Continuous crystallization method of monopotassium phosphate
Through the adsorption and vacuum concentration of weak acid chelating resins, the problem of protein and calcium and magnesium ions affecting potassium dihydrogen phosphate crystallization in corn soaked water is solved, and the continuous crystallization of potassium dihydrogen phosphate with high yield and low cost is achieved, saving Energy consumption.
Patent Information
- Application Number
- CN202310570915.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-19
- Publication Date
- 2024-11-22
AI Technical Summary
In the prior art, when preparing potassium dihydrogen phosphate from corn soaked in water, the presence of protein, calcium and magnesium ions leads to high costs, low yields, and the continuous crystallization cannot be achieved, and the evaporation process consumes a lot of energy.
Adsorption of the crude potassium dihydrogen phosphate solution by using weak acid chelating resin. The calcium and magnesium ions are removed through the exchange reaction of weak acid chelating resin with calcium and magnesium ions, and the calcium and magnesium ions are achieved through vacuum concentration and decolorization of activated carbon. Continuous crystallization.
The crystallization yield of potassium dihydrogen phosphate is increased by more than 95%, reducing energy consumption, achieving continuous crystallization of potassium dihydrogen phosphate, reducing the consumption of phosphoric acid, and avoiding the emission of the final mother liquor.
Smart Images

Figure BDA0004238557830000111
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of potassium dihydrogen phosphate crystallization, and in particular to a continuous crystallization method of potassium dihydrogen phosphate. Background Art
[0002] Potassium dihydrogen phosphate is an important chemical, which is widely used in agriculture, chemical industry, medicine and food industries. In the chemical industry, potassium dihydrogen phosphate can be used as a buffer, culture agent, raw material for potassium metaphosphate, fermentation aid, culture agent, enhancer and leavening agent for brewing yeast, etc. In agriculture, potassium dihydrogen phosphate is a high-concentration and high-efficiency phosphorus-potassium compound fertilizer; in medicine, potassium dihydrogen phosphate can be used to acidify urine and as a nutrient; in food, potassium dihydrogen phosphate can be used as a flavoring agent for synthetic sake.
[0003] Corn steep water is wastewater produced during the wet milling process of producing corn starch. Generally, about 0.8 tons of corn steep water is produced when 1 ton of corn is processed. Corn steep water contains a large amount of valuable substances such as protein, phytic acid, lactic acid and lipopolysaccharide, among which the content of phytic acid is about 1-2%. Phytic acid in corn steep water can be recovered to obtain potassium phytate, and potassium phytate can be further used to prepare potassium dihydrogen phosphate.
[0004] However, since the protein and calcium and magnesium ions originally present in the corn soaking water cannot be completely removed during the preparation process, some of the protein and calcium and magnesium ions will enter the final potassium dihydrogen phosphate crude solution. The presence of calcium and magnesium ions will make the potassium dihydrogen phosphate crystallization aqueous solution turbid, affecting the quality of the final product. The presence of protein will make the crystallization mother liquor viscous, which will make the mother liquor difficult to crystallize. For this reason, phosphoric acid needs to be added in the prior art to lower the pH of the solution (adjust the pH to 3.8) to increase the solubility of calcium and magnesium salts (pH between 3.0-4.0, H2PO4 - The proportion is 88%-98.6%, H3PO4 accounts for 12%-1%), and then it is crystallized by four-effect evaporation, and the mother liquor is recrystallized by single-effect evaporation, and the mother liquor is finally sold.
[0005] The method in the prior art not only increases the consumption of phosphoric acid, but also has a high cost. At the same time, the phosphoric acid combined with calcium and magnesium cannot be effectively released, resulting in a low crystallization yield of potassium dihydrogen phosphate. At the same time, due to the influence of protein and the presence of calcium and magnesium ions on crystallization, it is also impossible to achieve continuous crystallization of potassium dihydrogen phosphate. 3 Water consumption: 0.3m 3 Steam, single effect evaporation 1m 3 Water consumption: 1.2m 3 Steam, and the single-effect evaporation time is long, and the energy consumption is serious.
[0006] In view of the problems existing in the prior art, it is urgent to provide a continuous crystallization method for potassium dihydrogen phosphate prepared from corn soaking water. Summary of the invention
[0007] In view of this, the object of the present invention is to provide a continuous crystallization method of potassium dihydrogen phosphate, which is used to overcome the technical problems of high cost, low yield and inability to continuously crystallize in the potassium dihydrogen phosphate prepared by using corn soaking water as raw material in the prior art due to the presence of protein and calcium and magnesium ions.
[0008] In order to achieve the above object, the present invention provides a continuous crystallization method of potassium dihydrogen phosphate, comprising the following steps:
[0009] The crude potassium dihydrogen phosphate solution is adsorbed by a weakly acidic chelating resin to obtain an effluent;
[0010] Concentrating the effluent in vacuo to obtain a concentrated solution;
[0011] adding activated carbon to the concentrated solution for decolorization to obtain a decolorized solution;
[0012] Filtering the decolorized liquid to remove the activated carbon to obtain a filtrate;
[0013] The filtrate is crystallized to separate and obtain a crystallization mother liquor and potassium dihydrogen phosphate crystals;
[0014] The crystallization mother liquor is returned to the step of adsorption by the weakly acidic chelating resin, and the above crystallization process is repeated to achieve continuous crystallization of potassium dihydrogen phosphate.
[0015] The invention provides a continuous crystallization method of potassium dihydrogen phosphate, comprising the following steps: a crude potassium dihydrogen phosphate solution is adsorbed by a weakly acidic chelating resin, the effluent after the adsorption is decolorized, filtered and crystallized to obtain potassium dihydrogen phosphate crystals and a crystallization mother liquor, and the crystallization mother liquor is returned to the initial step to repeat the above crystallization process to achieve continuous crystallization. The invention selects a weakly acidic chelating resin with a specific skeleton (polystyrene copolymer or cross-linked copolymer of styrene and divinylbenzene) and a functional group (aminophosphonic acid or aminomethylphosphonic acid). Since the chelating resin is weakly acidic, and the calcium ions and magnesium ions contained in the crude potassium dihydrogen phosphate solution are alkaline metal ions, the weakly acidic hydrogen ions in the chelating resin can preferably exchange with the alkaline calcium ions and / or magnesium ions in the crude potassium dihydrogen phosphate solution, so that the weakly acidic chelating resin selectively adsorbs the calcium ions and magnesium ions in the crude potassium dihydrogen phosphate solution, and the aminophosphonic acid or aminomethylphosphonic acid in the functional group can form a multi-bond chelating bond with the exchanged calcium ions and magnesium ions, thereby firmly adsorbing the calcium ions and magnesium ions, and then selectively removing the corresponding calcium ions and magnesium ions in the crude potassium dihydrogen phosphate solution; in addition, The weakly acidic chelating resin used in the present invention (the weakly acidic chelating resin in the present invention can selectively remove divalent metal cations from wastewater containing monovalent cations) has no obvious adsorption effect on potassium ions. While removing calcium and magnesium, potassium ions in the solution are retained, so that the yield of potassium dihydrogen phosphate will not be reduced (after potassium ions are adsorbed by the resin, potassium dihydrogen phosphate will be converted into phosphoric acid); the effluent after adsorption is vacuum concentrated and decolorized, and the protein in the solution is further removed, and then the crystallization mother liquor and potassium dihydrogen phosphate crystals can be obtained after filtration and crystallization; the obtained crystallization mother liquor returns to the initial step, and the above-mentioned crystallization process is repeated to further recover potassium dihydrogen phosphate. There is no final mother liquor discharge in the production process, and the crystallization process will not be interrupted due to high calcium and magnesium content, so that continuous crystallization of potassium dihydrogen phosphate is achieved, and the crystallization yield of potassium dihydrogen phosphate is improved. Experiments show that the yield of potassium dihydrogen phosphate produced by the method of the present invention reaches more than 95%. DETAILED DESCRIPTION
[0016] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0017] The present invention provides a continuous crystallization method of potassium dihydrogen phosphate, comprising the following steps:
[0018] The crude potassium dihydrogen phosphate solution is adsorbed by a weakly acidic chelating resin to obtain an effluent;
[0019] Concentrating the effluent in vacuo to obtain a concentrated solution;
[0020] adding activated carbon to the concentrated solution for decolorization to obtain a decolorized solution;
[0021] Filtering the decolorized liquid to remove the activated carbon to obtain a filtrate;
[0022] The filtrate is crystallized to separate and obtain a crystallization mother liquor and potassium dihydrogen phosphate crystals;
[0023] The crystallization mother liquor is returned to the step of adsorption by the weakly acidic chelating resin, and the above crystallization process is repeated to achieve continuous crystallization of potassium dihydrogen phosphate.
[0024] The present invention firstly adsorbs a crude potassium dihydrogen phosphate solution through a weakly acidic chelating resin to obtain an effluent. In the present invention, the crude potassium dihydrogen phosphate solution is a solution containing calcium, magnesium ions and protein. As mentioned in the background technology of the present invention, the presence of calcium and magnesium ions will cause turbidity in the crystallization aqueous solution of potassium dihydrogen phosphate, affecting the quality of the final product. The presence of protein will make the crystallization mother liquor viscous, thereby causing the mother liquor to be difficult to crystallize. The present invention solves the problem of continuous crystallization of a crude potassium dihydrogen phosphate solution containing calcium, magnesium ions and protein. Further, the present invention solves the problem of continuous crystallization of a crude potassium dihydrogen phosphate solution prepared with corn soaking water as a raw material; the corn soaking water contains phytic acid 1.0-1.5%, potassium 0.3-0.9%, calcium 40ppm, magnesium 1700ppm, and protein about 5%; potassium phytate can be obtained by subjecting the corn soaking water to resin adsorption, potassium chloride analysis, membrane separation and other technologies, and potassium phytate contains about 100-150ppm calcium, about 2000-3000ppm magnesium, and about 1.0-1.5% protein; potassium phytate can be hydrolyzed to prepare potassium dihydrogen phosphate and inositol, but calcium, magnesium ions and protein cannot be completely removed during this preparation process, and most of them enter the crude potassium dihydrogen phosphate solution. Generally, the crude potassium dihydrogen phosphate solution prepared from corn soaking water contains about 15-30ppm calcium, about 300-600ppm magnesium, and about 0.5-1.4% protein. The present invention is a continuous crystallization method proposed for such a crude potassium dihydrogen phosphate solution.
[0025] In the present invention, the skeleton of the weak acid chelating resin is preferably a polystyrene copolymer or a cross-linked copolymer of styrene and divinylbenzene, and the functional group of the weak acid chelating resin is preferably aminophosphonic acid or aminomethylphosphonic acid; further preferably, the weak acid chelating resin is a macroporous weak acid chelating resin CH-93 having a polystyrene copolymer skeleton and aminomethylphosphonic acid groups, or a macroporous weak acid chelating resin LSC-500 having a cross-linked copolymer skeleton of styrene and divinylbenzene and aminophosphonic acid groups. Weakly acid chelating resin is a polymer compound that can selectively chelate specific metal ions in the form of ionic bonds or coordination bonds from a solution containing metal ions. The resin is composed of a cross-linked polymer (such as styrene / divinylbenzene resin) as a skeleton and connected with a special functional group. The weakly acid chelating resin in the present invention can selectively remove trace heavy metals such as calcium and magnesium in water bodies by selecting specific functional groups, without excessively adsorbing potassium ions in the solution. It should be understood that adsorption selectivity and adsorption capacity are two important indicators for evaluating the performance of chelating resins, wherein adsorption capacity depends on the specific surface area of the adsorbent material and the density of the surface functional groups, and adsorption selectivity depends on the type of the surface functional groups. Ion exchange resins utilize electrostatic action to combine with metal ions, which is different from the principle of adsorption of metal ions by ion exchange resins. The adsorption of metal ions by chelating resins is through the coordination reaction between the atoms on its functional groups (aminophosphonic acid and aminomethylphosphonic acid in the present invention) and metal ions, generating coordinated covalent bonds and forming structurally stable chelates. Therefore, the stability of chelates formed by different metal ions and different functional groups is different, which determines the height of the adsorption / selectivity of chelating resins to different metal ions; in addition, since the activity of functional groups under different pH conditions is different, pH is also a key factor determining the selectivity of chelating resins to metal ion adsorption; taking a chelating resin whose functional group is iminodiacetic acid group as an example, it has a very strong adsorption effect on nickel in the pH range of 3-5, and the selective adsorption order of metal ions is Ni>Zn>Co>Mg>Ca>Na.
[0026] As far as the present invention is concerned, the chelating resin whose functional group is aminomethylphosphonic acid or aminophosphonic acid has a strong adsorption effect on calcium and magnesium, and the inventors have found that under the weakly acidic (pH 5-6.5) chelating resin conditions in the present invention, the order of the adsorption capacity of the resin is Mg>Ca>K>Na.
[0027] Specifically, when the Ca in the treatment solution 2+ Mg 2+ When cations diffuse into the pores of the resin, the resin is 2+ Mg 2+ The selectivity for isocations is stronger than that for K + The selectivity of K + The Ca2+ that enters the resin pores2+ Mg 2+ The cations undergo a rapid exchange reaction, Ca 2+ Mg 2+ The cations are fixed to the resin exchange groups, and the exchanged cations diffuse into the pores of the resin and eventually diffuse into the water, ultimately achieving Ca 2+ Mg 2+ The cations are adsorbed, while K + The ions remain in the solution, achieving the effect of Ca 2+ Mg 2+ Ions and K + The separation of ions ensures the yield of potassium dihydrogen phosphate.
[0028] The weakly acidic chelating resin of the invention has an amino group / aminomethyl group and a phosphonic acid group. The invention uses styrene monomer and / or divinylbenzene monomer, ethylenediamine and phosphorous acid as raw materials, adds acid to adjust the pH value to 5-6.5 after swelling reaction, and then obtains the weakly acidic chelating resin of the invention through filtering, washing and drying. The weakly acidic chelating resin of the invention has a high adsorption performance for calcium and magnesium, and has a weak adsorption performance for potassium ions, and will not cause a decrease in the yield of potassium dihydrogen phosphate in the invention. The weakly acidic chelating resin of the invention is a good calcium and magnesium treatment resin applied to the invention.
[0029] In the present invention, the weakly acidic chelating resin absorbs calcium, magnesium and protein in the crude potassium dihydrogen phosphate solution, replaces the hydrogen ions in the resin, and the hydrogen ions then react with the phosphorus originally combined with calcium and magnesium to generate phosphoric acid. Therefore, the present invention does not need to add phosphoric acid during crystallization to increase the solubility of calcium and magnesium as in the prior art.
[0030] In the present invention, the feed amount of the crude potassium dihydrogen phosphate solution is preferably 5-6BV of the volume of the weakly acidic chelating resin, and the flow rate is preferably 4-5BV / h; the present invention has no special limitation on the carrier of the weakly acidic chelating resin, for example, a resin column or a glass column can be used, and the present invention has no special limitation on the diameter-to-height ratio of the resin column.
[0031] After obtaining the effluent, the present invention performs vacuum concentration on the effluent to obtain a concentrated solution. In the present invention, the temperature of the vacuum concentration is preferably 70-100°C, and the vacuum degree is preferably -0.07MPa to -0.10MPa; the solid content of the concentrated solution obtained by the present invention is preferably 60-65wt%, and the purpose of the vacuum concentration of the present invention is to improve the effect of the subsequent decolorization process; the present invention has no special restrictions on the equipment for vacuum concentration, such as a four-effect evaporator, and the four-effect evaporator used in the present invention can achieve continuous evaporation, which saves steam and has energy-saving effect compared with the single-effect evaporation of the mother liquor in the prior art.
[0032] After obtaining the concentrated solution, the present invention adds activated carbon to the concentrated solution for decolorization to obtain a decolorized solution. In the present invention, the addition amount of the activated carbon is preferably 1-5% of the volume of the concentrated solution, the decolorization temperature is preferably 90-95°C, and the decolorization time is preferably 15-30min; the present invention has no special limitation on the pore size of the activated carbon, for example, it can be 5-10um; the present invention has no special limitation on the source of the activated carbon, and commercially available products can be used.
[0033] After obtaining the decolorized liquid, the present invention filters the decolorized liquid to obtain a filtrate. In the present invention, the filtration preferably uses a candle filter or a plate-and-frame filter, the filter cloth pore size is preferably 800-1000 mesh, and the operating pressure is preferably 0.3-0.5 MPa. The present invention uses filtration to separate the decolorized activated carbon and the solution, which is convenient for subsequent steps.
[0034] After obtaining the filtrate, the present invention crystallizes the filtrate to separate and obtain a crystallization mother liquor and potassium dihydrogen phosphate crystals. In the present invention, the crystallization preferably includes: first heating the filtrate to 90-95°C, then cooling to 60-65°C for insulation reaction for 1.5-2h, then cooling to 50-55°C for insulation reaction for 0.8-1h, then cooling to 40-45°C for insulation reaction for 0.8-1h, then cooling to 30-35°C for insulation reaction for 0.8-1h, to obtain a crystallization mother liquor and potassium dihydrogen phosphate crystals; further, in the process of heating the filtrate, it is preferably further included to stir at a rate of 100-250rpm. The method of separating the crystallization mother liquor and potassium dihydrogen phosphate crystals of the present invention can be carried out by filtration. The present invention has no special limitation on the filtering method, such as filter paper filtration or suction filtration. When using filter paper filtration, for example, industrial filter paper can be used, and the pore size of the filter paper is preferably 5-10um; when using suction filtration, for example, a 5-10um sand core funnel can be used. Further, the filtration described in the present invention can also be carried out by filter cloth filtration or centrifugal separation by centrifuge; when using filter cloth filtration, the pore size of the filter cloth is preferably 5-10um; when using centrifuge separation, the filter cloth is preferably 800-1000 mesh, and the centrifuge speed is preferably 1000-2000rpm.
[0035] After obtaining potassium dihydrogen phosphate crystals (wet crystals), the present invention further comprises: drying the potassium dihydrogen phosphate crystals to obtain dried potassium dihydrogen phosphate crystals, wherein the drying conditions are preferably: drying temperature 100-140° C., and drying time 2-4 hours. The present invention has no special requirements for the drying equipment, such as fluidized bed drying or constant temperature drying oven drying.
[0036] After obtaining the crystallization mother liquor, the present invention further comprises: returning the crystallization mother liquor to the step of adsorption by the weakly acidic chelating resin, repeating the above-mentioned crystallization process, and realizing continuous crystallization of potassium dihydrogen phosphate. Since the crystallization mother liquor prepared by the method of the present invention has low contents of calcium, magnesium and protein, it can be directly returned to the initial step to be combined with the crude potassium dihydrogen phosphate solution or with the effluent to further extract the potassium dihydrogen phosphate therein, and the crystallization process will not be interrupted due to the high contents of calcium and magnesium, thereby realizing continuous crystallization of potassium dihydrogen phosphate, and there is no final mother liquor discharge in the production process, which has the characteristics of environmental protection.
[0037] Furthermore, after the crude potassium dihydrogen phosphate solution is adsorbed by a weakly acidic chelating resin, the method further comprises: the weakly acidic chelating resin after adsorption is resolved by hydrochloric acid to obtain a resolved solution, the resolved solution is mixed with corn soaking water, and other products are further prepared. In the present invention, the concentration of the hydrochloric acid is preferably 5-10wt%, the amount is preferably 1-2BV of the weakly acidic chelating resin, and the flow rate is preferably 3-5BV / h. The resolved solution obtained by hydrochloric acid contains valuable components of calcium and magnesium salts, which can be further recovered for the preparation of other products; for example, it is mixed with corn soaking water, evaporated to form a concentrated slurry for sale.
[0038] In order to better illustrate the technical solution of the present invention, the present invention also provides the following specific examples. It should be understood that the raw materials used in the following examples are all commercially available raw materials unless otherwise specified.
[0039] In particular, the main components of three batches of crude potassium dihydrogen phosphate solutions are listed in Table 1 below, and the crude potassium dihydrogen phosphate solutions are all provided by Zhucheng Haotian Pharmaceutical Co., Ltd.
[0040] Table 1 Composition of crude potassium dihydrogen phosphate solution of batches 1-3
[0041] serial number Potassium dihydrogen phosphate Calcium Magnesium ion protein other water Batch 1 21.55% 17ppm 452ppm 1.2% 0.1% 78.2% Batch 2 20.88% 15ppm 403ppm 1.1% 0.1% 79.1% Batch 3 21.08% 18ppm 389ppm 1.0% 0.1% 78.9%
[0042] Example 1
[0043] S1. Take 10L of crude potassium dihydrogen phosphate solution from batch 1 and pass it through a glass column filled with 2L CH-93 weakly acidic chelating resin at a flow rate of 4.5BV / h to obtain 9.85L of effluent;
[0044] S2. The effluent was concentrated under vacuum at 80°C and -0.08MPa to obtain 3.42L of a concentrate having a solid content of 63wt%;
[0045] S3. Add 34.2 g of activated carbon (pore size 8 μm) to the concentrate and decolorize for 25 min to obtain 3.42 L of decolorized solution;
[0046] S4. The decolorized liquid was added to the candle filter, the filter cloth pore size was 900 mesh, the operating pressure was 0.4MPa, and 3.35L of filtrate was obtained;
[0047] S5. The filtrate was first heated to 90°C with stirring at 150 rpm, then cooled to 60°C for reaction for 2 h, then cooled to 50°C for reaction for 1 h, then cooled to 40°C for reaction for 1 h, then cooled to 30°C for reaction for 1 h, filtered through 5 um filter paper to obtain 2.715 L of crystallization mother liquor and 1476 g of potassium dihydrogen phosphate; the potassium dihydrogen phosphate was dried at 105°C for 2 h to obtain 1358 g of potassium dihydrogen phosphate crystals;
[0048] S6. The crystallization mother liquor is returned to step S1 and mixed with the crude potassium dihydrogen phosphate solution in a volume ratio of 2.71:7.29, and then continues to enter the weakly acidic chelating resin to repeat the above steps S1-S6, and finally 2249g of dried potassium dihydrogen phosphate crystals are obtained again, and a total of 3607g of potassium dihydrogen phosphate crystals are obtained, and no final mother liquor is produced.
[0049] Example 2
[0050] S1. Take 10L of crude potassium dihydrogen phosphate solution from batch 2 and pass it through a glass column filled with 1.7L CH-93 weakly acidic chelating resin at a flow rate of 4BV / h to obtain 9.8L of effluent;
[0051] S2. The effluent was concentrated under vacuum at 100 ° C and -0.07 MPa to obtain 3.480 L of a concentrate having a solid content of 60 wt%;
[0052] S3. 104.4 g of activated carbon (pore size 5 μm) was added to the concentrate and decolorized for 15 min to obtain 3.480 L of decolorized solution;
[0053] S4. The decolorized liquid was added to a plate and frame filter, the filter cloth pore size was 1000 mesh, the operating pressure was 0.3MPa, and 3.40L of filtrate was obtained;
[0054] S5. The filtrate was first heated to 95°C with stirring at 100 rpm, then cooled to 65°C for 1.5 h, then cooled to 55°C for 0.8 h, then cooled to 45°C for 0.8 h, then cooled to 35°C for 0.8 h, filtered through 10 um filter paper to obtain 2.880 L of crystallization mother liquor and 1362 g of potassium dihydrogen phosphate; the potassium dihydrogen phosphate was dried at 100°C for 3 h to obtain 1253 g of potassium dihydrogen phosphate crystals;
[0055] S6. The crystallization mother liquor is returned to step S1 and mixed with the crude potassium dihydrogen phosphate solution in a volume ratio of 2.88:7.12, and then continues to enter the weakly acidic chelating resin to repeat the above steps S1-S6, and finally 2229g of dried potassium dihydrogen phosphate crystals are obtained again, and a total of 3482g of potassium dihydrogen phosphate crystals are obtained, and no final mother liquor is produced.
[0056] Example 3
[0057] S1. Take 10L of crude potassium dihydrogen phosphate solution from batch 3 and pass it through a glass column filled with 1.8L LSC-500 weakly acidic chelating resin at a flow rate of 5BV / h to obtain 9.8L of effluent;
[0058] S2. The effluent was concentrated under vacuum at 70°C and -0.10MPa to obtain 3.24L of a concentrate having a solid content of 65wt%;
[0059] S3. 162 g of activated carbon (pore size 10 μm) was added to the concentrate and decolorized for 30 min to obtain 3.24 L of decolorized solution;
[0060] S4. The decolorized liquid was added to the candle filter, the filter cloth pore size was 800 mesh, the operating pressure was 0.5 MPa, and 3.14 L of filtrate was obtained;
[0061] S5. The filtrate was first heated to 92 ° C with stirring at 250 rpm, then cooled to 62 ° C for 1.8 h, then cooled to 52 ° C for 0.9 h, then cooled to 42 ° C for 0.9 h, then cooled to 32 ° C for 0.9 h, and separated by a 900 mesh centrifuge (speed 1500 rpm) to obtain 2.535 L of crystallization mother liquor and 1489 g of potassium dihydrogen phosphate; the potassium dihydrogen phosphate was dried at 140 ° C for 4 h to obtain 1370 g of potassium dihydrogen phosphate crystals;
[0062] S6. The crystallization mother liquor is returned to step S1 and mixed with the effluent in a volume ratio of 2.5:7.5, and then continues to enter the weakly acidic chelating resin to repeat the above steps S1-S6, and finally 2173g of dried potassium dihydrogen phosphate crystals are obtained again, and a total of 3543g of potassium dihydrogen phosphate crystals are obtained, and no final mother liquor is produced.
[0063] Example 4
[0064] The 2L of weakly acidic chelating resin adsorbed in step S1 of Example 1 was analyzed with 2L of 8wt% hydrochloric acid solution at a flow rate of 4BV / h to obtain 1.9L of analytical solution (containing calcium and magnesium salts).
[0065] Example 5
[0066] The 2L of weakly acidic chelating resin adsorbed in step S1 of Example 2 was analyzed with 4L of 10wt% hydrochloric acid solution at a flow rate of 5BV / h to obtain 3.85L of analytical solution (containing calcium and magnesium salts).
[0067] Example 6
[0068] The 2L of weakly acidic chelating resin adsorbed in step S1 of Example 3 was analyzed with 3L of 5wt% hydrochloric acid solution at a flow rate of 3BV / h to obtain 2.9L of analytical solution (containing calcium and magnesium salts).
[0069] Comparative Example 1
[0070] The CH-93 weakly acidic chelating resin in Example 1 was replaced by an equal amount of D401 cationic resin, and other conditions remained unchanged.
[0071] A total of 3352 g of potassium dihydrogen phosphate crystals and 4320 ml of final mother liquor were obtained.
[0072] D401 cationic resin can adsorb cations, but it preferentially adsorbs potassium ions in a potassium ion environment and has a weaker adsorption capacity for calcium and magnesium.
[0073] Comparative Example 2
[0074] The CH-93 weakly acidic chelating resin in Example 2 was replaced by an equal amount of ZG-6 cationic resin, and other conditions remained unchanged.
[0075] A total of 3253 g of potassium dihydrogen phosphate crystals and 4280 ml of final mother liquor were obtained.
[0076] ZG-6 cationic resin absorbs calcium, magnesium and potassium at the same time, and the amount of potassium absorbed is more than 10 times the amount of calcium and magnesium. Therefore, it will lead to a reduction in potassium sources and part of potassium dihydrogen phosphate will be converted into phosphoric acid.
[0077] Comparative Example 3
[0078] The LSC-500 weakly acidic chelating resin in Example 3 was replaced by an equal amount of D732 cationic resin, and other conditions remained unchanged.
[0079] A total of 3313 g of potassium dihydrogen phosphate crystals and 4360 ml of final mother liquor were obtained.
[0080] D732 cationic resin can adsorb cations, but it preferentially adsorbs potassium ions in a potassium ion environment and has a weaker adsorption capacity for calcium and magnesium.
[0081] Table 2 below lists the recovery of potassium dihydrogen phosphate and the concentration of calcium and magnesium salts in the analytical solution in the examples and comparative examples, wherein the calcium and magnesium salt concentration data in comparative examples 1-3 are obtained by treating the resins in comparative examples 1-3 with the same steps and parameters as in examples 4-6.
[0082] Table 2 Recovery of potassium dihydrogen phosphate and concentration of calcium and magnesium salts in analytical solution in Examples and Comparative Examples
[0083]
[0084] Test Case
[0085] A: Determination method of potassium dihydrogen phosphate yield
[0086] Yield = total dry crystal weight / (concentration of crude potassium dihydrogen phosphate solution × liquid volume).
[0087] B: Determination of calcium and magnesium salt concentration
[0088] The concentration of calcium and magnesium salts can be measured according to the national standard GB 11905-89 (atomic absorption spectrophotometry).
[0089] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention is described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A continuous crystallization method for potassium dihydrogen phosphate, characterized in that: The following steps are involved: The crude potassium dihydrogen phosphate solution is adsorbed by a weakly acidic chelating resin to obtain an effluent; Concentrating the effluent in vacuo to obtain a concentrated solution; Adding activated carbon to the concentrated solution for decolorization to obtain a decolorized solution; Filtering the decolorized liquid to remove the activated carbon to obtain a filtrate; The filtrate is crystallized to separate and obtain a crystallization mother liquor and potassium dihydrogen phosphate crystals; The crystallization mother liquor is returned to the step of adsorption by the weakly acidic chelating resin, and the above crystallization process is repeated to achieve continuous crystallization of potassium dihydrogen phosphate.
2. The method according to claim 1, characterized in that The skeleton of the weak acid chelating resin is a polystyrene copolymer or a cross-linked copolymer of styrene and divinylbenzene, and the functional group of the weak acid chelating resin is aminophosphonic acid or aminomethylphosphonic acid.
3. The method according to claim 1, characterized in that The feed amount of the crude potassium dihydrogen phosphate solution is 5-6 BV of the volume of the weakly acidic chelating resin, and the flow rate is 4-5 BV / h; the temperature of the vacuum concentration is 70-100° C., and the vacuum degree is -0.07 MPa to -0.10 MPa.
4. The method according to claim 1, characterized in that The crude potassium dihydrogen phosphate solution has a calcium ion content of 15-30 ppm, a magnesium ion content of 300-600 ppm, a protein content of 0.5-1.4 wt %, and the balance is potassium dihydrogen phosphate.
5. The method according to claim 1, characterized in that The solid content of the concentrated liquid is 60-65 wt %.
6. The method according to claim 1, characterized in that The amount of activated carbon added is 1-5% of the volume of the concentrated solution, the decolorization temperature is 90-95° C., and the decolorization time is 15-30 minutes.
7. The method according to claim 1, characterized in that The filtration adopts a candle filter or a plate and frame filter, and the pore size of the filter cloth is 800-1000 meshes.
8. The method according to claim 1, characterized in that The crystallization comprises: first heating the filtrate to 90-95° C., then cooling to 60-65° C. for 1.5-2 hours, then cooling to 50-55° C. for 0.8-1 hour, then cooling to 40-45° C. for 0.8-1 hour, then cooling to 30-35° C. for 0.8-1 hour, and separating to obtain crystallization mother liquor and potassium dihydrogen phosphate crystals.
9. The method according to claim 1 or 8, characterized in that: The separation to obtain the crystallization mother liquor and potassium dihydrogen phosphate crystals is carried out by using filter paper, filter cloth, suction filtration or centrifugal separation in a centrifuge.
10. The method according to claim 1, characterized in that The step of returning the crystallization mother liquor to the adsorption step by the weakly acidic chelating resin specifically comprises: Before the crude potassium dihydrogen phosphate solution is adsorbed by the weakly acidic chelating resin, the method further includes mixing the crystallization mother liquor with the crude potassium dihydrogen phosphate solution; and / or, After the crude potassium dihydrogen phosphate solution is adsorbed by a weakly acidic chelating resin and before the effluent is vacuum concentrated, the method further comprises: mixing the crystallization mother liquor with the effluent.
Citation Information
Patent Citations
Method for extracting potassium from corn soaking solution to prepare glaserite and potassium sulfate
CN114149014A
Method for improving clarity of monopotassium phosphate product prepared from corn soaking water