Formation method of semiconductor structure

By forming a compensation layer on the substrate surface and performing source-drain doping during the process of the semiconductor structure, the problems of damage and depression in the active region are solved, and the electrical performance and quality of the semiconductor structure are improved.

CN119008413AActive Publication Date: 2024-11-22ZHEJIANG ICSPROUT SEMICONDUCTOR CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202411140194.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-22
Estimated Expiration
2044-08-19

AI Technical Summary

Technical Problem

The existing semiconductor structures are prone to damage and depression in the active area during the process, resulting in increased contact resistance of the device and decreased electrical performance, and these structural defects are difficult to detect and repair.

Method used

After forming the gate layer and side wall on the surface of the semiconductor substrate, the oxide layer is etched and removed to expose the substrate, and a compensation layer is formed on the substrate surface to perform source-drain doping to ensure that the top of the compensation layer is higher than the bottom of the gate layer. This forms a source-drain doped region that is not easily recessed, and improves the formation quality of the doped region.

Benefits of technology

Through the existence of the compensation layer, the recessed defects on the surface of the source-drain doped region are eliminated, contact resistance is reduced, electrical performance is improved, and the overall performance and quality of the semiconductor structure are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008413A_ABST
    Figure CN119008413A_ABST
Patent Text Reader

Abstract

The invention provides a method for forming a semiconductor structure. The method comprises the following steps: providing a substrate; forming a first oxide layer on the surface of the substrate; forming a gate layer on the surface of a part of the first oxide layer; forming a side wall on the side wall of the gate layer; etching to remove the first oxide layer at the two sides of the side wall until the surface of the substrate is exposed; forming a compensation layer on the surface of the exposed substrate, wherein the top surface of the compensation layer is higher than the bottom surface of the gate layer; source and drain doping is carried out on the substrate at the two sides of the side wall to form a source and drain doped region; the compensation layer higher than the bottom surface of the gate layer is removed, due to the existence of the compensation layer, the surfaces of the substrate on the two sides of the side wall are compensated, and after the source-drain doped region is formed, the top surface of the source-drain doped region is not lower than the bottom surface of the gate layer, so that the defect that the surface of the source-drain doped region is sunken is eliminated; and the forming quality of the source-drain doped region is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor manufacturing, and in particular to a method for forming a semiconductor structure. Background Art

[0002] Silicon substrate damage, also known as active area damage (AA Damage), usually refers to the loss of silicon caused by an unhealthy process flow, which is generally caused by factors such as dry etching, wet corrosion, natural oxidation, and stripping processes.

[0003] Severe active area damage can cause the device to lose function. Large silicon voids can usually be easily detected by defect analysis equipment. This type of damage is not allowed. Weak active area damage is usually called active area recess (AA Recess), which will increase the contact resistance of the device on the wafer and reduce the electrical performance. This structural defect is difficult to detect by non-destructive methods.

[0004] Therefore, how to reduce or even eliminate the depression and damage in the active area is a technical problem that needs to be solved urgently. Summary of the invention

[0005] The technical problem solved by the present invention is to provide a method for forming a semiconductor structure to improve the performance of the semiconductor structure.

[0006] To solve the above problems, the present invention provides a method for forming a semiconductor structure, comprising: providing a substrate; forming a first oxide layer on the surface of the substrate; forming a gate layer on the surface of a portion of the first oxide layer; forming a sidewall on the sidewall of the gate layer; etching and removing the first oxide layer on both sides of the sidewall until the surface of the substrate is exposed; forming a compensation layer on the exposed surface of the substrate, wherein the top surface of the compensation layer is higher than the bottom surface of the gate layer; performing source-drain doping on the substrate on both sides of the sidewall to form a source-drain doping region; and removing the compensation layer that is higher than the bottom surface of the gate layer.

[0007] Optionally, a metal silicide is formed on the top of the gate layer and the top surface of the source-drain doped region, and the top surface of the metal silicide is flush with the top surface of the substrate.

[0008] Optionally, the material of the compensation layer includes silicon or silicon germanium.

[0009] Optionally, after forming the gate layer and before forming the sidewalls, the method further includes implanting lightly doped drain ions into the substrate at both sides of the gate layer to form a lightly doped drain structure.

[0010] Optionally, the ion type of the lightly doped drain ion implantation is the same as the ion type of the source and drain doping.

[0011] Optionally, after the compensation layer is formed, a portion of the compensation layer is oxidized, and a compensation layer oxide is formed on the surface of the compensation layer that is not oxidized.

[0012] Optionally, the method for removing the compensation layer includes: removing the compensation layer oxide and a portion of the compensation layer until the surface is flush with the surface of the substrate.

[0013] Optionally, before forming the sidewall spacer, the method further includes: forming a second oxide layer on the sidewall of the gate layer, wherein the second oxide layer is also formed on the top surface of the gate layer.

[0014] Optionally, the second oxide layer on the top surface of the gate layer is removed while removing the compensation layer.

[0015] Optionally, during the source-drain doping process, the source-drain doping ions are simultaneously doped into a portion of the compensation layer in contact with the surface of the substrate.

[0016] Compared with the prior art, the technical solution of the present invention has the following advantages:

[0017] In the method for forming a semiconductor structure of the present invention, after a gate layer is formed on the substrate, a sidewall is formed on the sidewall of the gate layer, and the first oxide layer on both sides of the sidewall is etched away to expose the surface of the substrate. In the process of etching away the first oxide layer, damage is caused to the substrate at the bottom of the first oxide layer, causing loss of the substrate and causing a depression. At this time, a compensation layer is formed on the surface of the exposed substrate, and the top surface of the compensation layer is higher than the bottom surface of the gate layer. Source and drain doping is performed on the substrate on both sides of the sidewall to form a source and drain doping region. In the process of forming the source and drain doping region, due to the presence of the compensation layer, the surface of the substrate on both sides of the sidewall is compensated. After the source and drain doping region is formed, the top surface of the source and drain doping region will not be lower than the bottom surface of the gate layer, thereby eliminating the defect of the surface depression of the source and drain doping region and improving the formation quality of the source and drain doping region. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figures 1 to 4 is a schematic structural diagram of each step of a method for forming a semiconductor structure in one embodiment;

[0019] Figures 5 to 12 It is a schematic structural diagram of each step of a method for forming a semiconductor structure in one embodiment of the present invention. DETAILED DESCRIPTION

[0020] As the background technology, the performance of the existing semiconductor structure is poor. Figures 1 to 4 Provide explanation.

[0021] First, please refer to Figure 1, a substrate 100; oxidizing the surface of the substrate 100 to form an oxide layer 101; forming a gate layer 102 on a portion of the surface of the oxide layer 101; and forming a spacer layer 103 on the surface of the oxide layer 101 and the sidewall and top surface of the gate layer 102.

[0022] Please refer to Figure 2 , the spacer layer 103 is etched to form a spacer 104 on the sidewall of the gate layer 102 .

[0023] Please refer to Figure 3 , source-drain doping is performed on the substrate 100 on both sides of the sidewall 104 , and source-drain doping regions 105 are formed in the substrate 100 on both sides of the sidewall 104 .

[0024] Please refer to Figure 4 , the oxide layer 102 on the surface of the substrate 100 on both sides of the sidewall 104 is removed by etching to expose the top surface of the source / drain doped region 105 , and a metal silicide 106 is formed on the exposed top surface of the source / drain doped region 105 .

[0025] The inventors have found that the top surface of the source-drain doped region 105 formed by the above method is concave, which increases the contact resistance of the device and reduces the electrical performance. In addition, the defect of the concave source-drain doped region 105 is difficult to be detected by a non-destructive method, which greatly reduces the performance and quality of the semiconductor structure finally formed. This is because in the process of etching the sidewall layer 103, the oxide layer 101 at the bottom of the sidewall layer 103 is also partially etched away, thereby exposing the substrate 100 at the bottom. The exposed substrate 100 is also etched away during the etching process of the sidewall layer 103, so that the substrate 100 on both sides of the sidewall 104 is concave. In this way, the source-drain doped region 105 formed in the process of source-drain doping the substrate 100 on both sides of the sidewall 104 is also concave.

[0026] The inventors have found through research that after a gate layer is formed on the substrate, a side wall is formed on the side wall of the gate layer, and the first oxide layer on both sides of the side wall is etched away to expose the surface of the substrate. In the process of etching away the first oxide layer, damage is caused to the substrate at the bottom of the first oxide layer, causing loss of the substrate and causing a depression. At this time, a compensation layer is formed on the surface of the exposed substrate, and the top surface of the compensation layer is higher than the bottom surface of the gate layer. The substrate on both sides of the side wall is doped with a source or drain to form a source or drain doped region. In the process of forming the source or drain doped region, due to the presence of the compensation layer, the surface of the substrate on both sides of the side wall is compensated. After the source or drain doped region is formed, the top surface of the source or drain doped region will not be lower than the bottom surface of the gate layer, thereby eliminating the defect of the surface depression of the source or drain doped region, improving the formation quality of the source or drain doped region, and then reducing the contact resistance and improving the electrical performance.

[0027] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0028] First, please refer to Figure 5 , providing a substrate 200.

[0029] In this embodiment, the material of the substrate 200 is single crystal silicon.

[0030] In other embodiments, the material of the substrate 200 may also be semiconductor materials such as polycrystalline silicon or amorphous silicon, germanium, silicon germanium, gallium arsenide, etc.

[0031] In this embodiment, after providing the substrate 200 , the process further includes doping the substrate 200 to form a well region.

[0032] Please refer to Figure 6 , a first oxide layer 201 is formed on the surface of the substrate 200 .

[0033] In this embodiment, furnace tube thermal oxidation is used to grow a thick first oxide layer 201 on the surface of the substrate 200, and the first oxide layer 201 serves as a gate oxide layer.

[0034] In this embodiment, the first oxide layer 201 can also protect the substrate 200 to prevent impurities in the photoresist from diffusing into the substrate 200 during subsequent use of the photoresist, thereby ensuring the quality of the substrate 200.

[0035] Please refer to Figure 7 , a gate layer 202 is formed on a portion of the surface of the first oxide layer 201 .

[0036] In this embodiment, the material of the gate layer 202 is polysilicon.

[0037] In this embodiment, the method for forming the gate layer 202 includes: forming an initial gate layer 202 on the surface of the first oxide layer 201 ; patterning the initial gate layer 202 , and forming the gate layer 202 on a portion of the surface of the first oxide layer 201 .

[0038] In this embodiment, the process further includes: performing lightly doped drain ion implantation on the substrate 200 at both sides of the gate layer 202 to form a lightly doped drain structure 203 .

[0039] In this embodiment, the lightly doped drain structure 203 is used to form a low-doped extension region below the boundary of the gate layer 202 and between the source and drain. The extension region forms an impurity concentration gradient between the source and drain and the channel, thereby reducing the peak electric field near the drain and improving the reliability of the semiconductor structure.

[0040] In this embodiment, the ion type of the lightly doped drain ion implantation includes one of N-type ions and P-type ions. Specifically, for a PMOS transistor, the ion type of the lightly doped drain ion implantation may be BF 2 ; For NMOS transistors, the ions implanted into the lightly doped drain ions may be As.

[0041] In this embodiment, the method further includes: forming a second oxide layer 204 on the sidewall of the gate layer 202 , and the second oxide layer 204 is also formed on the top surface of the gate layer 202 .

[0042] In this embodiment, the purpose of forming the second oxide layer 204 on the sidewall and top surface of the gate layer 202 by using an oxidation process is to repair the gate layer 202 , thereby improving the quality of the gate layer 202 .

[0043] In this embodiment, the material of the second oxide layer 204 is silicon oxide.

[0044] Please refer to Figure 8 , forming a sidewall spacer 205 on the sidewall of the gate layer 202 .

[0045] In this embodiment, an initial spacer layer is formed on the surfaces of the second oxide layer 204 and the first oxide layer 201 ; the initial spacer layer is etched to form the spacer 205 on the surface of the second oxide layer 204 on the side wall of the gate layer 202 .

[0046] In this embodiment, the sidewall spacer 205 can protect the lightly doped drain structure 203 to prevent ions from being implanted into the extended region of the lightly doped drain structure 203 during the subsequent source and drain doping process.

[0047] In this embodiment, the material of the sidewall spacer 205 is silicon nitride.

[0048] In this embodiment, the process of etching the initial sidewall layer is an anisotropic dry etching process, and the etching gas of the anisotropic dry etching is Cl 2 and CF 4 .

[0049] Please refer to Fig. 9 , the first oxide layer 201 on both sides of the sidewall 205 is removed by etching until the surface of the substrate 200 is exposed.

[0050] In this embodiment, the process of etching and removing the first oxide layer 201 on both sides of the sidewall spacer 205 is a wet etching process.

[0051] In other embodiments, the first oxide layer 201 on both sides of the sidewall 205 may be removed by dry etching or other processes.

[0052] Please refer to Fig.10 A compensation layer 206 is formed on the exposed surface of the substrate 200 , and a top surface of the compensation layer 206 is higher than a bottom surface of the gate layer 202 .

[0053] In this embodiment, the material of the compensation layer 206 is silicon.

[0054] In other embodiments, the material of the compensation layer 206 may also be silicon germanium.

[0055] In this embodiment, the formation process of the compensation layer 206 is an epitaxial growth process, and the process parameters of the epitaxial growth process include the gas used including hydrogen (H 2 ), Hydrogen chloride (HCl) gas, DCS gas, SiH 4 Gas and B 2 H 6 Gas; wherein the hydrogen (H 2 ) gas flow rate is 10 to 3000 sccm; the gas flow rate of the hydrogen chloride (HCl) gas is 10 to 250 sccm; the gas flow rate of the DCS gas is 20 to 2500 sccm; the SiH 4 The gas flow rate of the gas is 10 to 700 sccm; 2 H 6 The gas flow rate of the gas is 5 to 400 sccm; the pressure range is 8 to 300 mTorr; and the temperature range is 600 to 850°C.

[0056] In this embodiment, the compensation layer 206 fills the depression in the substrate 200, so that the depressed part is filled and compensated, raising the surface of the substrate 200 on both sides of the side wall 205, eliminating the defect of the depression of the substrate 200, thereby helping to subsequently reduce the contact resistance and improve the electrical performance.

[0057] Please refer to Fig.11 , source-drain doping is performed on the substrate 200 on both sides of the sidewall 205 to form a source-drain doped region 207 .

[0058] In this embodiment, the ion type of the lightly doped drain ion implantation is the same as the ion type of the source and drain doping.

[0059] In this embodiment, during the source-drain doping process, the source-drain doping ions are simultaneously doped into the portion of the compensation layer 206 that is in contact with the surface of the substrate 200 .

[0060] In this embodiment, since silicon material is easily oxidized, after the compensation layer 206 is formed, part of the compensation layer 206 is oxidized, and a compensation layer oxide 206 b is formed on the surface of the unoxidized compensation layer 206 a.

[0061] Please refer to Fig.12 , remove the compensation layer 206 , and form a metal silicide 208 on the top of the gate layer 202 and the top surface of the source-drain doped region 207 , and the top surface of the metal silicide 208 is flush with the top surface of the substrate 200 .

[0062] In this embodiment, due to the presence of the compensation layer 206, the surface of the substrate 200 on both sides of the side wall 205 is compensated. After the source-drain doping region 207 is formed, the top surface of the source-drain doping region 207 will not be lower than the bottom surface of the gate layer 202, thereby eliminating the surface depression defect of the source-drain doping region 207, improving the formation quality of the source-drain doping region 207, and then reducing the contact resistance and improving the electrical performance.

[0063] In this embodiment, the method for removing the compensation layer 206 includes: removing the oxide of the compensation layer 206 and a portion of the compensation layer 206 until the surface is flush with the surface of the substrate 200 .

[0064] In this embodiment, the second oxide layer 204 on the top surface of the gate layer 202 is removed while the compensation layer 206 is removed.

[0065] In this embodiment, the method for forming the metal silicide 208 includes: forming a metal layer on the top surface of the gate layer 202 and the surface of the source and drain doping region 207 and a barrier layer formed on the surface of the metal layer, wherein the barrier layer prevents the metal layer from flowing during the rapid thermal annealing stage, resulting in uneven thickness of the metal silicide 208 and locally uneven resistance value.

[0066] In this embodiment, during the first rapid thermal annealing process, the metal layer is used to react with the substrate 200 and the gate layer 202 of the source and drain doping regions 207 to generate a high-resistance metal silicide 208; wet etching is used to remove the barrier layer and the unreacted metal layer to prevent bridging and circuit short circuit; and a second rapid thermal annealing is performed to transform the high-resistance metal silicide 208 into a low-resistance metal silicide 208.

[0067] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A method for forming a semiconductor structure, characterized in that: include: providing a substrate; forming a first oxide layer on the surface of the substrate; forming a gate layer on a surface of a portion of the first oxide layer; forming a sidewall spacer on a sidewall of the gate layer; Etching and removing the first oxide layer on both sides of the sidewall until the surface of the substrate is exposed; forming a compensation layer on the exposed surface of the substrate, wherein a top surface of the compensation layer is higher than a bottom surface of the gate layer; Performing source-drain doping on the substrate at both sides of the sidewall to form source-drain doped regions; The compensation layer is removed above a bottom surface of the gate layer.

2. The method for forming a semiconductor structure according to claim 1, wherein: A metal silicide is formed on the top of the gate layer and the top surface of the source-drain doped region, and the top surface of the metal silicide is flush with the top surface of the substrate.

3. The method for forming a semiconductor structure according to claim 1, wherein: The material of the compensation layer includes silicon and silicon germanium.

4. The method for forming a semiconductor structure according to claim 1, wherein: After forming the gate layer and before forming the sidewalls, the method further includes implanting lightly doped drain ions into the substrate at both sides of the gate layer to form a lightly doped drain structure.

5. The method for forming a semiconductor structure according to claim 4, wherein: The ion type of the lightly doped drain ion implantation is the same as the ion type of the source and drain doping.

6. The method for forming a semiconductor structure according to claim 1, wherein: After the compensation layer is formed, a portion of the compensation layer is oxidized, and a compensation layer oxide is formed on the surface of the compensation layer that is not oxidized.

7. The method for forming a semiconductor structure according to claim 6, wherein: The method for removing the compensation layer includes: removing the compensation layer oxide and a portion of the compensation layer until the surface is flush with the surface of the substrate.

8. The method for forming a semiconductor structure according to claim 1, wherein: Before forming the sidewall spacer, the method further includes: forming a second oxide layer on the sidewall of the gate layer, wherein the second oxide layer is also formed on the top surface of the gate layer.

9. The method for forming a semiconductor structure according to claim 8, wherein: The second oxide layer on the top surface of the gate layer is removed while the compensation layer is removed.

10. The method for forming a semiconductor structure according to claim 1, wherein: During the source-drain doping process, the source-drain doping ions are simultaneously doped into the portion of the compensation layer that is in contact with the surface of the substrate.

Citation Information

Patent Citations

  • Forming method of MOS (metal oxide semiconductor) transistor with buried channel

    CN102637601A

  • Semiconductor device and forming method thereof

    CN104752223A

  • Method for repairing damage on substrate in source / drain region

    CN104851775A

  • Semiconductor device and forming method thereof

    CN110957219A

  • Semiconductor device and manufacturing method thereof

    CN116646402A