Shaping manipulator and shaping method for aluminum electrolysis electrode block forming die
By using a shaping robot and laser scanning radar to inspect the aluminum electrolysis electrode block forming mold, the problem of uneven density of aluminum electrolysis electrode blocks has been solved, achieving efficient forming and stable use of electrode blocks, and improving the economy and environmental friendliness of aluminum electrolysis production.
Patent Information
- Application Number
- CN202411371550.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-29
- Publication Date
- 2024-11-26
AI Technical Summary
When aluminum electrolytic electrode blocks are pressed in the molding die, the shape of the upper surface of the material is uncontrollable, resulting in uneven density of the aluminum electrolytic electrode blocks, which easily leads to detachment, affecting service life and aluminum electrolysis production efficiency.
A shaping robot using an aluminum electrolytic electrode block forming mold, combined with laser scanning radar to detect the surface shape of the material, trims the surface of the material to ensure that it meets the preset shape requirements before pressing and forming.
It significantly improves the density uniformity of the electrode blocks, extends their service life, increases aluminum electrolysis production efficiency and product quality, reduces energy consumption, and minimizes unplanned downtime and maintenance.
Smart Images

Figure CN119017682A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of aluminum electrolysis forming equipment, and in particular to a shaping manipulator and a shaping method for an aluminum electrolysis electrode block forming die. Background Art
[0002] Aluminum electrolysis electrode blocks are an indispensable key component in the aluminum electrolysis production process, and are mainly used as anodes or cathodes in electrolytic cells. In the aluminum electrolysis process, the aluminum oxide solution (electrolyte) obtained after a series of chemical treatments of bauxite undergoes an electrolytic reaction in the electrolytic cell to generate aluminum liquid and oxygen. In this process, electrode blocks play a vital role.
[0003] The electrode block is mainly made of carbon raw materials such as petroleum coke, pitch coke and binder (such as coal tar) mixed, pressed and roasted. Its internal structure is dense, with good conductivity and high temperature resistance. The production of electrode blocks usually includes the following steps:
[0004] Ingredients: Mix the carbon raw materials, binder and additives evenly according to the proportion.
[0005] Kneading: The mixture is sent into a kneading machine for heating and stirring to fully moisten and mix the various raw materials to form a paste with a certain plasticity.
[0006] Molding: The paste is fed into the electrode block molding machine and pressed into the desired shape and size by pressure.
[0007] Pre-baking: The green body after forming is subjected to preliminary heat treatment in a pre-baking furnace to remove volatiles, improve strength, and prepare for subsequent calcination.
[0008] Calcination: Long-term high-temperature treatment (about 1000°C or above) in a high-temperature calcining furnace causes the paste to undergo a series of physical and chemical changes, forming a stable carbon skeleton structure and obtaining an electrode block with excellent performance.
[0009] Processing: The calcined electrode blocks are machined, such as drilling and grinding, to facilitate the installation of guide rods, connecting busbars and other accessories, and to meet the electrolytic cell assembly requirements.
[0010] The quality of the electrode block directly affects the efficiency, energy consumption, environmental performance and operational stability of the aluminum electrolysis. At present, when the aluminum electrolysis electrode block is pressed in the mold of the electrode block forming machine, the material is metered and put into the lower mold, and then the upper mold is pressed downward to form. Since the upper surface shape of the material after feeding is uncontrollable, the local accumulation of the material causes the pressed aluminum electrolysis electrode block to have poor uniformity in carbon density, which in turn causes the low-density parts of the aluminum electrolysis electrode block to fall off easily when used in subsequent aluminum electrolysis production, resulting in a shorter life of the aluminum electrolysis electrode block. Therefore, it is necessary to make improvements. Summary of the invention
[0011] The technical problem to be solved by the present invention is to provide a shaping manipulator and a shaping method for an aluminum electrolysis electrode block forming die.
[0012] In order to solve the above technical problems, the technical solution of the present invention is:
[0013] A shaping robot for an aluminum electrolytic electrode block forming mold comprises an electrically controlled rotating worktable, a servo linear electric cylinder, a servo linear electric cylinder and a shaping plate; the electrically controlled rotating worktable comprises a shell and an output shaft, the servo linear electric cylinder comprises a cylinder body and a lead screw, and the servo linear electric cylinder comprises a cylinder body and a lead screw; the shell is fixedly connected to the frame of an electrode block forming machine during operation; the servo linear electric cylinder is arranged horizontally, the cylinder body is fixedly connected to an output shaft; the cylinder body is fixedly connected to an end of a lead screw, the lead screw extends vertically downward, and the shaping plate is fixedly connected to the lower end of the lead screw.
[0014] Preferably, there are two shaping plates arranged in parallel.
[0015] Preferably, a plurality of drawing teeth are equidistantly arranged at the lower end of the shaping plate.
[0016] Preferably, a nozzle group is provided on one side of the shaping plate.
[0017] Preferably, an electrically controlled rotating worktable 2 is arranged between the shaping plate and the lead screw 2, and the electrically controlled rotating worktable 2 includes a shell 2 and an output shaft 2, the shell 2 is fixedly connected to the two ends of the lead screw, the output shaft 2 extends downward, and the two ends of the output shaft are fixedly connected to the shaping plate.
[0018] A shaping method for an aluminum electrolysis electrode block forming die, which uses the shaping manipulator as described above, and the method comprises the following steps:
[0019] S1. Putting materials into the lower mold of the electrode block forming machine;
[0020] S2. Use laser scanning radar to detect the surface shape of the material in the mold and perform the following judgment operations:
[0021] S21. If the surface shape of the material does not meet the requirements, the shaping robot is started to trim the surface of the material in the lower mold, and the shaping robot is reset after the trimming is completed;
[0022] S22. The laser scanning radar is activated again to detect the surface shape of the material in the lower mold. If the surface shape of the material does not meet the requirements, step S21 is repeated until the surface shape of the material meets the requirements. Then, the upper mold is controlled to perform pressing to obtain a formed electrode block.
[0023] Preferably, the method of using the laser scanning radar to detect the surface shape of the material in the mold is as follows:
[0024] S201. After each scan of the laser radar data, the data is transmitted to the control system through TCP communication. After parsing the data message of the laser radar, the n distance values of each point in the scanning moving direction are stored in an array DATA[n]; each time the laser radar moves a fixed distance and performs a scan, after m moves to complete the scanning of the entire material plane, m groups of data are obtained, and a two-dimensional array DATA[m, n] is created, in which the data stored is the distance value of all points from the entire material plane to the laser scanning radar;
[0025] S202. Create a two-dimensional array STANDARD[m, n] of plane data of a qualified plane; the two-dimensional array stores the distance value of each point of the qualified plane. When the value of DATA[m, n] is greater than or less than the value of the corresponding point of STANDARD[m, n] for points at the same position, there is a deviation in the plane of the detected material. The deviation between the detected material plane and the qualified plane is processed by matrix subtraction operation:
[0026] Assume that the m*n matrix composed of the data of the detection surface is D mn , the m*n matrix composed of the plane data of the qualified plane is S mn ; The matrix composed of deviation values is P mn ,get:
[0027] D mn -S mn =P mn
[0028] S203. Set a plane concave and convex standard value: T max , if T max <|P[a, b]|, indicating that the deviation value of this point is unqualified, Q[a, b] is assigned a value of 1, and the difference T max >||P[a, b]| is a qualified point, Q[a, b] is assigned 0, and a new deviation result matrix Q is obtained by traversing and checking each point through the program. mn , Q mn What is stored is the qualified or unqualified value of each point;
[0029] S204. By traversing the deviation result matrix Q mn Quickly obtain the exact position coordinates Q[a, b] of the unqualified points (ath row, bth column, where 0<a<m, 0<b<n);
[0030] S205. The minimum detection area for unqualified points is set as a minimum defect area with a length of X (mm) and a width of Y (mm), and the minimum defect area BUG[c, v] corresponding to the two-dimensional array DATA[m, n] is obtained by conversion, where the length of c corresponds to X (mm) and the length of v corresponds to Y (mm);
[0031] S206. By traversing the matrix Q mn , when the data Q[a, b]=1 of a certain point is detected, the data with row a, column b as the origin and row a+c, column b+v as the end point is taken out and put into BUG[c, v] for summation. When the data of each point in the minimum defect area are all 1, the summation value is: c*v. Due to the error in detection, a threshold Δ=0.7 to 1 is set to make a judgment:
[0032] When ∑BUG[c, v]>Δ*c*v, the surface shape of the material in this area is considered unqualified;
[0033] When ∑BUG[c, v]<Δ*c*v, the surface shape of the area is deemed qualified, and the next data is traversed: Q[a, b+1] or Q[a+1, b] and so on to complete the judgment of all areas.
[0034] Preferably, the laser scanning radar adopts horizontal movement scanning, and the laser scanning radar is controlled by a servo motor. When the motor rotates r times, the laser scanning radar advances a constant distance h. The corresponding ratio of the number of motor rotations r to h is k. The length of the object to be scanned is H. Then the number of motor rotations corresponding to the jth row of data can be obtained:
[0035] r = jH / km
[0036] Wherein: m is the number of columns of data collection, 0<j<m.
[0037] Preferably, the laser scanning radar adopts rotation scanning, the laser scanning radar is controlled by a servo motor, and the laser scanning radar moves along an arc; the laser scanning moves an angle β to scan the entire surface of the material, the vertical height of the laser scanning radar to the detected material is L, and the length of the detected object is H; each time the scanning line moves a distance h (h = H / m), then according to the trigonometric function relationship, the angle at the jth scan can be obtained as (where: 1<j<m):
[0038]
[0039] Where: m is the number of columns of data collection;
[0040] According to the high-precision control characteristics of the servo motor and the characteristics of the mechanical gear transmission ratio, the number of rotations of the servo motor is:
[0041]
[0042] You can get:
[0043]
[0044] The control system calculates the corresponding number of motor turns r by calculating the jth scan, and then triggers the program to store the laser scanning radar data into the corresponding DATA[j, n] column data, until all the column data of DATA[m, n] are collected.
[0045] The above technical solution has the following advantages:
[0046] 1. The shaping manipulator of the present invention significantly improves the density uniformity of the electrode block after pressing and forming by arranging the surface shape of the material after entering the forming mold, thereby enhancing the texture uniformity of the electrode block, and finally achieving a significant increase in the service life of the electrode block. This improvement is not only conducive to improving the efficiency and product quality of aluminum electrolysis production, but also helps to achieve a more economical and environmentally friendly electrolytic aluminum production process.
[0047] 2. The highly uniform compaction process helps ensure that the density of each part inside the electrode block is consistent. Density uniformity is crucial to the performance of the electrode block because it directly affects key properties such as conductivity, high temperature resistance, and oxidation resistance. Electrode blocks with uniform density can better conduct current and reduce energy loss during the electrolysis process; at the same time, their good structural stability helps resist electrolyte erosion and thermal expansion effects at high temperatures, extending service life.
[0048] 3. High-density and well-uniformed electrode blocks can conduct current more efficiently during the electrolysis of aluminum, reduce ohmic heat loss, and thus reduce the energy consumption of the electrolysis process. In addition, due to the improvement of the overall performance of the electrode blocks, unplanned downtime and maintenance work caused by electrode block failures are reduced, which indirectly improves the operating efficiency of the electrolytic cell and helps achieve the overall energy-saving and consumption-reduction goals. BRIEF DESCRIPTION OF THE DRAWINGS
[0049] Figure 1 It is a top view of the shaping robot in the present invention in a reset state, wherein part of the structure of the electrode block forming machine is shown;
[0050] Figure 2 It is a top view of the shaping manipulator in the present invention in a shaping state, wherein part of the structure of the electrode block forming machine is shown;
[0051] Figure 3 This is a front view of the shaping robot in the present invention in a shaping state, wherein a partial structure of the electrode block forming machine is shown;
[0052] Figure 4 for Figure 3 A magnified view of part A;
[0053] Figure 5 A schematic diagram of creating a two-dimensional array DATA[m, n] for the laser scanning radar in the shaping method of the present invention;
[0054] Figure 6 This is a principle diagram of the laser scanning radar in the shaping method of the present invention when it adopts rotation scanning;
[0055] In the figure:
[0056] 1-electrically controlled rotary table 1, 2-servo linear electric cylinder 1, 3-servo linear electric cylinder 2, 4-shaping plate, 5-housing 1, 6-output shaft 1, 7-cylinder body 1, 8-screw 1, 9-cylinder body 2, 10-screw 2, 11-pulling tooth, 12-nozzle group, 13-electrically controlled rotary table 2, 14-housing 2, 15-output shaft 2, 20-lower mold, 30-upper mold, 40-frame of electrode block forming machine. DETAILED DESCRIPTION
[0057] The specific embodiments of the present invention are further described below in conjunction with the accompanying drawings. It should be noted that the description of these embodiments is used to help understand the present invention, but does not constitute a limitation of the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0058] Example 1
[0059] As attached Figure 1-4 The shaping robot of the aluminum electrolytic electrode block forming mold shown in the figure includes an electrically controlled rotating worktable 1, a servo linear electric cylinder 2, a servo linear electric cylinder 3 and a shaping plate 4; the electrically controlled rotating worktable 1 includes a shell 5 and an output shaft 6, the servo linear electric cylinder 2 includes a cylinder body 7 and a lead screw 8, and the servo linear electric cylinder 23 includes a cylinder body 9 and a lead screw 10; the shell 5 is fixedly connected to the frame 40 of the electrode block forming machine when working; the servo linear electric cylinder 2 is horizontally arranged, the cylinder body 7 is fixedly connected to the output shaft 6; the cylinder body 9 is fixedly connected to the end of the lead screw 8, the lead screw 10 extends vertically downward, and the shaping plate 4 is fixedly connected to the lower end of the lead screw 10.
[0060] As a preferred technical solution of this embodiment, the shaping plates 4 are two and arranged in parallel, which can effectively improve the efficiency of trimming. The width of the shaping plates 4 is basically close to the width of the inner cavity of the lower mold 20 to ensure that the surface shape after shaping meets the requirements. The shape of the lower end of the shaping plate 4 is designed according to the pre-designed surface shape to ensure that the shape after each shaping is consistent. By replacing the shaping plates 4 with different lower end shapes, the production of electrode blocks of different specifications and shapes can be met.
[0061] As a further improved technical solution of this embodiment, a plurality of drawing teeth 11 are equidistantly arranged at the lower end of the shaping plate 4. The shape arrangement of the lower end of the drawing teeth 11 can be designed according to a pre-designed surface shape, which can effectively improve the efficiency and effect of shaping.
[0062] As a technical solution to further improve this embodiment, a nozzle group 12 is set on one side of the shaping plate 4, and the nozzle group 12 is used to spray soap liquid into the lower mold 20 before adding materials, so as to improve the uniformity of spraying the soap liquid onto the inner surface of the lower mold 20.
[0063] As a technical solution for further improving the present embodiment, an electrically controlled rotating worktable 13 is arranged between the shaping plate 4 and the lead screw 10. The electrically controlled rotating worktable 13 includes a shell 14 and an output shaft 15. The shell 14 is fixedly connected to the end of the lead screw 10. The output shaft 15 extends downward. The end of the output shaft 15 is fixedly connected to the shaping plate 4.
[0064] By setting up the electrically controlled rotating worktable 2 13, when the shaping robot is not working, the shaping plate 4 is rotated 90 degrees by driving the electrically controlled rotating worktable 2 13, thereby effectively shortening the retraction stroke of the servo linear electric cylinder 1 2 when resetting.
[0065] In this embodiment, the electric-controlled rotary table 1, the servo linear electric cylinder 1, the servo linear electric cylinder 2, and the electric-controlled rotary table 2 13 are all driven by servo motors, which have high control accuracy and fast operation speed. In order to improve the operation stability of the servo linear electric cylinder 1 and the servo linear electric cylinder 2, a common guide mechanism can be added between the housing and the lead screw of the electric cylinder, such as the guide structure disclosed in the authorization announcement number CN220629085U, or the guide mechanism disclosed in the announcement number CN220874345U, etc. Obviously, other commercially available servo electric cylinders with guide mechanisms can also be used.
[0066] The working process is as follows:
[0067] Before adding material into the lower mold 20, the shaping robot is in Figure 1In the position shown (reset state), the electric-controlled rotary table 1 rotates 90° counterclockwise, and the lead screw 210 of the servo linear electric cylinder 23 extends downward, so that the shaping plate 4 and the nozzle group 12 enter the lower mold 20 and are located at the left end of the lower mold 20 in the figure. At this time, the lead screw 18 of the servo linear electric cylinder 2 extends to the right side in the figure. While the servo linear electric cylinder 2 extends to the right, the nozzle group 12 sprays soap liquid synchronously; when the nozzle group 12 approaches the right side of the lower mold 20, the servo linear electric cylinder 2 stops, and the nozzle group 12 also stops spraying soap liquid, and then the shaping robot is reset to Figure 1 Then add material to the lower mold 20, as shown in FIG. Figure 2 and Figure 3 In the shaping state shown, the shaping robot is started again. First, the electric-controlled rotating worktable 1 rotates 90° counterclockwise, and the screw 210 of the servo linear electric cylinder 23 extends downward, so that the shaping plate 4 enters the lower mold 20 and is located at the left end of the lower mold 20 in the figure. The descending height is reasonably adjusted in real time according to the height of the material surface. At this time, the screw 18 of the servo linear electric cylinder 2 extends to the right side in the figure to drive the shaping plate 4 to move to the right side of the lower mold 20. When the shaping plate 4 approaches the right side of the lower mold 20, the servo linear electric cylinder 2 stops. At this time, the screw 18 of the servo linear electric cylinder 2 can also be retracted again to realize the reshaping of the material. The number of shaping times is reasonably set according to the shape and interval of the pulling teeth 11, and then the shaping robot is reset to Figure 1 At the position shown, the shaping of the material surface is completed and the subsequent pressing forming process can be carried out.
[0068] Before the material is shaped, the material stacking thickness of each area of the electrode block is calculated according to the compression ratio of the material used in the electrode block and the thickness value of each area after the electrode block is formed, so as to determine the surface shape of the material to be pressed (i.e., the qualified plane), and the shaping plate 4 is designed according to the qualified plane, as well as the control program of each driving element of the shaping robot, to shape the expected surface shape.
[0069] Example
[0070] A shaping method for an aluminum electrolysis electrode block forming die, which uses the shaping manipulator as described above, and the method comprises the following steps:
[0071] S1. Put material into the lower mold 20 of the electrode block forming machine;
[0072] S2. Use laser scanning radar to detect the surface shape of the material in the lower mold 20, and perform the following judgment operations:
[0073] S21. If the surface shape of the material does not meet the requirements, start the shaping manipulator to trim the surface of the material in the lower mold 20. The trimming method is shown in the corresponding content of Example 1. After the trimming is completed, the shaping manipulator is reset;
[0074] S22. The laser scanning radar is activated again to detect the surface shape of the material in the lower mold 20. If the surface shape of the material does not meet the requirements, step S21 is repeated until the surface shape of the material meets the requirements. Then, the upper mold 30 is controlled to perform pressing to obtain a formed electrode block.
[0075] In this embodiment, the method of the laser scanning radar detecting the surface shape of the material in the lower mold 20 is as follows:
[0076] S201. After each scan of the laser radar data, the data is transmitted to the control system through TCP communication. After parsing the data message of the laser radar, the n distance values of each point in the scanning moving direction are stored in an array DATA[n] (the value range of n varies according to the accuracy of the laser scanning radar, generally between 100-900); each time the laser radar moves a fixed distance and performs a scan, after m moves to complete the scanning of the entire material plane, m groups of data are obtained, and a two-dimensional array DATA[m, n] is created, in which the data stored is the distance value of all points from the entire material plane to the laser scanning radar;
[0077] S202. Create a two-dimensional array STANDARD[m, n] of plane data of a qualified plane; the two-dimensional array stores the distance value of each point of the qualified plane. When the value of DATA[m, n] is greater than or less than the value of the corresponding point of STANDARD[m, n] for points at the same position, there is a deviation (convex or concave) in the plane of the detected material, and the deviation between the plane of the detected material and the qualified plane is processed by matrix subtraction operation:
[0078] Assume that the m*n matrix composed of the data of the detection surface is D mn , the m*n matrix composed of the plane data of the qualified plane is S mn ; The matrix composed of deviation values is P mn ,get:
[0079] D mn -S mn =P mn
[0080] S203. Set a plane concave and convex standard value: T max , if T max <|P[a, b]|, indicating that the deviation value of this point is unqualified, Q[a, b] is assigned a value of 1, and the difference T max >|P[a, b]|, the point is a qualified point, Q[a, b] is assigned 0, and a new deviation result matrix Q is obtained by traversing and checking each point through the program. mn , Q mnWhat is stored is the qualified value (value is 0) or unqualified value (value is 1) of each point;
[0081] S204. By traversing the deviation result matrix Q mn Quickly obtain the exact position coordinates Q[a, b] of the unqualified points (ath row, bth column, where 0<a<m, 0<b<n);
[0082] S205. The minimum detection area for unqualified points is set as a minimum defect area with a length of X (mm) and a width of Y (mm), and the minimum defect area BUG[c, v] corresponding to the two-dimensional array DATA[m, n] is obtained by conversion, where the length of c corresponds to X (mm) and the length of v corresponds to Y (mm);
[0083] S206. By traversing the matrix Q mn , when the data Q[a, b]=1 of a certain point is detected, the data with row a, column b as the origin and row a+c, column b+v as the end point is taken out and put into BUG[c, v] for summation. When the data of each point in the minimum defect area are all 1, the summation value is: c*v. Due to the error in detection, a threshold Δ=0.7 to 1 is set to make a judgment:
[0084] When ∑BUG[c, v]>Δ*c*v, the surface shape of the material in this area is considered unqualified;
[0085] When ∑BUG[c, v]<Δ*c*v, the surface shape of the area is deemed qualified, and the next data is traversed: Q[a, b+1] or Q[a+1, b] and so on to complete the judgment of all areas.
[0086] As a specific technical solution of the laser scanning radar scanning method in this embodiment, the laser scanning radar adopts horizontal movement scanning, and the laser scanning radar is controlled by a servo motor. When the motor rotates r times, the laser scanning radar advances a constant distance h. The corresponding ratio of the number of motor rotations r to h is k. The length of the object to be scanned is H, then the number of motor rotations corresponding to the j-th row of data can be obtained:
[0087] r = jH / km
[0088] Wherein: m is the number of columns of data collection, 0<j<m.
[0089] As another scanning method of the laser scanning radar in this embodiment, the laser scanning radar adopts rotation scanning, the laser scanning radar is controlled by a servo motor, and the laser scanning radar moves along an arc; the laser scanning rotates at an angle β to scan the entire material surface, such as Figure 6As shown in the figure, the vertical height of the material scanned by the laser scanning radar is L, and the length of the material to be detected is H; each time the scanning line moves a distance h (h = H / m), then according to the trigonometric function relationship, the angle at the jth scan can be obtained as (where: 1<j<m):
[0090]
[0091] Where: m is the number of columns of data collection;
[0092] According to the high-precision control characteristics of the servo motor and the characteristics of the mechanical gear transmission ratio, the number of rotations of the servo motor is:
[0093]
[0094] You can get:
[0095]
[0096] The control system calculates the corresponding number of motor turns r by calculating the jth scan, and then triggers the program to store the laser scanning radar data into the corresponding DATA[j, n] column data, until all the column data of DATA[m, n] are collected.
[0097] When the electrode block is pressed and formed, the improvement of the surface shape accuracy of the material to be pressed is directly beneficial to the uniform compaction of the material in the subsequent pressing and forming process. After the material fills the lower mold 20, it is compressed and formed under the pressure of the upper mold 30. At this time, if the surface of the material has been pre-arranged into a preset shape, the pressure applied by the pressure head can be more evenly transmitted to the entire material layer, avoiding compaction differences caused by local stress concentration. Uniform compaction is not only beneficial to improving the overall density of the electrode block, but also can reduce internal stress and prevent cracking, deformation and other phenomena in the formed product.
[0098] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the described embodiments. For those skilled in the art, various changes, modifications, substitutions and variations of these embodiments are made without departing from the principles and spirit of the present invention, and still fall within the scope of protection of the present invention.
Claims
1. A shaping manipulator for an aluminum electrolytic electrode block forming mold, comprising an electrically controlled rotary table (1), a servo linear electric cylinder (2), a servo linear electric cylinder (3) and a shaping plate (4); the electrically controlled rotary table (1) comprises a housing (5) and an output shaft (6); the servo linear electric cylinder (2) comprises a cylinder body (7) and a lead screw (8); the servo linear electric cylinder (3) comprises a cylinder body (9) and a lead screw (10); the housing (5) is fixedly connected to a frame (40) of an electrode block forming machine during operation; the characteristics are as follows: The servo linear electric cylinder (2) is arranged horizontally, the cylinder body (7) is fixedly connected to the output shaft (6); the cylinder body (9) is fixedly connected to the end of the lead screw (8), the lead screw (10) extends vertically downward, and the shaping plate (4) is fixedly connected to the lower end of the lead screw (10).
2. The shaping manipulator for the aluminum electrolysis electrode block forming mold according to claim 1 is characterized in that: The shaping plates (4) consist of two pieces and are arranged in parallel.
3. The shaping manipulator for the aluminum electrolysis electrode block forming mold according to claim 1 or 2, characterized in that: A plurality of drawing teeth (11) are equidistantly arranged at the lower end of the shaping plate (4).
4. The shaping manipulator for the aluminum electrolysis electrode block forming mold according to claim 1 is characterized in that: A nozzle group (12) is arranged on one side of the shaping plate (4).
5. The shaping manipulator for the aluminum electrolysis electrode block forming mold according to claim 1 is characterized in that: An electrically controlled rotating worktable (13) is arranged between the shaping plate (4) and the second lead screw (10). The electrically controlled rotating worktable (13) comprises a second housing (14) and a second output shaft (15). The second housing (14) is fixedly connected to the end of the second lead screw (10). The second output shaft (15) extends downward, and the end of the second output shaft (15) is fixedly connected to the shaping plate (4).
6. A method for shaping an aluminum electrolysis electrode block forming die, characterized in that Using the plastic surgery manipulator as described in any one of claims 1 to 6, the method comprises the following steps: S1. Adding material to the lower mold (20) of the electrode block forming machine; S2. Use laser scanning radar to detect the surface shape of the material in the lower mold (20), and perform the following judgment operations: S21. If the surface shape of the material does not meet the requirements, the shaping robot is started to trim the surface of the material in the lower mold (20). After the trimming is completed, the shaping robot is reset; S22. The laser scanning radar is activated again to detect the surface shape of the material in the lower mold (20). If the surface shape of the material does not meet the requirements, step S21 is repeated until the surface shape of the material meets the requirements. Then, the lower mold (30) is controlled to perform pressing to obtain a formed electrode block.
7. The method for shaping an aluminum electrolysis electrode block forming mold according to claim 6, characterized in that: The method for the laser scanning radar to detect the surface shape of the material in the lower mold (20) is as follows: S201. After each scan of the laser radar data, the data is transmitted to the control system through TCP communication. After parsing the data message of the laser radar, the n distance values of each point in the scanning moving direction are stored in an array DATA[n]; each time the laser radar moves a fixed distance and performs a scan, after m moves to complete the scanning of the entire material plane, m groups of data are obtained, and a two-dimensional array DATA[m, n] is created, in which the data stored is the distance value of all points from the entire material plane to the laser scanning radar; S202. Create a two-dimensional array STANDARD[m, n] of plane data of a qualified plane; the two-dimensional array stores the distance value of each point of the qualified plane. When the value of DATA[m, n] is greater than or less than the value of the corresponding point of STANDARD[m, n] for points at the same position, there is a deviation in the plane of the detected material. The deviation between the detected material plane and the qualified plane is processed by matrix subtraction operation: Assume that the m*n matrix composed of the data of the detection surface is D mn , the m*n matrix composed of the plane data of the qualified plane is S mn ; The matrix formed by the deviation value is P mn ,get: D mn -S mn =P mn S203. Set a plane concave and convex standard value: T max , if T max <|P[a, b]|, indicating that the deviation value of this point is unqualified, Q[a, b] is assigned a value of 1, and the difference T max >|P[a, b]|, the point is a qualified point, Q[a, b] is assigned 0, and a new deviation result matrix Q is obtained by traversing and checking each point through the program. mn , Q mn What is stored is the qualified or unqualified value of each point; S204. By traversing the deviation result matrix Q mn Quickly obtain the exact position coordinates of the unqualified points Q[a, b] (row a, column b, where 0 <a<m,0<b<n); S205. The minimum detection area for unqualified points is set as a minimum defect area with a length of X (mm) and a width of Y (mm), and the minimum defect area BUG[c, v] corresponding to the two-dimensional array DATA[m, n] is obtained by conversion, where the length of c corresponds to X (mm) and the length of v corresponds to Y (mm); S206. By traversing the matrix Q mn , when the data Q[a, b]=1 of a certain point is detected, the data with row a, column b as the origin and row a+c, column b+v as the end point is taken out and put into BUG[c, v] for summation. When the data of each point in the minimum defect area are all 1, the summation value is: c*v. Due to the error in detection, a threshold Δ=0.7 to 1 is set to make a judgment: When ∑BUG[c, v]>Δ*c*v, the surface shape of the material in this area is considered unqualified; When ∑BUG[c, v]<Δ*c*v, the surface shape of the area is deemed qualified, and the next data is traversed: Q[a, b+1] or Q[a+1, b] and so on to complete the judgment of all areas.
8. The shaping method of the aluminum electrolysis electrode block forming mold according to claim 7, characterized in that: The laser scanning radar adopts horizontal movement scanning. The laser scanning radar is controlled by a servo motor. When the motor rotates r times, the laser scanning radar advances a constant distance h. The corresponding ratio of the number of motor rotations r to h is k. The length of the object to be scanned is H. Then the number of motor rotations corresponding to the j-th row of data can be obtained: r = jH / km Wherein: m is the number of columns of data collection, 0<j<m.
9. The method for shaping an aluminum electrolysis electrode block forming mold according to claim 7, characterized in that: The laser scanning radar adopts rotation scanning, and the laser scanning radar is controlled by a servo motor. The laser scanning radar moves along an arc. The laser scanning moves an angle β to scan the entire surface of the material. The vertical height of the material scanned by the laser scanning radar is L, and the length of the detected object is H. Each time the scanning line moves a distance h (h = H / m), according to the trigonometric function relationship, the angle at the jth scan can be obtained as (where: 1<j<m): Where: m is the number of columns of data collection; According to the high-precision control characteristics of the servo motor and the characteristics of the mechanical gear transmission ratio, the number of rotations of the servo motor is: You can get: The control system calculates the corresponding number of motor turns r by calculating the jth scan, and then triggers the program to store the laser scanning radar data into the corresponding DATA[j,n] column data, until all the column data of DATA[m,n] are collected.