like Figure 8As shown, by extending the reset rod 11 out of the cavity wall 12 of the movable mold core 1, it is ensured that when the injection molded part skeleton is injection molded, the reset rod 11 extends into the closed part of the identification skeleton 2 toward the end of the cavity of the movable mold core 1, and forms an insertion area that laterally penetrates the inner and outer surfaces of the cavity wall of the closed part. Then, when the encapsulated area 4 is injection molded, the reset rod 11 is retracted so that the reset rod 11 leaves the insertion area toward the end of the cavity of the movable mold core 1 to form a soft glue flow channel 3 that penetrates the cavity wall of the closed part, and after the soft glue is injected, it can be ensured that the inner and side encapsulated areas 4 of the identification skeleton 2 are filled with soft glue, and the colors of the identification skeleton 2 and the encapsulated areas 4 are different from each other. In this way, the injection molded part logo can be processed through the injection molding process. Compared with the logo with a surface coating structure in the prior art, the injection molded part logo of this embodiment has good scratch resistance and durability.

[0041] In addition, compared with the logo processed by pad printing or patch assembly methods in the prior art, the injection molded logo of this embodiment has the advantages of brighter appearance color, better wear resistance, better chemical corrosion resistance, better adhesion and more layered feeling.

[0042] Embodiment 2

[0043] Embodiment 2 provides a method for preparing an injection molded part logo. The method of Embodiment 2 is substantially the same as that of Embodiment 1, except that the injection molded part also includes a metal wire arranged at one end of the injection molded part skeleton, and the rubber coating area includes a first rubber coating area for wrapping the metal wire and a second rubber coating area for wrapping the injection molded part skeleton. For example, the injection molded part of this embodiment is a shell component of an ear-hook type headset.

[0044] The specific second mold is a two-color mold, the fixed mold of the two-color mold is provided with a first encapsulation cavity corresponding to the first encapsulation area and a second encapsulation cavity corresponding to the second encapsulation area, and the two-color mold is assembled on a two-color injection molding machine to complete two-color injection molding.

[0045] In this specific embodiment, the movable mold core moved out of the first mold is first inserted into the first encapsulation cavity of the second mold, and then the second mold is closed to encapsulate the metal wire and form a first encapsulation area, while ensuring precise positioning of the metal wire during molding.

[0046] Then the second mold is opened, and the movable mold of the second mold with the movable mold core is rotated 180 degrees to align the movable mold core on the movable mold of the second mold with the second overmolding cavity of the second mold. Then the second mold is closed to overmold the frame of the injection molded part and form a second overmolding area, and then a complete injection molded part is obtained.

[0047] By adopting the mobile mold core method, there will be no appearance problems such as burrs caused by gaps caused by the secondary placement of the injection molded product during the first mold molding, and manual processing of burrs can be avoided, which can reduce labor costs.

[0048] Compared with the prior art in which the molded part skeleton, the first rubber-coated area, and the second rubber-coated area each correspond to a single-color injection molding machine, this embodiment can effectively save the total number of injection molding machines, simplify the production process, and reduce the occupied area of ​​​​the production equipment. It can also improve the production yield and efficiency of injection molded parts. For example, the existing process requires 3 injection molding machines, while this embodiment only requires 2 injection molding machines, namely 1 single-color injection molding machine and 1 two-color injection molding machine.

[0049] Although the present invention has been specifically shown and described in conjunction with the preferred embodiments, it should be understood by those skilled in the art that various changes may be made to the present invention in form and details without departing from the spirit and scope of the present invention as defined by the appended claims, all of which are within the scope of protection of the present invention.

Claims

1. An injection mold for preparing an injection molded part logo, comprising a first mold and a second mold, characterized in that: It also includes a movable mold core respectively matched with the first mold and the second mold; The injection molded part comprises an injection molded part frame and a rubber-coated area wrapping the injection molded part frame, the injection molded part frame has a protruding identification frame, the identification frame has a closed sealing portion, the sealing portion has a cavity open to the outside, and the identification frame and the rubber-coated area are set to different colors from each other; The movable molds of the first mold and the second mold respectively have mounting cavities for cooperating with the movable mold core for positioning, and the movable mold core is detachably arranged in the mounting cavities of the movable molds of the first mold and the second mold; the first mold is used to cooperate in molding the injection molded part skeleton, and the second mold is used to cooperate in wrapping the injection molded part skeleton with soft glue to form the glue-wrapped area, and the outward side of the logo skeleton exposes the glue-wrapped area; A retractable reset rod is provided in the movable mold core, and the reset rod corresponds to the closing portion; When the molded part skeleton is injection molded in the first mold, the reset rod extends out of the cavity wall of the movable mold core, so that the reset rod extends into the closed portion of the logo skeleton toward the end of the cavity of the movable mold core and forms an insertion area, and the insertion area laterally penetrates the inner and outer surfaces of the cavity wall of the closed portion; When the rubber-coated area is injection molded in the second mold, the reset rod is retracted so that the reset rod leaves the insertion area toward the end of the cavity of the movable mold core to form a soft rubber flow channel that penetrates the cavity wall of the closed part, thereby ensuring that the inner and side rubber-coated areas of the logo skeleton are filled with soft rubber and forming the injection molded part logo at the same time.

2. The injection mold for preparing injection molded part marking according to claim 1, characterized in that: The reset rod includes an insert pin and a reset spring sleeved on the insert pin; a limit plate for limiting the extension distance of the insert pin is arranged in the movable mold core to adjust the flow rate of the soft rubber flowing through the soft rubber flow channel.

3. The injection mold for preparing injection molded part marking according to claim 2, characterized in that: The movable mold of the first mold is provided with a movable platen for abutting against the reset rod, so as to ensure that the reset rod is abutted by the movable platen and abuts against the limit plate during injection molding in the first mold.

4. The injection mold for preparing injection molded part marking according to any one of claims 1 to 3, characterized in that: When the reset rod retracts and resets, one end of the reset rod away from the cavity of the movable mold core protrudes out of the bottom of the movable mold core, and the movable mold of the second mold is provided with a makeshift groove for making way for the protruding part of the reset rod to protrude from the bottom of the movable mold core to ensure that the reset rod retracts and resets.

5. The injection mold for preparing injection molded part marking according to any one of claims 1 to 3, characterized in that: Positioning pins for guiding and positioning the movable mold core are arranged in the installation cavities of the movable molds of the first mold and the second mold, and the movable mold core is provided with positioning grooves matching the positioning pins.

6. The injection mold for preparing injection molded part marking according to any one of claims 1 to 3, characterized in that: The injection molded part includes a metal wire arranged at one end of the injection molded part frame, and the rubber coating area includes a first rubber coating area for coating the metal wire and a second rubber coating area for coating the injection molded part frame; the second mold is a two-color mold, and the fixed mold of the two-color mold is provided with two independent cavities to correspond one to one to the first rubber coating area and the second rubber coating area.

7. A method for preparing an injection molded part logo, comprising: using the injection mold for preparing an injection molded part logo according to any one of claims 1 to 6 to prepare an injection molded part logo, wherein the injection molded part comprises an injection molded part skeleton and a rubber-coated area that wraps the injection molded part skeleton, the injection molded part skeleton has a protruding logo skeleton, the logo skeleton has a closed closed portion, and the closed portion has a cavity that opens outward, characterized in that: The steps include: S1, inserting the movable mold core into the mounting cavity of the movable mold of the first mold, and then locking the movable mold core; S2, closing the first mold, and extending the retractable reset rod provided in the movable mold core out of the cavity wall of the movable mold core, so as to ensure that the protruding distance of the reset rod out of the cavity wall of the movable mold core is less than the thickness of the closed part of the logo skeleton itself, and then performing hard plastic injection molding to obtain an injection molded part skeleton with a first color, and at this time, the reset rod is inserted into the closed part of the logo skeleton toward one end of the injection molded part skeleton to form an insertion area, and the insertion area laterally penetrates the inner and outer surfaces of the cavity wall of the closed part; S3, moving the movable mold core carrying the molded part skeleton out after the first mold is opened, inserting the movable mold core carrying the molded part skeleton into the mounting cavity of the movable mold of the second mold, and then locking the movable mold core; S4, close the second mold and retract the reset rod to ensure that the end of the reset rod facing the injection molded part skeleton is away from the insertion area, and form a soft glue flow channel that penetrates the cavity wall of the closed part, and then inject and wrap the injection molded part skeleton with soft glue having a second color to ensure that the inner and side rubber-wrapped areas of the logo skeleton are filled with soft glue, thereby obtaining an injection molded part with an injection molded part logo.

8. The method for preparing an injection molded part mark according to claim 7, characterized in that: The reset rod includes an insert pin and a reset spring sleeved on the insert pin; a limit plate is provided in the movable mold core to limit the extension distance of the insert pin, so as to adjust the flow rate of soft rubber flowing through the soft rubber flow channel; when the reset rod retracts and resets, one end of the reset rod away from the cavity of the movable mold core protrudes from the bottom of the movable mold core, and the movable mold of the second mold is provided with a makeshift groove for making way for the protruding part of the reset rod to protrude from the bottom of the movable mold core, so as to ensure the retraction and reset of the reset rod.

9. The method for preparing an injection molded part mark according to claim 7, characterized in that: The movable mold core is positioned and installed by positioning pins arranged in the installation cavities of the movable molds of the first mold and the second mold respectively.

10. The method for preparing an injection molded part mark according to any one of claims 7 to 9, characterized in that: The injection molded part includes a metal wire arranged at one end of the injection molded part skeleton, and the rubber coating area includes a first rubber coating area for coating the metal wire and a second rubber coating area for coating the injection molded part skeleton; the second mold is a two-color mold, and the fixed mold of the two-color mold is provided with a first rubber coating cavity corresponding to the first rubber coating area and a second rubber coating cavity corresponding to the second rubber coating area; first, the movable mold core moved out of the first mold is inserted into the first rubber coating cavity of the second mold, and then the second mold is closed to coat the metal wire and form the first rubber coating area, while ensuring the precise positioning of the metal wire during molding; then the second mold is opened, and the movable mold of the second mold with the movable mold core is rotated to align the movable mold core on the movable mold of the second mold with the second rubber coating cavity of the second mold, and then the second mold is closed to coat the injection molded part skeleton and form the second rubber coating area.