Method for producing exhaust gas purification catalyst and liquid medicine vessel

By forming grooves of specific depth and width on the bottom surface of the drug solution container, and having the grooves interconnected and designed in a grid pattern, the problem of uneven width of the catalyst metal solution on the substrate is solved, thus achieving uniformity of exhaust purification performance and efficient utilization of the catalyst metal.

CN119013099APending Publication Date: 2024-11-22CATALER CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202380032033.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-30
Filing Date
2023-03-02
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the prior art, the catalyst metal solution has uneven ripple width on the substrate, resulting in uneven exhaust purification performance. In addition, the surface tension of the catalyst metal solution causes the liquid surface to bend, making it difficult to effectively control the loading.

Method used

A groove is formed on the bottom surface of the drug solution container. The depth and width of the groove are within a specific range. The grooves are interconnected and form a grid, which reduces the surface tension of the catalyst metal solution and introduces it into the substrate through capillary action, suppressing ripples on the support width.

Benefits of technology

It effectively suppressed the ripples in the bearing width of the catalyst metal support, improved the uniformity of exhaust gas purification performance and the utilization efficiency of catalyst metal, reduced the fluctuation of residual amount, and improved the quality stability of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119013099A_ABST
    Figure CN119013099A_ABST
Patent Text Reader

Abstract

According to the present invention, it is possible to provide a technique for suppressing corrugation in the support width of the catalyst metal support section in the exhaust gas purification catalyst. The manufacturing method disclosed herein includes: a step of preparing a substrate having an exhaust passage; a step for preparing a catalyst metal solution containing at least one catalyst metal functioning as a catalyst capable of oxidizing or reducing the exhaust gas component; a step of supplying the catalyst metal solution to the liquid medicine vessel without exposing the bottom surface of the liquid medicine vessel; a step in which the end of the base material is immersed in the catalyst metal solution supplied to the chemical solution vessel, and the catalyst metal solution is introduced into the exhaust passage of the base material; and a step in which the substrate into which the catalyst metal solution has been introduced is fired. Furthermore, grooves having a predetermined pattern are formed in the bottom surface of the liquid medicine vessel, the average depth of the grooves being 1.2 mm to 3 mm, and the average width of the grooves being 1.6 mm to 3 mm.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for producing a catalyst for purifying exhaust gas and a chemical liquid dish used in the production method. In addition, this application claims priority based on Japanese Patent Application No. 2022-057214 filed on March 30, 2022, the entire contents of which are incorporated herein by reference. Background Art

[0002] The exhaust gas discharged from the internal combustion engine contains harmful components such as carbon monoxide (CO), hydrocarbons (HC), and nitrogen oxides (NOx). An exhaust gas purification catalyst for purifying these harmful components is arranged in the exhaust passage of the internal combustion engine. The exhaust gas purification catalyst includes, for example: a substrate of a honeycomb structure in which a plurality of exhaust flow paths (cells) are separated by partition walls; and a catalyst metal supporting portion provided on the surface and / or inside of the substrate partition wall and containing a catalyst metal (for example, palladium (Pd), rhodium (Rh), platinum (Pt), etc.) for purifying by oxidizing or reducing the exhaust gas components.

[0003] For example, Patent Document 1 discloses a technique in which a substrate (also referred to as a washcoat carrier) is immersed in a container filled with a precious metal solution to support the precious metal on the substrate. In addition, a plurality of recessed portions are provided at the bottom of the recessed portion of the container for storing the substrate, and a high-concentration precious metal portion can be formed on the substrate corresponding to the recessed portions.

[0004] Patent Literature:

[0005] Patent Document 1: Japanese Patent Application Publication No. 2003-334444 Summary of the invention

[0006] In recent years, attention has been paid to the following technology: instead of forming a catalyst metal supporting portion on the entire substrate, the catalyst metal supporting portion is formed in a specified area, thereby improving the characteristics of the catalyst for exhaust gas purification. For this reason, as a low-cost technology for supporting a specified amount of catalyst metal in a specified width of a substrate, the inventors of the present invention have studied the implementation of the following technology: a specified amount of catalyst metal solution (for example, a noble metal solution) is prepared in a liquid medicine dish, the end of the substrate is immersed in the catalyst metal solution, and the catalyst metal solution is introduced into the exhaust passage of the substrate. In such a technology, the catalyst metal solution can be introduced into the exhaust passage of the substrate by capillary action. However, since the surface tension of the catalyst metal solution is large, when the amount of the catalyst metal solution prepared in the liquid medicine dish decreases, the catalyst metal solution tends to gather in the central part of the liquid medicine dish, and the liquid surface is bent in a manner that it becomes higher near the central part. Therefore, there is the following problem: the front end surface of the catalyst metal solution introduced into the substrate by the capillary action is formed into a wave shape, and the width of the catalyst metal supporting portion fluctuates (ripples in the supporting width) in the central part and the outer peripheral part of the substrate.

[0007] Therefore, the present invention is made to solve the above-mentioned problems, and its main purpose is to provide a technique for suppressing the ripples in the supporting width of the catalyst metal supporting portion in the exhaust gas purification catalyst. In addition, another purpose is to provide a chemical liquid dish having such technical features.

[0008] In order to solve the above-mentioned problems, a method for producing an exhaust gas purification catalyst disclosed herein (hereinafter, also simply referred to as “production method”) can be provided.

[0009] The manufacturing method disclosed herein is a manufacturing method for manufacturing an exhaust gas purification catalyst for purifying exhaust gas discharged from an internal combustion engine. The manufacturing method disclosed herein is characterized in that it includes: a step of preparing a substrate having an exhaust passage from an upstream end portion for introducing exhaust gas to a downstream end portion for discharging exhaust gas; a step of preparing a catalyst metal solution containing at least one catalyst metal that functions as a catalyst capable of oxidizing or reducing exhaust gas components; a step of providing the catalyst metal solution to the above-mentioned liquid medicine dish in a manner that does not expose the bottom surface of the liquid medicine dish; a step of immersing the above-mentioned upstream end portion or the above-mentioned downstream end portion of the above-mentioned substrate in the above-mentioned catalyst metal solution provided to the above-mentioned liquid medicine dish, and introducing the above-mentioned catalyst metal solution into the above-mentioned exhaust passage of the above-mentioned substrate; and a step of firing the above-mentioned substrate into which the above-mentioned catalyst metal solution has been introduced. In addition, a groove consisting of a prescribed pattern is formed on the above-mentioned bottom surface of the above-mentioned liquid medicine dish, the average depth of the above-mentioned groove is 1.2 mm or more and 3 mm or less, and the average width of the above-mentioned groove is 1.6 mm or more and 3 mm or less.

[0010] Here, "exhaust passage" refers to the area where the exhaust gas introduced into the substrate can flow, and is not limited to the space (cell) formed inside the substrate and the wall surface around it. The interior (pores) of the porous body constituting the substrate also constitutes a part of the exhaust passage as long as the exhaust gas can be introduced and flow.

[0011] With such a configuration, by forming a groove on the bottom surface of the drug liquid dish, the surface tension of the catalyst metal solution supplied to the drug liquid dish can be reduced, and the liquid surface of the catalyst metal solution supplied to the drug liquid dish can be suppressed from bending due to the surface tension. Thus, when the end of the substrate is immersed in the catalyst metal solution and the catalyst metal solution is introduced into the interior of the substrate by capillary phenomenon, the ripples of the front end surface of the substrate into which the catalyst metal solution is introduced can also be suppressed. As a result, the ripples on the supporting width of the catalyst metal supporting portion formed by firing can be suppressed.

[0012] In a preferred embodiment of the manufacturing method disclosed herein, the liquid level height of the catalyst metal solution provided to the liquid dish from the bottom surface is 0.37 mm or more. With such a configuration, the curvature of the liquid level of the catalyst metal solution provided to the liquid dish can be further suppressed, and thus, the ripples on the supporting width of the catalyst metal supporting portion can be suppressed at a higher level.

[0013] In a preferred embodiment of the manufacturing method disclosed herein, the grooves are formed in a mutually connected manner. With such a configuration, when the amount of the catalyst metal solution supplied to the liquid dish decreases, the liquid level of the catalyst metal solution in the grooves becomes constant, thereby further suppressing the ripples in the supporting width of the catalyst metal supporting portion.

[0014] In a preferred embodiment of the manufacturing method disclosed herein, the grooves are formed in a grid shape, thereby further reducing the surface tension of the catalyst metal solution and further suppressing the ripples in the supporting width of the catalyst metal supporting portion.

[0015] In a preferred embodiment, the grooves are formed at a predetermined pitch, which is 8 mm to 20 mm. With such a configuration, in addition to suppressing the ripples in the supporting width of the catalyst metal supporting portion, after the catalyst metal solution is introduced into the substrate, the amount of catalyst metal solution remaining in the solution dish (residual amount) becomes less, and the fluctuation of such residual amount can also be suppressed, thereby further suppressing the fluctuation of the amount of catalyst metal supported on the substrate.

[0016] In addition, according to the present invention, a liquid medicine dish used in the manufacture of an exhaust gas purification catalyst for purifying exhaust gas discharged from an internal combustion engine is provided. The liquid medicine dish disclosed herein has a bottom wall and a recessed portion formed by a side wall rising from the bottom wall. A groove formed by a prescribed pattern is formed on the surface of the recessed portion side of the bottom wall, the average depth of the groove is not less than 1.2 mm and not more than 3 mm, and the average width of the groove is not less than 1.6 mm and not more than 3 mm. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a flowchart showing the outline of the process of a method for producing an exhaust gas purification catalyst according to an embodiment.

[0018] Figure 2 It is a perspective view schematically showing an example of the structure of a substrate used in the exhaust gas purifying catalyst.

[0019] Figure 3 This is a cross-sectional view schematically showing a configuration when a catalytic metal solution is supplied to a chemical solution vessel according to one embodiment.

[0020] Figure 4 It is a plan view schematically showing the structure of a chemical solution dish according to one embodiment.

[0021] Figure 5 This is a partially enlarged view schematically showing the structure of the bottom surface of a chemical solution dish according to one embodiment.

[0022] Fig. 6A This is a schematic diagram showing a method of introducing a catalytic metal solution into a substrate using an example of a conventional chemical solution dish.

[0023] Figure 6B This is a schematic diagram showing a method of introducing a catalytic metal solution into a substrate using an example of a conventional chemical solution dish.

[0024] Figure 6C This is a schematic diagram showing a method of introducing a catalytic metal solution into a substrate using an example of a conventional chemical solution dish.

[0025] Figure 7 This is a graph showing the average remaining amount of the catalyst metal solution and its fluctuation σ in each example. DETAILED DESCRIPTION

[0026] Hereinafter, the preferred embodiment disclosed herein will be described with reference to the accompanying drawings. In addition, in this specification, matters other than matters not specifically mentioned and required for the implementation of the technology disclosed herein (e.g., the processing method of the liquid medicine dish, etc.) can be grasped as design matters for those skilled in the art based on the prior art in the field. The technology disclosed herein can be implemented based on the content disclosed in this specification and the technical knowledge in the field. In addition, the drawings in this specification are schematically represented for understanding the technical content disclosed herein, and the dimensional relationship (length, width, thickness, etc.) of each figure does not necessarily reflect the actual dimensional relationship. In addition, in this specification, when the numerical range is recorded as "A to B (here A and B are arbitrary numerical values)", it means "Above A and below B", and also includes the meaning of "exceeding A and below B", "exceeding A and below B" and "Above A and below B".

[0027] Figure 1 1 is a flowchart showing a schematic process of a method for producing an exhaust gas purification catalyst according to an embodiment. The present embodiment includes a material preparation step S10, an impregnation step S20, a drying step S30, and a calcination step S40.

[0028] <Material preparation process S10>

[0029] The material preparation step S10 includes steps of preparing a substrate, a catalyst metal solution, and a chemical solution vessel.

[0030] (Base material)

[0031] The substrate is a component constituting the skeleton of the exhaust gas purification catalyst. As the substrate, various raw materials and substrates that have been commonly used as substrates constituting exhaust gas purification catalysts can be used. For example, a ceramic substrate such as cordierite, aluminum titanate, silicon carbide (SiC) or the like having high heat resistance, or a metal substrate such as stainless steel can be used.

[0032] The shape of the substrate may be similar to that of a conventional exhaust gas purifying catalyst and is not particularly limited as long as it has an exhaust passage extending from an upstream end portion for introducing exhaust gas to a downstream end portion for discharging exhaust gas. Figure 2 1 is a perspective view schematically showing an example of the structure of a substrate used in an exhaust gas purification catalyst. Figure 2 As shown, the outer diameter of the substrate 10 is cylindrical. In addition, the substrate 10 has through holes, i.e., a plurality of cells 12, which are exhaust passages, in the long axis direction thereof. The plurality of cells 12 may have a honeycomb structure separated by partition walls (rib walls) 14. Figure 2In the embodiment, the shape of the small chamber 12 in the cross section perpendicular to the cylinder axis direction of the substrate 10 is a square, but it is not limited to this. For example, it can be a quadrilateral such as a parallelogram, a rectangle, a trapezoid, a triangle, other polygons (for example, a hexagon, an octagon), a circle, and other geometric shapes. In addition, the overall shape of the substrate 10 can also be an elliptical cylinder, a polygonal cylinder, etc. instead of a cylindrical shape.

[0033] Figure 2 The substrate 10 shown is a so-called straight-flow type in which the exhaust gas introduced from the upstream end 10a into the small chamber 12 directly passes through the small chamber 12 and is discharged from the downstream end 10b, but it is not particularly limited to this. For example, it can be a so-called wall-flow type substrate in which the exhaust gas introduced from the upstream end of a small chamber with only an upstream end opening moves to an adjacent small chamber with only a downstream end opening through a porous partition wall and is discharged from the downstream end of the small chamber. Alternatively, as long as the exhaust gas can flow in the pores, it can also be a sponge-like porous body with irregular pores formed therein.

[0034] Although not particularly limited, the capacity of the substrate 10 (the volume of the entire chamber 12) is usually 0.1 L or more (preferably 0.5 L or more), for example, 5 L or less (preferably 3 L or less, more preferably 2 L or less). In addition, the total length of the substrate 10 along the exhaust gas flow direction (cylinder axis direction) is usually set to about 10 mm to 500 mm (for example, 50 mm to 300 mm).

[0035] The cross-sectional area of ​​each cell 12 in the cross section perpendicular to the cylindrical axis direction of the substrate 10 is, for example, 0.6 mm 2 Above 2.5mm 2 Below, preferably 0.8mm 2 Above 2.2mm 2 When the thickness is within this range, the capillary phenomenon can be effectively generated while ensuring the flowability of the exhaust gas. By effectively generating the capillary phenomenon, the catalyst metal solution can be efficiently introduced into the exhaust passage of the substrate.

[0036] (Catalyst Metal Solution)

[0037] The catalyst metal solution is a material for forming a catalyst metal supporting portion (also referred to as a catalyst layer) having a function of purifying exhaust components on at least the surface of a partition wall of an exhaust passage facing a substrate. The catalyst metal solution contains at least one catalyst metal that functions as a catalyst capable of oxidizing or reducing exhaust components. In addition, the catalyst metal solution may contain a liquid medium.

[0038] As the catalyst metal, for example, palladium (Pd), rhodium (Rh), platinum (Pt) and other precious metals belonging to the platinum group elements or other metals that function as oxidation or reduction catalysts can be cited. Pd and Pt have excellent purification performance (oxidation purification ability) for carbon monoxide and hydrocarbons, and Rh has excellent purification performance (reduction purification performance) for NOx, so these are particularly preferred catalyst metals as three-way catalysts.

[0039] The catalyst metal is preferably contained in the catalyst metal solution in the form of ions. By calcining such a catalyst metal solution, catalyst metal particles can be generated. In addition, in order to make the concentration of the catalyst metal in the catalyst metal solution uniform, when the catalyst metal solution is introduced into the interior of the substrate by capillary phenomenon, a catalyst metal supporting portion in which the catalyst metal particles are highly uniformly distributed can also be formed. As the catalyst metal solution, for example, an aqueous solution of a water-soluble metal salt containing the catalyst metal, an aqueous solution containing a coordination compound of the catalyst metal, etc. can be used. As metal salts, for example, nitrates such as palladium nitrate and rhodium nitrate; sulfates such as palladium sulfate and rhodium sulfate, etc. can be listed. As coordination compounds of catalyst metals, tetraamine coordination compounds, amino coordination compounds, halogen coordination compounds, hydroxy coordination compounds, etc. can be exemplified.

[0040] In addition, in this specification, "catalyst metal solution" may include a mixture obtained by dispersing colloidal particles in a medium. Therefore, the catalyst metal may not be completely dissolved, for example, the catalyst metal may be included in the form of catalyst metal particles. The average particle size of such catalyst metal particles is not particularly limited, for example, it can be set to about 0.1nm to 1μm (typically, 1nm to 10nm). In addition, such an average particle size can be obtained by observing with a transmission electron microscope as an average value when measuring the particle size of 100 catalyst metal particles.

[0041] As a medium that can be used for the catalyst metal solution, for example, an aqueous solvent (for example, water, deionized water, pure water, etc.) can be appropriately used. The aqueous solvent can appropriately dissolve a metal salt containing a catalyst metal or a catalyst metal complex.

[0042] The catalyst metal solution may contain other additives such as a thickener, a dispersant, a surfactant, and a binder as long as it can be introduced into the interior of the substrate by capillary action.

[0043] The content of the catalyst metal in the catalyst metal solution as a whole is, for example, 0.1 mass % to 30 mass %, and can be 1 mass % to 15 mass %. By adjusting the content of the catalyst metal, the amount of the catalyst metal particles in the catalyst metal supporting portion can be adjusted. In addition, the content of the catalyst metal refers to the value of the catalyst metal when converted to atomic weight.

[0044] (Medicine liquid dish)

[0045] The chemical solution dish has a recessed portion capable of providing a catalyst metal solution. Figure 3 This is a cross-sectional view schematically showing a configuration when a catalytic metal solution is supplied to a chemical solution vessel according to one embodiment. Figure 4 It is a plan view schematically showing the structure of a chemical solution dish according to one embodiment.

[0046] Figure 5 This is a partially enlarged view schematically showing the structure of the bottom surface of a liquid medicine dish involved in one embodiment. The liquid medicine dish 30 has a bottom wall 32 and a side wall 34 rising from the outer periphery of the bottom wall 32, and has a recess 36 formed by the bottom wall 32 and the side wall 34. A groove 32b formed by a prescribed pattern is formed on the surface of the bottom wall 32 of the liquid medicine dish 30 on the side of the recess 36 (also referred to as "bottom surface 32a"). The present technology is characterized by such a groove 32b. In the following, Figures 6A to 6C 2 schematically shows a method of introducing the catalytic metal solution 20 into the substrate 10 using an example of a conventional chemical solution dish 130 , and the problems thereof will be described.

[0047] Figures 6A to 6C , a method of introducing the catalyst metal solution 20 into the interior of the substrate 10 (specifically, the exhaust passage of the substrate 10) by immersing the end portion of the substrate 10 (here, the upstream end portion 10a) in the catalyst metal solution 20 is schematically shown. Fig. 6A , Figure 6B , Figure 6C The order of implementation is as follows. Figures 6A to 6C As shown in FIG. 1 , the conventional chemical liquid dish 130 does not have a groove formed on the bottom surface 132a. When the catalyst metal solution 20 is provided in the recess 136 of such a chemical liquid dish 130, the catalyst metal solution 20 has a higher liquid level in the center of the provided catalyst metal solution 20 due to surface tension. That is, the liquid surface of the catalyst metal solution 20 becomes curved. When the end of the substrate 10 is immersed in the catalyst metal solution 20 (see FIG. 1 ), the catalyst metal solution 20 is placed in the bottom surface 132a of the conventional chemical liquid dish 130. When the catalyst metal solution 20 is placed in the recess 136 of the chemical liquid dish 130, the liquid level of the catalyst metal solution 20 becomes higher due to surface tension. Fig. 6A ), by capillary phenomenon, the catalyst metal solution 20 supplied to the liquid dish 130 is introduced into the exhaust passage (in the case of a honeycomb substrate, a pore having a small chamber and a partition wall, etc.) of the substrate 10 (refer to Figure 6B However, since the liquid surface of the catalyst metal solution 20 is curved, the front end surface of the catalyst metal solution 20 introduced into the substrate 10 is formed into a curved (corrugated) state. Furthermore, when the substrate 10 is fired in this state to form a catalyst metal supporting portion, fluctuations (corrugations) are generated in the supporting width (width from the end of the substrate 10) of the catalyst metal supporting portion. Figure 6CAs shown, typically, the catalyst metal supporting portion near the central portion of the substrate 10 has the largest supporting width, and the catalyst metal supporting portion near the peripheral portion of the substrate 10 has the smallest supporting width, and a difference L between the maximum and minimum values ​​of the catalyst metal supporting width occurs. When such a difference L is large, the exhaust purification performance becomes uneven between the central portion and the peripheral portion of the substrate, and the desired exhaust purification performance may not be achieved.

[0048] Furthermore, even when the amount of the catalyst metal solution 20 is increased in order to prevent the curvature of the liquid surface of the supplied catalyst metal solution 20, the amount of the catalyst metal solution 20 on the drug solution dish 130 decreases as the catalyst metal solution 20 is supplied to the inside of the substrate 10, and thus, as described above, a state is created in which the liquid surface height of the central portion of the catalyst metal solution 20 becomes high. Therefore, the adjustment of the supply amount of the catalyst metal solution 20 is not sufficient to suppress the ripples in the supporting width of the catalyst metal supporting portion.

[0049] On the other hand, in the drug liquid dish 30 disclosed here, a groove 32b consisting of a predetermined pattern is formed on the bottom surface 32a. In addition, the groove 32b has a predetermined depth (for example, 1.2 mm to 3 mm on average) and width (for example, 1.6 mm to 3 mm on average). By forming the groove 32b, the surface tension of the catalyst metal solution 20 provided to the drug liquid dish 30 can be reduced. Therefore, the curvature of the liquid surface of the catalyst metal solution 20 can be suppressed. Thus, the end of the substrate 10 is immersed in the catalyst metal solution 20, and when the catalyst metal solution is introduced into the interior of the substrate by capillary phenomenon, the ripples on its front end surface can be suppressed. As a result, the ripples on the supporting width of the catalyst metal supporting portion can be suppressed. In addition, since the surface tension of the catalyst metal solution is reduced by the groove 32b, the amount of the catalyst metal solution 20 remaining in the drug liquid dish 30 after the catalyst metal solution 20 is introduced into the interior of the substrate 10 by capillary phenomenon will be reduced. Therefore, by adopting the present technology, the catalyst metal solution 20 can be efficiently introduced into the interior of the substrate 10 for the desired width of the substrate 10. In addition, according to the research of the inventors of the present invention, the fluctuation of the amount of the catalyst metal solution 20 remaining in the chemical solution dish 30 is reduced. In other words, the catalyst metal solution 20 can be introduced into the interior of the substrate 10 with good reproducibility. Thereby, the quality stability can be improved.

[0050] The average depth D of the groove 32b of the chemical solution dish 30 (see Figure 3) is, for example, 1.2 mm or more, preferably 1.3 mm or more, more preferably 1.35 mm or more, and further preferably 1.39 mm or more. The greater the depth D of the groove 32b, the more the surface tension of the catalyst metal solution 20 can be reduced. On the other hand, there is no particular limitation, and the average depth D of the groove 32b is, for example, 5 mm or less, preferably 4 mm or less, and more preferably 3 mm or less. The greater the depth D of the groove 32b, the more the amount of catalyst metal solution 20 remaining in the drug liquid dish 30 after the catalyst metal solution 20 is introduced into the substrate 10, and therefore, it is disadvantageous in terms of cost. In addition, the depth D of the groove 32b refers to the distance from the deepest part of the groove 32b to the height of the bottom surface 32a of the drug liquid dish 30 in the cross section along the width direction of the groove 32b.

[0051] The average width W of the groove 32b of the chemical solution dish 30 (see Figure 5 ) is, for example, 1.6 mm or more, preferably 1.8 mm or more. When the width W of the groove 32b is too small, the surface tension of the catalyst metal solution 20 may not be sufficiently reduced. In addition, the average width W of the groove 32b is not particularly limited, for example, 5 mm or less, preferably 4 mm or less, more preferably 3 mm or less, further preferably 2.2 mm or less, and may be 2 mm or less. The larger the width W of the groove 32b, the more the amount of the catalyst metal solution 20 remaining in the drug solution dish 30 after the catalyst metal solution 20 is introduced into the substrate 10.

[0052] The ratio of the area of ​​the groove 32b of the chemical liquid dish 30 to the area of ​​the bottom surface 32a in a plan view is not particularly limited, and is, for example, 10% to 60%, preferably 30% to 50%. This can further reduce the surface tension of the catalyst metal solution.

[0053] The grooves 32b of the liquid medicine dish 30 are formed in a manner consisting of a predetermined pattern, and the grooves 32b are preferably interconnected. Thus, when the amount of the catalyst metal solution 20 supplied to the liquid medicine dish 30 decreases (for example, when the amount becomes lower than the height of the bottom surface 32a), the liquid level of the catalyst metal solution 20 in the grooves 32b becomes uniform, so that the ripples on the supporting width of the catalyst metal supporting portion can be further suppressed.

[0054] In this embodiment, if Figure 4 As shown in FIG. 1 , the grooves 32b of the drug solution dish are formed in a grid shape. In other words, the grooves 32b are formed with a plurality of grooves formed in a predetermined direction at a predetermined pitch P (the distance between adjacent grooves) and a plurality of grooves formed at a predetermined pitch in a manner intersecting the grooves at a predetermined angle (here, 90°) (see FIG. Figure 5 ). As a result, the surface tension of the catalyst metal solution can be further reduced, and thus, the ripples in the supporting width of the catalyst metal supporting portion can be further suppressed.

[0055] The pitch P of the grooves 32b is not particularly limited, and is, for example, 6 mm or more, preferably 8 mm or more. In addition, the pitch P of the grooves 32b is, for example, 20 mm or less, preferably 14 mm or less, and more preferably 10 mm or less. When it is within such a range, after the catalyst metal solution 20 is introduced into the substrate 10, the amount of the catalyst metal solution 20 remaining in the drug solution dish 30 becomes less, and the fluctuation of the amount becomes smaller.

[0056] In the present embodiment, the spacing of the grooves formed in the prescribed direction is formed in the same manner as the spacing of the grooves formed intersecting with the grooves. In other words, when viewed from above, the outer shape of the bottom surface 32a surrounded by the grooves 32b is formed in the form of a quadrilateral with the same side length. However, it is not limited to this, and it can also be designed that the spacing of the grooves formed in the prescribed direction is different from the spacing of the grooves formed intersecting with the grooves. In this case, the spacing of the grooves formed in the prescribed direction and the spacing of the grooves formed intersecting with the grooves can be within the range of the spacing P of the grooves 32b mentioned above.

[0057] In this embodiment, the cross-sectional shape of the groove 32b in the cross section along the width direction of the groove 32b (the outer shape of the groove) is formed in the form of an inverted triangle whose width gradually decreases as it goes to the bottom of the groove. As a result, after the catalyst metal solution 20 is introduced into the substrate 10, the amount of the catalyst metal solution 20 remaining in the liquid medicine dish 30 decreases, and the fluctuation of the catalyst metal loading amount of the catalyst metal loading portion can be suppressed. However, the cross-sectional shape of such a groove 32b is not limited thereto, and for example, it can be a semicircular shape, a quadrilateral shape, a polygon shape, etc.

[0058] In addition, if Figure 4 As shown, in this embodiment, the outer shape of the recess 36 of the liquid medicine dish 30 is circular when viewed from above. However, the outer shape of such a recess 36 is not particularly limited, and it can also be an ellipse, a polygon, etc. It is preferred that the outer shape of the recess 36 when viewed from above is the same shape as the outer shape of the cross section perpendicular to the cylindrical axis direction of the substrate 10. Thus, in order to allow the catalyst metal solution 20 to be more uniformly introduced into the substrate 10, the ripples on the supporting width of the catalyst metal supporting portion can be further suppressed.

[0059] The chemical dish 30 preferably has chemical resistance to the compound contained in the catalyst metal solution 20. Therefore, the material of the chemical dish 30 varies depending on the type of compound contained in the catalyst metal solution 20, and for example, stainless steel, polyvinyl chloride, acrylic resin, etc. can be used.

[0060] Furthermore, the chemical solution dish disclosed herein may be in the form of a jig or the like having a recessed portion capable of supplying the catalyst metal solution, as long as the manufacturing process disclosed herein can be implemented.

[0061] The material preparation step S10 includes providing the catalyst metal solution 20 to the drug liquid dish 30. Specifically, the catalyst metal solution 20 is added to the recess 36 of the drug liquid dish 30, and the catalyst metal solution 20 is provided in a manner that does not expose the bottom surface 32a of the drug liquid dish 30. At this time, if there is a portion where the bottom surface 32a of the drug liquid dish 30 is exposed, when the end of the substrate 10 is immersed in the catalyst metal solution 20, the amount of the catalyst metal solution introduced may be reduced or not introduced, which is not preferred.

[0062] The height H of the liquid surface of the catalyst metal solution 20 supplied to the liquid dish 30 (refer to Figure 3 ) is not particularly limited, and is preferably above 0.37 mm. Thus, the curvature of the liquid surface of the catalyst metal solution 20 provided to the liquid dish 30 can be suppressed, making it flatter, and therefore, the ripples on the holding width of the catalyst metal supporting portion can be suppressed at a higher level. In addition, the upper limit of the height H of the liquid surface is not particularly limited, and can be appropriately adjusted according to the desired holding width of the catalyst metal supporting portion. For example, it can be set to less than 300 mm. In addition, the height H of the liquid surface refers to the height calculated from the bottom surface 32a.

[0063] <Immersing step S20>

[0064] In the immersion step S20, the end portion (upstream end portion 10a or downstream end portion 10b) of the substrate 10 is immersed in the catalyst metal solution 20 supplied to the liquid dish 30. Since the substrate 10 has an exhaust passage through which exhaust gas can pass from the upstream end portion 10a to the downstream end portion 10b, the catalyst metal solution 20 supplied to the liquid dish 30 can be introduced into the exhaust passage by capillary action.

[0065] The immersion time can be changed according to the supporting width of the catalyst metal supporting portion to be formed or according to the amount of the catalyst metal solution 20 supplied to the liquid dish 30, and is therefore not particularly limited, and may be, for example, 5 seconds to 3 hours or 10 minutes to 2 hours.

[0066] <Drying step S30>

[0067] The drying process S30 can be implemented under the same conditions as the drying process implemented by various existing technologies in the art, and is not particularly limited. For example, the heating temperature in the drying process is 50° C. to 200° C., preferably 100° C. to 150° C. In addition, the drying time is 0.5 hour to 5 hours, preferably 1 hour to 3 hours. In addition, the drying process S30 is not a necessary process and can be omitted.

[0068] <Firing step S40>

[0069] In the firing step S40, the substrate 10 into which the catalyst metal solution 20 is introduced is fired to form a catalyst metal supporting portion on the substrate 10. When the catalyst metal solution 20 contains catalyst metal ions, catalyst metal particles are precipitated by firing, and such catalyst metal particles can be attached to the carrier (typically, attached to the partition wall 14 of the substrate 10). The firing conditions are not particularly limited and can be appropriately adjusted according to the structure of the substrate 10 and the composition of the catalyst metal solution. The firing temperature can be, for example, above 150°C, above 200°C, or above 250°C. On the other hand, the upper limit of the firing temperature can be below 1000°C, below 900°C, below 800°C, below 700°C, or below 600°C. In addition, the firing time can be above 5 minutes, above 0.5 hours, above 1 hour, or above 1.5 hours. The upper limit of the firing time can be below 8 hours, below 6 hours, or below 4 hours.

[0070] The above is a description of the general processes included in the manufacturing method involved in this embodiment, but the manufacturing method disclosed herein may further include other processes at any stage. For example, it may include a process of introducing a slurry containing a catalyst metal of a desired composition into a substrate, and forming a catalyst layer at a position different from the above-mentioned catalyst metal support portion. In this way, the exhaust purification performance of the exhaust purification catalyst can be improved. The specific composition and configuration of such a catalyst layer are not the characteristics of the present technology, so its description is omitted.

[0071] The manufacturing method disclosed herein can be appropriately used when a predetermined amount of catalyst metal supporting parts are formed in a predetermined width of a substrate. According to the present technology, it is possible to suppress the ripples in the supporting width of the catalyst metal supporting part, thereby suppressing the difference in exhaust purification performance generated between the central part and the peripheral part of the substrate. In addition, the present technology does not require the use of a device such as a suction device, and therefore can be easily implemented.

[0072] In addition, according to the present invention, there is provided a chemical liquid dish having the above-mentioned structure used for manufacturing an exhaust gas purification catalyst for purifying exhaust gas discharged from an internal combustion engine. In addition, the chemical liquid dish disclosed herein can also be used in other than the manufacturing process disclosed herein.

[0073] The exhaust gas purification catalyst manufactured using this technology can be applied to the exhaust system of an internal combustion engine installed in a vehicle, etc., to purify the exhaust gas discharged from various internal combustion engines. For example, it can be used as an exhaust gas purification catalyst for a gasoline engine or as an exhaust gas purification catalyst for a diesel engine.

[0074] Hereinafter, a test example of the technology disclosed here will be described. In addition, the following description is not intended to limit the technology disclosed here to the test example.

[0075] <Preparation of substrate and catalyst metal solution>

[0076] As a substrate, a straight-flow cylindrical honeycomb substrate (cordierite, axial length: 100 mm, diameter: 117 mm, cell density: 750 cpi) was prepared. Also, as a catalyst metal solution, a palladium nitrate solution (Pd equivalent: 13.5 mass %) was prepared.

[0077] <Preparation of the drug solution dish>

[0078] (Examples 1 to 8)

[0079] In each example, a liquid medicine dish having a grid-like groove on a circular bottom surface (diameter: 130 mm) was prepared. The depth of the groove, the width of the groove, and the spacing of the grooves of the liquid medicine dish in each example are shown in Table 1. In addition, the angle at which the grooves intersect is set to a right angle. In addition, the cross-sectional shape of the groove along the width direction of the groove is formed into an inverted triangle shape whose width gradually decreases as the bottom of the groove goes to the vertex.

[0080] (Reference example)

[0081] As a reference example, a chemical solution dish having no groove on the bottom surface of a circular shape (diameter: 130 mm) was prepared.

[0082] <Impregnation of base material>

[0083] Add 6g of catalyst metal solution to the liquid medicine dish. At this time, in each example, it was confirmed that the catalyst metal solution was filled until the bottom surface of the liquid medicine dish was not exposed as a whole. In addition, in Example 8, which has the largest volume of the tank among Examples 1 to 8, it was confirmed that the liquid level height of the catalyst metal solution from the bottom surface of the liquid medicine dish was 0.37mm. Afterwards, the end of the substrate in the axial direction (that is, the end surface of the chamber with the opening) was immersed in the catalyst metal solution in the liquid medicine dish, and the catalyst metal solution was introduced into the interior of the substrate by capillary phenomenon. Such immersion was performed for 5 seconds. Thereafter, a heat treatment was performed at 220°C for 5 minutes to produce a catalyst for exhaust purification having a catalyst metal carrier.

[0084] In each example, the amount of the catalyst metal solution added to the chemical solution dish was changed to 8 g, 10 g, and 16 g to produce exhaust gas purification catalysts. That is, in each example, four exhaust gas purification catalysts were produced.

[0085] <Ripple's evaluation>

[0086] The produced exhaust gas purification catalyst was heat treated so that the portion carrying Pd turned black. Thus, the catalyst was divided into two parts along the cylinder axis direction in a manner passing through the center of the end face of the exhaust gas purification catalyst, and the longest and smallest portions of the width in the cylinder axis direction of the portion whose cross section turned black were measured, and the difference between them was calculated as "waviness". In each example, the average value of the wavyness of the four exhaust gas purification catalysts produced above is shown in Table 1.

[0087] <Evaluation of the Remaining Amount of Catalyst Metal Solution>

[0088] After the catalyst metal solution was impregnated into the substrate, the amount of the catalyst metal solution remaining in the liquid reagent dish was measured using an electronic balance. In each example, the measurement was performed using the four exhaust gas purification catalysts manufactured as described above, and the standard deviation S was calculated using the following formula (1). In formula (1), n ​​represents the number of data (here n=4), and x i Represents each data value, x ave. The average of each data is shown in Table 1. The fluctuation σ of the data in each example is calculated by σ=3S. The average remaining amount (g) of the catalyst metal solution and the fluctuation σ of each example are shown in Table 1 and Figure 7 . Figure 7 The graph is represented by taking the average remaining amount of the catalyst metal solution of each example as the vertical axis and the fluctuation σ as the error bar.

[0089]

[0090]

Table 1

[0091] Table 1

[0092]

[0093] As shown in Table 1, in the reference example using a liquid medicine dish without a groove on the bottom surface, the corrugation of the catalyst metal supporting portion is large. In addition, as shown in Example 4, even if a liquid medicine dish with a groove formed on the bottom surface is used, the corrugation of the catalyst metal supporting portion cannot be suppressed when the depth and width of the groove are relatively small. On the other hand, when a liquid medicine dish with a groove having a depth of approximately 1.2 mm to 3 mm and a width of 1.6 mm to 3 mm is used (Examples 1 to 4, 6 to 8), the corrugation of the catalyst metal supporting portion is suppressed. In particular, in Example 4, it can be seen that: since corrugation of the catalyst metal supporting portion does not occur, the corrugation can be appropriately suppressed by making the depth and width of the groove approximately 1.8 mm to 2.2 mm.

[0094] As shown in Table 1 and Figure 7As shown, it can be seen that, when the reference example is compared with Examples 1 to 8, the residual amount of the catalyst metal solution in the liquid dish of Examples 1 to 8 is small and its fluctuation is also small. Therefore, by using the liquid dish with grooves formed on the bottom surface, the catalyst metal can be efficiently supported on the substrate. In addition, by comparing Examples 1 to 3, it can be seen that when the spacing of the grooves is 8 mm to 14 mm, the residual amount of the catalyst metal solution and its fluctuation can be further reduced.

[0095] Although specific examples of the present technology have been described in detail above, these are merely examples and do not limit the scope of protection. The technology described in the claims also includes various modifications and changes of the specific examples described above.

Claims

1. A method for producing an exhaust gas purification catalyst, wherein the exhaust gas purification catalyst purifies exhaust gas discharged from an internal combustion engine, the method for producing the exhaust gas purification catalyst comprising: a step of preparing a substrate having an exhaust passage extending from an upstream end portion for introducing exhaust gas to a downstream end portion for discharging exhaust gas; a step of preparing a catalyst metal solution, the catalyst metal solution containing at least one catalyst metal that functions as a catalyst capable of oxidizing or reducing exhaust gas components; The step of providing the catalyst metal solution to the chemical liquid dish in a manner that does not expose the bottom surface of the chemical liquid dish; The step of immersing the upstream end portion or the downstream end portion of the substrate in the catalyst metal solution supplied to the chemical solution dish, and introducing the catalyst metal solution into the exhaust passage of the substrate; and a step of firing the substrate into which the catalyst metal solution has been introduced, A groove having a predetermined pattern is formed on the bottom surface of the drug solution dish, wherein an average depth of the groove is not less than 1.2 mm and not more than 3 mm, and an average width of the groove is not less than 1.6 mm and not more than 3 mm.

2. The manufacturing method according to claim 1, characterized in that: The catalyst metal solution supplied to the chemical solution dish has a liquid level height of 0.37 mm or more from the bottom surface.

3. The manufacturing method according to claim 1 or 2, characterized in that: The grooves are formed in communication with each other.

4. The manufacturing method according to claim 3, characterized in that: The grooves are formed in a lattice shape.

5. The manufacturing method according to claim 4, characterized in that: The grooves are formed at a predetermined pitch, and the pitch is not less than 8 mm and not more than 20 mm.

6. A chemical liquid dish for use in the manufacture of an exhaust gas purification catalyst, the exhaust gas purification catalyst purifying exhaust gas discharged from an internal combustion engine, the chemical liquid dish being characterized by: having a recessed portion consisting of a bottom wall and side walls rising from the bottom wall, A groove having a predetermined pattern is formed on the surface of the bottom wall on the side of the recessed portion. The average depth of the groove is 1.2 mm or more and 3 mm or less. The average width of the grooves is not less than 1.6 mm and not more than 3 mm.

Citation Information

Patent Citations

  • Catalyst for cleaning exhaust gas

    JP2003334444A

  • Disinfectant composition and disinfecting spray

    JP2022057214A