Monomolecular array chip based on molybdenum disulfide doping and preparation method thereof
By depositing molybdenum disulfide doped coating materials on single-molecular array chips, the problem of low signal-to-noise ratio in the prior art is solved, the accuracy and reliability of detection are significantly improved, and the high in extremely trace molecular detection is achieved Sensitivity signal extraction.
Patent Information
- Application Number
- CN202411141725.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-08-20
AI Technical Summary
The signal-to-noise of existing single-molecule array chips is relatively low, which affects the accuracy and reliability of detection. It is especially difficult to accurately extract the target signal in single-molecule immune analysis.
Using a single-molecular array chip preparation method based on molybdenum disulfide doped coating material is deposited on the substrate chip, and the coating chip is formed using thermal evaporation thin film deposition technology and magnetron sputtering coating technology, and plasma cleaning is performed. , improve signal-to-noise ratio.
It significantly improves the signal-to-noise ratio of single-molecule array chips, enhances the accuracy and reliability of single-molecule immunoassays, and can provide stable single-molecule signals in extremely trace molecular detection.
Smart Images

Figure CN119020728A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of biological detection chips, in particular to the production technology of single molecule immune detection chips. Background Art
[0002] Single Molecule Array (SiMoA) technology is a method that uses single molecule counting to detect trace biomarkers. The detection limit of this technology can reach the order of femtogram (fg / mL), and it is currently the most representative single molecule immunoassay technology. The system is derived from a detection system developed by David Walt and David Duffy's team. Its detection principle is similar to digital PCR, and both are achieved through single molecule isolation combined with single molecule level signal amplification through a microreactor unit.
[0003] SiMoA technology is a single-molecule immunoassay based on microarray chips. It is to carve (or cast) thousands of micron-scale microwells on a millimeter-scale chip, each microwell has a volume of about 40 fl (i.e., a single-molecule array chip), and then distribute the immune complex magnetic beads in the microwells, and then count the fluorescent spots with the help of a high-resolution fluorescence microscope. According to the Poisson distribution theory, the ratio of the number of wells containing beads and fluorescent products at the same time to the total number of wells containing beads is calculated to determine the concentration of the detected substance in the test sample. The operation process is roughly as follows:
[0004] (1) using magnetic beads labeled with capture antibodies to capture antigens in the sample;
[0005] (2) labeling the captured antigen using a biotinylated detection antibody;
[0006] (3) adding streptavidin-galactosidase complex to bind to biotin on the detection antibody;
[0007] (4) The washed magnetic beads are mixed with the substrate and loaded into a single molecule array chip. The magnetic field is used to make the magnetic beads fall into microwells that are perfectly matched to their size, and an oil phase is added to physically isolate the microwells.
[0008] (5) The microwell containing galactosidase produces fluorescent products due to the catalysis of the substrate by the enzyme molecules;
[0009] (6) Performing fluorescence imaging on the microwell array and achieving quantitative detection by comparing the number of microwells emitting fluorescent signals with a standard curve.
[0010] One of the main problems of SiMoA technology is the low sensitivity of its single array signal, which directly affects the accuracy and reliability of detection. In practical applications, especially in single-molecule immunoassays, it is necessary to detect and analyze extremely small amounts of molecules. However, the signal-to-noise ratio of single-molecule array chips in the prior art is poor, which makes it difficult to accurately extract the target signal from the background noise, limiting its application breadth and accuracy in biomolecule detection. Summary of the invention
[0011] In order to solve the problems existing in the prior art, the present invention provides a single molecule array chip based on molybdenum disulfide doping and a preparation method thereof.
[0012] The technical solution adopted by the present invention is: a method for preparing a single-molecule array chip based on molybdenum disulfide doping, characterized in that: the production raw materials include a substrate chip and a molybdenum disulfide doped coating material; the molybdenum disulfide doped coating material is composed of a synergistic metal material and molybdenum disulfide in a mass ratio of 1:0.01 to 0.8; the synergistic metal material includes ruthenium.
[0013] As a further improvement of the present invention, the synergistic metal material is composed of ruthenium and palladium in a mass ratio of 1:0.3 to 1.5.
[0014] As a further improvement of the present invention, it also includes the step of forming a molybdenum disulfide doping material film on the substrate chip to obtain a coated chip. More preferably, the thickness of the molybdenum disulfide doping material film of the coated chip is 65-140 nm.
[0015] As a further improvement of the present invention, the base chip is selected from any one of a silicon single crystal substrate base chip, a FZ single crystal silicon wafer, a CZ single crystal silicon wafer, a semi-insulating single crystal silicon wafer, and an ultra-high purity single crystal silicon wafer.
[0016] The above-mentioned coated chip can be obtained by depositing the molybdenum disulfide doped coating material on the base chip through thermal evaporation thin film deposition technology, or by depositing the molybdenum disulfide doped coating material on the base chip through magnetron sputtering coating technology.
[0017] If thermal evaporation thin film deposition technology is used for coating, the following specific steps can be followed:
[0018] S1. Surface treatment of the substrate chip is performed by ultrasonic cleaning or argon plasma cleaning to remove residual organic matter and oxides;
[0019] S2, placing the molybdenum disulfide doped coating material in the vacuum chamber of the thermal evaporation coating machine, placing the substrate chip on the rotary coating table, controlling the rotation speed to 20-50 rpm, and the vacuum degree to 10 -6 ~10 -7torr, the heating temperature is 500-600℃ to start the thermal evaporation film deposition; during the deposition process, the deposition rate is measured in real time by a quartz crystal microbalance, and the evaporation rate is adjusted by adjusting the heating power and the evaporation source temperature to control the MoS2 deposition rate within The deposition rate of the enhanced metal material is controlled at
[0020] S3. The sample is released by gradually increasing the ambient pressure or opening the gas inlet valve to restore the atmospheric pressure and obtain a coated chip.
[0021] The above steps can ensure uniform and high-quality deposition of the metal film on the substrate surface, providing a reliable basis for the subsequent preparation of the single-molecule array chip.
[0022] As a further improvement of the present invention, the method further includes the step of plasma cleaning the coated chip.
[0023] The parameters of the above plasma cleaning can be set as follows: use high-purity oxygen as the cleaning gas, set the gas pressure to 0.1-1 mTorr, the gas flow rate to 5-20 sccm, the RF power to 100-500 W, and the cleaning time to 5-30 min.
[0024] The present invention also discloses a single-molecule array chip based on molybdenum disulfide doping, which is prepared by the preparation method of the single-molecule array chip based on molybdenum disulfide doping of the present invention.
[0025] The beneficial effect of the present invention is that the single-molecule array chip based on molybdenum disulfide doping prepared by the method of the present invention can significantly improve the signal-to-noise ratio of the single-molecule array chip, and further improve the accuracy and reliability of the technology in single-molecule immunoassay. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 This is a morphology image of the single molecule array chip of Example 1 under an atomic force microscope (AFM). DETAILED DESCRIPTION
[0027] The present invention is further described below in conjunction with embodiments.
[0028] Embodiment 1:
[0029] Prepare the single molecule array chip as follows:
[0030] (1) preparing a molybdenum disulfide doped coating material according to a mass ratio of a synergistic metal material to molybdenum disulfide of 1:0.15, wherein the synergistic metal material is ruthenium;
[0031] (2) Using ultrasonic cleaning to treat the surface of the substrate chip (silicon single crystal substrate substrate chip, cut from 4 inches, thickness 525 μm) to remove residual organic matter and oxides;
[0032] (3) The above-mentioned MoS2 doped coating material was placed in the vacuum chamber of the thermal evaporation coating machine, and the substrate chip was placed on the rotary coating table. The rotation speed was controlled to 45 rpm and the vacuum degree was 3×10 -7 torr, the heating temperature was 550℃ to start the thermal evaporation film deposition; during the deposition process, the deposition rate was measured in real time by a quartz crystal microbalance, and the evaporation rate was adjusted by adjusting the heating power and the evaporation source temperature to control the MoS2 deposition rate within The deposition rate of the enhanced metal material is controlled at When the thickness of the molybdenum disulfide doped material film of the coated chip reaches 80 nm, the gas inlet valve is opened to restore the atmospheric pressure to release the sample to obtain the coated chip.
[0033] (4) Use a plasma cleaning machine (CPC-G / Gplus) to clean the coated chip. Use high-purity oxygen (oxygen purity ≥ 99.995%) as the cleaning gas. Set the gas pressure to 0.5 mTorr, the gas flow rate to 15 sccm, the RF power to 400 W, and the cleaning time to 20 min. After the cleaning is completed, gradually restore the atmospheric pressure to complete the treatment, and obtain a single molecule array chip.
[0034] The surface morphology of the single molecule array chip was observed using an atomic force microscope (AFM). Figure 1 shown.
[0035] Embodiment 2:
[0036] Prepare the single molecule array chip as follows:
[0037] (1) preparing a molybdenum disulfide doped coating material according to a mass ratio of the synergistic metal material to molybdenum disulfide of 1:0.3, wherein the synergistic metal material is ruthenium;
[0038] (2) Using ultrasonic cleaning to treat the surface of the substrate chip (silicon single crystal substrate substrate chip, cut from 4 inches, thickness 525 μm) to remove residual organic matter and oxides;
[0039] (3) The above-mentioned MoS2 doped coating material was placed in the vacuum chamber of the thermal evaporation coating machine, and the substrate chip was placed on the rotary coating table. The rotation speed was controlled to 50 rpm and the vacuum degree was 2×10 -7 torr, the heating temperature was 500℃ to start the thermal evaporation film deposition; during the deposition process, the deposition rate was measured in real time by a quartz crystal microbalance, and the evaporation rate was adjusted by adjusting the heating power and the evaporation source temperature to control the MoS2 deposition rate within The deposition rate of the enhanced metal material is controlled at When the thickness of the molybdenum disulfide doped material film of the coated chip reaches 120 nm, the gas inlet valve is opened to restore the atmospheric pressure to release the sample to obtain the coated chip.
[0040] (4) Use a plasma cleaning machine (CPC-G / Gplus) to clean the coated chip. Use high-purity oxygen (oxygen purity ≥ 99.995%) as the cleaning gas. Set the gas pressure to 0.8 mTorr, the gas flow rate to 5 sccm, the RF power to 300 W, and the cleaning time to 10 min. After the cleaning is completed, gradually restore the atmospheric pressure to complete the treatment, and obtain a single molecule array chip.
[0041] Embodiment three:
[0042] This example is a comparative example of Example 1, and is implemented under the same conditions and steps as Example 1, except that the synergistic metal material is composed of ruthenium and palladium in a mass ratio of 1:0.8 (the mass ratio of the synergistic metal material to molybdenum disulfide and the thickness of the molybdenum disulfide doping material film remain unchanged). The specific steps are as follows:
[0043] (1) preparing a molybdenum disulfide doped coating material in a mass ratio of a synergistic metal material to molybdenum disulfide of 1:0.15, wherein the synergistic metal material is composed of ruthenium and palladium in a mass ratio of 1:0.8;
[0044] (2) Using ultrasonic cleaning to treat the surface of the substrate chip (silicon single crystal substrate substrate chip, cut from 4 inches, thickness 525 μm) to remove residual organic matter and oxides;
[0045] (3) The above-mentioned MoS2 doped coating material was placed in the vacuum chamber of the thermal evaporation coating machine, and the substrate chip was placed on the rotary coating table. The rotation speed was controlled to 45 rpm and the vacuum degree was 3×10 -7 torr, the heating temperature was 550℃ to start the thermal evaporation film deposition; during the deposition process, the deposition rate was measured in real time by a quartz crystal microbalance, and the evaporation rate was adjusted by adjusting the heating power and the evaporation source temperature to control the MoS2 deposition rate within The deposition rate of the enhanced metal material is controlled at When the thickness of the molybdenum disulfide doped material film of the coated chip reaches 80 nm, the gas inlet valve is opened to restore the atmospheric pressure to release the sample to obtain the coated chip.
[0046] (4) Use a plasma cleaning machine (CPC-G / Gplus) to clean the coated chip. Use high-purity oxygen (oxygen purity ≥ 99.995%) as the cleaning gas. Set the gas pressure to 0.5 mTorr, the gas flow rate to 15 sccm, the RF power to 400 W, and the cleaning time to 20 min. After the cleaning is completed, gradually restore the atmospheric pressure to complete the treatment, and obtain a single molecule array chip.
[0047] Comparative Example 1:
[0048] This comparative example is a control experiment of Example 1, and is implemented according to the same steps and conditions as Example 1, except that the step of coating the substrate chip is not included. The specific implementation steps are as follows:
[0049] (1) Ultrasonic cleaning is used to treat the surface of the substrate chip (silicon single crystal substrate substrate chip, cut from 4 inches, thickness 525 μm) to remove residual organic matter and oxides;
[0050] (2) Use a plasma cleaning machine (CPC-G / Gplus) to clean the coated chip. Use high-purity oxygen (oxygen purity ≥ 99.995%) as the cleaning gas. Set the gas pressure to 0.5 mTorr, the gas flow rate to 15 sccm, the RF power to 400 W, and the cleaning time to 20 min. After the cleaning is completed, gradually restore the atmospheric pressure to complete the treatment, and obtain a single molecule array chip.
[0051] Comparative Example 2:
[0052] This comparative example is a control experiment of Example 1, and is implemented according to the same steps and conditions as Example 1, except that the step of plasma cleaning the coated chip is not included. The specific implementation steps are as follows:
[0053] (1) preparing a molybdenum disulfide doped coating material according to a mass ratio of a synergistic metal material to molybdenum disulfide of 1:0.15, wherein the synergistic metal material is ruthenium;
[0054] (2) Using ultrasonic cleaning to treat the surface of the substrate chip (silicon single crystal substrate substrate chip, cut from 4 inches, thickness 525 μm) to remove residual organic matter and oxides;
[0055] (3) The above-mentioned MoS2 doped coating material was placed in the vacuum chamber of the thermal evaporation coating machine, and the substrate chip was placed on the rotary coating table. The rotation speed was controlled to 45 rpm and the vacuum degree was 3×10 -7 torr, the heating temperature was 550℃ to start the thermal evaporation film deposition; during the deposition process, the deposition rate was measured in real time by a quartz crystal microbalance, and the evaporation rate was adjusted by adjusting the heating power and the evaporation source temperature to control the MoS2 deposition rate within The deposition rate of the enhanced metal material is controlled at When the thickness of the molybdenum disulfide doped material film on the coated chip reaches 80 nm, the gas inlet valve is opened to restore the atmospheric pressure to release the sample, thereby obtaining a single molecule array chip.
[0056] Comparative Example 3:
[0057] This comparative example is a control experiment of Example 1, and is implemented according to the same steps and conditions as Example 1, with the only difference being that, under the premise that the total thickness of the coating remains unchanged, the coating material only uses the synergistic metal material (ruthenium). The specific implementation steps are as follows:
[0058] (1) Using ruthenium as the single coating material;
[0059] (2) Using ultrasonic cleaning to treat the surface of the substrate chip (silicon single crystal substrate substrate chip, cut from 4 inches, thickness 525 μm) to remove residual organic matter and oxides;
[0060] (3) The above coating materials were placed in the vacuum chamber of the thermal evaporation coating machine, and the substrate chip was placed on the rotary coating table. The rotation speed was controlled to 45 rpm and the vacuum degree was 3×10 -7 torr, the heating temperature is 550℃ to start the thermal evaporation film deposition; during the deposition process, the deposition rate is measured in real time by a quartz crystal microbalance, and the evaporation rate is adjusted by adjusting the heating power and the evaporation source temperature to control the deposition rate of the coating material within When the film thickness of the coated chip reaches 80 nm, the gas inlet valve is opened to restore the atmospheric pressure to release the sample to obtain the coated chip.
[0061] (4) Use a plasma cleaning machine (CPC-G / Gplus) to clean the coated chip. Use high-purity oxygen (oxygen purity ≥ 99.995%) as the cleaning gas. Set the gas pressure to 0.5 mTorr, the gas flow rate to 15 sccm, the RF power to 400 W, and the cleaning time to 20 min. After the cleaning is completed, gradually restore the atmospheric pressure to complete the treatment, and obtain a single molecule array chip.
[0062] Comparative Example 4:
[0063] This comparative example is a control experiment of Example 1, and is implemented according to the same steps and conditions as Example 1, with the only difference being that, under the premise that the total thickness of the coating remains unchanged, only molybdenum disulfide is used as the coating material. The specific implementation steps are as follows:
[0064] (1) MoS2 is used as the single coating material;
[0065] (2) Using ultrasonic cleaning to treat the surface of the substrate chip (silicon single crystal substrate substrate chip, cut from 4 inches, thickness 525 μm) to remove residual organic matter and oxides;
[0066] (3) The above-mentioned molybdenum disulfide coating material was placed in the vacuum chamber of the thermal evaporation coating machine, and the substrate chip was placed on the rotary coating table. The speed was controlled to 45 rpm and the vacuum degree was 3×10 -7 torr, the heating temperature was 550℃ to start the thermal evaporation film deposition; during the deposition process, the deposition rate was measured in real time by a quartz crystal microbalance, and the evaporation rate was adjusted by adjusting the heating power and the evaporation source temperature to control the MoS2 deposition rate within When the thickness of the molybdenum disulfide film on the coated chip reaches 80 nm, the gas inlet valve is opened to restore the atmospheric pressure to release the sample to obtain the coated chip.
[0067] (4) Use a plasma cleaning machine (CPC-G / Gplus) to clean the coated chip. Use high-purity oxygen (oxygen purity ≥ 99.995%) as the cleaning gas. Set the gas pressure to 0.5 mTorr, the gas flow rate to 15 sccm, the RF power to 400 W, and the cleaning time to 20 min. After the cleaning is completed, gradually restore the atmospheric pressure to complete the treatment, and obtain a single molecule array chip.
[0068] Comparative Example 5:
[0069] This comparative example is a control experiment of Example 1, and is implemented according to the same steps and conditions as Example 1, with the only difference being that the synergistic metal material is replaced by palladium from ruthenium (the mass ratio of the synergistic metal material to molybdenum disulfide and the thickness of the molybdenum disulfide doped material film remain unchanged). The specific implementation steps are as follows:
[0070] (1) preparing a molybdenum disulfide doped coating material according to a mass ratio of a synergistic metal material to molybdenum disulfide of 1:0.15, wherein the synergistic metal material is palladium;
[0071] (2) Using ultrasonic cleaning to treat the surface of the substrate chip (silicon single crystal substrate substrate chip, cut from 4 inches, thickness 525 μm) to remove residual organic matter and oxides;
[0072] (3) The above-mentioned MoS2 doped coating material was placed in the vacuum chamber of the thermal evaporation coating machine, and the substrate chip was placed on the rotary coating table. The rotation speed was controlled to 45 rpm and the vacuum degree was 3×10 -7 torr, the heating temperature was 550℃ to start the thermal evaporation film deposition; during the deposition process, the deposition rate was measured in real time by a quartz crystal microbalance, and the evaporation rate was adjusted by adjusting the heating power and the evaporation source temperature to control the MoS2 deposition rate within The deposition rate of the enhanced metal material is controlled at When the thickness of the molybdenum disulfide doped material film of the coated chip reaches 80 nm, the gas inlet valve is opened to restore the atmospheric pressure to release the sample to obtain the coated chip.
[0073] (4) Use a plasma cleaning machine (CPC-G / Gplus) to clean the coated chip. Use high-purity oxygen (oxygen purity ≥ 99.995%) as the cleaning gas. Set the gas pressure to 0.5 mTorr, the gas flow rate to 15 sccm, the RF power to 400 W, and the cleaning time to 20 min. After the cleaning is completed, gradually restore the atmospheric pressure to complete the treatment, and obtain a single molecule array chip.
[0074] Bioanalysis experiments of low-abundance substances:
[0075] The magnetic beads were modified with Tau217 primary antibody, and the Tau-217 secondary antibody was modified with NHS-Fitc. The Tau-217 antigen of different concentrations was captured by one-step method and sandwich method. After capture, the complex was dropped on the single molecule array chip for single molecule signal number statistical analysis. The specific experimental method is as follows:
[0076] 1. Experimental materials:
[0077] The single molecule array chips prepared in Examples 1 to 3 and Comparative Examples 1 to 5;
[0078] Tau217 primary antibody: antibody used to modify magnetic beads;
[0079] NHS-FITC: fluorescent dye used to modify Tau217 secondary antibody;
[0080] Tau217 antigen: target molecule for capture;
[0081] Magnetic beads: used to modify Tau217 primary antibody;
[0082] PBS buffer: used for dilution and washing.
[0083] 2. Experimental steps:
[0084] 1. Modification of magnetic beads:
[0085] (1) Dilute the Tau217 primary antibody to a final concentration of 10 μg / mL;
[0086] (2) Add Tau217 primary antibody to the magnetic beads, the reaction temperature is 25°C, and the reaction time is 1 hour;
[0087] 2. Modification of Tau217 secondary antibody:
[0088] (1) Dissolve NHS-FITC in PBS buffer at a concentration of 1 mg / mL;
[0089] (2) adding NHS-FITC to the Tau217 secondary antibody to form a Tau217 secondary antibody-NHS-FITC complex, the reaction temperature was 25°C, and the reaction time was 2 hours;
[0090] 3. Capture target molecules:
[0091] Using a one-step method, different concentrations of Tau217 antigen solutions (0.1 pg / mL, 0.5 pg / mL, 1 pg / mL, 10 pg / mL, 100 pg / mL, 1 ng / mL) were added to the modified magnetic beads. The reaction temperature was 4 °C and the reaction time was 12 h.
[0092] 4. Application of composites:
[0093] The captured Tau217 antigen complex was dropped onto the single-molecule array chip, and 10 μL of the complex solution was used for each chip;
[0094] 5. Single molecule signal intensity analysis:
[0095] Fluorescence imaging of single-molecule array chips was performed using a fluorescence microscope (Zeiss Axio Observer);
[0096] The FITC channel (excitation wavelength: 488 nm, emission wavelength: 515 nm) was used to detect and record the fluorescence signal; the number of single-molecule signals under the capture conditions of different concentrations of Tau217 antigen solutions was counted, and the results are shown in Table 1.
[0097] Table 1 Statistics of single molecule signal numbers under capture conditions of different concentrations of Tau217 antigen solutions
[0098]
[0099] It can be seen from the detection results of Examples 1 to 3 in Table 1 that the single-molecule array chip prepared by the method of the present invention can generate stable single-molecule signals under the capture conditions of Tau217 antigen solution with a concentration of 0.1 pg / mL to 1 ng / mL, and has the advantages of high detection sensitivity and stable signal intensity.
[0100] From the comparison of the detection results of Example 1 and Comparative Example 1 in Table 1, it can be seen that the single molecule array chip of the present invention has a significantly higher signal intensity than the common single molecule array chip without MoS2 doping coating.
[0101] From the comparison between Example 1 and Comparative Example 2 in Table 1, it can be seen that the single molecule signal intensity can be significantly improved by the plasma cleaning step of the present invention.
[0102] From the comparison of Example 1, Comparative Example 3 and Comparative Example 4 in Table 1, it can be seen that, under the premise that the coating thickness is exactly the same, the single-molecule signal intensity captured by the Tau217 antigen solution of different concentrations in Example 1 is significantly higher than that of Comparative Example 3 using only the synergistic metal (ruthenium) coating and Comparative Example 4 using only the molybdenum disulfide coating. It can be seen that the synergistic metal material and molybdenum disulfide of the present invention have a significant synergistic effect in improving the single-molecule signal intensity.
[0103] From the comparison of Example 3, Example 1 and Comparative Example 5 in Table 1, it can be seen that, under the conditions that the coating thickness is exactly the same and the mass ratio of the synergistic metal material and molybdenum disulfide is also the same, the single-molecule signal intensity captured by the Tau217 antigen solution of different concentrations in Example 3 is significantly higher than that of Example 1 using ruthenium alone as the synergistic metal material and Comparative Example 5 using palladium alone as the synergistic metal material. It can be seen that the components of the synergistic composite metal material of the present invention have a significant synergistic effect in improving the single-molecule signal intensity.
Claims
1. A method for preparing a single molecule array chip based on molybdenum disulfide doping, characterized in that: The production raw materials include a substrate chip and a molybdenum disulfide doped coating material; the molybdenum disulfide doped coating material is composed of a synergistic metal material and molybdenum disulfide in a mass ratio of 1:0.01 to 0.8; the synergistic metal material includes ruthenium.
2. The method for preparing a single molecule array chip based on molybdenum disulfide doping according to claim 1, characterized in that: The synergistic metal material is composed of ruthenium and palladium in a mass ratio of 1:0.3 to 1.
5.
3. The method for preparing a single molecule array chip based on molybdenum disulfide doping according to claim 2, characterized in that: The method also includes the step of forming a molybdenum disulfide doped material film on a substrate chip to obtain a film-coated chip.
4. The method for preparing a single molecule array chip based on molybdenum disulfide doping according to claim 3, characterized in that: The thickness of the molybdenum disulfide doped material film of the coated chip is 65-140 nm.
5. The method for preparing a single molecule array chip based on molybdenum disulfide doping according to claim 1, characterized in that: The base chip is selected from any one of a silicon single crystal substrate base chip, a FZ single crystal silicon wafer, a CZ single crystal silicon wafer, a semi-insulating single crystal silicon wafer, and an ultra-high purity single crystal silicon wafer.
6. The method for preparing a single molecule array chip based on molybdenum disulfide doping according to claim 3, characterized in that: The preparation steps of the coated chip are specifically as follows: depositing the molybdenum disulfide doped coating material on the base chip by thermal evaporation thin film deposition technology, thereby obtaining the coated chip.
7. The method for preparing a single molecule array chip based on molybdenum disulfide doping according to claim 6, characterized in that: The steps for preparing the coated chip are specifically as follows: S1. Surface treatment of the substrate chip is performed by ultrasonic cleaning or argon plasma cleaning to remove residual organic matter and oxides; S2, placing the molybdenum disulfide doped coating material in the vacuum chamber of the thermal evaporation coating machine, placing the substrate chip on the rotary coating table, controlling the rotation speed to 20-50 rpm, and the vacuum degree to 10 -6 ~10 -7 torr, the heating temperature is 500-600℃ to start thermal evaporation film deposition; During the deposition process, the deposition rate was measured in real time by a quartz crystal microbalance, and the evaporation rate was adjusted by adjusting the heating power and the evaporation source temperature to control the MoS2 deposition rate within The deposition rate of the enhanced metal material is controlled at S3. The sample is released by gradually increasing the ambient pressure or opening the gas inlet valve to restore the atmospheric pressure and obtain a coated chip.
8. The method for preparing a single molecule array chip based on molybdenum disulfide doping according to any one of claims 3 to 7, characterized in that: The method also includes the step of plasma cleaning the coated chip.
9. The method for preparing a single molecule array chip based on molybdenum disulfide doping according to claim 8, characterized in that: The plasma cleaning parameters are: using high-purity oxygen as the cleaning gas, setting the gas pressure to 0.1-1 mTorr, the gas flow rate to 5-20 sccm, the RF power to 100-500 W, and the cleaning time to 5-30 min.
10. A single molecule array chip doped with molybdenum disulfide obtained by the method for preparing a single molecule array chip doped with molybdenum disulfide according to any one of claims 1 to 9.
Citation Information
Patent Citations
Method for preparing molybdenum disulfide thin film
CN104498878A
Rare earth doped molybdenum sulfide monomolecular layer film and preparation method
CN110777356A
Electrochemical luminescence immunosensor and preparation and application thereof
CN114487059A
Nucleic acid detection chip, preparation method and nucleic acid detection method
CN115558705A
Signal enhanced type carcino-embryonic antigen rapid detection electrochemical luminescence sensing method