Silicon dioxide nanoparticle modified two-component polyurethane elastic wear-resistant coating and application thereof

Through the two-component polyurethane coating modified by silica nanoparticles, combined with specific polyols and silane coupling agents, the scratching problem of car-coated film coating during construction and use is solved, achieving high stretching and wear resistance The balance of properties meets the needs of car coat film and improves the weather resistance of the coating.

CN118995026APending Publication Date: 2024-11-22ZHEJIANG FULAI NEW MATERIAL CO LTD

Patent Information

Application Number
CN202411332574.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-24
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing car coat film coating is prone to scratches during construction and use, which requires thermal repair, and the hardened film coating lacks elasticity, resulting in cracks easily during installation and mounting, which cannot meet the tensile performance requirements of the car coat film.

Method used

Two-component polyurethane elastic wear-resistant coating modified with silica nanoparticles provides high elongation and wear resistance through the combination of nanosilicon dioxide dispersion and specific polyols, and uniform dispersion using silane coupling agent. Nanoparticles form chemical bonds, enhancing the hardness and stability of the coating.

Benefits of technology

Reduce scratches during normal construction and use, reduce post-treatment processes, keep the coating intact, meet the stretching needs of the car coat film, and improve weather resistance and gloss.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005057403580000051
    Figure BDA0005057403580000051
Patent Text Reader

Abstract

The invention belongs to the technical field of automobile protective films, and particularly discloses a silicon dioxide nanoparticle modified two-component polyurethane elastic wear-resistant coating and application thereof. The coating is prepared by mixing and curing a component A and a component B; the component A comprises a nano silicon dioxide dispersion liquid, polyester polyol, polycaprolactone polyol, organic silicon polyol and acrylic resin polyol, and the nano silicon dioxide dispersion liquid is formed by mixing nano silicon dioxide, polycarbonate polyol, an organic solvent and a silane coupling agent; and the component B comprises an auxiliary agent and an organic solvent. The flexible wear-resistant coating prepared according to the formula can avoid scratches, so that post-treatment procedures are effectively reduced, and manpower and time costs are saved; the coating is high in wear resistance and can maintain high stretching, so that the coating has excellent attachment performance; in addition, the coating also has good weather resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of automobile protective films and relates to a flexible wear-resistant coating, in particular to a two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles and application thereof. Background Art

[0002] Paint Protective Film (PPF), also known as "car cover film" or "invisible car cover", is a general term for a transparent protective film that is pasted on the outside of the car's paint surface. PPF paint protection film can protect the car's paint surface, prevent scratches in minor accidents and the impact of stones flying during driving on the paint surface, and prevent foreign objects from sticking to the car paint, such as acid rain, bird droppings, etc. At the same time, paint protection film can improve the appearance of the car and increase the brightness and gloss of the car paint. At present, the invisible car cover film manufacturers on the market include foreign companies such as 3M, LLumar, V-KOOL, etc., and domestic companies such as Kewei and Lucky.

[0003] The structure of car cover is generally composed of adhesive layer + TPU + self-repairing coating. Conventional self-repairing coating will cause scratches on the surface during the construction process, and the surface will be very rough and the glossiness will decrease. It is necessary to use a hot air gun to blow hot air or pour hot water for thermal repair to restore the scratches on the surface and restore the original glossiness. At present, car cover coating generally adopts heat-repairing polyurethane coating. External force destroys the surface molecular chain. Under heating, the molecules move and restore the original paint film properties. Conventional two-component polyurethane coating generally has a component composed of polyester polyol, acrylic polyol, or other polyols, and then adds a second component curing agent. The two components react under appropriate conditions to form an elastic network structure, and the self-repairing ability comes from this elastic network structure. During the scraping process, as long as the network structure is not destroyed, the collapsed network structure can rebound to the initial state under the external heat to complete the self-repair process. The problem is that if there is no external heat, the scratches can be seen.

[0004] Since the coating is prone to scratches during the actual construction process, the vehicle needs to be reprocessed with hot water or a hot air gun after the vehicle is installed, which increases the post-processing process. At the same time, during the later use, dust in the air will also cause scratches on the paint protection film. If it is not heated for a long time, the coating does not have a self-healing function. After a long time, the scratches are fixed and cannot be restored even if heated.

[0005] Although there are hardened film coatings on the market that have good wear resistance, these coatings are generally not elastic. The main base material of car cover film is TPU, which has an elongation rate of 300-400%. If the coating cannot be stretched, it will often be broken. For example, when installing and wrapping, PPF is usually stretched. If the coating elongation rate is too low, it will cause cracks in the coating. Therefore, hardened film coatings are not suitable for the PPF industry. In order to meet the tensile performance, the two-component polyol coating sacrifices rigidity and uses elasticity to meet the requirements of construction, so it often loses wear resistance and needs to be repaired by heating and other conditions. Summary of the invention

[0006] In order to solve the above problems, the present invention provides a two-component polyurethane elastic wear-resistant coating modified by silica nanoparticles and its application. The coating is a flexible, wear-resistant self-repairing coating, which can ensure that under normal construction, the self-repairing coating will not have scratches. On the one hand, it can reduce the post-construction processing procedures, and on the other hand, it can effectively avoid obvious scratches on the coating that affect the product appearance in conventional daily use. The car cover coating of the present invention can always remain in good condition and better protect the car paint. At the same time, the elongation rate is more than 100%, which fully meets the installation requirements of the car cover construction process.

[0007] In order to achieve the above object, the specific technical solution adopted by the present invention is as follows:

[0008] In the first aspect, the present invention provides a two-component polyurethane elastic wear-resistant coating modified by silica nanoparticles, which is made by mixing and curing component A and component B; the component A includes nano-silica dispersion, polyester polyol, polycaprolactone polyol, silicone polyol and acrylic resin polyol, and the nano-silica dispersion is a mixture of nano-silica, polycarbonate polyol, organic solvent and silane coupling agent; the component B includes an auxiliary agent and an organic solvent.

[0009] The present invention fills and grafts inorganic nano-silicon dioxide particles onto the two-component chain segments to provide rigid support points, while maintaining a high elastic elongation rate through the linking of the soft chain segments, and can also improve the wear resistance of the two-component coating. The preparation of nano-silicon dioxide dispersion is particularly important. The selection of particles with a particle size between 10 and 50 nanometers does not affect the scattering of light and the elastic elongation rate of the soft segment, but at the same time increases the wear resistance of the two-component polyurethane resin. By using a silane coupling agent, the nano-silicon dioxide is evenly dispersed, and the performance stability of the coating is improved; specifically, the silane coupling agent can react with the hydroxyl group on the surface of the nano-silicon dioxide to form a chemical bond, thereby evenly dispersing the nano-silicon dioxide in the mixed resin. In addition, the co-dispersed resin is also very important. According to the inventor's experiments, in the present invention, only the two-component polyurethane coating prepared using polycarbonate polyol as the co-dispersed resin has good tensile and wear resistance. The coating prepared by replacing it with other resins cannot have both properties.

[0010] Preferably, the raw materials of component A include, by mass, 5-15 parts of polycarbonate polyol, 45-55 parts of organic solvent, 0.3-0.8 parts of silane coupling agent, 10-20 parts of polyester polyol, 5-15 parts of polycaprolactone polyol, 15-25 parts of silicone polyol, and 10-20 parts of acrylic resin polyol; the raw materials of component B include, by mass, 5-10 parts of auxiliary agent and 25-35 parts of organic solvent.

[0011] Furthermore, the solid content of the nano-silicon dioxide dispersion is 10-30%. The solid content here refers to the ratio of the mass of nano-silicon dioxide to the sum of the mass of polycarbonate polyol, organic solvent and silane coupling agent. Too much nano-silicon dioxide may cause the coating liquid to have a bad appearance, such as reduced glossiness and transmittance.

[0012] Preferably, the auxiliary agent includes a curing agent, a dispersant and a leveling agent.

[0013] Furthermore, the curing agent is TDI-80, the dispersing agent is BYK-163, and the leveling agent is BYK-333. The selection of these additives can ensure the curing effect, dispersibility and leveling of the mixed resin.

[0014] Preferably, the organic solvent is toluene, which can ensure the fluidity, adhesion and drying speed of the mixed resin.

[0015] Preferably, in the selection of polymers, polycarbonate polyols with excellent mechanical properties, hydrolysis resistance, heat resistance, oxidation resistance, and wear resistance, as well as polycaprolactone polyols with stable activity, low viscosity, controllable molecular weight distribution, narrow distribution, low acid value and water content, and acrylic resin polyols with excellent weather resistance are selected to improve the performance of the coating.

[0016] In a second aspect, the present invention provides a method for preparing the two-component polyurethane elastic wear-resistant coating modified by silica nanoparticles, comprising the following steps:

[0017] Step 1: Preparation of nano-silicon dioxide dispersion: using a high-speed dispersing and grinding method to mix nano-silicon dioxide with polycarbonate polyol, an organic solvent and a silane coupling agent to prepare a uniformly dispersed and transparent nano-silicon dioxide dispersion;

[0018] Step 2, preparation of mixed resin: After mixing the nano-silicon dioxide dispersion with other raw materials of component A (i.e. polyester polyol, polycaprolactone polyol, silicone polyol and acrylic resin polyol), the mixture is mixed with the raw materials of component B (i.e. auxiliary agent and organic solvent) to obtain a mixed resin; the mixing order will also affect the dispersion effect. The present invention avoids the problem of reduced dispersion effect caused by too low viscosity of the coating liquid due to one-time mixing by mixing in steps;

[0019] Step 3: Preparation of coating: coating the mixed resin on the substrate, heating and curing to obtain a flexible wear-resistant self-repairing coating with high elongation, high wear resistance and excellent weather resistance.

[0020] In a third aspect, the present invention provides an application of the two-component polyurethane elastic wear-resistant coating modified by silica nanoparticles, which can be specifically applied as a self-repairing coating in car cover films.

[0021] The present invention has the following beneficial effects:

[0022] 1. The present invention prepares nano-silicon dioxide dispersion, and by adding a silane coupling agent, the nano-silicon dioxide can be evenly dispersed in the polycarbonate polyol, thereby improving the hardness and wear resistance of the coating. The coating is not easy to be scratched during normal construction and use, thereby reducing the post-construction processing process and improving the appearance of the product.

[0023] 2. The introduction of polyester polyol, polycarbonate polyol and polycaprolactone polyol in the mixed resin component of the present invention enables the coating to achieve a balance between elongation and wear resistance. Specifically, the introduction of polyester polyol can balance the oil-water balance of the system, ensure sufficient hydrophobicity while maintaining a high surface tension, thereby improving the elongation of the coating. The introduction of polycarbonate polyol and polycaprolactone polyol improves the wear resistance of the coating.

[0024] 3. The introduction of the organosilicon polyol in the mixed resin component of the present invention improves the weather resistance and air permeability of the coating. Specifically, the linear polydimethylsiloxane structure with alcoholic hydroxyl groups at both ends of the organosilicon polyol makes the glass transition temperature low and relatively soft, thereby improving the weather resistance of the coating.

[0025] 4. The introduction of acrylic resin polyol in the mixed resin component of the present invention makes the coating have excellent weather resistance and excellent bonding strength with the adhesive, and can have good wetting and bonding strength even without corona treatment.

[0026] In general, compared with the prior art, the present invention not only improves the hardness and wear resistance of the coating, but also achieves a balance between elongation and wear resistance, thus having a wider application prospect in practical applications. DETAILED DESCRIPTION

[0027] The present invention is further described below in conjunction with specific embodiments.

[0028] Example 1

[0029] Step 1: Preparation of nano-silicon dioxide dispersion. First, nano-silicon dioxide (particle size of 20 nanometers) is mixed with polycarbonate polyol (model NL1030B), toluene solvent and silane coupling agent (KH550). The mass of polycarbonate polyol is 10 grams, the mass of toluene solvent is 50 grams, and the mass of silane coupling agent is 0.5 grams. Then, the mixture is evenly dispersed by high-speed dispersion grinding to prepare a nano-silicon dioxide dispersion with a solid content of 20%.

[0030] Step 2: Preparation of mixed resin. Mix polyester polyol (model PETS-1000), nano-silicon dioxide dispersion obtained in step 1, polycaprolactone polyol (model PCL-1000), silicone polyol (model DMS-500) and acrylic resin polyol (model ACR-200). Among them, the mass of polyester polyol is 15 grams, the mass of polycaprolactone polyol is 10 grams, the mass of silicone polyol is 20g, and the mass of acrylic resin polyol is 15g. Then add curing agent (TDI-80), dispersant (BYK-163), leveling agent (BYK-333) and toluene solvent. Among them, the mass of curing agent is 5 grams, the mass of dispersant is 0.5 grams, the mass of leveling agent is 0.3 grams, and the mass of toluene solvent is 30g.

[0031] Step 3: Preparation of coating. The mixed resin is coated on the substrate, which is a common steel plate. During the coating process, the thickness of the coating is controlled to be 1 mm. Then, the coated substrate is placed in an oven and cured at a temperature of 100°C for 2 minutes.

[0032] Through the above steps, a flexible wear-resistant self-repairing coating with high elongation, high wear resistance and excellent weather resistance is obtained. The inventors compared the performance of the coating obtained in this embodiment with the coating on the market, including wear resistance and elongation. The wear resistance test method is: load 800g, use Martindale abrasion tester to test the gloss of the coating at the beginning and after friction with emery cloth (3M, model 281Q, 9 micron dry and wet emery cloth), the test speed is 45 times / min. The test results are shown in the following table. It can be seen that the coating of the present invention is significantly better than the coating on the market in terms of wear resistance and tensile properties.

[0033]

[0034] This specific implementation is only an explanation of the present invention, not a limitation of the present invention. Any changes made by those skilled in the art after reading the specification of the present invention will be protected by the patent law as long as they are within the scope of the claims of the present invention.

Claims

1. A two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles, characterized in that: The invention is prepared by mixing and curing component A and component B; the component A comprises nano-silicon dioxide dispersion, polyester polyol, polycaprolactone polyol, silicone polyol and acrylic resin polyol; the nano-silicon dioxide dispersion is a mixture of nano-silicon dioxide, polycarbonate polyol, organic solvent and silane coupling agent; the component B comprises an auxiliary agent and an organic solvent.

2. The two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles according to claim 1, characterized in that: The particle size of the nano silicon dioxide is 10-50nm.

3. The two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles according to claim 2, characterized in that: The raw materials of component A include, by mass, 5-15 parts of polycarbonate polyol, 45-55 parts of organic solvent, 0.3-0.8 parts of silane coupling agent, 10-20 parts of polyester polyol, 5-15 parts of polycaprolactone polyol, 15-25 parts of silicone polyol and 10-20 parts of acrylic resin polyol; the raw materials of component B include, by mass, 5-10 parts of auxiliary agent and 25-35 parts of organic solvent.

4. The two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles according to claim 3, characterized in that: The solid content of the nano silicon dioxide dispersion is 10-30%.

5. The two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles according to claim 1, characterized in that: The auxiliary agents include a curing agent, a dispersant and a leveling agent.

6. The two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles according to claim 5, characterized in that: The curing agent is TDI-80, the dispersing agent is BYK-163, and the leveling agent is BYK-333.

7. The two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles according to claim 1, characterized in that: The organic solvent is toluene.

8. The two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles according to any one of claims 1 to 7, characterized in that: The preparation method comprises the following steps: Step 1: Preparation of nano-silicon dioxide dispersion: using a high-speed dispersing and grinding method to mix nano-silicon dioxide with polycarbonate polyol, an organic solvent and a silane coupling agent to prepare a uniformly dispersed and transparent nano-silicon dioxide dispersion; Step 2, preparation of mixed resin: mixing the nano-silicon dioxide dispersion with other raw materials of component A, and then mixing with the raw materials of component B to obtain a mixed resin; Step 3: Preparation of coating: Apply the mixed resin on the substrate, heat and cure it to obtain a flexible, wear-resistant and self-repairing coating.

9. Use of the two-component polyurethane elastic wear-resistant coating modified by silicon dioxide nanoparticles as claimed in claim 8 in car cover films.

Citation Information

Patent Citations

  • Thermoplastic polyurethane elastomer nanocomposite and preparation method thereof

    CN114369220A

  • Fluoride-free bio-based polyurethane coating and preparation method thereof

    CN115612389A

  • Transparent coating composition for prepairing automobile

    KR1020160113346A

  • Coated substrate having enhanced scratch and mar resistance

    US20080160289A1

  • Transparent coating compositions containing nanoscale particles and having improved scratch resistance

    US6020419A

Cited By

  • Environment-friendly copolymer artificial leather and preparation process thereof

    CN120056548A