Integrated circuit chip welding device based on capillary tube control

Through the integrated circuit chip welding device based on capillary control, the problems of poor welding effect and improper temperature control are solved, and efficient and accurate welding is achieved, which is suitable for the production needs of small and medium-sized enterprises and reduces costs and operation difficulties.

CN119016823AInactive Publication Date: 2024-11-26BAODING VICTORY TRAFFIC FACILITIES ENG CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411506258.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-28
Publication Date
2024-11-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing integrated circuit welding technology has problems such as poor welding effect, improper pin temperature control, and insufficient welding isolation function. Especially for small and medium-sized enterprises and laboratories, the lack of flexible and easy-to-operate automation equipment leads to low production efficiency and High cost.

Method used

Adopt an integrated circuit chip soldering device based on capillary control, including the brush table body, solder liquid chamber, hot air chamber, solder block and control handle, and the solder liquid and hot air are transported through the capillary to achieve precise welding and heating of the chip pins, and Keep the chip stable through auxiliary limit modules, and flow control is achieved using a limited current baffle and an ergonomic-designed kneading handle.

Benefits of technology

Improve welding quality and efficiency, reduce operational difficulty and cost, reduce dummy and multiple welding, ensure welding accuracy and repeatability, suit the production needs of small and medium-sized enterprises, and reduce the cost of expensive automation equipment. dependency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119016823A_ABST
    Figure CN119016823A_ABST
Patent Text Reader

Abstract

The invention provides an integrated circuit chip welding device based on capillary tube control, and aims to solve the problems of poor welding effect, improper pin temperature control, insufficient welding isolation function and the like in the prior art. The device comprises a brush table body, a plurality of capillary through pipes, a soldering tin liquid bin, a hot air bin and a control handle. The brushing table body is provided with a capillary tube, a soldering tin flow tube and a hot air through tube which are used for conveying soldering tin liquid and hot air respectively. The lower end pipe orifice of the hot air through pipe is an inclined surface, and can perform air blowing heating on the soldering tin flow pipe and the lower end pin at the same time, so that the pin is heated in advance, and the problem that the normal-temperature pin reduces the soldering tin temperature of drop welding is avoided. A flow limiting baffle is arranged at the pipe opening of the upper end of the soldering tin flow pipe to control flowing-out and stopping of soldering tin liquid, and control over the welding process is facilitated. Stable limiting of the chip in the welding process is achieved, and the welding quality and the stability of the chip are improved; meanwhile, the welding isolation function is achieved, and the short circuit phenomenon is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electronic welding, and in particular to an integrated circuit chip welding device based on capillary control. Background Art

[0002] In the modern electronic manufacturing industry, the welding technology of integrated circuits (ICs) is the key to achieving miniaturization, high performance and high reliability of electronic products. Although traditional welding methods such as manual soldering and wave soldering have met production needs to a certain extent, with the development of science and technology and the improvement of product quality requirements, the limitations of these technologies have gradually emerged.

[0003] For the existing manual soldering technology, the operator needs to manually use tweezers to fix the chip and drip solder on the pins on the outside of the chip. However, this method has obvious defects: First, due to the small contact range between the tweezers and the chip, and the difficulty in manual operation to ensure the stability of the chip limit, the chip is prone to displacement during the soldering process, thus affecting the accuracy and quality of the soldering. Secondly, the pins at room temperature will quickly absorb the heat of the solder and lower the temperature of the solder, which not only increases the risk of cold soldering, but may also require multiple soldering to achieve the desired effect, seriously affecting production efficiency. In addition, manual soldering is difficult to achieve multi-directional flexible positioning, which makes the positioning of the integrated circuit solder joints not accurate enough, further reducing the reliability of the product.

[0004] As a highly automated welding technology, wave soldering has improved production efficiency, but its problems cannot be ignored. During the wave soldering process, all components are in a high temperature state. This high temperature environment may have an adverse effect on sensitive electronic components, causing changes in their internal structure, which in turn affects performance and reliability. In addition, wave soldering cannot effectively solve the problem of welding isolation, which is prone to short circuits and increase the defective rate of products. At the same time, since wave soldering uses tin immersion, it is inconvenient to suck out the solder, which limits its application in the field of fine welding.

[0005] Especially for small and medium-sized enterprises and factories, as well as laboratory applications, these units usually lack comprehensive automation equipment and have high investment budgets. Laboratories usually conduct small-scale trials and development work, requiring flexible and easy-to-operate equipment. Therefore, they need a solution that can improve production efficiency without significantly increasing investment costs.

[0006] In summary, the existing integrated circuit welding technology faces many challenges. In order to overcome these challenges, improve welding quality and efficiency, reduce production costs, and extend the service life of electronic products, it is urgent to develop a new welding technology. The present application proposes an integrated circuit chip welding device based on capillary control. Through a manually operated control handle and an auxiliary limit module, precise control of the welding process is achieved, which reduces the operating difficulty and technical requirements, and is very suitable for the production needs of small and medium-sized enterprises. The modular design of the device allows it to be adjusted and replaced according to different experimental requirements, and its stable welding effect ensures the accuracy and repeatability of the experimental data. Summary of the invention

[0007] The purpose of the present invention is to provide an integrated circuit chip welding device based on capillary control to solve the problems existing in the prior art such as poor welding effect, improper pin temperature control, insufficient welding isolation function, etc.

[0008] An integrated circuit chip welding device based on capillary control, comprising: The brush table body, as the basic structure of the entire device, is used to support and fix various components; A solder liquid tank is arranged in the brush table body and is used to store solder liquid; A hot air chamber, arranged in the brush table body, for providing pressurized hot air; The welding assembly includes a solder flow pipe and a hot air duct, both of which are composed of a plurality of capillaries. The solder flow pipe is communicated with the solder liquid tank and is used to transport solder liquid to perform one-to-one welding on chip pins; the hot air duct is communicated with the hot air tank and is used to transport hot air to heat the lower end of the solder flow pipe and the chip pins. The control handle is used to drive the entire brush table body and control the flow of solder liquid in the solder liquid tank to achieve precise control of the welding process.

[0009] A further improvement is that the lower end of the hot air duct is slightly curved and the duct opening is an inclined surface, so that the solder flow tube and the lower end pin can be heated by air blowing at the same time.

[0010] A further improvement is that the relationship between the slope angle of the lower end of the hot air duct and the heating range of the solder flow tube is: ; Wherein, d is the horizontal distance between the solder flow pipe and the lower end of the hot air duct, and θ is the angle of the pipe opening bevel at the lower end of the hot air duct, that is, the angle between the bevel and the horizontal plane.

[0011] After determining the heating range of the solder flow tube, the relationship between the slope angle of the lower end of the hot air duct and the heating efficiency of the solder flow tube can be determined as follows:

[0012] Among them, Q h is the heat transfer power of the horizontal component of the hot air duct, h is the convection heat transfer coefficient of the hot air duct, R(θ) is the contact range between the solder flow tube and the hot air, T w is the temperature of the hot air blown out of the hot air duct, T solder is the solder temperature in the solder flow tube.

[0013] Similarly, the relationship between the bevel angle of the lower end of the hot air duct and the heating efficiency of the chip pins is:

[0014] Wherein, Q is the power of heat transfer, h is the convection heat transfer coefficient of the hot air duct, D is the diameter of the hot air duct, θ is the slope angle of the pipe opening at the lower end of the hot air duct, and L is the pipe opening length of the hot air duct; T s is the chip pin surface temperature, T ∞ The temperature of the solder flow tube is the ambient temperature. In the solution of the present application, a further improvement is that the upper end of the solder flow tube extends into the solder liquid tank, and a flow limiting baffle is arranged at the tube opening of the upper end of the solder flow tube, one end of the flow limiting baffle is fixed in the solder liquid tank, and the other end is controlled by a connecting rod arranged on the control handle. When the control handle is pinched, the connecting rod drives one end of the flow limiting baffle to be lifted upward, and the tube opening of the upper end of the solder flow tube is no longer blocked, and the solder liquid flows into the solder flow tube; when the chip pins are soldered, the control handle is released, and the connecting rod drives one end of the flow limiting baffle to cover the tube opening of the upper end of the solder flow tube downward, so that the tin liquid no longer flows out.

[0015] The brush table body is also provided with an auxiliary limiting module. When welding, the chip is first placed at the position where welding is required on the integrated circuit board, and then the circuit board and the chip are limited by the auxiliary limiting module to keep the chip in a stable state during the welding process.

[0016] A further improvement is that the auxiliary limiting module includes a first limiting module and a second limiting module, the first limiting module is used to limit the circuit board to be welded, and the second limiting module is used to limit the chip to be welded.

[0017] A further improvement is that the first limiting module and the second limiting module are both composed of a buffer rubber pad, a partition, a compression spring, and a guide column, wherein the partition, the compression spring, and the guide column are all arranged in the buffer rubber pad, the compression spring is sleeved on the guide column, the partition is fixed to the compression spring, and the buffer rubber pad directly acts on the circuit board and the chip, and is used to perform its own compression adjustment for chips or circuit boards of different heights, and to limit the chip or circuit board.

[0018] Beneficial effects of the present invention: 1. By setting up multiple capillary tubes and welding auxiliary components, the chip is stably limited during the welding process, which improves the welding quality and chip stability.

[0019] 2. The design of the hot air duct allows the pins to be heated in advance, avoiding the problem of the normal temperature pins lowering the solder temperature of the drip soldering, and reducing the situation of cold soldering and multiple soldering. The lower end of the hot air duct is designed with a micro-arc surface, which is tilted downward to increase the contact area between the hot air and the solder flow tube, and improve the heating efficiency, thereby reducing energy consumption and costs, and improving the overall production efficiency and product quality level.

[0020] 3. A flow-limiting baffle is set on the solder flow tube and its opening and closing is controlled by pinching the control handle, so as to achieve precise control of the solder liquid flow to meet the personalized needs and usage scenario requirements of different users. Among them, the flow-limiting baffle is made of elastic material with good sealing performance and wear resistance; the pinching handle adopts ergonomic design and is easy to operate, thereby reducing labor intensity, improving work efficiency, and meeting the needs of large-scale production and application requirements.

[0021] 4. The welding device provided by the present application can reduce the reliance on expensive automated equipment, and small and medium-sized enterprises can reduce initial investment and operating costs. In addition, the design of the device improves welding efficiency and quality, reduces material waste and time loss caused by false welding or multiple welding, and further reduces production costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0023] Figure 1 : A three-dimensional schematic diagram of a welding device provided by the present invention; Figure 2 : A cross-sectional view of the welding device provided by the present invention Figure 1 ; Figure 3 : A cross-sectional view of the welding device provided by the present invention Figure 2 ; Figure 4 : A cross-sectional view of the welding device provided by the present invention Figure 3 ; Figure 5 : A cross-sectional view of the welding device provided by the present invention Figure 4 ; Figure 6 : A schematic cross-sectional view of an auxiliary limiting module of a welding device provided by the present invention; 1. Brush station body; 2. Solder liquid tank; 21. Tin inlet; 22. Tin inlet tube; 23. Electric heating wire; 3. Hot air tank; 31. Air inlet; 32. Air inlet tube 41. Solder flow tube; 42. Hot air duct; 5. Control handle; 51. Connecting rod; 52. Current limiting baffle; 61. First limit module; 62. Second limit module; 611. Buffer rubber pad; 612. Guide column; 613. Partition; 614. Compression spring. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0025] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, the present application is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0026] like Figure 1-5 As shown, the present application designs a capillary-controlled integrated circuit chip welding device, comprising: a brush station body 1, a solder liquid tank 2 and a hot air tank 3 arranged in the brush station body 1, a welding block, a control handle 5, etc.; wherein the brush station body 1, as the basic structure of the entire device, is used to support and fix each component; the solder liquid tank 2 is used to store solder liquid, and is connected to the solder flow pipe 41 to realize the function of automatically replenishing solder liquid, thereby reducing manual operation costs and time waste and improving overall production efficiency. The hot air tank 3 is used to provide pressurized hot air; the welding block includes a solder flow pipe 41 and a hot air duct 42, and the solder flow pipe 41 and the hot air duct 42 are both composed of multiple capillaries, and the solder flow pipe 41 is connected to the solder liquid tank 2, and is used to transport solder liquid to perform one-to-one welding on chip pins; the hot air duct 42 is connected to the hot air tank 3, and is used to transport hot air to heat the lower end of the solder flow pipe 41 and the chip pins.

[0027] like Figure 4 As shown, at the same time, a tin inlet tube 22 and an electric heating wire 23 are arranged in the brush table body 1; the solder liquid in the external solder melting device flows into the tin inlet tube 22 through the tin inlet port 21 arranged on the brush table body 1, and the solder liquid flows into the solder liquid tank 2 through the tin inlet tube 22. During this process, the electric heating wire 23 is continuously heated to ensure that the solder liquid will not condense. Among them, the electric heating wire 23 arranged at the solder liquid tank 2 is used to heat the solder in the solder liquid tank 2, ensuring that the tin can be melted in 8 seconds, so that the solder in the solder liquid tank 2 is in a fluid state.

[0028] like Figure 5 As shown, an air inlet pipe 32 is also provided in the brush table body 1, and the hot air from the external hot air device is introduced into the air inlet pipe 32 through the air inlet 31 provided on the brush table body 1, and the hot air enters the hot air bin 3, and then enters the hot air duct 42 from the hot air bin 3.

[0029] In the technical solution provided in this application, if Figure 2 As shown, the upper end of the solder flow tube 41 extends into the solder liquid tank 2, and a flow limiting baffle 52 is provided at the tube opening of the upper end of the solder flow tube 41. One end of the flow limiting baffle 52 is fixed in the solder liquid tank 2, and the other end is controlled by a connecting rod 51 provided on the control handle 5. When the control handle 5 is pinched, the connecting rod 51 drives one end of the flow limiting baffle 52 to be lifted upward. At this time, the tube opening of the upper end of the solder flow tube 41 is no longer blocked, and the solder liquid flows into the solder flow tube 41; Figure 3 As shown, when the chip pins are soldered, the control handle 5 is released, and the connecting rod 51 drives one end of the current limiting baffle 52 downward to cover the tube opening of the upper end of the solder flow tube 41, so that the tin liquid no longer flows out.

[0030] The brush table body 1 is also provided with an auxiliary limiting module. When welding, the chip is first placed at the position where welding is required on the integrated circuit board, and then the circuit board and the chip are limited by the auxiliary limiting module to keep the chip in a stable state during the welding process.

[0031] The auxiliary limiting module includes a first limiting module 61 and a second limiting module 62. The first limiting module 61 is used to limit the circuit board to be welded, and the second limiting module 62 is used to limit the chip to be welded.

[0032] like Figure 6As shown, the first limiting module 61 and the second limiting module 62 are both composed of a buffer rubber pad 611, a partition 613, a compression spring 614, and a guide column 612, wherein the partition 613, the compression spring 614, and the guide column 612 are all arranged in the buffer rubber pad 611, the compression spring 614 is sleeved on the guide column 612, the partition 613 is fixed to the compression spring 614, and the buffer rubber pad 611 directly acts on the circuit board and the chip, and is used to adjust its own compression for chips or circuit boards of different heights, and to limit the chip or circuit board. If the chip thickness is large, the buffer rubber pad 611 is compressed, and at the same time, the partition 613 is driven to squeeze the compression spring 614 to perform vertical compression along the direction of the guide column 612, so that it can be applied to chips of different thicknesses.

[0033] In the technical solution of the present application, it is particularly important to explain that the lower end of the hot air duct 42 is slightly curved and the duct opening is an inclined surface, so that the solder flow tube 41 and the lower end pin can be heated by air blowing at the same time.

[0034] The relationship between the slope angle of the lower end of the hot air duct 42 and the heating range of the solder flow tube 41 is: (1)

[0035] In formula (1), d is the horizontal distance between the solder flow pipe 41 and the lower end of the hot air duct 42, and θ is the angle of the pipe opening bevel at the lower end of the hot air duct 42, that is, the angle between the bevel and the horizontal plane.

[0036] The relationship between the slope angle of the lower end of the hot air duct 42 and the heating efficiency of the solder flow tube 41 is: (2)

[0037] In formula (2), Q h is the heat transfer power of the horizontal component of the hot air duct 42, h is the convection heat transfer coefficient of the hot air duct 42, R(θ) is the range of contact between the solder flow tube 41 and the hot air, T w is the temperature of the hot air blown out by the hot air duct 42, T solder is the solder temperature in the solder flow tube 41 .

[0038] The relationship between the bevel angle of the lower end of the hot air duct 42 and the heating efficiency of the chip pins is: (3)

[0039] In formula (3), Q is the power of heat transfer, h is the convection heat transfer coefficient of the hot air duct 42, D is the diameter of the hot air duct 42, θ is the slope angle of the pipe opening at the lower end of the hot air duct 42, and L is the pipe opening length of the hot air duct 42; T s is the chip pin surface temperature, T ∞ is the ambient temperature.

[0040] The convective heat transfer coefficient h is related to the airflow velocity and flow state. Changes in the angle of the slope will affect the speed and direction of the airflow, thereby affecting the convective heat transfer coefficient h. In most cases, the convective heat transfer coefficient can be estimated by the following empirical formula: (4)

[0041] In formula (4), Re is the Reynolds number, which reflects the flow state; Pr is the Prandtl number, which represents the ratio of momentum diffusion to heat diffusion of the fluid; C, n, and m are empirical constants related to the flow conditions.

[0042] (5)

[0043] In formula (5), is the gas density, v is the air velocity, L is the length of the hot air duct 42, is the gas viscosity.

[0044] In the technical solution of the present application, the bevel angle of the lower end of the hot air duct 42 is a key parameter because it directly affects the heating efficiency of the hot air on the solder flow tube 41 and the chip pins. The following are several specific embodiments to illustrate how to adjust this angle according to different needs: Example 1: Improving heating efficiency Assume that we are dealing with a scenario that requires rapid heating, such as soldering a larger chip or soldering in a low temperature environment. In order to maximize the heat transfer efficiency, we can increase the bevel angle of the lower end of the hot air duct 42. For example, according to formula (3), we set the bevel angle θ to 60 degrees, which will increase the contact area between the hot air and the chip pin surface, thereby increasing the heat transfer power Q and achieving faster heating speed.

[0045] Example 2: Uniform heating In some applications, it may be necessary to uniformly heat a plurality of small and densely arranged pins. In this case, we may wish to reduce the bevel angle of the lower end of the hot air duct 42 to reduce the direct impact of the hot air, thereby obtaining a more uniform temperature distribution. For example, setting the bevel angle θ to 30 degrees can reduce local overheating caused by direct impact of the airflow, thereby ensuring that all pins are evenly heated.

[0046] Example 3: Optimizing energy consumption and protecting components For sensitive electronic components, excessively high temperatures may cause damage. In this case, we need to carefully control the heating process to avoid overheating. According to formulas (2) and (3), by adjusting the bevel angle θ of the lower end of the hot air duct 42 to a medium value, such as 45 degrees, it is possible to ensure sufficient heating efficiency while avoiding thermal damage to sensitive components. In addition, this setting can also help us optimize energy consumption while maintaining welding quality.

[0047] Example 4: Adapting to different welding environments In different production environments, such as high humidity or variable temperature conditions, the welding process may need to be adjusted accordingly. By experimentally determining the optimal bevel angle in a specific environment, the stability and reliability of the welding process can be ensured. For example, in a high humidity environment, in order to quickly replace the moisture around the pin, according to formulas (2) and (3), it is necessary to temporarily increase the bevel angle θ to 50 degrees to improve the replacement efficiency of hot air.

[0048] It can be seen from the above embodiments that, for different welding requirements and environmental conditions, flexibly adjusting the bevel angle of the lower end of the hot air duct 42 is the key to achieving efficient and stable welding. Each setting needs to be optimized according to the actual welding effect to ensure the best welding quality and production efficiency.

[0049] It is worth noting that the welding block can be replaced according to the specifications of the chip. In the embodiment of the present application, welding blocks of multiple specifications can be set. In the embodiment of the present application, the specifications of the welding block are set according to the chip pin spacing specifications. Here, welding blocks of 0.5mm specifications, welding blocks of 0.65mm specifications, welding blocks of 0.8mm specifications, and welding blocks of 1.0mm specifications are respectively applied. Among them, 0.5mm, 0.65mm, 0.8mm, and 1.0mm are all the intervals between the solder flow tubes 41 composed of capillaries in the welding block.

[0050] Ten integrated circuit chips were welded under the following packaging processes, and the results are shown in the following table:

[0051] It can be seen from these experimental data that the capillary-controlled integrated circuit chip welding device provided by the present invention can achieve high-quality welding effects under different packaging processes without cold solder joints and pin adhesion. This fully demonstrates the significant advantages of the device in improving production efficiency, energy saving and environmental protection, and meeting large-scale production needs.

[0052] In the welding device provided by the present application, the solder flow pipe and the hot air duct work together during the welding process. The heat provided by the hot air duct allows the solder to melt quickly, while the solder flow pipe releases the solder at the right time to ensure that the solder flows accurately to the pins to achieve high-quality welding. This design not only improves the automation level of welding, but also effectively reduces human errors in the welding process and improves overall production efficiency.

[0053] It is worth noting that the above-described embodiments are only descriptions of the preferred modes of the present application, and are not intended to limit the scope of the present application. Without departing from the design spirit of the present application, various modifications and improvements made by ordinary technicians in the field to the technical solutions of the present application should fall within the scope of protection determined by the claims of the present application. It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variant thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such a process, method, article or device.

Claims

1. An integrated circuit chip welding device based on capillary control, characterized in that: include: The brush table body, as the basic structure of the entire device, is used to support and fix various components; A solder liquid tank is arranged in the brush table body and is used to store solder liquid; A hot air chamber, arranged in the brush table body, for providing pressurized hot air; The welding assembly includes a solder flow pipe and a hot air duct, both of which are composed of a plurality of capillaries. The solder flow pipe is communicated with the solder liquid tank and is used to transport solder liquid to perform one-to-one welding on chip pins; the hot air duct is communicated with the hot air tank and is used to transport hot air to heat the lower end of the solder flow pipe and the chip pins. The control handle is used to drive the entire brush table body and control the flow of solder liquid in the solder liquid tank to achieve precise control of the welding process.

2. The capillary-controlled integrated circuit chip bonding device according to claim 1, characterized in that: The lower end of the hot air duct is slightly curved, and the duct opening is an inclined surface, so that the solder flow tube and the lower end pin can be heated by air blowing at the same time.

3. The capillary-controlled integrated circuit chip bonding device according to claim 2, characterized in that: The relationship between the slope angle of the lower end of the hot air duct and the heating range of the solder flow tube is: R(θ)=d+d / cos(θ); Wherein, d is the horizontal distance between the solder flow pipe and the lower end of the hot air duct, and θ is the angle of the pipe opening bevel at the lower end of the hot air duct, that is, the angle between the bevel and the horizontal plane.

4. The capillary-controlled integrated circuit chip bonding device according to claim 3, characterized in that: The relationship between the slope angle of the lower end of the hot air duct and the heating efficiency of the solder flow tube is: Q h =h h * R(θ)*(T w - T solder ) Among them, Q h is the heat transfer power of the horizontal component of the hot air duct, h h is the heat transfer coefficient of the hot air duct in the horizontal direction, R(θ) is the contact range between the solder flow tube and the hot air, T w is the temperature of the hot air blown out of the hot air duct, T solder is the solder temperature in the solder flow tube.

5. The capillary-controlled integrated circuit chip bonding device according to claim 3, characterized in that: The relationship between the bevel angle of the lower end of the hot air duct and the heating efficiency of the chip pins is: Q=h * (π*D*L*sin(θ)) * (T s - T ∞ ) Wherein, Q is the power of heat transfer, h is the convective heat transfer coefficient, D is the diameter of the hot air duct, θ is the slope angle of the pipe opening at the lower end of the hot air duct, and L is the pipe opening length of the hot air duct; T s is the chip pin surface temperature, T ∞ is the ambient temperature.

6. The capillary-controlled integrated circuit chip bonding device according to claim 1, characterized in that: The upper end of the solder flow tube extends into the solder liquid bin, and a flow limiting baffle is arranged at the pipe opening of the upper end of the solder flow tube, one end of the flow limiting baffle is fixed in the solder liquid bin, and the other end is controlled by a connecting rod arranged on the control handle. When the control handle is pinched, the connecting rod drives one end of the flow limiting baffle to be lifted upward, and at this time, the pipe opening of the upper end of the solder flow tube is no longer blocked, and the solder liquid flows into the solder flow tube; when the chip pins are soldered, the control handle is released, and the connecting rod drives one end of the flow limiting baffle to cover the pipe opening of the upper end of the solder flow tube downward, so that the tin liquid no longer flows out.

7. The capillary-controlled integrated circuit chip bonding device according to claim 1, characterized in that: The brush table body is also provided with an auxiliary limiting module. When welding, the chip is first placed at the position where welding is required on the integrated circuit board, and then the circuit board and the chip are limited by the auxiliary limiting module to keep the chip in a stable state during the welding process.

8. The capillary-controlled integrated circuit chip bonding device according to claim 7, characterized in that: The auxiliary limiting module includes a first limiting module and a second limiting module, wherein the first limiting module is used to limit the circuit board to be welded, and the second limiting module is used to limit the chip to be welded.

9. The capillary-controlled integrated circuit chip bonding device according to claim 8, characterized in that: The first limiting module and the second limiting module are both composed of a buffer rubber pad, a partition, a compression spring, and a guide column, wherein the partition, the compression spring, and the guide column are all arranged in the buffer rubber pad, the compression spring is sleeved on the guide column, the partition is fixed to the compression spring, and the buffer rubber pad directly acts on the circuit board and the chip, and is used to perform its own compression adjustment for chips or circuit boards of different heights, and to limit the chip or circuit board.

Citation Information

Patent Citations

  • Press type automatic tin supply electric soldering iron

    CN104526101A

  • Rapid welding device for integrated circuit on circuit board

    CN117862623A

  • Automatic welder of circuit board welding machine

    CN205032825U

  • Efficient convenient and easy electric soldering iron capable of achieving solder-wire-free welding

    CN217701719U

  • Circuit board welding clamp for charging pile production

    CN221363434U