High-temperature-resistant nonmetal expansion joint
By using multi-layer skin and thermal insulation pads in non-metal expansion joints, combined with stainless steel frame and bolt components, the problems of insufficient radial compensation amount and poor high temperature resistance of the existing expansion joints are solved, and the system is improved Reliability and safety reduce environmental pollution and maintenance workload.
Patent Information
- Application Number
- CN202411351621.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-26
- Publication Date
- 2024-11-22
AI Technical Summary
The existing non-metal expansion joints in the ash sulfur flue of power plants have insufficient radial compensation, carbon steel frames are not resistant to corrosion, and poor skin resistance to high temperatures, resulting in air leakage, environmental pollution and safety hazards.
It adopts multi-layer structure skin and thermal insulation pads, combined with 316L stainless steel frame, tie rods and ear plates, to enhance the corrosion resistance and high temperature resistance of the expansion joints, and is fixedly connected through bolt components to increase the radial compensation.
It significantly improves the system operation reliability, reduces environmental pollution and maintenance workload caused by air leakage, eliminates safety hazards caused by corrosion, and ensures the stable operation of the equipment.
Smart Images

Figure CN118998490A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of expansion pieces, and in particular relates to a high temperature resistant non-metal expansion joint. Background Art
[0002] Expansion joints are flexible structures installed on container shells or pipelines to compensate for additional stress caused by temperature differences and mechanical vibrations. They absorb dimensional changes caused by thermal expansion and contraction of pipelines, ducts, containers, etc., or compensate for axial, lateral and angular displacements of pipelines, ducts, containers, etc. They have the advantages of reliable operation, good performance and compact structure, and have been widely used in chemical, metallurgical, nuclear power plants and other departments.
[0003] The non-metallic fabric expansion joints in the electrostatic precipitator part of the power plant's ash-sulfur flue have insufficient radial compensation, non-corrosion-resistant carbon steel frames, and poor high-temperature resistance of ordinary skins, resulting in multiple tears and damage on the outer surface of the skin, deformation of the guide plates, and serious air leakage. The increased oxygen content after the leakage caused an increase in the converted value of environmental protection parameters, posing an environmental risk and affecting the economy of the unit. After the expansion joint leaks, it can only be temporarily handled, which increases the workload of maintenance personnel. The leakage also causes serious corrosion of the insulation around the expansion joint, posing a risk of falling and injuring people. Summary of the invention
[0004] The object of the present invention is to provide a high-temperature resistant non-metal expansion joint which has sufficient radial compensation, is corrosion-resistant, high-temperature resistant and safer.
[0005] In order to achieve the above object, the present invention provides the following technical solutions: A high temperature resistant non-metal expansion joint, characterized in that it comprises a tie rod, a frame and an expansion joint body, wherein a pair of ear plates are fixedly connected at both ends of the tie rod, a pressure plate is fixedly arranged at the bottom of the ear plate, and the edge of the expansion joint body is arranged between the clamping plate and the frame; the clamping plate, the expansion joint body and the frame are fixedly connected by a bolt assembly; The expansion joint body includes a skin and a thermal insulation pad, and the thermal insulation pad is arranged inside the skin; the skin is composed of, from outside to inside: a layer of integral vulcanized fluororubber cloth with two cloths and three rubbers sandwiched between stainless steel wires, two layers of Kevlar Teflon, a layer of polytetrafluoroethylene membrane, two layers of alkali-free glass fiber cloth, a layer of polytetrafluoroethylene membrane, two layers of Teflon, and a layer of integral vulcanized fluororubber cloth with two cloths and three rubbers sandwiched between stainless steel wires; the fluororubber content of the integral vulcanized fluororubber cloth with two cloths and three rubbers sandwiched between stainless steel wires is greater than 70%.
[0006] Furthermore, the thickness of the stainless steel wire sandwiched two cloths and three rubbers integral vulcanized fluororubber cloth is 3 mm, the thickness of the tetrafluoro film is 0.8 mm, the thickness of the Teflon is 1.5 mm, the thickness of the alkali-free glass fiber cloth is 2 mm, and the thickness of the Kevlar Teflon is 1.5 mm.
[0007] Furthermore, the thermal insulation pad includes a layer of aluminum silicate ceramic fiber wool and two layers of stainless steel wire glass fiber cloth wrapped on the outside thereof; the aluminum silicate ceramic fiber wool has a thickness of 200 mm; The thickness of the stainless steel wire glass fiber cloth is not less than 3.5mm, and the density is not less than 2700g / m 2 The warp and weft density of stainless steel wire is not less than 18×9 / cm 2 .
[0008] Furthermore, the frame, the pull rod, the ear plate and the auxiliary installation materials are all made of 316L stainless steel.
[0009] Furthermore, the radial compensation amount of the high temperature resistant non-metallic expansion joint is 550 mm.
[0010] The beneficial effects of the present invention are: It solves the problems of air leakage and damage caused by insufficient radial compensation, non-corrosion resistance of carbon steel frame, and poor high temperature resistance of the skin in existing expansion joints. It greatly improves the reliability of system operation, effectively reduces environmental pollution caused by air leakage, improves the working environment of personnel, reduces the workload of maintenance personnel, eliminates the hidden dangers of falling and injuring people due to severe corrosion, and ensures the safe and stable operation of equipment.
[0011] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention and implement it according to the contents of the specification, the following is a detailed description of the preferred embodiments of the present invention in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 The figure is a schematic structural diagram of a high temperature resistant non-metallic expansion joint according to an embodiment of the present invention.
[0013] Explanation of the accompanying figures: 1. Ear plate; 2. Pull rod; 3. Expansion joint body; 4. Pressure plate; 5. Frame. DETAILED DESCRIPTION
[0014] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0015] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0016] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0017] In addition, the technical features involved in the different embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0018] See also Figure 1 The high temperature resistant non-metallic expansion joint shown in a preferred embodiment of the present application includes a pull rod 2, a frame 5 and an expansion joint body 3, a pair of ear plates 1 are fixedly connected at both ends of the pull rod 2, a pressure plate 4 is fixedly arranged at the bottom of the ear plate 1, and the pressure plate 4 and the frame 5 clamp the expansion joint body 3 and are fixedly connected with a bolt assembly.
[0019] The expansion joint body 3 includes a skin and a thermal insulation pad, which is arranged inside the skin; the skin has a total of ten layers, from outside to inside: a layer of stainless steel wire sandwiched two cloths and three rubbers integral vulcanized fluororubber cloth, two layers of Kevlar Teflon, a layer of polytetrafluoroethylene membrane, two layers of alkali-free glass fiber cloth, a layer of polytetrafluoroethylene membrane, two layers of Teflon, and a layer of stainless steel wire sandwiched two cloths and three rubbers integral vulcanized fluororubber cloth; among them, the fluororubber content of the stainless steel wire sandwiched two cloths and three rubbers integral vulcanized fluororubber cloth is greater than 70%.
[0020] Preferably, the thickness of the integral vulcanized fluororubber cloth with two cloths and three rubbers sandwiched with stainless steel wire is 3 mm, the thickness of the tetrafluoro film is 0.8 mm, the thickness of Teflon is 1.5 mm, the thickness of the alkali-free glass fiber cloth is 2 mm, and the thickness of Kevlar Teflon is 1.5 mm.
[0021] The thermal insulation pad includes a layer of aluminum silicate ceramic fiber wool and two layers of stainless steel wire glass fiber cloth wrapped on the outside. The thickness of the aluminum silicate ceramic fiber wool is 200mm, the thickness of the stainless steel wire glass fiber cloth is not less than 3.5mm, and the density is not less than 2700g / m2 The warp and weft density of stainless steel wire is not less than 18×9 / cm 2 .
[0022] The frame 5, tie rod 2, ear plate 1, bolts and other auxiliary materials are all made of 316L stainless steel to enhance the overall corrosion resistance of the expansion joint and ensure its service life.
[0023] Furthermore, the present application increases the radial compensation amount of the expansion joint to 550 mm to prevent the maintenance costs and safety hazards caused by damage to the expansion joint skin after long-term operation.
[0024] In summary, the present invention greatly enhances the corrosion resistance and high temperature resistance of the expansion joint by using a multi-layer structure of skin and thermal insulation pads, as well as a stainless steel frame and auxiliary materials. At the same time, the radial compensation amount is increased from 250mm to 550mm, thereby improving the reliability of the operating system, reducing the workload of maintenance personnel and avoiding environmental pollution.
[0025] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0026] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. High temperature resistant non-metal expansion joint, characterized by: It includes a pull rod, a frame and an expansion joint body, wherein a pair of ear plates are fixedly connected at both ends of the pull rod, a pressure plate is fixedly arranged at the bottom of the ear plate, and the edge of the expansion joint body is arranged between the clamping plate and the frame; the clamping plate, the expansion joint body and the frame are connected by a bolt assembly; The expansion joint body includes a skin and a thermal insulation pad, and the thermal insulation pad is arranged inside the skin; the skin is composed of, from outside to inside: a layer of integral vulcanized fluororubber cloth with two cloths and three rubbers sandwiched between stainless steel wires, two layers of Kevlar Teflon, a layer of polytetrafluoroethylene membrane, two layers of alkali-free glass fiber cloth, a layer of polytetrafluoroethylene membrane, two layers of Teflon, and a layer of integral vulcanized fluororubber cloth with two cloths and three rubbers sandwiched between stainless steel wires; the fluororubber content of the integral vulcanized fluororubber cloth with two cloths and three rubbers sandwiched between stainless steel wires is greater than 70%.
2. The high temperature resistant non-metal expansion joint according to claim 1, characterized in that: The thickness of the integral vulcanized fluororubber cloth with stainless steel wire sandwiched between two cloths and three rubbers is 3 mm, the thickness of the tetrafluoro film is 0.8 mm, the thickness of the Teflon is 1.5 mm, the thickness of the alkali-free glass fiber cloth is 2 mm, and the thickness of the Kevlar Teflon is 1.5 mm.
3. The high temperature resistant non-metal expansion joint according to claim 1, characterized in that: The thermal insulation pad includes a layer of aluminum silicate ceramic fiber wool and two layers of stainless steel wire glass fiber cloth wrapped outside the aluminum silicate ceramic fiber wool; the thickness of the aluminum silicate ceramic fiber wool is 200 mm; The thickness of the stainless steel wire glass fiber cloth is not less than 3.5mm, and the density is not less than 2700g / m 2 The warp and weft density of stainless steel wire is not less than 18×9 / cm 2 .
4. The high temperature resistant non-metal expansion joint according to claim 1, characterized in that: The frame, the pull rod, and the ear plate are all made of 316L stainless steel.
5. The high temperature resistant non-metal expansion joint according to claim 1, characterized in that: The radial compensation amount of the high temperature resistant non-metallic expansion joint is 550mm.
Citation Information
Cited By
High-temperature and high-pressure nonmetal expansion joint
CN119594270A
High-temperature and high-pressure nonmetal expansion joint
CN223294488U