High-conductivity and high-toughness copper alloy cable and preparation method thereof

Through low-temperature nitrogen flushing and hot and cold interaction technology, the oxidation problem during the cleaning of copper alloy cables is solved, and the preparation of copper alloy cables with high conductivity and high toughness is achieved, which extends the life of the copper wire and improves the bonding force of the protective rubber layer. .

CN119008117AInactive Publication Date: 2024-11-22WUXI ZHONGHUI WIRE & CABLE
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411201461.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The residual semiconducting water in the cleaning process of existing copper alloy cables leads to oxidation, affecting the life of the copper wire, and the adhesion of the protective adhesive layer causes gaps and humid environment to trigger oxidation reactions.

Method used

Using low-temperature nitrogen flushing and chip cleaning treatment and hot and cold interactive shaping technology, low-temperature nitrogen dilutes oxygen, cleans up dust and impurities on the surface of copper wire, and covers it with low-temperature nitrogen and motor-driven protective glue layer to ensure the low-oxygen environment and protective glue on the surface of copper wire The layer solidifies quickly.

Benefits of technology

Effectively reduce oxidative corrosion, prevent the formation of oxide layers, improve the conductivity and toughness of copper wire, extend the service life of copper wire, and enhance the bonding force between the protective adhesive layer and copper wire, avoiding bubble accumulation in traditional methods and oxidation problems.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008117A_ABST
    Figure CN119008117A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of high-conductivity cables, and particularly relates to a high-conductivity and high-toughness copper alloy cable and a preparation method thereof.The high-conductivity and high-toughness copper alloy cable comprises a high-toughness copper alloy cable body, and the high-toughness copper alloy cable body is formed by combining an alloy cable wire, a protective adhesive layer, an insulating plastic ring, a high-toughness adhesive layer and a solid protective adhesive layer; the surface of the alloy cable wire is provided with an insulating plastic ring, and the outer side surface of the insulating plastic ring is movably sleeved with a solid protective glue layer. A plurality of alloy cable wires are inserted into the cleaning box in cooperation with a roller, meanwhile, the separated alloy cable wires are compressed and folded together in cooperation with a rectangular groove and a conical sleeve on the inner side wall face of the cleaning box, and the alloy cable wires enter the cooling cleaning cavity along with continuous movement of the alloy cable wires; and at the moment, nitrogen is rapidly sprayed into the cooling cleaning cavity in cooperation with a nitrogen box, and the nitrogen is diffused in the cooling cleaning cavity along with the nitrogen.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of high-electricity cables, in particular to a copper alloy cable with high conductivity and high toughness and a preparation method thereof. Background Art

[0002] Wires and cables are wire products used to transmit electrical (magnetic) energy, information and realize electromagnetic energy conversion. Although the wire and cable industry is only a supporting industry, it accounts for 1 / 4 of the output value of my country's electrical industry. It has many product types and a wide range of applications, involving electricity, construction, communications, manufacturing and other industries. It is closely related to all sectors of the national economy. Wires and cables are also called the "arteries" and "nerves" of the national economy. They are indispensable basic equipment for transmitting electrical energy, transmitting information, manufacturing various motors, instruments, and meters, and realizing electromagnetic energy conversion. They are necessary basic products in the future electrification and information society.

[0003] In the current prior art, before assembling the copper alloy cable, the surface of the copper alloy cable wire needs to be cleaned to keep it clean. However, the existing cleaning device uses semi-conductive water to flush the dust and impurities on the surface of the copper wire. However, this method will cause semi-conductive water to remain inside the wound copper wire, so that the residual semi-conductive water will remain inside the copper wire during the later winding and wrapping, and a certain amount of oxygen will remain inside the semi-conductive water. As the protective layer is wrapped on the surface of the copper wire, the semi-conductive water is blocked inside. As time goes by, the oxygen inside the semi-conductive water will gradually The copper wire is gradually oxidized to form an oxide layer, which will gradually thicken over time, eventually leading to the loss of copper. The copper wire will generate a very high temperature when energized, and excessively high temperature will also affect the oxidation process of the copper wire. High temperature accelerates the oxidation reaction, and the protective adhesive layer on the surface of the copper wire is adhered to the surface of the copper wire using softened natural light. This adhesion method will leave a gap between the copper wire and the protective adhesive layer, which causes the semiconductor water inside the copper wire to gradually evaporate under heat, forming a humid closed environment in the protective adhesive layer. The copper wire undergoes an oxidation reaction with the oxygen in the semiconductor water in the humid environment to form copper oxide.

[0004] To this end, the present invention provides a copper alloy cable with high conductivity and high toughness and a preparation method thereof. Summary of the invention

[0005] In order to make up for the deficiencies of the prior art, at least one technical problem raised in the background technology is solved.

[0006] In the first aspect, the technical solution adopted by the present invention to solve its technical problem is: a high-conductivity and high-toughness copper alloy cable described in the present invention comprises a high-toughness copper alloy cable body, the high-toughness copper alloy cable body comprises an alloy cable wire, a protective rubber layer, an insulating plastic ring, a high-toughness rubber layer and a solid protective rubber layer. An insulating plastic ring is arranged on the surface of the alloy cable wire, and a solid protective rubber layer is movably sleeved on the outer surface of the insulating plastic ring. The number of the alloy cable wires is set to 12 groups, and the outer surfaces of the 12 groups of alloy cable wires are filled with protective rubber layers, and the outer surfaces of the protective rubber layers are covered and filled with a high-toughness rubber layer.

[0007] In a second aspect, a method for preparing a copper alloy cable with high conductivity and high toughness is provided, wherein the alloy cable wire is prepared by the following steps: S1. Gather 12 groups of alloy cable wires together, and wrap insulating plastic rings, solid protective rubber layers and protective layers on the surfaces of the alloy cable wires, and use positioning devices, rubber coating and filling devices and low-temperature flushing and chip removal devices that are movably sleeved on the outer surfaces of the alloy cable wires; S2, using low-temperature nitrogen gas inside a low-temperature flushing and chip cleaning device to perform low-temperature flushing and chip cleaning treatment on the surface of the alloy cable wire wrapped with a solid protective rubber layer and an insulating plastic ring; S3, as the alloy cable wire moves from the low-temperature flushing and chip cleaning device to the inner wall of the rubber-coated filling device, the protective rubber layer of the inner wall of the rubber-coated filling device is wrapped and covered on the surface; S4, centralized limiting; cooling and shaping the cable wire, after the protective rubber layer on the outer surface of the alloy cable wire is completely solidified, the high-toughness rubber layer is filled on the surface of the alloy cable wire in conjunction with the protective device of the alloy cable wire.

[0008] Preferably, the rubber coating and filling device includes a water tank movably connected to the outer surface of the alloy cable wire, the positioning device includes a support frame movably connected to the outer surface of one end of the alloy cable wire, the rubber coating and filling device includes a water tank movably connected to the outer surface of the alloy cable wire, a cleaning box is arranged on the water tank, the support frame and the outer surface of the alloy cable wire, and a connecting frame movably connected to the outer surface of the alloy cable wire is fixedly installed on the inner wall of the cleaning box.

[0009] Preferably, a nitrogen dilution unit is provided on the inner wall surface of the cleaning box, and the nitrogen dilution unit comprises a rectangular groove opened on the inner wall surface of the cleaning box, and the rectangular groove is in a trumpet shape. A cooling cleaning cavity is opened on the inner wall surface of the other side of the cleaning box, and the small end of the rectangular groove extends to the inner wall surface of the cooling cleaning cavity, and a conical sleeve movably sleeved on the outer surface of the alloy cable wire is slidably sleeved on the inner wall surface of the rectangular groove. A nitrogen box is fixedly installed on the top surface of the cleaning box, and the output end of the nitrogen box extends to the inner wall surface of the cooling cleaning cavity. A motor 1 whose output end is movably sleeved on the outer surface of the conical sleeve is fixedly installed on one side surface of the cleaning box; A backflow prevention limit cylinder is fixedly connected to the inner wall of the water tank, a conical shaping cylinder movably sleeved on the outer surface of the alloy cable wire is fixedly connected to the inner wall of the backflow prevention limit cylinder, a collecting cylinder is fixedly connected to the top surface of the backflow prevention limit cylinder, and the inner wall of the water tank and the outer surface of the backflow prevention limit cylinder are filled with low-temperature water.

[0010] Preferably, a cooling chamber is fixedly installed on one side surface of the water tank, and a heat dissipation slot is provided on the top surface of the cooling chamber.

[0011] Preferably, a second motor is fixedly mounted on a surface of one end of the support frame, and a clamping plate is fixedly connected to an output end of the second motor.

[0012] Preferably, a rectangular ring is fixedly connected to the outer surface of the clamping plate, a limiting arc plate is fixedly connected to the outer surface of the rectangular ring, the inner wall of the limiting arc plate is movably sleeved on the outer surface of the alloy cable wire, an arc-shaped positioning arm is fixedly connected to one end of the connecting frame, and a limiting slide bar is movably sleeved on the inner wall of the arc-shaped positioning arm.

[0013] Preferably, a clamping ring is provided on the inner wall surface of the position-limiting slide bar, an arc-shaped plate is fixedly connected to the inner wall surface of the clamping ring, and a closing cover is detachably mounted on the outer surface of the arc-shaped plate.

[0014] Preferably, a reflux pipe is fixedly connected to the output end of the nitrogen box, and the other end of the reflux pipe extends to the inner wall surface of the cooling and cleaning chamber.

[0015] The beneficial effects of the present invention are as follows: 1. The present invention discloses a copper alloy cable with high conductivity and high toughness and a preparation method thereof. A roller is used to insert a plurality of alloy cable wires into a cleaning box. At the same time, the rectangular grooves and the conical sleeves on the inner wall of the cleaning box are used to compress and close the separated alloy cable wires together. As the alloy cable wires continue to move, they enter the cooling cleaning chamber. At this time, a nitrogen box is used to quickly spray nitrogen into the cooling cleaning chamber. As the nitrogen diffuses in the cooling cleaning chamber, it mixes with the oxygen in the cooling cleaning chamber. As the nitrogen continues to increase, the mixed nitrogen is squeezed out and discharged. The oxygen ratio is diluted by the continuous expansion of nitrogen. The high-content low-temperature nitrogen will gradually mix with the alloy cable wire entering the cooling and cleaning chamber. At the same time, the low-temperature nitrogen is blown by the nitrogen box. The dust, impurities and water vapor on the surface of the alloy cable wire are cleaned by the high-speed blowing of low-temperature nitrogen, so that the surface of the copper wire is always in a low-oxygen environment, and the oxygen carried by the continuous movement of the alloy cable wire is reduced. The dust and impurities on the surface of the copper wire are flushed by low-temperature nitrogen, and the oxygen content is diluted by low-temperature nitrogen, which reduces the oxidation corrosion of the alloy cable wire caused by oxygen. 2. The present invention discloses a high-conductivity and high-toughness copper alloy cable and a preparation method thereof. At the same time, low-temperature nitrogen is used to cool the copper wire. The alloy cable wire in a low-temperature environment will produce a slight contraction due to the low temperature. As the alloy cable wire continues to move, it will enter the interior of the anti-backflow limit cylinder. The collecting cylinder is used to infuse a protective rubber layer into the interior of the anti-backflow limit cylinder. The motor is used to rotate a pair of conical sleeves. The rotating copper wire will be stirred inside the anti-backflow limit cylinder, so that the protective rubber layer will effectively cover the surface of the alloy cable wire. The protective rubber layer in the semi-solidified liquid state contains a very high temperature. When it comes into contact with the surface of the alloy cable wire, the protective rubber layer in the high temperature state will quickly absorb the low temperature gas on the surface of the low temperature copper wire. Under the interaction of hot and cold, the protective rubber layer that has just come into contact with the surface of the alloy cable wire will quickly condense and take shape, thereby reducing the accumulation of gas inside the protective rubber layer. The alloy cable wire that has lost its low temperature will gradually return to its original state. The slightly expanded alloy cable wire will slightly squeeze the protective rubber layer on the outer surface, thereby increasing the adhesion between the alloy cable wire and the protective rubber layer, achieving the effect of using the interaction of hot and cold to quickly shape the semi-solidified protective rubber layer, and solidifying from the inside out to reduce the accumulation of bubbles. 3. The present invention discloses a high-conductivity and high-toughness copper alloy cable and a preparation method thereof, which utilizes an arc plate and a closed cover on the inner wall of a clamping ring to limit the position of the alloy cable wire, while maintaining approximately the same spacing between each alloy cable wire, and cooperates with a pair of conical sleeves of a motor to rotate, so that multiple alloy cable wires can be effectively contacted and mixed with nitrogen, and when the anti-slip rubber layer is applied, the rotating alloy cable wire can be fully and effectively contacted with the protective rubber layer, and when the motor rotates the alloy cable wire, the limiting sliding bar on the outer surface of the clamping ring slides inside the arc-shaped positioning arm, so that the alloy cable wire can be limited and rotated. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The present invention will be further described below in conjunction with the accompanying drawings.

[0017] Figure 1 It is a schematic diagram of the process of the present invention; Figure 2 It is a schematic diagram of the cross-sectional three-dimensional structure of the cleaning box of the present invention; Figure 3 It is a schematic diagram of the three-dimensional structure of the cleaning box of the present invention; Figure 4 It is a schematic diagram of the cross-sectional three-dimensional structure of the cleaning box and the support frame of the present invention; Figure 5 It is a schematic diagram of a cross-sectional three-dimensional structure of a rectangular groove of the present invention; Figure 6 It is a schematic diagram of the cutaway three-dimensional structure of the tapered sleeve of the present invention; Figure 7 It is a schematic diagram of the three-dimensional structure of the support frame of the present invention; Figure 8 It is a schematic diagram of a cross-sectional three-dimensional structure of the connecting frame of the present invention; Fig. 9 It is a schematic diagram of the three-dimensional structure of the alloy cable wire of the present invention.

[0018] In the figure: 11, cleaning box; 111, rectangular groove; 112, motor one; 113, nitrogen box; 114, cooling cleaning chamber; 115, tapered sleeve; 116, reflux pipe; 12, support frame; 121, motor two; 122, clamping plate; 123, rectangular ferrule; 124, limiting arc plate; 13, alloy cable wire; 14, water tank; 141, anti-backflow limiting cylinder; 142, collecting cylinder; 143, tapered shaping cylinder; 144, low-temperature water; 145, cooling chamber; 146, heat exhaust notch; 15, connecting frame; 151, arc-shaped positioning arm; 152, limiting slide; 153, clamping ring; 154, arc plate; 155, closing cover. DETAILED DESCRIPTION

[0019] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods. Example 1

[0020] like Figure 1 - Figure 4 , Figure 6 and Fig. 9 As shown, a high-conductivity and high-toughness copper alloy cable of an embodiment of the present invention includes a high-toughness copper alloy cable main body, which includes an alloy cable wire 13, a protective rubber layer, an insulating plastic ring, a high-toughness rubber layer and a solid protective rubber layer. An insulating plastic ring is arranged on the surface of the alloy cable wire 13, and a solid protective rubber layer is movably sleeved on the outer surface of the insulating plastic ring. The number of alloy cable wires 13 is set to 12 groups, and the outer surfaces of the 12 groups of alloy cable wires 13 are filled with a protective rubber layer, and the outer surface of the protective rubber layer is covered with a high-toughness rubber layer. Example 2

[0021] like Figure 2 - Fig. 9 As shown, the present invention also provides a method for preparing a copper alloy cable with high conductivity and high toughness. The alloy cable wire 13 is prepared by the following steps: S1, gather 12 groups of alloy cable wires 13 together, and wrap insulating plastic rings, solid protective rubber layers and protective layers on the surfaces of the alloy cable wires 13, and use positioning devices, rubber coating and filling devices and low-temperature flushing and chip cleaning devices that are movably sleeved on the outer surfaces of the alloy cable wires 13; S2, using low-temperature nitrogen gas inside the low-temperature flushing and chip cleaning device to perform low-temperature flushing and chip cleaning treatment on the surface of the alloy cable wire 13 wrapped with a solid protective rubber layer and an insulating plastic ring; S3, when the alloy cable wire 13 moves from the low-temperature flushing and chip cleaning device to the inner wall of the rubber-coated filling device, the protective rubber layer of the inner wall of the rubber-coated filling device is wrapped and covered on the surface of 13; S4, centralized limiting; cooling and shaping the cable wire, until the protective rubber layer on the outer surface of the alloy cable wire 13 is completely solidified, the protective device of the alloy cable wire 13 is used to fill the surface of the alloy cable wire 13 with a high-toughness rubber layer.

[0022] Furthermore, if Figure 2 - Figure 8As shown, the rubber coating and filling device includes a water tank 14 movably sleeved on the outer surface of the alloy cable wire 13, the positioning device includes a support frame 12 movably sleeved on the outer surface of one end of the alloy cable wire 13, the rubber coating and filling device includes a water tank 14 movably sleeved on the outer surface of the alloy cable wire 13, and a cleaning box 11 is arranged on the outer surface of the water tank 14, the support frame 12 and the alloy cable wire 13. A connecting frame 15 movably sleeved on the outer surface of the alloy cable wire 13 is fixedly installed on the inner wall of the cleaning box 11. A nitrogen dilution unit is arranged on the inner wall of the cleaning box 11, and the nitrogen dilution unit includes a rectangular opening on the inner wall of the cleaning box 11. The groove 111 is in the shape of a trumpet. A cooling cleaning chamber 114 is provided on the inner wall surface of the other side of the cleaning box 11, and the small end of the rectangular groove 111 extends to the inner wall surface of the cooling cleaning chamber 114. A conical sleeve 115 movably sleeved on the outer surface of the alloy cable wire 13 is slidably sleeved on the inner wall surface of the rectangular groove 111. A nitrogen box 113 is fixedly installed on the top surface of the cleaning box 11, and the output end of the nitrogen box 113 extends to the inner wall surface of the cooling cleaning chamber 114. A motor 112 with an output end movably sleeved on the outer surface of the conical sleeve 115 is fixedly installed on one side surface of the cleaning box 11. A backflow prevention limit cylinder 141 is fixedly connected to the inner wall of the water tank 14, a conical shaping cylinder 143 movably sleeved on the outer surface of the alloy cable wire 13 is fixedly connected to the inner wall of the backflow prevention limit cylinder 141, a collecting cylinder 142 is fixedly connected to the top surface of the backflow prevention limit cylinder 141, and the inner wall of the water tank 14 and the outer surface of the backflow prevention limit cylinder 141 are filled with low-temperature water 144.

[0023] When the nitrogen dilution unit provided by the present invention is used, the roller is used to insert multiple alloy cable wires 13 into the interior of the cleaning box 11, and the rectangular grooves 111 and the conical sleeves 115 on the inner wall of the cleaning box 11 are used to compress and close the separated alloy cable wires 13 together. As the alloy cable wires 13 continue to move, they enter the interior of the cooling and cleaning chamber 114. At this time, the nitrogen box 113 is used to quickly spray nitrogen into the interior of the cooling and cleaning chamber 114. As the nitrogen diffuses inside the cooling and cleaning chamber 114, the oxygen inside the cooling and cleaning chamber 114 is mixed. As the nitrogen continues to increase, the nitrogen mixed in front is squeezed and discharged, and the continuous expansion of nitrogen is used to dilute the oxygen ratio, and the high content of low The warm nitrogen will gradually mix with the alloy cable wire 13 entering the cooling and cleaning chamber 114, and at the same time cooperate with the nitrogen box 113 to blow the low-temperature nitrogen, and use the high-speed blowing low-temperature nitrogen to clean the dust, impurities and water vapor on the surface of the alloy cable wire 13, so that the surface of the copper wire is always in a low-oxygen environment, reducing the oxygen carried by the alloy cable wire 13 as it moves continuously, achieving the effect of using low-temperature nitrogen to flush the dust and impurities on the surface of the copper wire, and then using low-temperature nitrogen to dilute the oxygen content, reducing the oxidation corrosion of the alloy cable wire 13 caused by oxygen, and avoiding oxygen from gradually oxidizing the alloy cable wire 13 to form an oxide layer. As time goes by, the oxide layer will gradually thicken, and eventually lead to copper loss; At the same time, low-temperature nitrogen is used to cool the copper wire. In the low-temperature environment, the alloy cable wire 13 will produce a small contraction due to the low temperature. As the alloy cable wire 13 continues to move, it will enter the interior of the anti-backflow limit cylinder 141, and the collecting cylinder 142 is used to inject a protective rubber layer into the interior of the anti-backflow limit cylinder 141. The motor 112 is used to rotate the conical sleeve 115. The rotating copper wire will be stirred inside the anti-backflow limit cylinder 141, so that the protective rubber layer will effectively cover the surface of the alloy cable wire 13. The protective rubber layer in the semi-solidified liquid state contains a very high temperature. When it contacts the surface of the alloy cable wire 13, the protective rubber layer in the high-temperature state will quickly absorb the low-temperature gas on the surface of the low-temperature copper wire. Under the interaction of cold and heat, the protective rubber layer that has just contacted the surface of the alloy cable wire 13 will quickly condense and take shape, thereby reducing the accumulation of gas inside the protective rubber layer, and the alloy cable wire 13 that has lost its low temperature will gradually Gradually restore to its original shape, the slightly enlarged alloy cable wire 13 will slightly squeeze the protective rubber layer on the outer surface, thereby increasing the adhesion between the alloy cable wire 13 and the protective rubber layer, achieving the effect of using cold and hot interaction to quickly shape the semi-solidified protective rubber layer, and solidifying from the inside out to reduce the accumulation of bubbles, avoiding the traditional protective rubber layer. The protective rubber layer extruded out is cylindrical, so that it is wrapped on the outer surface of the alloy cable wire 13, and gradually covers the surface of the alloy cable wire 13 as the protective rubber layer continues to cool down and solidify. This method will cause a large amount of air to accumulate inside the protective rubber layer, and the oxygen inside the air will gradually oxidize the copper wire to form an oxide layer. As time goes by, the oxide layer will gradually thicken, eventually leading to the loss of copper, and then the surface of the anti-backflow limit tube 141 is cooled by low-temperature water 144, so that the protective rubber layer and the anti-backflow limit tube 141 The fitting surface will be quickly solidified and fixed.

[0024] Furthermore, if Figure 1 - Figure 4 , Figure 6 and Figure 8As shown, a motor 2 121 is fixedly mounted on the surface of one end of the support frame 12, a clamping plate 122 is fixedly connected to the output end of the motor 2 121, a rectangular ferrule 123 is fixedly connected to the outer surface of the clamping plate 122, a limiting arc plate 124 is fixedly connected to the outer surface of the rectangular ferrule 123, the inner wall of the limiting arc plate 124 is movably sleeved on the outer surface of the alloy cable wire 13, an arc-shaped positioning arm 151 is fixedly connected to one end of the connecting frame 15, a limiting slide bar 152 is movably sleeved on the inner wall of the arc-shaped positioning arm 151, a clamping ring 153 is provided on the inner wall of the limiting slide bar 152, an arc plate 154 is fixedly connected to the inner wall of the clamping ring 153, a closing cover 155 is detachably mounted on the outer surface of the arc plate 154, a reflux pipe 116 is fixedly connected to the output end of the nitrogen box 113, and the other end of the reflux pipe 116 extends to the inner wall of the cooling and cleaning chamber 114.

[0025] When the arc positioning arm 151, the limiting slide bar 152, the clamping ring 153, the arc plate 154 and the closing cover 155 provided by the present invention are used to limit the position of the alloy cable wire 13 by using the arc plate 154 on the inner wall of the clamping ring 153 and the closing cover 155, and at the same time, the spacing between each alloy cable wire 13 is roughly maintained at the same time, and the conical sleeve 115 is rotated in cooperation with the motor 112, so that multiple alloy cable wires 13 can be effectively contacted and mixed with nitrogen, and the rotating alloy cable wire 13 can be fully and effectively contacted with the protective rubber layer when the anti-slip rubber layer is applied, and when the motor 112 rotates the alloy cable wire 13, the limiting slide bar 152 on the outer surface of the clamping ring 153 slides inside the arc positioning arm 151, so that the alloy cable wire 13 can be limited and rotated.

[0026] Furthermore, if Figure 2 - Figure 3 As shown, a cooling chamber 145 is fixedly installed on one side surface of the water tank 14 , and a heat dissipation slot 146 is provided on the top surface of the cooling chamber 145 .

[0027] When the cooling chamber 145 and the heat dissipation slot 146 provided by the present invention are in use, after the protective rubber layer is covered, the cooling chamber 145 is continuously moved and cooperated with the blower to blow the inside of the cooling chamber 145, and the high temperature emitted from the surface of the protective rubber layer is quickly blown away by the rapid flow of the airflow. As the hot air is continuously accumulated inside the cooling chamber 145, as the gas is continuously expanded, the gas will be discharged through the heat dissipation slot 146. As the hot air is continuously discharged and the subsequent cold air is continuously filled in, the inside of the cooling chamber 145 is always in a low-temperature environment, and the low-temperature gas will perform thermal interaction treatment with the hot air on the surface of the protective rubber layer, thereby quickly solidifying the surface of the protective rubber layer, thereby preventing the surface of the protective rubber layer from being deformed due to the continuous movement of the distance due to incomplete solidification.

[0028] The working principle provided by the present invention is as follows: a plurality of alloy cable wires 13 are inserted into the interior of the cleaning box 11 in cooperation with a roller, and at the same time, the rectangular grooves 111 and the conical sleeves 115 on the inner wall of the cleaning box 11 are used to compress and close the separated alloy cable wires 13 together, and as the alloy cable wires 13 continue to move, they enter the interior of the cooling cleaning chamber 114, and at this time, the nitrogen box 113 is used to quickly spray nitrogen into the interior of the cooling cleaning chamber 114, and as the nitrogen diffuses in the cooling cleaning chamber 114, it mixes with the oxygen in the cooling cleaning chamber 114, and as the nitrogen continues to increase, the nitrogen mixed in front is squeezed and discharged, so as to benefit The nitrogen is continuously expanded to dilute the oxygen ratio. The high-content low-temperature nitrogen will gradually mix with the alloy cable wire 13 entering the cooling and cleaning chamber 114. At the same time, the nitrogen box 113 is used to blow the low-temperature nitrogen. The high-speed blowing low-temperature nitrogen is used to clean the dust, impurities and water vapor on the surface of the alloy cable wire 13, so that the surface of the copper wire is always in a low-oxygen environment, reducing the oxygen carried by the continuous movement of the alloy cable wire 13, achieving the effect of using low-temperature nitrogen to flush the dust and impurities on the surface of the copper wire, and then using low-temperature nitrogen to dilute the oxygen content, reducing the oxidation corrosion of the alloy cable wire 13 caused by oxygen; At the same time, low-temperature nitrogen is used to cool the copper wire. In the low-temperature environment, the alloy cable wire 13 will produce a small contraction due to the low temperature. As the alloy cable wire 13 continues to move, it enters the interior of the anti-backflow limit cylinder 141, and the collecting cylinder 142 is used to inject a protective rubber layer into the interior of the anti-backflow limit cylinder 141. The motor 112 is used to rotate the conical sleeve 115. The rotating copper wire will be stirred inside the anti-backflow limit cylinder 141, so that the protective rubber layer will effectively cover the surface of the alloy cable wire 13. The protective rubber layer in the semi-solidified liquid state contains a very high temperature. When it comes into contact with the alloy cable wire 13, When the protective rubber layer is on the surface of the cable wire 13, the protective rubber layer in the high temperature state will quickly absorb the low-temperature gas on the surface of the low-temperature copper wire. Under the interaction of cold and heat, the protective rubber layer that just comes into contact with the surface of the alloy cable wire 13 will quickly condense and take shape, thereby reducing the accumulation of gas inside the protective rubber layer. The alloy cable wire 13 that has lost its low temperature will gradually return to its original state. The slightly expanded alloy cable wire 13 will slightly squeeze the protective rubber layer on the outer surface, thereby increasing the adhesion between the alloy cable wire 13 and the protective rubber layer, achieving the effect of quickly shaping the semi-solidified protective rubber layer by the interaction of cold and heat, and solidifying from the inside out to reduce bubble accumulation.

[0029] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A copper alloy cable with high conductivity and high toughness, characterized in that: The invention comprises a high-toughness copper alloy cable body, wherein the high-toughness copper alloy cable body comprises an alloy cable wire (13), a protective rubber layer, an insulating plastic ring, a high-toughness rubber layer and a solid protective rubber layer. An insulating plastic ring is arranged on the surface of the alloy cable wire (13), and a solid protective rubber layer is movably sleeved on the outer surface of the insulating plastic ring. The number of the alloy cable wires (13) is set to 12 groups, and the outer surfaces of the 12 groups of the alloy cable wires (13) are filled with a protective rubber layer, and the outer surfaces of the protective rubber layer are covered with a high-toughness rubber layer.

2. A method for preparing a copper alloy cable with high conductivity and high toughness, applicable to the copper alloy cable with high conductivity and high toughness as claimed in claim 1, characterized in that: The alloy cable wire (13) is prepared by the following steps: S1, gather 12 groups of alloy cable wires (13) together, and wrap insulating plastic rings, solid protective rubber layers and protective layers on the surfaces of the alloy cable wires (13), and use positioning devices, rubber coating and filling devices and low-temperature flushing and chip removal devices that are movably sleeved on the outer surfaces of the alloy cable wires (13); S2, using low-temperature nitrogen gas in a low-temperature flushing and chip-clearing device to perform low-temperature flushing and chip-clearing treatment on the surface of the alloy cable wire (13) wound with a solid protective rubber layer and an insulating plastic ring; S3, as the alloy cable wire (13) moves from the inside of the low-temperature flushing and chip cleaning device to the inner wall of the rubber coating and filling device, the protective rubber layer of the inner wall of the rubber coating and filling device is wrapped and covered on the surface of (13); S4, centralized limiting; cooling and shaping the cable wire, and after the protective rubber layer on the outer surface of the alloy cable wire (13) is completely solidified, a high-toughness rubber layer is filled on the surface of the alloy cable wire (13) in cooperation with the protective device of the alloy cable wire (13).

3. The method for preparing a copper alloy cable with high conductivity and high toughness according to claim 2, characterized in that: The rubber coating and filling device comprises a water tank (14) movably sleeved on the outer surface of the alloy cable wire (13); the positioning device comprises a support frame (12) movably sleeved on the outer surface of one end of the alloy cable wire (13); the rubber coating and filling device comprises a water tank (14) movably sleeved on the outer surface of the alloy cable wire (13); a cleaning box (11) is arranged on the outer surface of the water tank (14), the support frame (12) and the alloy cable wire (13); and a connecting frame (15) movably sleeved on the outer surface of the alloy cable wire (13) is fixedly installed on the inner wall surface of the cleaning box (11).

4. The method for preparing a copper alloy cable with high conductivity and high toughness according to claim 3, characterized in that: A nitrogen dilution unit is provided on the inner wall surface of the cleaning box (11), and the nitrogen dilution unit comprises a rectangular groove (111) provided on the inner wall surface of the cleaning box (11), and the rectangular groove (111) is shaped like a trumpet. A cooling cleaning chamber (114) is provided on the inner wall surface of the other side of the cleaning box (11), and the small end of the rectangular groove (111) extends to the inner wall surface of the cooling cleaning chamber (114). A conical sleeve (115) movably sleeved on the inner wall surface of the rectangular groove (111) is slidably sleeved on the outer surface of the alloy cable wire (13). A nitrogen box (113) is fixedly mounted on the top surface of the cleaning box (11), and the output end of the nitrogen box (113) extends to the inner wall surface of the cooling cleaning chamber (114). A motor (112) with an output end movably sleeved on the outer surface of the conical sleeve (115) is fixedly mounted on one side surface of the cleaning box (11); A backflow prevention limiting cylinder (141) is fixedly connected to the inner wall surface of the water tank (14), a conical shaping cylinder (143) movably sleeved on the outer surface of the alloy cable wire (13) is fixedly connected to the inner wall surface of the backflow prevention limiting cylinder (141), a collecting cylinder (142) is fixedly connected to the top surface of the backflow prevention limiting cylinder (141), and the inner wall surface of the water tank (14) and the outer surface of the backflow prevention limiting cylinder (141) are filled with low-temperature water (144).

5. The method for preparing a copper alloy cable with high conductivity and high toughness according to claim 4, characterized in that: A cooling chamber (145) is fixedly mounted on a side surface of the water tank (14), and a heat dissipation notch (146) is provided on the top surface of the cooling chamber (145).

6. The method for preparing a copper alloy cable with high conductivity and high toughness according to claim 3, characterized in that: A second motor (121) is fixedly mounted on a surface of one end of the support frame (12), and a clamping plate (122) is fixedly connected to an output end of the second motor (121).

7. The method for preparing a copper alloy cable with high conductivity and high toughness according to claim 6, characterized in that: A rectangular ferrule (123) is fixedly connected to the outer surface of the clamping plate (122), a limiting arc plate (124) is fixedly connected to the outer surface of the rectangular ferrule (123), the inner wall surface of the limiting arc plate (124) is movably sleeved on the outer surface of the alloy cable wire (13), and an arc-shaped positioning arm (151) is fixedly connected to one end of the connecting frame (15), and a limiting sliding strip (152) is movably sleeved on the inner wall surface of the arc-shaped positioning arm (151).

8. The method for preparing a copper alloy cable with high conductivity and high toughness according to claim 7, characterized in that: A clamping ring (153) is provided on the inner wall surface of the limiting slide bar (152), an arc-shaped plate (154) is fixedly connected to the inner wall surface of the clamping ring (153), and a closing cover (155) is detachably mounted on the outer surface of the arc-shaped plate (154).

9. The method for preparing a copper alloy cable with high conductivity and high toughness according to claim 4, characterized in that: A reflux pipe (116) is fixedly connected to the output end of the nitrogen box (113), and the other end of the reflux pipe (116) extends to the inner wall surface of the cooling and cleaning chamber (114).

Citation Information

Patent Citations

  • Flame retardation type crosslinking polyethylene insulation shield soft control cable and production technology thereof

    CN108550413A

  • Low-temperature-resistant composite cable for military industry

    CN116721804A

  • Thermoplastic cable and preparation method thereof

    CN117316502A

  • Processing device for cable shielding material

    CN218996439U