Method for metalizing side wall of cavity of cavity plate

By metallizing the cavity side wall of the cavity plate, the problem of resin loss in the signal transmission of the cavity plate is solved, the signal contact with the metal is realized, the loss is reduced, and the signal integrity is ensured.

CN119012573APending Publication Date: 2024-11-22AOSHIKANG TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411389456.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-08
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The cavity side walls of the existing cavity plates are not metallized, causing the signal to come into contact with the exposed resin during transmission, causing certain losses.

Method used

A method of metallization of the cavity side wall of the cavity plate, including preparing copper-free substrate, single-sided bonding pure glue, performing gong groove operation and single-sided lamination cooperation, and then performing a selective electroplating process to adjust the cavity Metalization is carried out internally and the copper slurry is sintered to ensure metalization of the side wall of the cavity.

Benefits of technology

Through metallization processing, all signals are in contact with metal to avoid contact with resin, effectively reducing signal loss and ensuring signal integrity and low loss.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119012573A_ABST
    Figure CN119012573A_ABST
Patent Text Reader

Abstract

The invention provides a method for metallizing the side wall of a cavity of a cavity plate. The method comprises the following steps: S1, preparing a copper-free substrate; s2, pure glue is attached to the single face; s3, carrying out groove milling operation; s4, single-side layer-adding lamination operation is carried out; s5, a selective electroplating process is carried out after lamination, and metallization is carried out in the cavity; s6, sintering the copper paste; s7, grooving the pure glue according to a copper paste sintering area and attaching the pure glue to the board surface; and S8, carrying out layer-adding lamination operation on the core plate on the other side. According to the method for metalizing the side wall of the cavity of the cavity board, after the side wall of the copper-free substrate is metalized, the copper paste sintering operation is carried out on the side wall, so that the metalized side wall is effectively ensured to be connected with the same layer of the upper core board, a metalized cavity is formed in a PCB in a real sense, all signals are in contact with metal, and the reliability of the PCB is improved. The contact with the resin is avoided, the signal loss is effectively reduced, the metallization of the side wall of the cavity is carried out, the integrity of the signal is effectively ensured, and the loss is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of cavity plates, and in particular to a method for metallizing a cavity side wall of a cavity plate. Background Art

[0002] As the field of communications electronics gradually develops towards high frequency and high speed of signals, higher requirements are placed on the low-loss transmission and impedance continuity of high-frequency and high-speed signals of signal lines in PCBs.

[0003] In high-speed products, it is hoped that the dielectric constant and dielectric loss factor of the material will become lower and lower. However, no matter how the material formula is improved, it is impossible to reduce the dielectric constant and dielectric loss factor of the material infinitely. Therefore, in 112G and 224G high-speed PCB applications, the reduction of dielectric loss has encountered a bottleneck. PCBs with cavities have become one of the solutions for future high-speed PCBs because the dielectric constant and dielectric loss factor of air are much lower than those of conventional resin substrates of current PCBs. PCBs with cavities (Printed Circuit Board) are circuit boards with special structures and are widely used in the field of electronics. PCBs with cavities are usually composed of multiple layers of materials. The outermost layer is an insulating substrate material, such as glass fiber reinforced epoxy resin. On the substrate, a series of complex processes are used to produce the conductive circuits and the installation positions of the electronic components. The cavity is one or more empty areas formed inside the PCB. This structure with a cavity has several important functions. First, the cavity can provide installation space for some special electronic components. For example, some components with higher heights or components that require special heat dissipation conditions can be placed in the cavity to ensure that the overall layout of the circuit board is more reasonable. Secondly, the cavity can also play a role in isolation and shielding. In some applications that are sensitive to signal interference, the cavity can effectively reduce the electromagnetic interference between different circuits and improve the performance and stability of the circuit. When making a PCB with a cavity, special processes and technologies are required. First, the position, size and shape of the cavity must be accurately planned in the design stage, and then Finally, in the manufacturing process, the formation of the cavity is achieved through lamination, drilling, etching and other process steps. Among them, the lamination process is to press multiple layers of materials together to form an overall circuit board structure, the drilling process is used to drill holes connecting different layers at specific locations, and the etching process is used to make conductive lines. PCBs with cavities have important applications in many fields. For example, in high-end electronic products such as communication equipment, computers, and medical equipment, PCBs with cavities can meet the strict requirements on circuit performance and spatial layout. At the same time, with the continuous development of electronic technology, the demand for PCBs with cavities is also increasing, which promotes the continuous innovation and progress of PCB manufacturing technology. In short, PCBs with cavities are a printed circuit board with special structure and important application value. Through ingenious design and advanced manufacturing technology, it provides strong support for the high performance and miniaturization of electronic equipment.

[0004] The existing cavity board method is to form the core board of the cavity layer, use a molding machine to gong out the shape of the cavity, and then press a core board on the upper and lower core boards to form a cavity in the board. After pressing, subsequent operations are carried out. The existing conventional method has no metallization on the cavity sidewalls, which are directly exposed resin. The signal touches the resin on the cavity sidewall during transmission, resulting in a certain loss.

[0005] Therefore, it is necessary to provide a method for metallizing the cavity sidewall of a cavity plate to solve the above technical problems. Summary of the invention

[0006] The present invention provides a method for metallizing the cavity side wall of a cavity plate, which solves the problem that the cavity side wall of the conventional practice is not metallized but directly exposed resin, and the signal touches the resin of the cavity side wall during transmission, resulting in certain losses.

[0007] In order to solve the above technical problems, the present invention provides a method for metallizing the cavity side wall of a cavity plate, comprising the following steps:

[0008] S1: Prepare a copper-free substrate;

[0009] S2: Single-sided adhesive bonding;

[0010] S3: Perform gong operation;

[0011] S4: Single-sided lamination and pressing operation;

[0012] S5: After pressing, a selective electroplating process is performed to metallize the cavity;

[0013] S6: Sintering copper slurry;

[0014] S7: groove the pure glue according to the copper paste sintering area and stick it on the board surface;

[0015] S8: Performing lamination and pressing operation on the core board on the other side;

[0016] S9: At this point, the metallization of the cavity sidewall has been completed, and the subsequent process is the normal process.

[0017] Preferably, the single-sided lamination operation requires the use of a laminating machine, which comprises: a laminating box; a processing cavity is opened inside the laminating box, limit rods are fixedly installed on both sides of the processing cavity, a moving table is slidably installed on the outer surface of the limit rods, a positioning frame is fixedly connected to the bottom of the moving table, mounting plates are fixedly installed on both sides of the bottom of the moving table, a servo motor is fixedly installed inside one of the mounting plates, a reciprocating screw is fixedly connected to the output shaft of the servo motor, a sliding rod is fixedly connected to the surface of the other mounting plate, and a cleaning device is threadedly engaged on the outer surface of the reciprocating screw.

[0018] Preferably, the cleaning device includes a cleaning scraper block, a mounting block, a threaded hole, a limit block and a limit hole, the mounting block is threadedly engaged with the outer surface of the reciprocating screw, the threaded hole is opened on one side of the outer surface of the mounting block, the cleaning scraper block is fixedly connected to the other side of the outer surface of the mounting block, the limit block is fixedly connected to one side of the outer surface of the cleaning scraper block, and the limit hole is opened on one side of the limit block surface.

[0019] Preferably, the cleaning scraper is in the shape of a right-angled triangle.

[0020] Preferably, a hydraulic cylinder is provided on the top of the movable platform, and a cylinder body of the hydraulic cylinder is fixedly connected to the middle of the top of the laminating box.

[0021] Preferably, a lamination table is fixedly installed in the middle of the processing chamber.

[0022] Preferably, a steam generator is fixedly mounted on one side of the bottom of the processing chamber, an air outlet pipe is fixedly connected to one side of the surface of the steam generator, and a high-temperature resistant vortex air pump is fixedly connected to one side of the air outlet pipe.

[0023] Preferably, an air guide pipe is fixedly connected to one side of the high temperature resistant vortex air pump.

[0024] Preferably, a vacuum box is fixedly installed on one side of the outer surface of the lamination box, and a vacuum tube is fixedly connected to the surface of the vacuum box.

[0025] Preferably, a box door is provided on the front of the lamination box.

[0026] Compared with the related art, the method for metallizing the cavity side wall of the cavity plate provided by the present invention has the following beneficial effects:

[0027] The present invention provides a method for metallizing the cavity side wall of a cavity board. After metallizing the side wall of a copper-free substrate, a copper paste sintering operation is performed on the upper side, thereby effectively ensuring that the metallization of the side wall is connected to the same layer of an upper core board, and a metallized cavity is truly formed in the PCB. All signals are in contact with the metal, avoiding contact with the resin, effectively reducing the signal loss, and metallizing the cavity side wall to effectively ensure the integrity of the signal and reduce the loss.

[0028] The present invention provides a method for metallizing the side wall of the cavity of a cavity plate, wherein the output shaft of a servo motor rotates to drive the reciprocating screw to rotate, the reciprocating screw rotates to engage a threaded cleaning scraper that slides on the surface of a positioning frame, the cleaning scraper slides on the bottom of the positioning frame, and the cleaning scraper scrapes off the material stuck to the bottom of the positioning frame. The device has a simple structure and strong practicality, avoids adhesion between the material and the pressing plate, automates scraping and cleaning, avoids manual cleaning by operators, improves the safety and convenience of operation, and improves the practicality of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 A schematic structural diagram of a first embodiment of a method for metallizing a cavity side wall of a cavity plate provided by the present invention;

[0030] Figure 2 for Figure 1 Schematic diagram of the cavity plate manufacturing process shown;

[0031] Figure 3 A schematic structural diagram of a second embodiment of a method for metallizing a cavity side wall of a cavity plate provided by the present invention;

[0032] Figure 4 for Figure 3 A schematic cross-sectional view of a lamination box is shown;

[0033] Figure 5 for Figure 4 An enlarged schematic diagram of point A is shown;

[0034] Figure 6 for Figure 5 The schematic diagram of the cleaning device structure is shown.

[0035] Numbers in the figure: 1. Copper-free substrate, 2. Pure glue, 3. Adding layer, 4. Laminating box, 5. Box door, 6. Processing chamber, 7. Hydraulic cylinder, 8. Moving table, 9. Positioning frame, 10. Limit rod, 11. Laminating table, 12. Steam generator, 13. High temperature resistant vortex air pump, 14. Air outlet pipe, 15. Air guide pipe, 16. Vacuum box, 17. Vacuum tube, 18. Mounting plate, 19. Servo motor, 20. Reciprocating screw, 21. Cleaning device, 211. Cleaning scraper block, 212. Mounting block, 213. Threaded hole, 214. Limit block, 215. Limit hole. DETAILED DESCRIPTION

[0036] The present invention will be further described below in conjunction with the accompanying drawings and implementation modes.

[0037] Please refer to Figure 1 and Figure 2 ,in, Figure 1 A schematic structural diagram of a first embodiment of a method for metallizing a cavity side wall of a cavity plate provided by the present invention; Figure 2 for Figure 1 A method for metallizing the cavity sidewall of a cavity plate comprises the following steps:

[0038] S1: Prepare a copper-free substrate;

[0039] S2: Single-sided adhesive bonding;

[0040] S3: Perform gong operation;

[0041] S4: Single-sided lamination and pressing operation;

[0042] S5: After pressing, a selective electroplating process is performed to metallize the cavity;

[0043] S6: Sintering copper slurry;

[0044] S7: groove the pure glue according to the copper paste sintering area and stick it on the board surface;

[0045] S8: Performing lamination and pressing operation on the core board on the other side;

[0046] S9: At this point, the metallization of the cavity sidewall has been completed, and the subsequent process is the normal process.

[0047] The working principle of the method for metallizing the cavity side wall of a cavity plate provided by the present invention is as follows:

[0048] When working, first prepare a copper-free substrate; then stick pure glue on one side of the copper-free substrate; at this time, perform the groove operation; single-sided lamination and pressing operation; after pressing, perform the selective electroplating process to metallize the cavity; sinter the copper paste; groove the pure glue according to the copper paste sintering area and stick it on the board surface; perform the lamination and pressing operation on the other side of the core board; at this point, the metallization of the cavity side wall has been completed, and the follow-up is the normal process.

[0049] Compared with the related art, the method for metallizing the cavity side wall of the cavity plate provided by the present invention has the following beneficial effects:

[0050] The present invention provides a method for metallizing the cavity side wall of a cavity board. After metallizing the side wall of a copper-free substrate, a copper paste sintering operation is performed on the upper side, thereby effectively ensuring that the metallization of the side wall is connected to the same layer of an upper core board, and a metallized cavity is truly formed in the PCB. All signals are in contact with the metal, avoiding contact with the resin, effectively reducing the signal loss, and metallizing the cavity side wall to effectively ensure the integrity of the signal and reduce the loss.

[0051] Second embodiment

[0052] Please refer to Figure 3 , Figure 4 , Figure 5 and Figure 6 Based on a method for metallizing the cavity sidewall of a cavity plate provided in the first embodiment of the present application, the second embodiment of the present application proposes another method for metallizing the cavity sidewall of a cavity plate. The second embodiment is only a preferred method of the first embodiment, and the implementation of the second embodiment will not affect the independent implementation of the first embodiment.

[0053] Specifically, the second embodiment of the present application provides a method for metallizing the cavity side wall of a cavity plate, which is different in that, in a method for metallizing the cavity side wall of a cavity plate, the single-sided lamination operation requires the use of a laminator, and the laminator includes: a laminating box 4; a processing cavity 6 is opened inside the laminating box 4, and both sides of the processing cavity 6 are fixedly installed with limit rods 10, and a moving table 8 is slidably installed on the outer surface of the limit rod 10, and a positioning frame 9 is fixedly connected to the bottom of the moving table 8, and mounting plates 18 are fixedly installed on both sides of the bottom of the moving table 8, and a servo motor 19 is fixedly installed inside one of the mounting plates 18, and a reciprocating screw 20 is fixedly connected to the output shaft of the servo motor 19, and a sliding rod is fixedly connected to the surface of the other mounting plate 18, and a cleaning device 21 is threadedly engaged on the outer surface of the reciprocating screw 20.

[0054] The cleaning device 21 includes a cleaning scraper block 211, a mounting block 212, a threaded hole 213, a limit block 214 and a limit hole 215. The mounting block 212 is threadedly engaged with the outer surface of the reciprocating screw 20, and the threaded hole 213 is opened on one side of the outer surface of the mounting block 212. The cleaning scraper block 211 is fixedly connected to the other side of the outer surface of the mounting block 212. The limit block 214 is fixedly connected to one side of the outer surface of the cleaning scraper block 211, and the limit hole 215 is opened on one side of the surface of the limit block 214.

[0055] The cleaning scraper 211 is in the shape of a right-angled triangle.

[0056] A hydraulic cylinder 7 is provided on the top of the moving platform 8 , and a cylinder body of the hydraulic cylinder 7 is fixedly connected to the middle of the top of the laminating box 4 .

[0057] A lamination table 11 is fixedly installed in the middle of the processing chamber 6 .

[0058] A steam generator 12 is fixedly installed on one side of the bottom of the processing chamber 6 , an air outlet pipe 14 is fixedly connected to one side of the surface of the steam generator 12 , and a high-temperature resistant vortex air pump 13 is fixedly connected to one side of the air outlet pipe 14 .

[0059] An air guide pipe 15 is fixedly connected to one side of the high temperature resistant vortex air pump 13 .

[0060] A vacuum box 16 is fixedly installed on one side of the outer surface of the lamination box 4 , and a vacuum tube 17 is fixedly connected to the surface of the vacuum box 16 .

[0061] The front of the lamination box 4 is provided with a box door 5 .

[0062] In the process of using the laminator, the cavity formed by the laminating table 2 is evacuated through the vacuum box, and the air in the cavity is sucked into the interior of the vacuum tube through the air suction port, and then the air is sucked away by the vacuum pump through the conveying action of the vacuum tube. The vacuuming is controlled by the control valve, so that the cavity is in a vacuum state. Since the hot pressing plate is in a vacuum environment, the heat loss is reduced, so that the hot pressing plate heats up faster, thereby increasing the heating rate of the hot pressing plate, thereby improving the working efficiency of the laminator. This is the prior art.

[0063] The cleaning scraper 211 is in the shape of a right-angled triangle, and the right-angled side is attached to the bottom surface of the positioning frame 9. When the cleaning scraper 211 moves, the inclined surface scrapes off the sticky material.

[0064] In the processing chamber 9, a sliding rod is fixed on the front side between the two mounting plates 18, and the two ends of the sliding rod are respectively fixedly connected to the surfaces of the two mounting plates 18. The limit block 214 is sleeved on the outer surface of the sliding rod through the limit hole 215, and the mounting block 212 is threadedly engaged with the outer surface of the reciprocating screw 20 through the threaded hole 213.

[0065] The working principle of the method for metallizing the cavity side wall of a cavity plate provided by the present invention is as follows:

[0066] During operation, the reciprocating screw 20 is first driven to rotate by the output shaft of the servo motor 19, and the reciprocating screw 20 rotates to threadedly engage the threaded hole 213 of the mounting block 212, and the mounting block 212 drives the cleaning scraper 211 and the limit block 214 to move, and the limit block 214 slides on the surface of the slide rod through the limit hole 215, so that the cleaning scraper 211 slides left and right on the surface of the positioning frame 9, and the cleaning scraper 211 slides at the bottom of the positioning frame 9, and the cleaning scraper 211 scrapes off the material stuck to the bottom of the positioning frame 9.

[0067] Compared with the related art, the method for metallizing the cavity side wall of the cavity plate provided by the present invention has the following beneficial effects:

[0068] The present invention provides a method for metallizing the side wall of the cavity of a cavity plate, wherein the reciprocating screw 20 is driven to rotate by the output shaft of a servo motor 19, and the reciprocating screw 20 rotates to engage a cleaning scraper 211 that slides on the surface of a positioning frame 9, and the cleaning scraper 211 slides on the bottom of the positioning frame 9, and the cleaning scraper 211 scrapes off the material stuck to the bottom of the positioning frame 9. The device has a simple structure and strong practicality, and can avoid adhesion between the material and the pressing plate, and can automatically scrape and clean, avoiding manual cleaning by operators, thereby improving the safety and convenience of operation and improving the practicality of the device.

[0069] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. A method for metallizing the cavity side wall of a cavity plate, characterized in that: The following steps are involved: S1: Prepare a copper-free substrate; S2: Single-sided adhesive bonding; S3: Perform gong operation; S4: Single-sided lamination and pressing operation; S5: After pressing, a selective electroplating process is performed to metallize the cavity; S6: Sintering copper slurry; S7: groove the pure glue according to the copper paste sintering area and stick it on the board surface; S8: Performing lamination and pressing operation on the core board on the other side; S9: At this point, the metallization of the cavity sidewall has been completed, and the subsequent process is the normal process.

2. A method for metallizing a cavity side wall of a cavity plate according to claim 1, characterized in that: The single-sided lamination operation requires the use of a laminating machine, which includes: a laminating box; a processing chamber is opened inside the laminating box, and limit rods are fixedly installed on both sides of the processing chamber, and a moving table is slidably installed on the outer surface of the limit rod, and a positioning frame is fixedly connected to the bottom of the moving table, and mounting plates are fixedly installed on both sides of the bottom of the moving table, one of the mounting plates has a servo motor fixedly installed inside, and a reciprocating screw is fixedly connected to the output shaft of the servo motor, and a sliding rod is fixedly connected to the surface of the other mounting plate, and a cleaning device is threadedly engaged on the outer surface of the reciprocating screw.

3. A method for metallizing a cavity side wall of a cavity plate according to claim 2, characterized in that: The cleaning device includes a cleaning scraper block, a mounting block, a threaded hole, a limit block and a limit hole, the mounting block is threadedly engaged with the outer surface of the reciprocating screw, the threaded hole is opened on one side of the outer surface of the mounting block, the cleaning scraper block is fixedly connected to the other side of the outer surface of the mounting block, the limit block is fixedly connected to one side of the outer surface of the cleaning scraper block, and the limit hole is opened on one side of the limit block surface.

4. A method for metallizing a cavity side wall of a cavity plate according to claim 3, characterized in that: The cleaning scraper is in the shape of a right-angled triangle.

5. The method for metallizing the cavity side wall of a cavity plate according to claim 2, characterized in that: A hydraulic cylinder is arranged on the top of the moving platform, and a cylinder body of the hydraulic cylinder is fixedly connected to the middle of the top of the laminating box.

6. The method for metallizing the cavity side wall of a cavity plate according to claim 2, characterized in that: A lamination table is fixedly installed in the middle of the processing chamber.

7. The method for metallizing the cavity side wall of a cavity plate according to claim 2, characterized in that: A steam generator is fixedly installed on one side of the bottom of the processing chamber, an air outlet pipe is fixedly connected to one side of the surface of the steam generator, and a high-temperature resistant vortex air pump is fixedly connected to one side of the air outlet pipe.

8. A method for metallizing a cavity side wall of a cavity plate according to claim 7, characterized in that: An air guide pipe is fixedly connected to one side of the high temperature resistant vortex air pump.

9. The method for metallizing the cavity side wall of a cavity plate according to claim 2, characterized in that: A vacuum box is fixedly installed on one side of the outer surface of the lamination box, and a vacuum tube is fixedly connected to the surface of the vacuum box.

10. The method for metallizing the cavity side wall of a cavity plate according to claim 2, characterized in that: The front of the lamination box is provided with a box door.