Novel foul and odorous gas adsorbent and preparation method thereof
By using new dirty odor gas adsorbents prepared by nano calcium hydroxide, modified zeolite microspheres and other materials, the problems of high cost and poor adsorption effect in the existing technology are solved, and efficient adsorption of various odors is achieved. , suitable for industrial applications.
Patent Information
- Application Number
- CN202411450303.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-17
- Publication Date
- 2024-11-26
AI Technical Summary
The production cost of existing dirty odor gas adsorbents is high and the adsorption effect of different odor or harmful gases varies.
The new type of odor gas adsorbent is formed by nano calcium hydroxide, modified zeolite microspheres, alumina, butyl titanate, anhydrous ethanol, nitric acid and deionized water, and is treated with specific stirring, heating, ultrasonication, etc. Steps are prepared to form a polysolid solid acid with good compatibility, and the adsorption capacity is improved by acid-base composite adsorption and physical adsorption.
It reduces production costs and energy consumption, improves the adsorption capacity of various odors, is suitable for large-scale and automated production, and simplifies the process flow.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of foul and odorous gas treatment, and specifically relates to a novel foul and odorous gas adsorbent and a preparation method thereof. Background Art
[0002] Smelly gas includes various odors and harmful gases, such as ammonia, hydrogen sulfide, mercaptans, dimethylthiomethylamine, formaldehyde, etc. At present, the methods for treating odorous gas include combustion, oxidation, absorption, adsorption, neutralization and biological methods. The combustion method has high decomposition efficiency, but the energy consumption, equipment and other processing costs are high, and secondary pollutants are easily generated during the treatment; the oxidation method has high treatment efficiency, but the cost of the oxidant used is high; the absorption method has a large treatment volume, but the treatment efficiency is not high, and the waste liquid after absorption still needs to be harmlessly treated; the neutralization method can quickly eliminate the impact of odor, but a large amount of neutralizer is required; the biological method has good removal efficiency and no secondary pollution, but the reaction conditions are difficult to control, and the investment and operation costs are high; the adsorption method has good treatment efficiency, simple operation, and relatively low treatment costs. It is widely used in industries and life, and is one of the main methods used and improved in the field of odor treatment. Its shortcomings are that the production cost of the adsorbent based on activated carbon is high, and there are obvious differences in the adsorption effect for different odors or harmful gases. Summary of the invention
[0003] In view of the above-mentioned deficiencies, the present invention discloses a novel odorous gas adsorbent and a preparation method thereof, which solves the problems of high production cost of the adsorbent and different adsorption effects of the adsorbent on different odors or harmful gases.
[0004] The present invention is achieved by adopting the following technical solutions: A novel foul gas adsorbent comprises the following raw material components in parts by weight: 30-40 parts of nano calcium hydroxide, 10-20 parts of modified zeolite microspheres, 10-20 parts of aluminum oxide, 20-40 parts of butyl titanate, 80-150 parts of anhydrous ethanol, 5-10 parts of nitric acid, and 5-10 parts of deionized water; The preparation method of the modified zeolite microspheres is to add a silane coupling agent and a zeolite to an ethanol solution in sequence, then stir and react at a temperature of 50 to 60° C. for 10 to 20 minutes, then add cellulose and continue to react for 30 to 60 minutes, then stand for 30 minutes and filter and dry to obtain the modified zeolite, wherein the mass ratio of the silane coupling agent, zeolite and cellulose is (0.1 to 0.5):10:(2 to 3), and the volume ratio of the ethanol solution and the mass ratio of the zeolite is (10 to 30) mL:1 g; add polyacrylic acid resin to deionized water under stirring conditions, heat to 60 to 80° C. and keep the temperature constant, then add the modified zeolite and continue to react for 3 to 5 hours, then naturally cool to room temperature, filter and dry to obtain the modified zeolite microspheres, and the mass ratio of the modified zeolite to the polyacrylic acid resin is 1:(5 to 10).
[0005] Furthermore, the particle size of the nano calcium hydroxide is 10 to 30 nm.
[0006] Furthermore, the ethanol solution is an ethanol solution with a mass fraction of 20% to 30%.
[0007] Furthermore, the particle size of the zeolite is 80-100 μm.
[0008] The preparation method of the novel foul gas adsorbent comprises the following steps: (1) Weigh each raw material component in proportion, add anhydrous ethanol to butyl titanate under stirring at a speed of 50 to 100 r / min, then add nitric acid and deionized water to react for 2 to 3 hours, then slowly add alumina and continue stirring for 1 to 2 hours to obtain a colloidal solution; (2) Add modified zeolite microspheres to the colloidal solution obtained in step (1), then stir at a speed of 200 to 300 r / min for 10 to 15 minutes, then add nano calcium hydroxide and continue stirring for 15 to 30 minutes, and then freeze-dry to obtain a new type of foul gas adsorbent.
[0009] Furthermore, in step (1), anhydrous ethanol is added to butyl titanate under stirring conditions at a speed of 50 to 100 r / min, and then nitric acid and deionized water are added after heating to 40 to 50° C. to react for 2 to 3 hours.
[0010] Furthermore, in step (1), the addition time of alumina is controlled within 20 to 30 minutes.
[0011] Furthermore, in step (2), the modified zeolite microspheres are added to the colloidal solution obtained in step (1), and then the solution is treated for 10 to 15 minutes under the conditions of stirring at a speed of 200 to 300 r / min and ultrasound; the frequency of the ultrasound is 20 to 40 KHz. The use of ultrasound treatment can improve the dispersion of the modified zeolite microspheres in the colloidal solution, which is conducive to the modified zeolite microspheres adsorbing and encapsulating the alumina and titanium dioxide particles.
[0012] Compared with the prior art, this technical solution has the following beneficial effects: 1. The present invention first uses cellulose and silane coupling agent to modify zeolite under certain conditions, and mixes the obtained modified zeolite with polyacrylic resin to obtain modified zeolite microspheres. At the same time, anhydrous ethanol and butyl titanate are mixed, and nitric acid and deionization are added to prepare titanium dioxide sol, and then aluminum oxide is added to prepare a composite sol of aluminum oxide and titanium dioxide. Then the modified zeolite microspheres and the composite sol are mixed, and the modified zeolite microspheres and the composite sol have good compatibility. The modified zeolite microspheres are used to adsorb and wrap aluminum oxide and titanium dioxide particles, and can promote the regular arrangement of aluminum oxide and titanium dioxide particles on the surface of the modified zeolite microspheres, thereby obtaining a multi-particle solid acid with good performance, and finally the obtained multi-particle solid acid and nano-calcium hydroxide are compounded to obtain a new type of foul gas adsorbent, and the adsorption capacity of the adsorbent for various odors is improved by using the synergistic effect of the composite adsorption of acid and base and the physical adsorption of nano-calcium hydroxide.
[0013] 2. The process of the present invention is simple, the reaction conditions are mild, it is easy to control, the energy consumption and raw material costs are low, and it is suitable for large-scale and automated production. DETAILED DESCRIPTION
[0014] The present invention is further described by the following examples, but is not intended to be limiting of the present invention. Specific experimental conditions and methods not specified in the following examples are conventional methods commonly known to those skilled in the art.
[0015] Example 1: A novel foul gas adsorbent, comprising the following raw material components in parts by weight: 35 parts of nano calcium hydroxide, 15 parts of modified zeolite microspheres, 12 parts of aluminum oxide, 30 parts of butyl titanate, 100 parts of anhydrous ethanol, 8 parts of nitric acid, and 6 parts of deionized water; The preparation method of the modified zeolite microspheres is to add a silane coupling agent and a zeolite to an ethanol solution in sequence, then stir and react at a temperature of 53° C. for 15 minutes, then add cellulose and continue to react for 45 minutes, then stand for 30 minutes and filter and dry to obtain the modified zeolite, wherein the mass ratio of the silane coupling agent, zeolite and cellulose is 0.2:10:2.3, and the volume ratio of the ethanol solution and the mass ratio of the zeolite is 20 mL:1 g; add polyacrylic acid resin to deionized water under stirring, heat to 75° C. and keep the temperature constant, then add the modified zeolite and continue to react for 4 hours, then naturally cool to room temperature, filter and dry to obtain the modified zeolite microspheres, wherein the mass ratio of the modified zeolite to the polyacrylic acid resin is 1:6; The particle size of the nano calcium hydroxide is 20 nm; the ethanol solution is an ethanol solution with a mass fraction of 25%; and the particle size of the zeolite is 90 μm.
[0016] The preparation method of the novel foul gas adsorbent described in this embodiment comprises the following steps: (1) Weigh each raw material component in proportion, add anhydrous ethanol to butyl titanate under stirring at a speed of 80 r / min, then heat to 42°C, add nitric acid and deionized water, react for 2.5 hours, then slowly add alumina and continue stirring for 1.5 hours. The addition time of alumina is controlled within 25 minutes to obtain a colloidal solution; (2) Adding modified zeolite microspheres to the colloidal solution obtained in step (1), and then treating it for 12 minutes under stirring speed of 250 r / min and ultrasonic conditions, adding nano calcium hydroxide and continuing stirring for 20 minutes, and then freeze-drying to obtain a new type of foul gas adsorbent; the frequency of the ultrasonic wave is 30 kHz.
[0017] Example 2: A novel foul gas adsorbent, comprising the following raw material components in parts by weight: 30 parts of nano calcium hydroxide, 10 parts of modified zeolite microspheres, 10 parts of aluminum oxide, 20 parts of butyl titanate, 80 parts of anhydrous ethanol, 5 parts of nitric acid, and 5 parts of deionized water; The preparation method of the modified zeolite microspheres is to add a silane coupling agent and a zeolite to an ethanol solution in sequence, then stir and react at a temperature of 50°C for 10 minutes, then add cellulose to continue to react for 30 minutes, and then stand for 30 minutes before filtering and drying to obtain the modified zeolite, wherein the mass ratio of the silane coupling agent, zeolite and cellulose is 0.1:10:2, and the volume ratio of the ethanol solution to the mass ratio of the zeolite is 10mL:1g; add polyacrylic acid resin to deionized water under stirring conditions, heat to 60°C and keep the temperature constant, then add the modified zeolite to continue to react for 3 hours, then naturally cool to room temperature, filter and dry to obtain the modified zeolite microspheres, and the mass ratio of the modified zeolite to the polyacrylic acid resin is 1:5; The particle size of the nano calcium hydroxide is 10 nm; the ethanol solution is an ethanol solution with a mass fraction of 20%; and the particle size of the zeolite is 80 μm.
[0018] The preparation method of the novel foul gas adsorbent described in this embodiment comprises the following steps: (1) Weigh each raw material component in proportion, add anhydrous ethanol to butyl titanate under stirring at a speed of 50 r / min, then heat to 40°C, add nitric acid and deionized water to react for 2 h, then slowly add alumina and continue stirring for 1 h. The addition time of alumina is controlled within 20 min to obtain a colloidal solution; (2) Adding modified zeolite microspheres to the colloidal solution obtained in step (1), and then treating the solution under ultrasonic conditions at a stirring speed of 200 r / min for 10 min, adding nano calcium hydroxide and continuing stirring for 15 min, and then freeze-drying to obtain a novel odorous gas adsorbent; the frequency of the ultrasonic treatment is 20 kHz.
[0019] Example 3: A novel foul gas adsorbent, comprising the following raw material components in parts by weight: 38 parts of nano calcium hydroxide, 18 parts of modified zeolite microspheres, 18 parts of aluminum oxide, 35 parts of butyl titanate, 120 parts of anhydrous ethanol, 7.5 parts of nitric acid, and 8 parts of deionized water; The preparation method of the modified zeolite microspheres is to add a silane coupling agent and a zeolite to an ethanol solution in sequence, then stir and react at a temperature of 58° C. for 15 minutes, then add cellulose to continue to react for 35 minutes, and then stand for 30 minutes and filter and dry to obtain the modified zeolite, wherein the mass ratio of the silane coupling agent, zeolite and cellulose is 0.4:10:2.7, and the volume ratio of the ethanol solution and the mass ratio of the zeolite is 25 mL:1 g; add polyacrylic acid resin to deionized water under stirring, heat to 65° C. and keep the temperature constant, then add the modified zeolite to continue to react for 4.5 hours, then naturally cool to room temperature, filter and dry to obtain the modified zeolite microspheres, and the mass ratio of the modified zeolite to the polyacrylic acid resin is 1:7.5; The particle size of the nano calcium hydroxide is 25 nm; the ethanol solution is an ethanol solution with a mass fraction of 25%; and the particle size of the zeolite is 85 μm.
[0020] The preparation method of the novel foul gas adsorbent described in this embodiment comprises the following steps: (1) Weigh each raw material component in proportion, add anhydrous ethanol to butyl titanate under stirring at a speed of 60 r / min, then heat to 48°C, add nitric acid and deionized water, react for 2.5 hours, then slowly add alumina and continue stirring for 1.5 hours. The addition time of alumina is controlled within 25 minutes to obtain a colloidal solution; (2) Adding modified zeolite microspheres to the colloidal solution obtained in step (1), and then treating it for 12 minutes under stirring speed of 250 r / min and ultrasonic conditions, adding nano calcium hydroxide and continuing stirring for 25 minutes, and then freeze-drying to obtain a new type of foul gas adsorbent; the frequency of the ultrasonic wave is 30 kHz.
[0021] Example 4: A novel foul gas adsorbent, comprising the following raw material components in parts by weight: 40 parts of nano calcium hydroxide, 20 parts of modified zeolite microspheres, 20 parts of aluminum oxide, 40 parts of butyl titanate, 150 parts of anhydrous ethanol, 10 parts of nitric acid, and 10 parts of deionized water; The preparation method of the modified zeolite microspheres is to add a silane coupling agent and a zeolite to an ethanol solution in sequence, then stir and react at a temperature of 60° C. for 20 minutes, then add cellulose and continue to react for 60 minutes, and then stand for 0.5:10:3, wherein the volume ratio of the ethanol solution to the mass ratio of the zeolite is 30 mL:1 g; add a polyacrylic acid resin to deionized water under stirring conditions, heat to 80° C. and keep the temperature constant, then add the modified zeolite and continue to react for 5 hours, then naturally cool to room temperature, filter and dry to obtain the modified zeolite microspheres, wherein the mass ratio of the modified zeolite to the polyacrylic acid resin is 1:10; The particle size of the nano calcium hydroxide is 30 nm; the ethanol solution is an ethanol solution with a mass fraction of 30%; and the particle size of the zeolite is 100 μm.
[0022] The preparation method of the novel foul gas adsorbent described in this embodiment comprises the following steps: (1) Weigh each raw material component in proportion, add anhydrous ethanol to butyl titanate under stirring at a speed of 100 r / min, then heat to 50°C and add nitric acid and deionized water to react for 3 hours, then slowly add alumina and continue stirring for 2 hours. The addition time of alumina is controlled within 30 minutes to obtain a colloidal solution; (2) Adding modified zeolite microspheres to the colloidal solution obtained in step (1), and then treating the solution under ultrasonic conditions at a stirring speed of 300 r / min for 15 min, adding nano calcium hydroxide and continuing stirring for 30 min, and then freeze-drying to obtain a novel foul gas adsorbent; the frequency of the ultrasonic treatment is 40 kHz.
[0023] Comparative Example 1: A novel odorous gas adsorbent, comprising the following raw material components in parts by weight: 35 parts of nano calcium hydroxide, 15 parts of zeolite, 12 parts of aluminum oxide, 30 parts of butyl titanate, 100 parts of anhydrous ethanol, 8 parts of nitric acid, and 6 parts of deionized water; The particle size of the nano calcium hydroxide is 20 nm.
[0024] The preparation method of the novel foul gas adsorbent described in this embodiment comprises the following steps: (1) Weigh each raw material component in proportion, add anhydrous ethanol to butyl titanate under stirring at a speed of 80 r / min, then heat to 42°C, add nitric acid and deionized water, react for 2.5 hours, then slowly add alumina and continue stirring for 1.5 hours. The addition time of alumina is controlled within 25 minutes to obtain a colloidal solution; (2) Add zeolite to the colloidal solution obtained in step (1), then treat it under ultrasonic conditions at a stirring speed of 250 r / min for 12 minutes, then add nano calcium hydroxide and continue stirring for 20 minutes, and then freeze-dry to obtain a new type of foul gas adsorbent; the frequency of the ultrasonic wave is 30 kHz.
[0025] Comparative Example 2: A novel foul gas adsorbent, comprising the following raw material components in parts by weight: 35 parts of nano calcium hydroxide, 15 parts of modified zeolite microspheres, 12 parts of aluminum oxide, and 100 parts of anhydrous ethanol; The preparation method of the modified zeolite microspheres is to add a silane coupling agent and a zeolite to an ethanol solution in sequence, then stir and react at a temperature of 53° C. for 15 minutes, then add cellulose and continue to react for 45 minutes, then stand for 30 minutes and filter and dry to obtain the modified zeolite, wherein the mass ratio of the silane coupling agent, zeolite and cellulose is 0.2:10:2.3, and the volume ratio of the ethanol solution and the mass ratio of the zeolite is 20 mL:1 g; add polyacrylic acid resin to deionized water under stirring, heat to 75° C. and keep the temperature constant, then add the modified zeolite and continue to react for 4 hours, then naturally cool to room temperature, filter and dry to obtain the modified zeolite microspheres, wherein the mass ratio of the modified zeolite to the polyacrylic acid resin is 1:6; The particle size of the nano calcium hydroxide is 20 nm; the ethanol solution is an ethanol solution with a mass fraction of 25%; and the particle size of the zeolite is 90 μm.
[0026] The preparation method of the novel foul gas adsorbent described in this embodiment comprises the following steps: (1) Weigh the raw material components in proportion, add anhydrous ethanol to alumina at a stirring speed of 80 r / min and continue stirring for 1.5 hours, then add modified zeolite microspheres, then treat at a stirring speed of 250 r / min and ultrasonic conditions for 12 minutes, then add nano calcium hydroxide and continue stirring for 20 minutes, and then freeze-dry to obtain a new type of foul gas adsorbent; the frequency of the ultrasound is 30 kHz.
[0027] Comparative Example 3: A novel foul gas adsorbent, comprising the following raw material components in parts by weight: 35 parts of nano calcium hydroxide, 12 parts of aluminum oxide, 30 parts of butyl titanate, 100 parts of anhydrous ethanol, 8 parts of nitric acid, and 6 parts of deionized water; The particle size of the nano calcium hydroxide is 20 nm.
[0028] The preparation method of the novel foul gas adsorbent described in this embodiment comprises the following steps: (1) Weigh each raw material component in proportion, add anhydrous ethanol to butyl titanate under stirring at a speed of 80 r / min, then heat to 42°C, add nitric acid and deionized water, react for 2.5 hours, then slowly add alumina and continue stirring for 1.5 hours. The addition time of alumina is controlled within 25 minutes to obtain a colloidal solution; (2) Adding nano calcium hydroxide to the colloidal solution obtained in step (1), stirring for 20 minutes, and then freeze-drying to obtain a novel odorous gas adsorbent; the frequency of the ultrasound is 30 KHz.
[0029] Experimental example: A new type of foul gas adsorbent was prepared according to the method described in Examples 1 to 4 and Comparative Examples 1 to 3. Equal weights of the above adsorbents were placed in an adsorption tank respectively. Then, at 25°C, the same kind of foul gas was introduced into each adsorption tank at the same speed. The foul gas after treatment in the adsorption tank was tested. The specific results are shown in Table 1.
[0030] Table 1 Test results
[0031] It can be seen from the above data that compared with the technical solutions of not using modified zeolite microspheres (Comparative Example 1), not using titanium dioxide sol (Comparative Example 2) and not using zeolite (Comparative Example 3), the new odorous gas adsorbent produced according to the present invention has significantly improved adsorption treatment effects on various odors and harmful gases.
[0032] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. A novel odorous gas adsorbent, characterized in that: The invention comprises the following raw material components in parts by weight: 30-40 parts of nano calcium hydroxide, 10-20 parts of modified zeolite microspheres, 10-20 parts of aluminum oxide, 20-40 parts of butyl titanate, 80-150 parts of anhydrous ethanol, 5-10 parts of nitric acid, and 5-10 parts of deionized water; The preparation method of the modified zeolite microspheres is to add a silane coupling agent and a zeolite to an ethanol solution in sequence, then stir and react at a temperature of 50 to 60° C. for 10 to 20 minutes, then add cellulose and continue to react for 30 to 60 minutes, then stand for 30 minutes and filter and dry to obtain the modified zeolite, wherein the mass ratio of the silane coupling agent, zeolite and cellulose is (0.1 to 0.5):10:(2 to 3), and the volume ratio of the ethanol solution and the mass ratio of the zeolite is (10 to 30) mL:1 g; add polyacrylic acid resin to deionized water under stirring conditions, heat to 60 to 80° C. and keep the temperature constant, then add the modified zeolite and continue to react for 3 to 5 hours, then naturally cool to room temperature, filter and dry to obtain the modified zeolite microspheres, and the mass ratio of the modified zeolite to the polyacrylic acid resin is 1:(5 to 10).
2. The novel foul gas adsorbent according to claim 1, characterized in that: The particle size of the nano calcium hydroxide is 10 to 30 nm.
3. The novel foul gas adsorbent according to claim 1, characterized in that: The ethanol solution is an ethanol solution with a mass fraction of 20% to 30%.
4. The novel foul gas adsorbent according to claim 1, characterized in that: The particle size of the zeolite is 80-100 μm.
5. The method for preparing the novel foul gas adsorbent according to any one of claims 1 to 4, characterized in that: The following steps are involved: (1) Weigh each raw material component in proportion, add anhydrous ethanol to butyl titanate under stirring at a speed of 50 to 100 r / min, then add nitric acid and deionized water to react for 2 to 3 hours, then slowly add alumina and continue stirring for 1 to 2 hours to obtain a colloidal solution; (2) Add modified zeolite microspheres to the colloidal solution obtained in step (1), then stir at a speed of 200 to 300 r / min for 10 to 15 minutes, then add nano calcium hydroxide and continue stirring for 15 to 30 minutes, and then freeze-dry to obtain a new type of foul gas adsorbent.
6. The preparation method according to claim 5, characterized in that: In step (1), anhydrous ethanol is added to butyl titanate under stirring conditions at a speed of 50 to 100 r / min, and then nitric acid and deionized water are added after heating to 40 to 50° C. to react for 2 to 3 hours.
7. The preparation method according to claim 5, characterized in that: In step (1), the addition time of alumina is controlled within 20 to 30 minutes.
8. The preparation method according to claim 5, characterized in that: In step (2), modified zeolite microspheres are added to the colloidal solution obtained in step (1), followed by treatment for 10 to 15 minutes under stirring at a speed of 200 to 300 r / min and ultrasound; the frequency of the ultrasound is 20 to 40 kHz.