Waterproof structure of coal mine tunnel roof and waterproof construction method
Through the combination of multi-layer waterproof design and grid cloth, the problem of easy aging and difficult maintenance of the waterproof structure of the coal mine mine roof is solved, achieving a more stable and long-term waterproof effect, enhancing the waterproof performance and service life.
Patent Information
- Application Number
- CN202411100390.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-22
AI Technical Summary
The waterproof structure of the roof of the existing coal mine mine road is easily affected by environmental factors and is difficult to repair. The waterproof coatings have strict requirements on the base layer and construction, resulting in unstable waterproof performance and short service life.
Adopt a multi-layer waterproof design, including polymer waterproof base treatment agent, sealing layer, waterproof coil, waterproof coating and protective layer, combined with grid cloth, enhance waterproof performance through multi-layer structure and protective devices, and through specific construction steps For example, the flame spray gun heating and sealing paste are tightly embedded to ensure the integrity of the waterproof layer.
It effectively extends the service life of the waterproof layer, reduces the risk of cracks and water seepage, improves the comprehensiveness and stability of waterproof performance, reduces the difficulty of maintenance, and enhances the erosion resistance of the waterproof layer.
Smart Images

Figure CN118997804A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of coal mine waterproofing, and in particular to a waterproofing structure of a coal mine tunnel roof and a waterproofing construction method. Background Art
[0002] Water seepage in the mine roof is a problem often encountered in coal mine production. If it is not handled in time, it will seriously affect the safe production of the mine. Waterproof materials can be covered on the tunnel roof to prevent water from seeping in. Waterproof coatings or waterproof membranes with low permeability are preferred. However, waterproof coatings or waterproof membranes alone cannot guarantee the comprehensiveness of waterproofing, and are easily affected by environmental factors and age, crack and fall off. They have a short service life and cannot maintain the waterproof effect for a long time. In addition, waterproof membranes are difficult to repair. Damage, degumming, and leakage in any part will lead to the loss of the waterproof function of the entire connected layer. If the damaged and defective parts cannot be found, the waterproof membrane can only be re-laid. The requirements of waterproof coatings on the base and construction are relatively strict. If the required requirements are not met, the waterproof performance will be greatly reduced. Summary of the invention
[0003] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a waterproof structure and a waterproof construction method for a coal mine tunnel roof. The waterproof structure and the waterproof construction method for the coal mine tunnel roof are intended to solve the technical problems that the prior art is easily affected by environmental factors and ages, the waterproof membrane is difficult to maintain, and the waterproof coating has relatively strict requirements on the base and construction.
[0004] The technical solution of the present invention is: a waterproof structure of a coal mine tunnel roof, including a first treated layer; also including a second treated layer, a sealing layer, a waterproof coiled material, a first waterproof coating, a second waterproof coating, a protective layer and a mesh cloth; the second treated layer, the sealing layer, the waterproof coiled material, the first waterproof coating, the second waterproof coating and the protective layer are sequentially arranged on the upper end of the first treated layer; a mesh cloth is arranged in the protective layer.
[0005] Preferably, both the first treatment layer and the second treatment layer are polymer waterproof base treatment agents, the thickness of the first treatment layer is 0.8 to 1 mm, and the thickness of the second treatment layer is 0.5 to 0.8 mm.
[0006] Preferably, the sealing layer is made of epoxy primer, polyurethane primer or acrylic primer, and the thickness of the sealing layer is 1 to 2 mm.
[0007] Preferably, the waterproofing membrane is an SBS modified asphalt waterproofing membrane or an APP modified asphalt waterproofing membrane, and the thickness of the waterproofing membrane is 1.2 to 5 mm.
[0008] Preferably, the materials of the first waterproof coating and the second waterproof coating are asphalt coating, polyurethane coating or acrylic coating, and the sum of the thicknesses of the first waterproof coating and the second waterproof coating is 1.5 to 2 mm.
[0009] Preferably, the material of the protective layer is concrete, and the thickness of the protective layer is 3 to 8 mm.
[0010] A waterproof construction method for a waterproof structure of a coal mine tunnel roof, comprising the waterproof structure of a coal mine tunnel roof as described above, and the steps are as follows:
[0011] Step 1: Clean the surface of the mine roof, remove floating dust, oil stains and dust, and level the uneven parts to ensure that the surface of the roof is flat;
[0012] Step 2: Apply a polymer waterproof base treatment agent on the top plate to form a first treatment layer after solidification, and apply a polymer waterproof base treatment agent on the surface of the first treatment layer in a direction perpendicular to the direction of the first treatment layer, and form a second treatment layer after solidification;
[0013] Step 3: Apply epoxy primer, polyurethane primer or acrylic primer and wait for it to dry to form a sealing layer;
[0014] Step 4: Cut the SBS modified asphalt waterproofing membrane or APP modified asphalt waterproofing membrane into the corresponding size, heat it back and forth evenly with a flame spray gun when paving, roll and paste the waterproofing membrane forward when it is just melted, heat the overlapping part of the waterproofing membrane with a spray gun, and make the two firmly bonded while hot, until the asphalt is squeezed out of the edge, and fill the end tightly with sealing paste;
[0015] Step 5: Apply asphalt paint, polyurethane paint or acrylic paint on the surface of the waterproof membrane to form a first waterproof coating after it is completely dried. Then apply asphalt paint, polyurethane paint or acrylic paint on the surface of the first waterproof coating to form a second waterproof coating after it is completely dried.
[0016] Step six: Pour concrete on the surface of the second waterproof coating, put mesh cloth into the concrete, and then continue pouring to completely wrap the mesh cloth. Start curing 12h to 18h after pouring, and the curing time lasts for 21 to 28 days. After curing, a protective layer is formed to obtain a complete waterproof structure.
[0017] Preferably, the pouring requirements of the protective layer are: completely covering the second waterproof coating, without omissions, cracks, bubbles, or falling off.
[0018] Preferably, the concrete curing methods include natural curing by sprinkling water, spraying film curing and plastic film wrapping curing.
[0019] Beneficial effects of the present invention:
[0020] 1. The overall multi-layer waterproof design further ensures the comprehensiveness of the waterproof performance. A protective device is also provided on the outside of the waterproof layer to resist the erosion and damage of the waterproof layer by the natural environment, delay the aging of the waterproof layer, and further increase the service life of the waterproof layer;
[0021] 2. The use of mesh cloth can reduce the chance of cracking of the protective layer, greatly reduce the cracking phenomenon, ensure the integrity of the waterproof membrane, and through the use of the first waterproof coating and the second waterproof coating, it plays a role in waterproofing, anti-seepage and protection, avoiding the problem of water seepage in the gaps caused by missed brushing. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 Shown is a schematic diagram of the cross-sectional structure of the waterproof structure of the roof of a coal mine tunnel according to the present invention.
[0023] Explanation of the accompanying drawings: 1. First treatment layer; 2. Second treatment layer; 3. Sealing layer; 4. Waterproof membrane; 5. First waterproof coating layer; 6. Second waterproof coating layer; 7. Protective layer; 8. Mesh cloth. DETAILED DESCRIPTION
[0024] The present invention will be further described below in conjunction with the accompanying drawings and embodiments.
[0025] Example 1
[0026] See also Figure 1 The present invention provides an embodiment: a waterproof structure of a coal mine tunnel roof, comprising a first treated layer 1; further comprising a second treated layer 2, a sealing layer 3, a waterproof coiled material 4, a first waterproof coating 5, a second waterproof coating 6, a protective layer 7 and a mesh cloth 8; the second treated layer 2, the sealing layer 3, the waterproof coiled material 4, the first waterproof coating 5, the second waterproof coating 6 and the protective layer 7 are sequentially arranged on the upper end of the first treated layer 1; a mesh cloth 8 is arranged inside the protective layer 7.
[0027] A waterproof construction method for a waterproof structure of a coal mine tunnel roof, comprising the waterproof structure of a coal mine tunnel roof as described above, and the steps are as follows:
[0028] Step 1: Clean the surface of the mine roof, remove floating dust, oil stains and dust, and level the uneven parts to ensure that the surface of the roof is flat;
[0029] Step 2: Apply a polymer waterproof base treatment agent on the top plate to form a first treatment layer 1 after solidification, and apply a polymer waterproof base treatment agent on the surface of the first treatment layer 1 in a direction perpendicular to the direction of the first treatment layer 1, and form a second treatment layer 2 after solidification;
[0030] Step 3: Apply epoxy primer and wait for it to dry to form a sealing layer 3;
[0031] Step 4: Cut the SBS modified asphalt waterproofing membrane into the corresponding size, heat it evenly with a flame spray gun when paving, roll and paste the waterproofing membrane 4 forward when it just melts, heat the overlapping part of the waterproofing membrane 4 with a spray gun, and make the two firmly bonded while hot, until the asphalt is squeezed out of the edge, and fill the end tightly with sealing paste;
[0032] Step 5: Apply asphalt paint on the surface of the waterproof coiled material 4 to form a first waterproof coating 5 after it is completely dried, and then apply asphalt paint on the surface of the first waterproof coating 5 to form a second waterproof coating 6 after it is completely dried;
[0033] Step six: pour concrete on the surface of the second waterproof coating 6, put the mesh cloth 8 into the concrete, and then continue pouring to completely wrap the mesh cloth 8. Start curing 12 hours after pouring, and the curing time lasts for 21 days. After curing, a protective layer 7 is formed to obtain a complete waterproof structure.
[0034] Example 2
[0035] See also Figure 1 The present invention provides an embodiment: a waterproof structure of a coal mine tunnel roof, comprising a first treated layer 1; further comprising a second treated layer 2, a sealing layer 3, a waterproof coiled material 4, a first waterproof coating 5, a second waterproof coating 6, a protective layer 7 and a mesh cloth 8; the second treated layer 2, the sealing layer 3, the waterproof coiled material 4, the first waterproof coating 5, the second waterproof coating 6 and the protective layer 7 are sequentially arranged on the upper end of the first treated layer 1; a mesh cloth 8 is arranged inside the protective layer 7.
[0036] A waterproof construction method for a waterproof structure of a coal mine tunnel roof, comprising the waterproof structure of a coal mine tunnel roof as described above, and the steps are as follows:
[0037] Step 1: Clean the surface of the mine roof, remove floating dust, oil stains and dust, and level the uneven parts to ensure that the surface of the roof is flat;
[0038] Step 2: Apply a polymer waterproof base treatment agent on the top plate to form a first treatment layer 1 after solidification, and apply a polymer waterproof base treatment agent on the surface of the first treatment layer 1 in a direction perpendicular to the direction of the first treatment layer 1, and form a second treatment layer 2 after solidification;
[0039] Step 3: Apply polyurethane primer and wait for it to dry to form a sealing layer 3;
[0040] Step 4: Cut the APP modified asphalt waterproofing membrane into the corresponding size, heat it back and forth evenly with a flame spray gun when paving, roll and paste the waterproofing membrane 4 forward when the waterproofing membrane 4 just melts, heat the overlapping part of the waterproofing membrane 4 with a spray gun, and make the two firmly bonded while hot, with asphalt squeezed out of the edge, and fill the end tightly with sealing paste;
[0041] Step 5: Apply polyurethane coating on the surface of the waterproof coiled material 4 to form a first waterproof coating 5 after it is completely dried, and then apply polyurethane coating on the surface of the first waterproof coating 5 to form a second waterproof coating 6 after it is completely dried;
[0042] Step six: pour concrete on the surface of the second waterproof coating 6, put the mesh cloth 8 into the concrete, and then continue pouring to completely wrap the mesh cloth 8. Start curing 18 hours after pouring and the curing time lasts for 28 days. After curing, a protective layer 7 is formed to obtain a complete waterproof structure.
[0043] Example 3
[0044] See also Figure 1 The present invention provides an embodiment: a waterproof structure of a coal mine tunnel roof, comprising a first treated layer 1; further comprising a second treated layer 2, a sealing layer 3, a waterproof coiled material 4, a first waterproof coating 5, a second waterproof coating 6, a protective layer 7 and a mesh cloth 8; the second treated layer 2, the sealing layer 3, the waterproof coiled material 4, the first waterproof coating 5, the second waterproof coating 6 and the protective layer 7 are sequentially arranged on the upper end of the first treated layer 1; a mesh cloth 8 is arranged inside the protective layer 7.
[0045] A waterproof construction method for a waterproof structure of a coal mine tunnel roof, comprising the waterproof structure of a coal mine tunnel roof as described above, and the steps are as follows:
[0046] Step 1: Clean the surface of the mine roof, remove floating dust, oil stains and dust, and level the uneven parts to ensure that the surface of the roof is flat;
[0047] Step 2: Apply a polymer waterproof base treatment agent on the top plate to form a first treatment layer 1 after solidification, and apply a polymer waterproof base treatment agent on the surface of the first treatment layer 1 in a direction perpendicular to the direction of the first treatment layer 1, and form a second treatment layer 2 after solidification;
[0048] Step 3: Apply acrylic primer and wait for it to dry to form a sealing layer 3;
[0049] Step 4: Cut the SBS modified asphalt waterproofing membrane into the corresponding size, heat it evenly with a flame spray gun when paving, roll and paste the waterproofing membrane 4 forward when it just melts, heat the overlapping part of the waterproofing membrane 4 with a spray gun, and make the two firmly bonded while hot, until the asphalt is squeezed out of the edge, and fill the end tightly with sealing paste;
[0050] Step 5: Apply acrylic paint on the surface of the waterproof coiled material 4 to form a first waterproof coating 5 after it is completely dried, and then apply acrylic paint on the surface of the first waterproof coating 5 to form a second waterproof coating 6 after it is completely dried;
[0051] Step six: pour concrete on the surface of the second waterproof coating 6, put the mesh cloth 8 into the concrete, and then continue pouring to completely wrap the mesh cloth 8. Start curing 16 hours after pouring and the curing time lasts for 24 days. After curing, a protective layer 7 is formed to obtain a complete waterproof structure.
[0052] Table 1 is a table of performance indicators of the waterproof structures of Examples 1, 2 and 3 of the present invention.
[0053]
[0054] Table 1
[0055] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of those skilled in the art without departing from the spirit of the present invention.
Claims
1. A waterproof structure for a roof of a coal mine, comprising a first treated layer (1); characterized in that: The invention also comprises a second treated layer (2), a sealing layer (3), a waterproof coiled material (4), a first waterproof coating (5), a second waterproof coating (6), a protective layer (7) and a mesh cloth (8); the second treated layer (2), the sealing layer (3), the waterproof coiled material (4), the first waterproof coating (5), the second waterproof coating (6) and the protective layer (7) are arranged in sequence on the upper end of the first treated layer (1); and the mesh cloth (8) is arranged inside the protective layer (7).
2. The waterproof structure of the roof of a coal mine tunnel according to claim 1, characterized in that: The first treatment layer (1) and the second treatment layer (2) are both polymer waterproof base treatment agents. The thickness of the first treatment layer (1) is 0.8 to 1 mm, and the thickness of the second treatment layer (2) is 0.5 to 0.8 mm.
3. The waterproof structure of a coal mine tunnel roof according to claim 1, characterized in that: The material of the sealing layer (3) is epoxy primer, polyurethane primer or acrylic primer, and the thickness of the sealing layer (3) is 1 to 2 mm.
4. The waterproof structure of a coal mine tunnel roof according to claim 1, characterized in that: The waterproofing roll (4) is an SBS modified asphalt waterproofing roll or an APP modified asphalt waterproofing roll, and the thickness of the waterproofing roll (4) is 1.2 to 5 mm.
5. The waterproof structure of the roof of a coal mine tunnel according to claim 1, characterized in that: The materials of the first waterproof coating (5) and the second waterproof coating (6) are asphalt coating, polyurethane coating or acrylic coating, and the sum of the thicknesses of the first waterproof coating (5) and the second waterproof coating (6) is 1.5 to 2 mm.
6. The waterproof structure of the roof of a coal mine tunnel according to claim 1, characterized in that: The material of the protective layer (7) is concrete, and the thickness of the protective layer (7) is 3 to 8 mm.
7. A waterproof construction method for a waterproof structure of a coal mine tunnel roof, characterized in that The waterproof structure of the roof of a coal mine tunnel according to claim 1 comprises the following steps: Step 1: Clean the surface of the mine roof, remove floating dust, oil stains and dust, and level the uneven parts to ensure that the surface of the roof is flat; Step 2: Applying a polymer waterproof base treatment agent on the top plate to form a first treatment layer (1) after solidification, applying a polymer waterproof base treatment agent on the surface of the first treatment layer (1) in a direction perpendicular to the direction of the first treatment layer (1), and forming a second treatment layer (2) after solidification; Step 3: Apply epoxy primer, polyurethane primer or acrylic primer, and wait for it to dry to form a sealing layer (3); Step 4: Cut the SBS modified asphalt waterproofing membrane or APP modified asphalt waterproofing membrane into corresponding sizes, heat it back and forth evenly with a flame spray gun when paving, roll and paste the waterproofing membrane (4) forward when the waterproofing membrane (4) has just melted, heat the overlapping part of the waterproofing membrane (4) with a spray gun, and make the two adhere firmly while hot, until the asphalt is squeezed out of the edge, and fill the end tightly with sealing paste; Step 5: Brushing asphalt paint, polyurethane paint or acrylic paint on the surface of the waterproof coiled material (4) to form a first waterproof coating (5) after it is completely dried, and then brushing asphalt paint, polyurethane paint or acrylic paint on the surface of the first waterproof coating (5) to form a second waterproof coating (6) after it is completely dried; Step 6: Pour concrete on the surface of the second waterproof coating (6), put the mesh cloth (8) into the concrete, and then continue pouring to completely wrap the mesh cloth (8). Start curing 12h to 18h after pouring, and the curing time lasts for 21 to 28 days. After curing, a protective layer (7) is formed to obtain a complete waterproof structure.
8. The waterproof construction method for the waterproof structure of the roof of a coal mine tunnel according to claim 7 is characterized by: The requirements for pouring the protective layer (7) are: completely covering the second waterproof coating (6), without omissions, cracks, bubbles, or falling off.
9. The waterproof construction method for the waterproof structure of the roof of a coal mine tunnel according to claim 8, characterized in that: Concrete curing methods include natural curing by sprinkling water, spraying film curing and plastic film wrapping curing.