Latent gate structure of double-layer battery insulation ring, injection mold and forming process
By adopting latent glue port structure and multi-point glue injection design in the injection mold of the double-layer battery insulating ring, the problems of water port material traces and dimensional defects in the existing technology are solved, sealing performance and production efficiency are improved, and battery leakage is reduced risk.
Patent Information
- Application Number
- CN202411095066.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-22
AI Technical Summary
In the injection molding technology of existing double-layer battery insulating rings, the direct-inlet rubber port structure causes molten plastic materials to easily appear when they enter the cavity, which affects the sealing performance and increases the risk of battery leakage.
Using latent rubber port structure and injection mold design, including the first rubber port and the second rubber port, the vertical latent section bypasses the upper large diameter section, so that the plastic material enters the cavity from the lower small diameter section and passes through multiple The dot-in glue and dual exhaust channel structure optimize the injection molding process to reduce gas residue and material flow resistance.
It effectively reduces the chance of battery leakage, improves sealing performance and product quality, achieves more uniform glue filling and dimensional accuracy, reduces the generation of bubbles, and improves overall production efficiency.
Smart Images

Figure CN118990942A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of product molding technology for double-layer battery insulating rings, and in particular to a latent gate structure, injection mold, and molding process for a double-layer battery insulating ring. Background Technology
[0002] After nearly 10 years of development, the market's requirements for the leakage resistance and safety of alkaline manganese batteries have reached a new level. The focus of technological improvement will shift to the research of high reliability technology for batteries. Sealing ring technology is a key technology in the research of high reliability technology for alkaline manganese batteries, and it is also the most difficult aspect of alkaline manganese battery technology.
[0003] The sealing ring not only determines the explosion-proof and leakage-proof performance of alkaline dry batteries, and is a key factor in solving battery explosion-proof and leakage-proof problems, but also has a significant impact on the internal space of the battery. Increasing the effective internal space of the battery to increase the filling amount of active materials in the positive and negative electrodes is a necessary means to improve the overall discharge capacity of the battery. Therefore, the research on optimizing the battery sealing ring structure and sealing ring materials is the main research direction of sealing ring technology.
[0004] Double-layer battery insulation rings possess superior structural performance and are currently one of the key components for improving battery reliability. Existing technology example 1, referring to patent document CN210040284U, discloses an alkaline dry cell battery sealing ring, including a sealing ring body with a central post in the middle. The central post has a central hole through which a current collector needle can pass, and glue storage grooves are provided at both ends of the central hole. This invention improves the structure of the alkaline dry cell battery sealing ring by providing glue storage grooves at the central hole. By providing glue storage grooves at both ends of the central hole, space is left between the current collector needle of the alkaline dry cell battery and the central hole for a sealing layer to be installed, thereby sealing both ends of the central hole and effectively improving the sealing performance of the sealing ring.
[0005] The molding technology of double-layer battery insulation ring is also particularly critical. Technical Example 2 (Patent Document CN201171060Y) states that "since the sealing ring is a rotating body, the mass distribution of the sealing ring is more uniform during injection molding." Therefore, most existing manufacturers achieve production through injection molds.
[0006] However, existing injection molding technologies for double-layer battery insulation rings all employ a straight-in gate structure. This allows molten plastic material to enter the mold cavity of the double-layer battery insulation ring from the upper, larger diameter section. Consequently, in the molded product, the sprue is located at the upper, larger diameter insulation section of the double-layer battery insulation ring. Even if the sprue is trimmed later, certain traces and dimensional defects will still remain at the upper, larger diameter insulation section. Since the upper, larger diameter insulation section is located on the outside and abuts against the inner wall of the battery's steel casing, requiring a sealing fit, the presence of sprue traces and dimensional defects makes the sealing function less stable, thus making the battery more prone to leakage. Summary of the Invention
[0007] To overcome the above-mentioned shortcomings of the prior art, the present invention provides a latent gate structure, injection mold and molding process for a double-layer battery insulating ring.
[0008] The technical solution of this invention to solve its technical problem is: a latent adhesive opening structure for a double-layer battery insulating ring, including a first adhesive opening, wherein the first adhesive opening comprises, in flow order:
[0009] The horizontal feeding section is connected and circumvents the first hot runner for glue injection.
[0010] The vertical concealment section has a high point and a low point, which are connected by an arc-shaped flow channel with a central angle of 90° and an inner diameter that gradually decreases from the high point to the low point.
[0011] The horizontal nozzle section is flared outwards from back to front in a funnel shape.
[0012] Furthermore, it also includes a second glue inlet, which is connected and communicates with the second glue inlet hot runner, and the second glue inlet has the same spatial structure as the first glue inlet;
[0013] The foremost end of the second nozzle has a short-pitch nozzle section, the length of which is less than the length of the horizontal nozzle section;
[0014] The first glue outlet is located inside the cavity, and the second glue outlet is located outside the cavity.
[0015] Another technical solution of the present invention is an injection mold for a double-layer battery insulating ring, comprising an upper mold assembly and a lower mold assembly capable of being closed and forming a cavity. The injection mold further comprises a latent nozzle structure for the double-layer battery insulating ring as described above. The cavity has an upper large-diameter section and a lower small-diameter section. The horizontal nozzle section and the short-distance nozzle section are aligned with and connected to the lower small-diameter section.
[0016] Preferably, the upper mold assembly has an upper glue inlet, which is connected to and communicates with the first glue inlet hot runner.
[0017] The first hot runner for glue injection has a straight main flow channel section and several first branch sections connected to the straight main flow channel section, and each first branch section is connected to one of the first glue inlets.
[0018] Another preferred structure is that the upper mold assembly has a side inlet, which is connected to and communicates with the second hot runner.
[0019] The second hot runner has a racetrack-shaped main runner section and several second branch sections connected to the racetrack-shaped main runner section. Each second branch section is connected to two adjacent second glue inlets.
[0020] In some preferred embodiments of the present invention, the cavity is provided with a horizontally arranged first exhaust channel, the first exhaust channel is located at the edge of the cavity, the first exhaust channel is also connected to a pressure holding pipe, the pressure holding pipe is connected to an external air source, and a pressure relief valve assembly is provided at the junction of the first exhaust channel and the pressure holding pipe.
[0021] Specifically, the pressure relief valve assembly includes a valve body, a rod sleeve formed in the valve body, a movable shaft passing through the rod sleeve, and a seal connected to one end of the movable shaft;
[0022] The valve body has a first connection port and a second connection port. The first connection port is connected to and in communication with a first exhaust channel, and the second connection port is connected to a pressure-holding pipe, and the pressure-holding pipe is in communication with the rod sleeve.
[0023] The valve body has a vent near the first connection port, and the sealing element can block or release the vent.
[0024] In some preferred embodiments of the present invention, the lower mold assembly has a rod-shaped core, the rod-shaped core including a core sleeve and a plurality of interchangeable core rods, and the core rods and the core sleeve are detachably connected.
[0025] Each core rod has a contoured end of a different shape, which extends out of the core sleeve and into the cavity.
[0026] More specifically, the core rod has a through-hole and vertically arranged second exhaust channel, the upper end of the second exhaust channel is an air inlet, the lower end of the second exhaust channel is an air outlet, and the air inlet has a constriction structure and the air outlet has an expansion structure.
[0027] The second exhaust channel is provided with a support part, and a spring is provided on the support part. The upper end of the spring abuts against a sealing ball. The diameter of the sealing ball is smaller than the diameter of the second exhaust channel, and the diameter of the sealing ball is larger than the diameter of the air inlet.
[0028] The spring force acts on the sealing ball, and when the internal pressure of the cavity is less than the spring force, the spring force drives the sealing ball to move upward and block the air inlet.
[0029] When the internal pressure of the cavity is greater than the elastic force of the spring, the internal pressure drives the sealing ball to move downward, so that the sealing ball separates from the air inlet, so that the internal gas enters the second exhaust channel through the air inlet and is discharged from the air outlet.
[0030] Another technical solution of the present invention is a molding process for a double-layer battery insulating ring, which uses the injection mold for the double-layer battery insulating ring as described above, and the process steps are as follows:
[0031] S1. Based on the model of the double-layer battery insulation ring to be formed, select a core rod that is compatible with the double-layer battery insulation ring, and assemble the selected core rod and core sleeve to form the required rod-shaped core.
[0032] S2. The upper mold assembly and the lower mold assembly are joined together to form a cavity that is compatible with the double-layer battery insulation ring to be formed, and the contoured end of the rod-shaped core extends into the cavity.
[0033] S3. Glue is fed from the top inlet. The molten plastic material flows along the first hot runner to each first inlet. Then, the molten plastic material passes through the horizontal feeding section, the vertical submerged section and the horizontal nozzle section and enters the lower small diameter section of the cavity. As the amount of glue fed increases, the molten plastic material fills the entire cavity.
[0034] S4. Second sprue injection: The molten plastic material flows along the second sprue hot runner to each second sprue, and then is injected into the lower small diameter section of the cavity through the short-pitch nozzle section. As the injection volume increases, the molten plastic material fills the entire cavity.
[0035] S5. During the injection molding process, when the molten plastic material enters the cavity, it compresses the gas in the cavity so that a part of the gas is discharged from the first lateral venting channel and the other part is discharged from the second vertical venting channel.
[0036] S6. Wait for the injection mold to cool down;
[0037] S7. After curing and molding, the upper mold assembly and the lower mold assembly are separated, and the molded double-layer battery insulation ring is taken out. At this time, multiple double-layer battery insulation rings are connected into one piece through the sprue material.
[0038] S8. The formed double-layer battery insulation ring has an upper large-diameter insulation section and a lower small-diameter insulation section. The sprue material on the lower small-diameter insulation section is trimmed off to obtain multiple independent double-layer battery insulation rings.
[0039] The beneficial effects of this invention are as follows:
[0040] 1. Featuring a concealed gate structure, the vertical concealed section in the first gate allows it to bypass the upper large-diameter section of the cavity, enabling molten plastic material to enter the mold cavity of the double-layer battery insulation ring from the lower small-diameter section. Consequently, the sprue material is located at the lower small-diameter insulating section of the double-layer battery insulation ring. Although there may be traces and dimensional defects on the lower small-diameter insulating section, it is located on the inside and does not contact the inner wall of the battery steel casing, thus not affecting the sealing performance and greatly reducing the probability of battery leakage.
[0041] 2. The vertical latent section has a high point and a low point. The central angle of the arc-shaped flow channel between the high point and the low point is 90°. The high point is for glue entry and the low point is for glue exit. This allows the vertical glue entry position to be adjusted so that the molten plastic material enters the cavity of the injection mold of the double-layer battery insulation ring from the lower small diameter section.
[0042] Third, the first gate serves as the main gate and the second gate serves as the secondary gate, forming a circumferential multi-point gate structure around the cavity. Multi-point gates result in better product quality, more uniform filling, reduced flow resistance and stress concentration of material within the mold, and improved product quality and dimensional accuracy.
[0043] Fourth, it features a straight main runner section, a cavity, and a racetrack-shaped main runner section distributed sequentially from the inside to the outside to achieve multi-point feeding. The structure is more reasonable and compact, and the runner is more direct without bending, making the entire injection mold smaller in size.
[0044] Fifth, a dual-exhaust channel structure is adopted. The first exhaust channel can promptly discharge high-pressure gas at the edge of the cavity horizontally, while the second exhaust channel can promptly discharge high-pressure gas inside the cavity vertically. The combination of the two exhaust channels enables faster and more efficient discharge of gas from all parts of the cavity, and the gas can be discharged from the nearest point, greatly reducing exhaust time and minimizing impact on the molten plastic material inside, reducing the chance of air bubbles in the product, and effectively improving product quality. Attached Figure Description
[0045] Figure 1 This is a schematic diagram of the structure of the double-layer battery insulation ring in this invention.
[0046] Figure 2 This is a schematic diagram of the structure of a double-layer battery insulation ring in the prior art.
[0047] Figure 3 This is a schematic diagram of the structure of the cavity and the first glue outlet in this invention.
[0048] Figure 4 This is a schematic diagram of the injection mold in this invention.
[0049] Figure 5 This is a cross-sectional view of the injection mold in this invention.
[0050] Figure 6 This is a partial structural schematic diagram of the injection mold in this invention.
[0051] Figure 7 This is a schematic diagram of the first and second inlet hot runners.
[0052] Figure 8 yes Figure 7 An enlarged schematic diagram of part A in the middle.
[0053] Figure 9 This is a cross-sectional view of a rod-shaped core.
[0054] Figure 10 This is a schematic diagram comparing the rod-shaped core in a sealed state and a vented state.
[0055] Figure 11 This is a comparative diagram of various specifications of contoured ends.
[0056] Figure 12 This is a schematic diagram comparing the pressure relief valve assembly in the sealed state and the venting state.
[0057] In the diagram: 1. Latent gate structure; 11. First gate; 111. Horizontal feed section; 112. Vertical latent section; 1121. High point; 1122. Low point; 1123. Arc-shaped runner; 113. Horizontal nozzle section; 12. Second gate; 2. Double-layer battery insulation ring; 21. Upper large-diameter insulation section; 22. Lower small-diameter insulation section; 23. Sprue material; 24. Inner hole; 3. Injection mold; 31. Upper mold assembly; 311. Upper gate; 312. First hot runner; 3121. Straight main runner section; 3122. First branch section; 313. Side gate; 314. Second hot runner; 3141. Racetrack-shaped main runner section; 3142. Second branch section; 32, lower mold assembly; 321, rod-shaped core; 3211, core sleeve; 3212, core rod; 3212a, contoured end; 33, cavity; 331, upper large-diameter section; 332, lower small-diameter section; 34, first exhaust channel; 341, pressure-holding pipe; 342, external air source; 343, pressure relief valve assembly; 3431, valve body; 3431a, first connection port; 3431b, second connection port; 3432, rod sleeve; 3433, movable shaft; 3434, seal; 3435, vent; 35, second exhaust channel; 351, air inlet; 352, air outlet; 353, support; 354, spring; 355, sealing ball; 356, gap. Detailed Implementation
[0058] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0059] Example 1
[0060] Reference Figures 1-12 The latent nozzle structure 1 of the double-layer battery insulation ring 2 includes a first nozzle 11, which, in the flow sequence, includes: a horizontal feed section 111, which is connected and conductive to the first hot runner 312; a vertical latent section 112, which has a high point 1121 and a low point 1122, which are connected by an arc-shaped flow channel 1123, the central angle of which is 90°, and the inner diameter of which gradually decreases from the high point 1121 to the low point 1122; and a horizontal nozzle section 113, which is flared outward from back to front. The flared structure allows for greater pressure in the initial spray section, a wider spray area, and effectively prevents clogging.
[0061] Reference Figure 2 In existing injection molding technologies for double-layer battery insulation rings 2, a straight-in gate structure is used. This allows molten plastic material to enter the cavity 33 of the injection mold 3 of the double-layer battery insulation ring 2 from the upper large-diameter section 331. As a result, in the molded product, the sprue 23 is located at the upper large-diameter insulation section 21 of the double-layer battery insulation ring 2. Even if the sprue 23 is trimmed later, certain traces and dimensional defects will still exist at the upper large-diameter insulation section 21. Since the upper large-diameter insulation section 21 is located on the outside and abuts against the inner wall of the battery steel shell, requiring a sealing fit, the presence of traces and dimensional defects in the sprue 23 makes the sealing function less stable, thus making the battery more prone to leakage.
[0062] Reference Figure 1 , Figure 3 Through the vertically recessed section 112 in the first sprue 11, the molten plastic material can bypass the upper large-diameter section 331 of the cavity 33, allowing it to enter the cavity 33 of the injection mold 3 for the double-layer battery insulation ring 2 from the lower small-diameter section 332. Consequently, the sprue 23 is located at the lower small-diameter insulation section 22 of the double-layer battery insulation ring 2. Although there are traces and dimensional defects on the lower small-diameter insulation section 22, it is located on the inside and does not contact the inner wall of the battery steel shell, thus not affecting the sealing performance and greatly reducing the probability of battery leakage.
[0063] On the other hand, it is particularly important to emphasize that the typical submerged injection gate, also known as a horn-shaped injection gate, has a central angle of 180 degrees in its curved section. Therefore, it cannot change the vertical injection position. When applied to a double-layer insulating battery ring, the injection position remains the upper large-diameter section 331 of the cavity 33. In the solution of this invention, the vertical submerged section 112 has a high point 1121 and a low point 1122. The central angle of the arc-shaped flow channel 1123 between the high point 1121 and the low point 1122 is 90°. Glue enters at the high point 1121 and exits at the low point 1122, thereby allowing adjustment of the vertical injection position so that the molten plastic material enters the cavity 33 of the injection mold 3 of the double-layer battery insulating ring 2 from the lower small-diameter section 332.
[0064] Preferably, the system further includes a second nozzle 12, which is connected and conductive to the second hot runner channel 314, and has the same spatial structure as the first nozzle 11. The front end of the second nozzle 12 has a short-pitch nozzle section, which, simply put, means that the length of the short-pitch nozzle section is less than the length of the horizontal nozzle section 113. The first nozzle 11 is located inside the cavity 33, and the second nozzle 12 is located outside the cavity 33. The glue injection method of the second nozzle 12 is similar to that of the first nozzle 11, and will not be described in detail here.
[0065] It is worth mentioning that, referring to Figures 1-3 The double-layer battery insulation ring 2 has a double-layer annular structure. In this invention, the first injection port 11 is used as the main injection point, and the second injection port 12 is used as the secondary injection port, forming a circumferential multi-point injection structure around the cavity 33. Compared with a single injection port, the advantages are at least as follows: First, the product quality is better, and more uniform injection filling can be achieved, reducing the flow resistance and stress concentration of the material in the mold, and improving the product's quality and dimensional accuracy. Second, multiple injection ports can inject material simultaneously or in batches, improving filling speed and efficiency. Third, multi-point injection can prevent local flow obstruction and material accumulation, making the overall flow more uniform, the venting smoother, and the internal pressure more stable. Fourth, the filling is more flexible. In production, the flow rate and pressure of different injection ports can be adjusted as needed to adapt to the production requirements of different product specifications.
[0066] Example 2
[0067] In this embodiment, refer to Figures 4-8 An injection mold 3 for a double-layer battery insulating ring 2 is provided, including an upper mold assembly 31 and a lower mold assembly 32 that can be closed to form a cavity 33. The injection mold 3 also includes the aforementioned latent nozzle structure 1 for the double-layer battery insulating ring 2. The cavity 33 has an upper large-diameter section 331 and a lower small-diameter section 332. The horizontal nozzle section 113 and the short-pitch nozzle section are aligned with and connected to the lower small-diameter section 332.
[0068] The upper mold assembly 31 has an upper glue inlet 311, which is connected to and communicates with the first glue inlet hot runner 312. The first glue inlet hot runner 312 has a straight main runner section 3121 and several first branch sections 3122 connected to the straight main runner section 3121. Each first branch section 3122 is connected to one of the first glue inlets 11. By setting multiple first branch sections 3122, multiple double-layer battery insulating rings 2 can be formed simultaneously.
[0069] On the other hand, the upper mold assembly 31 has a lateral glue inlet 313, which is connected to and communicates with the second glue inlet hot runner 314. The second glue inlet hot runner 314 has a racetrack-shaped main runner section 3141 and several second branch sections 3142 connected to the racetrack-shaped main runner section 3141. Each second branch section 3142 is connected to two adjacent second glue inlets 12. By setting multiple second branch sections 3142, multiple double-layer battery insulating rings 2 can be formed simultaneously.
[0070] It is worth mentioning that, referring to Figure 8 The straight main runner section 3121, cavity 33, and racetrack-shaped main runner section 3141 are distributed from the inside to the outside to achieve multi-point feeding. The structure is more reasonable and compact, and the runner is more direct without bending, so that the entire injection mold 3 is smaller in size.
[0071] Different models of double-layer battery insulation rings 2 have certain differences in internal structural details. Conventional technology requires the creation of corresponding injection molds 3, which leads to several drawbacks: firstly, increased mold manufacturing costs; secondly, the need to switch between different molds during processing, wasting significant time and reducing work efficiency; and thirdly, repeated disassembly and assembly greatly reduces production precision and product quality. To overcome these shortcomings, the preferred structural solution adopted is as follows: (Refer to...) Figures 9-10 The lower mold assembly 32 includes a rod-shaped core 321, which is a variable structure. Specifically, the rod-shaped core 321 includes a core sleeve 3211 and several interchangeable core rods 3212, and the core rods 3212 and the core sleeve 3211 are detachably connected; see reference. Figures 4 to 11 Each core rod 3212 has a contoured end 3212a of a different shape, which extends out of the core sleeve 3211 and into the cavity 33. For example, when the product of the double battery insulation ring needs to form an inner hole 24 with a diameter of 2mm, a core rod 3212 with a contoured end 3212a of 2mm diameter is used to cooperate with the core sleeve 3211; when the product of the double battery insulation ring needs to form an inner hole 24 with a diameter of 3mm, a core rod 3212 with a contoured end 3212a of 3mm diameter is used to cooperate with the core sleeve 3211. Alternatively, when a circular hole needs to be formed inside the product of the double battery insulation ring, a core rod 3212 with a cylindrical contoured end 3212a is used to cooperate with the core sleeve 3211; when a rectangular hole needs to be formed inside the product of the double battery insulation ring, a core rod 3212 with a quadrangular prism contoured end 3212a is used to cooperate with the core sleeve 3211.
[0072] The injection mold 3 of the present invention employs a dual venting channel structure, with the following design:
[0073] I. Adjustable exhaust structure: Refer to / 7. Figure 12 The cavity 33 is provided with a horizontally arranged first exhaust channel 34, which is located at the edge of the cavity 33. The first exhaust channel 34 is also connected to a pressure-holding pipe 341, which is connected to an external air source 342. A pressure relief valve assembly 343 is provided at the junction of the first exhaust channel 34 and the pressure-holding pipe 341. The external air source 342 is used to regulate and control the air pressure in the pressure-holding pipe 341.
[0074] The pressure relief valve assembly 343 includes a valve body 3431, a rod sleeve 3432 formed in the valve body 3431, a movable shaft 3433 passing through the rod sleeve 3432, and a sealing element 3434 connected to one end of the movable shaft 3433. The valve body 3431 has a first connection port 3431a and a second connection port 3431b. The first connection port 3431a is connected to and communicates with a first exhaust channel 34, and the second connection port 3431b is connected to a pressure holding pipe 341, and the pressure holding pipe 341 communicates with the rod sleeve 3432. The valve body 3431 has a vent 3435 near the first connection port 3431a, and the sealing element 3434 can block or release the vent 3435.
[0075] An example of how the pressure relief valve assembly 343 is used is as follows: If the pressure in the pressure-holding pipe 341 (second connection port 3431b) is set to 1.5 MPa, then when the pressure at the first exhaust channel 34 (first connection port 3431a) is greater than 1.5 MPa, the seal 3434 moves outward and separates from the vent 3435, allowing the pressure inside the cavity 33 to be discharged outward through the vent 3435. Once the pressure at the first exhaust channel 34 (first connection port 3431a) is equal to or less than 1.5 MPa, the seal 3434 moves inward and blocks the vent 3435, thus ensuring a relatively stable pressure and working environment inside the cavity 33. Specific critical pressure values can be set according to actual needs and are not specifically limited here.
[0076] It should be noted that when using a multi-cavity mold, multiple products can be molded in one injection molding. Multiple cavity units 33 are interconnected to form a complete cavity 33. Under pressure, the cavity unit 33 in the middle position first squeezes the gas into the cavity units 33 on the side, and then the gas is discharged from the cavity units 33 on the side to the first exhaust channel 34.
[0077] II. Fixed Pressure Exhaust Structure: Refer to Figures 9-10The core rod 3212 has a through-hole and vertically arranged second exhaust channel 35. The upper end of the second exhaust channel 35 is an air inlet 351, and the lower end of the second exhaust channel 35 is an air outlet 352. The air inlet 351 has a constricted structure, and the air outlet 352 has an flared structure. A support part 353 is provided in the second exhaust channel 35, and a spring 354 is provided on the support part 353. The upper end of the spring 354 abuts against a sealing ball 355. The diameter of the sealing ball 355 is smaller than the diameter of the second exhaust channel 35, so that when the sealing ball 355 is pushed open, a gap 356 is formed between the sealing ball 355 and the second exhaust channel 35, allowing gas to pass through. On the other hand, the diameter of the sealing ball 355 is larger than the diameter of the air inlet 351, and with the help of the constricted structure, the sealing ball 355 can successfully block the air inlet 351. The working principle of the fixed pressure exhaust structure is as follows: the elastic force of the spring 354 acts on the sealing ball 355, and when the internal pressure of the cavity 33 is less than the elastic force of the spring 354, the elastic force of the spring 354 drives the sealing ball 355 to move upward and block the air inlet 351; when the internal pressure of the cavity 33 is greater than the elastic force of the spring 354, the internal pressure drives the sealing ball 355 to move downward, so that the sealing ball 355 separates from the air inlet 351, so that the internal gas enters the second exhaust channel 35 through the air inlet 351 and is discharged from the air outlet 352.
[0078] It should be noted that, unlike the first exhaust channel 34, once the parameters of the spring 354 (such as wire diameter, length, etc.) are selected, the elastic force of the spring 354 will be fixed and cannot be changed during use.
[0079] During the injection molding process, the first venting channel 34 can promptly discharge high-pressure gas at the edge of the cavity 33 horizontally, while the second venting channel 35 can promptly discharge high-pressure gas within the cavity 33 vertically. The combination of these two venting channels allows for faster and more efficient gas discharge from all parts of the cavity 33, with gas being discharged from nearby locations, significantly reducing venting time and minimizing impact on the molten plastic material. This reduces the likelihood of air bubbles forming in the product and effectively improves product quality.
[0080] Example 3
[0081] A molding process for a double-layer battery insulation ring 2, using the injection mold 3 for the double-layer battery insulation ring 2 as described in claim 9, with reference to... Figures 1-12 The process steps are as follows:
[0082] S1. Based on the model of the double-layer battery insulation ring 2 to be formed, where different models of double-layer battery insulation ring 2 have certain differences in structure (e.g., the shape or size of the inner hole 24), select a core rod 3212 (with a contoured end 3212a that is adapted to the inner hole 24 and used to form the inner hole 24) that is compatible with the double-layer battery insulation ring 2. Assemble the selected core rod 3212 and the core sleeve 3211 to form the required rod-shaped core 321, and assemble the rod-shaped core 321 in the injection mold 3.
[0083] S2. The upper mold assembly 31 and the lower mold assembly 32 are closed to form a cavity 33 that is compatible with the double-layer battery insulation ring 2 to be formed. The contoured end 3212a of the rod-shaped core 321 extends into the cavity 33. The cavity 33 is preferably a multi-cavity mold, for example, it can produce 24 products, 48 products, or 96 products in one mold to improve production efficiency.
[0084] S3, the molten plastic material enters through the upper inlet 311. The molten plastic material flows along the first hot runner 312 to each first inlet 11. Then, the molten plastic material enters the lower small diameter section 332 of the cavity 33 through the horizontal feeding section 111, the vertical submerged section 112 and the horizontal nozzle section 113. As the amount of molten plastic increases, the molten plastic material fills the entire cavity 33.
[0085] Before injecting the glue in step S3, it is preferable to preheat the injection mold 3 to achieve the ideal working temperature;
[0086] S4. The molten plastic material enters through the second injection port 12. It flows along the second injection hot runner 314 to each of the second injection ports 12, and then is injected into the lower small diameter section 332 of the cavity 33 through the short-pitch nozzle section. As the amount of molten plastic increases, the molten plastic material fills the entire cavity 33.
[0087] It is worth mentioning that two injection gates (first gate 11 and second gate 12, with no specific limit on the number of each type of gate) can form a multi-point injection structure. There are various ways to use these two gates to achieve different injection molding effects. For example:
[0088] Method 1: Simultaneous glue feeding through two glue inlets (using the same plastic material) can greatly improve glue feeding efficiency and make glue feeding more uniform and comprehensive, preventing local glue shortages, missing glue, air bubbles, etc., which is conducive to improving product yield and quality.
[0089] Method 2: Simultaneous injection of plastic into two nozzles (using different plastic materials). Since different molten plastic materials have different material properties, such as different melting points and injection temperatures, by setting the first nozzle 11 and the second nozzle 12, different molten plastic materials can be injected and filled into the cavity 33 at the same time to form the desired product.
[0090] Method 3: Staggered injection of two injection points (using the same plastic material). Based on process requirements and material characteristics, the multi-point injection structure allows the same molten plastic material to be injected into the cavity 33 at staggered times to form the desired product.
[0091] Method 4: Staggered injection of two injection points (different plastic materials can be selected). According to process requirements and material characteristics, the multi-point injection structure can inject different molten plastic materials into the cavity 33 at different times to simulate the effect of two-color injection molding without mold change, so as to mold the required product.
[0092] S5. During injection molding, when the molten plastic material enters the cavity 33, it compresses the gas in the cavity 33, causing some gas to be discharged from the lateral first venting channel 34 and the other part from the vertical second venting channel 35. The arrangement of the first venting channel 34 and the second venting channel 35 forms a multi-channel, multi-directional (horizontal and vertical) venting structure, which effectively improves venting efficiency; eliminates the defects of incomplete venting, unidirectional venting, and easy bubble generation inherent in single-channel venting structures; improves cooling efficiency, helping the mold cool faster, thereby increasing production efficiency; and ensures effective venting prevents bubbles, shrinkage, or surface defects caused by air remaining inside the plastic part. Multiple venting channels help to evenly remove residual air, making the plastic part denser and with higher surface quality.
[0093] S6. Wait for the injection mold 3 to cool down. Cooling is achieved through water-cooling channels set in the upper mold assembly 31 and the lower mold assembly 32. Its working principle is similar to existing mold technology, and will not be described in detail here.
[0094] S7. After curing and molding, the upper mold assembly 31 and the lower mold assembly 32 are separated, and the molded double-layer battery insulating ring 2 is taken out. Due to the use of a multi-cavity mold structure, multiple double-layer battery insulating rings 2 are connected into one piece by the sprue material 23.
[0095] S8. The molded double-layer battery insulation ring 2 has an upper large-diameter insulation section 21 and a lower small-diameter insulation section 22. The sprue material 23 on the lower small-diameter insulation section 22 is trimmed off to obtain multiple independent double-layer battery insulation rings 2. It is worth mentioning that, with the help of the mold structure and injection molding process of the present invention, the upper large-diameter insulation section 21 in the double-layer battery insulation ring 2 can be guaranteed to have a complete and smooth outer wall. Although the sprue material 23 is located at the lower small-diameter insulation section 22 of the double-layer battery insulation ring 2, resulting in traces and dimensional defects on the lower small-diameter insulation section 22, the lower small-diameter insulation section 22 is located on the inside and does not abut against the inner wall of the battery steel shell. Therefore, it will not affect the sealing performance of the double-layer battery insulation ring 2, greatly reducing the probability of battery leakage.
[0096] The above description is merely a preferred embodiment of the present invention and does not constitute any limitation on the present invention. Any simple modifications, alterations, or equivalent structural changes made to the above embodiments based on the technical essence of the invention shall still fall within the protection scope of the present invention.
[0097] The above description is merely a preferred embodiment of the present invention and does not constitute any limitation on the present invention. Any simple modifications, alterations, or equivalent structural changes made to the above embodiments based on the technical essence of the invention shall still fall within the protection scope of the present invention.
Claims
1. The latent glue port structure of the double-layer battery insulation ring is characterized by: It comprises a first glue port (11), and the first glue port (11) comprises, in order of flow: A horizontal feeding section (111), which is connected to and in conduction with the first hot runner for glue feeding (312); A vertical latent section (112) having a high point (1121) and a low point (1122), wherein the high point (1121) and the low point (1122) are connected via an arc-shaped flow channel (1123), wherein the central angle of the arc-shaped flow channel (1123) is 90°, and the inner diameter of the arc-shaped flow channel (1123) gradually decreases from the high point (1121) to the low point (1122); The horizontal nozzle section (113) is in a trumpet shape expanding from the back to the front.
2. The latent glue port structure of the double-layer battery insulation ring according to claim 1 is characterized in that: It also includes a second glue port (12), the second glue port (12) is connected to and communicates with a second glue inlet hot runner (314), and the second glue port (12) has the same spatial structure as the first glue port (11); The front end of the second glue port (12) has a short-distance glue nozzle section, and the length of the short-distance glue nozzle section is less than the length of the horizontal glue nozzle section (113); The first glue opening (11) is distributed on the inner side of the mold cavity (33), and the second glue opening (12) is distributed on the outer side of the mold cavity (33).
3. An injection mold for a double-layer battery insulating ring, comprising an upper mold assembly (31) and a lower mold assembly (32) that can be relatively closed to form a mold cavity (33), characterized in that: The injection mold (3) also includes a latent glue nozzle structure (1) of the double-layer battery insulation ring (2) as described in claim 2, the cavity (33) has an upper large-diameter section (331) and a lower small-diameter section (332), and the horizontal glue nozzle section (113) and the short-distance glue nozzle section are both aligned with and connected to the lower small-diameter section (332).
4. The injection mold for the double-layer battery insulation ring according to claim 3, characterized in that: The upper mold assembly (31) has an upper glue inlet (311), and the upper glue inlet (311) is connected to and communicated with the first glue inlet hot runner (312); The first glue inlet hot runner (312) comprises a straight main runner section (3121) and a plurality of first branch sections (3122) connected to the straight main runner section (3121), and each first branch section (3122) is correspondingly connected to one of the first glue ports (11).
5. The injection mold for the double-layer battery insulation ring according to claim 4, characterized in that: The upper mold assembly (31) has a lateral glue inlet (313), and the lateral glue inlet (313) is connected to and communicated with the second glue inlet hot runner (314); The second glue inlet hot runner (314) comprises a racetrack-shaped main runner section (3141) and a plurality of second branch sections (3142) connected to the racetrack-shaped main runner section (3141), and each second branch section (3142) is correspondingly connected to two adjacent second glue ports (12).
6. The injection mold for the double-layer battery insulation ring according to claim 5, characterized in that: A first exhaust channel (34) arranged horizontally is provided in the mold cavity (33). The first exhaust channel (34) is arranged at the edge of the mold cavity (33). The first exhaust channel (34) is also connected to a pressure-maintaining pipeline (341). The pressure-maintaining pipeline (341) is connected to an external air source (342), and a pressure relief valve assembly (343) is provided at the joint between the first exhaust channel (34) and the pressure-maintaining pipeline (341).
7. The injection mold for the double-layer battery insulation ring according to claim 6, characterized in that: The pressure relief valve assembly (343) comprises a valve body (3431), a rod sleeve (3432) disposed in the valve body (3431), a movable shaft (3433) passing through the rod sleeve (3432), and a sealing member (3434) connected to one end of the movable shaft (3433); The valve body (3431) has a first connection port (3431a) and a second connection port (3431b), the first connection port (3431a) is connected to and communicates with the first exhaust channel (34), the second connection port (3431b) is connected to the pressure-maintaining pipe (341), and the pressure-maintaining pipe (341) is communicated with the rod sleeve (3432); The valve body (3431) is provided with a vent (3435) near the first connection port (3431a), and the sealing member (3434) can block or release the vent (3435).
8. The injection mold for the double-layer battery insulation ring according to claim 7, characterized in that: The lower mold assembly (32) has a rod-shaped core (321), and the rod-shaped core (321) includes a core sleeve (3211) and a plurality of core rods (3212) that can be replaced with each other, and the core rod (3212) and the core sleeve (3211) are detachably connected. Each core rod (3212) has a contoured end portion (3212a) of different shapes, and the contoured end portion (3212a) extends out of the core sleeve (3211) and extends into the mold cavity (33).
9. The injection mold for the double-layer battery insulation ring according to claim 8, characterized in that: The core rod (3212) has a second exhaust channel (35) that is through and vertically arranged, the upper end of the second exhaust channel (35) is an air inlet (351), the lower end of the second exhaust channel (35) is an air outlet (352), and the air inlet (351) has a contracting structure, and the air outlet (352) has an expanding structure; The second exhaust channel (35) is provided with a support portion (353), the support portion (353) is provided with a spring (354), the upper end of the spring (354) is in contact with a sealing ball (355), the diameter of the sealing ball (355) is smaller than the diameter of the second exhaust channel (35), and the diameter of the sealing ball (355) is larger than the diameter of the air inlet (351); The elastic force of the spring (354) acts on the sealing ball (355), and when the internal pressure of the cavity (33) is less than the elastic force of the spring (354), the elastic force of the spring (354) drives the sealing ball (355) to move upward and block the air inlet (351); When the internal pressure of the cavity (33) is greater than the elastic force of the spring (354), the internal pressure drives the sealing ball (355) to move downward, so that the sealing ball (355) is separated from the air inlet (351), so that the internal gas enters the second exhaust channel (35) through the air inlet (351) and is discharged from the air outlet (352).
10. A forming process for a double-layer battery insulating ring, characterized in that: The injection mold of the double-layer battery insulation ring as claimed in claim 9 is used, and the process steps are as follows: S1. According to the model of the double-layer battery insulating ring (2) to be formed, a core rod (3212) that is compatible with the double-layer battery insulating ring (2) is selected, and the selected core rod (3212) and the core sleeve (3211) are assembled to form the required rod-shaped core (321); S2, the upper mold assembly (31) and the lower mold assembly (32) are combined to form a mold cavity (33) that is compatible with the double-layer battery insulation ring (2) to be formed, and the contoured end portion (3212a) in the rod-shaped core (321) extends into the mold cavity (33); S3, glue is fed from the upper glue inlet (311), and the molten plastic material flows along the first glue feeding hot runner (312) to each first glue inlet (11), and then the molten plastic material successively passes through the horizontal feeding section (111), the vertical latent section (112) and the horizontal glue nozzle section (113) and enters the lower small diameter section (332) of the cavity (33). As the amount of glue fed increases, the molten plastic material fills the entire cavity (33); S4, the second glue inlet (12) is fed with glue, the molten plastic material flows along the second glue inlet hot runner (314) to each second glue inlet (12), and then is injected into the lower small diameter section (332) of the cavity (33) through the short-distance glue nozzle section, and as the amount of glue fed increases, the molten plastic material fills the entire cavity (33); S5. During the injection molding process, when the molten plastic material enters the cavity (33), the gas in the cavity (33) is squeezed so that a portion of the gas is discharged from the lateral first exhaust channel (34) and another portion is discharged from the vertical second exhaust channel (35); S6, waiting for the injection mold (3) to cool down; S7, after curing and molding, the upper mold assembly (31) and the lower mold assembly (32) are separated, and the molded double-layer battery insulation ring (2) is taken out. At this time, multiple double-layer battery insulation rings (2) are connected into one body through the nozzle material (23); S8. The formed double-layer battery insulation ring (2) has an upper large-diameter insulation section (21) and a lower small-diameter insulation section (22). The sprue material (23) on the lower small-diameter insulation section (22) is trimmed off to obtain a plurality of independent double-layer battery insulation rings (2).