All-electric multi-pole ring pulsed magnetic field forming press
By adopting the up and down synchronous pressing method of the fully electric multipole ring pulse magnetic field forming press and the pulse charging technology of reverse winding coil winding in the multipole magnetic ring forming press, the uneven pressing and orientation of the forming press are solved. Poor problems achieve denser and uniform multipole ring molding.
Patent Information
- Application Number
- CN202411487475.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-24
- Publication Date
- 2024-11-22
AI Technical Summary
The existing multi-pole magnetic ring forming presses have problems such as uneven pressing and poor product orientation, resulting in disordered magnetic orientation after forming.
A fully electric multi-pole ring pulse magnetic field forming press is designed, adopting up and down synchronous pressing method, and multiple sets of reverse winding coil windings are set on the outer circumference of the mold to form a uniform magnetic field through pulsed magnetic charging, thereby improving molding. density and orientation of multipole magnetic rings.
The press-formed multi-pole magnetic ring is achieved to be denser, uniform and has better product orientation, solving the problems of uneven pressing and poor orientation in the prior art.
Smart Images

Figure CN119008219A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of multi-polar magnetic ring processing devices, and in particular to a full-electric multi-polar ring pulse magnetic field forming press. Background Art
[0002] The magnetic field forming press mainly includes a sealed frame, in which a powder weighing device, a feeding device and a forming device are installed. The raw material powder first enters the powder weighing device through a barrel, and the powder weighing device weighs a certain amount of raw material powder and then puts it into the feeding device. Finally, the feeding device pushes it to the forming device, and the raw material powder is put into the forming mold, and then the raw material powder is pressed into shape. The raw materials of the multi-pole magnetic ring include but are not limited to neodymium iron boron, ferrite, rubber magnet, and samarium cobalt.
[0003] Existing radiation-oriented multi-pole magnetized ring products are widely used in micro-motors. This type of magnetic ring is generally manufactured by dry pressing. Since its magnetic orientation is disordered after molding, it is necessary to place the magnetic ring in a strong magnetic field for orientation to make the magnetic orientation of all magnetic powders consistent. In the prior art, raw material powder is usually added to the mold cavity, and while the mold is closed, a high-frequency current is passed through the coil winding arranged on the periphery of the mold cavity, so that the coil winding generates a high-frequency magnetic field to orient the NdFeB powder in the mold cavity and press it. However, the existing molding press has the problems of uneven pressing and poor product orientation, so it is necessary to improve the existing molding press. Summary of the invention
[0004] The purpose of the present invention is to provide a fully electric multi-pole ring pulse magnetic field forming press, which can form multi-pole magnetic rings that are denser, more uniform and have better product orientation.
[0005] The above technical objectives of the present invention are achieved through the following technical solutions: a fully electric multi-polar ring pulse magnetic field forming press, comprising a sealed box, a powder weighing device, a feeding device and a forming device are installed in the sealed box, the forming device comprises a frame, an upper guide plate, an upper die punch, an upper electric cylinder, a mold, a lower guide plate, a lower die punch, a lower electric cylinder, a core rod and a core-pulling electric cylinder, the mold is fixedly arranged in the frame, a magnetizing component is arranged on the periphery of the mold, the magnetizing component comprises a yoke body and a plurality of coil windings, the yoke body comprises a plurality of winding parts uniformly arranged on the periphery of the mold in a circumferential direction, each winding part is wound with a coil winding, The winding directions of the coil windings on adjacent winding parts are opposite, the upper punch is fixedly connected to the lower end of the upper guide plate, the upper guide plate is arranged at the upper end of the mold and can move vertically under the action of the upper electric cylinder, the lower punch is fixedly connected to the upper end of the lower guide plate, the lower guide plate is arranged at the lower end of the mold and can move vertically under the action of the lower electric cylinder, the core rod is arranged in the middle of the frame, the core rod can be extended and retracted along the mold cavity of the mold under the action of the core-pulling electric cylinder, the lower punch extends into the mold cavity of the mold, the lower punch, the core rod and the mold form an annular cavity for filling raw material powder, and the quantitative raw material powder weighed by the powder weighing device is transferred to the annular cavity through the feeding device.
[0006] Furthermore, the outer peripheries of the plurality of magnetic yoke bodies are connected to or formed with outer magnetic conductive rings, the winding portions are evenly distributed on the inner rings of the outer magnetic conductive rings in the circumferential direction, and the outer magnetic conductive rings are made of magnetic conductive material.
[0007] Furthermore, the winding parts are provided with four groups and are evenly distributed circumferentially between the mold and the outer magnetic conductive ring.
[0008] Furthermore, the lower die punch is provided with a connecting hole with an opening at the lower end surface, and the hole diameter of the connecting hole is adapted to the outer diameter of the core rod.
[0009] Furthermore, the lower electric cylinders are provided in two groups and are symmetrically arranged on both sides of the bottom of the frame, and the output ends of the lower electric cylinders are fixedly connected to the lower guide plate.
[0010] Furthermore, an escape channel is provided through the lower die punch, the aperture of the escape channel is adapted to the core rod, and the core rod can slide vertically along the escape channel.
[0011] Furthermore, the frame is provided with a guide column, and the upper guide plate and the lower guide plate are respectively sleeved on the frame and can slide vertically along the guide column.
[0012] Furthermore, the coil winding is a pulse coil.
[0013] Furthermore, the yoke body is provided with an inwardly recessed winding space at the position corresponding to the coil winding, the coil winding is arranged in the winding space, and a cover plate is fixedly installed on the upper end of the magnetizing component, and the cover plate covers the winding space at the upper end.
[0014] Furthermore, the upper die punch includes an upper connecting part, a necking part and a lower end head which are integrally formed from top to bottom, the outer diameter of the lower end head is adapted to the inner diameter of the mold cavity, the outer diameter of the upper connecting part is smaller than the outer diameter of the lower end head, the outer diameter of the necking part gradually increases from one end adjacent to the upper connecting part to one end adjacent to the lower end head, the outer diameter of one end of the necking part adjacent to the upper connecting part is consistent with the upper connecting part, and the outer diameter of one end of the necking part adjacent to the lower end head is consistent with the lower end head.
[0015] In summary, the present invention has the following beneficial effects: 1. The all-electric multi-pole ring pulse magnetic field forming press of the present invention makes the pressed multi-pole magnetic ring more compact, more uniform and with better product orientation through the synchronous pressing of the upper and lower parts; 2. The all-electric multi-polar ring pulse magnetic field forming press of the present invention has multiple groups of winding parts evenly distributed on the periphery of the mold and coil windings are wound around the periphery of each winding part. The winding directions of the coil windings on adjacent winding parts are set in opposite directions. The coil windings are pulse-magnetized to form an externally charged multi-polar magnetic ring. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a schematic diagram of the overall structure of the present invention.
[0017] Figure 2 It is a structural schematic diagram of the molding device of the present invention from a first viewing angle.
[0018] Figure 3 The present invention Figure 2 Enlarged view of point A.
[0019] Figure 4 The present invention Figure 2 Enlarged view of point B.
[0020] Figure 5 It is a structural schematic diagram of the molding device of the present invention from a second viewing angle.
[0021] Figure 6 It is a longitudinal cross-sectional view of the magnetizing assembly of the present invention.
[0022] Figure 7 It is a transverse cross-sectional view of the magnetizing assembly of the present invention.
[0023] Figure 8 It is the magnetic force line distribution diagram of the multi-pole magnetic ring of the present invention.
[0024] In the figure: 10, forming device; 20, frame; 21, guide column; 30, upper guide plate; 31, upper punch; 311, upper connecting part; 312, necking part; 313, lower end; 40, upper electric cylinder; 50, mold; 51, fixing seat; 60, lower guide plate; 61, lower punch; 611, avoidance channel; 70, lower electric cylinder; 80, core rod; 90, core-pulling electric cylinder; 100, magnetizing component; 1001, yoke body; 1002, coil winding; 1003, winding part; 1004, outer magnetic ring; 1005, winding space; 110, cover plate; 1101, upper column section; 1102, lower column section; 120, mounting plate. DETAILED DESCRIPTION
[0025] The present invention will be further described below in conjunction with the accompanying drawings.
[0026] like Figure 1-Figure 8 As shown, a fully electric multi-polar ring pulse magnetic field forming press includes a sealed box body, in which a powder weighing device, a feeding device and a forming device 10 are installed. The feeding device can reciprocate between the powder weighing device and the forming device 10. After the powder weighing device weighs a certain amount of raw material powder, the feeding device fills the raw material powder into the mold cavity of the mold 50 in batches. In the present invention, the powder weighing device and the feeding device are not drawn. Since the powder weighing device and the feeding device are prior art, they are not described in detail in the present invention.
[0027] The molding device 10 includes a frame 20, an upper guide plate 30, an upper die punch 31, an upper electric cylinder 40, a mold 50, a lower guide plate 60, a lower die punch 61, a lower electric cylinder 70, a core rod 80 and a core-pulling electric cylinder 90. The mold 50 is fixedly arranged in the frame 20. Specifically, a mounting plate 120 is fixedly arranged in the middle of the frame 20, and a fixing seat 51 is connected to the mounting plate 120. The mold 50 is fixedly arranged in the middle position of the fixing seat 51. A magnetizing component 100 is arranged on the periphery of the mold 50. The magnetizing component 100 includes a yoke body 1001 and a plurality of coil windings. Group 1002, the yoke body 1001 includes a plurality of winding parts 1003 uniformly arranged circumferentially on the outer periphery of the mold 50, each winding part 1003 is wound with a coil winding 1002, and the winding directions of the coil windings 1002 on adjacent winding parts 1003 are opposite. Specifically, the upper end surface of the fixed seat 51 is provided with a mounting groove into which the magnetizing component 100 partially extends, and the magnetizing component 100 is fixedly arranged on the mounting groove of the fixed seat 51. The setting of the mounting groove can improve the assembly efficiency, that is, it is convenient to position the magnetizing component 100 in the mounting groove.
[0028] The upper electric cylinder 40 is fixedly installed in the middle position of the top of the frame 20, the upper guide plate 30 is arranged at the upper end of the mold 50 and can move vertically under the action of the upper electric cylinder 40, the upper die punch 31 is fixedly connected to the lower end of the upper guide plate 30, the lower electric cylinder 70 and the core-pulling electric cylinder 90 are fixedly installed at the bottom of the frame 20, the lower guide plate 60 is arranged at the lower end of the mold 50 and can move vertically under the action of the lower electric cylinder 70, the lower die punch 61 is fixedly connected to the upper end of the lower guide plate 60, the core rod 80 is arranged in the middle of the frame 20, the core rod 80 can be extended and retracted along the mold cavity of the mold 50 under the action of the core-pulling electric cylinder 90, the lower die punch 61 extends into the mold cavity of the mold 50, the lower die punch 61, the core rod 80 and the mold 50 form an annular cavity for filling raw material powder, and the quantitative raw material powder weighed by the powder weighing device is transferred to the annular cavity through the feeding device.
[0029] In some embodiments, the outer periphery of the plurality of magnetic yoke bodies 1001 is connected to or formed with an outer magnetic conductive ring 1004, and the winding portion 1003 is evenly distributed circumferentially on the inner ring of the outer magnetic conductive ring 1004. The provision of the outer magnetic conductive ring 1004 can effectively prevent the magnetic field from leaking, thereby effectively improving the magnetic field strength of the outer ring of the multi-polar magnetic ring.
[0030] In some embodiments, the winding portion 1003 is provided with four groups and is evenly distributed circumferentially between the mold 50 and the outer magnetic conductive ring 1004 . The yoke body 1001 is adjacent to the upper and lower ends of the inner side of the mold 50 and has winding spaces 1005 . The coil winding 1002 is wound in the winding space 1005 of the yoke body 1001 .
[0031] In some embodiments, the lower punch 61 is provided with a connecting hole with an opening on the lower end face, and the aperture of the connecting hole is adapted to the outer diameter of the core rod 80. The present invention provides a connecting hole on the lower end face of the upper punch 31. During pressing, the upper punch 31 partially extends into the mold cavity and the core rod 80 extends into the connecting hole, thereby playing a positioning role, so that when pressing the raw material powder, the upper punch 31 and the core rod 80 can move downward smoothly and synchronously.
[0032] In some embodiments, two groups of lower electric cylinders 70 are provided and symmetrically arranged on both sides of the bottom of the frame 20. The output end of the lower electric cylinder 70 is fixedly connected to the lower guide plate 60. Specifically, the two lower electric cylinders 70 are a left lower electric cylinder 70 and a right lower electric cylinder 70. By providing two groups of lower electric cylinders 70, the two groups of lower electric cylinders 70 can improve the stability of driving the lower guide plate 60 to move while avoiding the core pulling electric cylinder 90.
[0033] In some embodiments, an avoidance channel 611 is provided through the lower punch 61, the aperture of the avoidance channel 611 is adapted to the core rod 80, the core rod 80 can slide vertically along the avoidance channel 611, and the avoidance channel 611 of the lower punch 61 and the core rod 80 are adapted to each other so that the core rod 80 and the lower punch 61 can slide smoothly against each other.
[0034] In some embodiments, the frame 20 is provided with a guide column 21, and the upper guide plate 30 and the lower guide plate 60 are respectively mounted on the frame 20 and can slide vertically along the guide column 21. Through the setting of the guide column 21, the stability of the upper guide plate 30 and the lower guide plate 60 during movement can be improved.
[0035] The coil winding 1002 is a pulse coil, and the magnetizing power supply of the all-electric multi-pole ring pulse magnetic field forming press includes four capacitors, and each group of capacitors is discharged in turn.
[0036] The yoke body 1001 is provided with an inwardly recessed winding space 1005 at a position corresponding to the coil winding 1002. The coil winding 1002 is provided at the winding space 1005. A cover plate 110 is fixedly installed at the upper end of the magnetizing component 100. The cover plate 110 covers the winding space 1005 at the upper end, and the winding space 1005 at the lower end is covered by a fixing seat 51. This arrangement can protect the coil winding 1002. In addition, the cover plate 110 of the present invention is provided by an upper column. The upper column segment 1101 and the lower column segment 1102 are composed or integrally formed, wherein the outer diameter of the upper column segment 1101 is smaller than the outer diameter of the lower column segment 1102, the inner diameter of the upper column segment 1101 is matched with the outer diameter of the mold 50, the upper end surface of the mold 50 is flush with the upper end surface of the upper column segment 1101, and the cover plate 110 plays a protective role when the feeding device (i.e., the feeding trolley) transfers the raw material powder into the mold 50. The setting of the upper column segment 1101 can play a protective role and prevent the feeding device from colliding with the mold 50.
[0037] In some embodiments, the upper punch 31 includes an upper connecting portion 311, a necking portion 312 and a lower end head 313 integrally formed from top to bottom, the outer diameter of the lower end head 313 is adapted to the inner diameter of the mold cavity of the mold 50, the outer diameter of the upper connecting portion 311 is smaller than the outer diameter of the lower end head 313, the outer diameter of the necking portion 312 gradually increases from one end adjacent to the upper connecting portion 311 to one end adjacent to the lower end head 313, the outer diameter of the end of the necking portion 312 adjacent to the upper connecting portion 311 is consistent with the upper connecting portion 311, and the outer diameter of the end of the necking portion 312 adjacent to the lower end head 313 is consistent with the lower end head 313. By designing the upper punch 31, the friction between the upper punch 31 and the mold 50 can be reduced when the upper punch 31 is pressed down.
[0038] In summary, the present invention has the following beneficial effects: 1. The all-electric multi-pole ring pulse magnetic field forming press of the present invention makes the pressed multi-pole magnetic ring more compact, more uniform and with better product orientation through the synchronous pressing of the upper and lower parts; 2. The all-electric multi-polar ring pulse magnetic field forming press of the present invention has multiple groups of winding parts 1003 evenly distributed on the periphery of the mold 50 and coil windings 1002 wound around the periphery of each winding part 1003, and the winding directions of the coil windings 1002 on adjacent winding parts 1003 are set in opposite directions. The coil windings 1002 are pulse-magnetized to form an externally charged multi-polar magnetic ring.
[0039] The method for forming a multi-polar magnetic ring of the present invention comprises the following steps: S1: Spraying a release agent: The core-pulling electric cylinder 90 drives the core rod 80 to move to a position where the upper end surface of the core rod 80 is 10 mm-20 mm lower than the upper end surface of the mold 50, and the release agent spraying device sprays the release agent into the mold cavity.
[0040] S2: Filling raw material powder: The raw material powder that has been quantitatively weighed is transferred into the mold 50 by a feeding device.
[0041] S3: (1) Pre-pressing the upper punch 31: the core rod 80 and the lower punch 61 remain stationary, and the upper electric cylinder 40 drives the upper punch 31 to move downward into the die cavity to pre-press the raw material powder, that is, the upper electric cylinder 40 quickly moves down to the pre-pressing position; (2) Pre-pressing the lower punch 61: the upper punch 31 and the core rod 80 remain stationary, and the lower electric cylinder 70 moves upward to pre-press the raw material powder and press the raw material powder to the magnetization center position.
[0042] S4: Magnetization: The multiple groups of coil windings 1002 are energized by a magnetization power supply, and the coil windings 1002 perform pulse magnetization on the formed magnetic rings in the mold 50 .
[0043] S5: Pressing and forming: the upper electric cylinder 40 drives the upper punch 31 to move downward, the core-pulling electric cylinder 90 drives the core rod 80 to move downward, and the lower electric cylinder 70 drives the lower punch 61 to move upward, wherein the upper end surface of the lower punch 61, the lower end surface of the upper punch 31 and the core rod 80 are all synchronously moved to the magnetization center position, thereby pressing the raw material powder in the die cavity for T1min until the pressing is completed; S6: Demagnetization: After the pressing is completed, the coil winding 1002 stops magnetizing the formed multi-polar magnetic ring. At this time, the upper electric cylinder 40 drives the upper die punch 31 to slightly lift a short distance.
[0044] S7: Demolding: The upper electric cylinder 40 drives the upper punch 31 to move upward, the lower electric cylinder 70 drives the lower punch 61 to move upward, and the core-pulling electric cylinder 90 drives the core rod 80 to move upward, thereby demolding the formed multi-polar magnetic ring. In step S7, when the lower punch 61 moves up until its upper end surface is flush with the upper end surface of the mold 50, the core-pulling electric cylinder 90 drives the core rod 80 to move down into the mold cavity.
[0045] Before step S1 or during step S1, a certain amount of NdFeB powder is weighed by a powder weighing device, and after the powder weighing device completes the weighing, the raw material powder is transferred to a powder box of a feeding device.
[0046] The above description is only a preferred embodiment of the present invention, so all equivalent changes or modifications made according to the structure, characteristics and principles described in the scope of the patent application of the present invention are included in the scope of the patent application of the present invention.
Claims
1. A fully electric multi-pole ring pulse magnetic field forming press, comprising a sealed box, in which a powder weighing device, a feeding device and a forming device (10) are installed, characterized in that: The forming device (10) comprises a frame (20), an upper guide plate (30), an upper die punch (31), an upper electric cylinder (40), a mold (50), a lower guide plate (60), a lower die punch (61), a lower electric cylinder (70), a core rod (80) and a core-pulling electric cylinder (90); the mold (50) is fixedly arranged in the frame (20); a magnetizing component (100) is arranged on the periphery of the mold (50); the magnetizing component (100) comprises a yoke body (1001) and a plurality of coil windings (1002); the yoke body (1001) comprises a plurality of winding parts (1003) uniformly arranged on the periphery of the mold (50); each winding part (1003) is wound with a coil winding (1002); the winding directions of the coil windings (1002) on adjacent winding parts (1003) are opposite. On the contrary, the upper die punch (31) is fixedly connected to the lower end of the upper guide plate (30), the upper guide plate (30) is arranged at the upper end of the mold (50) and can move vertically under the action of the upper electric cylinder (40), the lower die punch (61) is fixedly connected to the upper end of the lower guide plate (60), the lower guide plate (60) is arranged at the lower end of the mold (50) and can move vertically under the action of the lower electric cylinder (70), the core rod (80) is arranged in the middle of the frame (20), the core rod (80) can be extended and retracted along the mold cavity of the mold (50) under the action of the core pulling electric cylinder (90), the lower die punch (61) extends into the mold cavity of the mold (50), the lower die punch (61), the core rod (80) and the mold (50) form an annular cavity for filling raw material powder, and the quantitative raw material powder weighed by the powder weighing device is transferred to the annular cavity through the feeding device.
2. The all-electric multi-polar ring pulse magnetic field forming press according to claim 1, characterized in that: An outer magnetic conductive ring (1004) is connected to or formed on the outer periphery of the plurality of magnetic yoke bodies (1001), and the winding parts (1003) are evenly distributed in the inner circle of the outer magnetic conductive ring (1004) in the circumferential direction.
3. The all-electric multi-polar ring pulse magnetic field forming press according to claim 2, characterized in that: The winding parts (1003) are provided in four groups and are evenly distributed in the circumferential direction between the mold (50) and the outer magnetic conductive ring (1004).
4. The all-electric multi-polar ring pulse magnetic field forming press according to claim 1, characterized in that: The lower die punch (61) is provided with a communicating hole with an opening at the lower end surface, and the hole diameter of the communicating hole is matched with the outer diameter of the core rod (80).
5. The all-electric multi-polar ring pulse magnetic field forming press according to claim 1, characterized in that: The lower electric cylinders (70) are provided in two groups and are symmetrically arranged on both sides of the bottom of the frame (20), and the output ends of the lower electric cylinders (70) are fixedly connected to the lower guide plate (60).
6. The all-electric multi-polar ring pulse magnetic field forming press according to claim 5, characterized in that: An escape channel (611) is provided through the lower die punch (61), the aperture of the escape channel (611) is adapted to the core rod (80), and the core rod (80) can slide vertically along the escape channel (611).
7. The all-electric multi-polar ring pulse magnetic field forming press according to claim 1, characterized in that: The frame (20) is provided with a guide column (21), and the upper guide plate (30) and the lower guide plate (60) are respectively sleeved on the frame (20) and can slide vertically along the guide column (21).
8. A fully electric multi-polar ring pulse magnetic field forming press according to any one of claims 1 to 7, characterized in that: The coil winding (1002) is a pulse coil.
9. The all-electric multi-polar ring pulse magnetic field forming press according to claim 8, characterized in that: The yoke body (1001) is provided with an inwardly recessed winding space (1005) at a position corresponding to the coil winding (1002); the coil winding (1002) is arranged in the winding space (1005); a cover plate (110) is fixedly mounted on the upper end of the magnetizing component (100); the cover plate (110) covers the winding space (1005) at the upper end.
10. The all-electric multi-polar ring pulse magnetic field forming press according to claim 1, characterized in that: The upper die punch (31) comprises an upper connecting portion (311), a necking portion (312) and a lower end head (313) which are integrally formed from top to bottom. The outer diameter of the lower end head (313) is adapted to the inner diameter of the mold cavity of the mold (50). The outer diameter of the upper connecting portion (311) is smaller than the outer diameter of the lower end head (313). The outer diameter of the necking portion (312) gradually increases from one end adjacent to the upper connecting portion (311) to one end adjacent to the lower end head (313). The outer diameter of one end of the necking portion (312) adjacent to the upper connecting portion (311) is consistent with that of the upper connecting portion (311), and the outer diameter of one end of the necking portion (312) adjacent to the lower end head (313) is consistent with that of the lower end head (313).
Citation Information
Patent Citations
Magnetic aligning device of aeolotropism adhesive bonding or sintered multipolar annular magnetic body
CN101118807A
Multi-pole magnetic ring orientation and magnetization clamp and method
CN106252023A
Full-automatic floating type magnetic field forming press for radiation rings
CN108247046A
Suspension type self-adaptive hot pressing system of full-automatic floating type hot-pressing molding press
CN108247932A
Anisotropic inner circle orientation multi-pole magnetic ring and mold and preparation method thereof
CN112086259A
Cited By
Pulsed magnetic field forming press and forming method
CN121244957A