Wind power blade mold and wind power blade manufacturing method
By embedding sensing components and transmission components in the wind power blade mold, the strain value during the mold closing process is monitored in real time, and the problem of difficult to identify small gap mold bearing in the prior art is solved, and the monitoring efficiency and reliability of wind power blade manufacturing is improved.
Patent Information
- Application Number
- CN202411137573.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-11-26
AI Technical Summary
During the manufacturing process of wind power blades, it is difficult for the prior art to effectively identify and monitor assembly gaps below 0.5mm, resulting in a reduction in smoothness of the bonding process and a large amount of manual and resources are required to conduct tests one by one to eliminate the risk of bearing the mold.
Design a wind power blade mold, including a mold body and a monitoring mechanism, the sensing component is embedded in the first mold layer of the mold body, and the strain is detected through the fiber grating sensor and the temperature compensation sensor. The transmission component transmits data through the fiber cable and wireless communication, in real time Monitor the strain value during the mold clamping process and determine the strain critical value to judge the mold bearing phenomenon.
It improves the mold-carrying monitoring efficiency and reliability when closing the wind power blades, reduces manual verification time, enhances detection accuracy, and ensures the smoothness of the bonding process.
Smart Images

Figure CN119017604A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of wind turbine blade manufacturing, and in particular to a wind turbine blade mold and a wind turbine blade manufacturing method. Background Art
[0002] Wind turbine blades are an important part of wind turbine generator sets. After the introduction of new composite materials into the design and manufacturing of wind turbine blades, the manufacturing process of wind turbine blades has also undergone major changes. On the manufactured mold, a series of parts such as the main beam and skin of the blade are formed, which is the first link in the entire blade manufacturing. After the manufacture of various parts is completed, the parts need to be assembled, and finally the mold is closed and solidified to form a wind turbine blade. Before the formal gluing and mold closing, it is often necessary to perform trial assembly and other operation steps on the web and skin to verify whether the bonding gap is qualified. Trial mold assembly often uses solid glue, which is placed in points or strips in the length and width directions. This inspection method can often only identify larger gaps. For assembly gaps of extreme thickness, such as assembly gaps below 0.5mm, it often cannot play an identification role. For example, mold lifting below 0.5mm occurs in two places, but it is impossible to identify and analyze which mold lifting risk is more serious. It can only be eliminated and verified by testing one by one, which is often time-consuming and labor-intensive, resulting in a reduction in the smoothness of the bonding process and a large amount of manpower and resources. Summary of the invention
[0003] The embodiments of the present application provide a wind turbine blade mold and a method for manufacturing a wind turbine blade, which can improve the efficiency and reliability of mold monitoring when the wind turbine blade is molded.
[0004] In the first aspect, an embodiment of the present application provides a wind turbine blade mold, comprising: a mold body, comprising a main beam bonding area and an auxiliary beam bonding area, the main beam bonding area and the auxiliary beam bonding area extend along a first direction and are arranged along a second direction; the mold body also includes a first mold layer; a monitoring mechanism, comprising a sensor component and a transmission component; a plurality of sensor components are provided, and a plurality of sensor components are arranged in the first mold layer and are located in the main beam bonding area and the auxiliary beam bonding area; the transmission component is communicatively connected to the sensor component.
[0005] According to an embodiment of the first aspect of the present application, in the bonding area of the main beam, a plurality of sensor components are arranged in an array along a first direction and a second direction, a distance between two adjacent sensor components along the first direction is a first distance, a distance between two adjacent sensor components along the second direction is a second distance, and the second distance is smaller than the first distance; in the bonding area of the auxiliary beam, a plurality of sensor components are arranged in an array along the first direction and the second direction, a distance between two adjacent sensor components along the first direction is a third distance, a distance between two adjacent sensor components along the second direction is a fourth distance, and the fourth distance is smaller than the third distance.
[0006] According to an embodiment of the first aspect of the present application, the first distance is equal to the third distance, and the second distance is equal to the fourth distance.
[0007] According to an embodiment of the first aspect of the present application, the sensing component includes a fiber grating sensor, and the fiber grating sensor includes a strain sensor and a temperature compensation sensor; the strain sensor is flexibly packaged, the temperature compensation sensor is metal packaged, and the strain sensor and the temperature compensation sensor are connected.
[0008] According to an embodiment of the first aspect of the present application, the transmission component includes an optical fiber cable, an adjustment unit, a remote transmission unit and a monitoring and management unit; the adjustment unit is electrically connected to the sensing component through an optical fiber cable; the remote transmission unit is electrically connected to the adjustment unit; the remote transmission unit is wirelessly connected to the monitoring and management unit, and / or the remote transmission unit is wiredly connected to the monitoring and management unit.
[0009] According to an embodiment of the first aspect of the present application, the adjusting portion and the remote transmission portion are arranged at one end of the mold body along the first direction.
[0010] According to an embodiment of the first aspect of the present application, the mold body also includes a first side and a second side relative to each other, and also includes a second mold layer, a third mold layer and a fourth mold layer. Along the direction from the second side to the first side, the first mold layer, the second mold layer, the third mold layer and the fourth mold layer are stacked in sequence.
[0011] According to an embodiment of the first aspect of the present application, the distance from the sensor component to the first side is greater than or equal to the first reference distance and less than or equal to the second reference distance.
[0012] In the second aspect, an embodiment of the present application provides a method for manufacturing a wind turbine blade, comprising: pouring a first mold layer to form a mold body; determining a main beam bonding area and an auxiliary beam bonding area, the main beam bonding area and the auxiliary beam bonding area extending along a first direction and arranged along a second direction; pouring a sensor component into the first mold layer; connecting the transmission component to the sensor component to form a monitoring mechanism, and obtaining a wind turbine blade mold; loading the wind turbine blade material into the wind turbine blade mold; applying glue and closing the mold, while the monitoring mechanism detects the strain of the wind turbine blade material through the sensor component and obtains a strain monitoring value. If the strain monitoring value is always less than the strain critical value, no mold lifting occurs during the closing process, and a wind turbine blade can be obtained.
[0013] According to an embodiment of the second aspect of the present application, a method for obtaining a critical strain value includes: obtaining strain monitoring values of all sensor components when mold release occurs during the mold closing process; obtaining a strain load equation based on all strain monitoring values and the weight of the wind turbine blade material; and obtaining the critical strain value when mold release occurs during the mold closing process based on the strain load equation.
[0014] In the wind turbine blade mold and the wind turbine blade manufacturing method provided in the embodiment of the present application, the mold body is used to manufacture wind turbine blades, and the wind turbine blades can be formed. The main beam bonding area corresponds to the main beam of the wind turbine blade, and the auxiliary beam bonding area corresponds to the auxiliary beam of the wind turbine blade. The sensor component of the monitoring mechanism is arranged in the first mold layer of the mold body, and is located in the main beam bonding area and the auxiliary beam bonding area. When manufacturing the wind turbine blade mold of the embodiment of the present application, the sensor component is embedded in the first mold layer, so that the sensor component is fixed at the corresponding position in the mold body, so that in the mold monitoring of the wind turbine blade mold closing process, the detection of the sensor component is more accurate and reliable, and the monitoring efficiency is improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments of the present application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0016] Figure 1 A schematic diagram of the structure of a wind turbine blade mold according to an embodiment of the present application.
[0017] Figure 2 A schematic diagram of the structure of a monitoring mechanism for a wind turbine blade mold according to an embodiment of the present application.
[0018] Figure 3 This is a plan view of a wind turbine blade mold according to an embodiment of the present application.
[0019] Figure 4 Another structural schematic diagram of the monitoring mechanism of the wind turbine blade mold according to an embodiment of the present application.
[0020] Figure 5 A schematic diagram of a process of manufacturing a wind turbine blade according to an embodiment of the present application.
[0021] Reference numerals:
[0022] 1. Mold body; 11. Main beam bonding area; 12. Auxiliary beam bonding area; 13. First mold layer; 14. Second mold layer; 15. Third mold layer; 16. Fourth mold layer;
[0023] 2. Monitoring mechanism; 21. Sensing component; 22. Transmission component; 221. Optical fiber cable; 222. Adjustment unit; 223. Remote transmission unit; 224. Monitoring management unit;
[0024] X, first direction; Y, second direction. DETAILED DESCRIPTION
[0025] The features and exemplary embodiments of various aspects of the application will be described in detail below. In the detailed description below, many specific details are proposed to provide a comprehensive understanding of the application. However, it is obvious to those skilled in the art that the application can be implemented when some details in these specific details are not needed. The following description of the embodiments is only to provide a better understanding of the application by illustrating the example of the application.
[0026] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The embodiments will be described in detail below in conjunction with the accompanying drawings.
[0027] Relational terms such as first and second, etc., are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "comprises," "comprising," or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article, or device that includes a series of elements includes not only those elements, but also other elements that are not explicitly listed, or also includes elements that are inherent to such process, method, article, or device. In the absence of further restrictions, the elements defined by the statement "comprising ..." do not exclude the presence of additional identical elements in the process, method, article, or device that includes the elements.
[0028] It should be understood that when describing the structure of a component, when a layer or a region is referred to as being "on" or "over" another layer or another region, it may mean that it is directly on the other layer or another region, or that other layers or regions are included between it and the other layer or another region. Moreover, if the component is turned over, the layer or a region will be "below" or "beneath" another layer or another region.
[0029] In addition, the term "and / or" in this article is only a description of the association relationship between the associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0030] It should be understood that in the embodiment of the present application, "B corresponding to A" means that B is associated with A, and B can be determined according to A. However, it should also be understood that determining B according to A does not mean determining B only according to A, and B can also be determined according to A and / or other information.
[0031] The applicant discovered that when making a wind turbine blade, part of the material of the wind turbine blade will be placed in a wind turbine blade mold, so that the two halves of the wind turbine blade (skin shell or web) are formed separately, and then the two halves of the wind turbine blade are molded together with the mold to solidify to form the whole of the wind turbine blade. In the process of mold closing, there may be mold lifting, that is, half of the wind turbine blade material contacts and squeezes the other half of the mold, making it difficult for the two halves of the mold to be tightly connected together, causing strain or even damage to the material of the wind turbine blade. In order to detect whether there is mold lifting, clay is usually used to simulate the wind turbine blade material, and then the mold closing process is simulated to determine the size of the wind turbine blade material when no mold lifting occurs. However, it is necessary to simulate the mold closing multiple times to determine the reasonable size of the wind turbine blade material. In addition, if there are multiple mold lifting phenomena during the simulation process, it is not possible to determine which one or which parts can be adjusted to avoid mold lifting, and it is necessary to test them one by one, which will also reduce the detection efficiency.
[0032] In view of the above analysis, the applicant has proposed a wind turbine blade mold and a method for manufacturing a wind turbine blade. The wind turbine blade mold includes a mold body and a monitoring mechanism. The mold body is used to manufacture wind turbine blades and can shape the wind turbine blades. The main beam bonding area corresponds to the main beam of the wind turbine blade, and the auxiliary beam bonding area corresponds to the auxiliary beam of the wind turbine blade. The sensor component of the monitoring mechanism is arranged in the first mold layer of the mold body and is located in the main beam bonding area and the auxiliary beam bonding area. When manufacturing the wind turbine blade mold of the embodiment of the present application, the sensor component is embedded in the first mold layer, thereby fixing the sensor component at the corresponding position in the mold body. In the mold monitoring of the wind turbine blade mold closing process, the detection of the sensor component is more accurate and reliable, thereby improving the monitoring efficiency.
[0033] Figure 1 A schematic diagram of the structure of a wind turbine blade mold according to an embodiment of the present application. Figure 2 A schematic diagram of the structure of a monitoring mechanism for a wind turbine blade mold according to an embodiment of the present application.
[0034] See also Figure 1 and Figure 2 The embodiment of the present application provides a wind turbine blade mold, including: a mold body 1, including a main beam bonding area and an auxiliary beam bonding area, the main beam bonding area and the auxiliary beam bonding area extend along a first direction X and are arranged along a second direction Y; the mold body 1 also includes a first mold layer 13; a monitoring mechanism 2, including a sensor component 21 and a transmission component 22; a plurality of sensor components 21 are provided, and a plurality of sensor components 21 are arranged in the first mold layer 13, and are located in the main beam bonding area and the auxiliary beam bonding area; the transmission component 22 is communicatively connected with the sensor component 21.
[0035] The wind turbine blade mold of the embodiment of the present application can form half of the wind turbine blade, and the other half of the wind turbine blade can be formed using the wind turbine blade mold of the embodiment of the present application, or other common wind turbine blade molds. It can be understood that the windward surface and the covered surface of the wind turbine blade correspond to the two halves of the wind turbine blade respectively, and in addition, the first direction X corresponds to the axial direction of the wind turbine blade, and the second direction Y corresponds to the chord direction of the wind turbine blade.
[0036] The mold body 1 can hold the wind turbine blade material and is used to form half of the wind turbine blade. The main beam bonding area is used to bond and fix the main beam of the wind turbine blade, and the auxiliary beam bonding area is used to bond and fix the auxiliary beam of the wind turbine blade. Considering the shapes of the main beam and the auxiliary beam, the main beam bonding area and the auxiliary beam bonding area extend along the first direction X and are arranged along the second direction Y.
[0037] The monitoring mechanism 2 is used to monitor whether mold lifting occurs during the mold closing process. The sensor component 21 of the monitoring mechanism 2 can detect the strain of the mold body 1, and the transmission component 22 is communicatively connected to the sensor component 21. The strain signal detected by the sensor component 21 can be transmitted through the transmission component 22 for easy display and viewing. The transmission component 22 can transmit signals wirelessly or by wire. Considering that the mold lifting phenomenon mainly occurs at the main beam and the auxiliary beam, the sensor component 21 is located in the bonding area of the main beam and the bonding area of the auxiliary beam, and it can be determined whether mold lifting occurs by detecting the size of the strain. It can be understood that the sensor component 21 may or may not be set in the area outside the bonding area of the main beam and the bonding area of the auxiliary beam.
[0038] The sensor component 21 is arranged in the first mold layer 13 of the mold body 1. When the first mold layer 13 of the mold body 1 is manufactured, the sensor component 21 can be embedded in the first mold layer 13. Since the sensor component 21 is embedded in the first mold layer 13, during the mold closing process, the relative position of the sensor component 21 and the mold body 1 can always remain unchanged, so that the strain detected by the sensor component 21 can truly reflect the strain size at the corresponding position of the mold body 1, so as to reliably judge whether the mold lifting phenomenon occurs. In addition, since the relative position of the sensor component 21 and the mold body 1 can always remain unchanged, under the premise of determining the material weight (load), the strain of each position of the mold body 1 can be obtained, and then the relationship between the load and the strain of the mold body 1 (strain load equation) can be obtained, and the strain value when the mold lifting is critical during the mold closing process can be determined, and based on this, the strain value monitored by the sensor component 21 during the mold closing process is monitored to determine whether the monitored strain value exceeds the strain critical value, and then determine whether the mold lifting is enough to occur. In addition, since the sensor component 21 is disposed in the first mold layer 13 of the mold body 1 , the mold body 1 can also play a certain protective role on the sensor component 21 .
[0039] Figure 3 This is a plan view of a wind turbine blade mold according to an embodiment of the present application.
[0040] For further information, see Figure 3 , and combined with Figure 1 and Figure 2 In the bonding area of the main beam, a plurality of sensor components 21 are arranged in an array along the first direction X and the second direction Y, a distance between two adjacent sensor components 21 along the first direction X is a first distance, a distance between two adjacent sensor components 21 along the second direction Y is a second distance, and the second distance is smaller than the first distance; in the bonding area of the auxiliary beam, a plurality of sensor components 21 are arranged in an array along the first direction X and the second direction Y, a distance between two adjacent sensor components 21 along the first direction X is a third distance, a distance between two adjacent sensor components 21 along the second direction Y is a fourth distance, and the fourth distance is smaller than the third distance.
[0041] In the main beam bonding area 11, multiple sensor components 21 are arranged in an array along the first direction X and the second direction Y. The multiple sensor components 21 can detect the strain magnitude of each position in the main beam bonding area 11, thereby more accurately reflecting the overall strain change in the main beam bonding area 11. Considering that the bending degree of the wind turbine blade along the second direction Y (chord direction) is greater than the bending degree of the first direction X, the strain change along the second direction Y is more obvious, so the second distance is made smaller than the first distance, so that the strain change in the second direction Y can be detected more accurately.
[0042] Similarly, in the auxiliary beam bonding area 12, multiple sensor components 21 are arranged in an array along the first direction X and the second direction Y. The multiple sensor components 21 can detect the strain magnitude of each position in the auxiliary beam bonding area 12, thereby more accurately reflecting the overall strain change in the auxiliary beam bonding area 12. Considering that the bending degree of the wind turbine blade along the second direction Y (chord direction) is greater than the bending degree of the first direction X, the strain change along the second direction Y is more obvious, so the fourth distance is made smaller than the third distance, so that the strain change in the second direction Y can be detected more accurately.
[0043] Further, see Figures 1 to 3 , the first distance is equal to the third distance, and the second distance is equal to the fourth distance. Along the first direction X and the second direction Y, the strain change trends of the main beam bonding area 11 and the auxiliary beam bonding area 12 are close, so the first distance is equal to the third distance, and the second distance is equal to the fourth distance, so that the strain detection accuracy of the main beam bonding area 11 and the auxiliary beam bonding area 12 is consistent. When mold lifting occurs, the strain size of the detected main beam bonding area 11 and the auxiliary beam bonding area 12 is smaller when obtaining the relationship between the load and the strain of the mold body 1, and it is more accurate and reliable to monitor whether mold lifting occurs during mold closing. Exemplarily, the first distance and the third distance can be 100mm, and the second distance and the fourth distance can be 50mm.
[0044] Furthermore, the sensing component 21 includes a fiber grating sensor, and the fiber grating sensor includes a strain sensor and a temperature compensation sensor; the strain sensor is flexibly packaged, the temperature compensation sensor is metal packaged, and the strain sensor and the temperature compensation sensor are connected.
[0045] In the embodiment of the present application, the sensing component 21 can use a fiber grating sensor to detect the strain of the mold body 1. The fiber grating sensor can include a strain sensor and a temperature compensation sensor. The strain sensor adopts a flexible package to form a flexible sensor, and the temperature compensation sensor adopts a metal package to form a temperature sensor. Exemplarily, the size of the strain sensor is (20×5×1) mm, the linearity is 1%, the repeatability is 1%, the operating temperature is (-55~95)℃, the temperature measurement range is ±3000με, and the wavelength range is (1525~1565) nm. The size of the temperature compensation sensor is (32×11×1) mm, the linearity is 1%, the repeatability is 1%, the operating temperature is (-55~150)℃, the temperature measurement range is (-55~150)℃, and the wavelength range is (1525~1565) nm.
[0046] Figure 4 Another structural schematic diagram of the monitoring mechanism of the wind turbine blade mold according to an embodiment of the present application.
[0047] For further information, see Figure 4 The transmission component 22 includes an optical fiber cable 221, an adjustment unit 222, a remote transmission unit 223 and a monitoring management unit 224; the adjustment unit 222 is electrically connected to the sensor component 21 through the optical fiber cable 221; the remote transmission unit 223 is electrically connected to the adjustment unit 222; the remote transmission unit 223 is wirelessly connected to the monitoring management unit 224, and / or the remote transmission unit 223 is wiredly connected to the monitoring management unit 224.
[0048] The transmission component 22 is used to transmit the strain signal detected by the sensing component 21. The optical fiber cable 221 can be arranged on the first mold layer 13 together with the sensing component 21, and transmit the strain signal detected by the sensing component 21 to the adjustment unit 222. Exemplarily, the optical fiber cable 221 can adopt a high-strength non-armored optical cable, and the diameter of the single-core optical cable is 5mm. The adjustment unit 222 is used to modulate and demodulate the strain signal for further signal transmission. The adjustment unit 222 can adopt a fiber grating demodulator, which has the characteristics of high integration, multi-channel, and high speed, and can be built-in modular high-power light source. The remote transmission unit 223 transmits the modulated strain signal to the monitoring management unit 224, and the monitoring management unit 224 can store and process the strain signal data, and display the strain value and processing results. In addition, the monitoring management unit 224 can also issue a corresponding safety warning based on the results of data processing for maintenance management. The remote transmission unit 223 can transmit data in a wireless communication manner, for example, Bluetooth, infrared, mobile hotspot or general packet radio service (GPRS) for data transmission. The remote transmission unit 223 may also transmit data via wired communication, such as network cable transmission.
[0049] Furthermore, the adjustment part 222 and the remote transmission part 223 are arranged at one end of the mold body 1 along the first direction X. For example, the adjustment part 222 and the remote transmission part 223 can be arranged at the blade root to facilitate wired communication connection between the remote transmission part 223 and the monitoring management part 224.
[0050] Furthermore, the mold body 1 also includes a first side and a second side relative to each other, and also includes a second mold layer 14, a third mold layer 15 and a fourth mold layer 16. Along the direction from the second side to the first side, the first mold layer 13, the second mold layer 14, the third mold layer 15 and the fourth mold layer 16 are stacked in sequence.
[0051] The first side of the mold body 1 can be regarded as the inner side of the mold body 1, which is in contact with the material of the wind turbine blade, and the second side can be regarded as the outer side of the mold body 1, corresponding to the side of the mold body 1 that is away from the material of the wind turbine blade. The first mold layer 13, the second mold layer 14, the third mold layer 15 and the fourth mold layer 16 of the mold body 1 are stacked in sequence. When making the mold body 1, a pouring process is adopted, and the first mold layer 13, the second mold layer 14, the third mold layer 15 and the fourth mold layer 16 are poured in sequence, which can reduce the cavity inside the mold body 1. The first mold layer 13 can be a fiberglass layer, and 4 layers of surface felt can be made first, with a unit area mass of 30g / m 2 , and then make 2 to 4 layers of biaxial fibers (Biax), with a unit area mass of 400g / m 2, the sensor component 21 is arranged during the manufacturing process. It can be understood that the second mold layer 14, the third mold layer 15 and the fourth mold layer 16 can be one or more of a mold layer, a feature layer and a control function layer.
[0052] Further, the distance from the sensing component 21 to the first side is greater than or equal to the first reference distance and less than or equal to the second reference distance. Exemplarily, the first reference distance is 2 mm, and the second reference distance is greater than 3 mm, so that the strain detected by the sensing component 21 can truly reflect the strain of the first side of the mold body 1, and reduce the influence of the wind turbine blade material on the sensing component 21.
[0053] Figure 5 A schematic diagram of a process of manufacturing a wind turbine blade according to an embodiment of the present application.
[0054] See also Figure 5 The embodiment of the present application also provides a method for manufacturing a wind turbine blade. The wind turbine blade mold of the aforementioned embodiment of the present application can be used during the manufacturing process.
[0055] The method for manufacturing a wind turbine blade in the embodiment of the present application includes:
[0056] Step S1, making a mold body 1.
[0057] The first mold layer 13 is poured to form the mold body 1. The main beam bonding area and the auxiliary beam bonding area are determined according to the positions of the main beam and the auxiliary beam of the wind turbine blade to be manufactured. Considering the shapes of the main beam and the auxiliary beam, the main beam bonding area and the auxiliary beam bonding area extend along the first direction X and are arranged along the second direction Y. In the process of manufacturing the mold body 1, the sensor component 21 of the monitoring mechanism 2 is set in the first mold layer 13.
[0058] Step S2, connecting to monitoring mechanism 2.
[0059] The transmission component 22 of the monitoring mechanism 2 is connected to the sensor component 21 to form the monitoring mechanism 2, so that the strain signal monitored by the sensor component 21 can be transmitted through the transmission component 22 and used to monitor whether mold lifting occurs during mold closing. At this time, the obtained wind turbine blade mold can be the wind turbine blade mold of the aforementioned embodiment of the present application.
[0060] Step S3: loading wind turbine blade materials.
[0061] The wind turbine blade material is directly loaded into the wind turbine blade mold so that the wind turbine blade is partially formed.
[0062] Step S4, applying glue and closing the mold.
[0063] Connect and assemble the various parts of the wind turbine blade and the corresponding wind turbine blade mold together. In this process, the monitoring mechanism 2 detects the strain of the wind turbine blade material through the sensor component 21 to obtain the strain monitoring value. If the strain monitoring value of all positions is always less than the strain critical value corresponding to each position, the mold separation does not occur during the mold closing process, and the wind turbine blade is obtained. If the strain monitoring value of a certain position is greater than or equal to the strain critical value corresponding to the position at a certain moment, the mold separation occurs during the mold closing process, and the wind turbine blade material and / or the mold closing process should be adjusted.
[0064] Furthermore, the method for obtaining the critical strain value includes: obtaining the strain monitoring values of all sensor components 21 when mold release occurs during the mold closing process; obtaining the strain load equation based on all strain monitoring values and the weight of the wind turbine blade material; and obtaining the critical strain value when mold release occurs during the mold closing process based on the strain load equation.
[0065] The strain critical value should be obtained before the wind turbine blade manufacturing process, when it is determined that mold release occurs. In the case of mold release during the mold closing process, the weight of the wind turbine blade material is the load received by the wind turbine blade mold at this time, and the strain monitoring values of all sensor components 21 are obtained. The strain load equation can be obtained based on the load and the strain monitoring value. According to the strain load equation and the weight of the material of the actual wind turbine blade to be manufactured, the strain value at each position, that is, the strain critical value, can be obtained when mold release occurs critically. It can be understood that when obtaining the strain load equation, multiple tests can be carried out to correct and optimize the strain load equation so that the strain load equation can more truly reflect the relationship between the load (the weight of the wind turbine blade material) and the strain generated by the wind turbine blade mold, so as to obtain a more accurate strain critical value, and then more accurately and reliably judge whether mold release occurs in the actual wind turbine blade mold closing process.
[0066] In summary, the embodiment of the present application provides a wind turbine blade mold and a method for manufacturing a wind turbine blade, wherein the mold body is used to manufacture a wind turbine blade, and the wind turbine blade can be formed, the main beam bonding area corresponds to the main beam of the wind turbine blade, and the auxiliary beam bonding area corresponds to the auxiliary beam of the wind turbine blade. The sensor component of the monitoring mechanism is arranged in the first mold layer of the mold body, and is located in the main beam bonding area and the auxiliary beam bonding area. When manufacturing the wind turbine blade mold of the embodiment of the present application, the sensor component is embedded in the first mold layer, thereby fixing the sensor component at the corresponding position in the mold body, so that in the mold monitoring of the wind turbine blade mold closing process, the detection of the sensor component is more accurate and reliable, and the monitoring efficiency is improved.
[0067] The above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any technician familiar with the technical field can easily think of various equivalent modifications or replacements within the technical scope disclosed in the present application, and these modifications or replacements should be included in the protection scope of the present application. Therefore, the protection scope of the present application shall be based on the protection scope of the claims.
Claims
1. A wind turbine blade mold, characterized in that: include: The mold body comprises a main beam bonding area and an auxiliary beam bonding area, wherein the main beam bonding area and the auxiliary beam bonding area extend along a first direction and are arranged along a second direction; the mold body further comprises a first mold layer; The monitoring mechanism includes a sensor component and a transmission component; the sensor component is provided with multiple components, and the multiple sensor components are arranged in the first mold layer and located in the main beam bonding area and the auxiliary beam bonding area; the transmission component is communicatively connected with the sensor component.
2. The wind turbine blade mold according to claim 1, characterized in that: In the main beam bonding area, a plurality of the sensor components are arranged in an array along the first direction and the second direction, a distance between two adjacent sensor components along the first direction is a first distance, a distance between two adjacent sensor components along the second direction is a second distance, and the second distance is smaller than the first distance; In the auxiliary beam bonding area, multiple sensor components are arranged in an array along the first direction and the second direction, the distance between two adjacent sensor components along the first direction is a third distance, and the distance between two adjacent sensor components along the second direction is a fourth distance, and the fourth distance is smaller than the third distance.
3. The wind turbine blade mold according to claim 2, characterized in that: The first distance is equal to the third distance, and the second distance is equal to the fourth distance.
4. The wind turbine blade mold according to claim 1, characterized in that: The sensing component comprises a fiber grating sensor, and the fiber grating sensor comprises a strain sensor and a temperature compensation sensor; the strain sensor is flexibly packaged, the temperature compensation sensor is metal packaged, and the strain sensor and the temperature compensation sensor are connected.
5. The wind turbine blade mold according to claim 1, characterized in that: The transmission component includes an optical fiber cable, an adjustment unit, a remote transmission unit and a monitoring and management unit; the adjustment unit is electrically connected to the sensing component via the optical fiber cable; the remote transmission unit is electrically connected to the adjustment unit; the remote transmission unit is wirelessly connected to the monitoring and management unit, and / or the remote transmission unit is wiredly connected to the monitoring and management unit.
6. The wind turbine blade mold according to claim 5, characterized in that: The adjusting portion and the remote transmission portion are disposed at one end of the mold body along the first direction.
7. The wind turbine blade mold according to claim 1, characterized in that: The mold body also includes a first side and a second side opposite to each other, and also includes a second mold layer, a third mold layer and a fourth mold layer. Along the direction from the second side to the first side, the first mold layer, the second mold layer, the third mold layer and the fourth mold layer are stacked in sequence.
8. The wind turbine blade mold according to claim 7, characterized in that: The distance from the sensing component to the first side is greater than or equal to a first reference distance and less than or equal to a second reference distance.
9. A method for manufacturing a wind turbine blade, characterized in that: include: Pouring a first mold layer to form a mold body; determining a main beam bonding area and an auxiliary beam bonding area, wherein the main beam bonding area and the auxiliary beam bonding area extend along a first direction and are arranged along a second direction; and pouring a sensor component into the first mold layer; Connecting the transmission component to the sensor component in communication to form a monitoring mechanism, and obtaining a wind turbine blade mold; Loading the wind turbine blade material into the wind turbine blade mold; Glue is applied and the mold is closed. At the same time, the monitoring mechanism detects the strain of the wind turbine blade material through the sensor component and obtains the strain monitoring value. If the strain monitoring value is always less than the strain critical value, there is no mold release during the mold closing process and a wind turbine blade can be obtained.
10. The method for manufacturing a wind turbine blade according to claim 9, characterized in that: The method for obtaining the strain critical value includes: When mold release occurs during the mold closing process, the strain monitoring values of all the sensor components are obtained; the strain load equation is obtained based on all the strain monitoring values and the weight of the wind turbine blade material; the strain critical value when mold release occurs during the mold closing process can be obtained based on the strain load equation.