Antibacterial cream formula
By using antibacterial formulas of nano zinc oxide and lysozyme in cream paper, the stability and mildew problems of cream paper are solved, and efficient antibacterial effects and moisturizing properties are achieved, simplifying the production process and reducing costs.
Patent Information
- Application Number
- CN202411089610.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-26
AI Technical Summary
The cream paper made from ordinary creams has the risk of nourishing microorganisms and spoiling due to the existence of water, resulting in poor product stability.
The nano zinc oxide dispersion and lysozyme combined with the white oil emulsion are used to form an antibacterial cream formula. The nano zinc oxide dispersion includes 10%-20% nano zinc oxide, 0.5%-1.5% sodium polyacrylate, 2.0%-6.0% PEG-2000, white oil emulsion includes 20% #7 white oil, 4% Sipan-60, and 3% Tween-60, which is prepared by grinding and emulsification processes to form a broad-spectrum, powerful antibacterial antibacterial liquid.
It realizes the stability and anti-mold effect of cream paper, has zero-grade anti-mold effect, improves the softness and moisturizing properties of cream paper, reduces production costs and coating usage, and simplifies the production process.
Smart Images

Figure CN119015164A_ABST
Abstract
Description
Technical Field
[0001] The invention mainly relates to the field of cream preparation, and in particular to an antibacterial cream formula. Background Art
[0002] Cream tissue is a tissue with specially added moisturizing ingredients. It is different from the rough and dry tissue. It is more than three times softer than ordinary tissue. It is very suitable for wiping the skin, especially the delicate skin of babies. The cream needs to be prepared during the production process of cream paper.
[0003] The inventor discovered the following defects during the operation of the specific embodiment: However, the cream paper made from ordinary creams inevitably has the risk of nourishing microorganisms and deteriorating due to the presence of water.
[0004] It should be noted that the above contents belong to the technical cognition scope of the inventor. Since the technical contents in this field are vast and too complicated, the above contents of this application do not necessarily constitute prior art. Summary of the invention
[0005] 1. Technical problems to be solved by the invention: The present invention provides an antibacterial cream formula to solve the technical problems existing in the above-mentioned background technology.
[0006] 2. Technical solution: To achieve the above object, the technical solution provided by the present invention is: an antibacterial cream formula, comprising 1%-2% of nano zinc oxide dispersion, 2%-5% of white oil emulsion, 20%-30% of glycerol, 1% of lysozyme, and the rest of pure water; The white oil emulsion in the formula can give the paper a soft and smooth property, making the user feel silky; glycerin provides a good wet feeling and stable moisturizing properties.
[0007] Furthermore, the nano zinc oxide dispersion includes the following raw materials: 10%-20% nano zinc oxide, 0.5%-1.5% sodium polyacrylate, 2.0%-6.0% PEG-2000, 1%-5% pH buffer, and the rest is pure water.
[0008] Furthermore, the white oil emulsion comprises the following formula raw materials: 20% #7 white oil, 4% Span-60, 3% Tween-60, and the rest is pure water.
[0009] Furthermore, the nano zinc oxide and lysozyme are used for antibacterial and anti-mildew effects.
[0010] Furthermore, the nano zinc oxide dispersion is prepared by the following method: sodium polyacrylate and PEG-2000 are dissolved in pure water, stirred at 600 r / min to dissolve, zinc oxide powder is added for pre-dispersion, and after the pre-dispersion is completed, the sodium polyacrylate, PEG-2000 and zinc oxide mixture is put into a grinder and ground until the zinc oxide particle size D-90 is between 1nm and 100nm, thereby obtaining a stable nano zinc oxide dispersion.
[0011] Furthermore, the white oil emulsion is prepared by the following method: #7 white oil, Span-60, and Tween-60 are placed in an emulsifying kettle, heated at 80° C. to dissolve the components, stirred at a speed of 3000 r / min, and the remaining pure water is slowly added until the emulsification is completed.
[0012] Furthermore, the pH buffer is one of Tris-HCl, phosphate buffer and acetate buffer.
[0013] 3. Beneficial effects: Compared with the prior art, the technical solution provided by the present invention has the following beneficial effects: The present invention compounds nano zinc oxide with lysozyme to obtain an antibacterial liquid with a broad spectrum, strong antibacterial effect and zero-level mildew-proof effect. Nano zinc oxide has two antibacterial effects: photocatalytic antibacterial and metal ion dissolution antibacterial. Under light, especially ultraviolet light, nano zinc oxide can stimulate oxygen in the air to become active oxygen, and react with a variety of microorganisms to produce oxidation reactions, thereby killing bacteria. In the solution, zinc ions will also gradually become free, and when they come into contact with bacteria, they will combine with the bacteria to make them inactive, thereby killing the bacteria.
[0014] This antibacterial liquid has the advantages of high efficacy, mild use conditions, simple operation, low equipment requirements, extremely fast processing speed, and no secondary pollution.
[0015] The antibacterial cream prepared by the method ensures the stability of the cream paper product and gives the cream paper new efficacy. The new emulsification production process is simple, the cream production cost is low, the cream coating amount is small, and the cream has high versatility.
[0016] The present invention reduces the proportion of macromolecules in the cream by introducing white oil emulsion into the cream system, improves the uniformity and penetration efficiency of the cream during coating, and improves the softness and smoothness of the cream paper. At the same time, due to the improvement of penetration efficiency, the time required for the cream paper to stand still after coating is greatly shortened, so that it can be directly cut and packaged, thereby improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 This is a diagram showing the mildew-proof effect of ordinary paper of the present invention; Figure 2This is a diagram showing the anti-mildew effect of the antibacterial cream paper of the present invention; Figure 3 This is a diagram showing the antibacterial effect of ordinary paper of the present invention; Figure 4 This is an antibacterial effect diagram of the antibacterial cream of the present invention; Figure 5 This is a sensory evaluation comparison chart of the present invention; Figure 6 This is a comparison diagram of the moisturizing effect of the present invention; Figure 7 This is a sensory evaluation comparison chart of the present invention; Figure 8 This is a comparison diagram of the moisturizing effect of the present invention; Fig. 9 This is a sensory evaluation comparison chart of the present invention; Fig.10 This is a comparison diagram of the moisturizing effect of the present invention; Fig.11 This is a sensory evaluation comparison chart of the present invention; Fig.12 It is a comparison chart of the moisturizing effect of the present invention. DETAILED DESCRIPTION
[0018] To facilitate understanding of the present invention, the present invention will be described more comprehensively below with reference to the relevant drawings. Several embodiments of the present invention are shown in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive. Example 1
[0019] 1. Preparation of white oil emulsion (taking the preparation of 100g white oil emulsion as an example): Weigh 20g#7 white oil (liquid), 4g Span-60 (solid), and 3g Tween-60 (liquid), and melt and mix the components completely at 80℃ and 500r / min. After mixing evenly, maintain the temperature at 80℃, increase the stirring speed to 3000r / min, and slowly add 73g of pure water to complete emulsification. After emulsification, a stable white oil emulsion is obtained. In the process of slowly adding pure water, a complete phase change occurs, and the emulsification completion degree can be determined by observing the phase change process.
[0020] 2. Preparation of nano zinc oxide solution (taking the preparation of 100g nano zinc oxide solution as an example): Weigh 0.5g sodium polyacrylate, 1.5g PEG-2000, and 87.5g pure water, stir and dissolve at room temperature and 500r / min. Then add 10g zinc oxide powder, stir to obtain a suspension of sodium polyacrylate, PEG-2000, and zinc oxide. Pour the suspension into a grinder and grind to obtain a small-particle, stably dispersed nano zinc oxide solution.
[0021] 3. Preparation of antibacterial cream (taking the preparation of 100g antibacterial cream as an example): Take 1g of nano zinc oxide dispersion, 2g of white oil emulsion, 20g of glycerol, 1g of lysozyme, and 76g of pure water, stir and mix at 500r / min to obtain an antibacterial cream.
[0022] 4. Coating: Pour the antibacterial cream into the emulsion storage tank of the coating machine, turn on the coating machine, and the emulsion is evenly attached to the paper through the coating rubber roller. After cutting, the finished cream paper is obtained.
[0023] 5. Sample analysis: (1) Antibacterial and mildew proofing effect test: Take samples and refer to the standards "Test Method for Antibacterial Performance of Plastics" GB / T24128-2009 and "Sanitary Standard for Disposable Hygiene Products" GB15979-2002 Appendix C Product Bactericidal Performance, Antibacterial Performance and Stability Test Method C4 Dissolution Antibacterial (Inhibitory) Product Antibacterial Performance Test Method. Determine the antibacterial and mildew proofing effects of cream paper; (2) Sensory evaluation: Sensory evaluation of moistness, smoothness, and fluffiness. The base paper without cream coating was used as the benchmark with a score of 2 (out of 5), and compared with the coated cream paper; (3) Evaluation of moisturizing effect: Under the condition of 25℃ and 30% humidity, the base paper without cream coating was used as the benchmark and compared with the cream coated paper.
[0024] 6. Test results: (1) The antibacterial rate of cream paper is 99.99%, and the anti-mildew effect is zero level; uncoated base paper has no antibacterial or anti-mildew effect; (2) Sensory evaluation: Figure 5 As shown; (3) Evaluation of moisturizing effect: Figure 6 shown. Example 2
[0025] 1. Preparation of white oil emulsion (taking the preparation of 100g white oil emulsion as an example): Weigh 20g#7 white oil (liquid), 4g Span-60 (solid), and 3g Tween-60 (liquid), and melt and mix the components completely at 80℃ and 500r / min. After mixing evenly, maintain the temperature at 80℃, increase the stirring speed to 3000r / min, and slowly add 73g of pure water to complete emulsification. After emulsification, a stable white oil emulsion is obtained. In the process of slowly adding pure water, a complete phase change occurs, and the emulsification completion degree can be determined by observing the phase change process.
[0026] 2. Preparation of nano zinc oxide solution (taking the preparation of 100g nano zinc oxide solution as an example): Weigh 0.5g sodium polyacrylate, 1.5g PEG-2000, and 87.5g pure water, stir and dissolve at room temperature and 500r / min. Then add 10g zinc oxide powder, stir to obtain a suspension of sodium polyacrylate, PEG-2000, and zinc oxide. Pour the suspension into a grinder and grind to obtain a small-particle, stably dispersed nano zinc oxide solution.
[0027] 3. Preparation of antibacterial cream (taking the preparation of 100g antibacterial cream as an example): Take 1g of nano zinc oxide dispersion, 3g of white oil emulsion, 25g of glycerol, 1g of lysozyme, and 70g of pure water, stir and mix at 500r / min to obtain an antibacterial cream.
[0028] 4. Coating: Pour the antibacterial cream into the emulsion storage tank of the coating machine, turn on the coating machine, and the emulsion is evenly attached to the paper through the coating rubber roller. After cutting, the finished cream paper is obtained.
[0029] 5. Sample analysis: (1) Antibacterial and mildew proofing effect test: Take samples and refer to the standards "Test Method for Antibacterial Performance of Plastics" GB / T24128-2009 and "Sanitary Standard for Disposable Hygiene Products" GB15979-2002 Appendix C Product Bactericidal Performance, Antibacterial Performance and Stability Test Method C4 Dissolution Antibacterial (Inhibitory) Product Antibacterial Performance Test Method. Determine the antibacterial and mildew proofing effects of cream paper; (2) Sensory evaluation: Sensory evaluation of moistness, smoothness, and fluffiness. The base paper without cream coating was used as the benchmark with a score of 2 (out of 5), and compared with the coated cream paper; (3) Evaluation of moisturizing effect: Under the condition of 25℃ and 30% humidity, the base paper without cream coating was used as the benchmark and compared with the cream coated paper.
[0030] 6. Test results: (1) The antibacterial rate of cream paper is 99.99%, and the anti-mildew effect is zero level; uncoated base paper has no antibacterial or anti-mildew effect; (2) Sensory evaluation: Figure 7 As shown; (3) Evaluation of moisturizing effect: Figure 8 shown. Example 3
[0031] 1. Preparation of white oil emulsion (taking the preparation of 100g white oil emulsion as an example): Weigh 20g#7 white oil (liquid), 4g Span-60 (solid), and 3g Tween-60 (liquid), and melt and mix the components completely at 80℃ and 500r / min. After mixing evenly, maintain the temperature at 80℃, increase the stirring speed to 3000r / min, and slowly add 73g of pure water to complete emulsification. After emulsification, a stable white oil emulsion is obtained. In the process of slowly adding pure water, a complete phase change occurs, and the emulsification completion degree can be determined by observing the phase change process.
[0032] 2. Preparation of nano zinc oxide solution (taking the preparation of 100g nano zinc oxide solution as an example): Weigh 0.5g sodium polyacrylate, 1.5g PEG-2000, and 87.5g pure water, stir and dissolve at room temperature and 500r / min. Then add 10g zinc oxide powder, stir to obtain a suspension of sodium polyacrylate, PEG-2000, and zinc oxide. Pour the suspension into a grinder and grind to obtain a small-particle, stably dispersed nano zinc oxide solution.
[0033] 3. Preparation of antibacterial cream (taking the preparation of 100g antibacterial cream as an example): Take 2g of nano zinc oxide dispersion, 4g of white oil emulsion, 25g of glycerol, 1g of lysozyme, and 68g of pure water, stir and mix at 500r / min to obtain an antibacterial cream.
[0034] 4. Coating: Pour the antibacterial cream into the emulsion storage tank of the coating machine, turn on the coating machine, and the emulsion is evenly attached to the paper through the coating rubber roller. After cutting, the finished cream paper is obtained.
[0035] 5. Sample analysis: (1) Antibacterial and mildew proofing effect test: Take samples and refer to the standards "Test Method for Antibacterial Performance of Plastics" GB / T24128-2009 and "Sanitary Standard for Disposable Hygiene Products" GB15979-2002 Appendix C Product Bactericidal Performance, Antibacterial Performance and Stability Test Method C4 Dissolution Antibacterial (Inhibitory) Product Antibacterial Performance Test Method. Determine the antibacterial and mildew proofing effects of cream paper; (2) Sensory evaluation: Sensory evaluation of moistness, smoothness, and fluffiness. The base paper without cream coating was used as the benchmark with a score of 2 (out of 5), and compared with the coated cream paper; (3) Evaluation of moisturizing effect: Under the condition of 25℃ and 30% humidity, the base paper without cream coating was used as the benchmark and compared with the cream coated paper.
[0036] 6. Test results: (1) The antibacterial rate of cream paper is 99.99%, and the anti-mildew effect is zero level; uncoated base paper has no antibacterial or anti-mildew effect; (2) Sensory evaluation: Fig. 9 As shown; (3) Evaluation of moisturizing effect: Fig.10 shown. Example 4
[0037] 1. Preparation of white oil emulsion (taking the preparation of 100g white oil emulsion as an example): Weigh 20g#7 white oil (liquid), 4g Span-60 (solid), and 3g Tween-60 (liquid), and melt and mix the components completely at 80℃ and 500r / min. After mixing evenly, maintain the temperature at 80℃, increase the stirring speed to 3000r / min, and slowly add 73g of pure water to complete emulsification. After emulsification, a stable white oil emulsion is obtained. In the process of slowly adding pure water, a complete phase change occurs, and the emulsification completion degree can be determined by observing the phase change process.
[0038] 2. Preparation of nano zinc oxide solution (taking the preparation of 100g nano zinc oxide solution as an example): Weigh 0.5g sodium polyacrylate, 1.5g PEG-2000, and 87.5g pure water, stir and dissolve at room temperature and 500r / min. Then add 10g zinc oxide powder, stir to obtain a suspension of sodium polyacrylate, PEG-2000, and zinc oxide. Pour the suspension into a grinder and grind to obtain a small-particle, stably dispersed nano zinc oxide solution.
[0039] 3. Preparation of antibacterial cream (taking the preparation of 100g antibacterial cream as an example): Take 2g of nano zinc oxide dispersion, 5g of white oil emulsion, 30g of glycerol, 1g of lysozyme, and 62g of pure water, and stir and mix at 500r / min to obtain an antibacterial cream.
[0040] 4. Coating: Pour the antibacterial cream into the emulsion storage tank of the coating machine, turn on the coating machine, and the emulsion is evenly attached to the paper through the coating rubber roller. After cutting, the finished cream paper is obtained.
[0041] 5. Sample analysis: (1) Antibacterial and mildew proofing effect test: Take samples and refer to the standards "Test Method for Antibacterial Performance of Plastics" GB / T24128-2009 and "Sanitary Standard for Disposable Hygiene Products" GB15979-2002 Appendix C Product Bactericidal Performance, Antibacterial Performance and Stability Test Method C4 Dissolution Antibacterial (Inhibitory) Product Antibacterial Performance Test Method. Determine the antibacterial and mildew proofing effects of cream paper; (2) Sensory evaluation: Sensory evaluation of moistness, smoothness, and fluffiness. The base paper without cream coating was used as the benchmark with a score of 2 (out of 5), and compared with the coated cream paper; (3) Evaluation of moisturizing effect: Under the condition of 25℃ and 30% humidity, the base paper without cream coating was used as the benchmark and compared with the cream coated paper.
[0042] 6. Test results: (1) The antibacterial rate of cream paper is 99.99%, and the anti-mildew effect is zero level; uncoated base paper has no antibacterial or anti-mildew effect; (2) Sensory evaluation: Fig.11 As shown; (3) Evaluation of moisturizing effect: Fig.12 shown.
[0043] The above-described embodiments only express a certain implementation mode of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the patent scope of the present invention. It should be pointed out that, for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims.
Claims
1. An antibacterial cream formula, Features: The formula includes the following ingredients: Nano zinc oxide dispersion 1%-2%, white oil emulsion 2%-5%, glycerol 20%-30%, lysozyme 1%, and the rest is pure water; The white oil emulsion in the formula can give the paper a soft and smooth property, making the user feel silky; glycerin provides a good wet feeling and stable moisturizing properties.
2. An antibacterial cream formulation according to claim 1, Features: The nano zinc oxide dispersion comprises the following raw materials: 10%-20% nano zinc oxide, 0.5%-1.5% sodium polyacrylate, 2.0%-6.0% PEG-2000, 1%-5% PH buffer, and the rest is pure water.
3. An antibacterial cream formulation according to claim 1, Features: The white oil emulsion comprises the following raw materials: 20% #7 white oil, 4% Span-60, 3% Tween-60, and the rest is pure water.
4. The antibacterial cream formulation according to claim 1, Features: The nano zinc oxide and lysozyme are used for antibacterial and mildew-proofing.
5. An antibacterial cream formulation according to claim 1, Features: The nano zinc oxide dispersion is prepared by the following method: sodium polyacrylate and PEG-2000 are added to pure water, stirred and dissolved at 600 r / min, zinc oxide powder is added for pre-dispersion, and after the pre-dispersion is completed, the sodium polyacrylate, PEG-2000 and zinc oxide mixed solution is put into a grinder for grinding until the zinc oxide particle size D-90 is between 1nm and 100nm, so as to obtain a stable nano zinc oxide dispersion.
6. The antibacterial cream formulation according to claim 1, Features: The white oil emulsion is prepared by the following method: #7 white oil, Span-60 and Tween-60 are placed in an emulsifying kettle, heated at 80° C. to dissolve the components, stirred at a speed of 3000 r / min, and slowly added with the remaining pure water until emulsification is completed.
7. An antibacterial cream formulation according to claim 2, Features: The pH buffer is one of Tris-HCl, phosphate buffer and acetate buffer.