High-performance bio-based high polymer material and application thereof in 3D printing
By selecting biobased monomers and controlling polymerization reaction conditions, polymer materials with high biobased content and high mechanical properties were prepared, which solved the problem of insufficient performance of existing biobased materials and achieved high precision and complexity of 3D printing technology Shape manufacturing promotes sustainable development.
Patent Information
- Application Number
- CN202411115031.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-26
AI Technical Summary
The existing bio-based materials are difficult to meet the high requirements of 3D printing technology for material performance in terms of mechanical strength, thermal stability, processing performance, etc., which limits the development and application of bio-3D printing technology.
By selecting biobased monomers such as castor oil and soybean oil, using polymerization and post-treatment processes, the polymerization reaction conditions such as temperature, pressure and catalyst use are controlled to prepare high biobased content, excellent mechanical properties and biocompatibility. polymer material.
It has achieved high precision and complex shape manufacturing capabilities of materials, met the strict requirements of 3D printing for material performance, reduced environmental pollution, and promoted the application of 3D printing technology in medical, aviation, automobile and other fields.
Smart Images

Figure CN119019585A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of polymer materials and biological 3D printing, and specifically relates to a bio-based polymer material with high bio-based content and excellent mechanical properties. The material is specially designed for 3D printing technology to realize the manufacture of biocompatible products with complex shapes. Background Art
[0002] In the field of 3D printing technology, the choice of materials has a decisive influence on the printing process and the performance of the final product. At present, the main materials used in 3D printing include plastics, metals, ceramics, etc., among which plastics are the most common choice due to their low cost and easy processing. However, most of these materials are derived from non-renewable fossil fuels, which not only consume a lot of energy during the production process, but also are difficult to degrade after use, causing long-term pollution to the environment. In addition, the performance of these materials in terms of biocompatibility is also difficult to meet the high requirements of materials in the medical field.
[0003] With the enhancement of environmental awareness and the popularization of the concept of sustainable development, bio-based materials have gradually become the focus of research. Bio-based materials, derived from renewable biomass resources such as plants, animals and microorganisms, have the advantages of biodegradability and environmental friendliness. In the field of 3D printing, the development and utilization of bio-based materials have received widespread attention. However, the existing bio-based materials still have a large gap compared with fossil-based materials in terms of mechanical strength, thermal stability, processing performance, etc., and it is difficult to meet the high requirements of 3D printing for material performance.
[0004] Especially in the field of biological 3D printing, the requirements for materials are more stringent. Bio 3D printing technology aims to build three-dimensional tissue structures with biological activity by printing biological materials such as cells and biological factors, providing new technical means for tissue engineering, drug screening, etc. In this process, the materials must not only have good printing performance, but also have excellent biocompatibility, biodegradability, and the ability to promote cell growth and tissue regeneration. However, the performance of existing bio-based materials in these aspects is often difficult to meet the requirements, which limits the development and application of biological 3D printing technology.
[0005] The preparation process of 3D printing materials also has an important impact on printing quality and product performance. Traditional material preparation methods often make it difficult to accurately control the microstructure and properties of materials, and it is difficult to meet the high requirements of 3D printing for material uniformity and stability. Therefore, the development of new bio-based polymer materials and the exploration of efficient material preparation processes are of great significance for promoting the application of 3D printing technology in the fields of medicine, aviation, and automobiles. This can not only improve the mechanical properties and durability of the product, but also reduce environmental pollution and achieve sustainable development of materials.
[0006] The present invention relates to a high-performance bio-based polymer material for 3D printing and a preparation method and application thereof. The material is prepared by a specific polymerization reaction and post-treatment process, has excellent mechanical properties and biocompatibility, is particularly suitable for 3D printing technology, and can manufacture high-precision and complex-shaped biocompatible products. Summary of the invention
[0007] The preparation process of the bio-based polymer material of the present invention begins with selected bio-based monomers. These monomers include, but are not limited to, castor oil, soybean oil and their derivatives, which are extracted from renewable plant resources and have significant biodegradability and environmental sustainability. By polymerizing these bio-based monomers, we are able to produce polymer materials with at least 70% bio-based content, which not only reduces dependence on fossil fuels, but also reduces the environmental impact of the entire production process. During the polymerization stage, we use advanced control technology to ensure the efficiency of the reaction and the consistency of the product. The polymerization reaction is carried out under precisely controlled temperature (60°C to 120°C) and pressure (normal pressure to 10 atmospheres) conditions, which are optimized to maximize the conversion rate of the monomers and reduce the occurrence of side reactions. In addition, we have selected specific catalysts to promote the polymerization process and ensure the uniform growth of the polymer chain, thereby obtaining materials with excellent mechanical properties and processing properties. By precisely adjusting the conditions of the polymerization reaction, the materials of the present invention not only meet high standards in bio-based content, but also perform well in mechanical properties. Specifically, this material exhibits a tensile strength of at least 20MPa and an elongation at break of at least 100%, which enable the material to meet the strict requirements of 3D printing for material performance. In addition, the molecular weight distribution index (Mw / Mn) of the material is strictly controlled between 1.5 and 3.0, which helps to ensure the stability and consistency of the material during processing and application. Due to its high bio-based content, the energy consumption and greenhouse gas emissions of this material during the production process are much lower than those of traditional petroleum-based materials. In addition, the biodegradability of the material facilitates the treatment of waste generated after 3D printing and reduces environmental pollution. This material has a wide range of application potential, especially in industries such as medical, packaging, automotive and aviation, where it can not only provide high-performance solutions but also meet the requirements of these industries for environmental responsibility. Through the development and application of this material, we can drive the entire society towards a more sustainable development direction.
[0008] The polymerization reaction is carried out under a series of strictly controlled conditions to ensure the high performance and consistency of the material. Specifically, the polymerization reaction is carried out in a temperature range of 60°C to 120°C, and this temperature range is carefully selected to ensure that the bio-based monomers can efficiently participate in the polymerization reaction while avoiding the occurrence of side reactions. In addition to temperature control, the pressure of the polymerization reaction is also one of the key parameters. In the present invention, the pressure is controlled between normal pressure and 10 atmospheres, and this pressure range helps to optimize the solubility of the monomers and the mixing of the reactants, thereby promoting the uniform progress of the polymerization reaction. Appropriate pressure also helps to control the growth rate and molecular weight distribution of the polymer chain, further affecting the mechanical properties and processing properties of the final material. In the polymerization reaction, the use of at least one catalyst is crucial to controlling the reaction rate and improving the monomer conversion rate. The catalyst selected by the present invention can efficiently reduce the activation energy of the polymerization reaction, accelerate the connection process between the monomers, and maintain the controllability of the reaction. The type and amount of the catalyst are carefully screened and optimized to ensure that the polymerization reaction not only has a high conversion rate, but also can generate a polymer material with a desired molecular weight and molecular weight distribution. By optimizing the conditions of the polymerization reaction, including temperature, pressure and the use of catalysts, the materials of the present invention exhibit the desired mechanical properties and printing performance. For example, by adjusting the conditions of the polymerization reaction, a tensile strength of at least 20 MPa and an elongation at break of at least 100% can be obtained, which are essential for the interlayer bonding in 3D printing applications and the durability of the final product. In addition, precise control of the polymerization conditions also helps to obtain a uniform molecular weight distribution, thereby ensuring the fluidity and curing behavior of the material during the 3D printing process, and achieving high-precision printing and the manufacture of complex structures.
[0009] The present invention focuses on the control of molecular weight distribution. By precisely adjusting the conditions of the polymerization reaction, we can strictly control the molecular weight distribution index (Mw / Mn) of the material between 1.5 and 3.0. The molecular weight distribution index within this range is carefully selected to ensure the uniformity and stability of the material during processing and application. The molecular weight distribution index is an important parameter for measuring the uniformity of polymer materials. A lower Mw / Mn value indicates that the length of the polymer chain is relatively consistent, which helps to improve the mechanical properties and processing properties of the material. In the present invention, by optimizing the polymerization reaction conditions, such as reaction time, monomer concentration and catalyst dosage, we can obtain a polymer material with a uniform molecular weight distribution. This uniformity is particularly important for 3D printing because it ensures that the print has consistent physical and chemical properties in all directions.
[0010] A variety of polymerization control strategies are adopted. By accurately controlling the reaction time, the growth rate of the polymer chain can be adjusted, thereby affecting the distribution of molecular weight. By adjusting the initial concentration of the monomer, the rate of the polymerization reaction and the growth of the polymer chain can be controlled, thereby affecting the molecular weight distribution. In addition, the type and amount of the catalyst are also key factors affecting the molecular weight distribution. By selecting a suitable catalyst, the uniform progress of the polymerization reaction can be promoted, thereby obtaining a more uniform molecular weight distribution. In 3D printing applications, the molecular weight distribution of the material has a direct impact on the mechanical properties and surface quality of the printed part. By controlling Mw / Mn between 1.5 and 3.0, the material of the present invention can provide better interlayer bonding and fewer printing defects, such as interlayer peeling or holes. In addition, uniform molecular weight distribution also helps to improve the melt flowability and curing consistency of the material, which is crucial for achieving high-precision and complex geometric 3D printing. Through this precise control, the material of the present invention shows broad application prospects in high-end manufacturing fields such as medical, aviation, and automobiles.
[0011] The bio-based polymer material of the present invention achieves a tensile strength of at least 20 MPa through carefully designed polymerization reaction conditions. This performance is achieved by adjusting multiple polymerization parameters, including the initial concentration of monomers, reaction time, and the type and amount of catalyst. The increase in monomer concentration can increase the probability of chain growth, thereby enhancing the tensile strength without sacrificing the toughness of the material. In addition, extending the reaction time helps the polymer chain to reach a higher molecular weight, further enhancing the mechanical properties of the material. In addition to tensile strength, the material of the present invention also has an elongation at break of at least 100%, which gives the material good flexibility and impact resistance. The regulation of elongation at break involves the use of chain transfer agents in the polymerization reaction, the control of reaction temperature, and the optimization of molecular weight distribution. By using chain transfer agents reasonably, the length and distribution of polymer chains can be controlled to avoid excessively long chains causing the material to become brittle. At the same time, maintaining a suitable reaction temperature helps to balance the crystallinity of the material and the flexibility of the non-crystalline region, ensuring that the material can evenly disperse stress when stretched. The comprehensive regulation of mechanical properties is achieved through a series of interrelated polymerization steps. First, by optimizing the polymerization reaction conditions, such as accurately controlling the reaction temperature between 60°C and 120°C, the crystallization behavior of the material and the arrangement of the molecular chain can be adjusted, thereby affecting the tensile strength and elongation at break. Secondly, by adjusting the amount of catalyst, the polymerization rate and the growth of the polymer chain can be controlled, thereby adjusting the crosslinking density and network structure of the material. In addition, by controlling the polymerization reaction time, the molecular weight and molecular weight distribution can be accurately controlled to further optimize the mechanical properties of the material. The excellent mechanical properties of the invented material, especially the tensile strength of more than 20MPa and the elongation at break of more than 100%, make it an ideal choice for manufacturing products with complex shapes. These performance indicators not only meet the high requirements for materials in the 3D printing process, but also ensure the reliability and durability of the final product in practical applications. For example, when manufacturing biomedical implants or tissue engineering scaffolds, these mechanical performance indicators can ensure the stability and adaptability of the product in the in vivo environment. In addition, in the automotive and aviation fields, these properties also help to manufacture lightweight and high-strength components to meet high performance requirements. Through this comprehensive regulation strategy, the material of the present invention provides a broader space for the application of 3D printing technology.
[0012] The preparation of the bio-based polymer material of the present invention is a finely controlled multi-step process, which ensures the high performance and high purity of the material. The following are the specific steps of the preparation method:
[0013] S1. Establishment of inert gas atmosphere: Under the protection of nitrogen or argon, the bio-based monomer is heated in the reaction vessel to the set reaction temperature, which is set between 60°C and 120°C according to the type of monomer and the characteristics of the polymerization reaction. The use of inert gas prevents the occurrence of side reactions such as oxidation and ensures the purity of the polymerization reaction.
[0014] S2. Accurate addition of catalyst: After reaching the reaction temperature, the catalyst is added to the reaction system at a controlled stirring speed (e.g., 200 to 500 rpm). Accurate control of the stirring speed helps to evenly disperse the catalyst in the monomer, thereby promoting uniform polymerization.
[0015] S3. Maintenance of polymerization reaction: The polymerization reaction continues under the set conditions until the predetermined conversion rate is reached, which is usually over 90%. By real-time monitoring of the viscosity or chemical composition of the reaction system, we can accurately judge the progress of the reaction and adjust the reaction conditions accordingly.
[0016] S4. Removal of solvent and monomer: After the polymerization reaction is completed, the solvent and unreacted monomer in the reaction system are removed by molecular distillation or solvent evaporation technology. Molecular distillation is carried out under low temperature and high vacuum conditions to effectively separate the solvent and polymer, while solvent evaporation is carried out at a controlled temperature to minimize thermal degradation of the material.
[0017] S5. Separation and collection of polymer materials: Finally, the polymer materials are separated by filtration or centrifugation. Filtration uses a filter membrane with a specific pore size to remove possible suspended particles, while centrifugation uses centrifugal force to quickly separate solid polymers. The separated polymer materials are dried to remove residual solvents, and finally pure and uniform bio-based polymer materials are obtained.
[0018] The conversion rate of the polymerization reaction is a key indicator for measuring the purity and performance of the material. The conversion rate is at least 90%. This high standard ensures that the vast majority of monomer molecules participate in the reaction and are converted into polymer chains during the polymerization process. High conversion rate means that the content of unreacted monomers and by-products in the reaction system is extremely low, thereby ensuring the high purity of the final material. In addition, high conversion rate also helps to form longer polymer chains, enhance the mechanical properties of the material, such as tensile strength and elongation at break, and meet the strict requirements of 3D printing for material properties. In order to achieve a polymerization reaction conversion rate of at least 90%, the present invention adopts an efficient catalyst system and accurately controls the conditions of the polymerization reaction. By real-time monitoring of the chemical composition of the reaction system, such as by sampling analysis or online sensors, we can accurately evaluate the conversion rate and adjust the reaction conditions, such as temperature, pressure or catalyst dosage, in a timely manner. In addition, by optimizing the kinetics of the polymerization reaction, such as by adjusting the concentration of the initiator or using a chain transfer agent, the conversion rate can be further improved to ensure the efficient conduct of the polymerization reaction. The high conversion rate of the polymerization reaction has a direct impact on the final performance of the material. First, high conversion rates help increase the molecular weight of the material, thereby enhancing its mechanical properties, which is critical for the durability and reliability of 3D printed parts when under load. Second, high-purity materials can reduce impurity interference during the printing process and improve the surface quality and detail resolution of the prints. In addition, high conversion rates also help reduce the instability of the material in the post-processing stage, such as further reactions that may occur during heat treatment or chemical treatment, ensuring the stability and consistency of the material in 3D printing and subsequent applications. Through this sophisticated control strategy, the material of the present invention can meet the stringent requirements for material performance in the field of high-end manufacturing.
[0019] The bio-based polymer material of the present invention is suitable for 3D printing technology, especially photocuring printing method. This 3D printing method includes the following specific steps: Material loading in the resin tank: First, the prepared bio-based polymer material is filled into the resin tank of the 3D printer. This step requires the material to have appropriate viscosity and fluidity to facilitate uniform distribution in the resin tank and hierarchical construction during the printing process. Initialization of the photocuring process: Under the control of the 3D printer, at least one ultraviolet light source is started, and the wavelength of the light source is set in the range of 365nm to 405nm. This wavelength range can ensure that the photosensitizer in the material effectively absorbs ultraviolet energy, triggers a polymerization reaction, and realizes local curing of the material. Parameter control of the photocuring process: Light source power: The power of the ultraviolet light source is controlled between 100mW and 500mW to ensure sufficient energy density to initiate the photopolymerization reaction, while avoiding excessive energy causing overheating or damage to the material. Exposure time: The exposure time of each printed layer is set according to the photosensitivity of the material and the required curing depth, usually between a few seconds and tens of seconds. Layer thickness: The layer thickness in the 3D printing process can be adjusted according to the accuracy requirements of the printed part, generally in the range of 0.01mm to 0.1mm to achieve high-precision printing effects.
[0020] Optimization of the 3D printing process, printing path planning: Through precise printing path planning, ensure the uniformity and consistency of the material during the curing process, and avoid printing defects caused by local overheating or uneven curing. Environmental control: During the 3D printing process, control the temperature and humidity of the printing environment to reduce the impact of environmental factors on material properties and printing quality. Post-curing treatment: After printing is completed, the print is post-cured to improve the final performance of the material. Post-curing can be performed at room temperature or at a slightly higher temperature to accelerate the process.
[0021] Detailed steps for post-processing of 3D printed products: After the 3D printing process is completed, a series of post-processing steps must be performed to ensure the surface quality and biocompatibility of the printed products. First, use isopropyl alcohol or ethanol as a cleaning agent to ultrasonically clean the printed product to remove unreacted monomers and impurities. The frequency of ultrasonic cleaning is set at 40kHz to 60kHz, and the cleaning time is 5 to 10 minutes to ensure the cleaning effect. Next, post-curing treatment is carried out in a hot air cycle at 40℃ to 60℃, and the time is controlled at 1 to 2 hours to improve the cross-linking degree and mechanical properties of the material. The last step of post-processing is sterilization to ensure the biosafety of the product. This can be achieved by high-pressure steam sterilization or using chemical disinfectants. High-pressure steam sterilization is usually carried out at a temperature of 121℃ to 134℃ for about 15 to 30 minutes, and the specific parameters are determined according to the size and shape of the product. If a chemical disinfectant is selected, it is necessary to select the appropriate type of disinfectant and ensure that it is treated according to the recommended concentration and contact time to achieve the sterilization effect. The post-processing steps are critical to the final performance of the 3D printed product. Ultrasonic cleaning not only improves the surface finish of the product, but also removes residues that may affect biocompatibility. Post-curing treatment further enhances the mechanical properties and chemical stability of the material, ensuring the reliability of the product in complex application environments. The final sterilization treatment ensures that the product will not introduce microbial contamination in medical or biomedical applications, meeting the requirements of biosafety. Through this series of finely controlled post-processing steps, 3D printed bio-based polymer material products can meet high performance standards and are suitable for high-performance biocompatible product manufacturing.
[0022] The 3D printed products made of the bio-based polymer materials of the present invention have broad application prospects in the biomedical field due to their high precision and complex shape manufacturing capabilities. These products can be customized according to specific biomedical needs, such as scaffolds for tissue engineering, with a porosity of 70% to 90% and a pore size of 200 microns to 400 microns to promote cell migration and angiogenesis; drug release systems achieve zero-order or pulsed release of drugs by customizing geometric shapes and sizes to ensure that drugs are released at a predetermined rate in the body; and personalized biocompatible implants, such as joint replacement parts or dental implants, can be customized according to the patient's anatomical structure to improve the adaptability of the implant and patient comfort. These applications not only demonstrate the innovative potential of 3D printing technology in the biomedical field, but also provide patients with safer and more effective treatment options.
[0023] The bio-based polymer material of the present invention has a bio-based content of at least 70%, which significantly reduces the dependence on fossil fuels, thereby effectively reducing carbon emissions during the production process, which not only reduces the burden on the environment, but also meets the current urgent requirements for sustainable development. The bio-based characteristics of this material are derived from renewable resources, such as castor oil and soybean oil, which can absorb carbon dioxide in the atmosphere through photosynthesis during their growth, further enhancing the environmental friendliness of the material. In addition, the present invention adopts energy-saving and emission-reduction measures in the synthesis, processing and post-processing of the material, ensuring that the environmental impact of the entire product life cycle is minimized, demonstrating the application potential of 3D printing technology in green manufacturing.
[0024] The technical solution of the present invention can mainly bring about the following three specific technical effects:
[0025] 1. Enhanced mechanical properties and durability: The bio-based polymer material of the present invention achieves a tensile strength of at least 20MPa and an elongation at break of at least 100% by precisely controlling the conditions of the polymerization reaction, which enables the material to exhibit excellent mechanical properties during the 3D printing process. This high-performance material can print complex structural parts that are wear-resistant and impact-resistant, significantly improving the durability and reliability of the product, especially in application scenarios that are subject to mechanical stress.
[0026] 2. Excellent biocompatibility and safety: After specially designed post-processing steps, including ultrasonic cleaning, post-curing and high-pressure steam sterilization, the material of the present invention ensures high biocompatibility and is suitable for direct contact with human cells and tissues. This is crucial for the manufacture of medical products such as tissue engineering scaffolds and drug release systems, as they need to interact with organisms without causing immune responses or toxicity, thereby ensuring the safety and effectiveness of the products.
[0027] 3. Environmental friendliness and sustainability: The material of the present invention contains at least 70% bio-based content, which is derived from renewable resources, reducing dependence on fossil fuels and reducing carbon emissions during the production process. This environmentally friendly attribute not only responds to the global pursuit of sustainable development, but also meets the market demand for green products. In addition, the biodegradability of the material reduces long-term environmental pollution and provides a cleaner and more sustainable manufacturing solution. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 The polymerization reaction flow chart of the present invention is
[0029] Figure 2 This is a 3D printing process flow chart of the present invention
[0030] Figure 3 This is the post-processing flow chart of the present invention
[0031] Figure 4 The flow chart of the preparation of polymer materials of the present invention is DETAILED DESCRIPTION
[0032] The following will be combined with the attached embodiment of the present invention Figures 1 to 4 , the technical solutions in the embodiments of the present invention are clearly and completely described. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0033] The bio-based polymer material of the present invention and its application in 3D printing are described in detail through the following specific implementation steps.
[0034] Bio-based polymer materials are composed of carefully selected bio-based monomers, which have a bio-based content of at least 70%. Specifically, the bio-based monomers include castor oil, soybean oil, or derivatives obtained by chemical modification, all of which are derived from renewable plant resources. These bio-based monomers are converted into polymer materials through precisely controlled polymerization reactions, which not only ensure the biodegradability of the materials, but also significantly reduce the environmental footprint of the production process. The polymerization reaction is carried out under a series of strictly controlled conditions to ensure the high performance of the materials. The reaction temperature is precisely controlled between 60°C and 120°C to ensure the effective conversion of the monomers and the uniform growth of the polymer chains. The pressure is controlled at normal pressure to 10 atmospheres to optimize the kinetics of the polymerization reaction. In addition, a specific catalyst is selected to promote the polymerization process, ensuring at least 90% monomer conversion, thereby obtaining a high-purity polymer material. The molecular weight distribution index (Mw / Mn) is strictly controlled between 1.5 and 3.0, which helps to ensure the consistency and processability of the material. By precisely adjusting the conditions of the polymerization reaction, the material of the present invention exhibits excellent mechanical properties. Specifically, the material has a tensile strength of at least 20MPa and an elongation at break of at least 100%, which are achieved by adjusting the parameters of the polymerization reaction, such as monomer concentration, catalyst dosage and reaction time. These mechanical performance indicators are critical to meeting the strict requirements for materials in the 3D printing process, ensuring the durability and reliability of the printed parts. Energy consumption and greenhouse gas emissions during the production process are significantly lower than those of traditional petroleum-based materials, thanks to its at least 70% bio-based content. The biodegradability of the material further reduces long-term environmental pollution and provides a cleaner and more sustainable manufacturing solution. In addition, the biocompatibility of the material makes it have broad application prospects in the medical field, such as being used to manufacture tissue engineering scaffolds, drug release systems, etc. These applications can not only provide high-performance solutions, but also meet the high requirements of the medical industry for material safety and effectiveness.
[0035] Bio-based polymer materials are prepared by finely controlling the polymerization reaction conditions to ensure that the materials have excellent mechanical properties and printing performance. The polymerization reaction is carried out under strictly controlled temperature and pressure conditions. The specific parameters are as follows: Temperature control, the polymerization reaction is carried out in a precise temperature range of 60°C to 120°C. The selection of this temperature range is based on a deep understanding of the polymerization behavior of bio-based monomers, ensuring that the monomers can be effectively converted into polymer chains during the reaction process while avoiding excessive polymerization or side reactions. Pressure control, the reaction is carried out in the range of normal pressure to 10 atmospheres. This pressure range helps to promote the dissolution of monomers and the uniform mixing of reactants, thereby improving the efficiency of the polymerization reaction and the quality of the product. Catalyst use, at least one catalyst is introduced into the reaction system to increase the polymerization rate and control the growth of polymer chains. The amount and type of catalyst are carefully selected to ensure at least 90% monomer conversion while obtaining an ideal molecular weight distribution.
[0036] By precisely controlling the conditions of the polymerization reaction, the material of the present invention exhibits the desired mechanical properties and printing performance. For example, the tensile strength of the material is at least 20MPa, and the elongation at break is at least 100%, and these performance indicators are achieved by adjusting the parameters of the polymerization reaction. Specifically, tensile strength: By optimizing the temperature and catalyst dosage of the polymerization reaction, the tensile strength of the material is controlled to at least 20MPa, which provides the necessary mechanical support for 3D printed parts. Elongation at break: By adjusting the pressure and monomer concentration of the polymerization reaction, the elongation at break of the material is controlled to at least 100%, ensuring the flexibility and fracture resistance of the printed part when subjected to force. Molecular weight distribution: Precise control of the polymerization reaction also ensures that the molecular weight distribution index (Mw / Mn) of the material is between 1.5 and 3.0, which helps the fluidity and curing behavior of the material during 3D printing, achieving high-precision printing and the manufacture of complex structures.
[0037] A systematic polymerization optimization strategy was adopted. Through experimental design methods (such as response surface analysis or orthogonal experimental design), various parameters of the polymerization reaction were comprehensively optimized. This approach not only improved the performance of the material, but also shortened the R&D cycle and reduced production costs. With this method, we can quickly obtain bio-based polymer materials that meet specific application requirements.
[0038] Bio-based polymer materials pay special attention to the precise control of molecular weight distribution in polymerization reactions. The molecular weight distribution index (Mw / Mn) is a key parameter for measuring the polydispersity of polymer materials, which directly affects the processing properties of the materials and the performance of the final application. In the present invention, by finely adjusting the conditions of the polymerization reaction, we control the Mw / Mn within a narrow range of 1.5 to 3.0, and this range is selected based on a deep understanding of the material processing and performance requirements.
[0039] Process parameters for molecular weight distribution control, polymerization reaction time: controlled within 2 to 6 hours to ensure that the monomers react fully while avoiding overpolymerization. Initial monomer concentration: set within the range of 0.5M to 2.0M to adjust the polymerization rate and molecular weight. Catalyst dosage: accurately metered to achieve high conversion rate according to the activity of the catalyst and the scale of the reaction system. Reaction temperature: maintained at 60°C to 120°C to optimize the kinetics and molecular weight growth of the polymerization reaction. Reaction pressure: adjusted at atmospheric pressure to 10 atmospheres to maintain the uniformity of the reaction system and the miscibility of the reactants. Through the precise control of the above process parameters, the material of the present invention exhibits excellent uniformity and stability. For example, when Mw / Mn is close to 1.5, the material exhibits lower polydispersity, which helps to improve the interlayer bonding strength and overall consistency of the printed parts during 3D printing. At the same time, controlling Mw / Mn not to exceed 3.0 ensures that the material has sufficient fluidity during processing without sacrificing its mechanical strength, which is particularly important for printing parts with complex geometries. Analytical techniques such as gel permeation chromatography (GPC) are used to monitor and adjust the polymerization reaction. By providing real-time feedback on molecular weight changes during the polymerization process, we can dynamically adjust the reaction conditions to ensure that the Mw / Mn of the final material is always within the target range. This fine control strategy not only improves the performance of the material, but also increases the flexibility and repeatability of the production process, providing a reliable and high-performance bio-based polymer material for 3D printing.
[0040] Bio-based polymer materials achieve a tensile strength of at least 20MPa and an elongation at break of at least 100% by finely controlling the polymerization reaction conditions. These mechanical performance parameters are critical to meet the manufacturing requirements of complex-shaped products. Tensile strength: By optimizing the polymerization reaction conditions, especially increasing the initial concentration of the monomer to 1.5M to 2.5M, and using an appropriate amount of efficient catalyst in the polymerization reaction, we are able to prepare materials with a tensile strength of at least 20MPa. This strength level is determined by dynamic mechanical analysis (DMA) testing to ensure that the material has sufficient resistance to deformation when stretched. Elongation at break: In order to obtain an elongation at break of at least 100%, the present invention specifically controls the reaction temperature between 70°C and 90°C and the polymerization time in the range of 3 hours to 5 hours during the polymerization process. These conditions help to form polymer chains with appropriate flexibility, so that they can withstand large deformations before breaking. The initial concentration of the monomer is precisely adjusted from 1.5M to 2.5M to ensure appropriate cross-linking of the polymer chains during the polymerization process, thereby enhancing the tensile strength. Maintaining the reaction temperature at 70°C to 90°C helps balance the crystalline and non-crystalline regions of the material, thereby obtaining good elongation at break. By controlling the polymerization time to 3 hours to 5 hours, the molecular weight and molecular weight distribution can be precisely controlled, thereby adjusting the toughness and ductility of the material. The comprehensive optimization of mechanical properties is achieved through a series of interrelated polymerization steps. By adjusting the monomer concentration, temperature, time and catalyst dosage in the polymerization reaction, we not only achieved a tensile strength of at least 20MPa and an elongation at break of at least 100%, but also maintained the uniformity and stability of the material. The precise control of these parameters is achieved through a real-time monitoring and feedback adjustment system, ensuring the performance consistency of each batch of materials. Excellent mechanical properties make it an ideal choice for manufacturing complex-shaped products in 3D printing technology. For example, in the biomedical field, these performance indicators can ensure that the printed tissue engineering scaffolds or implants have sufficient mechanical strength and appropriate flexibility in the in vivo environment. In the aerospace field, these mechanical performance indicators help to manufacture lightweight and high-strength parts to meet high-performance requirements. Through this comprehensive regulation strategy, the material of the present invention provides a broader space for the application of 3D printing technology and ensures the reliability and durability of the final product in practical applications.
[0041] The preparation of the bio-based polymer material of the present invention is a finely controlled multi-step process, which ensures the high performance and high purity of the material. The following are the specific steps and parameters of the preparation method:
[0042] S1. Establishment of inert gas atmosphere: Under the protection of nitrogen or argon, the bio-based monomer is heated in the reaction vessel to the set reaction temperature, which is set between 60°C and 120°C according to the type of monomer and the characteristics of the polymerization reaction. The flow rate of the inert gas is controlled at 0.5 to 1.0 liters / minute to ensure that there is no oxygen in the reaction system to prevent the occurrence of side reactions such as oxidation.
[0043] S2. Accurate addition of catalyst: After reaching the reaction temperature, the catalyst is added to the reaction system at a controlled stirring speed (e.g., 200 to 500 rpm). The amount of catalyst used depends on the specific requirements of the polymerization reaction, usually 0.1% to 1.0% of the weight of the monomer.
[0044] S3. Maintenance of polymerization reaction: The polymerization reaction is continued under the set conditions until a predetermined conversion rate is reached, which is usually more than 90%. The reaction time is usually set at 2 to 6 hours according to the kinetic characteristics of the polymerization reaction.
[0045] S4. Removal of solvent and monomer: After the polymerization reaction is completed, the solvent and unreacted monomer in the reaction system are removed by molecular distillation or solvent evaporation technology. Molecular distillation is carried out at low temperature of -20℃ to -40℃ and high vacuum conditions to effectively separate the solvent and polymer. Solvent evaporation is carried out at a temperature of 40℃ to 60℃ to minimize thermal degradation of the material.
[0046] S5. Separation and collection of polymer materials: Filtration uses a filter membrane with a pore size of 0.2 to 0.45 microns to remove possible suspended particles. Centrifugal separation is performed at a speed of 3000 to 5000 rpm, using centrifugal force to quickly separate solid polymers. The separated polymer materials are dried in hot air at 40°C to 60°C to remove residual solvents, and finally pure and uniform bio-based polymer materials are obtained.
[0047] In the preparation process of the bio-based polymer material of the present invention, the conversion rate of the polymerization reaction is a key factor to ensure the high purity and high performance of the material. We have achieved a conversion rate of at least 90% by precisely controlling the conditions of the polymerization reaction. This conversion rate is achieved by strict control of the following parameters: Catalyst efficiency, the selected catalyst has high activity and can promote efficient polymerization of monomers in a short time, and the amount of catalyst is accurate to 0.5% to 1.5% of the weight of the monomer. Initiator concentration, the concentration of the initiator is set to 0.01M to 0.1M to ensure that the polymerization reaction starts quickly and maintains a high conversion rate. Polymerization time, the reaction time is controlled between 3 hours and 6 hours to ensure sufficient time to achieve a high conversion rate while avoiding over-polymerization. Reaction temperature, the polymerization reaction temperature is precisely controlled between 65°C and 75°C. This temperature range is conducive to the activity of the catalyst and reduces the occurrence of side reactions.
[0048] A high conversion rate means that more monomers participate in polymerization to form longer polymer chains, thereby increasing the molecular weight of the material and enhancing its mechanical properties. A conversion rate of at least 90% reduces the content of unreacted monomers and low molecular weight by-products and improves the purity of the material, which is crucial for subsequent 3D printing processing and the safety of the final product. High-purity materials exhibit better fluidity and curing consistency during 3D printing, which helps to print products with high precision and complex geometries. Materials with high conversion rates show better chemical stability during post-processing, such as heat treatment or chemical cross-linking, reducing the possibility of further reactions and ensuring the reliability of the product. Through the precise control of the above parameters, the bio-based polymer material of the present invention not only meets the high requirements of 3D printing for material properties, but also has excellent mechanical properties and biocompatibility, and is suitable for manufacturing various high-performance biocompatible products.
[0049] The bio-based polymer material of the present invention is suitable for 3D printing technology, especially photocuring printing method. This 3D printing method includes the following specific steps: material loading in the resin tank, filling the prepared bio-based polymer material into the resin tank of the 3D printer. This step requires the material to have appropriate viscosity and fluidity to facilitate uniform distribution in the resin tank and hierarchical construction during the printing process. Initialization of the photocuring process, under the control of the 3D printer, start at least one ultraviolet light source, and the wavelength of the light source is set in the range of 365nm to 405nm. This wavelength range can ensure that the photosensitizer in the material effectively absorbs ultraviolet energy, triggers a polymerization reaction, and realizes local curing of the material. The power of the ultraviolet light source is controlled at 100mW to 500mW to ensure sufficient energy density to initiate the photopolymerization reaction, while avoiding excessive energy causing overheating or damage to the material. The exposure time of each printed layer is set according to the photosensitivity of the material and the required curing depth, usually between a few seconds and tens of seconds. The layer thickness in the 3D printing process can be adjusted according to the accuracy requirements of the print, generally in the range of 0.01mm to 0.1mm, to achieve a high-precision printing effect.
[0050] Through precise printing path planning, the uniformity and consistency of the material during the curing process are ensured to avoid printing defects caused by local overheating or uneven curing. During the 3D printing process, the temperature and humidity of the printing environment are controlled to reduce the impact of environmental factors on material properties and printing quality. After printing is completed, the print is post-cured to improve the final properties of the material. Post-curing can be performed at room temperature or at a slightly higher temperature to accelerate the process.
[0051] After 3D printing, the product needs to undergo specific post-processing steps to optimize its physical and chemical properties. The specific steps and related parameters are as follows: Use isopropyl alcohol or ethanol as a cleaning agent, and its concentration is controlled at 99.5% to 100% (volume fraction). The frequency of ultrasonic cleaning is set at 40kHz to 60kHz to ensure the cleaning effect. The cleaning time is controlled at 5 minutes to 10 minutes to ensure that the cleaning agent can fully penetrate and remove residues. During the cleaning process, the power of the ultrasonic wave is maintained at 100W to 500W to provide sufficient mechanical force. Post-curing treatment: The post-curing treatment is carried out in a hot air circulation box with a temperature set at 40℃ to 60℃. The wind speed of the hot air circulation is controlled at 1m / s to 2m / s to ensure that the hot air can evenly penetrate the print. The post-curing time is adjusted according to the thickness of the print and the required performance, and is generally controlled at 1 hour to 2 hours. After the post-curing treatment is completed, the print is naturally cooled to ambient temperature at room temperature for subsequent quality inspection or application.
[0052] After 3D printing, the product needs to go through a meticulous post-processing process to optimize its performance and ensure biocompatibility. Here are the specific steps and their operating parameters: Use isopropyl alcohol or ethanol with a concentration of 99.5% to 100% as a cleaning agent. During the cleaning process, the frequency of the ultrasound is set at 40kHz to 60kHz and the power is between 100W and 500W. The cleaning time is controlled at 5 to 10 minutes to completely remove the residue. The cleaned print is placed in a hot air circulation box with a temperature set at 40℃ to 60℃. The post-curing time is set at 1 to 2 hours according to the size and material properties of the print to fully cure the material. High-pressure steam sterilization is carried out at 121℃ to 134℃ for 15 to 30 minutes to ensure the killing of all microorganisms. Use chemical disinfectants and treat them according to the manufacturer's recommended concentration and contact time.
[0053] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited by the above embodiments. The above embodiments and descriptions are only preferred examples of the present invention and are not intended to limit the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A high-performance bio-based polymer material for 3D printing, characterized in that: The material is prepared from at least one bio-based monomer through a controlled polymerization reaction, wherein the bio-based monomer is selected from castor oil, soybean oil or derivatives thereof.
2. The material according to item 1, characterized in that The polymerization reaction is carried out at a temperature of 60° C. to 120° C. and a pressure of normal pressure to 10 atmospheres, and at least one catalyst is used during the reaction.
3. The material according to item 1, characterized in that The post-polymerization treatment includes a molecular distillation or solvent evaporation step to remove unreacted monomers and catalyst residues.
4. The material according to any one of 1, characterized in that The molecular weight distribution index (Mw / Mn) of the material is controlled between 1.5 and 3.
0.
5. The material according to any one of item 1, characterized in that By adjusting the polymerization conditions, the tensile strength of the material is at least 20 MPa and the elongation at break is at least 100%.
6. A method for preparing the material as described in any one of item 1, characterized in that: The method comprises the following steps: S1. heating the bio-based monomer to a reaction temperature in an inert gas atmosphere; S2. Adding the catalyst under controlled stirring speed; S3. Maintaining the polymerization reaction until a predetermined conversion rate is reached; S4. removing the solvent and unreacted monomer by molecular distillation or solvent evaporation; S5. Separate and collect the final polymer material by filtration or centrifugation.
7. The method according to 6, characterized in that The conversion rate of the polymerization reaction is at least 90%, and the biobased content of the material is at least 70%.
8. A 3D printing method using the material described in any one of 1 to 7, characterized in that: The method includes photocuring the material in a resin tank of a 3D printer, wherein the photocuring process includes at least one ultraviolet light source having a wavelength of 365nm to 405nm.
9. The 3D printing method according to 8, characterized in that: The post-processing of the 3D printed product includes the following steps: ultrasonic cleaning using isopropyl alcohol or ethanol; post-curing treatment in a hot air cycle of 40° C. to 60° C.; and sterilization treatment by high-pressure steam sterilization or chemical disinfectant.
10. A 3D printed product, characterized in that: Made from the material as described in any one of 1 to 9 by a 3D printing method, having at least one biomedical application, such as a tissue engineering scaffold, a drug release system or a biocompatible implant.