Battery sealing nail welding quality detection method

By directly welding sealing elements after the battery is refilled with electrolyte and detecting pressure changes in a closed space, the problem of inaccurate helium detection in existing technologies is solved, and efficient and accurate quality inspection of sealing nail welding is achieved.

CN118999939APending Publication Date: 2024-11-22JIANGSU TIANHE ENERGY STORAGE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411185688.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In existing technologies, after the battery sealing nails are welded, the helium gas testing process can easily lead to the filling hole becoming blocked or insufficient overflow, resulting in the failure of the sealing test and the risk of leakage.

Method used

After the battery is refilled with electrolyte, a sealing element is directly used for welding, and a closed space is formed above the sealing element. The first gas is filled in and the pressure change is detected. If the pressure remains unchanged, the first gas is removed and the second gas is filled in. The pressure of the second gas is detected to determine the welding quality.

Benefits of technology

It improves the accuracy and efficiency of sealing nail welding quality inspection, reduces gas consumption and inspection time, lowers material costs, and ensures inspection accuracy and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118999939A_ABST
    Figure CN118999939A_ABST
Patent Text Reader

Abstract

The invention discloses a battery sealing nail welding quality detection method which specifically comprises the following steps: after secondary liquid injection of a battery, directly using a sealing element to weld the battery; sealing the space above the sealing element to form a sealed space; filling a first gas into the closed space, and detecting the pressure change; if the pressure is not changed, the first gas in the closed space is exhausted, and the closed space is filled with the second gas; and the pressure of the second gas in the closed space is detected, and the welding quality is judged. Helium does not need to be injected after secondary liquid injection of the battery, and defect detection can be directly and accurately carried out on the sealing nail area after the sealing element is used for welding, so that the detection precision can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of battery detection, and in particular to a method for detecting the welding quality of battery sealing nails. Background Art

[0002] At present, in the manufacturing process of square shell lithium batteries, generally after the secondary liquid injection of the battery, it is necessary to inject helium and then install a sealing rubber nail, and then use an aluminum sheet to weld and seal the liquid injection hole, and then use a helium detector to test the sealing performance of the welding. However, the rubber nail and the liquid injection hole usually have an interference fit, which can easily block the liquid injection hole, resulting in the helium injected into the battery being unable to overflow during the test; or the amount of helium overflowing is small, resulting in the failure of the sealing quality test of the sealing nail welding, causing the battery with poor welding to flow out, making the subsequent battery cell circulation process have a great risk of leakage.

[0003] Therefore, it is urgent to propose a battery sealing nail welding quality detection method to solve the above problems. Summary of the invention

[0004] The purpose of the present invention is to propose a battery sealing nail welding quality inspection method, which does not need to inject helium after the secondary liquid injection of the battery, and can directly and accurately perform defect inspection on the sealing nail area after welding with the sealing element, thereby improving the inspection accuracy.

[0005] In order to solve the above technical problems, the present invention provides a battery sealing nail welding quality detection method, which specifically includes the following:

[0006] After the battery is refilled, the battery is welded directly using the sealing element;

[0007] sealing the space above the sealing element to form a closed space; and

[0008] A first gas is filled into the closed space, and a pressure change is detected.

[0009] Furthermore, the sealing element includes a glue nail and a sealing nail.

[0010] Furthermore, after the secondary liquid injection of the battery, the sealing element is directly used to weld the battery, which specifically includes: applying glue nails after the secondary liquid injection of the battery, and then directly welding the sealing nails.

[0011] Furthermore, the space above the sealing element is sealed to form a closed space, which specifically includes: transferring the welded battery to a helium injection station, and sealing the space above the sealing pin in the closed space.

[0012] Furthermore, the step of filling the closed space with the first gas and detecting the pressure change specifically includes: filling the closed space with the first gas at a predetermined pressure, maintaining the pressure for a predetermined time, and then detecting the pressure change.

[0013] Furthermore, the predetermined pressure ranges from 1 to 3 bar.

[0014] Furthermore, the step of filling the closed space with the first gas and detecting the pressure change specifically includes: if the pressure cannot be maintained, determining that the welding is abnormal.

[0015] Furthermore, the method further includes: if the pressure remains unchanged, exhausting the first gas in the closed space and filling it with the second gas; detecting the pressure of the second gas in the closed space to judge the welding quality.

[0016] Furthermore, the first gas includes nitrogen; and the second gas includes helium.

[0017] Furthermore, if the pressure remains unchanged, the first gas in the closed space is removed and the second gas is filled in, which specifically includes: if the pressure remains unchanged, vacuuming the closed space to remove the first gas and maintaining the vacuum state; then filling the closed space with the second gas at a specified pressure and maintaining it for a specified time.

[0018] Furthermore, the specified pressure ranges from 2 to 5 bar.

[0019] Furthermore, the pressure of the second gas in the enclosed space is detected to judge the welding quality, specifically including: breaking the vacuum after the second gas reaches the pressure holding time, transferring the battery to the helium inspection station, and performing helium inspection after evacuating the enclosed space. If the helium leakage rate of the battery is greater than a predetermined parameter, it is determined to be unqualified and the welding has defects; if the helium leakage rate of the battery is less than or equal to the predetermined parameter, it is determined to be qualified and the welding has no defects.

[0020] Furthermore, the holding time ranges from 30 to 120 seconds.

[0021] Through the above technical solution, the present invention has the following beneficial effects:

[0022] After the battery is refilled with liquid, the sealing element is directly used to weld the battery; the space above the sealing element is sealed to form a closed space; the first gas is filled into the closed space to detect the pressure change; if the pressure remains unchanged, the first gas in the closed space is removed and the second gas is filled; and the pressure of the second gas in the closed space is detected to judge the welding quality. The present invention does not need to inject helium after the battery is refilled with liquid, and can directly and accurately detect defects in the sealing nail area after welding using the sealing element, which can improve the detection accuracy. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a flow chart of a method for detecting welding quality of battery sealing nails in one embodiment of the present invention;

[0024] Figure 2 This is a specific flow chart of a method for detecting welding quality of battery sealing nails in one embodiment of the present invention;

[0025] Figure 3 It is a structural schematic diagram of a battery located at a helium injection station in a battery sealing nail welding quality inspection method according to an embodiment of the present invention;

[0026] Figure 4 It is a structural schematic diagram of a battery located at a helium inspection station in a battery sealing nail welding quality inspection method in one embodiment of the present invention.

[0027] In the figure, 1, battery; 2, top cover; 3, rubber nails; 4, sealing nails; 5, closed space; 6, first gas; 7, second gas. DETAILED DESCRIPTION

[0028] A battery sealing nail welding quality detection method of the present invention will be described below in conjunction with a schematic diagram, wherein a preferred embodiment of the present invention is shown, and it should be understood that those skilled in the art can modify the present invention described herein while still achieving the advantageous effects of the present invention. Therefore, the following description should be understood as being widely known to those skilled in the art, and not as a limitation of the present invention.

[0029] The serial numbers of the components herein, such as "first", "second", etc., are only used to distinguish the objects described and do not have any order or technical meaning. The "connection" and "coupling" mentioned in this application, unless otherwise specified, include direct and indirect connections (couplings). In the description of the present invention, it should be understood that the orientation or positional relationship indicated by the terms "upper", "lower", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", etc. are based on the orientation or positional relationship shown in the accompanying drawings, which is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation to the present invention.

[0030] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0031] The present invention is described in more detail in the following paragraphs by way of example with reference to the accompanying drawings. The advantages and features of the present invention will become more apparent from the following description and claims. It should be noted that the drawings are in very simplified form and in non-precise proportions, and are only used to facilitate and clearly assist in illustrating the purpose of the embodiments of the present invention.

[0032] like Figure 1-Figure 2 As shown, the embodiment of the present invention proposes a battery sealing nail welding quality detection method, which specifically includes the following steps:

[0033] S1. After the battery 1 is filled with liquid for the second time, the battery 1 is directly welded using a sealing element (for example, the sealing element is welded to the top cover 2 of the battery 1);

[0034] S2, sealing the space above the sealing element to form a closed space 5 (for example, using a sealing cover to cover the sealing element to form the closed space 5); and

[0035] S3. Fill the closed space 5 with the first gas 6 and detect pressure changes.

[0036] This embodiment also includes the following steps: S4, if the pressure remains unchanged, exhausting the first gas 6 in the closed space 5 and filling it with the second gas 7; and S5, detecting the pressure of the second gas 7 in the closed space 5 to determine the welding quality.

[0037] In a specific example, the sealing element includes a glue nail 3 and a sealing nail 4. Those skilled in the art will appreciate that the sealing element can be selected according to actual needs, and can also include other embodiments besides the glue nail 3 and the sealing nail 4 in this embodiment.

[0038] In S1, after the battery 1 is filled with liquid for the second time, the sealing element is directly used to weld the battery 1, which specifically includes: applying glue nails 3 after the battery 1 is filled with liquid for the second time, and then directly welding the sealing nails 4. By directly using sealing elements for welding after the battery 1 is filled with liquid for the second time, additional steps and operations are reduced, and the entire process flow of manufacturing and testing of the battery 1 is simplified. Through direct welding, it can be ensured that the contact between the sealing nail 4 and the battery 1 shell is closer and the welding is more firm, thereby improving the overall quality of the welding. Welding the sealing nail 4 immediately after the battery 1 is filled with liquid for the second time can more effectively seal the interior of the battery 1, reduce the risk of gas leakage, and improve the sealing performance of the battery 1. In addition, direct welding reduces waiting time and operating steps, thereby shortening the production cycle and improving the efficiency and production capacity of the battery 1 production.

[0039] In S2, the space above the sealing element is sealed to form a closed space 5, which specifically includes: transferring the welded battery 1 to the helium injection station, and sealing the top of the sealing nail 4 in the closed space 5. By forming a closed space 5 above the sealing nail 4, the flow and detection of helium can be more accurately controlled to ensure the accuracy of the test results. The setting of the closed space 5 allows helium to act more concentratedly on the welding area, thereby more effectively detecting the welding quality between the sealing nail 4 and the glue nail 3. It can also help prevent helium from leaking to the external environment during the detection process, ensuring the stability and safety of the detection environment. It helps to reduce unnecessary helium consumption during the detection process, thereby reducing material costs. In addition, it can also make the detection process faster and more efficient, reduce the detection time, and thus improve the overall production efficiency.

[0040] In S3, the first gas 6 is filled into the closed space 5, and the pressure change is detected, which specifically includes: filling the first gas 6 with a predetermined pressure into the closed space 5, and detecting the pressure change after maintaining it for a predetermined time. By detecting the pressure change of the first gas 6 in the closed space 5, it is possible to quickly identify whether there is a leak during the welding process of the battery 1, thereby improving the response speed of the detection. By maintaining the gas pressure for a predetermined time and detecting the pressure change, it is possible to more sensitively detect tiny leaks and ensure the sealing quality of the battery 1. By maintaining the pressure for a predetermined time, it is possible to distinguish between transient pressure fluctuations and actual leaks, thereby reducing misjudgments caused by external factors. By quickly and accurately identifying leaks, further detection and analysis of the problematic battery 1 is reduced, thereby reducing the detection cost.

[0041] Preferably, the predetermined pressure ranges from 1 to 3 bar. For example, it may be 1 bar, 1.5 bar, 2 bar, 2.5 bar, 3 bar, and so on. The pressure range of 1 to 3 bar provides a moderate working pressure for detection, which is neither too high to cause damage to the structure of the battery 1, nor too low to reduce the sensitivity of the detection. Detection within this pressure range can reduce the amount of gas used, thereby reducing material costs and environmental impact. It helps to more accurately identify small leaks caused by welding defects and improve the accuracy of leak detection. It is known to those skilled in the art that the range of the predetermined pressure can also be other ranges other than those in this embodiment while achieving the same effect.

[0042] Preferably, the range of the predetermined time is between 3-5s. For example, it can be 3s, 3.5s, 4s, 4.5s and 5s, etc. The predetermined time of 3-5 seconds allows for rapid pressure detection, thereby speeding up the entire detection process and improving production efficiency. Within this range, it can be ensured that the gas is fully distributed in the enclosed space 5, so that possible leaks can be detected more accurately. It is known to those skilled in the art that the range of the predetermined time can also be other ranges than those in this embodiment while achieving the same effect.

[0043] Furthermore, the first gas 6 is filled into the closed space 5, and the pressure change is detected, which specifically includes: if the pressure cannot be maintained, it is judged as welding abnormality (for example, welding abnormality is judged by judging whether there is gas leakage). If the pressure cannot be maintained, the leakage problem can be immediately identified, providing instant feedback for the production process and accelerating the problem solving.

[0044] In S4, if the pressure remains unchanged, the first gas 6 in the enclosed space 5 is removed and the second gas 7 is filled in, which specifically includes: if the pressure remains unchanged, the first gas 6 in the enclosed space 5 is evacuated and the vacuum state is maintained; and then the second gas 7 at a specified pressure is filled in the enclosed space 5 and maintained for a specified time. By removing the first gas 6 and maintaining the vacuum state, an interference-free environment is provided for the filling and detection of the second gas 7, ensuring the accuracy of the detection. Rapidly switching to the filling and detection of the second gas 7 reduces waiting and conversion time and improves production efficiency. Filling the second gas 7 under controlled conditions helps to maintain the consistency of the detection data and facilitates subsequent analysis and quality control.

[0045] Preferably, the range of the specified pressure is between 2-5 bar. For example, it can be 2 bar, 3 bar, 4 bar and 5 bar, etc. It is known to those skilled in the art that the range of the specified pressure can also be other ranges than those in the present embodiment while achieving the same effect. According to the specific type of battery 1 and welding process requirements, the most suitable pressure value can be flexibly selected. By accurately controlling the pressure within the range of 2-5 bar, the welding quality can be detected more carefully and the accuracy of the detection can be improved.

[0046] Preferably, the range of the specified time is between 30-120 seconds. For example, it may be 30 seconds, 50 seconds, 70 seconds, 90 seconds, 110 seconds, 120 seconds, etc. It is known to those skilled in the art that the range of the specified time may also be other ranges than those in this embodiment while achieving the same effect. By setting the range of 30-120 seconds, the welding quality can be detected more meticulously and the accuracy of the detection can be improved.

[0047] As a preferred embodiment, the first gas 6 includes nitrogen. Nitrogen is an inert gas. Using nitrogen for detection can reduce the safety risks caused by gas reactions. By using nitrogen for accurate detection, the welding quality of the battery 1 can be ensured and the overall quality of the final product can be improved. It is known to those skilled in the art that other inert gases besides nitrogen can also be used to achieve the same effect.

[0048] In S5, the second gas 7 includes helium. The detection of the pressure of the second gas 7 in the closed space 5 and the judgment of the welding quality specifically include: breaking the vacuum after the second gas 7 reaches the holding time, transferring the battery 1 to the helium inspection station, and performing helium inspection after evacuating the closed space 5. If the helium leak rate of the battery 1 is greater than the predetermined parameter, it is judged to be unqualified and the welding is defective; if the helium leak rate of the battery 1 is less than or equal to the predetermined parameter, it is judged to be qualified and there is no defect in the welding. Among them, the predetermined parameters can be selected according to the actual situation, so as to make the detection method more flexible and adaptable to different production needs and standards. By performing the vacuum breaking operation after the holding time, the consistency of the detection conditions is ensured and the accuracy of the welding quality detection is improved. Through the detection of the helium leak rate, it is possible to accurately judge whether there are defects in the welding of the battery 1, ensuring that only qualified products enter the market.

[0049] Preferably, the range of the holding time is between 30-120s. For example, it can be 30s, 50s, 70s, 90s, 110s and 120s, etc. It is known to those skilled in the art that the range of the holding time can also be other ranges other than those in this embodiment while achieving the same effect. In addition, a moderate holding time can avoid excessive internal pressure on the battery 1 and reduce the risk of damage to the battery 1 due to excessive holding time.

[0050] In a specific example, combining Figure 2 , Figure 3 and Figure 4 As shown, after the battery 1 is filled with liquid for the second time, the glue nail 3 is applied, and then the sealing nail 4 is welded directly; the welded battery 1 is transferred to the helium injection station, and the sealing nail 4 is sealed in a small space, that is, a closed space 5 is formed. First, nitrogen with a pressure of 1-3 bar is injected for 3-5 seconds. If the pressure cannot be maintained, it is judged as a large leak (i.e., leakage). If the pressure remains unchanged, the nitrogen in the small space is evacuated to maintain the vacuum state. After the battery 1 that is filled with nitrogen to maintain the pressure is evacuated to remove the nitrogen, helium with a pressure of 2-5 bar is injected into the sealing nail 4 for 30-120 seconds. If there is a welding defect at the sealing nail 4, helium enters the gap between the sealing nail 4 and the glue nail 3 and remains. Helium cannot enter the battery cell without welding defects. After the helium pressure is maintained for 30-120 seconds, the vacuum is broken and the battery is transferred to the helium inspection station. The sealing nail 4 is still sealed in a small space (i.e., a closed space 5 is formed) and then evacuated for helium inspection. If the helium leak rate of the battery cell is higher than 9.9×10 -7 Pa*m 3 / s is judged as NG (unqualified), less than or equal to 9.9×10- 7 Pa*m 3 / s is judged as OK (qualified).

[0051] In this embodiment, the battery 1 is filled with liquid for the second time and then the glue nail 3 is applied, and then the sealing nail 4 is welded directly; the welded battery 1 is transferred to the helium injection station, and the sealing nail 4 is sealed in a small space (i.e., a closed space 5 is formed). First, inject nitrogen at a pressure of 2.6 bar for 3 seconds. If the pressure cannot be maintained, it is judged as a large leak (i.e., leakage). If the pressure remains unchanged, evacuate the nitrogen in the small space to maintain the vacuum state. After the battery 1 that is filled with nitrogen to maintain the pressure is evacuated to remove the nitrogen, helium at a pressure of 3 bar is injected into the sealing nail 4 for 90 seconds. If there is a welding defect at the sealing nail 4, helium will enter the gap between the sealing nail 4 and the glue nail 3 and remain there. Helium cannot enter the battery cell with no welding defects. After the helium pressure is maintained for 90 seconds, the vacuum is broken and the battery is transferred to the helium inspection station. The sealing nail 4 is further sealed in a small space and evacuated for helium inspection. If the helium leak rate of the battery cell is higher than 9.9×10 -7 Pa*m 3 / s is judged as NG (failure), less than or equal to 9.9×10 -7 Pa*m 3 / s is judged as OK (qualified).

[0052] In summary, the battery sealing nail welding quality detection method proposed in the present invention has the following advantages:

[0053] After the battery is refilled with liquid, the sealing element is directly used to weld the battery; the space above the sealing element is sealed to form a closed space; the first gas is filled into the closed space to detect the pressure change; if the pressure remains unchanged, the first gas in the closed space is removed and the second gas is filled; and the pressure of the second gas in the closed space is detected to judge the welding quality. The present invention does not need to inject helium after the battery is refilled with liquid, and can directly and accurately detect defects in the sealing nail area after welding using the sealing element, which can improve the detection accuracy.

[0054] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

Claims

1. A battery sealing nail welding quality detection method, characterized in that: The details include: After the battery is refilled, the battery is welded directly using the sealing element; sealing the space above the sealing element to form a closed space; and A first gas is filled into the closed space, and a pressure change is detected.

2. The battery sealing nail welding quality detection method according to claim 1, characterized in that: The sealing element comprises a glue nail and a sealing nail.

3. The battery sealing nail welding quality detection method according to claim 2, characterized in that: After the secondary liquid injection of the battery, the sealing element is directly used to weld the battery, which specifically includes: after the secondary liquid injection of the battery, glue nails are applied, and then the sealing nails are directly welded.

4. The battery sealing nail welding quality detection method according to claim 3, characterized in that: The process of sealing the space above the sealing element to form a closed space specifically includes: transferring the welded battery to a helium injection station, and sealing the space above the sealing pin in the closed space.

5. The battery sealing nail welding quality detection method according to claim 4, characterized in that: The step of filling the closed space with the first gas and detecting the pressure change specifically includes: filling the closed space with the first gas at a predetermined pressure, maintaining the pressure for a predetermined time, and then detecting the pressure change.

6. The battery sealing nail welding quality detection method according to claim 5, characterized in that: The predetermined pressure ranges from 1 to 3 bar.

7. The battery sealing nail welding quality detection method according to claim 5, characterized in that: The step of filling the closed space with the first gas and detecting the pressure change specifically includes: if the pressure cannot be maintained, determining that the welding is abnormal.

8. The battery sealing nail welding quality detection method according to claim 1, characterized in that: Also includes: If the pressure remains unchanged, the first gas in the closed space is exhausted and the second gas is filled in; the pressure of the second gas in the closed space is detected to judge the welding quality.

9. The battery sealing nail welding quality detection method according to claim 8, characterized in that: The first gas includes nitrogen; and the second gas includes helium.

10. The battery sealing nail welding quality detection method according to claim 9, characterized in that: If the pressure remains unchanged, the first gas in the closed space is discharged and the second gas is filled in, which specifically includes: if the pressure remains unchanged, the first gas in the closed space is discharged by vacuuming and maintaining the vacuum state; then the second gas at a specified pressure is filled in the closed space and maintained for a specified time.

11. The battery sealing nail welding quality detection method according to claim 10, characterized in that: The specified pressure ranges from 2 to 5 bar.

12. The battery sealing nail welding quality detection method according to claim 10, characterized in that: The detecting the pressure of the second gas in the enclosed space and judging the welding quality specifically includes: performing a vacuum breaking operation after the second gas reaches the pressure holding time, transferring the battery to a helium inspection station, and performing a helium inspection after evacuating the enclosed space. If the battery helium leakage rate is greater than a predetermined parameter, it is determined to be unqualified and the welding has defects; if the battery helium leakage rate is less than or equal to the predetermined parameter, it is determined to be qualified and the welding has no defects.

13. The battery sealing nail welding quality detection method according to claim 12, characterized in that: The holding time ranges from 30 to 120 seconds.